Display device and method for manufacturing display device
By designing an organic insulating layer, a planarization layer, an inorganic insulating layer and a partition structure in the display device, the problems of water dispersion and organic layer deterioration caused by cracks in the inorganic insulating layer are solved, and the reliability and luminous performance of the display device are improved.
Patent Information
- Application Number
- CN202410695189.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-06-05
- Filing Date
- 2024-05-31
- Publication Date
- 2024-12-06
AI Technical Summary
In the display device, the prior art is difficult to effectively suppress the problem of reduced reliability, especially due to cracks in the inorganic insulating layer and deterioration of the organic layer.
By forming an organic insulating layer, a planarization layer, an inorganic insulating layer and a partition structure on the substrate, the planarization layer contacts the side of the lower electrode to cover the periphery of the lower electrode, and evaporates the organic layer and the upper electrode to be formed by evaporation using the partition wall as a mask. Ensure the flatness of the inorganic insulating layer and the correct shape of the partition wall.
The cracks in the inorganic insulating layer are effectively suppressed, the divergence path of moisture is blocked, the deterioration of the organic layer is prevented, and the reliability and luminous performance of the display device are improved.
Smart Images

Figure CN119095434A_ABST
Abstract
Description
[0001] Cross-references to related applications
[0002] This application claims the priority based on Japanese Patent Application No. 2023-092277 filed on June 5, 2023, and cites all the contents described in the Japanese application. Technical Field
[0003] Embodiments of the present invention relate to a display device and a method for manufacturing the display device. Background Art
[0004] In recent years, display devices using organic light-emitting diodes (OLEDs) as display elements have become practical. The display element includes a pixel circuit including a thin film transistor, a lower electrode connected to the pixel circuit, an organic layer covering the lower electrode, and an upper electrode covering the organic layer. The organic layer includes a light-emitting layer, and functional layers such as a hole transport layer and an electron transport layer.
[0005] In display elements, a technology for suppressing a decrease in reliability is required. Summary of the invention
[0006] An object of the embodiments is to provide a display device and a method for manufacturing the display device that can suppress a decrease in reliability.
[0007] According to one embodiment, a display device includes:
[0008] A substrate; an organic insulating layer, which is arranged above the above-mentioned substrate; a lower electrode, which is arranged on the above-mentioned organic insulating layer; a planarization layer, which is arranged on the above-mentioned organic insulating layer and in contact with the side surface of the above-mentioned lower electrode; an inorganic insulating layer, which covers the above-mentioned planarization layer and covers the peripheral portion of the above-mentioned lower electrode; a partition wall, which has a lower portion and an upper portion, the lower portion is arranged on the above-mentioned inorganic insulating layer and is formed of a conductive material, and the upper portion is arranged on the above-mentioned lower portion and protrudes from the side surface of the above-mentioned lower portion; an organic layer, which is surrounded by the above-mentioned partition wall, arranged on the above-mentioned lower electrode, and includes a light-emitting layer; and an upper electrode, which is surrounded by the above-mentioned partition wall, arranged on the above-mentioned organic layer, and in contact with the above-mentioned lower portion of the above-mentioned partition wall.
[0009] According to one embodiment, a method for manufacturing a display device, wherein:
[0010] An organic insulating layer is formed above a substrate, a lower electrode is formed on the organic insulating layer, a positive photosensitive resin is applied to cover the organic insulating layer and the lower electrode, the photosensitive resin is patterned, a planarization layer in contact with a side surface of the lower electrode is formed, an inorganic insulating layer covering the planarization layer and covering a peripheral portion of the lower electrode is formed, a partition having a lower portion and an upper portion is formed, the lower portion is located above the inorganic insulating layer and is formed of a conductive material, the upper portion is located above the lower portion and protrudes from a side surface of the lower portion, an organic layer located above the lower electrode and including a light-emitting layer is formed by vapor deposition using the partition as a mask, and an upper electrode located above the organic layer and in contact with the lower portion of the partition is formed by vapor deposition using the partition as a mask.
[0011] According to the embodiments, it is possible to provide a display device and a method for manufacturing the display device that can suppress a decrease in reliability. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] Figure 1 This is a diagram showing an example of the configuration of a DSP of a display device.
[0013] Figure 2 It is a diagram showing an example of the layout of sub-pixels SP1 , SP2 , and SP3 .
[0014] Figure 3 It is along Figure 2 A schematic cross-sectional view of the display device DSP taken along line AB in FIG.
[0015] Figure 4 It is a plan view showing an example of the planarization layer 13 .
[0016] Figure 5 It is a diagram for explaining a method of manufacturing the display device DSP.
[0017] Figure 6 It is a diagram for explaining a method of manufacturing the display device DSP.
[0018] Figure 7 It is a diagram for explaining a method of manufacturing the display device DSP.
[0019] Figure 8 It is a diagram for explaining a method of manufacturing the display device DSP.
[0020] Fig. 9 It is a diagram for explaining a method of manufacturing the display device DSP.
[0021] Fig.10 It is a diagram for explaining a method of manufacturing the display device DSP.
[0022] Fig.11It is a diagram for explaining a method of manufacturing the display device DSP.
[0023] Fig.12 It is a diagram for explaining a method of manufacturing the display device DSP.
[0024] Fig.13 It is a diagram for explaining a method of manufacturing the display device DSP.
[0025] Fig.14 It is a diagram for explaining a method of manufacturing the display device DSP.
[0026] Fig.15 This is a diagram for explaining a method of forming the planarization layer 13 .
[0027] Fig.16 This is a diagram for explaining another method of forming the planarization layer 13 .
[0028] Fig.17 This is a diagram for explaining another method of forming the planarization layer 13 .
[0029] Fig.18 It is a diagram showing an example of the cross-sectional shape of the planarizing layer 13 .
[0030] Fig.19 It is a diagram showing another example of the cross-sectional shape of the planarizing layer 13 .
