Method for manufacturing packaging film
By manufacturing spacer chambers in the packaging film and filling fluids, the problem of volume increase caused by air chamber closure is solved, the volume reduction of the gas chamber and the thermal insulation is improved, and the high logistics cost and thermal insulation in the prior art are solved. A problem of insufficient.
Patent Information
- Application Number
- CN202210237462.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2017-08-18
- Filing Date
- 2018-08-17
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2038-08-17
AI Technical Summary
When used, the volume of the existing bubble packaging film increases due to the enclosure of the air chamber, resulting in high logistics costs. In order to minimize the volume, the packaging film needs to be cut or needle-punched, which affects the thermal insulation and storage properties.
By producing a molded film that forms the lower and side open air chambers at intervals, the gas chamber is filled with fluid and closed, and then the fluid is discharged in the closed state, and the molded film, the lower film and the upper film are wound to achieve the gas chamber. Minimize volume without cutting or needle puncture.
Without cutting or needle-punching the air chamber, the thermal insulation is greatly improved and the volume of the packaging film is reduced, which is convenient for storage and handling, and saves logistics costs.
Smart Images

Figure CN114654865B_ABST
Abstract
Description
[0001] This application is a divisional application of the Chinese invention patent application with application number 201880052241.7, application date August 17, 2018, and invention name “Method for manufacturing packaging film”. Technical Field
[0002] The present invention relates to a method for manufacturing a packaging film which can not only greatly improve heat insulation but also minimize the volume of the air cell without cutting or opening a part of the air cell by needle punching, thereby facilitating storage and transportation. Background Art
[0003] Packaging materials usually not only make the appearance of the packaged items more beautiful, but also protect the packaged items from external impacts, etc., especially when packaging electrical and electronic products or automobile parts such as bumpers, fenders and doors. Generally, a first foam paper film or bubble packaging film is used inside the carton to isolate the electrical and electronic products or automobile parts from the inner and outer sides of the carton wall, thereby absorbing and alleviating external impact forces that may be applied to the packaged items.
[0004] When bubble packaging film is used, the bubbles enclosed in air chamber units will inevitably lead to an increase in volume and thus further lead to the problem of excessively high logistics costs such as distribution.
[0005] In order to solve the above-mentioned problems, the applicant has proposed a method for manufacturing a packaging film that can not only significantly save logistics costs by minimizing the volume during storage and transportation, but also significantly improve the thermal insulation and storage properties through Korean Registered Patent Gazette Registration No. 10-1752100 (hereinafter referred to as "Prior Art 1"), Korean Registered Patent Gazette Registration No. 10-1752101 (hereinafter referred to as "Prior Art 2") and Korean Patent Application Application No. 10-2016-0117724 (hereinafter referred to as "Prior Art 3").
[0006] However, the prior arts 1 and 2 require cutting the other side of the packaging film to discharge the fluid in the packaging film to the outside in order to minimize the volume of the packaging film, while the prior art 3 requires cutting or puncturing a portion of the packaging film in order to minimize the volume of the packaging film. Summary of the invention
[0007] The object of the present invention is to solve the above-mentioned existing problems and provide a method for manufacturing a packaging film that can not only greatly improve the thermal insulation but also minimize the volume of the air cell without cutting or puncturing a part of the air cell, thereby facilitating storage and transportation.
[0008] In order to achieve the above-mentioned purpose, the present invention provides a method for manufacturing a packaging film, the method comprising: a) a step of manufacturing a molding film in which a plurality of air chambers are formed at a certain interval and are open on the lower side and one side and protrude upward; b) a step of joining a lower side film having one end portion longer than one end portion of the molding film to the lower side of the molding film in a manner in which one side of the plurality of air chambers of the molding film is open; c) a step of filling a fluid into the interior of the plurality of air chambers of the molding film in a manner in which the plurality of air chambers are convexly expanded; d) a step of closing one side of the plurality of air chambers of the molding film in a manner in which the plurality of air chambers are convexly expanded; e) a step of joining an upper side film to the upper portion of the plurality of air chambers in a manner in which the upper portion of the space between the plurality of convexly expanded air chambers is closed; f) a step of releasing the closed state of the plurality of air chambers and discharging the fluid from the interior of the plurality of air chambers; and g) a step of roll-winding the molding film, the lower side film and the upper side film onto the outer surface of a winding roller.
[0009] Preferably, the molded film in step a) is produced by melt-extruding a thermoplastic synthetic resin onto an embossing roll having molded grooves having a shape corresponding to the air cells formed at regular intervals on its outer peripheral surface.
