Titanium chloride slag smelting device

By designing a titanium chloride slag smelting device, smelting is exothermic by using the raw materials' redox reaction and exothermic heat recovery, the problems of high energy consumption and high pollution in traditional titanium slag smelting methods are solved, and low-cost and low-pollution are achieved High-efficiency titanium chloride slag production.

CN222100102UInactive Publication Date: 2024-12-03BENGBU GUOTAI NANO MATERIALS CO LTD

Patent Information

Application Number
CN202323578444.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-26
Publication Date
2024-12-03
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Traditional titanium slag smelting methods have problems with high energy consumption and high equipment investment costs, especially electric furnace smelting requires a lot of electricity, and the waste acid and waste slag are seriously polluted to the environment.

Method used

A titanium chloride slag smelting device was designed, using the first mixer, the second mixer, the cloth chute and the smelting vertical furnace, and using raw materials by mixing titanium powder with ferrous oxide and ilmenite and coal powder. Their redox reaction exotherms and smels, reduces external energy consumption, and is connected to the waste heat boiler through the flue gas ring pipe, and uses the waste heat to recover energy.

Benefits of technology

The smelting of titanium chloride slag that requires almost no external energy consumption has been achieved, which reduces the cost of equipment investment, increases the grade of titanium slag, reduces pollution, and solves the problems of high energy consumption and environmental pollution in traditional methods.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222100102U_ABST
    Figure CN222100102U_ABST
Patent Text Reader

Abstract

The utility model provides a titanium chloride slag smelting device and aims to solve the problems of high energy consumption and environmental pollution in the conventional titanium slag smelting technology. The device comprises a first material mixer, a second material mixer, a material distribution chute, a smelting shaft furnace and the like. Titanium powder is mixed with ferric oxide, ilmenite is mixed with coal powder, and then raw materials are evenly distributed in a smelting shaft furnace through a material distribution chute. In the smelting process, smelting is conducted through heat released by the oxidation-reduction reaction of the raw materials, energy provided by the outside is not needed, and energy consumption is reduced. High-temperature flue gas is recycled through the waste heat boiler, and energy consumption is reduced. The device has the advantages of low investment cost, small environmental pollution, high energy utilization rate and the like, can improve the grade of titanium slag, and is suitable for large-scale production.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the field of metallurgical engineering, in particular to a titanium chloride slag smelting device. Background Art

[0002] There are three methods for titanium slag smelting: acid leaching, reduction corrosion, and electric furnace smelting. Acid leaching and reduction corrosion will produce waste acid and waste slag, causing environmental pollution. Electric furnace smelting is the main process for titanium slag smelting, which is a high-energy consumption, low-pollution production process. Research and use of raw material pre-reduction and hot charging can only reduce power consumption to a limited extent, and cannot fundamentally solve the problem of high power consumption of electric furnaces.

[0003] Among them, the acid-soluble titanium slag TiO2: 74% ≤ TiO2 ≤ 85%, the chloride titanium slag TiO2: 85% ≤ TiO2 ≤ 92%. As the TiO2 grade increases, a lot of heat is consumed. Titanium slag smelting includes acid leaching, reduction corrosion, and electric furnace smelting. Acid leaching and reduction corrosion will produce waste acid and waste slag, causing environmental pollution. Electric furnace smelting is the main process of titanium slag smelting. In essence, ilmenite is mixed with solid reducing agents and added to the electric furnace for reduction smelting. The iron oxide in the ore is selectively reduced to metallic iron, and the titanium oxide is enriched in the slag. After slag and iron separation, titanium slag and by-product metallic iron are obtained; the large amount of heat required for the reduction reaction is provided by arc heat, which consumes a lot of electricity.

[0004] Titanium chloride slag is an important metallurgical raw material. The traditional smelting method has the problems of low efficiency and high energy consumption. Therefore, it is particularly important to develop an efficient and energy-saving titanium chloride slag smelting method and device.