[0031] Fig. 20 It is a diagram for explaining a process of selectively forming the planarization layer 13 in the display area DA. DETAILED DESCRIPTION
[0032] One embodiment will be described with reference to the drawings.
[0033] The disclosed content is only an example, and for those skilled in the art, the content that can be easily thought of with respect to appropriate changes that maintain the gist of the invention is of course included in the scope of the present invention. In addition, in order to make the description clearer, the drawings sometimes schematically show the width, thickness, shape, etc. of each part compared to the actual method, but this is only an example and does not limit the interpretation of the present invention. In addition, in this specification and each figure, the same reference numerals are sometimes used to mark the constituent elements that perform the same or similar functions as the constituent elements described above with respect to the already appeared figures, and repeated detailed descriptions are appropriately omitted.
[0034] It should be noted that, in the accompanying drawings, as needed, for easy understanding, mutually orthogonal X-axis, Y-axis and Z-axis are recorded. The direction along the X-axis is called the first direction X, the direction along the Y-axis is called the second direction Y, and the direction along the Z-axis is called the third direction Z. The situation of observing various elements parallel to the third direction Z is called top view. It should be noted that terms such as top, above, between, and opposite to each other that represent the positional relationship between two or more constituent elements include not only the situation where two or more constituent elements of an object are in direct contact, but also the situation where they are separated from each other by gaps or other constituent elements. In addition, the positive direction of the Z-axis is called top or above.
[0035] The display device involved in this embodiment is an organic electroluminescent display device having an organic light emitting diode (OLED) as a display element, and can be mounted on a television, a personal computer, an in-vehicle device, a tablet terminal, a smartphone, a mobile phone terminal, etc.
[0036] Figure 1 This is a diagram showing an example of the configuration of a DSP of a display device.
[0037] The display device DSP includes a display panel PNL on an insulating substrate 10. The display panel PNL includes a display area DA for displaying an image and a peripheral area SA outside the display area DA. The substrate 10 may be glass or a flexible resin film.
[0038] In the present embodiment, the shape of the substrate 10 in plan view is a rectangle, however, the shape of the substrate 10 in plan view is not limited to a rectangle, and may be other shapes such as a square, a circle, or an ellipse.
[0039] The display area DA includes a plurality of pixels PX arranged in a matrix in a first direction X and a second direction Y. The pixel PX includes a plurality of sub-pixels SP. In one example, the pixel PX includes a sub-pixel SP1 of a first color, a sub-pixel SP2 of a second color, and a sub-pixel SP3 of a third color. The first color, the second color, and the third color are mutually different colors. It should be noted that the pixel PX may also include sub-pixels SP of other colors such as white together with the sub-pixels SP1, SP2, and SP3, or may include sub-pixels SP of other colors such as white instead of any of the sub-pixels SP1, SP2, and SP3. It should be noted that the combination of sub-pixels may be composed of a combination of two elements instead of three elements, or may be composed of four or more elements such as a sub-pixel SP4 in addition to the sub-pixels SP1 to SP3.
[0040] The sub-pixel SP includes a pixel circuit 1 and a display element 20 driven by the pixel circuit 1. The pixel circuit 1 includes a pixel switch 2, a driving transistor 3, and a capacitor 4. The pixel switch 2 and the driving transistor 3 are switching elements composed of, for example, thin film transistors.
[0041] The gate electrode of the pixel switch 2 is connected to the scanning line GL. One of the source electrode and the drain electrode of the pixel switch 2 is connected to the signal line SL, and the other is connected to the gate electrode of the driving transistor 3 and the capacitor 4. In the driving transistor 3, one of the source electrode and the drain electrode is connected to the power line PL and the capacitor 4, and the other is connected to the anode of the display element 20.
[0042] It should be noted that the configuration of the pixel circuit 1 is not limited to the illustrated example. For example, the pixel circuit 1 may include more thin film transistors and capacitors.
[0043] The display element 20 is an organic light emitting diode (OLED) as a light emitting element, sometimes referred to as an organic EL element.
[0044] The peripheral area SA is provided with terminals TE for connecting an IC chip or a flexible printed circuit board.
[0045] Figure 2 It is a diagram showing an example of the layout of sub-pixels SP1 , SP2 , and SP3 .
[0046] exist Figure 2 In the example of FIG. 1 , the sub-pixel SP2 and the sub-pixel SP3 are arranged in the second direction Y. The sub-pixel SP1 and the sub-pixel SP2 are arranged in the first direction X, and the sub-pixel SP1 and the sub-pixel SP3 are arranged in the first direction X.
[0047] When the sub-pixels SP1, SP2, and SP3 are arranged in this way, columns of sub-pixels SP2 and SP3 arranged alternately in the second direction Y and columns of a plurality of sub-pixels SP1 arranged in the second direction Y are formed in the display area DA. These columns are arranged alternately in the first direction X.
[0048] It should be noted that the layout of the sub-pixels SP1, SP2, and SP3 is not limited to Figure 2 As another example, the sub-pixels SP1, SP2, and SP3 in each pixel PX may be arranged in sequence in the first direction X.
[0049] The inorganic insulating layer 5 and the partition 6 are arranged in the display area DA. The inorganic insulating layer 5 has openings AP1, AP2, and AP3 in the sub-pixels SP1, SP2, and SP3, respectively. The inorganic insulating layer 5 having these openings AP1, AP2, and AP3 is sometimes called a rib.
[0050] The partition 6 overlaps with the inorganic insulating layer 5 in a plan view. The partition 6 is formed in a lattice shape surrounding the openings AP1, AP2, and AP3. It can be said that the partition 6 has openings in the sub-pixels SP1, SP2, and SP3 similarly to the inorganic insulating layer 5.
[0051] The sub-pixels SP1 , SP2 , and SP3 include display elements 201 , 202 , and 203 as the display elements 20 , respectively.
