Magnetic material split-flow roasting device and system and using method
By using magnetic poles and baffles to separate magnetic materials from non-magnetic materials in the magnetic material split roasting device, and completing roasting in the fluidized roasting area, the problem of high land occupation and maintenance costs of pyrite system is solved, and high efficiency is achieved The magnetic separation and roasting process improves product purity and resource utilization.
Patent Information
- Application Number
- CN202411170222.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-23
- Publication Date
- 2024-11-29
AI Technical Summary
The existing pyrite comprehensive treatment system covers a large area, has high investment, high maintenance costs, complex process flow, and is difficult to efficiently separate magnetic materials, affecting the efficiency of resource utilization.
Design a magnetic material split roasting device, using magnetic poles and baffles inside the outer shell to separate magnetic materials and non-magnetic materials under the action of airflow, and the magnetic materials are calcined in the fluidized roasting area, simplifying the process flow and reducing system occupation and maintenance costs.
The integrated magnetic separation and roasting of pyrite is realized, which reduces the system's footprint and investment, reduces maintenance costs, improves the purity and yield of roasted products, and complies with the simplicity and efficiency requirements of national industrial policies.
Smart Images

Figure CN119043014A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a split-flow roasting device and system and a use method, and in particular to a split-flow roasting device and system for magnetic materials and a use method, belonging to the technical field of iron ore magnetic separation roasting. Background Art
[0002] Pyrite Fe 1-x S (0<x<0.223) is an iron sulfide mineral, which is abundant in nature and mostly exists in associated forms. Its surface is dark bronze yellow, and its magnetic strength varies. The strength of its magnetic force depends on the number of vacancies of iron atoms in its internal structure. It can usually be recovered by magnetic separation. The composition of pyrrhotite is relatively complex, and it is usually mixed with magnetic materials (such as iron, copper and nickel). There are almost no single crystal system pyrrhotite minerals in nature, and more than 70% are mixed crystal systems. Therefore, it is difficult to separate them using a single separation method. Since some Fe 2+ Fe 3+ Instead, in order to maintain the balance of electricity prices, 2+ Vacancies appear at the positions to form empty solid solutions. Due to the different arrangements of lattice vacancies, pyrrhotite forms many structures, with hexagonal HPO and monoclinic MPO being two common types. Due to the defects in the pyrrhotite crystal structure, it is more easily oxidized than other sulfide minerals in the presence of oxidants such as oxygen or trivalent iron ions, which is not conducive to flotation. At present, wet magnetic separation is mainly used to enrich pyrrhotite. The obtained pyrrhotite concentrate is filtered and dried before entering the boiling furnace roasting system for the preparation of sulfuric acid products, and the by-product is sulfuric acid slag.
[0003] However, the existing wet magnetic separation process uses a large amount of water, requires regular maintenance, and cannot discharge coarse-grained gangue. The overall process of pyrrhotite magnetic separation, filtration, drying, and roasting is complicated, and there are multiple transfer processes between the magnetic separation and roasting processes, which greatly increases the difficulty and complexity of operations in the actual production process, while reducing the process efficiency.
[0004] The comprehensive pyrrhotite processing system of magnetic separation, filtration, drying and roasting of pyrrhotite occupies a large area, requires large investment, and has high energy consumption. Daily maintenance and upkeep require a lot of manpower, material and financial resources, and the maintenance cost is high, which significantly increases the production cost. At the same time, the pyrrhotite processing system is composed of multiple devices. If one of the devices fails, it may affect the stability and reliability of the entire system.
[0005] Based on the above reasons, the existing pyrrhotite comprehensive processing system of magnetic separation, filtration, drying and roasting seriously affects the efficient utilization of pyrrhotite resources.
[0006] In addition, there are many magnetic iron-containing materials in nature, including magnetite, hematite, titanomagnetite and other high-iron materials, as well as recyclable solid wastes such as iron tailings, steel slag, and magnetic slag generated in industrial production processes. There is also an urgent need for a system and magnetic separation and roasting method that has a small footprint, small investment, short process, simple process flow, and complies with national industrial policies. Summary of the invention
[0007] In view of the problems in the prior art that the comprehensive treatment system of pyrrhotite occupies a large area, has a large investment, high maintenance cost, and a complicated process flow, the present invention provides a magnetic material diversion roasting device, in which magnetic poles and baffles are arranged inside an outer shell, and the mixed material enters the outer shell horizontally under the action of airflow, and the magnetic material and non-magnetic material are separated under the adsorption effect of the magnetic pole and the action of gravity, and the magnetic material is roasted in the outer shell to obtain a roasted product.
[0008] According to a first embodiment of the present invention, a magnetic material split-flow roasting device is provided.
