Lubricating oil composition
By adding phosphites of specific structures to the lubricating oil and controlling the content of thiadiazole and benzotriazole, the problem of insufficient glue resistance and copper corrosion resistance of lubricating oil in the electric drive unit is solved, and efficient lubrication is achieved Performance and stability.
Patent Information
- Application Number
- CN202380039787.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-05-16
- Filing Date
- 2023-05-12
- Publication Date
- 2024-12-06
AI Technical Summary
The lubricating oil composition used in the existing electric drive units has shortcomings in terms of glue resistance and copper corrosion resistance, and it is difficult to meet the stability requirements for long-term use.
By adding phosphites with specific structures to the lubricating oil composition and limiting the content of thiadiazole and benzotriazole, the kinematic viscosity of the lubricating oil reaches 4.2mm2/s at 100°C, thereby improving the lubricating oil Gluing resistance and copper corrosion resistance.
It realizes a lubricating oil composition that maintains excellent copper corrosion resistance and glue resistance during long-term use, and is suitable for lubrication of electric drive units such as gear boxes and motors, and improves the stability and wear resistance of the device.
Smart Images

Figure SMS_1 
Figure SMS_2 
Figure SMS_3
Abstract
Description
Technical Field
[0001] The present invention relates to a lubricating oil composition, an electric drive unit, use of the lubricating oil composition and a method for producing the lubricating oil composition. Background Art
[0002] Various devices such as engines, transmissions, speed reducers, compressors, and hydraulic devices have mechanisms such as torque converters, clutches, gear bearing mechanisms, oil pumps, and hydraulic control mechanisms. Lubricating oil compositions are used in these mechanisms, and lubricating oil compositions that can meet various requirements have been developed.
[0003] For example, Patent Document 1 discloses a transmission lubricating oil composition for the purpose of providing a transmission lubricating oil composition capable of improving high temperature stability and shear stability and suppressing a decrease in low temperature fluidity accompanying long-term use. The composition is characterized in that the composition contains a predetermined base oil and a predetermined amount of poly(meth)acrylate and satisfies predetermined parameters.
[0004] In recent years, the development of electric drive units including electric motors, gearboxes, and inverters has been advancing, and lubricating oil compositions suitable for the electric drive units are required. For example, Patent Document 2 discloses a lubricating oil composition suitable for electric drive units, which contains a predetermined phosphite and a thiadiazole derivative, for the purpose of providing a lubricating oil composition having high extreme pressure properties, high durability and wear resistance, and high volume ratio inefficiency.
[0005] Prior art literature
[0006] Patent Literature
[0007] Patent Document 1: International Publication No. 2020 / 213644
[0008] Patent Document 2: International Publication No. 2021 / 193869 Summary of the invention
[0009] Problems to be solved by the invention
[0010] The lubricating oil composition used in the electric drive unit is required to have properties such as scuffing resistance, copper corrosion resistance, etc. That is, a new lubricating oil composition having properties suitable for lubrication of various mechanisms assembled in the device (such as scuffing resistance, copper corrosion resistance, etc.) is required.
[0011] Means for solving problems
[0012] The present inventors have found that by setting the kinematic viscosity of a lubricating oil composition to a predetermined range and containing a predetermined phosphite, it is possible to provide a lubricating oil composition that does not reduce the anti-seizing property even without using a thiadiazole compound and exhibits excellent copper corrosion resistance in a copper corrosion resistance test for a long period of time (for example, 168 hours in the examples described below). The present invention has been completed based on the above findings.
[0013] That is, the present invention provides the following embodiments [1] to [9].
[0014] [1] A lubricating oil composition comprising a base oil (A) and a phosphite (B), wherein the phosphite (B) has at least one sulfur-containing group having 2 to 20 carbon atoms and having at least one -(S)x- group (x is an integer of 1 or more) between two adjacent carbon atoms in the alkyl group structure;
[0015] The content of the thiadiazole compound is less than 0.05% by mass based on the total amount of the lubricating oil composition.
[0016] The kinematic viscosity of the lubricating oil composition at 100°C is 4.2 mm 2 / s or more.
[0017] [2] The lubricating oil composition according to [1], wherein the phosphite compound (B) comprises at least one selected from the group consisting of a compound (B1) represented by the following general formula (b-1) and a compound (B2) represented by the following general formula (b-2).
[0018]
Chemical formula 1
[0019]
[0020] (Where R B11 , R B21 and R B22 Each independently represents an alkyl group having 1 to 19 carbon atoms, and bB11, bB21 and bB22 each independently represent an integer of 1 to 10.
[0021] [3] The lubricating oil composition according to [1] or [2], wherein the content of the benzotriazole compound is less than 0.05% by mass based on the total amount of the lubricating oil composition.
[0022] [4] The lubricating oil composition according to any one of [1] to [3], wherein the content of the phosphite compound (B) is 0.15 mass % or more and less than 1.00 mass % based on the total amount of the lubricating oil composition.
[0023] [5] The lubricating oil composition according to any one of [1] to [4], wherein the base oil (A) is at least one selected from the group consisting of mineral oil, poly-α-olefin, isoparaffin, polyalkylene glycol, ester synthetic oil, ether synthetic oil, alkylbenzene synthetic oil, alkylnaphthalene synthetic oil, GTL, CTL and BTL.
[0024] [6] The lubricating oil composition according to any one of [1] to [5], which is used for lubricating an electric drive unit including at least a gear box and a motor.
[0025] [7] An electric drive unit filled with the lubricating oil composition described in any one of [1] to [5], the electric drive unit comprising at least a gear box and a motor.
[0026] [8] Use of a lubricating oil composition, wherein the lubricating oil composition according to any one of [1] to [5] is used for lubricating an electric drive unit including at least a gear box and a motor.
[0027] [9] A method for producing a lubricating oil composition, which is a method for producing the lubricating oil composition according to any one of [1] to [5], wherein the lubricating oil composition is prepared by blending a phosphite compound (B) into a base oil (A) so that the content of the thiadiazole compound is less than 0.05% by mass based on the total amount of the lubricating oil composition and the kinematic viscosity of the lubricating oil composition at 100° C. is 4.2 mm 2 / s or more,
[0028] The phosphite compound (B) has at least one group having 2 to 19 carbon atoms, wherein the group having 2 to 19 carbon atoms is obtained by replacing one -CH2- group bonded to carbon atoms at both ends of an alkyl group having 3 to 20 carbon atoms with a -S- group.
