Forging and pressing production line after magnesium-aluminum alloy hub casting
By employing a production method that combines casting and forging, and utilizing an inert gas-protected magnesium-aluminum alloy wheel production line, the problems of raw material waste and high energy consumption in magnesium-aluminum alloy wheel production have been solved, achieving efficient and low-cost wheel manufacturing.
Patent Information
- Application Number
- CN202420306249.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-20
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2034-02-20
AI Technical Summary
The current production of magnesium-aluminum alloy wheels suffers from low raw material utilization and high energy consumption, especially with significant waste generated during the forging pretreatment process.
The production method of casting first and then forging is adopted. The production line consists of equipment such as a preheating feeder, alloy melting furnace, wheel hub casting machine, blank holding furnace, and forging press. Inert gas is used to protect the melting and heat preservation, and the casting blank is directly forged to eliminate defects and improve material utilization.
It improves the quality of magnesium-aluminum alloy wheels, reduces raw material waste and energy consumption, simplifies the production process, increases production efficiency, and reduces costs.
Smart Images

Figure CN221966681U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of automobile wheel hub production and manufacturing, in particular to a magnesium-aluminum alloy wheel hub casting and post-forging production line. Background Art
[0002] With the development of science and technology, the use of automobiles has become more common. As one of the important components of the automobile driving system, the wheel hub is also a safety component with high requirements. It not only bears the weight of the automobile, but also reflects the appearance of the automobile. The integrity and stability of the wheel hub structure are very important for the safe use of the wheel. With the increasing demand for lightweight automobiles, magnesium-aluminum alloy wheels are gradually replacing traditional steel wheels in modern automobile manufacturing and are widely promoted and applied, especially magnesium alloy wheels, which are not only light in weight and high in strength, but also have good damping performance.
[0003] There are two main production methods for magnesium-aluminum alloy wheels: casting and forging. Casting production includes gravity casting, low-pressure casting, extrusion casting, etc., and quality defects such as slag inclusions and pores, subcutaneous pores, air pockets, shrinkage holes, and pinholes are easily generated during casting. Therefore, the current production of magnesium-aluminum alloy wheels is mainly based on forging production. Forging production uses rods as blanks. After the bar blanks are heated to the required forging temperature, the blanks are placed in the forging die of the forging press, and the bar blanks are forged into shape using a forging punch to produce magnesium-aluminum alloy wheels.
[0004] However, the bars required for forging need to be processed before heating. First, the rod heads at both ends of the bar blank need to be sawed off, and then the outer skin on the surface of the bar blank needs to be turned off, which leads to low raw material utilization and high waste. First, when sawing the bar, there will be about 3% loss, plus the sawed off rod heads and turned off outer skin, the whole processing process will waste 30~40% of raw materials. In addition, the heating treatment of the bar blank before forging requires more energy. Utility Model Content
[0005] To sum up, in order to overcome the shortcomings of the prior art problems, the utility model provides a magnesium-aluminum alloy wheel hub casting and then forging production line, which adopts a production method of casting first and then forging to realize the production of magnesium-aluminum alloy wheel hubs, firstly cast a blank of the magnesium-aluminum alloy wheel hub, and the cast blank is forged and formed by a forging machine, thereby realizing the production of the magnesium-aluminum alloy wheel hub, the production method of casting first and then forging, eliminates defects such as pores in the casting product by forging, and improves the quality of the wheel hub. At the same time, the casting production can overcome the problem of raw material waste caused by the processing of bar billets, and the casting and then forging, the temperature of the blank after casting itself is high, and there is no need to heat it, and it can be directly forged for production, thereby reducing energy consumption.
[0006] In order to solve the above technical problems, the technical solution adopted by the utility model is:
[0007] A magnesium-aluminum alloy wheel hub casting and post-forging production line, which includes: a preheating feeder, an alloy melting furnace, a wheel hub casting machine, a No. 1 transfer robot, a blank holding furnace, a No. 2 transfer robot, a forging press, a No. 3 transfer robot, a conveyor belt and an inert gas supply station.
[0008] The preheating feeder is used to preheat the magnesium-aluminum alloy ingots and add the preheated alloy ingots into the alloy melting furnace. The discharge port of the preheating feeder corresponds to the feed port of the alloy melting furnace. An inert gas supply station is arranged on one side of the alloy melting furnace. The inert gas supply station is connected to the inner cavity of the alloy melting furnace and the inner cavity of the solution insulation furnace of the hub casting machine through pipelines. The alloy melting furnace melts the magnesium-aluminum alloy ingots into alloy solution under the protection of the inert gas. The liquid outlet of the alloy melting furnace is connected to the liquid inlet of the solution insulation furnace of the hub casting machine through a liquid transfer pipe. Under the protection of the inert gas, the alloy solution in the alloy melting furnace enters the solution insulation furnace through the liquid transfer pipe. The hub casting machine is used to cast the alloy solution into a hub blank.