[0005] The invention with application number CN202111114703.3 provides a method for preparing titanium chloride slag from titanium concentrate, which relates to the field of chemical metallurgy technology. The method mainly comprises obtaining slag by magnetic roasting, ball milling, wet magnetic separation, granulation, and smelting, and the slag is subjected to oxidation roasting and reduction roasting, pressurized acid leaching, and calcination in sequence to obtain titanium chloride slag. The utility model method combines magnetic roasting, desiliconization and decalcification, and titanium chloride slag upgrading technology to prepare a low-calcium and magnesium, high-grade titanium chloride slag product suitable for large-scale boiling chlorination.

[0006] However, the method for preparing titanium chloride slag in the above patent requires energy to be provided from the outside, which consumes a lot of energy and has the disadvantage of high equipment investment cost. Utility Model Content

[0007] The purpose of the utility model is to provide a titanium chloride slag smelting device to solve the problems raised in the above background technology:

[0008] (1) How to provide a device that utilizes the heat released by the redox reaction of the raw materials for smelting, does not require external energy, fundamentally saves energy consumption, and has low equipment investment costs.

[0009] In order to achieve the above purpose, the utility model provides the following technical solutions:

[0010] In order to achieve the above purpose, the utility model also provides the following technical solutions:

[0011] A titanium chloride slag smelting device;

[0012] It includes a first mixer, a second mixer, a material distribution chute and a smelting vertical furnace;

[0013] The first mixer is used to mix titanium powder and ferric oxide raw materials, and the second mixer is used to mix ilmenite and pulverized coal raw materials. The outlets of the first mixer and the second mixer are aligned with the inlet of the distribution chute, and the outlet of the distribution chute is aligned with the opening of the smelting vertical furnace. The distribution chute can be used to evenly distribute the raw materials discharged from the first mixer or the second mixer in the smelting vertical furnace. A water-cooled ignition gun is provided at the upper part of the inner cavity of the smelting vertical furnace, a slag outlet for discharging slag and an iron outlet for discharging molten iron are provided at the lower part of the smelting vertical furnace, a flue gas ring pipe communicating with the inner cavity of the smelting vertical furnace is provided at the upper part of the smelting vertical furnace, and the smelting vertical furnace is also provided with a nitrogen delivery pipe communicating with the inner cavity of the smelting vertical furnace.

[0014] On the basis of the above technical solution, the present invention can also be improved as follows.

[0015] Furthermore, the flue gas ring pipe of the smelting vertical furnace is connected to the waste heat boiler, and the high-temperature flue gas in smelting passes through the flue gas riser to the flue gas ring pipe and then enters the waste heat boiler to produce steam after mixing.

[0016] Furthermore, it also includes a conveying component, which includes at least a belt conveyor, and the belt conveyor is located at the lower side of the outlets of the first mixer and the second mixer.

[0017] Furthermore, the conveying assembly also includes a belt elevator, the end of the belt conveyor is connected to the beginning of the belt elevator, and the end of the belt elevator is aligned with the inlet of the material distribution chute.

[0018] Further, it also includes a first feeding belt weighing machine, a second feeding belt weighing machine, a third feeding belt weighing machine and a fourth feeding belt weighing machine;

[0019] Further, the silo outlet of the titanium powder raw material is aligned with the upper side of the first feeding belt weighing machine, the silo outlet of the ferric oxide raw material is aligned with the upper side of the second feeding belt weighing machine, and the end of the first feeding belt and the end of the second feeding belt weighing machine are both aligned with the feeding port of the first mixer;

[0020] The silo outlet of the ilmenite raw material is aligned with the upper side of the third feeding belt weighing machine, the silo outlet of the pulverized coal raw material is aligned with the upper side of the fourth feeding belt weighing machine, and the ends of the third feeding belt weighing machine and the fourth feeding belt weighing machine are both aligned with the feeding port of the second mixer.

[0021] After adopting such a structure, the titanium chloride slag smelting device overcomes the problem of large amounts of "three wastes" generated by sulfuric acid and reduction corrosion methods in the existing titanium slag smelting technology. Although electric furnace smelting has less pollution, it consumes a lot of electricity and has a high investment cost. The titanium chloride slag smelting device is a smelting equipment with little pollution and almost no external energy consumption. It relies on the oxidation-reduction reaction of the raw materials themselves to release a large amount of heat to achieve the purpose of titanium slag smelting, and at the same time can improve the grade of titanium slag. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 It is a schematic diagram of an embodiment of the titanium chloride slag smelting device.