[0029] Effects of the Invention
[0030] A lubricating oil composition according to a preferred embodiment of the present invention is a lubricating oil composition having properties suitable for lubricating various mechanisms incorporated in a device, and a more specific lubricating oil composition according to a preferred embodiment of the present invention can improve the anti-seizing property and the copper corrosion resistance in a well-balanced manner. Therefore, these lubricating oil compositions can be suitably used for lubrication of an electric drive unit including at least a gear box and a motor, for example. DETAILED DESCRIPTION
[0031] Regarding the numerical range described in this specification, the upper limit and the lower limit can be arbitrarily combined. For example, when the numerical range is described as "preferably 30 to 100, more preferably 40 to 80", the range of "30 to 80" and the range of "40 to 100" are also included in the numerical range described in this specification. In addition, for example, when the numerical range is described as "preferably 30 or more, more preferably 40 or more, and preferably 100 or less, more preferably 80 or less", the range of "30 to 80" and the range of "40 to 100" are also included in the numerical range described in this specification.
[0032] In addition, as a numerical range described in this specification, for example, the description of "60 to 100" means a range of "60 or more and 100 or less".
[0033] In the provisions of the upper limit and the lower limit described in this specification, the numerical range from the lower limit to the upper limit can be specified by appropriately selecting and arbitrarily combining the various options.
[0034] Furthermore, various requirements described as preferred aspects described in this specification may be combined in plural.
[0035] In addition, in this specification, kinematic viscosity and viscosity index mean the value measured or calculated according to JIS K2283:2000.
[0036] The content of phosphorus atoms (P) refers to a value measured in accordance with JPI-5S-38-92.
[0037] The content of sulfur atoms (S) refers to a value measured in accordance with JIS K2541-6:2013.
[0038] [Composition of Lubricating Oil Composition]
[0039] A lubricating oil composition according to one embodiment of the present invention comprises a base oil (A) (hereinafter also referred to as “component (A)”), a phosphite (B) (hereinafter also referred to as “component (B)”), a thiadiazole compound content of less than 0.05% by mass based on the total amount of the lubricating oil composition, and a kinematic viscosity of the lubricating oil composition at 100° C. of 4.2 mm 2 / s or more.
[0040] A lubricating oil composition according to another embodiment of the present invention comprises component (A) and component (B), wherein the content of the thiadiazole compound and the benzotriazole compound are each less than 0.05% by mass based on the total amount of the lubricating oil composition, and the kinematic viscosity of the lubricating oil composition at 100° C. is 4.2 mm 2 / s or more.
[0041] The lubricating oil composition of one embodiment of the present invention contains a phosphite (B) having a predetermined structure together with a base oil (A), thereby being able to form a lubricating oil composition having improved seizure resistance and copper corrosion resistance in a well-balanced manner at a predetermined 100° C. kinematic viscosity even when the contents of the thiadiazole compound (C) and the benzotriazole compound (D) are limited or substantially no thiadiazole compound (C) and the benzotriazole compound (D) are contained.
[0042] Since the lubricating oil composition according to one embodiment of the present invention has such characteristics, it can be suitably used for lubrication of an electric drive unit including at least a gear box and a motor, for example.
[0043] In the lubricating oil composition of one embodiment of the present invention, the total content of components (A) and (B) is preferably 50% by mass or more, more preferably 60% by mass or more, more preferably 70% by mass or more, further preferably 75% by mass or more, further preferably 80% by mass or more, further preferably 85% by mass or more, particularly preferably 90% by mass or more, based on the total amount (100% by mass) of the lubricating oil composition. The total content may be 100% by mass or less, 99.5% by mass or less, 99.0% by mass or less, or 98.0% by mass or less.
[0044] Hereinafter, the details of each component contained in the lubricating oil composition according to one embodiment of the present invention will be described.
[0045] <Ingredient (A): Base oil>
[0046] Examples of the base oil as the component (A) used in one embodiment of the present invention include one or more selected from mineral oils and synthetic oils.
[0047] Examples of mineral oils include atmospheric residues obtained by atmospheric distillation of crude oils such as paraffinic crude oil, intermediate base crude oil, and naphthenic crude oil; distillates obtained by vacuum distillation of these atmospheric residues; refined oils obtained by subjecting the distillates to one or more refining treatments such as solvent deasphalting, solvent extraction, hydrocracking, solvent dewaxing, catalytic dewaxing, and hydrofining (hydrocracking); mineral oils (GTL) obtained by isomerizing wax produced from natural gas by the Fischer-Tropsch process or the like (GTL wax (Gas To Liquids WAX)); mineral oils (CTL) obtained by isomerizing wax produced from coal by the Fischer-Tropsch process or the like (CTL wax (Coal To Liquids WAX)); mineral oils (BTL) obtained by isomerizing wax produced from biomass by the Fischer-Tropsch process or the like (BTL wax (Biomass To Liquids WAX)), etc.
[0048] Examples of synthetic oils include poly-α-olefins such as α-olefin homopolymers or α-olefin copolymers (e.g., α-olefin copolymers having 8 to 14 carbon atoms such as ethylene-α-olefin copolymers); isomeric paraffins; polyalkylene glycols; ester-based synthetic oils such as polyol esters, dibasic acid esters, and phosphate esters; ether-based synthetic oils such as polyphenylene ethers; alkylbenzene-based synthetic oils; and alkylnaphthalene-based synthetic oils.
[0049] The lubricating oil composition according to one embodiment of the present invention may contain a cycloparaffin-based synthetic oil as a base oil, or may not substantially contain the cycloparaffin-based synthetic oil.
[0050] More specifically, in the lubricating oil composition of one embodiment of the present invention, the content of the cycloparaffinic synthetic oil can be, for example, less than 0.05 mass %, less than 0.03 mass %, less than 0.01 mass %, or less than 0.001 mass %, based on the total amount of component (A) contained in the lubricating oil composition.
[0051] Examples of the cycloparaffin-based synthetic oil include cycloparaffin-based synthetic oils containing a cyclohexane ring, a cycloheptane ring, a bicycloheptane ring, a bicyclooctane ring, and the like.
