Protective material structure for FHM punching
By spraying and curing the polymer acrylic laser protective film on the surface of the FHM, capturing and removing the drilling residue, the problem of residue contamination during the drilling process of the FHM is solved, the product yield and production efficiency are improved, and the cost is reduced.
Patent Information
- Application Number
- CN202420254805.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-02
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2034-02-02
AI Technical Summary
During the FHM drilling process, the prior art cannot effectively prevent residue contamination and damage, resulting in a decrease in product yield.
A polymer acrylic-based laser protective film was used to cover the surface of the FHM and cured by spraying and forming a film to form a 10 μm thick protective film to capture and remove residues generated during hole punching.
Effectively protect the FHM surface, avoid pollution and scratches, improve product yield, simplify film formation and cleaning operations, and reduce production costs and budgets.
Smart Images

Figure CN222053765U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the field of display technology, and specifically relates to a protective material structure for FHM punching. Background Art
[0002] FHM (Fine Hybrid Mask) is a composite metal mask. PI film is a thin film insulating material, and Invar film is a nickel-iron alloy film. In the existing FHM technology, there are two main structural technologies, namely double-layer structure and three-layer structure. Regardless of the structure, laser drilling is required in the end. However, when using laser drilling, a lot of residues will be generated, and these residues will also cause major pollution and defects in the final product, greatly reducing the product yield.
[0003] After searching, the applicant found that the Chinese patent document with publication number CN214352937U disclosed a protective device for a hollow plastic plate punching machine on October 8, 2021, including a connecting support seat and a protective plate, a lifting device is fixed at the middle position of the upper end of the connecting support seat, a punch device is fixed at the middle position of the front end of the lifting device, a slide rail device is fixed at the lower position of the front end of the connecting support seat, a fixed frame is fixed at the lower end of the connecting support seat, a rolling track is fixed at the middle rear position and the front position of the upper end of the fixed frame, a punched plastic plate is placed at the upper end of the rolling track, a protective plate is fixed at the upper position of the front end of the fixed frame, the fixed sleeve is socketed with the connecting sleeve, and the connecting sleeve is socketed in the fixed sleeve.
[0004] The device cannot protect the FHM from being contaminated and damaged by residues when drilling holes. Utility Model Content
[0005] The utility model aims to provide a protective material structure for FHM punching, which can protect the FHM from being polluted and damaged by residues during the FHM punching.
[0006] In order to solve the above technical problems, the technical solution adopted by the present invention is as follows: the present invention comprises an FHM, and protective structures are provided on the surfaces of both sides of the FHM.
[0007] The protection structure includes a protection film, and the protection film covers the FHM.
[0008] As a solution, the FHM includes a PI film; Invar films are provided on both the upper and lower sides of the PI film.
[0009] The protective film is disposed on the surface of the Invar film.
[0010] The protective film is connected to the surface of the Invar film by curing.
[0011] As another solution, the FHM includes a PI film; an Invar film is disposed on one side of the PI film.
[0012] The protective films are respectively arranged on the surfaces of the Invar film and the PI film.
[0013] The protective film is respectively connected to the surfaces of the Invar film and the PI film by curing.
[0014] The protective film is a polymer acrylic laser protective film.
[0015] The thickness of the protective film is 10 μm.
[0016] The beneficial effects of this application are:
[0017] After the FHM is manufactured, a polymer acrylic laser protective liquid is sprayed on the upper and lower sides to form the protective film; the protective film is then heated and cured to firmly connect the protective film to the surface of the FHM; the FHM can then be laser punched, and the residue generated during the punching will fall onto the protective film, and then the protective film and the punching residue are washed away.
[0018] In this way, when the FHM is punched, the FHM product can be protected from being contaminated by residues or scratched on the surface; the specification accuracy of the product is guaranteed, and the product yield is effectively improved; the film formation and cleaning operations of the protective film on the FHM are simple, the operation time is short, and the production efficiency of the staff is effectively improved; the protective film comprehensively protects the surface of the FHM, has a good protective effect, and has no negative effects such as pollution and damage to the FHM; the production cost of the protective film is low, which effectively reduces the production budget and is suitable for popularization and use.
