Production method of environment-friendly Gerer fiber

By optimizing the drying equipment and cooling structure, the problems of long drying time and poor cooling effect in environmentally friendly Grey fiber molding are solved, and the high quality, green and environmentally friendly characteristics and stability of the product are achieved.

CN118957781AActive Publication Date: 2024-11-15TONGKUN GRP
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202411300698.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-18
Publication Date
2024-11-15
Estimated Expiration
2044-09-18

AI Technical Summary

Technical Problem

The existing environmentally friendly Grey fibers are bonded due to the long drying time of the masterbatch during molding and have poor cooling effect, resulting in short length and poor texture of the product air barrel.

Method used

By optimizing the drying equipment, the capacity of the masterbatch drying barrel is reduced, the drying temperature is lowered, the dry air intake pressure is enhanced, and the feed head is installed at the feed port of the screw extruder for mixing the masterbatch and slices, increasing the length of the cooling air barrel , adopts a specific metal sand ratio and filter mesh configuration to improve the winding forming mechanism.

Benefits of technology

The masterbatch drying time is shortened, the bonding phenomenon is avoided, the cooling effect is improved, the feel, texture and production stability of the product are improved, and the green and environmentally friendly characteristics of the product are ensured.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118957781A_ABST
    Figure CN118957781A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of production of environment-friendly Gray fibers, in particular to a production method of the environment-friendly Gray fibers, which comprises the following steps: preparing the environment-friendly Gray fibers, adding master batches into drying equipment for drying, crystallizing slices, and adding the slices into the drying equipment for drying; mixing and drying are conducted, the dried master batches and slices are added into the discharging hopper at the same time, the air blower is controlled through the controller, after air enters the air blower through the air inlet pipe, the air inlet valve pipe is opened, the air enters the discharging hopper, and air blowing drying is conducted on the master batches and the slices. The cooling forming mechanism is used for cooling the environment-friendly Gray fibers, the cooled environment-friendly Gray fibers are oiled through an oil nozzle, and then the environment-friendly Gray fibers are wound through the winding forming mechanism.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of production of environmentally friendly grey fibers, and in particular to a production method of environmentally friendly grey fibers. Background Art

[0002] Under the premise that the country currently takes green, environmental protection and low carbon as the theme of the times, environmental protection and anti-fouling are hot terms in textile enterprises. The release of the most stringent new "Environmental Protection Law" in history indicates that the printing and dyeing industry will pay more attention to environmental protection, and potential complementary technologies will receive more attention. Among many technologies, the undyed fiber produced by solution coloring technology not only reduces the printing and dyeing process, saves energy and reduces emissions, but also in the consumption and use of fiber products, the fabric is brightly colored, uniform in color, durable, not easy to fade, friendly to the human body, and has great development prospects.

[0003] When the existing environmentally friendly Grey fiber is formed, a screw extruder is usually used to extrude the masterbatch and the slice. However, when the existing screw extruder is extruded, the proportion of the masterbatch added is too small, the original masterbatch drying barrel is too large, and the masterbatch drying time is long, resulting in the adhesion of the masterbatch. In addition, when the environmentally friendly Grey fiber after the filament is extruded enters the wind tube during extrusion molding, the wind tube length is too short and the cooling effect is poor.

[0004] To this end, we propose a production method for environmentally friendly Grey fiber. This invention is different from the conventional fiber production method in that a hole is opened at the feed port of the screw extruder, and the masterbatch feeding pipe is placed on the hole to mix the slices at the feed port. At the same time, by increasing the length of the wind tube, the cooling effect of the variety is improved, and the product quality is improved by optimizing the masterbatch drying process and the component filtering process. The product of this invention has the characteristics of soft and comfortable feel, rich texture, strong drape, easy to care for and rich suede. The product has excellent performance and is green and environmentally friendly, and is a typical representative of green fiber. Summary of the invention

[0005] In view of the problems in the prior art, the present invention provides an environmentally friendly gray fiber production method, which is convenient for mixing masterbatch and slices into a screw extruder, thereby improving the production efficiency of the product.

[0006] The technical solution adopted by the present invention to solve the technical problem is a method for producing an environmentally friendly gray fiber, comprising the steps of:

[0007] To prepare environmentally friendly Grey fiber, the master batch is added into the drying device for drying, the slices are crystallized, and then the slices are added into the drying device for drying;

[0008] The mixed drying includes a structure of a lower hopper, a controller, a blower, an air inlet pipe, an air inlet valve pipe, a motor shaft and blades. The dried masterbatch and slices are added into the lower hopper at the same time. The blower is controlled by the controller. After the blower takes in air through the air inlet pipe, the air inlet valve pipe is opened to allow the air to enter the lower hopper to blow dry the masterbatch and slices. The motor is controlled by the controller. The motor drives the shaft, and the shaft drives the blades to rotate in the lower hopper to turn over and dry the masterbatch and slices.