[0052] The component (A) used in one embodiment of the present invention preferably contains one or more selected from mineral oils classified into Group II and Group III in the API (American Petroleum Institute) base oil category, and synthetic oils.
[0053] From the viewpoint of providing a lubricating oil composition capable of reducing seizure on sliding members, the kinetic viscosity of component (A) used in one embodiment of the present invention at 100° C. is preferably 2.5 mm 2 / s or more, more preferably 2.7 mm 2 / s or more, more preferably 2.9 mm 2 / s or more, particularly preferably 3.1 mm 2 / s or more, and preferably 8.0 mm / s from the viewpoint of obtaining a lubricating oil composition with excellent cooling performance 2 / s or less, more preferably 7.5mm 2 / s or less, more preferably 7.0 mm 2 / s or less, more preferably 6.5mm 2 / s or less, particularly preferably 6.0 mm 2 / s or less.
[0054] The viscosity index of the component (A) used in one embodiment of the present invention is preferably 70 or more, more preferably 80 or more, further preferably 90 or more, and particularly preferably 100 or more.
[0055] In one embodiment of the present invention, when a mixed oil composed of two or more base oils is used as component (A), the kinematic viscosity and viscosity index of the mixed oil are preferably within the above ranges. Therefore, the mixed oil can be prepared so as to achieve the kinematic viscosity and viscosity index within the above ranges by using a low-viscosity base oil and a high-viscosity base oil in combination.
[0056] In this case, the mixed oil may be a mixed oil obtained by combining two or more base oils having kinematic viscosities and viscosity indexes at 100° C. within the above ranges, or a mixed oil obtained by combining a base oil having kinematic viscosities and viscosity indexes at 100° C. within the above ranges with a base oil not within the above ranges. In addition, a mixed oil adjusted to be within the above ranges by combining a low-viscosity base oil having kinematic viscosities and viscosity indexes at 100° C. not within the above ranges with a high-viscosity base oil may be used.
[0057] Even when the kinematic viscosity and viscosity index of component (A) at 100° C. are not within the above ranges, the kinematic viscosity and viscosity index of the lubricating oil composition at 100° C. may be within the ranges described below.
[0058] In the lubricating oil composition of one embodiment of the present invention, the content of component (A) is preferably 30% by mass or more, more preferably 40% by mass or more, more preferably 50% by mass or more, further preferably 60% by mass or more, further preferably 70% by mass or more, further preferably 80% by mass or more, particularly preferably 90% by mass or more, based on the total amount (100% by mass) of the lubricating oil composition. It may be 99.9% by mass or less, 99.5% by mass or less, 99.0% by mass or less, 98.5% by mass or less, or 98.0% by mass or less.
[0059] <Ingredient (B): Phosphite>
[0060] In a lubricating oil composition of one embodiment of the present invention, as component (B), a phosphite is contained, wherein at least one sulfur-containing group having 2 to 20 carbon atoms is substituted with at least one -(S)x- group (x is an integer of 1 or more, preferably an integer of 1 to 10, more preferably an integer of 1 to 5, further preferably an integer of 1 to 3, further preferably 1 or 2, and particularly preferably 1) between two adjacent carbon atoms in the structure of the alkyl group. By containing component (B) in a lubricating oil composition having a predetermined kinematic viscosity at 100° C., a lubricating oil composition having improved anti-seizing and anti-copper corrosion can be obtained.
[0061] In one embodiment of the present invention, component (B) may be used alone or in combination of two or more. In addition, component (B) may have one sulfur-containing group or two sulfur-containing groups in the same molecule. The phosphite having one sulfur-containing group in the same molecule (phosphite monoester) and the phosphite having two sulfur-containing groups in the same molecule (phosphite diester) may be used alone or in combination. From the viewpoint of preparing a lubricating oil composition with further improved anti-seizure properties, it is preferred to use a phosphite monoester and a phosphite diester in combination.
[0062] From the above viewpoint, the sulfur-atom-containing group of the phosphite of the component (B) is preferably a group represented by the following general formula (bi).
[0063]
Chemical formula 2
[0064]
[0065] In the above general formula (bi), R b is a straight chain or branched chain alkyl group, A b is a straight chain or branched alkylene group, R b and A b The total number of carbon atoms in is 2 to 20. x is an integer greater than or equal to 1. * represents a bonding position to a phosphorus atom.
[0066] Although R b and A b The total number of carbon atoms is 2 to 20, but is preferably 3 to 18, more preferably 4 to 16, further preferably 5 to 14, and further preferably 6 to 12 from the viewpoint of providing a lubricating oil composition having further improved seizure resistance.
[0067] x is an integer greater than or equal to 1, and is preferably an integer of 1 to 10, more preferably an integer of 1 to 5, further preferably an integer of 1 to 3, further preferably 1 or 2, and particularly preferably 1, from the viewpoint of obtaining a lubricating oil composition having further improved copper corrosion resistance.
[0068] Can be selected as R b The number of carbon atoms in the alkyl group is preferably 1-18, more preferably 1-16, further preferably 3-14, further preferably 4-12, and particularly preferably 6-10.
[0069] As an option for R bThe above-mentioned alkyl group includes, for example, methyl, ethyl, propyl (n-propyl, isopropyl), butyl (n-butyl, sec-butyl, tert-butyl, isobutyl), pentyl, hexyl, 2-ethylhexyl, heptyl, octyl, nonyl, decyl, undecyl, dodecyl, tridecyl, tetradecyl, hexadecyl, octadecyl and the like.
[0070] Can be selected as A b The number of carbon atoms in the alkylene group is preferably 1-18, more preferably 1-16, more preferably 1-12, further preferably 1-10, further preferably 1-8, further preferably 1-6, and particularly preferably 2-4.
[0071] As an option for A b The above-mentioned alkylene group includes, for example, methylene, 1,1-ethylene, 1,2-ethylene, 1,3-propylene, 1,2-propylene, 2,2-propylene and other various propylene groups, various butylene groups, various pentylene groups, various hexylene groups, various heptylene groups, various octylene groups, various nonylene groups, various decylene groups, various undecylene groups, various dodecylene groups, various tridecylene groups, various tetradecylene groups, various pentadecylene groups, various hexadecylene groups, various heptadecylene groups, various octadecylene groups and the like.