[0009] A magnetic material splitting roasting device comprises an outer shell, a baffle and a magnetic pole. A gas-solid mixed feed port is provided at the upper part of the side wall of the outer shell. The baffle is arranged vertically inside the outer shell, and the height of the top of the baffle is not higher than the height of the lower end of the gas-solid mixed feed port. Above the top of the baffle is a magnetic separation zone, and the magnetic pole is arranged at the upper part of the magnetic separation zone, and the height of the magnetic pole is higher than the height of the upper end of the gas-solid mixed feed port. A non-magnetic material channel from top to bottom is formed between the side wall of the baffle facing the gas-solid mixed feed port and the inner side wall of the outer shell, and a non-magnetic material outlet is provided at the bottom of the non-magnetic material channel. A magnetic material conveying zone from top to bottom is formed between the side wall of the baffle facing away from the gas-solid mixed feed port and the inner side wall of the outer shell. The bottom or side of the magnetic material conveying zone is connected to the fluidized roasting zone through a transition channel. An oxidizing gas inlet is provided on the side and / or bottom of the fluidized roasting zone.
[0010] Preferably, the baffle can move laterally. Preferably, the baffle is connected to the outer shell via a slide rail.
[0011] Preferably, the baffle is a retractable structure. Preferably, 1 / 4 to 1 / 2 of the upper portion of the baffle is a retractable plate.
[0012] Preferably, the device comprises a plurality of said magnetic poles. The plurality of said magnetic poles are arranged at the upper part of the magnetic selection zone. Preferably, the plurality of said magnetic poles are evenly distributed in the horizontal direction at the upper part of the magnetic selection zone;
[0013] Preferably, the magnetism of the plurality of magnetic poles decreases in sequence in a direction away from the gas-solid mixing feed port.
[0014] Preferably, the magnetic pole is an electromagnet.
[0015] Preferably, a magnetic pole cleaning unit is provided at the magnetic pole.
[0016] Preferably, the device further comprises a sieve plate, which is disposed transversely above the baffle plate and below the gas-solid mixing feed port, and whose two ends are respectively connected to the two sides of the inner side wall of the outer shell.
[0017] Preferably, the sieve plate has a sieve hole diameter of 1 to 5 mm, preferably 1 to 3 mm.
[0018] Preferably, the sieve plate is arranged at an inclination, and the angle between the sieve plate and the horizontal plane is 5 to 45°, preferably 10 to 30°.
[0019] Preferably, a discharge port is provided at a connection between the outer shell and the lower side of the sieve plate.
[0020] Preferably, the fluidized roasting zone is arranged at the outer side of the magnetic material conveying zone or above the magnetic separation zone. Preferably, an oxidizing gas nozzle is provided at the oxidizing gas inlet. Preferably, the oxidizing gas nozzle is arranged with the gas outlet end higher than the gas inlet end. Preferably, the angle between the oxidizing gas nozzle and the horizontal plane is 15 to 75°, preferably 30 to 60°.
[0021] Preferably, a temperature monitoring unit is provided on the side wall of the fluidized roasting zone.
[0022] Preferably, a gas flow monitoring unit is provided at the gas-solid mixture feed inlet.
[0023] Preferably, a gas flow monitoring unit is provided at the oxidizing gas inlet.
[0024] According to a second embodiment of the present invention, a magnetic material split-flow roasting system is provided.
[0025] A magnetic material split flow roasting system, the system comprises a magnetic material split flow roasting device, a grinding device, a screening device, an inert gas source and an oxidizing gas source. The discharge port of the grinding device is connected to the feed port of the screening device through a pipeline. The discharge port of the screening device is connected to the gas-solid mixed feed port through a pipeline. The inert gas source is connected to the gas-solid mixed feed port through a pipeline. The oxidizing gas source is connected to the oxidizing gas inlet through a pipeline.
[0026] Preferably, the sieve hole diameter of the screening device is 0.01-1 mm, preferably 0.1-0.5 mm.
[0027] According to a third embodiment of the present invention, a split-flow roasting method for magnetic materials is provided.
[0028] A magnetic material split-flow roasting method, the method comprising the following steps:
[0029] 1) After grinding and screening, the mixed material to be split and roasted enters the magnetic material split and roasting device under the impetus of inert gas flow.
[0030] 2) In the magnetic material diversion roasting device, the non-magnetic material falls directly into the non-magnetic material channel under the action of gravity, and the magnetic material falls into the magnetic material conveying area under the influence of the upward force of the magnetic pole and gravity, and is transported to the fluidized roasting area through the transition channel.
[0031] 3) The non-magnetic material is discharged from the non-magnetic material outlet, and the magnetic material is discharged from the magnetic material outlet after the roasting is completed in the fluidized roasting zone, thereby completing the magnetic separation and split roasting of the mixed material.
[0032] Preferably, the method also includes: determining the distance between the baffle and the gas-solid mixing feed port in the horizontal direction according to the particle size of the mixed material, the content of magnetic material in the mixed material, the flow rate of the inert gas flow, the baffle height and the magnetic pole strength, so as to ensure that all non-magnetic materials fall into the non-magnetic material channel and the magnetic materials fall into the magnetic material conveying area.
