Anti-cracking crucible and evaporation equipment
By adopting an elliptical arc-shaped transition area and gradually increasing thickness design at the junction of the bottom wall and the side wall of the crucible, the cracking problem caused by the concentration of the crucible is solved, the structural strength and use range are improved, and the consumption cost is reduced.
Patent Information
- Application Number
- CN202420473702.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-12
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2034-03-12
AI Technical Summary
The transition design of the bottom and wall corners of the existing crucible leads to stress concentration, resulting in the crucible being prone to rupture during the evaporation and cooling process.
The junction of the bottom wall and the side wall of the crucible adopts an elliptical arc-shaped transition area. The length and diameter of the ellipse are parallel to the side wall, the short diameter is parallel to the bottom wall, the ratio of the length and diameter to the short diameter is 2.5 to 3.5, and the thickness of the bottom wall is Gradually increase from the center to the edge, increasing the flange to enhance strength.
Effectively alleviate the problem of stress concentration, improve the structural strength of the crucible, reduce the cracking and breakage rate, is suitable for evaporation of more materials, reduce the cost of crucible consumption, and improve the utilization rate of equipment.
Smart Images

Figure CN222008001U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of vacuum coating, in particular to an anti-cracking crucible and evaporation equipment. Background Art
[0002] During the evaporation process, a crucible is used as a heating carrier for the evaporation material. The transition design between the bottom and the wall of the crucible is usually an inner fillet transition. The materials commonly used to make crucibles have high high temperature resistance and thermal shock resistance. However, due to different uses and functions, the thermal expansion coefficient of the evaporation material is quite different from that of the crucible material. For example, the expansion coefficient of common metals and crucible materials differs by an order of magnitude, resulting in large temperature changes between the crucible and the evaporation material during the evaporation heating and cooling process, generating thermal stress that causes the crucible to be damaged by tensile stress or shear force.
[0003] Research has shown that when the rounded corner transition is subjected to tension, a high stress concentration is generated at a certain position at the midpoint of the rounded corner transition structure. Numerical analysis shows that its stress concentration coefficient is as high as 1.9. When there is a huge difference between the strength of the crucible material and the strength and thermal expansion coefficient of the evaporated material in the solid state, the crucible is very likely to be broken and damaged due to thermal stress. Utility Model Content
[0004] In view of this, the purpose of the embodiments of the utility model is to provide a crack-resistant crucible and evaporation equipment to solve the technical problem of the prior art that the stress concentration coefficient is high due to the transition between the rounded corners of the bottom and the wall of the crucible, which leads to the cracking of the crucible.
[0005] In order to achieve the above objectives, in a first aspect, an embodiment of the utility model provides an anti-breakage crucible, the crucible comprising a bottom wall and a side wall, wherein a transition area at the intersection of the bottom wall and the side wall is in an elliptical arc shape.
[0006] In some possible implementations, the transition area is a quarter arc of an ellipse.
[0007] In some possible implementations, the major diameter of the ellipse is parallel to the side wall, and the minor diameter of the ellipse is parallel to the bottom wall.
[0008] In some possible implementations, a ratio of the major diameter of the ellipse to the minor diameter of the ellipse is 2.5 to 3.5.
[0009] In some possible implementations, the ratio of the major diameter of the ellipse to the minor diameter of the ellipse is 3.
[0010] In some possible implementations, the crucible is cylindrical.
[0011] In some possible implementations, the mouth of the crucible has a flange.
[0012] In some possible implementations, the length of the flange is 1 mm to 4 mm.
[0013] In some possible implementations, the thickness of the bottom wall gradually increases from the center to the edge.
[0014] In a second aspect, an embodiment of the utility model provides an evaporation device, the evaporation device comprising:
[0015] A vacuum evaporation chamber, and an unwinding roller, a winding roller and the anti-breakage crucible according to any one of the first aspects arranged in the vacuum evaporation chamber;
[0016] The unwinding roller and the winding roller are used to guide the film;
[0017] The crucible is located below the film and is used to heat the evaporation material and deposit the gas layer with the evaporation material on the film.