[0072] Among them, A can be selected b The above alkylene group is preferably -(CH2) n - (n is an integer of 1 to 19, preferably an integer of 1 to 16, more preferably an integer of 1 to 12, further preferably an integer of 1 to 10, further preferably an integer of 1 to 8, further preferably an integer of 1 to 6, and particularly preferably an integer of 2 to 4).
[0073] In one embodiment of the present invention, examples of the phosphite used as the component (B) include phosphites represented by the following general formula (b-1) or (b-2).
[0074]
Chemical formula 3
[0075]
[0076] In the above formula, R B11 , R B21 and R B22 Each of the linear or branched alkyl groups independently has preferably 1 to 18 carbon atoms, more preferably 1 to 16 carbon atoms, further preferably 3 to 14 carbon atoms, further preferably 4 to 12 carbon atoms, and particularly preferably 6 to 10 carbon atoms.
[0077] In addition, bB11, bB21 and bB22 are each independently an integer of 1 to 10, preferably 1 to 19, more preferably 1 to 16, more preferably 1 to 12, further preferably 1 to 10, further preferably 1 to 8, further preferably 1 to 6, and particularly preferably 2 to 4.
[0078] As an option for R B11 , R B21 and R B22 The above alkyl group can be selected as R in the above general formula (bi) B1 The same is true for the above-mentioned alkyl group, and the suitable number of carbon atoms and specific groups are also the same.
[0079] In one embodiment of the present invention, the phosphite used as the component (B) may be in the form of an amine salt.
[0080] As the amine forming the amine salt, a compound represented by the following general formula (b-3) is preferable. The amine may be used alone or in combination of two or more.
[0081]
Chemical formula 4
[0082]
[0083] In the general formula (b-3), r is an integer of 1 to 3, and preferably 1.
[0084] R x Each independently represents an alkyl group having 6 to 18 carbon atoms, an alkenyl group having 6 to 18 carbon atoms, an aryl group having 6 to 18 carbon atoms, or a hydroxyalkyl group having 6 to 18 carbon atoms.
[0085] It should be noted that when there are multiple R x In the case of multiple R x They can be the same or different from each other.
[0086] In the lubricating oil composition of one embodiment of the present invention, the total content of component (B) is preferably 0.15% by mass or more, more preferably 0.16% by mass or more, even more preferably 0.17% by mass or more, and particularly preferably 0.18% by mass or more, based on the total amount (100% by mass) of the lubricating oil composition, from the viewpoint of providing a lubricating oil composition having further improved anti-seizing properties. Furthermore, from the viewpoint of providing a lubricating oil composition having further improved copper corrosion resistance, the total content of component (B) is preferably less than 1.00% by mass, more preferably 0.95% by mass or less, more preferably 0.90% by mass or less, even more preferably 0.85% by mass or less, even more preferably 0.80% by mass or less, even more preferably 0.75% by mass or less, even more preferably 0.70% by mass or less, even more preferably 0.65% by mass or less, even more preferably 0.60% by mass or less, even more preferably 0.55% by mass or less, even more preferably 0.50% by mass or less, even more preferably 0.45% by mass or less, and particularly preferably 0.40% by mass or less.
[0087] In the lubricating oil composition of one embodiment of the present invention, from the viewpoint of obtaining a lubricating oil composition having a good balance between scuffing resistance and copper corrosion resistance, component (B) preferably contains both a compound (B1) represented by the above general formula (b-1) and a compound (B2) represented by the above general formula (b-2).
[0088] In one embodiment of the present invention, the content ratio of compound (B1) to compound (B2) [(B1) / (B2)] is preferably 1 / 20 to 20 / 1, more preferably 1 / 18 to 18 / 1, further preferably 1 / 16 to 16 / 1, further preferably 1 / 14 to 14 / 1, further preferably 1 / 12 to 12 / 1, and particularly preferably 1 / 10 to 10 / 1, in terms of mass ratio.
[0089] From the above viewpoints, in the lubricating oil composition of one embodiment of the present invention, the content of component (B) in terms of phosphorus atoms, based on the total amount (100 mass %) of the lubricating oil composition, is preferably 20 mass ppm or more, more preferably 50 mass ppm or more, more preferably 100 mass ppm or more, further preferably 120 mass ppm or more, further preferably 150 mass ppm or more, further preferably 170 mass ppm or more, particularly preferably 200 mass ppm or more, and is preferably 800 mass ppm or less, more preferably 700 mass ppm or less, further preferably 600 mass ppm or less, further preferably 500 mass ppm or less, and particularly preferably 400 mass ppm or less.
[0090] From the above viewpoints, in the lubricating oil composition of one embodiment of the present invention, the content of component (B) in terms of sulfur atom is preferably 10 mass ppm or more, more preferably 50 mass ppm or more, more preferably 100 mass ppm or more, further preferably 150 mass ppm or more, further preferably 170 mass ppm or more, further preferably 200 mass ppm or more, particularly preferably 230 mass ppm or more, and is preferably 800 mass ppm or less, more preferably 700 mass ppm or less, further preferably 600 mass ppm or less, further preferably 500 mass ppm or less, and particularly preferably 400 mass ppm or less.
[0091] <Thiadiazole compounds>
[0092] In the lubricating oil composition of one embodiment of the present invention, the content of the thiadiazole compound is limited to less than 0.05% by mass based on the total amount of the lubricating oil composition. If the content of the thiadiazole compound is 0.05% by mass or more, copper turns black in a long-term copper corrosion test. In the lubricating oil composition of one embodiment of the present invention, by limiting the content of the thiadiazole as described above and containing the above-mentioned component (B), the kinematic viscosity of the lubricating oil composition at 100° C. is adjusted to a predetermined range, thereby being able to form a lubricating oil composition with improved scuffing resistance and copper corrosion resistance in a well-balanced manner.
[0093] In the lubricating oil composition of one embodiment of the present invention, the content of the thiadiazole compound is less than 0.05 mass %, more preferably less than 0.03 mass %, further preferably less than 0.01 mass %, particularly preferably less than 0.001 mass %, based on the total amount of the lubricating oil composition.