[0009] The melt extrusion includes a structure: an extruder, a controller and a metering pump. After the mixed and dried slices and masterbatch are added into the screw extruder, the screw extruder is controlled by the controller, and the screw extruder fuses and extrude the slices and masterbatch, so that the melt of the fused masterbatch and slices enters the metering pump for metering and weighing, and the metering pump can evenly discharge the melt into the spinneret hole of the screw extruder for extrusion;

[0010] The spinneret discharging structure includes: an extruder and a spinneret assembly. The melt after extrusion is transported to the conveying spinneret assembly. The spinneret assembly adopts a 5 / 10 mesh 180g metal sand ratio process and is filtered with a nine-layer integrated net to achieve the wire forming of the melt;

[0011] The cooling molding includes a structure: a spinneret assembly, a cooling mechanism and an oil nozzle for oiling. The melt is formed after passing through the spinneret assembly, and the environmentally friendly Grey fiber enters the cooling mechanism. The cooling mechanism can effectively improve the cooling conditions of the tow by lengthening the length of the cooling air cylinder. The environmentally friendly Grey fiber after cooling and molding is oiled through the oil nozzle.

[0012] The winding forming structure includes: a winding forming mechanism, the formed environment-friendly Grey fiber enters the winding forming mechanism, and the winding forming mechanism is wound to form the environment-friendly Grey fiber.

[0013] By adopting the above technical scheme, when the environmentally friendly Grey fiber is extruded, since a feed head is connected and installed at the feed inlet of the screw extruder, and a lower hopper is connected and installed at the top of the feed head through a discharge valve pipe, after the dried masterbatch and slices are added into the lower hopper, the motor is controlled by the controller so that the motor drives the rotating shaft at its output end to rotate, and since blades are installed on the shaft wall of the rotating shaft, the blades flip the masterbatch and slices in the lower hopper, and then the blower is controlled by the controller so that after the air inlet pipe is fed with air, since the exhaust port of the blower is connected to the outer wall of the lower hopper through the air inlet valve pipe, the air is discharged through the blower. The blower blows air into the lower hopper to dry the masterbatch and the slices to avoid crystallization of the masterbatch and the slices, so that the mixed masterbatch and the slices enter the screw extruder to extrude the environmentally friendly Grey fiber. The extruded environmentally friendly Grey fiber enters the metering pump and is transported to the spinneret assembly through the metering pump. The environmentally friendly Grey fiber is extruded and formed through the spinneret assembly. The extruded environmentally friendly Grey fiber enters the cooling and forming mechanism, and the cooling and forming mechanism cools the environmentally friendly Grey fiber. The cooled environmentally friendly Grey fiber is oiled with an oil nozzle and then wound by the winding and forming mechanism.

[0014] Specifically, the mixed drying optimization and improvement are as follows: first, the drying equipment is optimized. We reduced the capacity of the original masterbatch drying barrel from 300kg to 100kg. This adjustment shortens the drying time of the masterbatch in the barrel, thereby reducing the occurrence of bonding. Second, the drying temperature is adjusted. We lowered the drying temperature by 20 degrees. This measure helps the masterbatch to be dried under milder conditions, making the water evaporation more uniform and stable, preventing the masterbatch from excessive shrinkage and deformation during the drying process, and effectively solving the bonding problem. Third, the intake pressure is enhanced. We increased the intake pressure of the dry air by 0.2MPa from the original pressure. This change enhances the impact of the drying airflow on the masterbatch, improves the drying efficiency, and further prevents the bonding of the masterbatch.

[0015] By adopting the above technical solutions, firstly, we optimized the drying equipment. We reduced the capacity of the original masterbatch drying barrel from 300kg to 100kg. This adjustment shortened the drying time of the masterbatch in the barrel, thereby reducing the occurrence of bonding. Secondly, we adjusted the drying temperature. We lowered the drying temperature by 20 degrees. This measure helps to dry the masterbatch under milder conditions, making the water evaporation more uniform and stable, preventing the masterbatch from excessive shrinkage and deformation during the drying process, and effectively solving the bonding problem. Thirdly, we increased the intake pressure of the dry air by 0.2MPa from the original pressure. This change enhanced the impact of the drying airflow on the masterbatch, improved the drying efficiency, and further prevented the bonding of the masterbatch.

[0016] Specifically, the melt extrusion step: open a hole at the feed head of the screw extruder, place the feed hopper on the hole, make the slices and the masterbatch start to mix at the feed head of the screw extruder, melt through the screw extruder and further mix evenly before entering the box for spinning. Compared with the conventional dyeing method, the solution coloring omits the subsequent dyeing and finishing process in the production process, and is superior to the conventional dyeing in terms of color fastness, color uniformity and raw material utilization.

