A mold for casting steel pipe insert of aluminum alloy casting and molding method thereof

By using ring-shaped fake tires and positioning block design in aluminum alloy casting molds, the problems of complex mold structure and aluminum liquid leakage in resin sand low-pressure casting are solved, and the casting size is accurate and positioned accurately is achieved, reducing scrap rate and production costs are reduced. .

CN118045976BActive Publication Date: 2024-11-22西安西开精密铸造有限责任公司 +2
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
CN202410005793.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-01-02
Publication Date
2024-11-22
Estimated Expiration
2044-01-02

Smart Images

  • Figure CN118045976B_ABST
    Figure CN118045976B_ABST
Patent Text Reader

Abstract

The invention discloses a mold for casting a steel pipe insert of an aluminum alloy casting and a molding method thereof, belonging to the technical field of casting, comprising a casting mold, a core box and a steel pipe insert with a positioning block; the casting mold comprises a mold body, a mold annular false tire tightly attached to the outer circle of the mold body flange, and a positioning block false tire located in a pit of the mold annular false tire; the core box is used to manufacture a sand core placed at the bottom of the lower half mold prepared by the casting mold, and a withdrawal block is arranged on the core box, and the withdrawal block extends into the core box; the manufactured sand core has a sand filling hole, and there is no core dividing surface at this position, so there is no obvious seam, and there is no grinding seam to damage the steel pipe insert; a positioning block is arranged at one end of the steel pipe insert with a positioning block, the positioning block is placed in the groove of the positioning block of the lower half mold, and the other elbow end extends into the sand core; the mold structure of the steel pipe insert cast by the aluminum alloy casting is simple, and it is convenient for manufacturing and on-site molding operations, aluminum liquid will not leak into the pipeline, and obvious bubbles will not appear in the casting.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of casting, and in particular relates to a mold for casting a steel pipe insert of an aluminum alloy casting and a molding method thereof. Background Art

[0002] Aluminum alloy inlay castings have the advantages of both the light weight of aluminum alloy and the high strength, pressure resistance, and wear resistance of steel. As equipment manufacturing develops towards lightweight and high mobility, inlay castings are increasingly used in the fields of automobiles, aerospace, weapons, etc. In aluminum alloy inlay casting, usually when making or shaping the mold, grooves for positioning half of the two ends of the insert are made on the half mold or half cavity. Before pouring, the insert is pre-placed in the corresponding groove position of the aluminum alloy casting mold cavity or cavity and the mold or box is closed. Then the molten aluminum is poured into the mold cavity or cavity. After cooling and solidification, the insert is tightly wrapped in the poured aluminum alloy casting.

[0003] For the intersection of the cover plate and the cylinder, the evenly distributed multiple steel pipe inserts are connected from the raised end face behind the cover plate flange along the wall of the cover plate to the aluminum alloy casting inside the cylinder. It is advisable to adopt the resin sand low-pressure casting process with the flange facing down and the upper and lower parting. For the positioning of the insert molding, the conventional method is to horizontally part the center of the insert end face on the outer side of the casting, and the inner cavity of the casting is parted by the surface formed by the center line of the insert. The grooves for positioning half of the insert at both ends are made in the lower half mold, and a groove for positioning half is made in the upper half mold, and a groove for positioning half is made in the sand core. The Chinese invention patent with the publication number CN201510952231.7 discloses a manufacturing process for aluminum alloy investment casting with embedded steel pipe fittings, which includes the steps of coating steel pipe fittings-drying steel pipe fittings-coating the shell surface layer-drying the surface layer-coating the transition layer-drying the transition layer-coating the coarse sand layer-drying-baking-cleaning and drying-splicing combination. The invention can effectively solve the problems of complex and difficult coating process, easy penetration of molten metal into the inlays, and easy sparking in the casting when encountering a structure with inlaid parts during the production process of the traditional mold shell. The mold shell produced by this process has the advantages of high strength, good sealing, and uniform texture. It will not have the problem of aluminum alloy liquid leakage such as steel pipe fittings, and can also avoid the occurrence of problems such as sparking in the casting. A Chinese invention patent with publication number CN201610206785.7 discloses a cast aluminum alloy motor housing with a built-in stainless steel spiral coil water channel, including an aluminum alloy cast motor housing, a stainless steel spiral coil water channel connected to a water cooling circulation system is inlaid and cast in the motor housing, and one end of the stainless steel spiral coil water channel is connected to a process support skeleton; the invention does not need to be molded several times when the prefabricated stainless steel spiral coil water channel is molded in the EPS white mold of the motor housing, and does not need to fill sand inside the stainless steel spiral coil water channel before casting, the production cycle is greatly shortened, and the production efficiency is effectively improved. By arranging a process support skeleton in the motor housing and arranging a water inlet, a water outlet structure and an auxiliary structure on the stainless steel spiral coil water channel, it is ensured that the aluminum alloy motor housing with a built-in stainless steel spiral coil water channel has high strength, a stable and reliable structure, is not easy to deform and crack, can improve the casting accuracy of the motor housing, reduce the casting defects of the motor housing, and reduce the production cost.However, the existing resin sand low-pressure casting process steel pipe insert molding has the following problems: the mold of this parting method needs to place multiple false tires with mold structures on the back of the flange, and the false tires are relatively thin. The steel pipe insert part of the inner cavity of the casting is positioned as one end of the steel pipe insert, half of which is in the core box and the other half is in the model, and the mold is relatively complicated; the straight-end steel pipe insert extends out of the casting, and the steel pipe insert part on the outer side of the casting is positioned as the other end of the steel pipe insert, which is divided into two halves by the parting surface, belonging to the upper mold and the lower mold respectively. This part is relatively thin and easy to deform, resulting in inaccurate positioning; the upper and lower molds made, the parting surface outside the casting cavity is a plane, in order to prevent the upper and lower boxes from firing during the pouring process. , mud ropes are often placed, resulting in large deviations in casting size; when sand cores are placed in the lower mold, gaps are likely to occur between the cores during pouring, and the inserts extending into the inner cavity of the casting are likely to be damaged during grinding of the casting; when the cylinder is not a straight cylinder or the cylinder diameter increases from the cover end to the other end, there is a problem that the lower box cannot be demoulded, then sand cores are required for the part that cannot be demoulded, and core assembly is required for subsequent box assembling. During the pouring process, gaps are likely to occur between the core assemblies, and the inserts extending into the inner cavity of the casting are likely to be damaged during grinding of the casting; due to the presence of a parting surface at the insert positioning location, there is a risk that aluminum liquid flows from the parting surface into the steel pipe insert during casting, causing the risk of scrapping the casting. The Chinese invention patent with publication number CN201510952231.7 discloses a process for manufacturing an aluminum alloy investment casting shell with an inlaid steel pipe fitting. Each investment casting requires a wax mold, and other materials used are relatively expensive, resulting in a high overall production cost. At the same time, investment casting is suitable for producing small parts with complex shapes, high precision requirements or difficult to perform other processing. It is more troublesome to use investment casting for castings that are too heavy, and the castings produced generally do not exceed 25Kg. The binder used is silica sol, which has poor wettability on the investment mold. The coating of the surface, transition layer, and coarse sand layer is a coating and drying process, which takes a long time and is difficult to control. A Chinese invention patent with publication number CN201610206785.7 discloses a cast aluminum alloy motor housing with a built-in stainless steel spiral coil water channel. The lost foam casting process is adopted. Each casting of the blank motor housing requires a prefabricated stainless steel spiral coil water channel. The prefabricated stainless steel spiral coil water channel is formed in the motor housing EPS white mold and an integrated motor housing EPS white mold containing the prefabricated stainless steel spiral coil water channel is processed. The production cost of the casting is high. In addition, the lost foam casting is cast under negative pressure. Therefore, a negative pressure extraction device is also required.