[0033] In the present invention, a baffle and a magnetic pole are arranged inside the outer shell, and a gas-solid mixed feed port is opened on the side wall of the outer shell, so that the inner part of the outer shell is divided into an upper magnetic separation zone, a lower magnetic material conveying zone and a non-magnetic material channel. Under the action of the airflow, the mixed material enters the inner part of the outer shell from the gas-solid mixed feed port on the outer shell. Since the magnetic pole is arranged at the upper part of the magnetic separation zone, the magnetic material in the mixed material will be adsorbed by the magnetic pole, and the magnetic material and the non-magnetic material will also be affected by gravity. Under the action of two directions, the non-magnetic material directly falls into the non-magnetic material channel, while the horizontal movement distance of the magnetic material is farther. The magnetic material enters the magnetic material conveying zone, and then enters the fluidized roasting zone through the transition channel, and an oxidizing gas inlet is opened on the side wall or bottom wall of the fluidized roasting zone to roast the magnetic material.
[0034] In the present invention, the baffle is configured to be able to move laterally and / or retractable to meet the needs of changing the position of the upper end of the baffle and the baffle as a whole, thereby achieving adaptive adjustment under changing working conditions. For example, in the actual production process, when the material particle size, wind force, magnetic strength of the magnetic pole or material properties change, the horizontal movement distance between the non-magnetic material and the magnetic material will change. The present invention configures the baffle to be a movable and / or retractable structure to adjust the horizontal position of the baffle and / or the height of the upper end of the baffle according to the needs of the production process.
[0035] In the present invention, multiple magnetic poles can be arranged at the top of the magnetic separation zone, so that the magnetic material is continuously adsorbed by the magnetic poles and moves horizontally over a longer distance, so as to distinguish the falling areas of the magnetic material and the non-magnetic material, and determine the specific setting position of the baffle. Preferably, according to the distance from the gas-solid mixing feed port, the magnetism of the multiple magnetic poles at the top of the magnetic separation zone is controlled to gradually weaken from near to far, so as to avoid the horizontal displacement distance of the magnetic material being too long. Further preferably, an electromagnet is used as the magnetic pole, and the magnetic strength of the electromagnet can be adjusted in real time according to the specific needs in the production process.
[0036] In the present invention, the distance between the baffle and the gas-solid mixing feed port in the horizontal direction is determined according to the particle size of the mixed material, the content of the magnetic material in the mixed material, the flow rate of the inert gas flow, the height of the baffle and the magnetic pole strength, so as to ensure that all the non-magnetic materials fall into the non-magnetic material channel and the magnetic materials fall into the magnetic material conveying area. The specific calculation process is as follows:
[0037] First, in the vertical direction, it is assumed that the distance between the baffle and the lowermost end of the gas-solid mixing feed inlet is x.
[0038] To ensure that all non-magnetic materials enter the non-magnetic material channel, it is necessary to ensure that the non-magnetic materials do not exceed the baffle under the action of gravity after entering the magnetic separation zone from the top of the gas-solid mixing feed port. In the vertical direction, the non-magnetic material is only affected by gravity. At the same time, since the initial velocity of the non-magnetic material in the vertical direction is 0, the falling time of the non-magnetic material can be obtained as:
[0039]
[0040] Wherein, x is the distance between the baffle and the lower end of the gas-solid mixing feed inlet, m; z is the height of the gas-solid mixing feed inlet, m; g is the gravitational acceleration, which is 9.8 N / kg.
[0041] In addition, the initial horizontal velocity v0 of the non-magnetic material when it enters the gas-solid mixing feed inlet is measured, and the distance y1 between the baffle and the gas-solid mixing feed inlet in the horizontal direction can be obtained:
[0042] y1=v0*t1
[0043] Where, v0 is the initial velocity of the non-magnetic material in the horizontal direction, m / s. y1 is the minimum distance between the baffle and the gas-solid mixing feed inlet in the horizontal direction.
[0044] Then, to ensure that all magnetic materials enter the magnetic material conveying area, the magnetic materials entering the magnetic separation area from the bottom of the gas-solid mixing feed inlet need to pass over the baffle under the action of gravity and magnetic pole attraction. In the vertical direction, the magnetic materials are affected by gravity and magnetic pole attraction, where the magnetic pole adsorption force is:
[0045]
[0046] Where B is the magnetic field strength, T; A is the surface area of the magnet, m 2 ; μ is the magnetic permeability, which is 1; d is the distance between the magnetic material and the magnetic pole, m.
[0047] Then the acceleration of the magnetic material in the vertical direction is:
[0048]
[0049] Where, F is the adsorption force of the magnetic material by the magnetic pole, N; m is the weight of the magnetic material, kg.