[0017] By adopting the above technical scheme, a hole is opened at the feed head of the screw extruder, and the feed hopper is placed on the hole, so that the slices and the masterbatch begin to mix at the feed head of the screw extruder, are melted by the screw extruder, and are further mixed evenly before entering the box for spinning. Compared with the conventional dyeing method, the solution coloring omits the subsequent dyeing and finishing process in the production process, and is superior to the conventional dyeing in terms of color fastness, color uniformity, and raw material utilization.

[0018] Specifically, the spinneret assembly adopts a 5 / 10 mesh 180g metal sand ratio process and is matched with a nine-layer integrated net for filtering.

[0019] By adopting the above technical solution, we have adopted a specific metal sand ratio scheme, that is, 5 / 10 mesh metal sand and 800 mesh nine-layer integrated filter. This configuration can ensure that impurities cannot penetrate the filter during the production process, thereby avoiding the filter clogging the wire holes. At the same time, we have also improved the diverter plate so that the melt can flow more evenly around, further ensuring the uniform distribution of component pressure.

[0020] Specifically, the cooling mechanism can effectively improve the cooling conditions of the filament bundle by lengthening the length of the cooling duct. The original duct length is only 191 mm. However, by adding a layer of 85 mm high device on the bellows, the duct length is increased to 276 mm, forming an extended cooling zone.

[0021] By adopting the above technical scheme, the improvement of the wind tube device has successfully improved the stability of product production. The original wind tube length was only 191 mm, which resulted in poor cooling effect and unstable production process when spinning extremely coarse monofilaments. In order to solve this problem, we modified the bellows structure and added a circle of device with a height of about 85 mm to the original bellows, so that the total length of the wind tube reached 276 mm. In addition, we also adjusted the wind pressure of the wind tube to ensure that the filament bundle is effectively cooled. These improvement measures effectively improved the cooling effect of this variety, improved production stability, and reduced the phenomenon of hair and broken ends in the subsequent processing process.

[0022] Specifically, the winding and forming mechanism adopts the utility model patent of "a wire guide structure device of a TMT winding machine-5 wire cake wire path". By changing the opening direction of the fifth U-shaped wire guide, the wire bundle no longer frequently contacts the U-shaped wire guide due to the angle problem, but contacts the circular wire guide instead. The contact position of the wire bundle and the wire guide is adjusted, which improves the stability of the production site and ensures the stability of the product's physical indicators.

[0023] By adopting the above technical solution and changing the opening direction of the fifth U-shaped wire guide, the yarn bundle no longer frequently contacts the U-shaped wire guide due to the angle problem, but contacts the circular wire guide instead, thereby adjusting the contact position of the yarn bundle and the wire guide, improving the stability of the production site and ensuring the stability of the product's physical indicators.

[0024] Specifically, it also includes a screw extruder, wherein a feed head is installed at the feed inlet of the screw extruder, a discharge valve pipe is installed at the top of the feed head, a lower hopper is installed at the other end of the discharge valve pipe, a cover plate is fixedly installed on the top of the lower hopper, a motor is installed at the plate wall of the cover plate by bolts, a rotating shaft is installed at the output end of the motor, blades are welded at the outer wall of the rotating shaft, a blower is installed at the shell wall of the screw extruder by bolts, an air inlet of the blower is installed with an air inlet pipe, the exhaust port of the blower is connected to the outer wall of the lower hopper through the air inlet valve pipe, and a controller is installed on the shell wall of the screw extruder.

[0025] By adopting the above technical scheme, when the environmentally friendly Grey fiber is extruded, since a feed head is connected and installed at the feed inlet of the screw extruder, and a lower hopper is connected and installed at the top of the feed head through a discharge valve pipe, after the dried masterbatch and slices are added into the lower hopper, the motor is controlled by the controller so that the motor drives the rotating shaft at its output end to rotate, and since blades are installed on the shaft wall of the rotating shaft, the blades flip the masterbatch and slices in the lower hopper, and then the blower is controlled by the controller so that after the air inlet pipe is fed with air, since the exhaust port of the blower is connected to the outer wall of the lower hopper through the air inlet valve pipe, the air is discharged through the blower. The blower blows air into the lower hopper to dry the masterbatch and the slices to avoid crystallization of the masterbatch and the slices, so that the mixed masterbatch and the slices enter the screw extruder to extrude the environmentally friendly Grey fiber. The extruded environmentally friendly Grey fiber enters the metering pump and is transported to the spinneret assembly through the metering pump. The environmentally friendly Grey fiber is extruded and formed through the spinneret assembly. The extruded environmentally friendly Grey fiber enters the cooling and forming mechanism, and the cooling and forming mechanism cools the environmentally friendly Grey fiber. The cooled environmentally friendly Grey fiber is oiled with an oil nozzle and then wound by the winding and forming mechanism.