[0004] In view of the problems in the existing resin sand low-pressure casting process, such as complex mold structure, easy deformation of the steel pipe insert part on the outer side of the casting of the mold, inaccurate positioning, large deviation of the casting size, damage to the insert due to grinding the seam next to the insert, and aluminum liquid drilling into the insert causing the casting to be scrapped, it is urgent to find a mold for casting steel pipe inserts of aluminum alloy castings and a molding method thereof to simplify the mold structure, protect the insert, and prevent aluminum liquid from drilling into the insert. Summary of the invention

[0005] In order to overcome the shortcomings of the above-mentioned prior art, the purpose of the present invention is to provide a mold for casting steel pipe inserts of aluminum alloy castings and a molding method thereof, so as to solve the technical problems in the existing resin sand low-pressure casting process, such as complex mold structure, easy deformation of the steel pipe insert part outside the casting of the mold, resulting in inaccurate positioning, large dimensional deviation of the casting, damage to the insert due to grinding the seam next to the insert, and aluminum liquid drilling into the insert, resulting in the scrapping of the casting.

[0006] In order to achieve the above object, the present invention adopts the following technical solutions:

[0007] The invention discloses a mold for casting a steel pipe insert of an aluminum alloy casting, comprising a casting mold, a core box and a steel pipe insert with a positioning block; the casting mold comprises a mold main body, a mold annular false tire tightly attached to the outer circle of a flange of the mold main body, and a positioning block false tire located in a pit of the mold annular false tire; a pull-out block is arranged on the core box, and the pull-out block extends into the core box; a positioning block is arranged at one end of the steel pipe insert with the positioning block, and the positioning block is placed in a positioning block groove of a lower half mold, and the other elbow end extends into a sand core.

[0008] Preferably, the positioning block fake tire is a plate-like structure with a side wall connected to a cylindrical structure, the cylindrical structure is connected to the raised end face on the back of the mold body flange, the plate-like structure has an upward and downward draft angle of 3-10° from the middle of the thickness, and the length of the cylindrical structure is greater than 10mm.

[0009] Preferably, the cross-section of the mold's annular fake tire is an isosceles trapezoidal structure above the back of the mold main body flange, the height is the distance from the back of the mold main body flange to the center of the straight tube end of the steel pipe insert with a positioning block, the length of the top short side is 10-50mm larger than the dimension of the fake tire positioning block in the direction perpendicular to the end face of the cylinder, and the angle between the hypotenuse and the vertical line of the bottom edge is 3-10°.

[0010] Further preferably, the cross-section of the mold annular fake tire is a right-angled trapezoidal structure between the front and back sides of the mold main body flange, the right-angled side is in contact with the outer circle of the mold main body flange, the gap is less than 0.5mm, and the hypotenuse is on a straight line with one hypotenuse of the isosceles trapezoid of the mold annular fake tire cross-section.