[0052] The display element 201 of the sub-pixel SP1 includes a lower electrode LE1, an upper electrode UE1, and an organic layer OR1, which overlap with the opening AP1 respectively. The peripheral portion of the lower electrode LE1 is covered by the inorganic insulating layer 5. The display element 201 including the lower electrode LE1, the organic layer OR1, and the upper electrode UE1 is surrounded by the partition wall 6 when viewed from above. The peripheral portions of the organic layer OR1 and the upper electrode UE1 overlap with the inorganic insulating layer 5 when viewed from above. The organic layer OR1 includes, for example, a light-emitting layer that emits light in a blue wavelength region.
[0053] The display element 202 of the sub-pixel SP2 includes a lower electrode LE2, an upper electrode UE2, and an organic layer OR2, which overlap with the opening AP2 respectively. The peripheral portion of the lower electrode LE2 is covered by the inorganic insulating layer 5. The display element 202 including the lower electrode LE2, the organic layer OR2, and the upper electrode UE2 is surrounded by the partition wall 6 when viewed from above. The peripheral portions of the organic layer OR2 and the upper electrode UE2 overlap with the inorganic insulating layer 5 when viewed from above. The organic layer OR2 includes, for example, a light-emitting layer that emits light in the green wavelength region.
[0054] The display element 203 of the sub-pixel SP3 includes a lower electrode LE3, an upper electrode UE3, and an organic layer OR3, which overlap with the opening AP3 respectively. The peripheral portion of the lower electrode LE3 is covered by the inorganic insulating layer 5. The display element 203 including the lower electrode LE3, the organic layer OR3, and the upper electrode UE3 is surrounded by the partition wall 6 when viewed from above. The peripheral portions of the organic layer OR3 and the upper electrode UE3 overlap with the inorganic insulating layer 5 when viewed from above. The organic layer OR3 includes, for example, a light-emitting layer that emits light in the red wavelength region.
[0055] exist Figure 2 In the example, the outer shapes of the lower electrodes LE1, LE2, LE3 are indicated by dotted lines, and the outer shapes of the organic layers OR1, OR2, OR3 and the upper electrodes UE1, UE2, UE3 are indicated by single-dot chain lines. It should be noted that the outer shapes of the lower electrodes, organic layers, and upper electrodes shown in the figure are not limited to reflecting accurate shapes.
[0056] The lower electrodes LE1, LE2, and LE3 correspond to, for example, anodes of the display element, and the upper electrodes UE1, UE2, and UE3 correspond to cathodes or common electrodes of the display element.
[0057] The lower electrode LE1 is connected to the pixel circuit 1 (refer to Figure 1 The lower electrode LE2 is connected to the pixel circuit 1 of the sub-pixel SP2 through the contact hole CH2. The lower electrode LE is connected to the pixel circuit 1 of the sub-pixel SP3 through the contact hole CH3.
[0058] exist Figure 2 In the example, the area of the opening AP1, the area of the opening AP2, and the area of the opening AP3 are different from each other. The area of the opening AP1 is larger than the area of the opening AP2, and the area of the opening AP2 is larger than the area of the opening AP3. In other words, the area of the lower electrode LE1 exposed from the opening AP1 is larger than the area of the lower electrode LE2 exposed from the opening AP2, and the area of the lower electrode LE2 exposed from the opening AP2 is larger than the area of the lower electrode LE3 exposed from the opening AP3.
[0059] Figure 3 It is along Figure 2 A schematic cross-sectional view of the display device DSP taken along line AB in FIG.
[0060] The circuit layer 11 is disposed on the substrate 10. The circuit layer 11 includes Figure 1 The circuit layer 11 is covered with an insulating layer 12 , which is an organic insulating layer that flattens the unevenness generated in the circuit layer 11 .
[0061] The lower electrodes LE1, LE2, and LE3 are disposed on the insulating layer 12 and are separated from each other. The lower electrodes LE1, LE2, and LE3 are connected to the pixel circuits 1 of the sub-pixels SP1, SP2, and SP3 through contact holes provided in the insulating layer 12. Figure 3 is omitted, but is equivalent to Figure 2 CH1, CH2, CH3.
[0062] The planarization layer 13 is disposed on the insulating layer 12 to expose the upper surfaces of the lower electrodes LE1, LE2, and LE3 and to contact the side surfaces of the lower electrodes LE1, LE2, and LE3. The planarization layer 13 has the same thickness as the lower electrodes LE1, LE2, and LE3. In one example, the thickness of the planarization layer 13 is 50 to 100 nm.
[0063] The inorganic insulating layer 5 covers the planarizing layer 13 and the peripheral edges of the lower electrodes LE1, LE2, and LE3. The opening AP1 of the inorganic insulating layer 5 overlaps with the lower electrode LE1, the opening AP2 overlaps with the lower electrode LE2, and the opening AP3 overlaps with the lower electrode LE3.
[0064] The partition wall 6 has a lower portion (stem) 61 which is arranged on the inorganic insulating layer 5 and has conductivity, and an upper portion (shade) 62 which is arranged on the lower portion 61. The lower portion 61 of the partition wall 6 shown on the right side of the figure is located between the opening AP1 and the opening AP2. The lower portion 61 of the partition wall 6 shown on the left side of the figure is located between the opening AP2 and the opening AP3. The upper portion 62 has a greater width than the lower portion 61. Both ends of the upper portion 62 protrude from the side surfaces of the lower portion 61. Such a shape of the partition wall 6 is called a cantilever.
[0065] The organic layer OR1 contacts the lower electrode LE1 through the opening AP1 , covers the lower electrode LE1 exposed from the opening AP1 , and has its peripheral portion located on the inorganic insulating layer 5 . The upper electrode UE1 covers the organic layer OR1 and contacts the lower portion 61 .
