Photoetching process of tuning fork wafer
Through the combined process of laser lithography and wet corrosion, the problem of low accuracy and efficiency in tuning fork wafer manufacturing is solved, and high-precision and high-efficiency tuning fork wafer production is achieved.
Patent Information
- Application Number
- CN202411251260.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-07
- Publication Date
- 2024-12-03
AI Technical Summary
In the existing tuning fork wafer manufacturing, the wire cutting method leads to low manufacturing accuracy and low production efficiency.
The raw material wafer is cut by laser lithography technology to form a semi-finished wafer, and then the tuning fork wafer is separated by wet corrosion, and the manufacturing accuracy and efficiency are improved using specific cutting profiles and corrosion conditions.
Improves the manufacturing accuracy and production efficiency of tuning fork wafers, ensuring high-precision cutting and separation effects.
Smart Images

Figure CN119070768A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of quartz crystal processing, and in particular to a photolithography and etching process for a tuning fork wafer. Background Art
[0002] Crystal oscillators, also known as quartz crystal resonators, are commonly used in clocks, mobile phones, tablets, microcomputers, calculators, home appliance automatic control and industrial automatic control. Crystal oscillators are very important components in electronic products. Tuning fork chips are the main components of crystal oscillators. During the operation of the crystal oscillator, the tuning fork chip vibrates to generate an oscillation circuit. The tuning fork chip that converts electrical energy and mechanical energy into each other works in a resonant state to provide stable and accurate single-frequency oscillation.
[0003] At present, the tuning fork wafer manufacturing generally uses wire cutting to cut the raw material wafer into tuning fork wafers, with a cutting size error of 100 to 300 microns, and then the electrodes are made on the tuning fork wafers by vacuum silver plating. With respect to the above-mentioned related technologies, the inventor believes that the tuning fork wafers cut by wire cutting have low manufacturing precision and low production efficiency, so there are certain areas for improvement. Summary of the invention
[0004] In order to improve the production efficiency of tuning fork wafers, the present application provides a photolithography etching process for tuning fork wafers.
[0005] The photolithography etching process of a tuning fork wafer provided in the present application adopts the following technical solution: A photolithography etching process for a tuning fork wafer comprises the following steps: Presetting the cutting contour line of the tuning fork wafer on the raw wafer; Cutting the raw wafer using laser lithography based on the cutting contour line to form a semi-finished wafer, wherein the semi-finished wafer is dotted to form a contour pattern of the tuning fork wafer; The semi-finished wafer is wet-etched as a whole to separate the tuning fork wafer.
[0006] Preferably, the tuning fork wafers are distributed in an array in the cutting contour; The cutting contour line has a transverse cutting line, a longitudinal cutting line and a middle waist-shaped cutting line, wherein the transverse cutting line is used to form two side edges of the tuning fork wafer, the longitudinal cutting line is used to form two end faces of the tuning fork wafer, and the middle waist-shaped cutting line is used to form a tuning fork groove of the tuning fork wafer.
[0007] Preferably, the transverse cutting lines in the cutting contour are cut at 47% of the peak power of the laser lithography, the longitudinal cutting lines are cut at 51% of the peak power of the laser lithography, and the middle waist-shaped cutting lines are cut at 50% of the peak power of the laser lithography.
[0008] Preferably, the spot coverage range of the laser lithography is 0.5-5 microns, the hole center distance of the tuning fork wafer contour pattern point breaks on the semi-finished wafer is 1-10 microns, and non-penetrating cracks are formed between adjacent point breaks of the contour pattern.
[0009] Preferably, the laser pulse width of laser lithography is picoseconds or femtoseconds.
[0010] Preferably, the semi-finished wafer is wet-etched as a whole to separate the tuning fork wafer, the temperature of the etching solution in the wet etching is 75±5° C., the pH value of the etching solution is 2.7-2.8, and the thickness of the wet-etched tuning fork semi-finished wafer is 50 microns.
[0011] Preferably, the semi-finished wafer is wet-etched as a whole to separate the tuning fork wafer, and the semi-finished wafer is placed in an etching device for wet etching as a whole.