[0018] The beneficial technical effects of the above technical solution are:
[0019] The utility model provides an anti-crack crucible and evaporation equipment, the crucible includes a bottom wall and a side wall, and the transition area at the intersection of the bottom wall and the side wall is an elliptical arc. This embodiment optimizes the structure of the transition area of the crucible, and designs the original circular transition into an elliptical transition, thereby greatly alleviating the stress concentration problem in the transition area, improving the structural strength of the crucible, and avoiding the cracking of the crucible due to a high stress concentration coefficient. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0021] Figure 1 This is a partial structural schematic diagram of an anti-breakage crucible according to an embodiment of the utility model;
[0022] Figure 2 It is an overall schematic diagram of an anti-breakage crucible according to an embodiment of the utility model;
[0023] Figure 3 It is a structural schematic diagram of a thin film evaporation device according to an embodiment of the utility model.
[0024] Description of Figure Numbers:
[0025] 1. Crucible; 11. Bottom wall; 12. Side wall; C. Transition area; R, major diameter; r, minor diameter; A, flange;
[0026] 2. Evaporation equipment; 20. Vacuum evaporation chamber; 21. Unwinding roller; 22. Winding roller; 23. Guide roller. DETAILED DESCRIPTION
[0027] The features and exemplary embodiments of various aspects of the utility model will be described in detail below. In the detailed description below, many specific details are proposed in order to provide a comprehensive understanding of the utility model. However, it is obvious to those skilled in the art that the utility model can be implemented without the need for some of these specific details. The following description of the embodiment is only to provide a better understanding of the utility model by illustrating an example of the utility model. In the drawings and the following description, at least part of the known structures and technologies are not shown in order to avoid unnecessary ambiguity to the utility model; and, for clarity, the size of some structures may be exaggerated. In addition, the features, structures or characteristics described below may be combined in one or more embodiments in any suitable manner.
[0028] Figure 1 Schematic diagram of the partial structure of an anti-breakage crucible according to an embodiment of the utility model. Figure 1 As shown, the crucible includes a bottom wall 11 and a side wall 12, and the transition area C at the intersection of the bottom wall 11 and the side wall 12 is an elliptical arc. In this embodiment, by optimizing the structure of the transition area C of the crucible, the original circular transition area is designed as an elliptical transition area, thereby greatly alleviating the stress concentration problem in the transition area C, improving the structural strength of the crucible, and avoiding the cracking of the crucible due to a high stress concentration coefficient. That is, the intersection of the bottom wall 11 and the side wall 12 of the anti-crack crucible of this embodiment adopts an elliptical arc design, which enables the crucible to evenly distribute stress when heated, effectively preventing cracking.
[0029] like Figure 1 As shown, in some embodiments, the transition area is a quarter arc of an ellipse. In this embodiment, since the transition area is a quarter arc of an ellipse, the thickness of the wall at the transition area C can be increased, and the stress is evenly distributed in the crucible wall structure by increasing the thickness.
[0030] The inventors have found in actual applications that when the evaporation material is metal, the crucible is prone to cracking and damage at the remaining aluminum position at the bottom after the residual material is left. This embodiment optimizes the structural parameters of the cracking position at the bottom of the crucible through experimental verification and theoretical analysis, alleviates the stress concentration problem, and optimizes the material parameters to improve the overall structural strength of the crucible, thereby reducing or even avoiding the cracking of the crucible within a certain residual material range.
[0031] like Figure 1 As shown, in some embodiments, the long diameter R of the ellipse is parallel to the side wall, and the short diameter r of the ellipse is parallel to the bottom wall. In this embodiment, the long diameter of the ellipse is along the direction of the side wall, so that the transition in the vertical stress direction is smoother, thereby greatly alleviating the stress concentration problem in the transition area, improving the structural strength of the crucible, and making it suitable for the evaporation of more materials.
[0032] In some embodiments, the ratio of the long diameter of the ellipse to the short diameter of the ellipse is 2.5 to 3.5. Optionally, the ratio of the long diameter R of the ellipse to the short diameter r of the ellipse is 3. In this case, it is possible to save evaporation materials and energy costs, stop heating after the process is completed, and greatly reduce the cracking and breakage rate of the crucible, thereby reducing the crucible consumption cost.
[0033] Figure 2 : is an overall schematic diagram of an anti-breakage crucible according to an embodiment of the utility model, such as Figure 2 As shown, in some embodiments, the overall shape of the crucible is cylindrical.
[0034] like Figure 2 As shown, in some embodiments, the mouth of the crucible has a flange A, and the length of the flange A is 1 mm to 4 mm to enhance the strength of the edge of the crucible.