[0009] The No. 1 transfer robot is arranged between the discharge tray assembly of the wheel hub casting machine and the feed port of the blank insulation furnace, and is used to transfer the wheel hub blank cast by the wheel hub casting machine to the blank insulation furnace. The blank insulation furnace is used to insulate the wheel hub blank. The No. 2 transfer robot is arranged between the discharge port of the blank insulation furnace and the forging press, and is used to transfer the wheel hub blank insulated in the blank insulation furnace to the forging press. The forging press is used to forge the wheel hub blank. The No. 3 transfer robot is arranged before the forging press and the conveyor belt, and is used to rotate the forged wheel hub onto the conveyor belt. The conveyor belt is used to transport the formed wheel hub to subsequent processing procedures.
[0010] Furthermore, a spraying machine for spraying the cast wheel hub is provided on one side of the forging machine.
[0011] Furthermore, the wheel hub casting machine is a low-pressure casting machine, comprising a casting frame, a casting upper platen, a casting lower platen, a wheel hub casting mold and a solution insulation furnace.
[0012] The middle part of the casting frame is provided with a casting lower platen, on which a wheel hub casting mold and a horizontal power device for opening and closing the wheel hub casting side mold are provided. The upper part of the casting frame is provided with a casting upper platen, on which an upper and lower power device for opening and closing the wheel hub casting upper mold is provided.
[0013] A hollow mold cavity is provided in the wheel hub casting mold, a pouring hole connected to the mold cavity is provided at the bottom of the wheel hub casting mold, a solution insulation furnace is arranged in the frame below the casting lower platen, the liquid inlet of the solution insulation furnace is connected to the liquid outlet of the alloy melting furnace through a liquid transfer pipe, a liquid rising port is provided on the solution insulation furnace, the liquid rising port is connected to the pouring hole, low-pressure inert gas is introduced into the solution insulation furnace through an inert gas supply station, and under the action of pressure, the alloy solution in the solution insulation furnace enters the mold cavity in the wheel hub casting mold through the liquid rising port and the pouring hole under the protection of the inert gas.
[0014] Furthermore, a discharging tray assembly for receiving and discharging the wheel hub blank after casting is arranged on the frame between the casting upper platen and the casting lower platen.
[0015] Furthermore, the wheel hub casting mold comprises a wheel hub casting bottom mold, a wheel hub casting upper mold and a wheel hub casting side mold, the wheel hub casting bottom mold, the wheel hub casting upper mold and the wheel hub casting side mold are surrounded to form a wheel hub casting mold, the pouring hole is arranged on the wheel hub casting bottom mold, and the wheel hub casting bottom mold is relatively fixedly arranged on the casting lower platen.
[0016] The wheel hub casting side mold is located on the casting lower platen. The wheel hub casting side mold is composed of at least two casting sub-molds. Each casting sub-mold is connected to a horizontal power device that can push the casting sub-mold to move horizontally. The horizontal power device drives the casting sub-mold to move horizontally to realize the opening and closing of the wheel hub casting sub-mold.
[0017] The wheel hub casting upper mold is connected to the upper and lower power devices, and the upper and lower power devices drive the wheel hub casting upper mold to move up and down to realize the opening and closing of the wheel hub casting upper mold.
[0018] Furthermore, the wheel hub casting bottom mold, the wheel hub casting upper mold and the wheel hub casting side mold are all provided with cooling water circulation pipelines for cooling the wheel hub blank.
[0019] Furthermore, the forging machine includes a forging frame, a forging workbench, a forging fixed plate, a forging moving block, a forging bottom die, a forging forming die, a forging die core, a flanging punch and a forging clamping sleeve.