[0023] Figure 2 It is a schematic diagram of a distribution chute and a smelting vertical furnace in an embodiment of the titanium chloride slag smelting device.

[0024] Description of the numbers in the figure:

[0025] Silo for titanium powder raw material - 110; silo for ferric oxide raw material - 120; silo for ilmenite raw material - 130; silo for coal powder raw material - 140; first feeding belt weighing machine - 210; second feeding belt weighing machine - 220; third feeding belt weighing machine - 230; fourth feeding belt weighing machine - 240; first mixer - 310; second mixer - 320; material distribution chute - 400; first robotic arm - 410; smelting vertical furnace - 500; iron outlet - 510; slag outlet - 520; flue gas ring duct - 530; nitrogen delivery pipe - 540; refractory cover plate - 550; waste heat boiler - 600; belt conveyor - 710; belt elevator - 720. DETAILED DESCRIPTION

[0026] In order to make the above-mentioned purposes, features and advantages of the utility model more obvious and easy to understand, the specific implementation of the utility model is described in detail below in conjunction with the accompanying drawings. In the following description, many specific details are set forth to facilitate a full understanding of the utility model. However, the utility model can be implemented in many other ways different from those described herein, and those skilled in the art can make similar improvements without violating the connotation of the utility model, so the utility model is not limited by the specific implementation disclosed below.

[0027] The terms "vertical", "horizontal", "left", "right" and similar expressions used herein are for illustrative purposes only and do not represent the only implementations.

[0028] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art in the technical field of the present invention. The terms used herein in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more related listed items.

[0029] See also Figures 1 to 2 shown.

[0030] The titanium chloride slag smelting device in this embodiment is a device dedicated to the titanium chloride slag smelting method. The titanium chloride slag smelting device includes a first mixer 310, a second mixer 320, a material distribution chute 400, a smelting shaft furnace 500, a conveying assembly, a first feeding belt weighing machine 210, a second feeding belt weighing machine 220, a third feeding belt weighing machine 230 and a fourth feeding belt weighing machine 240.

[0031] The outlet of the silo 110 for the titanium powder raw material is aligned with the upper side of the first feeding belt weighing machine 210, and the outlet of the silo 120 for the ferric oxide raw material is aligned with the upper side of the second feeding belt weighing machine 220. The ends of the first feeding belt and the second feeding belt weighing machine 220 are both aligned with the feeding port of the first mixer 310.

[0032] The outlet of the ilmenite raw material silo 130 is aligned with the upper side of the third feeding belt weighing machine 230, and the outlet of the pulverized coal raw material silo 140 is aligned with the upper side of the fourth feeding belt weighing machine 240. The ends of the third feeding belt weighing machine 230 and the fourth feeding belt weighing machine 240 are both aligned with the feeding port of the second mixer 320.

[0033] The first mixer 310 is used to mix titanium powder and ferric oxide raw materials, and the second mixer 320 is used to mix ilmenite and coal powder raw materials. The outlets of the first mixer 310 and the second mixer 320 are aligned with the inlet of the distribution chute 400. The distribution chute 400 is arranged beside the opening of the smelting shaft furnace through the first mechanical arm 410, so that the outlet of the distribution chute 400 can be aligned with the opening of the smelting shaft furnace 500. The distribution chute 400 can be used to evenly distribute the raw materials discharged from the first mixer 310 or the second mixer 320. The material is distributed in the smelting vertical furnace 500. A water-cooled ignition gun (not shown in the figure) is provided at the upper part of the inner cavity of the smelting vertical furnace 500. A slag outlet 520 for discharging molten slag and an iron outlet 510 for discharging molten iron are provided at the lower part of the smelting vertical furnace 500. A flue gas ring 530 communicating with the inner cavity of the smelting vertical furnace 500 is provided at the upper part of the smelting vertical furnace 500. The smelting vertical furnace 500 is also provided with a nitrogen delivery pipe 540 communicating with the inner cavity of the smelting vertical furnace 500. The opening of the smelting vertical furnace 500 is provided with a refractory cover plate 550 for sealing the inner cavity of the smelting vertical furnace 500.