[0012] Preferably, the etching device comprises a frame and a storage bin arranged in the frame, wherein a corrosion barrel is placed in the storage bin, a wafer storage barrel is placed in the corrosion barrel, an etching liquid is provided in the corrosion barrel, the inner cavity of the wafer storage barrel and the inner cavity of the corrosion barrel are mutually ventilated, and a driving component for driving the wafer storage barrel to rotate is arranged on the frame; The wafer holding barrel comprises a holding barrel body and a wafer holding rack. The inner cavity of the holding barrel body and the inner cavity of the etching barrel are in communication with each other. The wafer holding rack is fixed in the holding barrel body. A plurality of wafer mounting blocks are arranged at intervals on the wafer holding rack. Wafer slots are formed between adjacent wafer mounting blocks. The driving assembly is connected to the wafer holding rack.
[0013] Preferably, the containing barrel body is provided with suction cylinders on both sides of the wafer containing rack, a suction piston is provided in the suction cylinder, a suction inlet and a suction outlet are connected to the suction cylinder, an inlet check valve is installed on the suction inlet, an outlet check valve is installed on the suction outlet, a plurality of flow ports facing the wafer slot are arranged at intervals on the wafer mounting block, a flow channel for connecting all the flow ports is provided on the wafer containing rack, the suction outlet on the suction cylinder is connected to the flow channel, and a linkage assembly for driving the suction piston to move is provided in the corrosion barrel.
[0014] Preferably, the linkage assembly includes a linkage rod arranged on the suction piston, and a linkage ring arranged on the inner wall of the corrosion barrel, the linkage ring is arranged in a wave shape, a linkage slide groove is arranged in the linkage ring, a through groove communicating with the linkage slide groove is opened on the side of the linkage ring, and a linkage roller cooperating with the linkage slide groove is installed on the end of the linkage rod.
[0015] In summary, the present application includes at least one of the following beneficial technical effects: In the present application, the raw material wafer is first cut by laser lithography, and then the tuning fork wafer is separated by wet etching. The tuning fork wafer is manufactured with high precision and high production efficiency by the above method. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 It is a schematic diagram of the process flow of the photolithography and etching process of the tuning fork wafer.
[0017] Figure 2 is a schematic diagram of the cutting contour line.
[0018] Figure 3 It is a structural schematic diagram of the corrosion device.
[0019] Figure 4 It is a first structural schematic diagram of a wafer holding barrel.
[0020] Figure 5 It is a second structural schematic diagram of the wafer holding barrel.
[0021] Figure 6 It is a schematic diagram of the installation of the suction cylinder.
[0022] Description of reference numerals: 100, transverse cutting line; 200, longitudinal cutting line; 300, middle waist-shaped cutting line; 1, frame; 2, storage bin; 3, corrosion barrel; 4, wafer storage barrel; 41, storage barrel body; 42, wafer storage rack; 43, wafer slot; 5, etching liquid; 6, driving assembly; 61, driving support frame; 62, driving support plate; 63, column; 64, first driving motor; 65, driving shaft; 66, connecting seat; 67. Second drive motor; 68. Drive screw; 7. Filter assembly; 71. Connecting sleeve; 72. Filter cloth; 8. Locking bolt; 9. Connecting handle; 10. Heat transfer medium; 11. Electric heating tube; 12. Suction cylinder; 13. Suction piston; 14. Suction inlet; 15. Suction outlet; 16. Circulation port; 17. Circulation channel; 18. Linkage assembly; 181. Linkage rod; 182. Linkage ring; 183. Linkage roller. DETAILED DESCRIPTION
[0023] The following is combined with Figure 1-6 This application is described in further detail.
[0024] A photolithography etching process for tuning fork wafer, referring to Figure 1 As shown, the following steps are included: Step S100, presetting a cutting contour line of a tuning fork wafer on a raw wafer.
[0025] Step S200, cutting the raw material wafer by laser lithography based on the cutting contour line to form a semi-finished wafer, wherein the semi-finished wafer is dotted to form a contour pattern of the tuning fork wafer.