[0011] Preferably, a plurality of positioning block pits are evenly distributed on the annular fake tire of the mold, and the side walls of the positioning block pits are 3-10 degrees; the portion below the middle of the fake tire in the thickness direction of the positioning block is placed in the positioning block pit, and the fitting clearance between the two is less than 0.5mm.

[0012] Preferably, the length of the withdrawal block extending into the core box is greater than the length of the elbow extending into the inner cavity by 5-30 mm.

[0013] Preferably, the distance around the withdrawal block from the nearest point where the steel pipe insert with the positioning block extends into the elbow end is 5-30 mm.

[0014] Preferably, the positioning block is a plate-shaped structure.

[0015] The present invention also discloses a method for molding a steel pipe insert of an aluminum alloy casting using the above-mentioned mold, comprising the following steps:

[0016] 1) Pour dry sand into the open end of the elbow of the steel pipe insert with a positioning block, and then seal, plug and solidify the opening;

[0017] 2) Place the casting mold on the base plate, put on the sand box, place the chiller and pouring channel, and complete the upper mold after filling with sand, tamping, leveling and curing;

[0018] 3) Turn over the upper mold, remove the mold ring fake tire, put the positioning block fake tire, and then place the mold core head part, chiller and pouring channel on top. After sand filling, tamping, flattening and curing, the lower mold is completed;

[0019] 4) In the process of upper and lower mold molding, a core box is used for core making, the extracted block is placed in the hole opened on the outer wall of the core box, the corresponding runner and chill are placed on the core box, and the sand core is made after filling with sand, tamping, leveling and curing;

[0020] 5) After the lower mold is solidified, pull out the lower mold and turn it over; remove the mold parts in the upper and lower molds to obtain the upper and lower molds with the cavity facing upwards;

[0021] 6) After the sand core is solidified, pull out the block and take out the sand core;

[0022] 7) Apply high temperature resistant alcohol-based paint to the upper mold, lower mold and sand core;

[0023] 8) Install the sand core into the lower mold, extend the elbow end of the steel pipe insert with positioning block after pouring dry sand into the sand filling hole of the sand core, place the positioning block end of the steel pipe insert with positioning block in the groove of the annular boss of the lower mold, and squeeze it forward to seal the sand filling hole. After solidification, grind and trim to complete the shape of the steel pipe insert.

[0024] Preferably, in step 1), dry sand is poured into the open end of the steel pipe insert with the positioning block to a depth of 20-50 mm from the open end, and then the opening is sealed with resin sand, compacted and solidified.

[0025] Compared with the prior art, the present invention has the following beneficial effects:

[0026] The invention discloses a mold for casting a steel pipe insert of an aluminum alloy casting, comprising a casting mold, a core box and a steel pipe insert with a positioning block; the casting mold comprises a mold main body, a mold annular false tire tightly attached to the outer circle of a flange of the mold main body, and a positioning block false tire located in a pit of the mold annular false tire; the annular false tire is adopted on the outer circle of the flange so that the casting cavity is completely in the upper mold, and the size of the casting obtained by pouring is more accurate; an annular groove is made in the upper mold, and an annular convex groove is made in the lower mold, and the upper mold and the lower mold are combined to have a sealing structure, without the risk of artillery fire, and without the need to wind mud ropes; the curved surface parting at the positioning position of the steel pipe insert of the upper mold and the lower mold is realized, so that there is an operating space for placing the steel pipe insert. When making the upper mold, the positioning block fake tire is in the positioning block groove of the upper mold, and the positioning block groove in the annular groove of the upper mold is formed; when making the lower mold, the annular fake tire is removed, and the positioning block fake tire is installed to form the positioning block groove of the annular boss of the lower mold, and the steel pipe insert positioning block has a positioning structure in the upper mold and the lower mold. The core box is used to manufacture the sand core placed at the bottom of the lower mold prepared by the casting mold. The core box is provided with a pull-out block, and the pull-out block extends into the core box; the manufactured sand core has a sand filling hole, and there is no core dividing surface at this position, so there is no obvious seam, and there is no problem of grinding and seam damage to the steel pipe insert; the steel pipe insert with a positioning block is provided with a positioning block at one end, and the positioning block is placed in the positioning block groove of the lower mold, and the other elbow end extends into the sand core; the mold structure of the aluminum alloy casting steel pipe insert is simple, easy to make, the steel pipe insert is accurately positioned, the casting size precision is high, there is no obvious seam, and there will be no leakage of aluminum alloy aluminum liquid into the pipeline, and there will be no obvious bubbles in the casting.

[0027] Furthermore, the positioning block fake tire is a plate-like structure with a side wall connected to a cylindrical structure, the cylindrical structure is connected to the raised end face on the back of the flange of the mold main body, the plate has an upward and downward draft angle of 3-10° from the middle of the thickness, and the length of the cylinder is greater than 10mm; the positioning block grooves of the upper and lower molds are inclined, which is convenient for the box assembly operation; the plate-like structure of the fake tire positioning block is more than 10mm away from the mold main body, which is convenient for tamping during molding and sand filling, and the positioning block grooves of the upper and lower molds close to the cavity side are regular in shape and have sufficient strength, which is convenient for squeezing operations during positioning; the positioning block of the steel pipe insert of the cast casting blank has a cutting distance of more than 10mm from the protrusion on the back of the casting flange, which is convenient for removing the positioning block.

