High-temperature-resistant, corrosion-resistant and irradiation-resistant fluororubber for nuclear use and preparation method thereof
By combining high fluorine content fluorine rubber with peroxide vulcanization system and adding reinforcement and stabilizer, a stable network structure is formed, which solves the problem of insufficient performance of nuclear rubber in high temperature, corrosion and irradiation environments, and achieves the realization of the ability of nuclear rubber High durability and processing performance improvements under extreme conditions.
Patent Information
- Application Number
- CN202411404521.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-10
- Publication Date
- 2024-12-06
AI Technical Summary
Existing nuclear rubber materials have poor performance in high temperature, corrosion and irradiation environments, difficult to maintain elasticity and durability, and insufficient processing performance.
The high fluorine rubber content is combined with the peroxide vulcanization system, and reinforcement, filler and stabilizer are added to form a stable network structure through vulcanization and radiation resistance, which improves high temperature and radiation resistance.
Maintain elasticity and durability in the temperature range of -40°C to +250°C, resist aging and chemical structural changes in the radiation environment, and improve wear resistance and service life.
Smart Images

Figure CN119081318A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of nuclear rubber, in particular to a nuclear high temperature resistant, corrosion resistant and radiation resistant fluororubber and a preparation method thereof. Background Art
[0002] High temperature resistant, corrosion resistant and radiation resistant fluororubber for nuclear use is a special rubber material widely used in the nuclear industry. The preparation process of high temperature resistant, corrosion resistant and radiation resistant fluororubber for nuclear use is also very important. Through reasonable formula design and production process, it can be ensured that fluororubber has good processing performance and reliability while maintaining excellent performance. Therefore, the present invention proposes a high temperature resistant, corrosion resistant and radiation resistant fluororubber for nuclear use and a preparation method thereof. Summary of the invention
[0003] To achieve the above-mentioned purpose, the present invention provides the following technical scheme: a high-temperature resistant, corrosion-resistant and radiation-resistant fluororubber for nuclear use, wherein a fluororubber raw rubber with a high fluorine content and excellent performance is selected as a basic material. There are many types of fluororubber raw rubber, such as vinylidene fluoride-hexafluoropropylene copolymer (Viton A), tetrafluoroethylene-propylene copolymer (Viton B), etc. Since nuclear fluororubber needs to be resistant to high temperature and radiation, a peroxide vulcanization system is usually selected. The peroxide vulcanizing agent can induce a cross-linking reaction of the fluororubber at high temperature to form a stable network structure, thereby improving the high-temperature resistance and radiation resistance of the rubber.
[0004] Preferably, in order to improve the physical and mechanical properties and processing properties of the fluororubber, it is necessary to add appropriate amounts of reinforcing agents and fillers. Commonly used reinforcing agents include carbon black, white carbon black, etc., and fillers include calcium carbonate, barium sulfate, etc. In order to prevent the fluororubber from aging under harsh environments such as high temperature and radiation, it is necessary to add stabilizers and antioxidants. These additives can absorb or neutralize harmful free radicals, thereby extending the service life of the fluororubber.
[0005] Preferably, the types and amounts of the vulcanizing agent, reinforcing agent, filler, stabilizer and antioxidant are determined, and small and medium tests are carried out to verify the rationality and feasibility of the formula.
[0006] Preferably, the temperature and time need to be controlled during the mixing process to ensure that the raw materials are fully mixed and uniformly mixed, and the parameters such as temperature, pressure and speed need to be controlled during the molding process to ensure that the size and shape of the product meet the requirements.
[0007] Preferably, if it is necessary to further improve the radiation resistance of the fluororubber, a radiation resistance treatment is performed during or after the preparation process. The radiation resistance treatment usually adopts methods such as radiation crosslinking or radiation grafting, which induces crosslinking or grafting reactions of the fluororubber molecular chains through radiation, thereby improving its radiation resistance.