[0026] According to the technical solution defined in steps S100 to S200, specifically, the raw material wafer is a silicon dioxide wafer, which is formed by cutting a silicon dioxide crystal block. In this embodiment, each raw material wafer is in a square shape with a self-defined specification.
[0027] A cutting contour line of the tuning fork wafer is preset on the raw wafer. In this embodiment, the raw wafer is cut by laser lithography equipment, and the cutting contour line is pre-stored in the laser lithography equipment. By placing the raw wafer in the laser lithography equipment, the laser lithography equipment can laser cut the raw wafer along the cutting contour line to form a contour pattern of the tuning fork wafer on the raw wafer.
[0028] The tuning fork chips are distributed in an array in the cutting contour line. The tuning fork chips are distributed in an array in a state where the heads are connected to the heads and the tails are connected to the tails. For details, refer to Figure 2 As shown. The cutting contour line includes a transverse cutting line 100, a longitudinal cutting line 200 and a middle waist-shaped cutting line 300. The transverse cutting line 100 is used to form two side edges of the tuning fork wafer, the longitudinal cutting line 200 is used to form two end faces of the tuning fork wafer, and the middle waist-shaped cutting line 300 is used to form a tuning fork groove of the tuning fork wafer. The tuning fork wafer can be cut and formed by the transverse cutting line 100, the longitudinal cutting line 200 and the middle waist-shaped cutting line 300, and the number of cutting times is small, so as to form as many tuning fork wafers as possible on the raw wafer with the least number of cutting times.
[0029] The horizontal cutting line 100 in the cutting contour is cut at 47% of the peak power of the laser lithography, the vertical cutting line 200 is cut at 51% of the peak power of the laser lithography, and the middle waist-shaped cutting line 300 is cut at 50% of the peak power of the laser lithography. The cutting speed of the laser lithography is 120.00 mm / s, and the peak power can be set according to the actual situation, which is not specifically limited in this embodiment.
[0030] By changing the cutting power of the transverse cutting line 100 , the longitudinal cutting line 200 and the middle waist-shaped cutting line 300 , the shaping effect of the tuning fork wafer can be ensured during the cutting process, and the tuning fork wafer will not break or crack.
[0031] In one embodiment, the laser pulse width of laser lithography is picoseconds or femtoseconds, the spot coverage range of laser lithography is 0.5-5 microns, the center distance of the holes of the tuning fork wafer contour pattern point breaks on the semi-finished wafer is 1-10 microns, and non-penetrated cracks are formed between adjacent point breaks of the contour pattern, that is, the spot of laser lithography can penetrate the raw wafer, and due to the characteristics of the raw wafer being made of silicon dioxide, non-penetrated cracks are formed between adjacent point breaks, and the crack is in a semi-penetrated state, that is, there is a crack but it is not completely penetrated.
[0032] Step S300, wet etching the entire semi-finished wafer to separate the tuning fork wafer.
[0033] According to the technical solution defined in step S300, specifically, the semi-finished wafer is wet-etched as a whole to separate the tuning fork wafer, and the semi-finished wafer is placed in an etching device for overall wet etching. In one embodiment, the temperature of the etching solution 5 in the wet etching is 75±5°C, the pH value of the etching solution 5 is 2.7-2.8, and the thickness of the wet-etched tuning fork semi-finished wafer is 50 microns.
[0034] By wet etching the semi-finished wafer, due to the anisotropy of the corrosion of the silicon dioxide material, that is, when the surface of the semi-finished wafer is corroded by 0.05 mm, the side of the semi-finished wafer is only corroded by 0.005 mm. Therefore, when the semi-finished wafer is wet-etched in the etching solution 5, the surface of the semi-finished wafer will be corroded. The wet etching not only removes the loose layer on the surface of the semi-finished wafer, but also corrodes the above-mentioned non-penetrated cracks, thereby separating the tuning fork wafer from the semi-finished wafer.
[0035] The loose layer is a functionally damaged layer on the surface of the raw wafer during the grinding process.