[0094] It should be noted that in the lubricating oil composition of one embodiment of the present invention, it is preferred that the thiadiazole compound is substantially not contained. Here, "substantially not containing a thiadiazole compound" means that the lubricating oil composition in which the thiadiazole compound is intentionally blended is excluded, and it does not mean that the embodiment in which the thiadiazole compound is inevitably blended is excluded, but the content of such thiadiazole compound is also preferably as small as possible. Specifically, the content of the thiadiazole compound inevitably mixed is less than 0.05% by mass, more preferably less than 0.03% by mass, further preferably less than 0.01% by mass, and particularly preferably less than 0.001% by mass based on the total amount of the lubricating oil composition.
[0095] In one embodiment of the present invention, examples of the thiadiazole compound include compounds having a thiadiazole ring, and examples thereof include compounds represented by any one of the following general formulae (c-1) to (c-4).
[0096]
Chemical formula 5
[0097]
[0098] In the above formula, R c1 and R c2 Each is independently a hydrocarbon group.
[0099] m and n may each independently be an integer of 1 to 10, an integer of 1 to 6, an integer of 1 to 4, or an integer of 2 to 3.
[0100] As an option for R c1 and R c2 The above hydrocarbon groups include, for example, methyl, ethyl, propyl (n-propyl, isopropyl), butyl (n-butyl, sec-butyl, tert-butyl, isobutyl), pentyl, hexyl, heptyl, octyl, 2-ethylhexyl, nonyl, 1,1-dimethylheptyl, decyl, undecyl, dodecyl, tridecyl, tetradecyl, pentadecyl, hexadecyl, heptadecyl, octadecyl and other linear or branched alkyl groups; vinyl, propenyl, butenyl, pentenyl, hexenyl, heptenyl, octenyl, nonenyl, decyl, Straight-chain or branched alkenyl groups such as alkenyl, undecenyl, dodecenyl, tridecenyl, tetradecenyl, and pentadecenyl; cycloalkyl groups which may have an alkyl group such as cyclohexyl, dimethylcyclohexyl, ethylcyclohexyl, propylcyclohexyl, butylcyclohexyl, and heptylcyclohexyl; aryl groups such as phenyl, naphthyl, anthracenyl, biphenyl, and terphenyl; alkylaryl groups such as tolyl, dimethylphenyl, butylphenyl, nonylphenyl, methylbenzyl, and dimethylnaphthyl; arylalkyl groups such as phenylmethyl, phenylethyl, and diphenylmethyl, etc.
[0101] Can be selected as R c1 and R c2 The number of carbon atoms of the hydrocarbon group may be 1 or more, 2 or more, 3 or more, or 5 or more, and may be 30 or less, 20 or less, 16 or less, or 12 or less.
[0102] <Benzotriazole compounds>
[0103] In the lubricating oil composition of one embodiment of the present invention, the content of the benzotriazole compound is limited to less than 0.05% by mass based on the total amount of the lubricating oil composition. In the lubricating oil composition of one embodiment of the present invention, by limiting the content of the benzotriazole compound as described above and containing the above-mentioned component (B), the kinematic viscosity of the lubricating oil composition at 100° C. is adjusted to a predetermined range, thereby being able to form a lubricating oil composition with improved scuffing resistance and copper corrosion resistance in a well-balanced manner.
[0104] In the lubricating oil composition of one embodiment of the present invention, the content of the benzotriazole compound is less than 0.05% by mass, more preferably less than 0.03% by mass, further preferably less than 0.01% by mass, and particularly preferably less than 0.001% by mass, based on the total amount of the lubricating oil composition.
[0105] It should be noted that in the lubricating oil composition of one embodiment of the present invention, it is preferred that the benzotriazole compound is not substantially contained. Here, "substantially not containing a benzotriazole compound" means that the lubricating oil composition in which the benzotriazole compound is intentionally blended is excluded, and it does not mean that the embodiment in which the benzotriazole compound is inevitably blended is excluded, but the content of such benzotriazole compound is also preferably as small as possible. Specifically, the content of the inevitably mixed benzotriazole compound is less than 0.05% by mass, more preferably less than 0.03% by mass, further preferably less than 0.01% by mass, and particularly preferably less than 0.001% by mass based on the total amount of the lubricating oil composition.
[0106] In one embodiment of the present invention, examples of the benzotriazole compound include compounds having a benzotriazole structure, and examples thereof include compounds represented by the following general formula (d-0).
[0107]
Chemical formula 6
[0108]
[0109] In the above general formula (d-0), R D1 It is a hydrocarbon group which may contain at least one atom selected from the group consisting of an oxygen atom, a sulfur atom and a nitrogen atom, or a hydrogen atom.
[0110] R D2 Each independently is a hydrocarbon group which may contain at least one atom selected from the group consisting of an oxygen atom, a sulfur atom and a nitrogen atom.
[0111] z1 may be an integer of 0-4, an integer of 0-2, or an integer of 0-1.
[0112] Examples of the hydrocarbon group include an alkyl group, an alkenyl group, a cycloalkyl group, an aryl group, and a group formed by combining two or more of these groups.
[0113] Can be selected as R D1 The number of carbon atoms of the hydrocarbon group is, for example, 1 to 30, 3 to 26, or 6 to 20.
[0114] Can be selected as R D2 The number of carbon atoms in the hydrocarbon group is, for example, 1 to 20, 1 to 12, 1 to 6, or 1 to 2.
[0115] Examples of the alkyl group include methyl, ethyl, propyl (n-propyl, isopropyl), butyl (n-butyl, isobutyl, sec-butyl, tert-butyl), pentyl (n-pentyl, isopentyl, neopentyl), hexyl, heptyl, octyl, 2-ethylhexyl, nonyl, decyl, undecyl, dodecyl, tridecyl, tetradecyl, pentadecyl, hexadecyl, heptadecyl, and octadecyl.
[0116] The alkyl group may be a linear alkyl group or a branched alkyl group.
[0117] Examples of the alkenyl group include vinyl group, propenyl, butenyl, pentenyl, hexenyl, heptenyl, octenyl, nonenyl, decenyl, dodecenyl, tridecenyl, tetradecenyl, pentadecenyl, hexadecenyl, and octadecenyl (oleyl) groups.
[0118] The alkenyl group may be a straight-chain alkenyl group or a branched-chain alkenyl group.