[0026] Beneficial effects of the present invention:

[0027] (1) The method for producing an environmentally friendly grey fiber described in the present invention comprises the following steps: when the environmentally friendly grey fiber is extruded, a feed head is connected to the feed inlet of the screw extruder, and a lower hopper is connected to the top of the feed head through a discharge valve pipe, so that after the dried masterbatch and slices are added into the lower hopper, the motor is controlled by a controller so that the motor drives the rotating shaft at its output end to rotate, and blades are installed on the shaft wall of the rotating shaft so that the blades flip the masterbatch and slices in the lower hopper, and then the blower is controlled by the controller so that after the air enters the air inlet pipe, the air outlet of the blower is connected to the outer wall of the lower hopper through the air inlet valve pipe. The blower is used to blow air into the lower hopper, so as to dry the masterbatch and the slices to avoid crystallization of the masterbatch and the slices, so that the mixed masterbatch and the slices enter the screw extruder to extrude the environmentally friendly Grey fiber. The extruded environmentally friendly Grey fiber enters the metering pump and is transported to the spinneret assembly through the metering pump. The environmentally friendly Grey fiber is extruded and formed through the spinneret assembly. The extruded environmentally friendly Grey fiber enters the cooling and forming mechanism, and the cooling and forming mechanism cools the environmentally friendly Grey fiber. The cooled environmentally friendly Grey fiber is oiled with an oil nozzle, and then the environmentally friendly Grey fiber is wound through the winding and forming mechanism.

[0028] (2) In the production method of an environmentally friendly grey fiber described in the present invention, the original masterbatch drying barrel has a large capacity, which leads to a long drying time of the masterbatch, thereby causing the masterbatch to stick together. In order to solve this problem, we replaced the original 300kg masterbatch drying barrel with a 100kg capacity, and at the same time lowered the drying temperature by about 20 degrees and increased the dry air intake pressure by 0.2MPa. These adjustments shortened the drying time of the masterbatch from more than 30 hours to about 10 hours, successfully solving the problem of masterbatch sticking, while ensuring that the moisture content of the masterbatch meets the process requirements.

[0029] (3) The production method of the environmentally friendly Grey fiber described in the present invention is based on in-depth experimental research and combined with production experience. We have adopted a specific metal sand ratio scheme, that is, 5 / 10 mesh metal sand and 800 mesh nine-layer integrated filter screen. This configuration can ensure that impurities cannot penetrate the filter screen during the production process, thereby avoiding the filter screen from clogging the wire holes. At the same time, we have also improved the diverter plate so that the melt can flow more evenly around, further ensuring the uniform distribution of component pressure. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] The present invention is further described below in conjunction with the accompanying drawings and embodiments.

[0031] Figure 1 It is a schematic diagram of the main structure of the present invention;

[0032] Figure 2 It is a schematic diagram of the lower hopper structure of the present invention;

[0033] Figure 3 It is a schematic diagram of the blade structure of the present invention;

[0034] Figure 4 It is a schematic diagram of the production process structure of the present invention;

[0035] In the figure: 1. screw extruder; 2. lower hopper; 3. controller; 4. blower; 5. air inlet pipe; 6. motor; 7. discharge valve pipe; 8. air inlet valve pipe; 9. blades; 10. cover plate; 11. feed head; 12. metering pump; 13. spinneret assembly; 14. cooling mechanism; 15. oiling nozzle; 16. winding and forming mechanism; 17. rotating shaft. DETAILED DESCRIPTION

[0036] In order to make the technical means, creative features, objectives and effects achieved by the present invention easy to understand, the present invention is further explained below in conjunction with specific implementation methods.

[0037] In order to facilitate the impurity removal and screening of crude terephthalic acid, thereby improving the production efficiency of the product, as an embodiment of the present invention, Figure 1 , Figure 2 , Figure 3 and Figure 4 As shown, the production method of an environmentally friendly gray fiber described in the present invention comprises the steps of:

[0038] To prepare environmentally friendly Grey fiber, the master batch is added into the drying device for drying, the slices are crystallized, and then the slices are added into the drying device for drying;

[0039] The mixed drying includes a structure of: a lower hopper 2, a controller 3, a blower 4, an air inlet pipe 5, an air inlet valve pipe 8, a motor 6 shaft 17 and blades 9. The dried masterbatch and slices are added into the lower hopper 2 at the same time. The blower 4 is controlled by the controller 3. After the blower 4 takes in air through the air inlet pipe 5, the air inlet valve pipe 8 is opened to allow the air to enter the lower hopper 2 to blow dry the masterbatch and slices. The motor 6 is controlled by the controller 3. The motor 6 drives the shaft 17. The shaft 17 drives the blades 9 to rotate in the lower hopper 2 to turn over and dry the masterbatch and slices.