[0050] At the same time, since the initial velocity of the magnetic material in the vertical direction is 0, the time it takes for the magnetic material to fall to the top of the baffle is:
[0051]
[0052] The maximum distance y2 between the baffle and the gas-solid mixing feed inlet in the horizontal direction is obtained as:
[0053] y2=v0*t2
[0054] Wherein, v0 is the initial velocity of the non-magnetic material in the horizontal direction, m / s. y2 is the maximum distance between the baffle and the gas-solid mixing feed port in the horizontal direction.
[0055] According to the above calculation, the distance y between the baffle and the gas-solid mixing feed inlet in the horizontal direction is: y1 <y<y2。
[0056] In the present invention, the height of the upper end of the baffle, the strength of the magnetic pole and other parameters can be adjusted according to the actual working conditions, and the position of the baffle in the horizontal direction can be calculated based on the adjusted parameters to achieve complete separation of non-magnetic materials and magnetic materials as much as possible, thereby improving the purity and yield of the final roasting product.
[0057] In the present invention, a sieve plate is arranged at the top of the baffle plate to screen out large particles in the mixed material, which is convenient for gas flow control in the subsequent process. Preferably, the sieve plate is arranged at an angle, and a discharge port is arranged at the connection between the sieve plate and the outer shell, and the large particles are discharged from the discharge port and sent to the grinding device for secondary grinding, thereby improving the comprehensive utilization rate of pyrrhotite.
[0058] In the present invention, a cleaning unit is provided at the magnetic pole to prevent small particles of magnetic material from moving upward and being adsorbed on the magnetic pole, thereby affecting the magnetism of the magnetic pole.
[0059] In the present invention, the fluidized roasting zone can be arranged at the outer side of the magnetic material conveying zone (such as Figure 2), the magnetic material conveying zone is connected to the fluidized roasting zone through a transition channel extending to the outside thereof. In addition, the fluidized roasting zone can also be arranged on the upper part of the magnetic material conveying zone (such as Figure 1 ), after the transition channel extends to the outside of the magnetic material conveying area, it continues to extend upward to the bottom of the fluidized roasting area. In addition, an air inlet can be set at the bottom of the transition channel outside the magnetic material conveying area, and an inert gas can be introduced to make the magnetic material therein move upward.
[0060] In the present invention, an oxidizing gas nozzle is provided at the oxidizing gas inlet, and the oxidizing nozzle is preferably provided at an angle so that the gas is ejected upward, so that the magnetic material is fluidized and roasted. In the present invention, a temperature monitoring unit and a gas flow unit are provided to further monitor the temperature and gas flow inside the magnetic material split roasting device.
[0061] Compared with the prior art, the present invention has the following beneficial effects:
[0062] 1. The present invention provides a magnetic material split roasting device and system and a method of use, which utilizes the magnetic pole above the magnetic separation zone to fully separate the magnetic material and the non-magnetic material, and then fully roasts the magnetic material in the fluidized roasting zone to obtain a roasted product, thereby realizing the integrated magnetic separation roasting of pyrrhotite. The system footprint is effectively reduced, and the investment and maintenance costs are reduced.
[0063] 2. The magnetic material diversion roasting device and system and use method provided by the present invention have a simple process flow and strong feasibility. The baffle can be adjusted according to parameters such as the properties of the mixed material, wind force, magnetic pole magnetic strength, etc. in the actual production process. The obtained roasting product has a high purity and complies with national industrial policies. BRIEF DESCRIPTION OF THE DRAWINGS
[0064] Figure 1 A structural schematic diagram of a magnetic material split-flow roasting device provided by the present invention.
[0065] Figure 2 Another structural schematic diagram of a magnetic material split-flow roasting device provided by the present invention.
[0066] Figure numerals: 1: outer shell; 2: baffle; 3: magnetic pole; 4: gas-solid mixed feed inlet; 5: non-magnetic material outlet; 6: transition channel; 7: oxidizing gas inlet; 8: sieve plate; 9: discharge port; 10: oxidizing gas nozzle; A: magnetic selection area; B: non-magnetic material channel; C: magnetic material conveying area; D: fluidized roasting area. DETAILED DESCRIPTION
[0067] The technical solution of the present invention is illustrated below by way of example, and the scope of protection requested by the present invention includes but is not limited to the following embodiments.
[0068] According to a first embodiment of the present invention, a magnetic material split-flow roasting device is provided.
[0069] A magnetic material splitting roasting device comprises an outer shell 1, a baffle 2 and a magnetic pole 3. A gas-solid mixing feed port 4 is provided at the upper part of the side wall of the outer shell 1. The baffle 2 is arranged vertically inside the outer shell 1, and the height of the top of the baffle 2 is not higher than the height of the lower end of the gas-solid mixing feed port 4. Above the top of the baffle 2 is a magnetic separation zone A, and the magnetic pole 3 is arranged at the upper part of the magnetic separation zone A, and the height of the magnetic pole 3 is higher than the height of the upper end of the gas-solid mixing feed port 4. A non-magnetic material channel B from top to bottom is formed between the side wall of the baffle 2 facing the gas-solid mixing feed port 4 and the inner side wall of the outer shell 1, and a non-magnetic material outlet 5 is provided at the bottom of the non-magnetic material channel B. A magnetic material conveying zone C from top to bottom is formed between the side wall of the baffle 2 facing away from the gas-solid mixing feed port 4 and the inner side wall of the outer shell 1. The bottom or side of the magnetic material conveying zone C is connected to the fluidized roasting zone D through a transition channel 6. The side and / or bottom of the fluidized calcining zone D is provided with an oxidizing gas inlet 7 .
