Longitudinal silicon carbide device

By optimizing the structure and process of vertical silicon carbide devices, the problems of weak gate control capability and insufficient freewheeling capability of silicon carbide power MOSFETs were solved, achieving the effects of low resistance conductivity, strong gate control and low loss.

CN221928089UActive Publication Date: 2024-10-29GLOBAL POWER TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420390658.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-29
Publication Date
2024-10-29
Estimated Expiration
2034-02-28

AI Technical Summary

Technical Problem

Existing silicon carbide power MOSFETs have weak gate control capabilities, requiring a high gate voltage to achieve full conduction. Furthermore, the body diode has weak freewheeling capability, which may cause surge current to damage the device during turn-off.

Method used

Design a vertical silicon carbide device, including a silicon carbide substrate, a drift layer, a source region, first and second gate insulating regions, first and second gate metal layers, a source metal layer, and a drain metal layer. By optimizing the thickness and doping concentration of each layer, a simple structure, strong gate control capability, low gate drive loss, low off-state loss, and strong body diode freewheeling capability are achieved.

Benefits of technology

The device achieves low resistance conductivity, strong gate control capability, low off-state leakage current, low body diode on-resistance, strong freewheeling capability, and has a simple fabrication process and low cost.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221928089U_ABST
    Figure CN221928089U_ABST
Patent Text Reader

Abstract

The utility model provides a longitudinal silicon carbide device, which comprises a silicon carbide substrate and a drift layer, the drift layer is connected to the upper side surface of the silicon carbide substrate, and the middle part of the drift layer is provided with a source region; the bottom of the first gate insulation region is connected to the drift layer, and the right side of the first gate insulation region is connected to the left side of the source region; the bottom of the second gate insulation region is connected to the drift layer, and the left side of the second gate insulation region is connected to the right side of the source region; the first gate metal layer is arranged in the first gate insulation region; the second gate metal layer is arranged in the second gate insulation region; the source electrode metal layer is connected to the source region; the drain electrode metal layer is connected to the lower side surface of the silicon carbide substrate; and the gate control capability of the device and the follow current capability of the body diode are high.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to a longitudinal silicon carbide device. Background Art

[0002] Silicon carbide power devices have been widely used, but in order to achieve high performance, high power density and low cost of power electronic systems.

[0003] Existing silicon carbide power MOSFETs have the problem of relatively weak gate control capability, so a higher gate voltage is required to achieve full conduction of the device; and the body diode in the silicon carbide power device has weak freewheeling capability, and the surge current during shutdown may damage the device. Utility Model Content

[0004] The technical problem to be solved by the utility model is to provide a longitudinal silicon carbide device, so that the device has a simple structure, a simple preparation process, a strong gate control capability, a small gate drive loss, a low off-state loss and a strong body diode freewheeling capability.

[0005] The utility model is implemented as follows: a vertical silicon carbide device, comprising:

[0006] A silicon carbide substrate,

[0007] a drift layer, the drift layer being connected to the upper side of the silicon carbide substrate, and a source region being provided in the middle of the drift layer;

[0008] a first gate insulating region, wherein the bottom of the first gate insulating region is connected to the drift layer, and the right side of the first gate insulating region is connected to the left side of the source region;

[0009] a second gate insulating region, wherein the bottom of the second gate insulating region is connected to the drift layer, and the left side of the second gate insulating region is connected to the right side of the source region;

[0010] A first gate metal layer, wherein the first gate metal layer is disposed in the first gate insulating region;

[0011] a second gate metal layer, wherein the second gate metal layer is disposed in the second gate insulating region;

[0012] a source metal layer connected to the source region;

[0013] and a drain metal layer connected to the lower side of the silicon carbide substrate.

[0014] Furthermore, the thickness of the silicon carbide substrate is 10-100 nm.

[0015] Furthermore, the drift layer has a thickness of 1000-5000 nm.

[0016] Furthermore, the thickness of the source region is 100-300 nm.

[0017] Furthermore, the thickness of the first gate insulating region is 100-500 nm, the thickness of the second gate insulating region is 100-500 nm, and the thickness of the first gate insulating region and the second gate insulating region are both greater than or equal to the thickness of the source region.