[0020] A forging workbench is arranged in the middle of the forging machine frame, the forging bottom die is pressed onto the forging workbench through a bottom die pressing plate, a forging forming die and a side oil cylinder are arranged on the bottom die pressing plate, the forging forming die is arranged around the forging bottom die, the forging bottom die penetrates into the inner cavity of the forging forming die from the lower end of the forging forming die, the forging forming die is composed of at least two forging sub-dies, each of which is connected to a side oil cylinder capable of driving the forging sub-dies to move horizontally, a forging fixing plate is arranged on the upper part of the forging machine frame, a vertically arranged forging guide column is arranged between the forging workbench and the forging fixing plate, a forging moving block capable of moving up and down along the forging guide column is arranged on the forging guide column, the forging moving block is fastened to the telescopic rod of the forging main oil cylinder, the forging main oil cylinder is fastened to the forging fixing plate,
[0021] The lower end of the forging moving block is fastened with the forging upper template, a forging die core is arranged in the middle of the forging upper template, the forging die core is pressed onto the forging moving block through the forging upper template, a flanging cylinder is arranged on the forging moving block, the telescopic rod of the flanging cylinder passes through the forging upper template and is connected with the flanging punch below the forging upper template, a through hole is arranged in the flanging punch, the forging die core passes through the through hole of the flanging punch, a forging clamping cylinder is arranged on the forging upper template, a forging clamping sleeve is connected to the telescopic rod of the forging clamping cylinder, the forging clamping sleeve corresponds to the forging forming die, when the forging clamping sleeve is mounted outside the forging forming die, the forging clamping sleeve clamps the forging forming die from the outside to the inside.
[0022] Furthermore, an ejector cylinder is arranged on the forging machine frame below the forging workbench, and a telescopic rod of the ejector cylinder is connected to an ejector rod arranged in the forging bottom die.
[0023] Furthermore, the inner hole of the forging clamping sleeve is a tapered hole, and the shape of the forging forming die is a cone that is small at the top and large at the bottom. Driven by the forging clamping cylinder, the forging clamping sleeve is mounted on the outside of the forging forming die from top to bottom, and the tapered hole in the forging clamping sleeve clamps the forging forming die from outside to inside.
[0024] Furthermore, the lower end of the forging upper template is hoisted and connected to the forging middle template via a demoulding rod, a through hole is provided in the forging middle template, the forging clamping sleeve is interference fit with the through hole, and the forging clamping sleeve and the forging middle template are fastened and connected by bolts.
[0025] The beneficial effects of the utility model are:
[0026] 1. The utility model realizes the production of magnesium-aluminum alloy wheel hubs by a production method of first casting and then forging. A blank of the magnesium-aluminum alloy wheel hub is first cast, and the cast blank is forged by a forging press, thereby realizing the production of the magnesium-aluminum alloy wheel hub. The production method of first casting and then forging can eliminate defects such as pores in the casting product by forging, thereby improving the quality of the wheel hub. At the same time, the casting production can overcome the problem of waste of raw materials caused by the processing of bar blanks. After casting and forging, the temperature of the blank after casting is high, and there is no need to heat it, and it can be directly forged, thereby reducing energy consumption.
[0027] 2. The utility model provides inert gas to the alloy melting furnace and the solution insulation furnace of the wheel hub casting machine through an inert gas supply station, so that the magnesium-aluminum alloy is melted under the protection of the inert gas, and the molten alloy solution enters the solution insulation furnace under the protection of the inert gas. The protection of the inert gas can prevent the alloy from being oxidized.
[0028] 3. The production line of the utility model has a simple structure, is easy to use, improves the production efficiency of the wheel hub, reduces the production cost, and can mass-produce wheel hubs with good performance. In addition, the cast wheel hub blank can directly cast the wheel hub pattern, while the traditional bar forging production wheel hub cannot forge the pattern. Therefore, compared with the traditional forging production wheel hub, the utility model can reduce the material waste caused by further processing the wheel hub pattern after forging. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] Figure 1 It is a schematic diagram of the structure of the utility model;
[0030] Figure 2 It is a schematic diagram of the top view structure of the utility model;
[0031] Figure 3 It is a structural schematic diagram of a wheel hub casting machine of the utility model;
[0032] Figure 4 For the utility model Figure 3 A right view structural diagram of ;
[0033] Figure 5 It is a structural schematic diagram of the forging machine of the utility model. DETAILED DESCRIPTION
[0034] The utility model is further described in detail below in conjunction with the accompanying drawings.