[0070] Preferably, the baffle 2 can move laterally. Preferably, the baffle is connected to the outer shell 1 via a slide rail.
[0071] Preferably, the baffle is a retractable structure. Preferably, 1 / 4 to 1 / 2 of the upper portion of the baffle is a retractable plate.
[0072] Preferably, the device comprises a plurality of magnetic poles 3. The plurality of magnetic poles 3 are arranged on the upper part of the magnetic selection area A. Preferably, the plurality of magnetic poles 3 are evenly distributed in the horizontal direction on the upper part of the magnetic selection area A.
[0073] Preferably, the magnetism of the plurality of magnetic poles 3 decreases in sequence in a direction away from the gas-solid mixing feed port 4 .
[0074] Preferably, the magnetic pole 3 is an electromagnet.
[0075] Preferably, a magnetic pole cleaning unit is provided at the magnetic pole 3 .
[0076] Preferably, the device further comprises a sieve plate 8. The sieve plate 8 is transversely arranged above the baffle plate 2 and below the gas-solid mixing feed port 4. Both ends of the sieve plate 8 are connected to both sides of the inner side wall of the outer shell 1 respectively.
[0077] Preferably, the sieve plate 8 has a sieve hole diameter of 1 to 5 mm, preferably 1 to 3 mm.
[0078] Preferably, the sieve plate 8 is tilted, and the angle between the sieve plate 8 and the horizontal plane is 5 to 45°, preferably 10 to 30°.
[0079] Preferably, a discharge port 9 is provided at the connection between the outer shell 1 and the lower side of the sieve plate 8 .
[0080] Preferably, the fluidized roasting zone D is arranged at the outer side of the magnetic material conveying zone C or above the magnetic separation zone A. Preferably, an oxidizing gas nozzle 10 is provided at the oxidizing gas inlet 7 .
[0081] Preferably, the oxidizing gas nozzle 10 is tilted so that the gas outlet is higher than the gas inlet. Preferably, the angle between the oxidizing gas nozzle 10 and the horizontal plane is 15 to 75°, preferably 30 to 60°.
[0082] Preferably, a temperature monitoring unit is provided on the side wall of the fluidized roasting zone D.
[0083] Preferably, a gas flow monitoring unit is provided at the gas-solid mixture feed inlet 4 .
[0084] Preferably, a gas flow monitoring unit is provided at the oxidizing gas inlet 7 .
[0085] According to a second embodiment of the present invention, a magnetic material split-flow roasting system is provided.
[0086] A magnetic material split flow roasting system, the system comprises a magnetic material split flow roasting device, a grinding device, a screening device, an inert gas source and an oxidizing gas source. The discharge port of the grinding device is connected to the feed port of the screening device through a pipeline. The discharge port of the screening device is connected to the gas-solid mixed feed port through a pipeline. The inert gas source is connected to the gas-solid mixed feed port through a pipeline. The oxidizing gas source is connected to the oxidizing gas inlet 7 through a pipeline.
[0087] Preferably, the sieve hole diameter of the screening device is 0.01-1 mm, preferably 0.1-0.5 mm.
[0088] According to a third embodiment of the present invention, a split-flow roasting method for magnetic materials is provided.
[0089] A magnetic material split-flow roasting method, the method comprising the following steps:
[0090] 1) After grinding and screening, the mixed material to be split and roasted enters the magnetic material split and roasting device under the impetus of inert gas flow.
[0091] 2) In the magnetic material diversion roasting device, the non-magnetic material falls directly into the non-magnetic material channel under the action of gravity, and the magnetic material falls into the magnetic material conveying area under the influence of the upward force of the magnetic pole and gravity, and is transported to the fluidized roasting area through the transition channel.
[0092] 3) The non-magnetic material is discharged from the non-magnetic material outlet, and the magnetic material is discharged from the magnetic material outlet after the roasting is completed in the fluidized roasting zone, thereby completing the magnetic separation and split roasting of the mixed material.
[0093] Preferably, the method also includes: determining the distance between the baffle and the gas-solid mixing feed port in the horizontal direction according to the particle size of the mixed material, the content of magnetic material in the mixed material, the flow rate of the inert gas flow, the baffle height and the magnetic pole strength, so as to ensure that all non-magnetic materials fall into the non-magnetic material channel and the magnetic materials fall into the magnetic material conveying area.