[0018] The utility model has the following advantages: the device has a simple structure, a simple preparation process, a strong gate control capability, a small gate drive loss, a low off-state loss and a strong body diode freewheeling capability. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] The present invention will be further described below in conjunction with the embodiments with reference to the accompanying drawings.

[0020] Figure 1 The utility model is a schematic diagram of a planar gate silicon carbide MOSFET based on a diamond substrate.

[0021] Figure 2 The utility model is a flow chart of a method for manufacturing a planar gate silicon carbide MOSFET based on a diamond substrate.

[0022] Figure 3 This is a cross-sectional view of the process of a planar gate silicon carbide MOSFET based on a diamond substrate in the utility model. Figure 1 .

[0023] Figure 4 This is a cross-sectional view of the process of a planar gate silicon carbide MOSFET based on a diamond substrate in the utility model. Figure 2 .

[0024] Figure 5 This is a cross-sectional view of the process of a planar gate silicon carbide MOSFET based on a diamond substrate in the utility model. Figure 3 .

[0025] Figure 6 This is a cross-sectional view of the process of a planar gate silicon carbide MOSFET based on a diamond substrate in the utility model. Figure 4 .

[0026] Figure 7 This is a cross-sectional view of the process of a planar gate silicon carbide MOSFET based on a diamond substrate in the utility model. Figure 5 .

[0027] Figure 8 This is a cross-sectional view of the process of a planar gate silicon carbide MOSFET based on a diamond substrate in the utility model. Figure 6 .

[0028] Fig. 9This is a cross-sectional view of the process of a planar gate silicon carbide MOSFET based on a diamond substrate in the utility model. Figure 7 . DETAILED DESCRIPTION

[0029] like Figure 1 As shown, the utility model provides a vertical silicon carbide device, comprising:

[0030] A silicon carbide substrate 1,

[0031] a drift layer 2, wherein the drift layer 2 is connected to the upper side of the silicon carbide substrate 1, and a source region 21 is provided in the middle of the drift layer 2;

[0032] a first gate insulating region 3, wherein the bottom of the first gate insulating region 3 is connected to the drift layer 2, and the right side of the first gate insulating region 3 is connected to the left side of the source region 21;

[0033] a second gate insulating region 4, wherein the bottom of the second gate insulating region 4 is connected to the drift layer 2, and the left side of the second gate insulating region 4 is connected to the right side of the source region 21;

[0034] A first gate metal layer 5, wherein the first gate metal layer 5 is disposed in the first gate insulating region 3;

[0035] A second gate metal layer 6, wherein the second gate metal layer 6 is disposed in the second gate insulating region 4;

[0036] A source metal layer 7, wherein the source metal layer 7 is connected to the source region 21;

[0037] and a drain metal layer 8 , wherein the drain metal layer 8 is connected to the lower side of the silicon carbide substrate 1 .

[0038] The substrate is a silicon carbide N-type substrate with a doping concentration of 1×10 15 cm -3 ~8×10 15 cm -3 The thickness is 10-100nm. This doping concentration is to improve the withstand voltage near the drain of the device. The thickness is within this range, thin enough, and will not affect the drain contact resistance of the device, reducing the on-resistance of the device. The drift layer is silicon carbide N-type epitaxial, and its doping concentration is 1×10 16 cm -3 ~1×10 17 cm -3, with a thickness of 1000-5000nm. The drift layer is the main voltage-resistant structure of the device. Its thickness needs to be thick enough to ensure the voltage-resistant capability. In order to achieve a compromise between voltage-resistant and on-resistance, the corresponding thickness and doping concentration are set; at this thickness, a voltage-resistant effect of 600V can be achieved, and at this doping concentration, the on-resistance is not too large. The doping concentration of the p-type source region is 6×10 19 cm -3 ~5×10 20 cm -3 , the thickness is 100-300nm, the doping concentration of the P-type source region is selected mainly to improve the gate control capability of the device; the thickness of the first gate insulating region and the second gate insulating region are both greater than or equal to the thickness of the source region, and the gate control capability is improved by matching the thickness with the trench gate depth.