[0066] The organic layer OR2 contacts the lower electrode LE2 through the opening AP2 , covers the lower electrode LE2 exposed from the opening AP2 , and its peripheral portion is located on the inorganic insulating layer 5 . The upper electrode UE2 covers the organic layer OR2 and contacts the lower portion 61 .
[0067] The organic layer OR3 contacts the lower electrode LE3 through the opening AP3 , covers the lower electrode LE3 exposed from the opening AP3 , and its peripheral portion is located on the inorganic insulating layer 5 . The upper electrode UE3 covers the organic layer OR3 and contacts the lower portion 61 .
[0068] exist Figure 3 In the example, sub-pixel SP1 has cap layer CP1 and sealing layer SE1, sub-pixel SP2 has cap layer CP2 and sealing layer SE2, and sub-pixel SP3 has cap layer CP3 and sealing layer SE3. Cap layers CP1, CP2, and CP3 respectively function as optical adjustment layers for improving the extraction efficiency of light emitted from organic layers OR1, OR2, and OR3.
[0069] The cap layer CP1 is disposed on the upper electrode UE1 .
[0070] The cap layer CP2 is disposed on the upper electrode UE2.
[0071] The cap layer CP3 is disposed on the upper electrode UE3. It should be noted that the cap layers CP1, CP2, and CP3 may be omitted.
[0072] The sealing layer SE1 is disposed on the cap layer CP1 , in contact with the partition wall 6 , and continuously covers each member of the sub-pixel SP1 .
[0073] The sealing layer SE2 is disposed on the cap layer CP2 , in contact with the partition wall 6 , and continuously covers each member of the sub-pixel SP2 .
[0074] The sealing layer SE3 is disposed on the cap layer CP3 , in contact with the partition wall 6 , and continuously covers the components of the sub-pixel SP3 .
[0075] exist Figure 3 In the example, a portion of each of the organic layer OR1, the upper electrode UE1 and the cover layer CP1 is located on the partition wall 6 around the sub-pixel SP1. These portions are separated from the portions of the organic layer OR1, the upper electrode UE1 and the cover layer CP1 located at the opening AP1 (the portions constituting the display element 201).
[0076] Similarly, portions of the organic layer OR2, the upper electrode UE2 and the cover layer CP2 are each located on the partition wall 6 around the subpixel SP2, and these portions are separated from portions of the organic layer OR2, the upper electrode UE2 and the cover layer CP2 located in the opening AP2 (portions constituting the display element 202).
[0077] Similarly, portions of the organic layer OR3, the upper electrode UE3 and the cover layer CP3 are respectively located on the partition wall 6 around the sub-pixel SP3, and these portions are separated from portions of the organic layer OR3, the upper electrode UE3 and the cover layer CP3 located in the opening AP3 (portions constituting the display element 203).
[0078] The ends of the sealing layers SE1, SE2, and SE3 are located on the partition walls 6. Figure 3 In the example, the ends of the sealing layers SE1 and SE2 located on the partition wall 6 between the sub-pixels SP1 and SP2 are separated from each other, and the ends of the sealing layers SE2 and SE3 located on the partition wall 6 between the sub-pixels SP2 and SP3 are separated from each other.
[0079] The sealing layers SE1, SE2, and SE3 are covered with the resin layer RL1. The resin layer RL1 is covered with the sealing layer 14. The sealing layer 14 is covered with the resin layer RL2.
[0080] The inorganic insulating layer 5 , the sealing layers SE1 , SE2 , SE3 , and the sealing layer 14 are formed of an inorganic insulating material such as silicon nitride (SiNx), silicon oxide (SiOx), silicon oxynitride (SiON), or aluminum oxide (Al 2 O 3 ).
[0081] The insulating layer 12 is formed of a resin. The planarizing layer 13 is formed of a positive photosensitive resin. The planarizing layer 13 may be formed of a material different from that of the insulating layer 12 or may be formed of the same material as that of the insulating layer 12 .
[0082] The lower portion 61 of the partition wall 6 is formed of a conductive material and is electrically connected to the upper electrodes UE1, UE2, and UE3. The upper portion 62 of the partition wall 6 is formed of a conductive material, for example, but may also be formed of an insulating material. The lower portion 61 is formed of a material different from that of the upper portion 62.
[0083] The lower electrodes LE1 , LE2 , and LE3 are multilayer bodies including, for example, a transparent electrode formed of an oxide conductive material such as indium tin oxide (ITO) and a metal electrode (reflective electrode) formed of a metal material such as silver.
[0084] The organic layer OR1 includes a light-emitting layer EM1. The organic layer OR2 includes a light-emitting layer EM2. The organic layer OR3 includes a light-emitting layer EM3. The light-emitting layer EM1, the light-emitting layer EM2, and the light-emitting layer EM3 are formed of different materials. In one example, the light-emitting layer EM1 is formed of a material that emits light in a blue wavelength region, the light-emitting layer EM2 is formed of a material that emits light in a green wavelength region, and the light-emitting layer EM3 is formed of a material that emits light in a red wavelength region.
[0085] In addition, each of the organic layers OR1, OR2, and OR3 includes a plurality of functional layers such as a hole injection layer, a hole transport layer, an electron blocking layer, a hole blocking layer, an electron transport layer, and an electron injection layer.
[0086] The upper electrodes UE1 , UE2 , and UE3 are formed of a metal material such as an alloy of magnesium and silver (MgAg).
[0087] The cap layers CP1, CP2, and CP3 are multilayer bodies of multiple thin films. The multiple thin films are all transparent and have different refractive indices. It should be noted that at least one of the cap layers CP1, CP2, and CP3 can be omitted.
[0088] Figure 4 It is a plan view showing an example of the planarization layer 13 .
