A kind of water washing liquid for primary treatment of exhaust gas in refinery
A refinery waste gas and water washing technology, which is applied in water/sewage treatment, adsorbed water/sewage treatment, water/sludge/sewage treatment, etc. It can solve problems such as increased treatment costs, different content of waste gas components, and failure to meet emission standards. , to reduce the difficulty of post-processing, easy to use, and reduce the cost of post-processing
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Publication Date
- 2018-02-09
Abstract
Description
Technical field:
[0001] The invention relates to the technical field of waste gas treatment, in particular to a water washing liquid for primary treatment of waste gas in a refinery. Background technique:
[0002] Refinery exhaust gas is mainly discharged from heating furnaces and chimneys, as well as the exhaust gas discharged by heating and burning fuel through oil refining. The main pollutants are nitrogen oxides and sulfur dioxide. If the exhaust gas is directly discharged into the air, it will directly affect the air quality and pollute the environment. Therefore, in recent years, the treatment and emission standards for the refinery exhaust gas have become stricter. At present, there are many treatment methods for refinery exhaust gas, but most of them have the problems of complicated treatment steps and poor treatment process stability, resulting in different component content of the final treatment exhaust gas, and even some of the exhaust gas cannot meet the emission sta...
Examples
Embodiment 1
[0014] (1) Add 5 parts of silica gel powder and 4 parts of polyacrylamide to 120 parts of n-butanol, heat to reflux for 10 minutes, then add 5 parts of calcium stearate and 2 parts of sodium silicate, and continue to reflux for 5 minutes , Get material I;
[0015] (2) Add 10 parts of sodium carboxymethyl cellulose and 8 parts of lauryl alcohol polyoxyethylene ether to 800 parts of water, stir to form a uniform solution, then add 4 parts of glucoside and 1 part of urea, mix well and keep at 0-5℃ Let it stand for 8h, and then get material II;
[0016] (3) Add material I, 15 parts of fumed white carbon black, 12 parts of nano montmorillonite powder, 10 parts of polyaluminum chloride, 6 parts of molecular sieve powder and 8 parts of ferric sulfate to material II, mix well and add to the ball mill, Ball mill to fineness less than 50μm.
Embodiment 2
[0018] (1) Add 8 parts of silica gel powder and 5 parts of polyacrylamide to 150 parts of n-butanol, heat to reflux for 10 minutes, then add 3 parts of calcium stearate and 3 parts of sodium silicate, and continue to reflux for 5 minutes , Get material I;
[0019] (2) Add 12 parts of sodium carboxymethyl cellulose and 6 parts of polyoxyethylene laureth to 1000 parts of water, stir to form a uniform solution, then add 6 parts of glucoside and 2 parts of urea, mix well and keep at 0-5℃ Let it stand for 8h, and then get material II;
[0020] (3) Add material I, 20 parts of fumed white carbon black, 10 parts of nano montmorillonite powder, 15 parts of polyaluminum chloride, 8 parts of molecular sieve raw powder and 5 parts of ferric sulfate to material II, mix well and add to the ball mill, Ball mill to fineness less than 50μm.