[0035] like Figure 2 As shown, in some embodiments, the thickness of the bottom wall 11 gradually increases from the center to the edge. The distribution that the bottom center is thinner and the edge gradually thickens can optimize stress distribution and strengthen the crucible structure.
[0036] In actual application, the inventors found through extensive research that the structural material of the crucible is subjected to tension when the internal evaporated material is heated. When the vertical wall and the bottom of the crucible transition, there is a large stress in the transition area. The conventional transition method is a rounded corner transition, which is mostly considered from the convenience of processing technology, and the influence of structural strength is not considered. There is a large stress concentration problem in the rounded corner area, which leads to damage of the crucible. The utility model optimizes the transition contour curve, changes the inner rounded corner transition to an elliptical transition, and thickens the regional structural dimensions. The transition in the vertical stress direction is smoother, thereby greatly alleviating the stress concentration problem in the transition area and improving the structural strength of the crucible.
[0037] Figure 3 Schematic diagram of the structure of a thin film evaporation device according to an embodiment of the utility model. Figure 3As shown, the evaporation device includes: a vacuum evaporation chamber 20, and an unwinding roller 21, a winding roller 22 and any of the above-mentioned anti-crack crucibles 1 arranged in the vacuum evaporation chamber 20, and may also include a guide roller 23 and the like for guiding and flattening the film during the film evaporation process. In the evaporation device of the embodiment of the utility model, since the crucible has high strength and is not easy to crack, it can be applied to the evaporation of more materials, improve production efficiency, and improve equipment utilization.
[0038] In the description of the embodiments of the present utility model, it should be noted that the directions or positional relationships indicated by the terms "upper, lower, inner and outer" are based on the directions or positional relationships shown in the drawings, and are only for the convenience of describing the present utility model and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as limiting the present utility model. In addition, the terms "first, second or third" are only used for descriptive purposes and cannot be understood as indicating or implying relative importance.
[0039] In the embodiments of the present invention, unless otherwise clearly specified and limited, the terms "install, connect, connect" should be understood in a broad sense, for example: it can be a fixed connection, a detachable connection or an integral connection; it can also be a mechanical connection, an electrical connection or a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0040] Although the present invention has been described with reference to preferred embodiments, various modifications may be made thereto and parts thereof may be replaced with equivalents without departing from the scope of the present invention. In particular, the various technical features mentioned in the various embodiments may be combined in any manner as long as there is no structural conflict. The present invention is not limited to the specific embodiments disclosed herein, but includes all technical solutions falling within the scope of the claims.
Claims
1. A crack-resistant crucible (1), characterized in that: The crucible comprises a bottom wall (11) and a side wall (12), and a transition area (C) at the intersection of the bottom wall (11) and the side wall (12) is in the shape of an elliptical arc.
2. The anti-breakage crucible according to claim 1, characterized in that: The transition area (C) is a 1 / 4 arc of the ellipse.
3. The anti-breakage crucible according to claim 2, characterized in that: The major diameter (R) of the ellipse is parallel to the side wall (12), and the minor diameter (r) of the ellipse is parallel to the bottom wall (11).
4. The anti-breakage crucible according to claim 2, characterized in that: The ratio of the major diameter (R) of the ellipse to the minor diameter (r) of the ellipse is 2.5 to 3.
5.
5. The anti-breakage crucible according to claim 4, characterized in that: The ratio of the major diameter (R) of the ellipse to the minor diameter (r) of the ellipse is 3.
6. The anti-breakage crucible according to claim 1, characterized in that: The crucible is cylindrical.
7. The anti-breakage crucible according to claim 6, characterized in that: The mouth of the crucible has a flange (A).
8. The anti-breakage crucible according to claim 7, characterized in that: The length of the flange (A) is 1 mm to 4 mm.
9. The anti-breakage crucible according to claim 1, characterized in that: The thickness of the bottom wall (11) gradually increases from the center to the edge.
10. A vapor deposition device (2), characterized in that: The evaporation equipment comprises: a vacuum evaporation chamber (20), and an unwinding roller (21), a winding roller (22) and any one of the anti-breakage crucibles (1) according to claims 1 to 5, which are arranged in the vacuum evaporation chamber (20); The unwinding roller (21) and the winding roller (22) are used to guide the film; The crucible (1) is located below the film and is used to heat the evaporation material and deposit the gas layer containing the evaporation material on the film.