[0089] The planarization layer 13 is formed in a lattice shape when viewed from above. The lower electrodes LE1, LE2, and LE3 are each surrounded by the planarization layer 13. That is, the side surface of the lower electrode LE1 is in contact with the planarization layer 13 throughout the entire circumference. Similarly, the side surface of the lower electrode LE2 is in contact with the planarization layer 13 throughout the entire circumference, and the side surface of the lower electrode LE3 is also in contact with the planarization layer 13 throughout the entire circumference. Thus, the step difference between the adjacent lower electrodes LE1, LE2, and LE3 is mitigated by the planarization layer 13.
[0090] Thus, the planarization layer 13 mitigates the step difference between the lower electrodes LE1, LE2, LE3, and the upper surface of the inorganic insulating layer 5 overlapping the planarization layer 13 and the lower electrodes LE1, LE2, LE3 is planarized. Thus, the generation of cracks in the inorganic insulating layer 5 caused by the step difference between the lower electrodes LE1, LE2, LE3 is suppressed.
[0091] The cracks in the inorganic insulating layer 5 may become a diffusion path for the moisture contained in the insulating layer 12. Therefore, when the cracks penetrate the inorganic insulating layer 5, there is a risk that the moisture contained in the insulating layer 12 is transferred to the end of the lower electrode LE and penetrates the cracks. In this case, the organic layer OR located on the inorganic insulating layer 5 is damaged by the moisture that has penetrated the cracks, resulting in a decrease in the light emitting performance.
[0092] As described above, according to this embodiment, the generation of cracks in the inorganic insulating layer 5 is suppressed, and thus the diffusion path of the moisture contained in the insulating layer 12 is blocked. This suppresses the degradation of the organic layer OR located on the inorganic insulating layer 5 due to moisture. Therefore, the reduction in reliability can be suppressed.
[0093] Furthermore, since the surface of the inorganic insulating layer 5 serving as the base of the partition 6 is flattened, the partition 6 can be formed in a desired shape.
[0094] Furthermore, assuming that cracks are generated in the inorganic insulating layer 5 , the area contributing to the display of each sub-pixel can be increased compared to the case where the width of the lower portion 61 of the partition 6 is increased so as to cover the cracks.
[0095] Furthermore, assuming that cracks occur in the inorganic insulating layer 5 , electrical insulation between adjacent lower electrodes LE can be ensured compared to a case where adjacent lower electrodes LE are arranged close to each other and the end of each lower electrode LE is located directly below the lower portion 61 .
[0096] In addition, the planarization layer 13 formed of resin is covered by the inorganic insulating layer 5 and is not exposed from the inorganic insulating layer 5. Therefore, contact between the organic layer OR and the planarization layer 13 is avoided. Thus, degradation of the organic layer OR due to moisture contained in the planarization layer 13 can be suppressed.
[0097] Next, refer to Figures 5 to 14 The manufacturing method of the display device DSP is described. Figures 5 to 14 In the figure, the lower part of the insulating layer 12 is omitted.
[0098] First, if Figure 5 As shown, the substrate SUB is prepared for processing. The process of preparing the substrate SUB includes: a process of forming an insulating layer 12; and a process of forming the lower electrode LE1 of the sub-pixel SP1, the lower electrode LE2 of the sub-pixel SP2, and the lower electrode LE3 of the sub-pixel SP3 on the insulating layer 12. The process of forming the lower electrodes LE1, LE2, and LE3 includes: a process of forming a transparent conductive layer; a process of forming a metal layer; and a process of patterning these conductive layers and the metal layer together.
[0099] Next, if Figure 6As shown, a planarization layer 13 is formed on the insulating layer 12. The process of forming the planarization layer 13 will be described in detail later, and includes: applying a photosensitive resin covering the insulating layer 12 and the lower electrodes LE1, LE2, LE3; and patterning the photosensitive resin.
[0100] Next, if Figure 7 As shown, an inorganic insulating layer 5 is formed to cover the lower electrodes LE1, LE2, LE3 and the planarization layer 13. In one example, silicon oxynitride is deposited on the entire display area DA by CVD (Chemical-Vapor Deposition).
[0101] Next, if Figure 8 As shown, a partition wall 6 is formed on the inorganic insulating layer 5. The process of forming the partition wall 6 includes: a process of forming a metal layer on the inorganic insulating layer 5; a process of forming a thin film on the metal layer; a process of forming a resist corresponding to the shape of the partition wall 6 on the thin film; a process of etching the thin film and the metal layer in sequence using the resist as a mask; and a process of removing the resist. By patterning the metal layer, a lower portion 61 located on the inorganic insulating layer 5 is formed. In addition, by patterning the thin film, an upper portion 62 located on the lower portion 61 and protruding from the side of the lower portion 61 is formed.
[0102] Next, if Fig. 9 As shown, openings AP1, AP2, and AP3 are formed in the inorganic insulating layer 5. The opening AP1 overlaps with the lower electrode LE1, the opening AP2 overlaps with the lower electrode LE2, and the opening AP3 overlaps with the lower electrode LE3. The inorganic insulating layer 5 formed in this way covers the planarization layer 13 and covers the peripheral portions of the lower electrodes LE1, LE2, and LE3.
[0103] It should be noted that in the above example, the openings AP1 , AP2 , and AP3 are formed after the partition 6 is formed. However, the present invention is not limited to this example, and the partition 6 may be formed after the inorganic insulating layer 5 having the openings AP1 , AP2 , and AP3 is formed.
[0104] Next, the display element 201 is formed.
[0105] First, if Fig.10 As shown, using the partition wall 6 as a mask, materials for forming the hole injection layer, hole transport layer, electron blocking layer, light-emitting layer (EM1), hole blocking layer, electron transport layer, electron injection layer and other layers are sequentially evaporated on the lower electrode LE1 to form an organic layer OR1.
[0106] Then, a mixture of magnesium and silver is deposited on the organic layer OR1 using the partition wall 6 as a mask to form an upper electrode UE1 . The upper electrode UE1 covers the organic layer OR1 and is in contact with the lower portion 61 .