[0040] The melt extrusion includes a structure of an extruder 1, a controller 3 and a metering pump 12. After the mixed and dried slices and masterbatch are added into the screw extruder 1, the screw extruder 1 is controlled by the controller 3, and the screw extruder 1 fuses and extrude the slices and masterbatch, so that the melt of the fused masterbatch and slices enters the metering pump 12 for metering and weighing, and the metering pump 12 can evenly discharge the melt into the spinneret hole of the screw extruder 1 for extrusion;

[0041] The spinneret discharging structure includes: an extruder 1 and a spinneret assembly 13. The melt after extrusion is transported to the conveying spinneret assembly 13. The spinneret assembly adopts a 5 / 10 mesh 180g metal sand ratio process and is filtered with a nine-layer integrated net to achieve the wire forming of the melt;

[0042] The cooling molding includes a structure: a spinneret assembly 13, a cooling mechanism 14 and an oil nozzle 15. The melt is formed after passing through the spinneret assembly 13, and the environmentally friendly Grey fiber enters the cooling mechanism 14. The cooling mechanism 14 can effectively improve the cooling condition of the tow by lengthening the length of the cooling air cylinder. The environmentally friendly Grey fiber after cooling and molding passes through the oil nozzle 15;

[0043] The winding forming structure includes: a winding forming mechanism 16, the formed environment-friendly grey fiber enters the winding forming mechanism 16, and the winding forming mechanism 16 is wound to form the environment-friendly grey fiber.

[0044] During use, when the environmentally friendly Grey fiber is extruded, since the feed port of the screw extruder 1 is connected to and installed with a feed head 11, and the top of the feed head 11 is connected to and installed with a lower hopper 2 through a discharge valve pipe 7, after the dried masterbatch and slices are added into the lower hopper 2, the motor 6 is controlled by the controller 3 so that the motor 6 drives the rotating shaft 17 at its output end to rotate, and since blades 9 are installed on the shaft wall of the rotating shaft 17, the blades 9 turn over the masterbatch and slices in the lower hopper 2, and then the blower 4 is controlled by the controller 3 so that after the air inlet pipe 5 is fed with air, since the air outlet of the blower 4 is connected to the outer wall of the lower hopper 2 through the air inlet valve pipe 8, The blower 4 is used to blow air into the lower hopper 2, so as to dry the masterbatch and the slices to avoid crystallization of the masterbatch and the slices, so that the mixed masterbatch and the slices enter the screw extruder 1 to extrude the environmentally friendly Grey fiber. The extruded environmentally friendly Grey fiber enters the metering pump 12, and is transported to the spinneret assembly 13 by the metering pump 12. The environmentally friendly Grey fiber is extruded and formed by the spinneret assembly 13. The extruded environmentally friendly Grey fiber enters the cooling and molding mechanism, and the cooling and molding mechanism cools the environmentally friendly Grey fiber. The cooled environmentally friendly Grey fiber is oiled by the oil nozzle 15, and then the environmentally friendly Grey fiber is wound by the winding and molding mechanism 16.

[0045] For the drying process of masterbatch and chips, for example, Figure 4 As shown in the figure, the mixed drying optimization and improvement are as follows: first, the drying equipment is optimized. We reduced the capacity of the original masterbatch drying barrel from 300kg to 100kg. This adjustment shortens the drying time of the masterbatch in the barrel, thereby reducing the occurrence of bonding. Second, the drying temperature is adjusted. We lowered the drying temperature by 20 degrees. This measure helps the masterbatch to be dried under milder conditions, making the water evaporation more uniform and stable, preventing the masterbatch from excessive shrinkage and deformation during the drying process, and effectively solving the bonding problem. Third, the intake pressure is enhanced. We increased the intake pressure of the dry air by 0.2MPa from the original pressure. This change enhances the impact of the drying airflow on the masterbatch, improves the drying efficiency, and further prevents the bonding of the masterbatch.

[0046] When using, first optimize the drying equipment. We reduced the capacity of the original masterbatch drying barrel from 300kg to 100kg. This adjustment shortened the drying time of the masterbatch in the barrel, thereby reducing the occurrence of bonding. Second, adjust the drying temperature. We lowered the drying temperature by 20 degrees. This measure helps the masterbatch to dry under milder conditions, making the water evaporation more uniform and stable, preventing the masterbatch from excessive shrinkage and deformation during the drying process, and effectively solving the bonding problem. Third, increase the intake pressure. We increased the intake pressure of the dry air by 0.2MPa from the original pressure. This change enhances the impact of the drying airflow on the masterbatch, improves the drying efficiency, and further prevents the masterbatch from bonding.

[0047]

[0048]

[0049] For masterbatch and chip melt extrusion processing, exemplary, such as Figure 4 As shown, the melt extrusion step is as follows: a hole is opened at the feed head 11 of the screw extruder 1, and the feed hopper is placed on the hole, so that the slices and the masterbatch begin to mix at the feed head 11 of the screw extruder 1, and are melted by the screw extruder 1 and further mixed evenly before entering the box for spinning. Compared with the conventional dyeing method, the solution coloring omits the subsequent dyeing and finishing process in the production process, and is superior to the conventional dyeing in terms of color fastness, color uniformity, and raw material utilization.