[0028] Furthermore, the cross-section of the annular fake tire of the mold is an isosceles trapezoidal structure above the back of the mold main body flange, the height is the distance from the back of the mold main body flange to the center of the straight tube end of the steel pipe insert with a positioning block, the angle between the hypotenuse and the vertical line of the base is 3-10°, the part above the back of the annular groove flange made by the upper mold is an isosceles trapezoidal structure, and the part above the back of the annular boss flange made by the lower mold is a matching isosceles trapezoidal structure, which is convenient for the box assembly operation, and the length of the short side of the top is 10-50mm larger than the dimension of the fake tire positioning block in the direction perpendicular to the cylindrical end face, so that the outer side of the annular groove of the positioning block fake tire can be easily packed when the lower mold is filled with sand, and the positioning block groove on the molded annular convex groove has a regular shape.

[0029] Furthermore, the cross-section of the mold annular fake tire is a right-angled trapezoidal structure between the front and back sides of the mold main body flange, the right-angled side is in contact with the outer circle of the mold main body flange, the gap is less than 0.5mm, and the hypotenuse is on a straight line with one hypotenuse of the isosceles trapezoid of the cross-section of the mold annular fake tire. In order to produce a right-angled trapezoidal structure cavity between the front and back sides of the upper half mold flange, a right-angled trapezoidal structure sand mold is produced between the front and back sides of the lower half mold flange. The right-angled side forms the outer diameter surface of the casting blank flange, and the mating surfaces of the upper half mold and the lower half mold are conical surfaces with beveled sides, which are easy to assemble, and the conical surfaces with beveled sides are an integral surface, which is convenient for processing and manufacturing.

[0030] Furthermore, a number of positioning block pits are evenly distributed on the annular fake tire of the mold, and the side walls of the pits are 3-10° for placing the positioning block fake tire; the part below the middle in the thickness direction of the positioning block fake tire is placed in the positioning block pit, and the fitting clearance between the two is less than 0.5mm, in order to ensure the positioning accuracy of the steel pipe insert.

[0031] Furthermore, the length of the pull-out block extending into the core box is greater than the length of the bent pipe extending into the inner cavity by 5-30mm, ensuring that the steel pipe insert extends into the sand filling hole of the sand core. When the steel pipe insert positioning block is placed in the positioning block groove of the lower mold, it will not support the sand filling hole of the sand core. The steel pipe insert positioning block cannot be placed in the positioning block groove of the lower mold, and the amount of sand filling work to seal the sand filling hole is as small as possible.

[0032] Furthermore, the distance around the pull-out block from the nearest point of the elbow end of the steel pipe insert with the positioning block is 5-30mm, ensuring that the steel pipe insert extends into the sand filling hole of the sand core. When the steel pipe insert positioning block is placed in the positioning block groove of the lower mold, it will not rub around the sand filling hole of the sand core. The steel pipe insert positioning block cannot be placed in the positioning block groove of the lower mold, and the amount of sand filling work to seal the sand filling hole is as little as possible.

[0033] Furthermore, the positioning block is a plate-shaped structure, which is easy to manufacture and easy to achieve positioning.

[0034] The present invention also discloses a molding method for casting steel pipe inserts of aluminum alloy castings using the above mold. The molding method using the above mold includes the following steps: 1) pouring dry sand into the open end of the elbow of the steel pipe insert with a positioning block, and then sealing, plugging and solidifying the opening; exhausting the gas in the steel pipe insert to prevent the steel pipe from preheating during the pouring process, causing the gas to expand and blow out, resulting in bubble defects in the casting. 2) placing the casting mold on the bottom plate, placing the chill and the pouring channel, and putting on the sand box. After filling with sand, tamping, scraping and solidifying, the upper half mold is completed; putting it on the floor to make the upper half mold parting surface flat, putting on the sand box, and facilitating the hoisting and flipping 180°. The chill, pouring channel, etc. are required for the casting process. 3) The upper mold is turned over, the annular dummy of the mold is removed, and the positioning block dummy is placed on it, in order to shape the annular boss and the positioning block groove for the lower mold; then the mold core head part is placed on top, in order to shape the sand core core head positioning in the lower mold, so that the sand core can be accurately placed in the lower mold; the chiller and runner are required for the casting process, and then the sand box is put on to facilitate the lifting of the lower mold. After sand filling, tamping, leveling and curing, the molding of the lower mold is completed. 4) In the process of molding the upper and lower molds, a core box is used for core making, and the pull-out block is placed in the hole opened on the outer wall of the core box, in order to shape the sand filling hole on the sand core for the bent end of the steel pipe insert to extend into the sand core. The corresponding runner and chiller are placed on the core box for the casting process. After sand filling, tamping, leveling and curing, the sand core is made. 5) After the lower mold is solidified, pull out the mold and turn it over; remove the mold parts in the upper and lower molds to obtain the upper and lower molds with the cavity facing upwards; complete the demoulding of the upper and lower molds. 6) After the sand core is solidified, pull out the block and take out the sand core; complete the preparation of the sand core with sand-filled holes. 7) Apply high-temperature resistant alcohol-based paint to the upper and lower molds; before installing the steel pipe inserts, complete the surface paint of the casting and sand core. Otherwise, after the steel pipe inserts are installed, the brushing operation will be affected and difficult to operate, resulting in partial inadequate brushing and difficult to clean sand sticking to the cast. 8) Load the sand core into the lower mold, extend the elbow end of the steel pipe insert with the positioning block after pouring dry sand into the sand filling hole of the sand core, place the positioning block end of the steel pipe insert with the positioning block in the groove of the annular boss of the lower mold, and squeeze it forward, and use resin sand to plug the sand filling hole. After solidification, polish and repair the mold, and brush the high-temperature resistant alcohol-based paint on the position of the sand mold plugging to complete the modeling of the steel pipe insert; the positioning block end of the steel pipe insert is placed in the groove of the positioning block of the lower mold for one end positioning, and then fill the sand filling hole of the sand core with sand for solidification to complete the positioning and fixing of the other end. Compared with investment casting and lost foam casting, the present invention can achieve mass production and has obvious cost advantages. One end of the steel pipe insert is positioned in the lower mold, and the other end is inserted into the sand core sand filling hole and positioned by plugging, which better realizes the modeling and positioning of the steel pipe insert, the mold structure is relatively simple, the steel pipe insert is more accurately positioned, and the casting size deviation is small.The sand core is filled with sand holes, and there is no core splitting surface at this position. Therefore, there is no obvious seam at this position, and there is no risk of damaging the steel pipe insert due to grinding seams. There will be no leakage of aluminum alloy liquid into the pipe, and obvious bubbles in the casting. The mold structure is simple and easy to make.

