Slab feeding method for increasing average charging temperature of thick hot-rolled products

Through the method of alternately loading of storage and direct-connected blanks, the problem of excessive residence time of slabs is solved, the furnace temperature and output are improved, the production cost is reduced, and the production efficiency and energy-saving effect are improved.

CN119076657APending Publication Date: 2024-12-06BAOSTEEL ZHANJIANG IRON & STEEL CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411281264.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-13
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

In the prior art, the slabs of thick-specification hot-rolled products stay in the slab warehouse for too long, resulting in a low furnace temperature, affecting production efficiency and energy-saving effects.

Method used

By using the method of alternate loading of storage and direct-connected blanks, the storage and direct-connected blanks in each steel loading plan can reduce the residence time of the slab in the inventory, and conduct quality inspections in the slab warehouse and Temperature field management.

Benefits of technology

It effectively improves the average furnace loading temperature of thick-specification hot-rolled products, shortens the time of slabs in the furnace, increases the hourly output of the production line, reduces production costs, and creates economic benefits.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119076657A_ABST
    Figure CN119076657A_ABST
Patent Text Reader

Abstract

The invention discloses a plate blank feeding method for effectively increasing the average charging temperature of thick-specification hot-rolled products, which comprises the following steps of: determining the planned number of steel charging according to the total steel tapping amount of a rolling plan, and sequentially carrying out steel charging and feeding on plate blanks of each steel charging plan according to a manner of alternately feeding stored blanks and directly connected blanks. Wherein the operation of alternately feeding the stored blanks and the directly-connected blanks in each plan is as follows: firstly, calculating the quantity of the stored blanks and the quantity of the directly-connected blanks; the blanks are stored according to the blank storage amount, the newly-stored blanks are directly-connected blanks, direct feeding is carried out, during the period, the directly-connected blanks and the stored blanks are alternately fed, the production continuity is met, and finally the remaining stored blanks are loaded. By means of the method, it is not needed to wait for feeding after all the slabs are put in storage, on the premise that production continuity is guaranteed, the staying time of the slabs in a slab yard is shortened, and therefore the average charging temperature is increased. The in-furnace time of the plate blank is shortened, and the hourly yield of a production line is improved, so that the production cost of enterprises is reduced, and actual economic benefits are created for the enterprises.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of steel production, and in particular relates to a slab feeding method for improving the average furnace charging temperature of thick-gauge hot-rolled products. Background Art

[0002] Thick hot-rolled products generally include hot-rolled common structural products with a finished thickness of more than 12 mm, usually referring to hot-rolled common structural products with a yield strength of ≤355 mPa. The production process includes converter, RH, continuous casting, cutting, hot delivery, hot charging, heating and rolling steps.

[0003] At present, hot delivery and hot charging can connect the entire process of steel production more closely, effectively reduce the process links in the production process, and significantly improve production efficiency. In the existing production process, the rhythm of the cutting process slabs sent to the slab warehouse is slower than the rhythm of loading into the furnace. In order to ensure the stability of production and the continuity of planned transition, thick specifications are produced in batches. Therefore, the production process of thick specifications is: after the slabs are cut, they are first sent to the slab warehouse for temporary storage. After all the slabs are delivered, the slabs that meet the requirements are loaded into the furnace from the slab warehouse according to the rolling plan. Hot delivery and hot charging can greatly reduce the reheating temperature and time in the heating furnace, and the amount of iron oxide scale is also reduced. The thickness of the decarburization layer and the oxidation dot layer can also be effectively controlled. With the hot delivery and hot charging process, the higher the temperature of the slab entering the furnace, the shorter the heating residence time in the furnace, and the less gas consumption during heating, the more energy-saving the production and the higher the output. The existing method of storing all thick slabs temporarily before loading them into the furnace will result in a lower temperature for the slabs first fed in, especially when the steel output is large. The longer the slabs stay in the slab warehouse, the lower the temperature of the slabs fed into the furnace. Therefore, how to improve the average charging temperature of thick hot-rolled products has become a new research topic. Summary of the invention

[0004] The present invention provides a slab loading method for improving the average charging temperature of thick-gauge hot-rolled products, which can reduce the residence time of the slabs in the slab warehouse and effectively improve the average charging temperature of thick-gauge hot-rolled products in the production process.

[0005] To achieve the above objectives, the present invention adopts the following technical scheme: the number of steel charging plans is determined according to the total amount of steel produced in the rolling plan, and the number of slabs required for each steel charging plan is N furnaces, where 3≤N≤7, and N is an integer. The slabs of each steel charging plan are charged in turn in the manner of alternating loading of storage slabs and direct-connected slabs;

[0006] The operation steps of the alternate loading method of billet storage and direct billet in each steel loading plan are as follows:

[0007] (1) First calculate the stock volume a,

[0008]

[0009] (3) Calculate the amount of direct-connected billet b, b = Na.