[0050] When in use, an opening is opened at the feed head 11 of the screw extruder 1, and a feed hopper is placed on the opening, so that the slices and the masterbatch begin to mix at the feed head 11 of the screw extruder 1, are melted by the screw extruder 1, and further mixed evenly before entering the box for spinning. Compared with conventional dyeing methods, the solution coloring omits the subsequent dyeing and finishing process in the production process, and is superior to conventional dyeing in terms of color fastness, color uniformity, and raw material utilization.

[0051]

[0052] For masterbatch and chip extrusion filtration processing, for example, Figure 4 As shown, the spinneret assembly 13 adopts a 5 / 10 mesh 180g metal sand ratio process and is matched with a nine-layer integrated net for filtering.

[0053] When using it, we adopted a specific metal sand ratio scheme, that is, 5 / 10 mesh metal sand and 800 mesh nine-layer integrated filter. This configuration can ensure that impurities cannot penetrate the filter during the production process, thereby avoiding the filter clogging the wire holes. At the same time, we have also improved the diverter plate so that the melt can flow more evenly around, further ensuring the uniform distribution of component pressure.

[0054] When cooling the environmentally friendly gray fiber, for example, Figure 4 As shown, the cooling mechanism 14 can effectively improve the cooling conditions of the filament bundle by lengthening the length of the cooling air duct. The original length of the air duct is only 191 mm. However, by adding a layer of 85 mm high device on the bellows, the length of the air duct is increased to 276 mm, forming an extended cooling zone.

[0055] During use, the improvement of the wind tube device successfully improved the stability of product production. The original wind tube length was only 191 mm, which resulted in poor cooling effect and unstable production process when spinning extremely coarse monofilament varieties. In order to solve this problem, we modified the bellows structure and added a circle of device with a height of about 85 mm to the original bellows, so that the total length of the wind tube reached 276 mm. In addition, we also adjusted the wind pressure of the wind tube to ensure that the filament bundle is effectively cooled. These improvement measures effectively improved the cooling effect of this variety, improved production stability, and reduced the phenomenon of hair and broken ends in the subsequent processing process.

[0056]

[0057] For environmentally friendly grey fiber winding, for example, Figure 4 As shown, the winding and forming mechanism adopts the utility model patent of "a wire guide structure device of a TMT winding machine-5 wire cake wire path", by changing the opening direction of the fifth U-shaped wire guide, the wire bundle no longer frequently contacts the U-shaped wire guide due to the angle problem, but contacts the circular wire guide instead, and adjusts the contact position of the wire bundle and the wire guide, thereby improving the stability of the production site and ensuring the stability of the physical indicators of the product.

[0058] When in use, by changing the opening direction of the fifth U-shaped wire guide, the yarn bundle no longer frequently contacts the U-shaped wire guide due to angle problems, but contacts the circular wire guide instead. The contact position of the yarn bundle and the wire guide is adjusted, which improves the stability of the production site and ensures the stability of the product's physical indicators.

[0059] In order to grind and screen the crude terephthalic acid, for example, Figure 1 , Figure 2 and Figure 3As shown, it also includes a screw extruder 1, a feed head 11 is connected and installed at the feed port of the screw extruder 1, a discharge valve pipe 7 is connected and installed at the top of the feed head 11, a lower hopper 2 is connected and installed at the top of the lower hopper 2, a cover plate 10 is fixedly installed on the top of the lower hopper 2, a motor 6 is installed on the plate wall of the cover plate 10 by bolts, a rotating shaft 17 is installed at the output end of the motor 6, and blades 9 are welded on the outer wall of the rotating shaft 17, a blower 4 is installed on the shell wall of the screw extruder 1 by bolts, an air inlet of the blower 4 is connected and installed with an air inlet pipe 5, the exhaust port of the blower 4 is connected to the outer wall of the lower hopper 2 through an air inlet valve pipe 8, and a controller 3 is installed on the shell wall of the screw extruder 1.

[0060] During use, when the environmentally friendly Grey fiber is extruded, since the feed port of the screw extruder 1 is connected to and installed with a feed head 11, and the top of the feed head 11 is connected to and installed with a lower hopper 2 through a discharge valve pipe 7, after the dried masterbatch and slices are added into the lower hopper 2, the motor 6 is controlled by the controller 3 so that the motor 6 drives the rotating shaft 17 at its output end to rotate, and since blades 9 are installed on the shaft wall of the rotating shaft 17, the blades 9 turn over the masterbatch and slices in the lower hopper 2, and then the blower 4 is controlled by the controller 3 so that after the air inlet pipe 5 is fed with air, since the air outlet of the blower 4 is connected to the outer wall of the lower hopper 2 through the air inlet valve pipe 8, The blower 4 is used to blow air into the lower hopper 2, so as to dry the masterbatch and the slices to avoid crystallization of the masterbatch and the slices, so that the mixed masterbatch and the slices enter the screw extruder 1 to extrude the environmentally friendly Grey fiber. The extruded environmentally friendly Grey fiber enters the metering pump 12, and is transported to the spinneret assembly 13 by the metering pump 12. The environmentally friendly Grey fiber is extruded and formed by the spinneret assembly 13. The extruded environmentally friendly Grey fiber enters the cooling and molding mechanism, and the cooling and molding mechanism cools the environmentally friendly Grey fiber. The cooled environmentally friendly Grey fiber is oiled by the oil nozzle 15, and then the environmentally friendly Grey fiber is wound by the winding and molding mechanism 16.