[0019] The protective material structure for punching FHM is provided with protective films arranged on the upper and lower sides of the FHM, which can fully protect the surface of the FHM; when the FHM is punching, the FHM product is effectively prevented from being contaminated by residues or surface scratches and damage; the specification accuracy of the product is guaranteed, and the product yield is effectively improved; the film formation and cleaning operations of the protective film on the FHM are simple, the operation time is short, and the production efficiency of the staff is effectively improved; at the same time, the production cost of the protective film is low, which effectively reduces the production budget and is suitable for comprehensive promotion and use. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] The specific implementation of the utility model is further described in detail below in conjunction with the accompanying drawings, wherein:
[0021] Figure 1This is a schematic diagram of the structure of the protective material for FHM punching.
[0022] Figure 2 This is a schematic diagram of the FHM punching protective material structure after punching.
[0023] Figure 3 This is a schematic diagram of the FHM three-layer structure of the FHM punching protection material structure.
[0024] Figure 4 This is a schematic diagram of the structure of the FHM two-layer structure of the FHM punching protection material structure.
[0025] The marks in the above figure are:
[0026] Marked in the figure: 1. FHM, 2. Protective film, 3. Invar film, 4. PI film. DETAILED DESCRIPTION
[0027] The following is a further detailed explanation of the specific implementation methods of the utility model through the description of the embodiments with reference to the accompanying drawings, with the aim of helping those skilled in the art to have a more complete, accurate and in-depth understanding of the inventive concept and technical solution of the utility model and facilitating its implementation.
[0028] Figure 1 The FHM punching protection material structure shown includes FHM1, and protection structures are provided on both side surfaces of FHM1.
[0029] The protective structure can protect the FHM1 product from being contaminated by residues or scratched and damaged on the surface when the FHM1 is being punched; the specification accuracy of the product is guaranteed and the product yield is effectively improved; the protective structure provides comprehensive protection for the surface of the FHM1 with good protection effect, and at the same time has no negative impact on the FHM1 such as contamination and damage.
[0030] The protective structure includes a protective film 2, which covers the FHM1. The FHM1 is placed on a slit coater, and a polymer acrylic laser protective liquid is used to form a film on the upper and lower surfaces of the FHM1 at a speed of 5um / sec by spraying, and then heated and cured to firmly connect the protective film 2 to the surface of the FHM1; thus, the protective film 2 can provide protection for the FHM1 during the punching operation; the residue generated during the punching will fall onto the protective film 2, and then the FHM1 with the holes is placed in a water washing machine for cleaning at a flow rate of 8L / min, and the protective film 2 and the punching residue can be washed away. The film formation and cleaning operation of the protective film 2 on the FHM1 is simple, the operation time is short, and the production efficiency of the staff is effectively improved.
[0031] As an embodiment, FHM1 includes PI film 4; Invar film 3 is provided on both upper and lower sides of PI film 4. In the existing FHM1 manufacturing technology, FHM1 has a three-layer structure in which Invar film 3 is plated on both upper and lower sides of PI film 4; therefore, when performing laser drilling operation, the three-layer FHM1 needs to protect the Invar film 3 on both sides of PI film 4 to prevent drilling residue from falling onto Invar film 3, causing it to be contaminated or scratched.
[0032] The protective film 2 is arranged on the surface of the Invar film 3. The protective film 2 can provide comprehensive protection for the Invar film 3; when punching, the punching residue will only fall onto the protective film 2 arranged on the surface of the Invar film 3, effectively preventing the Invar film 3 from being contaminated and damaged; when the punching is completed, the protective film 2 and the punching residue are washed off from the Invar film 3 together to obtain a processed product.
[0033] The protective film 2 is connected to the surface of the Invar film 3 by curing. The protective film 2 is formed on the surface of the Invar film 3 by spraying a polymer acrylic laser protection liquid, and then heated at 100 degrees for 10 minutes to heat and cure it, so that the protective film 2 and the surface of the Invar film 3 are tightly connected; the curing speed of heating curing is fast, the finished product has high strength, and it is more suitable for connecting the protective film 2 and the Invar film 3.
[0034] As another embodiment, the FHM1 includes a PI film 4; an Invar film 3 is disposed on one side of the PI film 4. In the existing FHM1 manufacturing technology, the FHM1 has a two-layer structure in which the Invar film 3 is plated on one side of the PI film 4; thus, when the two-layer FHM1 is subjected to laser drilling, the bottom surface of the PI film 4 and the top surface of the Invar film 3 need to be protected to prevent drilling residues from falling onto the Invar film 3 and the PI film 4, causing them to be contaminated or scratched.