[0008] A method for preparing high temperature resistant, corrosion resistant and radiation resistant fluororubber for nuclear use comprises the following steps:
[0009] S1: Raw material selection, fluororubber raw rubber, vulcanizing agent, reinforcing agent, filler, stabilizer and antioxidant;
[0010] S2: Formula design: determine the formula of fluororubber according to the use environment and performance requirements. The formula design comprehensively considers factors such as the material's high temperature resistance, corrosion resistance, radiation resistance, and processing performance;
[0011] S3: Mixing: adding raw materials such as fluororubber, vulcanizing agent, reinforcing agent, filler, stabilizer and antioxidant into an internal mixer according to a certain proportion for mixing;
[0012] S4: calendering or extrusion, the mixed fluororubber rubber is molded by a calender or extruder;
[0013] S5: Vulcanization: put the molded fluororubber products into a vulcanization tank and vulcanize them at a certain temperature and pressure;
[0014] S6: Post-processing: Post-processing of the vulcanized fluororubber products, such as deburring, cleaning, drying, etc. During the post-processing process, attention should be paid to protecting the surface quality of the products to avoid scratches and contamination.
[0015] Compared with the prior art, the present invention has the following beneficial effects:
[0016] The fluororubber of the present invention can maintain its elasticity and durability under extreme temperature conditions, and can generally be used in a temperature range of -40°C to +250°C. In a radiation environment, the fluororubber can maintain its elasticity and chemical stability, and is not prone to hardening, embrittlement or chemical structure changes. The fluororubber has high wear resistance and aging resistance, and can be used in mechanical equipment that rotates at high speed and moves frequently, and is not prone to aging and deterioration. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 The present invention is a flow chart for preparing the high temperature resistant, corrosion resistant and radiation resistant fluororubber. DETAILED DESCRIPTION
[0018] See also Figure 1 The present invention provides a technical solution: a nuclear high temperature resistant, corrosion resistant, radiation resistant fluororubber, such as Figure 1As shown, fluororubber raw rubber with high fluorine content and excellent performance is selected as the basic material. There are many types of fluororubber raw rubber, such as vinylidene fluoride-hexafluoropropylene copolymer (Viton A), tetrafluoroethylene-propylene copolymer (Viton B), etc. Since nuclear fluororubber needs to be resistant to high temperature and radiation, a peroxide vulcanization system is usually selected. The peroxide vulcanizing agent can induce a cross-linking reaction of fluororubber at high temperature to form a stable network structure, thereby improving the high temperature resistance and radiation resistance of the rubber;
[0019] In order to improve the physical and mechanical properties and processing properties of fluororubber, it is necessary to add an appropriate amount of reinforcing agent and filler. Commonly used reinforcing agents include carbon black, white carbon black, etc., and fillers include calcium carbonate, barium sulfate, etc. In order to prevent fluororubber from aging under harsh environments such as high temperature and radiation, it is necessary to add stabilizers and antioxidants. These additives can absorb or neutralize harmful free radicals, thereby extending the service life of fluororubber. Determine the type and amount of vulcanizer, reinforcing agent, filler, stabilizer and antioxidant, and conduct small and medium tests to verify the rationality and feasibility of the formula. During the mixing process, it is necessary to control the temperature and time to ensure that the raw materials are fully mixed and evenly mixed. During the molding process, it is necessary to control parameters such as temperature, pressure and speed to ensure that the size and shape of the product meet the requirements. If it is necessary to further improve the radiation resistance of fluororubber, radiation resistance treatment is carried out during or after the preparation process. Radiation resistance treatment usually adopts methods such as radiation cross-linking or radiation grafting. The cross-linking or grafting reaction of the fluororubber molecular chain is induced by radiation, thereby improving its radiation resistance.