[0039] The first gate insulating region and the second gate insulating region are both silicon dioxide formed by oxidation, and the thickness of the first gate insulating region and the second gate insulating region is 100-500nm, which can ensure both the growth speed of the gate oxide and the gate withstand voltage characteristics of the device.

[0040] When positive voltage is applied to the first gate metal layer and the second gate metal layer, the parts on both sides of the P-type source region close to the first gate insulating region and the second gate insulating region diffuse to the middle to form a conductive channel. Since the conductive channel is formed by the first gate metal layer and the second gate metal layer, only a lower gate voltage is required to form the conductive channel, thereby achieving low-resistance conduction of the device. Since the device is under zero gate bias conditions, the device conductive path is completely shut off by the space charge region formed by the P-type source region and the drift layer, so its off-state leakage is small; and the first gate metal layer and the second gate metal layer simultaneously control the conductive channel on both sides, and the gate control capability is strong.

[0041] The P-type source region and the source metal of the device form an ohmic contact, and the P-type source region and the drift layer form a pn junction. During the freewheeling of the device body diode, the delayed current flows along the source metal layer, the P-type source region, the drift layer, the SiC substrate and the drain metal layer, which is the same as the conductive channel when the device is turned on, so the on-resistance of its body diode is low and the freewheeling capability is strong. The device has a simple structure and a simple preparation process, and can achieve both high performance and relatively low cost.

[0042] like Figures 1 to 9 As shown, the method for manufacturing the above-mentioned silicon carbide device includes:

[0043] Step 1: obtaining a silicon carbide substrate 1 with a drift layer 2, and depositing metal on the silicon carbide substrate 1 to form a drain metal layer 8, and epitaxially growing a source region 21 on the drift layer 2;

[0044] Step 2: forming a barrier layer a on the source region, and etching the barrier layer a and the source region 21 to the drift layer 2 to form left and right insulating regions b, and then oxidizing the left and right insulating regions to form insulating blocks c;

[0045] Step 3, re-forming the barrier layer a, and etching the barrier layer a and the insulating block c to form a first gate insulating region 3 and a second gate insulating region 4, and performing metal deposition on the first gate insulating region 3 and the second gate insulating region 4 to form a first gate metal layer 5 and a second gate metal layer 6;

[0046] Step 4: re-form the barrier layer a, and etch the barrier layer a to form a source metal region d, and perform metal deposition on the source metal region d to form a source metal layer 7;

[0047] Step 5: Remove the barrier layer a to complete the manufacturing process.

[0048] Although the specific implementation methods of the present invention are described above, those skilled in the art should understand that the specific embodiments described are only illustrative and are not intended to limit the scope of the present invention. Equivalent modifications and changes made by those skilled in the art in accordance with the spirit of the present invention should be included in the scope of protection of the claims of the present invention.

Claims

1. A vertical silicon carbide device, characterized in that: include: A silicon carbide substrate, a drift layer, the drift layer being connected to the upper side of the silicon carbide substrate, and a source region being provided in the middle of the drift layer; a first gate insulating region, wherein the bottom of the first gate insulating region is connected to the drift layer, and the right side of the first gate insulating region is connected to the left side of the source region; a second gate insulating region, wherein the bottom of the second gate insulating region is connected to the drift layer, and the left side of the second gate insulating region is connected to the right side of the source region; A first gate metal layer, wherein the first gate metal layer is disposed in the first gate insulating region; a second gate metal layer, wherein the second gate metal layer is disposed in the second gate insulating region; a source metal layer connected to the source region; and a drain metal layer connected to the lower side of the silicon carbide substrate.

2. A vertical silicon carbide device according to claim 1, characterized in that: The thickness of the silicon carbide substrate is 10-100 nm.

3. A vertical silicon carbide device according to claim 1, characterized in that: The drift layer has a thickness of 1000-5000 nm.

4. A vertical silicon carbide device according to claim 1, characterized in that: The thickness of the source region is 100-300 nm.

5. A vertical silicon carbide device according to claim 1, characterized in that: The thickness of the first gate insulating region is 100-500 nm, the thickness of the second gate insulating region is 100-500 nm, and the thickness of the first gate insulating region and the second gate insulating region are both greater than or equal to the thickness of the source region.