[0094] Example 1
[0095] A magnetic material splitting roasting device comprises an outer shell 1, a baffle 2 and a magnetic pole 3. A gas-solid mixing feed port 4 is provided at the upper part of the side wall of the outer shell 1. The baffle 2 is arranged vertically inside the outer shell 1, and the height of the top of the baffle 2 is not higher than the height of the lower end of the gas-solid mixing feed port 4. Above the top of the baffle 2 is a magnetic separation zone A, and the magnetic pole 3 is arranged at the upper part of the magnetic separation zone A, and the height of the magnetic pole 3 is higher than the height of the upper end of the gas-solid mixing feed port 4. A non-magnetic material channel B from top to bottom is formed between the side wall of the baffle 2 facing the gas-solid mixing feed port 4 and the inner side wall of the outer shell 1, and a non-magnetic material outlet 5 is provided at the bottom of the non-magnetic material channel B. A magnetic material conveying zone C from top to bottom is formed between the side wall of the baffle 2 facing away from the gas-solid mixing feed port 4 and the inner side wall of the outer shell 1. The bottom of the magnetic material conveying zone C is connected to the fluidized roasting zone D through a transition channel 6. The side of the fluidized calcining zone D is provided with an oxidizing gas inlet 7 .
[0096] Example 2
[0097] The embodiment 1 is repeated, except that the baffle 2 can move laterally. The baffle is connected to the outer shell 1 via a slide rail.
[0098] Example 3
[0099] The second embodiment is repeated, except that the baffle is a retractable structure. The upper 1 / 2 of the baffle is a retractable plate.
[0100] Example 4
[0101] Repeat Example 3, except that the device includes five magnetic poles 3. The five magnetic poles 3 are evenly distributed in the horizontal direction above the magnetic selection area A.
[0102] In the direction away from the gas-solid mixing feed port 4, the magnetism of the five magnetic poles 3 decreases in sequence.
[0103] Example 5
[0104] Example 4 is repeated, except that the magnetic pole 3 is an electromagnet.
[0105] A magnetic pole cleaning unit is provided at the magnetic pole 3 .
[0106] Example 6
[0107] The embodiment 5 is repeated, except that the device further comprises a sieve plate 8. The sieve plate 8 is transversely arranged above the baffle plate 2 and below the gas-solid mixing feed port 4. Both ends of the sieve plate 8 are connected to both sides of the inner side wall of the outer shell 1 respectively.
[0108] The sieve plate 8 has a sieve hole diameter of 2 mm.
[0109] Example 7
[0110] Example 6 is repeated, except that the sieve plate 8 is tilted, and the angle between the sieve plate 8 and the horizontal plane is 15°.
[0111] A discharge port 9 is provided at the connection between the outer shell 1 and the lower side of the sieve plate 8 .
[0112] Example 8
[0113] Example 7 was repeated, except that the fluidized roasting zone D was arranged outside the magnetic material conveying zone C.
[0114] Example 9
[0115] Example 7 was repeated, except that the fluidized roasting zone D was arranged above the magnetic separation zone A.
[0116] Example 10
[0117] Example 9 is repeated, except that an oxidizing gas nozzle 10 is provided at the oxidizing gas inlet 7. The oxidizing gas nozzle 10 is tilted so that the gas outlet end is higher than the gas inlet end. The angle between the oxidizing gas nozzle 10 and the horizontal plane is 45°.
[0118] Embodiment 11
[0119] Example 10 was repeated, except that a temperature monitoring unit was provided on the side wall of the fluidized roasting zone D.
[0120] A gas flow monitoring unit is provided at the gas-solid mixing feed inlet 4 .
[0121] A gas flow monitoring unit is provided at the oxidizing gas inlet 7 .
[0122] Example 12
[0123] A magnetic material split flow roasting system, the system comprises the magnetic material split flow roasting device described in Example 11, a grinding device, a screening device, an inert gas source and an oxidizing gas source. The discharge port of the grinding device is connected to the feed port of the screening device through a pipeline. The discharge port of the screening device is connected to the gas-solid mixed feed port through a pipeline. The inert gas source is connected to the gas-solid mixed feed port through a pipeline. The oxidizing gas source is connected to the oxidizing gas inlet 7 through a pipeline.
[0124] The sieve hole diameter of the sieving device is 0.3 mm.
[0125] Application Example 1
[0126] The system described in Example 12 is used to separate and roast the mixed material containing 50% magnetic material. The specific method is as follows:
[0127] 1) The mixed material to be split and roasted is ground and sieved in turn to obtain a small particle mixed material with a particle size of less than or equal to 0.3 mm. The small particle mixed material is added to the magnetic material split roasting device described in Example 11 under the driving action of a nitrogen gas flow of 4.7 m / s.
