Metal organic complex and application of metal organic complex in organic electronic device

An organic electronic device, metal organic technology

CN107629087AActive Publication Date: 2018-01-26JIANGSU UNIV OF SCI & TECH
0 Cites 2 Cited by

Patent Information

Authority / Receiving Office
CN · China
Current Assignee / Owner
Publication Date
2018-01-26

Smart Images

  • Figure 1
    Figure 1
  • Figure 2
    Figure 2
  • Figure 3
    Figure 3
Patent Text Reader

Abstract

The invention provides a metal organic complex, which is the double-core metal complex taking 2-pyrimidine-benzimidazole as a bridging ligand, wherein two central metals are independent transitional metal elements. The invention also provides an application of the metal organic complex in an organic electronic device, and the organic electronic device can be an organic light-emitting diode, an organic photovoltaic battery, an organic field effect transistor, an organic luminous field effect transistor, an organic laser, an organic spinning-electron device, an organic sensor or an organic plasmon emission diode. The double-core metal complex has two luminescence centers, and can effectively increase the luminescence efficiency of the complex and the performance of the corresponding devices.
Need to check novelty before this filing date? Find Prior Art

Description

technical field

[0001] The invention relates to an organic luminescent material, especially a metal-organic complex and its application in organic electronic devices. Background technique

[0002] Organic light-emitting diodes (OLEDs) have great potential for applications in optoelectronic devices such as flat panel displays and lighting due to the synthetic versatility, relatively low fabrication cost, and excellent optical and electrical properties of organic semiconductor materials.

[0003] In order to improve the luminous efficiency of organic light-emitting diodes, various light-emitting material systems based on fluorescence and phosphorescence have been developed. Organic light-emitting diodes using fluorescent materials have the characteristics of high reliability, but their internal electroluminescence quantum The efficiency is limited to 25%, because the probability ratio of excitons to generate singlet excited states and triplet excited states is 1:3. In 1999, Pr...

Examples

Embodiment 1

[0027] The metal-organic complex represented by chemical formula (101) is prepared through the following processes:

[0028]

[0029] (1) Synthesis of intermediate iridium dichloro bridge Ir-Cl:

[0030] Place 2-phenylpyridine (11.32g, 72.9mmol) and iridium trichloride hydrate (10.48g, 30mmol) in a dry two-necked flask, vacuumize and nitrogen cycle three times, then add 360mL ethylene glycol monoethyl ether and A mixed solution of 120 mL of water was stirred and reacted at 110° C. for 24 hours, cooled to room temperature, filtered with suction, washed with n-hexane, and dried to obtain 12.8 g of a yellow solid with a yield of 80%. No further purification was required, and the reaction was directly carried out in the next step.

[0031] (2) Synthesis of intermediate complex L-1:

[0032] Place 2-cyanopyrimidine (0.315g, 3mmol) and 1,2-phenylenediamine (0.32g, 3mmol) in a dry two-necked flask, stir and react at 160°C for 2 hours under nitrogen atmosphere, and cool to room te...

Embodiment 2

[0044] Fabrication and Characterization of Organic Light Emitting Diode (OLED) Devices:

[0045] The fabrication steps of an OLED device with ITO / PEDOT:PSS(40nm) / / EML(80nm) / TPBi(30nm) / LiF(1nm) / Al(120nm) / cathode are as follows:

[0046] 1) The ITO was ultrasonically treated with an aqueous solution containing 5% Decon90 cleaning solution for 30 minutes, then ultrasonically cleaned several times with deionized water, then ultrasonically cleaned with isopropanol, and dried with nitrogen; treated under oxygen plasma for 5 minutes to clean the ITO surface and enhance the work function of the ITO electrode;

[0047] 2) Spin-coat PEDOT:PSS (CLEVIOS P VP AI 4083) solution on the ITO treated in step 1) to obtain a 40nm film, and anneal at 150°C in air for 20 minutes after spin-coating;

[0048] 3) First poly(9-vinylcarbazole) (PVK), polybutadiene (PBD), and the dinuclear iridium complex Ir-Ir obtained in Example 1 were dissolved in toluene according to the ratio of 70:30:15, The conc...