[0107] Then, using the partition wall 6 as a mask, a high refractive index material for forming the first transparent layer TL1 and a low refractive index material for forming the second transparent layer TL2 are sequentially deposited on the upper electrode UE1 to form a cap layer CP1.
[0108] The organic layer OR1 , the upper electrode UE1 , and the cap layer CP1 are continuously formed while maintaining a vacuum environment.
[0109] Then, the sealing layer SE1 is formed by the CVD method so as to continuously cover the cap layer CP1 and the partition wall 6 .
[0110] The organic layer OR1 , the upper electrode UE1 , the cap layer CP1 and the sealing layer SE1 are formed at least in the entire display area DA and are arranged not only in the sub-pixel SP1 but also in the sub-pixels SP2 and SP3 .
[0111] When the organic layer OR1, the upper electrode UE1, and the cap layer CP1 are formed by evaporation, the material released from the evaporation source is blocked by the upper portion 62. Therefore, a portion of the organic layer OR1, the upper electrode UE1, and the cap layer CP1 is stacked on the upper portion 62. The organic layer OR1, the upper electrode UE1, and the cap layer CP1 located on the upper portion 62 are separated from the organic layer OR1, the upper electrode UE1, and the cap layer CP1 located directly above the lower electrode LE1.
[0112] The sealing layer SE1 covers the cap layer CP1 just above the bank 6 and covers the cap layer CP1 just above the lower electrode LE1 , and is in contact with the bank 6 .
[0113] Next, if Fig.11 As shown in FIG. 1 , a resist RS patterned into a predetermined shape is formed on the sealing layer SE1 . The resist RS overlaps the sub-pixel SP1 and a part of the partition wall 6 around it.
[0114] Next, if Fig.12 As shown, the sealing layer SE1, the cap layer CP1, the upper electrode UE1, and the organic layer OR1 exposed from the resist RS are sequentially removed by etching using the resist RS as a mask, thereby exposing the lower electrode LE2 of the sub-pixel SP2 and the lower electrode LE3 of the sub-pixel SP3.
[0115] Then, the resist RS is removed. Thus, the display element 201 is formed in the sub-pixel SP1.
[0116] Next, if Fig.13 As shown, the display element 202 is formed. The steps of forming the display element 202 are the same as the steps of forming the display element 201. That is, an organic layer OR2 including a light-emitting layer EM2, an upper electrode UE2, a cover layer CP2, and a sealing layer SE2 are sequentially formed on the lower electrode LE2. Then, a resist is formed on the sealing layer SE2, and the sealing layer SE2, the cover layer CP2, the upper electrode UE2, and the organic layer OR2 are patterned in sequence by etching using the resist as a mask. After the patterning, the resist is removed. Thus, the display element 202 is formed in the sub-pixel SP2, and the lower electrode LE3 of the sub-pixel SP3 is exposed.
[0117] Next, if Fig.14 As shown, the display element 203 is formed. The steps of forming the display element 203 are the same as the steps of forming the display element 201. That is, an organic layer OR3 including a light-emitting layer EM3, an upper electrode UE3, a cap layer CP3, and a sealing layer SE3 are sequentially formed on the lower electrode LE3. Then, a resist is formed on the sealing layer SE3, and the sealing layer SE3, the cap layer CP3, the upper electrode UE3, and the organic layer OR3 are patterned in sequence by etching using the resist as a mask. After the patterning, the resist is removed. Thus, the display element 203 is formed in the sub-pixel SP3.
[0118] Then, form Figure 3 The resin layer RL1, the sealing layer 14 and the resin layer RL2 are shown. Thus, the display device DSP is completed.
[0119] It should be noted that in the above manufacturing process, it is assumed that the display element 201 is formed first, the display element 202 is formed next, and the display element 203 is formed last, but the formation order of the display elements 201, 202, and 203 is not limited to this example.
[0120] Next, a method for forming the planarization layer 13 will be described.
[0121] Fig.15 This is a diagram for explaining a method of forming the planarization layer 13 .
[0122] First, as shown in the upper section, a positive photosensitive resin PR is applied to cover the insulating layer 12 and the plurality of lower electrodes LE. The plurality of lower electrodes LE here correspond to Figure 3 Any of the lower electrodes LE1, LE2, and LE3 shown. The lower electrodes LE are respectively a multilayer body of the first layer L1, the second layer L2, and the third layer L3. The first layer L1 and the third layer L3 are both transparent electrodes. The second layer L2 is a metal electrode such as silver. That is, each of the lower electrodes LE has a metal electrode that can serve as a reflective electrode between a pair of transparent electrodes.
[0123] Next, as shown in the middle section, the entire surface of the photosensitive resin PR is exposed without using a mask. The area of the photosensitive resin PR that overlaps with the lower electrode LE is exposed to light irradiated from the light source of the exposure device, and is also exposed to light reflected by the second layer L2 of the lower electrode LE. The area of the photosensitive resin PR that does not overlap with the lower electrode LE (or the area that overlaps with the adjacent lower electrodes LE) is exposed to light irradiated from the light source. Therefore, the exposure amount of the area overlapping with the lower electrode LE is greater than the exposure amount of the area that does not overlap with the lower electrode LE. Through the above steps, the surface layer of the photosensitive resin PR is exposed and becomes soluble in the developer.
[0124] Next, as shown in the lower section, the photosensitive resin PR is developed. By developing the photosensitive resin PR, the surface layer of the photosensitive resin PR is removed, the upper surface of the lower electrode LE is exposed, and the photosensitive resin PR remains between the lower electrodes LE.
[0125] Then, the photosensitive resin PR is fired to remove moisture from the photosensitive resin PR, thereby forming the planarization layer 13 .
[0126] Fig.16 FIG. 1 is a diagram for explaining another method of forming the planarization layer 13. Fig.15 The description content is repeated.
[0127] First, a positive type photosensitive resin PR is applied to cover the insulating layer 12 and the plurality of lower electrodes LE.