[0020] A method for preparing high temperature resistant, corrosion resistant and radiation resistant fluororubber for nuclear use comprises the following steps:
[0021] S1: Raw material selection, fluororubber raw rubber, vulcanizing agent, reinforcing agent, filler, stabilizer and antioxidant;
[0022] S2: Formula design: determine the formula of fluororubber according to the use environment and performance requirements. The formula design comprehensively considers factors such as the material's high temperature resistance, corrosion resistance, radiation resistance, and processing performance;
[0023] S3: Mixing: adding raw materials such as fluororubber, vulcanizing agent, reinforcing agent, filler, stabilizer and antioxidant into an internal mixer according to a certain proportion for mixing;
[0024] S4: calendering or extrusion, the mixed fluororubber rubber is molded by a calender or extruder;
[0025] S5: Vulcanization: put the molded fluororubber products into a vulcanization tank and vulcanize them at a certain temperature and pressure;
[0026] S6: Post-processing: Post-processing of the vulcanized fluororubber products, such as deburring, cleaning, drying, etc. During the post-processing process, attention should be paid to protecting the surface quality of the products to avoid scratches and contamination.
Claims
1. A high temperature resistant, corrosion resistant and radiation resistant fluororubber for nuclear use, characterized in that: The fluororubber raw rubber with high fluorine content and excellent performance is selected as the basic material. There are many types of fluororubber raw rubber, such as vinylidene fluoride-hexafluoropropylene copolymer (Viton A), tetrafluoroethylene-propylene copolymer (Viton B), etc. Since nuclear fluororubber needs to be resistant to high temperature and radiation, a peroxide vulcanization system is usually selected. The peroxide vulcanizing agent can induce a cross-linking reaction of the fluororubber at high temperature to form a stable network structure, thereby improving the high temperature resistance and radiation resistance of the rubber.
2. The high temperature resistant, corrosion resistant and radiation resistant fluororubber for nuclear use according to claim 1, characterized in that: In order to improve the physical and mechanical properties and processing properties of fluororubber, it is necessary to add appropriate amounts of reinforcing agents and fillers. Commonly used reinforcing agents include carbon black, white carbon black, etc., and fillers include calcium carbonate, barium sulfate, etc. In order to prevent fluororubber from aging under harsh environments such as high temperature and radiation, it is necessary to add stabilizers and antioxidants. These additives can absorb or neutralize harmful free radicals, thereby extending the service life of fluororubber.
3. The high temperature resistant, corrosion resistant and radiation resistant fluororubber for nuclear use according to claim 1, characterized in that: The types and amounts of vulcanizing agents, reinforcing agents, fillers, stabilizers and antioxidants are determined, and small and medium tests are carried out to verify the rationality and feasibility of the formula.
4. The high temperature resistant, corrosion resistant and radiation resistant fluororubber for nuclear use according to claim 1, characterized in that: The temperature and time need to be controlled during the mixing process to ensure that the raw materials are fully mixed and evenly mixed. The temperature, pressure, speed and other parameters need to be controlled during the molding process to ensure that the size and shape of the product meet the requirements.
5. The high temperature resistant, corrosion resistant and radiation resistant fluororubber for nuclear use according to claim 1, characterized in that: If it is necessary to further improve the radiation resistance of the fluororubber, a radiation resistance treatment is performed during or after the preparation process. The radiation resistance treatment usually adopts methods such as radiation crosslinking or radiation grafting, which induces crosslinking or grafting reactions of the fluororubber molecular chains through radiation, thereby improving its radiation resistance.
6. A method for preparing a high temperature resistant, corrosion resistant and radiation resistant fluororubber for nuclear use according to any one of claims 1 to 5, characterized in that: The following steps are involved: S1: Raw material selection, fluororubber raw rubber, vulcanizing agent, reinforcing agent, filler, stabilizer and antioxidant; S2: Formula design: determine the formula of fluororubber according to the use environment and performance requirements. The formula design comprehensively considers factors such as the material's high temperature resistance, corrosion resistance, radiation resistance, and processing performance; S3: Mixing: adding raw materials such as fluororubber, vulcanizing agent, reinforcing agent, filler, stabilizer and antioxidant into an internal mixer according to a certain proportion for mixing; S4: calendering or extrusion, the mixed fluororubber rubber is molded by a calender or extruder; S5: Vulcanization: put the molded fluororubber products into a vulcanization tank and vulcanize them at a certain temperature and pressure; S6: Post-processing: Post-processing of the vulcanized fluororubber products, such as deburring, cleaning, drying, etc. During the post-processing process, attention should be paid to protecting the surface quality of the products to avoid scratches and contamination.