[0035] The protective film 2 is respectively arranged on the surface of the Invar film 3 and the PI film 4. The protective film 2 can provide comprehensive protection for the bottom surface of the PI film 4 and the top surface of the Invar film 3; when punching, the punching residue will only fall onto the protective film 2 arranged on the PI film 4 and the Invar film 3, effectively preventing the bottom surface of the PI film 4 and the top surface of the Invar film 3 from being contaminated and damaged; when the punching is completed, the protective film 2 and the punching residue are washed off from the PI film 4 and the Invar film 3 to obtain the processed product.
[0036] The protective film 2 is respectively connected to the surface of the Invar film 3 and the PI film 4 by curing. The protective film 2 is formed on the surface of the Invar film 3 and the PI film 4 by spraying a polymer acrylic laser protection liquid, and then heated at 100 degrees for 10 minutes to heat and cure it, so that the protective film 2 is tightly connected to the surface of the Invar film 3 and the PI film 4; the curing speed of the heat curing is fast, the finished product has high strength, and it is more suitable for connecting the protective film 2 with the Invar film 3 and the PI film 4.
[0037] The protective film 2 is a polymer acrylic laser protective film. The protective film 2 is a polymer acrylic laser protective liquid that is sprayed on the upper and lower surfaces of FHM1, and then heated and cured to form a laser protective film that is firmly connected to the surface of FHM1; the polymer acrylic laser protective film has good hardness and anti-pollution performance; it can protect FHM1 from being polluted and scratched by punching residues, and it will not react with FHM1, preventing FHM1 from being polluted and damaged by the protective film 2.
[0038] The thickness of the protective film 2 is 10 μm. The protective film 2 is set to be 10 μm thick, which can fully protect the FHM 1 from being contaminated and scratched by the punching residue and can also be easily cleaned and removed from the FHM 1.
[0039] The specific working process of the utility model is as follows:
[0040] Place the processed FHM1 on a slit coater, and use a polymer acrylic laser protection liquid to spray on the upper and lower surfaces of the FHM1 at a speed of 5um / sec, with a thickness of about 10um each, and heat it at 100 degrees for 10 minutes to heat and cure it;
[0041] The FHM1 coated with the protective film 2 is placed on a laser punching machine for punching operation;
[0042] The FHM1 with holes punched in it is placed in a water washing machine for cleaning at a flow rate of 8 L / min, the protective film 2 and punching residue are removed, and the final FHM product is completed.
[0043] The above is an exemplary description of the utility model in conjunction with the accompanying drawings. Obviously, the specific implementation of the utility model is not limited to the above-mentioned method. As long as various non-substantial improvements are made using the method concept and technical solution of the utility model; or the above concept and technical solution of the utility model are directly applied to other occasions without improvement, they are all within the protection scope of the utility model.
Claims
1. A protective material structure for FHM punching, characterized in that: The invention comprises a FHM (1), wherein protective structures are arranged on both side surfaces of the FHM (1).
2. The FHM punching protection material structure according to claim 1, characterized in that: The protective structure comprises a protective film (2), and the protective film (2) covers the FHM (1).
3. The FHM punching protection material structure according to claim 2, characterized in that: The FHM (1) comprises a PI film (4); Invar films (3) are provided on both the upper and lower sides of the PI film (4).
4. The FHM punching protection material structure according to claim 3, characterized in that: The protective film (2) is arranged on the surface of the Invar film (3).
5. The FHM punching protection material structure according to claim 4, characterized in that: The protective film (2) is connected to the surface of the Invar film (3) by curing.
6. The FHM punching protection material structure according to claim 2, characterized in that: The FHM (1) comprises a PI film (4); an Invar film (3) is provided on one side of the PI film (4).
7. The FHM punching protection material structure according to claim 6, characterized in that: The protective film (2) is respectively arranged on the surface of the Invar film (3) and the PI film (4).
8. The FHM punching protection material structure according to claim 7, characterized in that: The protective film (2) is respectively connected to the surfaces of the Invar film (3) and the PI film (4) by curing.
9. The FHM punching protection material structure according to any one of claims 2 to 8, characterized in that: The protective film (2) is a polymer acrylic laser protective film.
10. The FHM punching protection material structure according to claim 9, characterized in that: The thickness of the protective film (2) is 10 μm.