[0035] like Figure 1 , Figure 2As shown, a magnesium-aluminum alloy wheel hub casting and forging production line, which includes: a preheating feeder 1, an alloy melting furnace 2, a wheel hub casting machine 3, a No. 1 transfer robot 4, a blank insulation furnace 5, a No. 2 transfer robot 6, a forging press 7, a No. 3 transfer robot 8, a conveyor belt 9 and an inert gas supply station 10, wherein the preheating feeder 1 is used to preheat the magnesium-aluminum alloy ingot and add the preheated alloy ingot into the alloy melting furnace 2, the discharge port of the preheating feeder 1 corresponds to the feed port of the alloy melting furnace 2, an inert gas supply station 10 is arranged on one side of the alloy melting furnace 2, the inert gas supply station 10 is connected to the inner cavity of the alloy melting furnace 2 and the inner cavity of the solution insulation furnace 34 of the wheel hub casting machine 3 through pipelines, the alloy melting furnace 2 melts the magnesium-aluminum alloy ingot into an alloy solution under the protection of the inert gas, and the liquid outlet of the alloy melting furnace 2 is connected to the inner cavity of the alloy melting furnace 2 and the solution insulation furnace 34 of the wheel hub casting machine 3 through pipelines, the alloy melting furnace 2 melts the magnesium-aluminum alloy ingot into an alloy solution under the protection of the inert gas, and the liquid outlet of the alloy melting furnace 2 is connected to the inner cavity of the alloy melting furnace 2 and the solution insulation furnace 34 of the wheel hub casting machine 3 through pipelines, The liquid transfer pipe is connected to the liquid inlet of the solution insulation furnace 34 of the hub casting machine 3. Under the protection of inert gas, the alloy solution in the alloy melting furnace 2 enters the solution insulation furnace 34 through the liquid transfer pipe. The hub casting machine 3 is used to cast the alloy solution into a hub blank. The No. 1 transfer robot 4 is arranged between the discharge tray assembly 37 of the hub casting machine 3 and the feed port of the blank insulation furnace 5, and is used to transfer the hub blank cast by the hub casting machine 3 to the blank insulation furnace 5. The blank insulation furnace 5 is used to insulate the hub blank. The No. 2 transfer robot 6 is arranged between the discharge port of the blank insulation furnace 5 and the forging press 7, and is used to transfer the hub blank insulated in the blank insulation furnace 5 to the forging press 7. The forging press 7 is used to forge the hub blank. A sprayer 11 for spraying the cast hub is provided on one side of the forging press 7. The No. 3 transfer robot 8 is arranged before the forging machine 7 and the conveyor belt 9, and is used to rotate the forged wheel hub onto the conveyor belt 9. The conveyor belt 9 is used to transport the formed wheel hub to the subsequent processing procedure.
[0036] like Figure 3 , Figure 4As shown, the wheel hub casting machine 3 includes a casting frame 31, a casting upper platen 32, a casting lower platen 33, a wheel hub casting mold 38 and a solution insulation furnace 34. The middle part of the casting frame 31 is provided with a casting lower platen 33, and the casting lower platen 33 is provided with a wheel hub casting mold 38 and a horizontal power device 35 for opening and closing the wheel hub casting side mold 383. The upper part of the casting frame 31 is provided with a casting upper platen 32, and the casting upper platen 32 is provided with an upper and lower power device 36 for opening and closing the wheel hub casting upper mold 382. The wheel hub casting mold 38 is provided with The mold cavity has a hollow structure. The bottom of the wheel hub casting mold 38 is provided with a pouring hole connected to the mold cavity. A solution insulation furnace 34 is arranged in the frame below the casting lower platen 33. The liquid inlet of the solution insulation furnace 34 is connected to the liquid outlet of the alloy melting furnace 2 through a liquid transfer pipe. The solution insulation furnace 34 is provided with a liquid riser, which is connected to the pouring hole. By introducing low-pressure inert gas into the solution insulation furnace 34, the alloy solution in the solution insulation furnace 34 enters the mold cavity in the wheel hub casting mold 38 through the liquid riser and the pouring hole under the protection of the inert gas under pressure. A discharge tray assembly 37 for receiving and outputting the cast wheel hub blank is provided on the frame between the casting upper platen 32 and the casting lower platen 33.
[0037] The hub casting mold 38 includes a hub casting bottom mold 381, a hub casting upper mold 382 and a hub casting side mold 383. The hub casting bottom mold 381, the hub casting upper mold 382 and the hub casting side mold 383 are arranged to form the hub casting mold 38. The pouring hole is arranged on the hub casting bottom mold 381. The hub casting bottom mold 381 is relatively fixedly arranged on the casting lower platen 33. The hub casting side mold 383 is located on the casting lower platen 33. The hub casting side mold 383 is composed of at least two casting sub-molds. Each casting sub-mold is connected to a horizontal power device 35 that can push the casting sub-mold to move horizontally. The horizontal power device 35 drives the casting sub-mold to move horizontally to realize the opening and closing of the hub casting sub-mold. The hub casting upper mold 382 is connected to the upper and lower power devices 36. The upper and lower power devices 36 drive the hub casting upper mold 382 to move up and down to realize the opening and closing of the hub casting upper mold 382. The hub casting bottom mold 381, the hub casting upper mold 382 and the hub casting side mold 383 are all provided with cooling water circulation pipelines for cooling the hub blank.