[0119] Examples of the cycloalkyl group include cyclopropyl, cyclobutyl, cyclopentyl, cyclohexyl, cycloheptyl, cyclooctyl, and adamantyl.
[0120] Examples of the aryl group include a phenyl group, a naphthyl group, an anthryl group, a phenanthryl group, a biphenyl group, a terphenyl group, and a phenylnaphthyl group.
[0121] <Various additives>
[0122] The lubricating oil composition of one embodiment of the present invention may contain various additives as necessary within a range that does not impair the effects of the present invention.
[0123] Examples of such additives include pour point depressants, viscosity index improvers, antioxidants, metal detergents, ashless dispersants, rust inhibitors, and defoaming agents.
[0124] These lubricating oil additives may be used alone or in combination of two or more.
[0125] The content of each of these various additives can be appropriately adjusted within a range that does not impair the effects of the present invention. The content of each additive independently is usually 0.001 to 15 mass %, preferably 0.005 to 10 mass %, and more preferably 0.01 to 8 mass %, based on the total amount (100 mass %) of the lubricating oil composition.
[0126] [Pour point depressant]
[0127] The lubricating oil composition of one embodiment of the present invention may further contain a pour point depressant. The pour point depressants may be used alone or in combination of two or more.
[0128] Examples of the pour point depressant used in one embodiment of the present invention include ethylene-vinyl acetate copolymers, condensates of chlorinated paraffin and naphthalene, condensates of chlorinated paraffin and phenol, polymethacrylates, and polyalkylstyrenes.
[0129] The pour point depressant used in one embodiment of the present invention may have a mass average molecular weight (Mw) of 5,000 or more, 7,000 or more, 10,000 or more, 15,000 or more, 20,000 or more, 25,000 or more, 30,000 or more, 35,000 or more, 40,000 or more, 45,000 or more, 50,000 or more, 55,000 or more, or 60,000 or more, and may be 150,000 or less, 120,000 or less, 100,000 or less, 90,000 or less, or 80,000 or less.
[0130] [Viscosity index improver]
[0131] The lubricating oil composition of one embodiment of the present invention may further contain a viscosity index improver. The viscosity index improver may be used alone or in combination of two or more.
[0132] Examples of the viscosity index improver used in one embodiment of the present invention include polymers such as non-dispersed polymethacrylate, dispersed polymethacrylate, olefin copolymers (e.g., ethylene-propylene copolymers), dispersed olefin copolymers, and styrene copolymers (e.g., styrene-diene copolymers, styrene-isoprene copolymers).
[0133] The weight average molecular weight (Mw) of the viscosity index improver used in one embodiment of the present invention may be 5,000 or more, 7,000 or more, 10,000 or more, 15,000 or more, or 20,000 or more, and may be 1,000,000 or less, 700,000 or less, 500,000 or less, 300,000 or less, 200,000 or less, 100,000 or less, or 50,000 or less.
[0134] [Antioxidants]
[0135] The lubricating oil composition of one embodiment of the present invention may further contain an antioxidant. The antioxidant may be used alone or in combination of two or more.
[0136] As the antioxidant used in one embodiment of the present invention, for example, amine antioxidants such as alkylated diphenylamine, phenylnaphthylamine, and alkylated phenylnaphthylamine; phenol antioxidants such as 2,6-di-tert-butylphenol, 4,4'-methylenebis(2,6-di-tert-butylphenol), 3-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate, and 3-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate; sulfur antioxidants such as phenothiazine, dioctadecyl sulfide, 3,3'-dilauryl thiodipropionate, and 2-mercaptobenzimidazole.
[0137] [Metallic detergent]
[0138] The lubricating oil composition of one embodiment of the present invention may further contain a metallic detergent. The metallic detergent may be used alone or in combination of two or more.
[0139] As the metal detergent used in one embodiment of the present invention, metal salts such as metal sulfonates, metal salicylates and metal phenates can be cited. In addition, as the metal atom constituting the metal salt, a metal atom selected from alkali metals and alkaline earth metals is preferred, more preferably sodium, calcium, magnesium or barium, and further preferably calcium.
[0140] In the lubricating oil composition of one embodiment of the present invention, the metallic detergent preferably includes one or more selected from the group consisting of calcium sulfonate, calcium salicylate, and calcium phenate, and more preferably includes calcium sulfonate.
[0141] The content of calcium sulfonate is preferably 50 to 100 mass %, more preferably 60 to 100 mass %, further preferably 70 to 100 mass %, and further preferably 80 to 100 mass %, based on the total amount (100 mass %) of the metallic detergent contained in the lubricating oil composition.
[0142] The base number of the metal detergent is preferably 0 to 600 mgKOH / g.
[0143] Among them, in the lubricating oil composition of one embodiment of the present invention, the metallic detergent is preferably an overbased metallic detergent having a base value of 100 mgKOH / g or more.
[0144] The base number of the overbased metal detergent is 100 mgKOH / g or more, preferably 150 to 500 mgKOH / g, and more preferably 200 to 450 mgKOH / g.
[0145] In addition, in this specification, "base number" means the base number measured by the perchloric acid method based on 7. of JIS K2501:2003 "Petroleum products and lubricating oils-Neutralization number test method".
[0146] [Ashless dispersant]
[0147] From the viewpoint of improving the dispersibility of component (B), the lubricating oil composition of one embodiment of the present invention may further contain an ashless dispersant. The ashless dispersants may be used alone or in combination of two or more.
[0148] As the ashless dispersant used in one embodiment of the present invention, alkenyl succinic acid imide is preferred, and examples thereof include alkenyl succinic acid bisimide represented by the following general formula (e-1) and alkenyl succinic acid monoimide represented by the following general formula (e-2).
[0149]
Chemical formula 7
[0150]
[0151] In the above general formulas (e-1) and (e-2), R E1 , R E2 and R E3 Each independently is an alkenyl group having a mass average molecular weight (Mw) of 500 to 3000 (preferably 900 to 2500).
[0152] As an option for R E1 , R E2 and R E3 Examples of the alkenyl group include a polybutenyl group, a polyisobutenyl group, and an ethylene-propylene copolymer. Among them, a polybutenyl group or a polyisobutenyl group is preferred.