[0061] When processing the environmentally friendly Grey fiber, the original masterbatch drying barrel has a large capacity, which leads to a long drying time for the masterbatch, thus causing the masterbatch to stick together. In order to solve this problem, we replaced the original 300kg masterbatch drying barrel with a 100kg capacity, and at the same time lowered the drying temperature by about 20 degrees and increased the dry air intake pressure by 0.2MPa. These adjustments shortened the drying time of the masterbatch from more than 30 hours to about 10 hours, successfully solving the problem of masterbatch sticking, and ensuring that the moisture content of the masterbatch meets the process requirements. When the screw extruder 1 is discharged, the feed port of the screw extruder 1 is connected with a feed head 11, and the top of the feed head 11 is connected with a lower hopper 2 through a discharge valve pipe 7. After the dried masterbatch and slices are added into the lower hopper 2, the motor 6 is controlled by the controller 3, so that the motor 6 drives the rotating shaft 17 at its output end to rotate. Since the shaft wall of the rotating shaft 17 is equipped with a blade 9, the blade 9 turns over the masterbatch and slices in the lower hopper 2. Then, the blower 4 is controlled by the controller 3, so that after the air inlet 5 enters, the air outlet of the blower 4 is connected to the lower hopper 2. The outer wall is connected by an air inlet valve pipe 8, so that air is blown into the lower hopper 2 through the blower 4, so as to dry the masterbatch and the slices to avoid crystallization of the masterbatch and the slices, so that the mixed masterbatch and the slices enter the screw extruder 1 to extrude the environmentally friendly Grey fiber. The extruded environmentally friendly Grey fiber enters the metering pump 12 and is transported to the spinneret assembly 13 through the metering pump 12. After in-depth experimental research and combined with production experience, we have adopted a specific metal sand ratio scheme, that is, 5 / 10 mesh metal sand and 800 mesh nine-layer comprehensive filter screen. This ratio The arrangement can ensure that impurities cannot penetrate the filter screen during the production process, thereby avoiding the situation where the filter screen is blocked by the wire holes. At the same time, we have also improved the diverter plate so that the melt can flow more evenly around, further ensuring the uniform distribution of component pressure. The environmentally friendly Grey fiber is extruded and formed by the spinneret assembly 13. The extruded environmentally friendly Grey fiber enters the cooling and forming mechanism. The cooling and forming mechanism cools the environmentally friendly Grey fiber. The cooled environmentally friendly Grey fiber is oiled by the oil nozzle 15, and then the environmentally friendly Grey fiber is wound by the winding and forming mechanism 16.

[0062] The above shows and describes the basic principles, main features and advantages of the present invention. Those skilled in the art should understand that the present invention is not limited to the above embodiments. The above embodiments and descriptions are only for explaining the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention. The scope of the present invention is defined by the attached claims and their equivalents.

Claims

1. A method for producing an environmentally friendly grey fiber, characterized in that: Includes steps: To prepare environmentally friendly Grey fiber, the master batch is added into the drying device for drying, the slices are crystallized, and then the slices are added into the drying device for drying; The mixed drying comprises a structure of: a lower hopper (2), a controller (3), a blower (4), an air inlet pipe (5), an air inlet valve pipe (8), a motor (6) shaft (17) and blades (9); the dried masterbatch and slices are added into the lower hopper (2) at the same time; the blower (4) is controlled by the controller (3); after the blower (4) takes in air through the air inlet pipe (5), the air inlet valve pipe (8) is opened to allow the air to enter the lower hopper (2) to blow and dry the masterbatch and slices; the motor (6) is controlled by the controller (3); the motor (6) drives the shaft (17); the shaft (17) drives the blades (9) to rotate in the lower hopper (2) to turn over and dry the masterbatch and slices; The melt extrusion comprises a structure of an extruder (1), a controller (3) and a metering pump (12). After the mixed and dried slices and masterbatch are added into the screw extruder (1), the screw extruder (1) is controlled by the controller (3), and the screw extruder (1) fuses and extrude the slices and masterbatch, so that the melt of the fused masterbatch and slices enters the metering pump (12) for metering and weighing, and the metering pump (12) discharges the melt evenly into the spinneret hole of the screw extruder (1) for extrusion; The spinneret discharging structure comprises: an extruder (1) and a spinneret assembly (13), wherein the melt after extrusion is transported to the transport spinneret assembly (13), wherein the spinneret assembly adopts a 5 / 10 mesh 180 g metal sand ratio process and is filtered with a nine-layer integrated net to achieve the spinning and forming of the melt; The cooling molding comprises a structure of a spinneret assembly (13), a cooling mechanism (14) and an oil nozzle (15). The melt is formed after passing through the spinneret assembly (13), and the environmentally friendly Grey fiber enters into the cooling mechanism (14). The cooling mechanism (14) can effectively improve the cooling conditions of the fiber bundle by lengthening the length of the cooling air cylinder. The environmentally friendly Grey fiber after cooling molding passes through the oil nozzle (15). The winding forming structure comprises a winding forming mechanism (16), the formed environmentally friendly Grey fiber enters the winding forming mechanism (16), and the winding forming mechanism (16) is wound to form the environmentally friendly Grey fiber.