[0035] Furthermore, dry sand is poured into the open end of the steel pipe insert with a positioning block to a depth of 20-50 mm from the open end, and then the opening is sealed with resin sand, compacted and solidified; this prevents the dry sand of the steel pipe insert from leaking out during installation, which weakens the effect of exhausting gas in the steel pipe, and prevents the resin sand from being difficult to bond with the sand core when resin sand is used to seal the sand filling hole after the dry sand leaks out, resulting in sand inclusion defects in the cast casting. BRIEF DESCRIPTION OF THE DRAWINGS

[0036] Figure 1 Schematic diagram of a blank of an aluminum alloy casting for a cast steel pipe insert of the present invention; wherein (a) is a front view schematic diagram of an aluminum alloy casting for a cast steel pipe insert; (b) is a cross-sectional schematic diagram of an aluminum alloy casting for a cast steel pipe insert;

[0037] Figure 2 It is a schematic diagram of the structure of a steel pipe insert with a positioning block disclosed in the present invention;

[0038] Figure 3 It is a schematic diagram of the structure of a mold for casting steel pipe inserts of an aluminum alloy casting of the present invention;

[0039] Figure 4 It is a schematic diagram of the upper half of a mold for casting a steel pipe insert of an aluminum alloy casting according to the present invention;

[0040] Figure 5 It is a schematic diagram of the lower half of a mold for casting a steel pipe insert of an aluminum alloy casting according to the present invention;

[0041] Figure 6 This is a schematic diagram of the structure of a core box for casting a steel pipe insert of an aluminum alloy casting of the present invention;

[0042] Figure 7 It is a schematic diagram of preparing a sand core from a core box of a cast steel pipe insert of an aluminum alloy casting of the present invention;

[0043] Figure 8 The present invention is a schematic diagram of the shape of an aluminum alloy casting steel pipe insert.

[0044] Among them: 1-casting blank, 11-steel pipe insert, 2-steel pipe insert with positioning block, 3-casting mold, 31-mold body, 32-mold annular fake tire, 33-positioning block fake tire, 4-upper mold, 5-lower mold, 6-core box, 61-extraction block, 7-sand core. DETAILED DESCRIPTION

[0045] In order to enable those skilled in the art to better understand the scheme of the present invention, the technical scheme in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the present invention.

[0046] It should be noted that the terms "first", "second", etc. in the specification and claims of the present invention and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the data used in this way can be interchanged where appropriate, so that the embodiments of the present invention described herein can be implemented in an order other than those illustrated or described herein. In addition, the terms "including" and "having" and any variations thereof are intended to cover non-exclusive inclusions, for example, a process, method, system, product or device that includes a series of steps or units is not necessarily limited to those steps or units that are clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or devices.

[0047] The present invention is further described in detail below in conjunction with the accompanying drawings:

[0048] See also Figure 1 It is a schematic diagram of a blank of an aluminum alloy casting for a cast steel pipe insert; wherein, a is a schematic diagram of the front view of the aluminum alloy casting for the cast steel pipe insert; b is a schematic diagram of the cutaway view of the aluminum alloy casting for the cast steel pipe insert; it can be seen from the figure that the main body of the casting blank 1 is a structure where a cover plate and a cylinder intersect, and there are at least three protrusions on the back of the cover plate flange, and a reinforcing rib structure is provided corresponding to the inner cavity of the protrusions, and the steel pipe insert 11 extends from the protruding end face on the back of the cover plate flange along the cover plate wall to the inner cavity of the cylinder, and extends an elbow out of the inner cavity.