[0034] The flue gas ring duct 530 of the smelting vertical furnace 500 is connected to the waste heat boiler 600. The high-temperature flue gas in smelting passes through the flue gas riser to the flue gas ring duct 530 and then enters the waste heat boiler 600 to generate steam after mixing.

[0035] The conveying assembly includes a belt conveyor 710 and a belt elevator 720. The belt conveyor 710 is located at the lower side of the outlets of the first mixer 310 and the second mixer 320. The end of the belt conveyor 710 is connected to the beginning of the belt elevator 720, and the end of the belt elevator 720 is aligned with the inlet of the material distribution chute 400.

[0036] The titanium chloride slag smelting device is used to implement a titanium chloride slag smelting method, which includes the following steps:

[0037] a) Preparation of thermite-like auxiliary materials:

[0038] The titanium powder raw material is conveyed to the first mixer 310 through the first feeding belt weighing machine 210, and the ferric oxide raw material is conveyed to the first mixer 310 through the second feeding belt weighing machine 220, and the titanium powder and the ferric oxide are mixed in a mass ratio of 3:2 to obtain thermite-like auxiliary material;

[0039] b) Preparation of main materials:

[0040] The ilmenite raw material is conveyed to the second mixer 320 through the third feeding belt weighing machine 230, and the coal powder raw material is conveyed to the second mixer 320 through the fourth feeding belt weighing machine 240, and the ilmenite and coal powder are mixed in a mass ratio of 8:2 to obtain the main production material;

[0041] c) Fabric:

[0042] Thermite-like auxiliary materials or production main materials are transported to the smelting shaft furnace 500 through the conveying assembly and the material distribution chute 400. Specifically, a layer of production main materials (about 15-20 cm thick) is firstly distributed in the smelting shaft furnace 500, and then a layer of thermite-like auxiliary materials (about 10-15 cm thick) is distributed. This is repeated. When the distribution is completed, it is ensured that the uppermost layer is thermite-like auxiliary materials. The mass ratio of production main materials to thermite-like auxiliary materials is 3:1.

[0043] d) Ignition and reduction: The smelting shaft furnace 500 is closed, and the top layer of thermite auxiliary materials in the smelting shaft furnace 500 is ignited using a water-cooled ignition gun. The thermite auxiliary materials will release a large amount of heat, causing the next layer of production main materials to melt and reduce, and the molten slag iron will ignite the lower layer of thermite auxiliary materials, and this process is repeated until the smelting is completed;

[0044] e) Discharging and cooling: After the slag and molten iron are discharged through the slag outlet 520 and the iron outlet 510 of the smelting vertical furnace 500, nitrogen is introduced to cool them to below the ignition point of the thermite auxiliary material, thereby completing the titanium chloride slag smelting.

[0045] The titanium chloride slag smelting method utilizes a similar aluminothermic reaction to cause the raw material itself to undergo an oxidation-reduction reaction. Since the formation enthalpy of the oxide is extremely low, a large amount of heat is released in a short time, so that the iron oxide is reduced and separated in the smelting vertical furnace 500. At the same time, the titanium dioxide produced by the auxiliary material plays a role in improving the overall titanium slag grade.

[0046] In the prior art, the grade of titanium slag is mainly based on the content of TiO2 in the titanium slag. Moreover, thermite is a mixture of aluminum powder and refractory metal oxides. Common thermite is a mixture of aluminum powder and ferric oxide powder in a pink ratio (about 1:2.95). When ignited with an igniter, the reaction proceeds violently to obtain aluminum oxide and elemental iron and release a large amount of heat. The temperature can reach 2500°C and emit a dazzling light, which can melt the generated iron. Thermite is an important component of the thermite reaction, which plays an important role in high-temperature outdoor operations such as rail welding. It can be used to initiate some reactions that require high temperatures. Other elements are mixed with metal oxides and ignited, and a strong redox reaction will also occur, with an effect similar to thermite reaction. The elements can be aluminum, magnesium, calcium, titanium, silicon, boron - not limited to metals, and the metal oxides can be boron trioxide, silicon dioxide, chromium trioxide, manganese dioxide, ferric oxide, ferric oxide, copper oxide and lead tetraoxide. Sometimes these reactions are also called "magnesothermal method", "silicothermal method", "calcothermal method", "carbothermal method", etc. according to the reducing agent in the reaction.