[0010] (3) The slabs sent to the slab warehouse are stacked and temporarily stored on both sides of the roller until the number reaches the storage quantity a, and the storage is completed.

[0011] (4) The slabs fed in again are used as direct-connected slabs and are directly sent to the roller conveyor for loading into the furnace. When a furnace of direct-connected slabs is loaded into the furnace, the storage slabs described in step (3) are used to follow the loading into the furnace. When the direct-connected slabs of the next furnace are delivered, the storage slabs are stopped for loading. Step (4) is repeated until all the direct-connected slabs b are loaded.

[0012] (5) Check whether there are any stored blanks on both sides of the roller. If there are, load all the remaining blanks.

[0013] Furthermore, the slabs are first subjected to quality inspection before being put into storage: if the slabs have no quality problems, they are directly put into storage; if the slabs have quality problems, the quality problems are first processed as required and then put into storage after the processing is completed.

[0014] Furthermore, the temperature field in the slab warehouse is managed. Management measures include normalizing the closing of doors and windows of the slab warehouse, building slow cooling walls in the slab warehouse, and stacking the slabs in a centralized manner.

[0015] The beneficial effect of the present invention is that compared with the prior art, the present invention stores the slabs first, then directly connects the slabs and alternately loads the slabs, and finally loads the remaining slabs. There is no need to wait for all the slabs to be stored before loading. Under the premise of ensuring production continuity, the residence time of the slabs in the slab warehouse is reduced, thereby achieving an increase in the average furnace charging temperature. In turn, the time of the slabs in the furnace can be shortened, the hourly output of the production line can be increased, thereby reducing the production cost of the enterprise and creating actual economic benefits for the enterprise. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 The present invention is a flow chart of slab loading in a single steel charging plan in the method of the present invention. DETAILED DESCRIPTION

[0017] In order to enable those skilled in the art to fully understand the technical content described in the present invention, the present invention is further described in detail below in conjunction with specific factual cases.

[0018] like Figure 1As shown, the present invention determines the number of steel charging plans according to the total amount of steel output in the rolling plan, and the amount of slabs required for each steel charging plan is N furnaces, wherein 3≤N≤7. In specific production, it is assumed that the total amount of steel output in the casting plan is M furnaces. When M≤N, it is one steel charging plan; when M>N, the number of plans = M / 7. If it is divisible, the quotient is the number of plans, and if there is a remainder, the quotient+1 is the number of plans. For example, if the total amount of steel output in the casting plan is 11 furnaces, the number of plans is 2; in actual production, the amount of slabs N in each plan can be determined according to the actual situation, such as 7 furnaces for the first plan and 4 furnaces for the second plan; or the first plan can be 6 furnaces and the second plan can be 5 furnaces.

[0019] After the planned number is determined, the slabs of each loading plan are loaded in turn by alternating loading of storage slabs and direct-connected slabs.

[0020] like Figure 1 As shown, the operation steps of the alternate loading method of billet storage and direct billet loading in each steel loading plan are as follows: (1) first calculate the billet storage amount a,

[0021]

[0022] (2) Calculate the amount of direct-connected billets b, b = Na.

[0023] (3) The slabs sent to the slab warehouse are stacked and temporarily stored on both sides of the roller until the number reaches the storage quantity a, and the storage is completed.

[0024] (4) The slabs fed in again are used as direct-connected slabs and are directly sent to the roller conveyor for loading into the furnace. When a furnace of direct-connected slabs is loaded into the furnace, the storage slabs described in step (3) are used to follow the loading into the furnace. When the direct-connected slabs of the next furnace are delivered, the storage slabs are stopped for loading. Step (4) is repeated until all the direct-connected slabs b are loaded.

[0025] (5) Check whether there are any stored blanks on both sides of the roller. If there are, load all the remaining blanks.

[0026] Preferably, the slabs are first subjected to quality inspection before entering the warehouse: if there are no quality problems with the slabs, they are directly put into the warehouse; if there are quality problems with the slabs, the quality problems are first processed as required and then put into the warehouse after the processing is completed. In addition, the present invention also manages the temperature field in the slab warehouse, and the management measures include normalized closing management of doors and windows of the slab warehouse, construction of slow cooling walls in the slab warehouse, and centralized stacking of the slabs.

[0027] Implementation case 1.

[0028] This example adopts the slab charging method of the present invention. Starting from the converter, the continuous casting machine outputs 11 furnaces of 3,850 tons of 28mm Q355B hot-rolled products at one time, which is divided into two steel charging plans of slab quantities of 6 furnaces and 5 furnaces.

[0029] The first batch of slabs is planned to be 6 furnaces; the calculation shows that the storage amount That is, the storage quantity is 3 furnaces; the direct connection quantity b=6-3, which is 3 furnaces. The specific operation is: after the slabs from the 1st to 3rd furnaces are put into storage, they are concentrated and stacked on both sides of the loading roller. After the first piece of the 4th furnace is put into storage, the slabs start to be directly loaded. After all the loading of the 4th furnace is completed, the storage slabs are loaded immediately, and when the 5th furnace is delivered, they are directly connected again. In this way, the loading of the slabs from the 6 furnaces in the plan is completed.