[0049] See also Figure 2 It is a schematic diagram of the structure of the steel pipe insert with positioning block disclosed in the present invention; as can be seen from the figure, one end of the steel pipe insert 2 with positioning block is provided with a positioning block, and the other end is an elbow end, which is open and used for pouring dry sand.

[0050] See also Figure 3 It is a schematic diagram of the structure of a mold for casting a steel pipe insert of an aluminum alloy casting of the present invention; as can be seen from the figure, the casting mold 3 includes a mold body 31, a mold annular fake tire 32 that is tightly attached to the outer circle of the flange of the mold body 31, and a positioning block fake tire 33 located in the pit of the mold annular fake tire 32.

[0051] See also Figure 4 It is a schematic diagram of the upper half of a mold for casting a steel pipe insert of an aluminum alloy casting according to the present invention; Figure 5 It is a schematic diagram of the lower half mold of the mold for casting steel pipe inserts of an aluminum alloy casting of the present invention; as can be seen from the figure, the upper half mold 4 is a square structure as a whole, with a recessed mold 3 cover plate shape in the middle, and three positions for placing steel pipe inserts 2 with positioning blocks are opened on the cover plate shape, and a cylindrical hole for placing sand cores 7 is reserved in the center of the square structure; the lower half mold 5 is a square structure as a whole, with a convex mold 3 cover plate shape in the middle, and three positions for placing steel pipe inserts 2 with positioning blocks are opened on the cover plate shape, and a cylindrical pit for placing sand cores 7 is reserved in the center of the square structure.

[0052] See also Figure 6 This is a schematic diagram of the structure of a core box for casting a steel pipe insert of an aluminum alloy casting of the present invention; Figure 7 It is a schematic diagram of preparing a sand core from a core box for casting a steel pipe insert of an aluminum alloy casting according to the present invention; as can be seen from the figure, a pull-out block 61 is provided on the core box 6, and the pull-out block 61 extends into the core box 6; corresponding runners and chills are placed on the core box 6, and after sand filling, tamping, leveling and curing, the sand core 7 is made.

[0053] See also Figure 8 It is a schematic diagram of the molding of a steel pipe insert of an aluminum alloy casting of the present invention; as can be seen from the figure, a sand core 7 is installed in the lower half mold 5, and the elbow end of the steel pipe insert 2 with a positioning block after pouring dry sand is extended into the sand filling hole of the sand core 7, and the positioning block end of the steel pipe insert 2 with a positioning block is placed in the groove of the annular boss of the lower half mold 5 and squeezed forward, and then the sand filling hole is sealed, and after solidification, it is polished and trimmed to complete the molding of the steel pipe insert.

[0054] The present invention provides a molding method for casting a steel pipe insert of an aluminum alloy casting, which is specifically as follows:

[0055] 1) Making a steel pipe insert 2 with a positioning block; pouring dry sand from the open end of the steel pipe insert 2 with a positioning block, 20-50 mm away from the open end; sealing the opening with resin sand, plugging and solidifying.

[0056] 2) The casting mold 3, including the model body 31, the mold annular fake tire 32, and the positioning block fake tire 33, is correctly installed and placed on the bottom plate, the sand box is put on, the chiller, the pouring channel, etc. are placed, the resin sand is filled, and it is compacted, scraped and solidified to complete the upper mold 4.

[0057] 3) The upper mold 4 is turned over, the mold annular fake tire 32 is removed and the positioning block fake tire 33 is replaced. In addition, the lower mold part of the mold, such as the mold core head part, cold iron, runner, etc., is placed, filled with resin sand, and tamped, scraped and cured to complete the molding of the lower mold 5.

[0058] 4) During the molding process of the upper mold 4 and the lower mold 5, the core box 6 is used for core making. The extraction block 61 of the core box 6 is put in place, the corresponding runner, chiller, etc. are placed on the core box 6, and the sand filling, tamping, leveling and curing are started to complete the production of the sand core 7.

[0059] 5) After confirming that the lower half mold 5 is solidified, pull out the half mold 5 and turn it over; extract the mold parts in the upper half mold 4 and the lower half mold 5 to obtain the upper half mold 4 and the lower half mold 5 with the cavity facing upward.

[0060] 6) After confirming that the sand core 7 is solidified, pull out the block 61 and then remove the sand core 7.

[0061] 7) Apply high temperature resistant alcohol-based paint to the upper and lower molds twice in a row.

[0062] 8) Brush the sand core 7 with a high-temperature resistant alcohol-based paint, lower it into the lower mold 5, extend the elbow end of the steel pipe insert 2 with a positioning block into the sand filling hole of the sand core 7, place the positioning block end in the groove in the annular groove of the lower mold 5, and squeeze it forward, and then use resin sand to seal the sand filling hole of the sand core 7 extending into the elbow. After the resin sand is cured, grind and repair it to ensure that the surface of the sand core 7 at the root of the steel pipe at the end of the sand core 7 has a smooth transition to complete the shaping of the steel pipe insert.