[0036] Reference Figure 3 As shown, the etching device includes a frame 1 and a containing chamber 2 arranged in the frame 1, a corrosion barrel 3 is placed in the containing chamber 2, a wafer containing barrel 4 is placed in the corrosion barrel 3, an etching liquid 5 is provided in the corrosion barrel 3, the inner cavity of the wafer containing barrel 4 and the inner cavity of the corrosion barrel 3 are mutually circulated, and a driving component 6 for driving the wafer containing barrel 4 to rotate is arranged on the frame 1.
[0037] The corrosion barrel 3 is made of PVC plastic material. In one embodiment, the etching solution 5 is ammonium bifluoride solution.
[0038] Reference Figure 4 and Figure 5As shown, the wafer holding barrel 4 includes a holding barrel body 41 and a wafer holding rack 42. The inner cavity of the holding barrel body 41 and the inner cavity of the etching barrel 3 are in communication with each other. The wafer holding rack 42 is fixed in the holding barrel body 41. A plurality of wafer mounting blocks are arranged at intervals on the wafer holding rack 42. Wafer slots 43 are formed between adjacent wafer mounting blocks. Semi-finished wafers are vertically inserted in the wafer slots 43. The driving assembly 6 is connected to the wafer holding rack 42.
[0039] In order to maintain the communication between the inner cavity of the containing barrel body 41 and the inner cavity of the corrosion barrel 3, a connecting port is provided at the bottom of the containing barrel body 41, and a filter mesh assembly 7 is provided on the connecting port. The filter mesh assembly 7 includes a connecting sleeve 71 and a filter mesh cloth 72, and the connecting sleeve 71 is detachably connected to the connecting port of the containing barrel body 41, that is, the connecting sleeve 71 is detachably connected to the containing barrel body 41 by connecting bolts, the connecting sleeve 71 is axially penetrated, and the filter mesh cloth 72 covers the connecting sleeve 71.
[0040] Therefore, when the semi-finished wafers in the wafer holding rack 42 are corroded, tuning fork wafers will be left, and the tuning fork wafers will fall onto the filter mesh cloth 72. The filter mesh cloth 72 and the connecting sleeve 71 can be removed from the holding barrel 41 through the detachable connecting sleeve 71, thereby facilitating the pouring out of the tuning fork wafers on the filter mesh cloth 72.
[0041] The wafer holding rack 42 is fixed to the holding barrel 41 by means of locking bolts 8 , and a connecting handle 9 for connecting the driving assembly 6 is provided on the wafer holding rack 42 .
[0042] Reference Figure 3 As shown, the driving assembly 6 includes a driving support frame 61 disposed on the frame 1, and a driving support plate 62 is slidably mounted on the driving support frame 61 in the vertical direction, that is, four columns 63 are disposed on the driving support frame 61, and four corners of the driving support plate 62 are slidably mounted on the columns 63. A first driving motor 64 is fixed on the driving support plate 62, and a driving shaft 65 is connected to the output shaft of the first driving motor 64. The driving shaft 65 extends into the middle storage bin 2 to be connected to the wafer storage barrel 4, and the end of the driving shaft 65 is specifically connected to the connecting handle 9 of the wafer storage frame 42, wherein a connecting seat 66 is provided at the end of the driving shaft 65 to be connected to the connecting handle 9.
[0043] The driving support frame 61 is provided with a driving part for driving the driving support plate 62 to move up and down. The driving part can realize the up and down movement of the wafer holding barrel 4, so as to facilitate the placement of the wafer holding barrel 4 into the etching barrel 3, and then the wafer holding barrel 4 can be rotated in the circumferential direction through the first driving motor 64, so that the wafer holding barrel 4 rotates, so that the semi-finished wafers in the wafer holding barrel 4 can contact with the etching liquid 5, and the tuning fork wafers obtained after etching can fall onto the filter cloth 72 more smoothly.
[0044] In one embodiment, the driving unit includes a second driving motor 67 fixed on the driving support frame 61 , and a driving screw 68 is connected to the output shaft of the second driving motor 67 . The driving screw 68 is threadedly mounted on the driving support plate 62 .