[0128] Next, the photosensitive resin PR is exposed using a mask M1. The mask M1 has an opening OP and a low transmittance portion LT having a transmittance lower than that of the opening OP. The opening OP has a shape corresponding to the lower electrode LE. The low transmittance portion LT has a shape corresponding to the area where the planarization layer 13 is to be formed (the area that does not overlap with the lower electrode LE). It should be noted that the low transmittance portion LT has a width larger than the interval between adjacent lower electrodes LE and overlaps with the end of the lower electrode LE. When the photosensitive resin PR is exposed through such a mask M1, such an exposure condition is achieved: the exposure amount of the area overlapping with the lower electrode LE is larger than the exposure amount of the area not overlapping with the lower electrode LE.
[0129] The region of the photosensitive resin PR overlapping with the lower electrode LE is exposed to light transmitted through the opening OP, and is also exposed to light reflected by the second layer L2 of the lower electrode LE. The region of the photosensitive resin PR not overlapping with the lower electrode LE is exposed to light transmitted through the low transmittance portion LT, and is also exposed to diffuse light reflected by the second layer L2 of the lower electrode LE. Therefore, the surface layer of the photosensitive resin PR is exposed and becomes soluble in the developer.
[0130] Next, after the photosensitive resin PR is developed, the photosensitive resin PR is fired, thereby forming the planarization layer 13 .
[0131] Fig.17 FIG. 1 is a diagram for explaining another method of forming the planarization layer 13. Fig.15 The description content is repeated.
[0132] First, a positive type photosensitive resin PR is applied to cover the insulating layer 12 and the plurality of lower electrodes LE.
[0133] Next, the entire surface of the photosensitive resin PR is exposed without using a mask.
[0134] Next, the photosensitive resin PR is exposed using a mask M2. The mask M2 has an opening OP and a light shielding portion LS. The opening OP has a shape corresponding to the lower electrode LE. The light shielding portion LS has a shape corresponding to the area where the planarization layer 13 is to be formed (the area that does not overlap with the lower electrode LE). It should be noted that the light shielding portion LS has a width greater than the interval between adjacent lower electrodes LE and overlaps with the end of the lower electrode LE.
[0135] The region of the photosensitive resin PR that overlaps with the lower electrode LE is exposed in the previous whole-surface exposure process, and is exposed to light that passes through the opening OP in the exposure process through the mask M2. The region of the photosensitive resin PR that does not overlap with the lower electrode LE is exposed in the previous whole-surface exposure process, and on the other hand, is shielded by the light shielding portion LS in the exposure process through the mask M2. By forming such a difference in exposure amount, the photosensitive resin PR in the region that overlaps with the lower electrode LE is exposed in a manner that can be reliably removed, and the photosensitive resin PR in the region that does not overlap with the lower electrode LE is exposed in a manner that can remove the surface layer and leave a residue at the bottom.
[0136] Next, after the photosensitive resin PR is developed, the photosensitive resin PR is fired, thereby forming the planarization layer 13 .
[0137] Next, a cross-sectional shape that can form the planarizing layer 13 will be described.
[0138] Fig.18 It is a diagram showing an example of the cross-sectional shape of the planarizing layer 13 .
[0139] The upper surface US13 of the planarization layer 13 protrudes from the upper surface US1 of the lower electrode LE1 and the upper surface US2 of the lower electrode LE2. In the example shown in the figure, the entire upper surface US13 protrudes from the upper surface US1 and the like to form a convex surface. It is also possible that a portion of the upper surface US13 protrudes from the upper surface US1 and the like. It should be noted that in Fig.18 Although the lower electrode LE3 is not shown, at least a portion of the upper surface US13 protrudes from each upper surface of the lower electrodes LE1, LE2, and L3. In one example, the thickness of the planarization layer 13 is the largest at the midpoint that is substantially equidistant from the adjacent lower electrodes LE.
[0140] Fig.19 It is a diagram showing another example of the cross-sectional shape of the planarizing layer 13 .
[0141] The upper surface US13 of the planarization layer 13 is recessed than the upper surface US1 of the lower electrode LE1 and the upper surface US2 of the lower electrode LE2. In the example shown in the figure, the entire upper surface US13 is recessed than the upper surface US1, etc., forming a concave surface. It is also possible that a portion of the upper surface US13 is recessed than the upper surface US1, etc. Fig.19 Although the lower electrode LE3 is not shown, at least a portion of the upper surface US13 is recessed relative to the upper surfaces of the lower electrodes LE1, LE2, and L3. In one example, the thickness of the planarization layer 13 is smallest at the midpoints that are approximately equidistant from the adjacent lower electrodes LE.
[0142] Fig. 20 It is a diagram for explaining a process of selectively forming the planarization layer 13 in the display area DA.
[0143] First, as shown in the upper stage, a positive type photosensitive resin PR is applied to cover the insulating layer 12 and the plurality of lower electrodes LE. At this time, the photosensitive resin PR is applied not only to the display area DA but also to the peripheral area SA.
[0144] Next, as shown in the middle section, the photosensitive resin PR is exposed using a mask M1. The mask M1 has an opening OP and a low transmittance portion LT having a transmittance lower than that of the opening OP. The opening OP has a shape corresponding to the lower electrode LE and has a shape corresponding to the peripheral area SA. The low transmittance portion LT has a shape corresponding to the area where the planarization layer 13 is to be formed (the area that does not overlap with the lower electrode LE). When the photosensitive resin PR is exposed through such a mask M1, such an exposure condition is achieved: the exposure amount of the area overlapping with the lower electrode LE and the peripheral area SA is large compared to the exposure amount of the area that does not overlap with the lower electrode LE in the display area DA.