2. The method for producing an environmentally friendly grey fiber according to claim 1, characterized in that: The mixed drying optimization and improvement are as follows: first, the drying equipment is optimized. We reduced the capacity of the original masterbatch drying barrel from 300kg to 100kg. This adjustment shortens the drying time of the masterbatch in the barrel, thereby reducing the occurrence of bonding. Second, the drying temperature is adjusted. We lowered the drying temperature by 20 degrees. This measure helps the masterbatch to be dried under milder conditions, making the water evaporation more uniform and stable, preventing the masterbatch from excessive shrinkage and deformation during the drying process, and effectively solving the bonding problem. Third, the intake pressure is enhanced. We increased the intake pressure of the dry air by 0.2MPa from the original pressure. This change enhances the impact of the drying airflow on the masterbatch, improves the drying efficiency, and further prevents the bonding of the masterbatch.

3. The method for producing an environmentally friendly gray fiber according to claim 2, characterized in that: The melt extrusion step comprises: opening an opening at the feed head (11) of the screw extruder (1), placing the feed hopper on the opening, allowing the slices and the masterbatch to begin to mix at the feed head (11) exiting the screw extruder (1), melting through the screw extruder (1), further mixing evenly, and then entering the spinning box. Compared with conventional dyeing methods, the dope dyeing method omits the subsequent dyeing and finishing process during the production process, and is superior to conventional dyeing in terms of color fastness, color uniformity, and raw material utilization.

4. The method for producing an environmentally friendly gray fiber according to claim 3, characterized in that: The spinneret assembly (13) adopts a 5 / 10 mesh 180g metal sand ratio process and is matched with a nine-layer integrated net for filtering.

5. The method for producing an environmentally friendly grey fiber according to claim 4, characterized in that: The cooling mechanism (14) can effectively improve the cooling conditions of the filament bundle by lengthening the length of the cooling duct. The original duct length is only 191 mm. However, by adding a layer of 85 mm high device on the wind box, the duct length is increased to 276 mm, forming an extended cooling zone.

6. The method for producing an environmentally friendly grey fiber according to claim 5, characterized in that: The winding and forming mechanism adopts the utility model patent of "a wire guide structure device of a TMT winding machine-5 wire cake wire paths". By changing the opening direction of the fifth U-shaped wire guide, the wire bundle no longer frequently contacts the U-shaped wire guide due to angle problems, but contacts the circular wire guide instead. The contact position of the wire bundle and the wire guide is adjusted, which improves the stability of the production site and ensures the stability of the product's physical indicators.

7. A method and device for producing an environmentally friendly gray fiber according to claims 1-6 is as follows, characterized in that: It also comprises a screw extruder (1), wherein a feed head (11) is connected and installed at the feed inlet of the screw extruder (1), a discharge valve pipe (7) is connected and installed at the top of the feed head (11), a lower hopper (2) is installed at the other end of the discharge valve pipe (7), a cover plate (10) is fixedly installed at the top of the lower hopper (2), a motor (6) is installed at the plate wall of the cover plate (10) by bolts, a rotating shaft (17) is installed at the output end of the motor (6), a blade (9) is welded to the outer wall of the rotating shaft (17), a blower (4) is installed at the shell wall of the screw extruder (1) by bolts, an air inlet of the blower (4) is connected and installed with an air inlet pipe (5), an air exhaust port of the blower (4) is connected to the outer wall of the lower hopper (2) by an air inlet valve pipe (8), and a controller (3) is installed at the shell wall of the screw extruder (1).

Citation Information

Patent Citations

  • Functional nylon 6 fiber production method

    CN104862811A

  • Vacuum rotary automatic dryer for fruits, vegetables, cereals, herbs, medicines and granulate

    CN107923705A

  • Energy-saving compact polyester chip crystallizing and drying system

    CN111773762A

  • Polyamide fiber production method

    CN112959541A

  • Anti-snagging high-density microfiber production equipment and production process

    CN114672886A