[0128] 2) In the magnetic material splitting roasting device, the non-magnetic material falls directly into the non-magnetic material channel under the action of gravity, and the magnetic material channel falls into the magnetic material conveying area under the influence of the upward force of the magnetic pole and gravity, and is conveyed to the fluidized roasting area through the transition channel;
[0129] 3) The non-magnetic material is discharged from the non-magnetic material outlet, and the magnetic material is discharged from the magnetic material outlet after the roasting is completed in the fluidized roasting zone, thereby completing the magnetic separation and split roasting of the mixed material.
[0130] The method further comprises:
[0131] In the vertical direction, the distance between the baffle and the lowest end of the gas-solid mixed feed inlet is x=2m. To ensure that all non-magnetic materials enter the non-magnetic material channel, it is necessary to ensure that the non-magnetic materials do not exceed the baffle under the action of gravity after entering the magnetic separation area from the upper end of the gas-solid mixed feed inlet. In the vertical direction, the non-magnetic material is only affected by gravity. At the same time, since the initial velocity of the non-magnetic material in the vertical direction is 0, the falling time of the non-magnetic material can be obtained as:
[0132]
[0133] Wherein, x is the distance between the baffle and the lower end of the gas-solid mixing feed inlet, which is 2m; z is the height of the gas-solid mixing feed inlet, which is 5m; g is the gravitational acceleration, which is 9.8N / kg.
[0134] In addition, it is measured that when the non-magnetic material enters from the gas-solid mixing feed port, the initial velocity in the horizontal direction v0 = 4.7 m / s. It can be obtained that in the horizontal direction, the distance y1 between the baffle and the gas-solid mixing feed port is:
[0135] y1=v0*t1=5.64m
[0136] Where, v0 is the initial velocity of the non-magnetic material in the horizontal direction, which is 4.7 m / s. y1 is the minimum distance between the baffle and the gas-solid mixing feed inlet in the horizontal direction.
[0137] Then, to ensure that all magnetic materials enter the magnetic material conveying area, the magnetic materials entering the magnetic separation area from the bottom of the gas-solid mixing feed inlet need to pass over the baffle under the action of gravity and magnetic pole attraction. In the vertical direction, the magnetic materials are affected by gravity and magnetic pole attraction, where the magnetic pole adsorption force is:
[0138]
[0139] Where B is the magnetic field strength, which is 3.5A / m; A is the surface area of the magnet, which is 3m 2 ; μ is the magnetic permeability, which is 1; d is the distance between the magnetic material and the magnetic pole, which is 6.3m.
[0140] Then the acceleration of the magnetic material in the vertical direction is:
[0141]
[0142] Where F is the adsorption force of the magnetic material by the magnetic pole, N; m is the weight of the magnetic material, which is 0.05 kg.
[0143] At the same time, since the initial velocity of the magnetic material in the vertical direction is 0, the time it takes for the magnetic material to fall to the top of the baffle is:
[0144]
[0145] The maximum distance y2 between the baffle and the gas-solid mixing feed inlet in the horizontal direction is obtained as:
[0146] y2=v0*t2=8.6m
[0147] Wherein, v0 is the initial velocity of the non-magnetic material in the horizontal direction, m / s. y2 is the maximum distance between the baffle and the gas-solid mixing feed port in the horizontal direction.
[0148] According to the above calculation, the distance y between the baffle and the gas-solid mixing feed inlet in the horizontal direction is: 5.64m <y<8.6m。
[0149] The horizontal distance between the baffle and the gas-solid mixed feed port is adjusted to 6m, and the mixed material entering the magnetic material diversion and roasting device is diverted, and the mixed material is roasted with the magnetic material to obtain a roasted product. The iron oxide content in the roasted product is 98.7%, and the yield is 97.2%. In addition, the recovery rate of non-magnetic materials is 99.8%.
[0150] Example 1 was repeatedly applied, except that the distance between the baffle and the gas-solid mixed feed port was changed to divert and roast the magnetic material. The iron oxide content of the roasted product was detected and the yield was calculated. At the same time, the recovery rate of the non-magnetic material was calculated. The results are shown in Table 1.
[0151] Table 1
[0152]
[0153] According to Examples 1 to 6, in the actual production process, the distance between the baffle and the gas-solid mixed feed port is calculated and controlled by factors such as the baffle height and the magnetic pole strength, which can effectively improve the purity and yield of iron oxide in the roasting product, fully separate the magnetic material and the non-magnetic material, and realize integrated magnetic separation roasting.
Claims
1. A magnetic material splitting roasting device, Features: The device comprises an outer shell (1), a baffle (2) and a magnetic pole (3); a gas-solid mixed feed inlet (4) is provided at the upper part of the side wall of the outer shell (1); the baffle (2) is arranged vertically inside the outer shell (1), and the height of the top of the baffle (2) is not higher than the height of the lower end of the gas-solid mixed feed inlet (4); a magnetic separation zone (A) is located above the top of the baffle (2), and the magnetic pole (3) is arranged at the upper part of the magnetic separation zone (A), and the height of the magnetic pole (3) is higher than the height of the upper end of the gas-solid mixed feed inlet (4); the baffle (2) is oriented toward the gas-solid mixed feed inlet (4 ) on one side and the inner side wall of the outer shell (1) form a non-magnetic material channel (B) from top to bottom, and a non-magnetic material outlet (5) is provided at the bottom of the non-magnetic material channel (B); a magnetic material conveying zone (C) is formed from top to bottom between the side wall of the baffle (2) on the side away from the gas-solid mixing feed port (4) and the inner side wall of the outer shell (1); the bottom or side of the magnetic material conveying zone (C) is connected to the fluidized roasting zone (D) through a transition channel (6); and an oxidizing gas inlet (7) is provided on the side and / or bottom of the fluidized roasting zone (D).