[0145] The region of the photosensitive resin PR that overlaps with the lower electrode LE and the peripheral region SA are exposed to light that has passed through the opening OP. The region of the photosensitive resin PR that does not overlap with the lower electrode LE of the display region DA is exposed to light that has passed through the low transmittance portion LT. Therefore, the surface layer of the photosensitive resin PR in the display region DA is exposed, and the entire photosensitive resin PR in the peripheral region SA is exposed. The exposed region of the photosensitive resin PR becomes soluble in the developer.
[0146] Next, as shown in the next section, after the photosensitive resin PR is developed, the photosensitive resin PR is fired. Thus, the planarization layer 13 is formed. In addition, in the peripheral area SA, the photosensitive resin PR is removed. Thus, in the peripheral area SA, Figure 1 The terminals TE and the like shown are exposed from the planarization layer 13 .
[0147] exist Fig. 20 In the use Fig.16 The case where the photosensitive resin PR in the peripheral area SA is removed by using the mask M1 shown in the figure is described, but it is also possible to use Fig.17 The mask M2 shown removes the photosensitive resin PR in the peripheral area SA. Fig.15 In the entire surface exposure step shown, the photosensitive resin PR in the peripheral area SA can also be removed.
[0148] As described above, according to the present embodiment, it is possible to provide a display device and a method for manufacturing a display device that can suppress a decrease in reliability.
[0149] Based on the display device and the manufacturing method thereof described above as the embodiments of the present invention, any display device and the manufacturing method thereof that can be implemented by appropriately designing and modifying by a person skilled in the art also belongs to the scope of the present invention as long as it includes the gist of the present invention.
[0150] Within the scope of the present invention, those skilled in the art can think of various variations, which also belong to the scope of the present invention. For example, embodiments obtained by adding, deleting or designing the above-mentioned embodiments appropriately by those skilled in the art, or embodiments obtained by adding, omitting or changing the conditions of the processes are included in the scope of the present invention as long as they have the gist of the present invention.
[0151] In addition, regarding other effects brought about by the methods described in the above-mentioned embodiments, regarding the effects that are clear based on the records in this specification, or the effects that can be appropriately thought of by those skilled in the art, it is of course understood that they are the effects brought about by the present invention.
Claims
1. A display device comprising: substrate; an organic insulating layer, disposed above the substrate; A lower electrode, which is disposed on the organic insulating layer; a planarization layer, which is disposed on the organic insulating layer and contacts the side surface of the lower electrode; an inorganic insulating layer covering the planarization layer and covering a peripheral portion of the lower electrode; a partition wall having a lower portion and an upper portion, wherein the lower portion is disposed on the inorganic insulating layer and is formed of a conductive material, and the upper portion is disposed on the lower portion and protrudes from a side surface of the lower portion; an organic layer surrounded by the partition wall, disposed on the lower electrode, and including a light-emitting layer; and An upper electrode is surrounded by the partition wall, disposed on the organic layer, and in contact with the lower portion of the partition wall.
2. The display device according to claim 1, wherein: The planarization layer is formed in a lattice shape in a plan view.
3. The display device according to claim 1, wherein: At least a portion of an upper surface of the planarization layer protrudes further than an upper surface of the lower electrode.
4. The display device according to claim 1, wherein: At least a portion of an upper surface of the planarization layer is recessed relative to an upper surface of the lower electrode.
5. The display device according to claim 1, wherein: The planarization layer is formed of a positive photosensitive resin.
6. The display device according to claim 1, further comprising: a capping layer disposed on the upper electrode; and a sealing layer, which is disposed on the cover layer and is formed of an inorganic insulating material, in, The sealing layer covers the cap layer directly above the lower electrode and is in contact with the partition wall.
7. A method for manufacturing a display device, wherein: forming an organic insulating layer on the substrate, forming a lower electrode on the organic insulating layer, coating a positive photosensitive resin covering the organic insulating layer and the lower electrode, patterning the photosensitive resin to form a planarization layer in contact with the side surface of the lower electrode, forming an inorganic insulating layer covering the planarization layer and covering the peripheral portion of the lower electrode, forming a partition wall having a lower portion and an upper portion, the lower portion being located on the inorganic insulating layer and formed of a conductive material, and the upper portion being located on the lower portion and protruding from a side surface of the lower portion, By vapor deposition using the partition wall as a mask, an organic layer including a light-emitting layer is formed on the lower electrode. An upper electrode located on the organic layer and in contact with the lower portion of the partition wall is formed by vapor deposition using the partition wall as a mask.
8. The method for manufacturing a display device according to claim 7, wherein: The process of patterning the photosensitive resin includes: The entire surface of the photosensitive resin is exposed without using a mask, developing the photosensitive resin, The photosensitive resin is fired.
9. The method for manufacturing a display device according to claim 7, wherein: The process of patterning the photosensitive resin includes: exposing the photosensitive resin under an exposure condition in which the exposure amount of the region overlapping with the lower electrode is greater than the exposure amount of the region not overlapping with the lower electrode, developing the photosensitive resin, The photosensitive resin is fired.
10. The method for manufacturing a display device according to claim 7, wherein: The process of patterning the photosensitive resin includes: The entire surface of the photosensitive resin is exposed without using a mask, The photosensitive resin is exposed using a mask, wherein the mask has an opening in a region overlapping with the lower electrode and shields a region not overlapping with the lower electrode from light, developing the photosensitive resin, The photosensitive resin is fired.
11. The method for manufacturing a display device according to claim 7, wherein: Further, after forming the upper electrode, forming a cap layer on the upper electrode, On the cover layer, a sealing layer is formed using an inorganic insulating material. The sealing layer covers the cap layer directly above the lower electrode and is in contact with the partition wall.
12. The method for manufacturing a display device according to claim 11, wherein: Further, after forming the sealing layer, forming a patterned resist over the sealing layer, The sealing layer, the cap layer, the upper electrode, and the organic layer exposed from the resist are sequentially removed by etching.
Citation Information
Patent Citations
Oval cavity washing device, oral cavity washing method, and oral cavity washing program