[0153] A E1 , A E2 and A E3 Each is independently an alkylene group having 2 to 5 carbon atoms.
[0154] e1 is an integer of 0-10, preferably an integer of 1-4, and more preferably 2 or 3.
[0155] e2 is an integer of 1 to 10, preferably an integer of 2 to 5, and more preferably 3 or 4.
[0156] It should be noted that the compound represented by the general formula (e-1) or (e-2) may be a modified alkenyl succinimide obtained by reacting with one or more selected from boron compounds, alcohols, aldehydes, ketones, alkylphenols, cyclic carbonates, epoxy compounds and organic acids.
[0157] [Rust inhibitor]
[0158] The lubricating oil composition of one embodiment of the present invention may further contain a rust inhibitor. The rust inhibitor may be used alone or in combination of two or more.
[0159] Examples of the rust inhibitor used in one embodiment of the present invention include fatty acids, alkenyl succinic acid half esters, fatty acid soaps, alkyl sulfonates, polyhydric alcohol fatty acid esters, fatty acid amines, oxidized paraffins, and alkyl polyoxyethylene ethers.
[0160] [Defoaming agent]
[0161] The lubricating oil composition of one embodiment of the present invention may further contain a defoaming agent. The defoaming agent may be used alone or in combination of two or more.
[0162] Examples of the defoaming agent used in one embodiment of the present invention include alkyl silicone-based defoaming agents, fluorosilicone-based defoaming agents, and fluoroalkyl ether-based defoaming agents.
[0163] <Method for producing lubricating oil composition>
[0164] A method for producing a lubricating oil composition according to one embodiment of the present invention comprises the steps of blending a component (B) with a component (A), wherein the kinematic viscosity of the lubricating oil composition at 100° C. is 4.2 mm 2 / s or more. In addition, the method for producing a lubricating oil composition of one embodiment of the present invention does not include the step of blending a thiadiazole compound. The method for producing a lubricating oil composition of another embodiment of the present invention does not include the step of blending a benzotriazole compound. The method for producing a lubricating oil composition of yet another embodiment of the present invention does not include the step of blending a thiadiazole compound and a benzotriazole compound.
[0165] The method for producing a lubricating oil composition according to one embodiment of the present invention preferably includes a step of blending other additives as necessary.
[0166] Preferred compounds and blending amounts of the component (A), the component (B) and various additives are as described above.
[0167] In addition, additives such as the viscosity index improver, the pour point depressant, and the antifoaming agent are preferably blended in a state of being dissolved in the diluent oil.
[0168] [Properties of Lubricating Oil Composition]
[0169] From the viewpoint of providing a lubricating oil composition having further improved anti-seizure properties, the kinematic viscosity of the lubricating oil composition of one embodiment of the present invention at 100° C. is preferably 4.2 mm 2 / s or more, more preferably 4.3 mm 2 / s or more, more preferably 4.4 mm 2 / s or more, and preferably 8.0 mm / s from the viewpoint of obtaining a lubricating oil composition with improved cooling performance 2 / s or less, more preferably 7.5mm 2 / s or less, more preferably 7.0 mm 2 / s or less, more preferably 6.5mm 2 / s or less, particularly preferably 6.0 mm 2 / s or less.
[0170] The viscosity index of the lubricating oil composition of one embodiment of the present invention is preferably 90 or more, more preferably 100 or more, even more preferably 110 or more, even more preferably 120 or more, and particularly preferably 130 or more.
[0171] [Application of lubricating oil composition]
[0172] The lubricating oil composition according to a preferred embodiment of the present invention can improve the scuffing resistance and copper corrosion resistance in a well-balanced manner.
[0173] In view of such characteristics, the lubricating oil composition of one embodiment of the present invention can be suitably used for lubrication of mechanisms such as torque converters, wet clutches, gear bearing mechanisms, oil pumps, and hydraulic control mechanisms installed in various devices such as engines, transmissions, speed reducers, compressors, and hydraulic devices.
[0174] Among them, the lubricating oil composition of one embodiment of the present invention is preferably used for lubricating various mechanisms of an electric drive unit including at least a gear box and a motor. The electric drive unit is mounted on a fuel cell vehicle, an electric vehicle, and a hybrid vehicle.
[0175] When the lubricating oil composition of one embodiment of the present invention is used in an electric drive unit, it plays the role of cooling the motor and lubricating the gearbox. In particular, the lubricating oil composition of one embodiment of the present invention has excellent anti-seizing and copper corrosion resistance, so the lubricity of the gearbox is good, and has excellent copper corrosion resistance, so it has the characteristic of preventing corrosion of copper-based components constituting the motor even when used for cooling the motor.
[0176] In addition, in view of the above-mentioned characteristics of the lubricating oil composition of one embodiment of the present invention, the present invention can also provide the following [1] and [2].
[0177] [1] An electric drive unit filled with the lubricating oil composition according to one embodiment of the present invention, the electric drive unit comprising at least a gear box and an electric motor.
[0178] [2] Use of a lubricating oil composition, wherein the lubricating oil composition according to one embodiment of the present invention is applied to an electric drive unit including at least a gear box and a motor.
[0179] Preferred embodiments of the lubricating oil composition described in [1] and [2] are as described above.
[0180] Example
[0181] Next, the present invention will be described in more detail by way of examples, but the present invention is not limited to these examples. It should be noted that the methods for measuring various physical properties are as follows.
[0182] (1) Kinematic viscosity and viscosity index
[0183] The measurement and calculation were performed in accordance with JIS K2283:2000.
[0184] (2) Phosphorus atom content
[0185] The measurement was performed in accordance with JPI-5S-38-92.
[0186] (3) Sulfur atom content
[0187] The measurement was conducted in accordance with JIS K2541-6:2013.
[0188] Examples 1 to 3, Comparative Examples 1 to 5
[0189] Components (A) and (B) shown in Table 2 and other additives were added in the amounts shown in Table 1 and mixed thoroughly to prepare lubricating oil compositions. The details of the components used in the preparation of the lubricating oil compositions are as follows. It should be noted that the lubricating oil compositions of Examples 1 to 3 do not contain a benzotriazole compound.
[0190] <Ingredients (A)>
[0191] ・Mineral oil (a1): 70N mineral oil classified as Group II of API base oil category, kinematic viscosity at 100°C = 3.1 mm 2 / s, viscosity index = 109.