[0045] It is worth noting that a heat conducting medium 10 is provided in the storage bin 2. In one embodiment, the heat conducting medium 10 is water. An electric heating tube 11 for heating the heat conducting medium 10 is provided in the storage bin 2. The electric heating tube 11 is used to heat the heat conducting medium 10 and keep the heat conducting medium 10 in a constant temperature state. The heated heat conducting medium 10 can increase the temperature of the etching solution 5, thereby improving the etching efficiency of the etching solution 5 on the semi-finished wafer.
[0046] In the present application, in order to further improve the corrosion effect of the etching solution 5 on the semi-finished wafer, the tuning fork wafer can be effectively separated from the semi-finished wafer.
[0047] Reference Figure 6 As shown, a suction cylinder 12 is provided on both sides of the wafer holding rack 42 on the containing barrel body 41, a suction piston 13 is provided in the suction cylinder 12, a suction inlet 14 and a suction outlet 15 are connected to the suction cylinder 12, the suction inlet 14 and the suction outlet 15 are respectively connected to the inner cavity of the suction cylinder 12, wherein an inlet check valve is installed on the suction inlet 14, and an outlet check valve is installed on the suction outlet 15.
[0048] A plurality of flow ports 16 are arranged at intervals on the wafer mounting block, and the flow ports 16 are arranged toward the side of the wafer slot 43. A flow channel 17 for connecting the flow ports 16 is arranged on the wafer holding rack 42. The suction outlet 15 on the suction cylinder 12 is connected to the flow channel 17. A linkage assembly 18 for driving the suction piston 13 to move is arranged in the corrosion barrel 3.
[0049] In one embodiment, the linkage assembly 18 includes a linkage rod 181 disposed on the suction piston 13, and a linkage ring 182 disposed on the inner wall of the corrosion barrel 3. The linkage ring 182 is sleeved and fixed on the inner wall of the corrosion barrel 3. The linkage ring 182 and the corrosion barrel 3 are coaxially arranged. The linkage ring 182 is arranged in a wave shape. A linkage slide groove is arranged in the linkage ring 182. The shape of the linkage slide groove is the same as that of the linkage ring 182 and is arranged in a wave shape. A through groove communicating with the linkage slide groove is opened on the side of the linkage ring 182. A linkage roller 183 cooperating with the linkage slide groove is installed at the end of the linkage rod 181. Among them, the cross section of the linkage slide groove is arranged in an I-shaped arrangement, and the arrangement of the through groove facilitates the linkage roller 183 to be embedded in the linkage slide groove and form a sliding match with the linkage slide groove.
[0050] Therefore, when the chip holding barrel 4 rotates in the corrosion barrel 3, the linkage roller 183 will form a sliding fit with the linkage slide groove, and the linkage slide groove is arranged in a wave shape, so that when the chip holding barrel 4 rotates, the linkage rod 181 can drive the suction piston 13 to perform a suction action, thereby being able to extract the etching liquid 5 in the corrosion barrel 3 and pressurize it to be discharged from the flow port 16 to the chip slot 43. On the one hand, the flow effect of the etching liquid 5 in the chip slot 43 is improved, and the corrosion effect of the etching liquid 5 on the semi-finished chip is improved. On the other hand, the tuning fork chip that has been corroded can be further separated from the semi-finished chip.
[0051] The above are all preferred embodiments of the present application, and the protection scope of the present application is not limited thereto. Therefore, any equivalent changes made according to the structure, shape, and principle of the present application should be included in the protection scope of the present application.
Claims
1. A tuning fork wafer photolithography etching process, characterized in that: The steps include: Presetting the cutting contour line of the tuning fork wafer on the raw wafer; Cutting the raw wafer using laser lithography based on the cutting contour line to form a semi-finished wafer, wherein the semi-finished wafer is dotted to form a contour pattern of the tuning fork wafer; The semi-finished wafer is wet-etched as a whole to separate the tuning fork wafer.
2. The photolithography etching process of a tuning fork wafer according to claim 1, characterized in that: The tuning fork wafers are distributed in an array in the cutting contour; The cutting contour line comprises a transverse cutting line (100), a longitudinal cutting line (200) and a middle waist-shaped cutting line (300), wherein the transverse cutting line (100) is used to form two side edges of the tuning fork wafer, and the longitudinal cutting line (200) is used to form two end faces of the tuning fork wafer. The middle waist-shaped cutting line (300) is used to form the tuning fork groove of the tuning fork wafer.