[0063] The present invention discloses a mold structure for casting a steel pipe insert of an aluminum alloy casting, which mainly comprises a steel pipe insert 2 with a positioning block, a casting mold 3 and a core box 6. The steel pipe insert 2 with a positioning block has a positioning block at the straight pipe end, which is a plate-like structure, and the upper and lower surfaces are parallel to the flange surface. The positioning block fake tire is a plate-like structure with a side wall connected to a cylindrical structure, and the plate has a draft angle of 3-10° upward and downward from the middle of the thickness, and the length of the cylinder is greater than 10 mm. The mold body 31 of the casting mold 3 has a flange outside, and the mold annular fake tire 32 is closely attached to the outer circle of the flange. The cross section of the mold annular fake tire 32 is an isosceles trapezoidal structure above the back of the mold body 31 flange, and the height is the distance from the back of the flange to the center of the straight tube end of the steel pipe insert 11. The length of the short side of the top is greater than the dimension of the fake tire positioning block in the vertical cylindrical end face direction of 10-50mm, and the angle between the hypotenuse and the vertical line of the bottom edge is 3-10°; the cross section of the mold annular fake tire 32 is a right-angled trapezoidal structure between the front and back of the mold body 31 flange, the right-angled side is attached to the outer circle of the flange, the gap is less than 0.5mm, and the hypotenuse is on a straight line with one hypotenuse of the isosceles trapezoid; on the mold annular fake tire 32, the positioning block pits are evenly distributed, and the side wall of the pit of the plate-like structure is 3-10°. The part below the middle of the positioning block fake tire 33 in the thickness direction is placed in the mold annular fake tire 32 pit, and the matching gap between the two is less than 0.5mm.

[0064] The core box 6 has a pull-out block 61, the length of the pull-out block 61 extending into the core box 6 is greater than the length of the elbow penetrating into the inner cavity by 5-30mm, and the distance around the pull-out block 61 to the nearest point of the elbow into which the steel pipe insert 2 extends is 5-30mm.

[0065] Compared with the prior art, the present invention has the following technical effects:

[0066] (1) Compared with investment casting and lost foam casting, the present invention can be mass-produced and has obvious cost advantages.

[0067] (2) The annular fake tire is a whole, and the positioning block fake tire is not divided into two halves. It is also a whole, there is no deformation problem, and the positioning accuracy is more accurate.

[0068] (3) An annular groove is made in the upper mold, and an annular convex groove is made in the lower mold. The upper and lower molds have a sealing structure when combined. There is no risk of fire, no need to wrap mud ropes, and the basic dimensional accuracy of the blank casting is better.

[0069] (4) One end of the steel pipe insert of the present invention is positioned in the lower mold, and the other end is extended into the sand core filling hole and positioned by blocking, which better realizes the molding positioning of the steel pipe insert and reduces the number of core boxes.

[0070] (5) The sand core of the present invention adopts sand-filled holes, and there is no core dividing surface at this position. Therefore, there is no obvious seam at this position, and there is no possibility of damaging the steel pipe insert due to grinding the seam.

[0071] (6) The present invention will not cause aluminum alloy liquid to leak into the pipeline, nor will it cause obvious bubbles to appear in the casting.

[0072] (7) The mold of the present invention has a simple structure and is easy to manufacture.

[0073] The above contents are only for explaining the technical idea of ​​the present invention and cannot be used to limit the protection scope of the present invention. Any changes made on the basis of the technical solution in accordance with the technical idea proposed by the present invention shall fall within the protection scope of the claims of the present invention.

Claims

1. A mold for casting steel pipe inserts with aluminum alloy castings, characterized in that: It comprises a casting mold (3), a core box (6) and a steel pipe insert (2) with a positioning block; The casting mold (3) comprises a mold body (31), a mold annular fake tire (32) closely attached to the outer circle of the flange of the mold body (31), and a positioning block fake tire (33) located in a recess of the mold annular fake tire (32); Pour dry sand into the open end of the elbow of the steel pipe insert (2) with the positioning block, and then seal, plug and solidify the opening; place the casting mold (3) on the bottom plate, put on the sand box, place the chiller and the pouring channel, and complete the upper mold (4) after filling with sand, tamping, leveling and solidifying; turn the upper mold (4) over, remove the mold annular dummy (32), place the positioning block dummy (33), and then place the mold core head part, chiller and pouring channel on top, and complete the lower mold (5) after filling with sand, tamping, leveling and solidifying; The core box (6) is provided with a pull-out block (61), and the pull-out block (61) extends into the core box (6); During the molding process of the upper mold (4) and the lower mold (5), a core box (6) is used for core making, a pull-out block (61) is placed in a hole opened on the outer wall of the core box (6), a corresponding runner and a chiller are placed on the core box (6), and after sand filling, compaction, leveling and solidification, the sand core (7) is made; after the lower mold (5) is solidified, the lower mold (5) is pulled out and turned over; the mold parts in the upper mold (4) and the lower mold (5) are removed to obtain the upper mold (4) and the lower mold (5) with the cavity facing upward; after the sand core (7) is solidified, the pull-out block (61) is pulled out and the sand core (7) is taken out; and the upper mold (4), the lower mold (5) and the sand core (7) are coated with a high-temperature resistant alcohol-based paint; The steel pipe insert (2) with a positioning block has a positioning block at one end, the positioning block is placed in the positioning block groove of the lower half mold (5), and the other elbow end extends into the sand core (7); The sand core (7) is installed in the lower mold (5), and the elbow end of the steel pipe insert (2) with a positioning block after pouring dry sand is extended into the sand filling hole of the sand core (7). The positioning block end of the steel pipe insert (2) with a positioning block is placed in the groove of the annular boss of the lower mold (5), and after being squeezed forward, the sand filling hole is sealed. After solidification, it is polished and trimmed to complete the shaping of the steel pipe insert.