[0192] ・Mineral oil (a2): 100N mineral oil classified as Group III of API base oil category, kinematic viscosity at 100°C = 4.2 mm 2 / s, viscosity index = 122.
[0193] <Ingredient (B)>
[0194] ・“Phosphite (b)”: R in the above general formula (b-1) B11 For n-octyl (-C8H 17 ), a compound corresponding to component (B1) in which bB11 is 2(1,2-ethylene (-C2H4-)) (a compound represented by the following formula (b-1-1)) and R in the above general formula (b-2) B11 , R B22 For n-octyl (-C8H 17), bB11, bB22 are 2 (1,2-ethylene (-C2H4-)) compounds corresponding to component (B2) (compounds represented by the following formula (b-2-1)) mixed in a ratio of component (B1) / component (B2) = 9 / 1 (mass ratio). Sulfur atom content = 10.7% by mass, phosphorus atom content = 10% by mass.
[0195] <Other additives other than components (A) and (B)>
[0196] ・Extreme pressure agent: Thiadiazole (2,5-bis(1,1-dimethylheptyl disulfide)-1,3,4-thiadiazole, in the above general formula (c-1), m=n=2, R C1 and R C2 The thiadiazole is a 1,1-dimethylheptyl group (a compound represented by the following formula (c-1-1)).
[0197]
Chemical formula 8
[0198]
[0199] ・Extreme pressure agent: Tricresyl phosphate.
[0200] ・Viscosity index improver: Polymethacrylate-based viscosity index improver (content based on resin component conversion: 0.13% by mass).
[0201] ・“Additive mixture”: An additive mixture prepared by mixing an antioxidant, a metallic detergent, an ashless dispersant, a pour point depressant and a defoamer and diluting the mixture with 70N hydrocracked mineral oil.
[0202] The kinematic viscosity and viscosity index of the prepared lubricating oil composition were measured or calculated, and the following tests were performed. The results are shown in Table 1.
[0203] (1) FZG bonding test (A10 / 16.6R / 90)
[0204] According to ASTM D5182, using A10 gears, under the conditions of sample oil temperature of 90°C, rotation speed of 2900 rpm, and running time of about 7.5 minutes, the load is increased stepwise as specified to determine the load level at which seizure occurs. The higher the value of this level, the better the anti-seizure property of the lubricating oil composition.
[0205] (2) Copper corrosion resistance test
[0206] According to the test tube method of JIS K2513 "Petroleum Products Copper Plate Corrosion Test Method", the copper plate corrosion test was carried out under the conditions of a test temperature of 150°C and a test time of 168 hours, and the discoloration state of the copper plate was observed. Based on the "Table 1 Classification of Corrosion Based on Copper Plate Corrosion Standard" of JIS K2513 shown in Table 1 below, the copper corrosion resistance in the liquid phase was evaluated. It should be noted that in Table 2, the "color change number (subdivision symbol)" is recorded, and the smaller the number of the color change number, the smaller the copper corrosion resistance, and the degree of corrosion is indicated in alphabetical order.
[0207]
Table 1
[0208]
[0209]
Table 2
[0210]
[0211] As can be seen from Table 2, the lubricating oil compositions prepared in Examples 1 to 3 showed excellent results in terms of both anti-seizing and anti-copper corrosion. On the other hand, the results of Comparative Examples 1, 2, and 5 showed good anti-copper corrosion but poor anti-seizing. Furthermore, the results of Comparative Examples 3 and 4 showed good anti-seizing but poor anti-copper corrosion.
Claims
1. A lubricating oil composition comprising a base oil (A) and a phosphite (B), wherein the phosphite (B) has at least one sulfur-containing group having 2 to 20 carbon atoms and having at least one -(S)x- group between two adjacent carbon atoms in the alkyl structure, wherein: x is an integer greater than or equal to 1, The content of the thiadiazole compound is less than 0.05% by mass based on the total amount of the lubricating oil composition. The kinematic viscosity of the lubricating oil composition at 100°C is 4.2 mm 2 / s or more.
2. The lubricating oil composition according to claim 1, wherein The phosphite (B) contains at least one selected from the group consisting of a compound (B1) represented by the following general formula (b-1) and a compound (B2) represented by the following general formula (b-2). In the general formula (b-1) and the general formula (b-2), R B11 , R B21 and R B22 Each independently represents an alkyl group having 1 to 19 carbon atoms, b B11 、b B21 and b B22 Each independently represents an integer of 1 to 10.
3. The lubricating oil composition according to claim 1 or 2, wherein The content of the benzotriazole compound is less than 0.05 mass % based on the total amount of the lubricating oil composition.
4. The lubricating oil composition according to any one of claims 1 to 3, wherein The content of the phosphite (B) is 0.15 mass % or more and less than 1.00 mass % based on the total amount of the lubricating oil composition.
5. The lubricating oil composition according to any one of claims 1 to 4, wherein The base oil (A) is at least one selected from mineral oil, poly-α-olefin, isoparaffin, polyalkylene glycol, ester synthetic oil, ether synthetic oil, alkylbenzene synthetic oil, alkylnaphthalene synthetic oil, GTL, CTL and BTL. 6 . The lubricating oil composition according to claim 1 , which is used for lubrication of an electric drive unit comprising at least a gear box and a motor. 7 . An electric drive unit filled with the lubricating oil composition according to claim 1 , comprising at least a gear box and a motor.
8. Use of a lubricating oil composition, wherein: The lubricating oil composition according to any one of claims 1 to 5 is used for lubrication of an electric drive unit including at least a gear box and a motor.
9. A method for producing a lubricating oil composition, which is a method for producing the lubricating oil composition according to any one of claims 1 to 5, A phosphite (B) is added to a base oil (A), wherein the phosphite (B) has at least one sulfur-containing group having 2 to 20 carbon atoms and having at least one -(S)x- group between two adjacent carbon atoms in the alkyl structure, wherein: x is an integer greater than or equal to 1, The content of the thiadiazole compound is less than 0.05% by mass based on the total amount of the lubricating oil composition, and the kinematic viscosity of the lubricating oil composition at 100° C. reaches 4.2 mm 2 / s is prepared in the above manner.