[0038] like Figure 5As shown, the forging machine 7 includes a forging frame 71, a forging workbench 72, a forging fixed plate 73, a forging moving block 74, a forging bottom die 75, a forging forming die 76, a forging die core 77, a flanging punch 78 and a forging clamping sleeve 79. The forging workbench 72 is arranged in the middle of the forging frame 71. The forging bottom die 75 is pressed on the forging workbench 72 through a bottom die pressing plate 710. The bottom die pressing plate 710 is provided with There are a forging die 76 and a side oil cylinder 711. The forging die 76 is arranged around the forging bottom die 75. The forging bottom die 75 penetrates into the inner cavity of the forging die 76 from the lower end of the forging bottom die 76. A positioning groove is arranged on the outer circumference of the forging bottom die 75, and a positioning block is arranged on the inner wall of the forging die 76. The positioning block and the positioning groove cooperate with each other to realize the positioning of the forging bottom die 75 and the forging die 76. The forging forming die 76 is composed of two forging sub-dies, each of which is connected to a side cylinder 711 capable of driving the forging sub-dies to move horizontally. A forging fixed plate 73 is provided on the upper part of the forging frame 71, and a vertically arranged forging guide column 712 is provided between the forging workbench 72 and the forging fixed plate 73. A forging moving block 74 capable of moving up and down along the forging guide column 712 is provided on the forging guide column 712. The forging moving block 74 is fastened to the telescopic rod of the forging main oil cylinder 713, and the forging main oil cylinder 713 is fastened to the forging fixed plate 73. The lower end of the forging moving block 74 is fastened to the forging upper template 714, and a forging die core 77 is provided in the middle of the forging upper template 714. The forging die core 77 is press-fitted on the forging moving block 7 through the forging upper template 714. 4, a flanging cylinder 715 is provided on the forging moving block 74, and the telescopic rod of the flanging cylinder 715 passes through the forging upper template 714 and is connected to the flanging punch 78 below the forging upper template 714, a through hole is provided in the flanging punch 78, and the forging die core 77 passes through the through hole of the flanging punch 78, and a forging clamping cylinder 716 is provided on the forging upper template 714, and a forging clamping sleeve 79 is connected to the telescopic rod of the forging clamping cylinder 716, and the forging clamping sleeve 79 corresponds to the forging forming die 76, and the lower end of the forging upper template 714 is hoisted and connected to the forging middle template 719 through a demoulding pull rod 718, and the forging middle template 719 is provided with a through hole, and the forging clamping sleeve 79 is interference fit with the through hole, and the forging clamping sleeve 79 is fastened to the forging middle template 719 by bolts. The inner hole of the forging clamping sleeve 79 is a tapered hole, and the shape of the forging forming die 76 is a cone that is small at the top and large at the bottom. Driven by the forging clamping cylinder 716, the forging clamping sleeve 79 is mounted on the outside of the forging forming die 76 from top to bottom, and the tapered hole in the forging clamping sleeve 79 clamps the forging forming die 76 from the outside to the inside.An ejector cylinder 717 is provided on the forging machine frame 71 below the forging workbench 72 , and a telescopic rod of the ejector cylinder 717 is connected to a ejector rod provided in the forging bottom die 75 .