[0030] The second steel loading plan has 5 furnaces of slabs. The calculation shows that the slab storage quantity That is, the storage quantity is 2 furnaces, and the direct connection quantity b=5-2 is 3 furnaces. The specific operation is: after the slabs from the 7th and 8th furnaces are put into storage, they are concentrated and stacked on both sides of the loading roller. After the first piece of the 9th furnace is put into storage, the slabs start to be directly connected, and the storage is alternately loaded during this period to ensure continuous production until all the slabs are loaded.

[0031] According to the method of the above-mentioned implementation case 1, the average time from slab cutting to furnace loading is 1.04h, and the average furnace loading temperature of the slab is 809℃. After the slab is put into the furnace, the heating furnace has been drawing steel at the optimal rhythm, with an average furnace outlet temperature of 1191℃, an average furnace time of 222min, and a calculated hourly output of 827t / h.

[0032] Implementation case 2.

[0033] This example adopts the slab loading method of the present invention. Starting from the converter, the continuous casting machine has a steel output of 6 furnaces of 2100 tons of 12-15mm specification Q355B hot-rolled products at one time. The steel output is less than 7. It is implemented according to a steel loading plan. It can be calculated that the storage amount a is 3 furnaces and the direct-connected amount is 3 furnaces. The specific operation is: the slabs of the 1st to 3rd furnaces are concentrated and stacked on both sides of the loading roller after the 1st piece of the 4th furnace is stored. After the 4th furnace is fully loaded, the storage billets are loaded immediately, and when the 5th furnace is delivered, they are directly connected again. In this way, the loading is alternated to complete the loading of all the slabs in the plan.

[0034] According to the method of the above-mentioned implementation case 2, the average time from slab cutting to furnace loading is 1.05h, and the average furnace loading temperature of the slab is 824℃. After the slab is put into the furnace, the heating furnace always uses the optimal rhythm to extract steel, the average furnace temperature is 1226℃, the average furnace time is 166min, and the calculated hourly output is 879t / h.

[0035] The above are only preferred embodiments of the present invention. It should be noted that the above preferred embodiments should not be regarded as limiting the present invention, and the protection scope of the present invention should be based on the scope defined by the claims. For those skilled in the art, several improvements and modifications can be made without departing from the spirit and scope of the present invention, and these improvements and modifications should also be regarded as the protection scope of the present invention.

Claims

1. A slab feeding method for increasing the average charging temperature of thick hot-rolled products, characterized in that: Determine the number of steel charging plans according to the total amount of steel produced in the rolling plan. The number of slabs required for each steel charging plan is N furnaces, where 3≤N≤7; load the slabs of each steel charging plan in turn by alternating loading of storage slabs and direct-connection slabs; The operation steps of the alternate loading method of billet storage and direct billet in each steel loading plan are as follows: (1) First calculate the stock volume a, (2) Calculate the amount of direct-connected billets b, b = Na; (3) The slabs sent to the slab warehouse are stacked and temporarily stored on both sides of the roller until the number reaches the storage quantity a, and the storage is completed; (4) The slabs fed in again are directly fed to the roller conveyor for loading into the furnace as direct-connected slabs; when a furnace of direct-connected slabs is loaded into the furnace, the storage slabs described in step (3) are used to load the slabs into the furnace immediately; when the direct-connected slabs of the next furnace are fed in, the storage slabs are stopped for loading; and step (4) is repeated until all the direct-connected slabs b are loaded; (5) Check whether there are any stored blanks on both sides of the roller. If there are, load all the remaining blanks.

2. The control method for increasing the average charging temperature of thick hot-rolled products according to claim 1, characterized in that: The slabs are first subjected to quality inspection upon entering the warehouse: If the slab has no quality problems, it will be put into storage directly; If there are any quality problems with the slab, it should be processed as required first and then put into storage after the processing is completed.

3. The control method for increasing the average charging temperature of thick hot-rolled products according to claim 1 or 2, characterized in that: The temperature field in the slab warehouse is managed. Management measures include normal closing of doors and windows of the slab warehouse, construction of slow cooling walls in the slab warehouse and centralized stacking of slabs.

Citation Information

Patent Citations

  • Slab yard and heating furnace layout for thick plate cold blank and hot blank split charging and charging method through same

    CN112575175A

  • Steel enterprise heating furnace group optimization scheduling method based on multi-agent simulation

    CN116088439A

  • Method and system for shortening steel charging interval time of hot delivery direct charging

    CN116571581A

  • Alternative loading of continuously cast plate slab and microcomputer optimized heating technology

    CN1178840A

  • Layout of slab storerooms and furnaces for separate charging of cold blanks and hot blanks of thick plate, and furnace charging method

    US20220316801A1