A technology of polymetallic oxide ore and recovery method, which is applied in chemical instruments and methods, wet separation, solid separation, etc., can solve the problems of slime, low ore grade, and inability to use directly, so as to improve the recovery rate and improve the taste. , significant economic and social benefits
Patent Information
- Authority / Receiving Office
- CN · China
- Current Assignee / Owner
- Publication Date
- 2009-12-30
Smart Images
Figure 1
Abstract
Description
technical field
[0001] The invention relates to a method for comprehensive recovery of quartz vein polymetallic oxide ore resources, which belongs to the technical field of mineral processing. Background technique
[0002] At present, the existing technologies in the field of mineral processing are all developing and researching on primary ore, and the development of primary ore is relatively mature, because primary ore has the characteristics of easy mineral processing, high enrichment ratio, simple process, and low cost. Compared with primary ores, polymetallic oxide ores have a high oxidation rate and serious muddying, making it difficult to concentrate and collect, which is a major technical problem at home and abroad. In addition, due to the low grade of ores, they cannot be directly used, so they are all regarded as " "Stay ore" treatment or direct abandonment cannot produce economic benefits. At present, there is still no effective method to recover various metals in ...
Examples
Embodiment 1
[0018] Embodiment 1: the comprehensive recovery method of quartz vein polymetallic oxide ore resources according to the present invention comprises the following steps: (1) crushing and grinding the raw ore of quartz vein polymetallic oxide ore, and then carrying out flotation, the The agent added in the first step flotation is the regulator sodium sulfide 150g / t 原矿 , slime dispersant water glass 100g / t 原 矿 , sodium hexametaphosphate 100g / t 原矿 , Inhibitor kerosene 200g / t 原矿 , sodium oleate 100g / t 原矿 , active agent copper sulfate 100g / t 原矿 , Foaming agent No. 2 oil 100g / t 原矿 , collector black medicine 50g / t 原矿 And collector xanthate 100g / t 原矿 , separated into molybdenum concentrate and tailings; (2) adding sodium carbonate 100kg / t to molybdenum concentrate 钼精矿 And sodium hydroxide 25kg / t 钼精矿 , control the PH value to 11, form leaching residue and immersion liquid, use carbon slurry method to extract alloy gold from leaching residue, and the agent used for carbon slurry...
Embodiment 2
[0019] Embodiment 2: the comprehensive recovery method of quartz vein polymetallic oxide ore resources according to the present invention comprises the following steps: (1) crushing and grinding the raw ore of quartz vein polymetallic oxide ore, and then carrying out flotation, the The agent added in the first step flotation is the regulator sodium sulfide 600g / t 原矿 , Slime dispersant water glass 200g / t 原 矿 , sodium hexametaphosphate 200g / t 原矿 , Inhibitor kerosene 500g / t 原矿 , sodium oleate 100g / t 原矿 , active agent copper sulfate 300g / t 原矿 , Foaming agent No. 2 oil 300g / t 原矿 , collector black medicine 150g / t 原矿 And collector xanthate 300g / t 原矿 , separated into molybdenum concentrate and tailings; (2) Add sodium carbonate 200kg / t to molybdenum concentrate 钼精矿 And sodium hydroxide 60kg / t 钼精矿 , control the PH value to 12, form the leaching residue and the leaching liquid, and extract alloy gold from the leaching residue by the carbon slurry method, and the agent used for ...
Embodiment 3
[0020] Embodiment 3: the comprehensive recovery method of quartz vein polymetallic oxide ore resources according to the present invention comprises the following steps: (1) crushing and grinding the raw ore of quartz vein polymetallic oxide ore, and then carrying out flotation, the The agent added in the first step flotation is the regulator sodium sulfide 1000g / t 原矿 , Slime dispersant water glass 300g / t 原矿 , sodium hexametaphosphate 300g / t 原矿 , Inhibitor kerosene 800g / t 原矿 , sodium oleate 300g / t 原矿 , active agent copper sulfate 500g / t 原矿 , Foaming agent No. 2 oil 500g / t 原矿 , collector black medicine 300g / t 原矿 And collector xanthate 500g / t 原矿 , separated into molybdenum concentrate and tailings; (2) Add sodium carbonate 300kg / t to molybdenum concentrate 钼精矿 And sodium hydroxide 100kg / t 钼精矿 , control the PH value to 14, form leaching residue and immersion liquid, use carbon slurry method to extract alloy gold from leaching residue, and the agent used for carbon slurry e...