[0039] This embodiment takes the production of magnesium alloy wheel hub as an example. When in use, the inert gas supply station 10 is started, and the inert gas supply station 10 introduces inert gas into the alloy melting furnace 2 and the insulation furnace 34 of the casting machine, and the magnesium alloy ingot or aluminum alloy ingot is placed in the preheating feeder 1, and the preheating feeder 1 is started. The preheating feeder 1 preheats the magnesium alloy ingot or aluminum alloy ingot at a preheating temperature of 150-200°C, and the preheated magnesium alloy ingot is added to the alloy melting furnace 2, and the alloy melting furnace 2 is started. Under the protection of the inert gas, the magnesium alloy ingot in the alloy melting furnace 2 is heated to melt it into a magnesium alloy solution, and the melting temperature of the magnesium alloy ingot is 630-720°C; then, under the protection of the inert gas, the magnesium alloy solution in the alloy melting furnace 2 enters along the liquid transfer pipe. In the solution insulation furnace 34 of the hub casting machine 3, the upper and lower power devices 36 and the horizontal power device 35 of the hub casting machine 3 are started to close the hub casting mold 38, and then, an inert gas with a pressure of 0.05~0.3Mpa is delivered to the solution insulation furnace 34 through the inert gas supply station 10. Under the action of the pressurized inert gas, the alloy solution in the solution insulation furnace 34 enters the mold cavity, and under the action of the cooling water circulating in the cooling water circulation pipeline of the hub casting machine 3, the magnesium alloy solution is cooled and solidified into a magnesium alloy hub blank. The upper and lower power devices 36 and the horizontal power device 35 are started again, the hub casting mold 38 is opened and the hub blank is moved to the discharge tray assembly 37, and the casting of the magnesium alloy hub blank is completed.
[0040] Start the No. 1 transfer robot 4, which transfers the wheel hub blank on the discharge tray assembly 37 of the wheel hub casting machine 3 to the blank insulation furnace 5. In the blank insulation furnace 5, the wheel hub blank moves from the feed port to the discharge port of the blank insulation furnace 5. Start the No. 2 transfer robot 6, which rotates the wheel hub blank in the blank insulation furnace 5 to the forging forming die 76 of the forging press 7. Start the side oil cylinder 711 of the forging press 7, which drives the two forging parting dies to close from the outside to the inside. The forging die 76 is formed, and the forging clamping cylinder 716 is started. The telescopic rod of the forging clamping cylinder 716 drives the forging clamping sleeve 79 to be mounted on the outside of the forging die 76 from top to bottom. The forging clamping sleeve 79 clamps the forging die 76, thereby clamping the cast wheel hub blank. The forging main cylinder 713 is started, and the telescopic rod of the forging main cylinder 713 pushes the forging moving block 74 to move downward along the forging guide column 712. The forging die core 77 forges the wheel hub blank located in the forging die 76, thereby forging the wheel hub. Start the flanging cylinder 715, which pushes the flanging punch 78 to move downward, and extrude and flange the forged wheel hub. Start the forging main cylinder 713 again, and the telescopic rod of the forging main cylinder 713 retracts, driving the forging moving block 74 to move upward along the forging guide column 712, so that the forging die core 77 and the flanging punch 78 move upward. After they move upward for a distance, under the action of the demoulding pull rod 718, the forging middle template 719 and the forging clamping sleeve 79 move upward, so that the forging clamping sleeve 79 is separated from the forging forming die 76; start the side cylinder 711, and the telescopic rod of the side cylinder 711 drives the forging parting die to move from the inside to the outside, so that the forging forming die 76 is opened from the inside to the outside. Start the ejection cylinder 717, and the ejection cylinder 717 pushes the ejector rod to eject the forged magnesium alloy wheel hub upward. The No. 3 transfer robot 8 is started, and the No. 3 transfer robot 8 transfers the forged magnesium alloy wheel hub to the conveyor belt 9, and the formed magnesium alloy wheel hub is transported to the next process by the conveyor belt 9.
[0041] The utility model can design the forging die of the forging forming die 76 into a forging lower die and a forging upper die arranged up and down, and the forging upper die is fastened to the upper end of the forging lower die by bolts. When it is necessary to process wheels of the same diameter but different widths, it is only necessary to remove the forging upper die from the upper end of the forging lower die and replace the forging upper die of the corresponding width, without changing the forging lower die 18 and other parts of the forging press 7, and the operation is simple, convenient and fast.
[0042] It should be noted that the above embodiments are illustrative of the technical solution of the utility model rather than limiting. Equivalent substitutions made by ordinary technicians in the relevant technical field or other modifications made according to the prior art should be included in the scope of rights required by the utility model as long as they do not exceed the idea and scope of the technical solution of the utility model.