3. The photolithography etching process of a tuning fork wafer according to claim 2, characterized in that: The transverse cutting line (100) in the cutting contour line is cut at 47% of the peak power of laser lithography, the longitudinal cutting line (200) is cut at 51% of the peak power of laser lithography, and the middle waist-shaped cutting line (300) is cut at 50% of the peak power of laser lithography.
4. The photolithography etching process of a tuning fork wafer according to claim 1, characterized in that: The spot coverage range of laser lithography is 0.5-5 microns, the hole center distance of the tuning fork wafer contour pattern point breaks on the semi-finished wafer is 1-10 microns, and non-penetrating cracks are formed between adjacent point breaks of the contour pattern.
5. The photolithography etching process of a tuning fork wafer according to claim 1, characterized in that: Laser lithography uses laser pulses with a width of picoseconds or femtoseconds.
6. The photolithography etching process of a tuning fork wafer according to claim 1, characterized in that: The semi-finished wafer is wet-etched as a whole to separate the tuning fork wafer. The temperature of the etching solution (5) in the wet etching is 75±5° C., the pH value of the etching solution (5) is 2.7-2.8, and the thickness of the tuning fork semi-finished wafer is 50 μm.
7. The photolithography etching process of a tuning fork wafer according to claim 1, characterized in that: The semi-finished wafer is wet-etched as a whole to separate the tuning fork wafer, and the semi-finished wafer is placed in an etching device for wet etching as a whole.
8. The photolithography etching process of a tuning fork wafer according to claim 7, characterized in that: The etching device comprises a frame (1) and a storage chamber (2) arranged in the frame (1); an etching barrel (3) is placed in the storage chamber (2); a wafer storage barrel (4) is placed in the etching barrel (3); an etching liquid (5) is provided in the etching barrel (3); the inner cavity of the wafer storage barrel (4) and the inner cavity of the etching barrel (3) are in communication with each other; and a driving component (6) for driving the wafer storage barrel (4) to rotate is arranged on the frame (1); The wafer holding barrel (4) comprises a holding barrel body (41) and a wafer holding rack (42), the inner cavity of the holding barrel body (41) and the inner cavity of the etching barrel (3) are in communication with each other, the wafer holding rack (42) is fixed in the holding barrel body (41), a plurality of wafer mounting blocks are arranged on the wafer holding rack (42) at intervals, and wafer slots (43) are formed between adjacent wafer mounting blocks, and the driving component (6) is connected to the wafer holding rack (42).
9. The photolithography etching process of a tuning fork wafer according to claim 8, characterized in that: The containing barrel body (41) is provided with a suction cylinder (12) on both sides of the wafer containing rack (42), a suction piston (13) is provided in the suction cylinder (12), a suction inlet (14) and a suction outlet (15) are connected to the suction cylinder (12), an inlet non-return valve is installed on the suction inlet (14), an outlet non-return valve is installed on the suction outlet (15), a plurality of flow ports (16) facing the wafer slot (43) are arranged at intervals on the wafer mounting block, a flow channel (17) for connecting all the flow ports (16) is arranged on the wafer containing rack (42), the suction outlet (15) on the suction cylinder (12) is connected to the flow channel (17), and a linkage assembly (18) for driving the suction piston (13) to move is arranged in the corrosion barrel (3).
10. The photolithography etching process of a tuning fork wafer according to claim 9, characterized in that: The linkage assembly (18) comprises a linkage rod (181) arranged on the suction piston (13), and a linkage ring (182) arranged on the inner wall of the corrosion barrel (3); the linkage ring (182) is arranged in a wave shape, a linkage slide groove is arranged in the linkage ring (182), a through groove communicating with the linkage slide groove is opened on the side of the linkage ring (182), and a linkage roller (183) cooperating with the linkage slide groove is installed at the end of the linkage rod (181).
Citation Information
Cited By
Surface crystal wafer and processing method of surface crystal oscillator
CN119995540A