2. The mold for casting steel pipe inserts with aluminum alloy castings according to claim 1, characterized in that: The positioning block fake tire (33) is a plate-like structure with a side wall connected to a cylindrical structure, the cylindrical structure is connected to the raised end surface of the back of the flange of the mold body, the plate-like structure has an upward and downward draft angle of 3-10° from the middle of the thickness, and the length of the cylindrical structure is greater than 10 mm.

3. The mold for casting steel pipe inserts with aluminum alloy castings according to claim 1, characterized in that: The cross section of the mold annular fake tire (32) is an isosceles trapezoidal structure above the back of the flange of the mold body (31), the height is the distance from the back of the flange of the mold body (31) to the center of the straight tube end of the steel tube insert (2) with a positioning block, the length of the top short side is 10-50 mm greater than the dimension of the fake tire positioning block in the direction perpendicular to the end face of the cylinder, and the angle between the hypotenuse and the vertical line of the bottom side is 3-10°.

4. The mold for casting steel pipe inserts with aluminum alloy castings according to claim 3, characterized in that: The cross section of the mold annular fake tire (32) is a right-angled trapezoidal structure between the front and back sides of the mold body (31) flange, the right-angled side is in contact with the outer circle of the mold body (31) flange, the gap is less than 0.5 mm, and the hypotenuse is on a straight line with one hypotenuse of the isosceles trapezoid of the cross section of the mold annular fake tire (32).

5. The mold for casting steel pipe inserts with aluminum alloy castings according to claim 1, characterized in that: A plurality of positioning block pits are evenly distributed on the mold annular fake tire (32), and the side walls of the positioning block pits are 3-10 degrees; the portion below the middle in the thickness direction of the positioning block fake tire (33) is placed in the positioning block pit, and the matching clearance between the two is less than 0.5mm.

6. The mold for casting steel pipe inserts with aluminum alloy castings according to claim 1, characterized in that: The length of the extraction block (61) extending into the core box (6) is greater than the length of the bent pipe extending into the inner cavity by 5-30 mm.

7. The mold for casting steel pipe inserts with aluminum alloy castings according to claim 1, characterized in that: The distance around the extraction block (61) from the nearest point of the steel pipe insert (2) with the positioning block extending into the elbow end is 5-30 mm.

8. The mold for casting steel pipe inserts with aluminum alloy castings according to claim 1, characterized in that: The positioning block is a plate-shaped structure.

9. A molding method for casting steel pipe inserts of aluminum alloy castings, characterized in that: The molding process using the mold described in any one of claims 1 to 8 comprises the following steps: 1) Pour dry sand into the open end of the elbow of the steel pipe insert with a positioning block (2), and then seal, plug and solidify the opening; 2) Place the casting mold (3) on the base plate, put on the sand box, place the chiller and the pouring channel, fill with sand, tamp, level and solidify, and complete the upper mold (4); 3) The upper mold (4) is turned over, the mold annular fake tire (32) is removed, and the positioning block fake tire (33) is placed on top, and then the mold core head part, chiller and pouring channel are placed on top, and after sand filling, tamping, scraping and curing, the lower mold (5) is completed; 4) During the molding process of the upper mold (4) and the lower mold (5), a core box (6) is used for core making, the extraction block (61) is placed in a hole opened on the outer wall of the core box (6), a corresponding runner and a chiller are placed on the core box (6), and after sand filling, tamping, leveling and curing, the sand core (7) is made; 5) After the lower mold (5) is solidified, the lower mold (5) is pulled out and turned over; the mold parts in the upper mold (4) and the lower mold (5) are removed to obtain the upper mold (4) and the lower mold (5) with the cavity facing upward; 6) After the sand core (7) is solidified, the extraction block (61) is pulled out to remove the sand core (7); 7) Apply high temperature resistant alcohol-based paint to the upper mold (4), the lower mold (5) and the sand core (7); 8) The sand core (7) is installed in the lower mold (5), and the elbow end of the steel pipe insert (2) with a positioning block after being poured with dry sand is extended into the sand filling hole of the sand core (7). The positioning block end of the steel pipe insert (2) with a positioning block is placed in the groove of the annular boss of the lower mold (5), and after being squeezed forward, the sand filling hole is sealed. After solidification, it is polished and trimmed to complete the shaping of the steel pipe insert.

10. The molding method of aluminum alloy casting steel pipe insert according to claim 9, characterized in that: In step 1), dry sand is poured into the open end of the steel pipe insert (2) with a positioning block to a depth of 20-50 mm from the open end, and then the opening is sealed with resin sand, compacted and solidified.

Citation Information

Patent Citations

  • Process for manufacturing shell with embedded steel pipe through aluminum alloy investment casting

    CN105522110A

  • Cast aluminum alloy motor casing with built-in stainless steel spiral coiled pipe water channel

    CN107294256A

  • Shaping structure and manufacturing process of casting elongated hole sand core

    CN103752767A

  • Casting mold and forming method for box body of gearbox

    CN105382206A

  • Lower cylinder block pouring mould and lower cylinder block pouring method

    CN106493307A