Claims
1. A magnesium-aluminum alloy wheel hub casting and forging production line, characterized by: It includes a preheating feeder (1), an alloy melting furnace (2), a wheel hub casting machine (3), a No. 1 transfer robot (4), a blank holding furnace (5), a No. 2 transfer robot (6), a forging press (7), a No. 3 transfer robot (8), a conveyor belt (9) and an inert gas supply station (10). The preheating feeder (1) is used to preheat the magnesium-aluminum alloy ingot and add the preheated alloy ingot into the alloy melting furnace (2). The discharge port of the preheating feeder (1) corresponds to the feed port of the alloy melting furnace (2). An inert gas supply station (10) is provided on one side of the alloy melting furnace (2). The inert gas supply station (10) is connected to the inner cavity of the alloy melting furnace (2) and the inner cavity of the solution insulation furnace (34) of the hub casting machine (3) through pipelines. The alloy melting furnace (2) melts the magnesium-aluminum alloy ingot into an alloy solution under the protection of the inert gas. The liquid outlet of the alloy melting furnace (2) is connected to the liquid inlet of the solution insulation furnace (34) of the hub casting machine (3) through a liquid transfer pipe. Under the protection of the inert gas, the alloy solution in the alloy melting furnace (2) enters the solution insulation furnace (34) through the liquid transfer pipe. The hub casting machine (3) is used to cast the alloy solution into a hub blank. The first transfer robot (4) is arranged between the discharge tray assembly (37) of the wheel hub casting machine (3) and the feed port of the blank insulation furnace (5), and is used to transfer the wheel hub blank cast by the wheel hub casting machine (3) to the blank insulation furnace (5), and the blank insulation furnace (5) is used to keep the wheel hub blank warm. The second transfer robot (6) is arranged between the discharge port of the blank insulation furnace (5) and the forging press (7), and is used to transfer the wheel hub blank kept warm in the blank insulation furnace (5) to the forging press (7), and the forging press (7) is used to forge the wheel hub blank. The third transfer robot (8) is arranged between the forging press (7) and the conveyor belt (9), and is used to rotate the forged wheel hub onto the conveyor belt (9), and the conveyor belt (9) is used to transport the formed wheel hub to a subsequent processing procedure.
2. The magnesium-aluminum alloy wheel hub post-casting forging production line according to claim 1, characterized in that: The wheel hub casting machine (3) is a low-pressure casting machine, comprising a casting frame (31), a casting upper platen (32), a casting lower platen (33), a wheel hub casting mold (38) and a solution holding furnace (34). A casting lower platen (33) is disposed in the middle of the casting frame (31), and a wheel hub casting mold (38) and a horizontal power device (35) for opening and closing the wheel hub casting side mold (383) are disposed on the casting lower platen (33); a casting upper platen (32) is disposed on the upper part of the casting frame (31), and an upper and lower power device (36) for opening and closing the wheel hub casting upper mold (382) is disposed on the casting upper platen (32). The wheel hub casting mold (38) is provided with a mold cavity with a hollow structure, and the bottom of the wheel hub casting mold (38) is provided with a pouring hole connected to the mold cavity. A solution insulation furnace (34) is arranged in the frame below the casting lower platen (33), and the liquid inlet of the solution insulation furnace (34) is connected to the liquid outlet of the alloy melting furnace (2) through a liquid transfer pipe. The solution insulation furnace (34) is provided with a liquid riser, and the liquid riser is connected to the pouring hole. Low-pressure inert gas is introduced into the solution insulation furnace (34) through an inert gas supply station (10). Under the action of pressure, the alloy solution in the solution insulation furnace (34) enters the mold cavity in the wheel hub casting mold (38) through the liquid riser and the pouring hole under the protection of the inert gas.
3. The magnesium-aluminum alloy wheel hub post-casting forging production line according to claim 2 is characterized in that: A discharging tray assembly (37) for receiving and discharging the wheel hub blank after casting is arranged on the frame between the casting upper platen (32) and the casting lower platen (33).
4. The magnesium-aluminum alloy wheel hub post-casting forging production line according to claim 2, characterized in that: The wheel hub casting mold (38) comprises a wheel hub casting bottom mold (381), a wheel hub casting upper mold (382) and a wheel hub casting side mold (383); the wheel hub casting bottom mold (381), the wheel hub casting upper mold (382) and the wheel hub casting side mold (383) are arranged to form the wheel hub casting mold (38); the pouring hole is arranged on the wheel hub casting bottom mold (381); the wheel hub casting bottom mold (381) is relatively fixedly arranged on the casting lower platen (33); The wheel hub casting side mold (383) is located on the casting lower platen (33). The wheel hub casting side mold (383) is composed of at least two casting sub-molds. Each casting sub-mold is connected to a horizontal power device (35) capable of driving the casting sub-mold to move horizontally. The horizontal power device (35) drives the casting sub-mold to move horizontally, thereby realizing the opening and closing of the wheel hub casting sub-mold. The wheel hub casting upper mold (382) is connected to the upper and lower power devices (36), and the upper and lower power devices (36) drive the wheel hub casting upper mold (382) to move up and down, thereby realizing the opening and closing of the wheel hub casting upper mold (382).