2. The device according to claim 1, Features: The baffle (2) can move laterally; preferably, the baffle is connected to the outer shell (1) via a slide rail; and / or The baffle is a retractable structure; preferably, 1 / 4 to 1 / 2 of the upper portion of the baffle is a retractable plate.
3. The device according to claim 1 or 2, Features: The device comprises a plurality of magnetic poles (3); the plurality of magnetic poles (3) are arranged at the upper part of the magnetic selection area (A); preferably, the plurality of magnetic poles (3) are evenly distributed in the horizontal direction of the upper part of the magnetic selection area (A); Preferably, the magnetic properties of the plurality of magnetic poles (3) decrease in sequence in a direction away from the gas-solid mixing feed port (4); Preferably, the magnetic pole (3) is an electromagnet; Preferably, a magnetic pole cleaning unit is provided at the magnetic pole (3).
4. The device according to any one of claims 1 to 3, Features: The device further comprises a sieve plate (8); the sieve plate (8) is transversely arranged above the baffle plate (2) and below the gas-solid mixing feed port (4); the two ends of the sieve plate (8) are respectively connected to the two sides of the inner side wall of the outer shell (1); Preferably, the sieve hole diameter of the sieve plate (8) is 1 to 5 mm, preferably 1 to 3 mm.
5. The device according to any one of claims 1 to 4, Features: The sieve plate (8) is arranged obliquely, and the angle between the sieve plate (8) and the horizontal plane is 5 to 45°, preferably 10 to 30°; Preferably, a discharge port (9) is provided at the connection between the outer shell (1) and the lower side of the sieve plate (8).
6. The device according to claim 5, Features: The fluidized roasting zone (D) is arranged on the outer side of the magnetic material conveying zone (C) or above the magnetic separation zone (A); preferably, an oxidizing gas nozzle (10) is provided at the oxidizing gas inlet (7).
7. The device according to claim 6, Features: The oxidizing gas nozzle (10) is tilted so that the gas outlet end is higher than the gas inlet end; preferably, the angle between the oxidizing gas nozzle (10) and the horizontal plane is 15 to 75°, preferably 30 to 60°.
8. The device according to any one of claims 1 to 7, Features: A temperature monitoring unit is provided on the side wall of the fluidized roasting zone (D); and / or A gas flow monitoring unit is provided at the gas-solid mixing feed port (4); and / or A gas flow monitoring unit is provided at the oxidizing gas inlet (7).
9. A magnetic material split-flow roasting system, Features: The system comprises a magnetic material split-flow roasting device, a grinding device, a screening device, an inert gas source and an oxidizing gas source as described in any one of claims 1 to 8; the discharge port of the grinding device is connected to the feed port of the screening device through a pipeline; the discharge port of the screening device is connected to the gas-solid mixed feed port through a pipeline; the inert gas source is connected to the gas-solid mixed feed port through a pipeline; the oxidizing gas source is connected to the oxidizing gas inlet through a pipeline; Preferably, the sieve hole diameter of the screening device is 0.01-1 mm, preferably 0.1-0.5 mm.
10. A method for split-flow roasting of magnetic materials or a method applied to the system of claim 9, Features: The method comprises the following steps: 1) After grinding and screening, the mixed material to be split and roasted enters the magnetic material split and roasting device under the driving action of the inert gas flow; 2) In the magnetic material split-flow roasting device, the non-magnetic material falls directly into the non-magnetic material channel under the action of gravity, and the magnetic material falls into the magnetic material conveying area under the influence of the upward force of the magnetic pole and gravity, and is transported to the fluidized roasting area through the transition channel; 3) The non-magnetic material is discharged from the non-magnetic material outlet, and the magnetic material is discharged from the magnetic material outlet after the roasting is completed in the fluidized roasting zone, thus completing the magnetic separation and split roasting of the mixed material; Preferably, the method also includes: determining the distance between the baffle and the gas-solid mixing feed port in the horizontal direction according to the particle size of the mixed material, the content of magnetic material in the mixed material, the flow rate of the inert gas flow, the baffle height and the magnetic pole strength, so as to ensure that all non-magnetic materials fall into the non-magnetic material channel and the magnetic materials fall into the magnetic material conveying area.
Citation Information
Cited By
Dry grinding beneficiation method and system for refractory hematite
CN119456158A