[0047] The above is only one embodiment of the present invention. It should be pointed out that a person skilled in the art can make several modifications and improvements without departing from the principle of the present invention, and these should also be regarded as belonging to the protection scope of the present invention.

Claims

1. A titanium chloride slag smelting device, characterized in that: It includes a first mixer (310), a second mixer (320), a material distribution chute (400) and a smelting vertical furnace (500); The first mixer (310) is used to mix titanium powder and ferric oxide raw materials, and the second mixer (320) is used to mix ilmenite and coal powder raw materials. The outlets of the first mixer (310) and the second mixer (320) are aligned with the inlet of the distribution chute (400), and the outlet of the distribution chute (400) is aligned with the opening of the smelting shaft furnace (500). The distribution chute (400) can be used to mix the raw materials discharged from the first mixer (310) or the second mixer (320). The material is evenly distributed in the smelting vertical furnace (500). A water-cooled ignition gun is provided at the upper part of the inner cavity of the smelting vertical furnace (500). A slag outlet (520) for discharging molten slag and an iron outlet (510) for discharging molten iron are provided at the lower part of the smelting vertical furnace (500). A flue gas ring pipe (530) communicating with the inner cavity of the smelting vertical furnace (500) is provided at the upper part of the smelting vertical furnace (500). The smelting vertical furnace (500) is also provided with a nitrogen delivery pipe (540) communicating with the inner cavity of the smelting vertical furnace (500).

2. The titanium chloride slag smelting device according to claim 1, characterized in that: The flue gas ring pipe (530) of the smelting vertical furnace (500) is connected to the waste heat boiler (600), and the high-temperature flue gas in smelting passes through the flue gas riser to the flue gas ring pipe (530) and then enters the waste heat boiler (600) to generate steam after mixing.

3. The titanium chloride slag smelting device according to claim 1, characterized in that: It also includes a conveying assembly, which includes at least a belt conveyor (710). The belt conveyor (710) is located at the lower side of the outlets of the first mixer (310) and the second mixer (320).

4. The titanium chloride slag smelting device according to claim 3, characterized in that: The conveying assembly further comprises a belt elevator (720), the end of the belt conveyor (710) is connected to the beginning of the belt elevator (720), and the end of the belt elevator (720) is aligned with the inlet of the material distribution chute (400).

5. The titanium chloride slag smelting device according to claim 1, characterized in that: It also includes a first feeding belt weighing machine (210), a second feeding belt weighing machine (220), a third feeding belt weighing machine (230) and a fourth feeding belt weighing machine (240); The outlet of the silo (110) for the titanium powder raw material is aligned with the upper side of the first feeding belt weighing machine (210), the outlet of the silo (120) for the ferric oxide raw material is aligned with the upper side of the second feeding belt weighing machine (220), and the end of the first feeding belt and the end of the second feeding belt weighing machine (220) are both aligned with the feeding port of the first mixer (310); The outlet of the silo (130) for the ilmenite raw material is aligned with the upper side of the third feeding belt weighing machine (230), the outlet of the silo (140) for the pulverized coal raw material is aligned with the upper side of the fourth feeding belt weighing machine (240), and the ends of the third feeding belt weighing machine (230) and the fourth feeding belt weighing machine (240) are both aligned with the feeding port of the second mixer (320).

Citation Information

Patent Citations

  • A method for preparing titanium chloride slag from titanium concentrate

    CN114084902B

Cited By

  • Titanium chloride slag smelting method and titanium chloride slag smelting device

    CN117535529A

  • Method and equipment for smelting titanium chloride slag

    CN117535529B