5. The magnesium-aluminum alloy wheel hub post-casting forging production line according to claim 4, characterized in that: The wheel hub casting bottom mold (381), the wheel hub casting upper mold (382) and the wheel hub casting side mold (383) are all provided with cooling water circulation pipelines for cooling the wheel hub blank.
6. The magnesium-aluminum alloy wheel hub post-casting forging production line according to claim 1, characterized in that: The forging machine (7) comprises a forging frame (71), a forging workbench (72), a forging fixed plate (73), a forging moving block (74), a forging bottom die (75), a forging forming die (76), a forging die core (77), a flanging punch (78) and a forging clamping sleeve (79). A forging workbench (72) is arranged in the middle of the forging machine frame (71), the forging bottom die (75) is press-fitted onto the forging workbench (72) via a bottom die pressing plate (710), a forging forming die (76) and a side oil cylinder (711) are arranged on the bottom die pressing plate (710), the forging forming die (76) is arranged around the forging bottom die (75), the forging bottom die (75) penetrates into the inner cavity of the forging forming die (76) from the lower end of the forging forming die (76), and the forging forming die (76) is composed of at least two forging sub-dies. Each forging die is connected to a side oil cylinder (711) capable of driving the forging die to move horizontally; a forging fixed plate (73) is provided on the upper part of the forging frame (71); a vertically arranged forging guide column (712) is provided between the forging workbench (72) and the forging fixed plate (73); a forging moving block (74) capable of moving up and down along the forging guide column (712) is provided on the forging guide column (712); the forging moving block (74) is tightly connected to the telescopic rod of the forging main oil cylinder (713); The main oil cylinder (713) is fastened to the forging fixed plate (73); the lower end of the forging moving block (74) is fastened to the forging upper template (714); a forging die core (77) is arranged in the middle of the forging upper template (714); the forging die core (77) is press-fitted onto the forging moving block (74) through the forging upper template (714); a flanging oil cylinder (715) is arranged on the forging moving block (74); a telescopic rod of the flanging oil cylinder (715) passes through the forging upper template (714) and a flanging punch below the forging upper template (714); (78) is connected, the flanging punch (78) is provided with a through hole, the forging die core (77) passes through the through hole of the flanging punch (78), the forging upper template (714) is provided with a forging clamping cylinder (716), the telescopic rod of the forging clamping cylinder (716) is connected with a forging clamping sleeve (79), the forging clamping sleeve (79) corresponds to the forging forming die (76), when the forging clamping sleeve (79) is sleeved outside the forging forming die (76), the forging clamping sleeve (79) clamps the forging forming die (76) from the outside to the inside.
7. The magnesium-aluminum alloy wheel hub post-casting forging production line according to claim 6, characterized in that: An ejector cylinder (717) is provided on the forging machine frame (71) below the forging workbench (72), and a telescopic rod of the ejector cylinder (717) is connected to a ejector rod provided in the forging bottom die (75).
8. The magnesium-aluminum alloy wheel hub post-casting forging production line according to claim 6, characterized in that: The inner hole of the forging clamping sleeve (79) is a tapered hole, and the shape of the forging forming die (76) is a tapered hole with a small top and a large bottom. The forging clamping sleeve (79) is driven by the forging clamping cylinder (716) to be sleeved on the outside of the forging forming die (76) from top to bottom, and the tapered hole in the forging clamping sleeve (79) clamps the forging forming die (76) from outside to inside.
9. The magnesium-aluminum alloy wheel hub post-casting forging production line according to claim 6, characterized in that: The lower end of the forging upper template (714) is hoisted and connected to the forging middle template (719) via a demoulding rod (718); a through hole is provided in the forging middle template (719); the forging clamping sleeve (79) is interference fit with the through hole, and the forging clamping sleeve (79) and the forging middle template (719) are fastened and connected by bolts.
10. The magnesium-aluminum alloy wheel hub post-casting forging production line according to claim 1, characterized in that: A spraying machine (11) for spraying the cast wheel hub is provided on one side of the forging machine (7).
Citation Information
Cited By
Magnesium-aluminum alloy hub production line and production process thereof
CN118122925A
Full-automatic high-pressure casting assembly line for hubs
CN122142285A