[0010] Preferably, the lower film in step b) is joined to the molded film by a lower film roller and a lower film squeezing roller, wherein the lower film roller rolls up the lower film, and the lower film squeezing roller squeezes the lower film rolled out from the lower film roller on the embossing roller.
[0011] Preferably, the molded film in step a) is manufactured using an embossing roller having molded grooves having shapes corresponding to the air cells formed at regular intervals on the outer peripheral surface.
[0012] Preferably, the lower film in step b) is joined to the molded film by a lower film roller, an adhesive coating unit, and a lower film squeezing roller. The lower film roller rolls up the lower film, the adhesive coating unit applies adhesive to the lower film rolled out from the lower film roller at a certain interval, and the lower film squeezing roller squeezes the lower film rolled out from the lower film roller on the embossing roller.
[0013] Preferably, in the above step b), one side and the other side of the plurality of air cells of the above formed film are all open.
[0014] Preferably, in the above step c), the fluid is temporarily filled into the interior of the plurality of air chambers using a fluid injector for injecting the fluid into the interior of the plurality of air chambers.
[0015] Preferably, in the step d), in a state where the interiors of the plurality of air chambers are temporarily filled with a fluid, the plurality of air chambers are temporarily closed when passing through a pressing portion that presses one side of the plurality of air chambers.
[0016] Preferably, in the step d), the plurality of air chambers are temporarily closed when passing through a pressing portion that presses one side and the other side of the plurality of air chambers while the fluid is temporarily filled inside the plurality of air chambers.
[0017] Preferably, the extrusion unit is composed of a flatbed conveyor.
[0018] Preferably, the upper film in step e) is joined to the plurality of air chambers by an upper film roller, an adhesive coating unit and an upper film squeezing roller. The upper film roller rolls up the upper film, the adhesive coating unit applies adhesive to the upper film rolled out from the upper film roller at a certain interval, and the upper film squeezing roller squeezes the upper film rolled out from the upper film roller onto the plurality of air chambers.
[0019] The present invention can not only greatly improve the heat insulation, but also minimize the volume of the air chamber without cutting or opening a part of the air chamber by needle punching, thereby facilitating storage and transportation. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 This is a block diagram schematically illustrating a manufacturing process of a packaging film manufacturing method according to an embodiment of the present invention.
[0021] Figure 2 This is a side view schematically showing a manufacturing process of a method for manufacturing a packaging film according to an embodiment of the present invention.
[0022] Figure 3 This is a perspective view schematically illustrating an example of joining a molded film and a lower film using an embossing roller and a lower film roller in one embodiment.
[0023] Figure 4 This is a perspective view schematically illustrating another example of joining a molded film and a lower film using an embossing roller and a lower film roller in one embodiment.
[0024] Figure 5 The present invention schematically illustrates an example of a process of sealing a plurality of air chambers while the plurality of air chambers are filled with fluid. Figure 3 Cross-sectional view along line AA.
[0025] Figure 6 The present invention schematically illustrates another example of a process for sealing a plurality of air chambers while the plurality of air chambers are filled with fluid. Figure 4 Cross-sectional view along line BB in FIG.
[0026] Figure 7 Each of the perspective views schematically illustrates a state where an upper film is bonded to a plurality of air cells of a molded film in one embodiment.
[0027] Figure 8 This is a partially enlarged side view showing an enlarged process of winding the molded film, the lower film, and the upper film on a winding roll in a squeezed state.
[0028] Fig. 9 This is a side view schematically showing a manufacturing process of a method for manufacturing a packaging film according to another embodiment of the present invention.
[0029] Fig.10 This is a perspective view schematically illustrating a molded film and a lower film that are joined to each other by an embossing roll and a lower film roll in another embodiment.
[0030] Fig.11 This is a perspective view schematically illustrating a molded film and a lower film that are joined to each other by an embossing roll and a lower film roll in another embodiment.
[0031] Fig.12 This is a perspective view schematically showing a state in which an upper film is bonded to a plurality of air cells of a molded film in another embodiment.
[0032] Figures 13 to 17 This is a perspective view schematically showing a state in which a molding film, a lower film, and an upper film are joined in a state in which a check valve is provided. DETAILED DESCRIPTION
[0033] Next, the preferred embodiments applicable to the present invention will be described in detail with reference to the accompanying drawings. The scope of the claims of the present invention is not limited to the embodiments described below, and a person having general knowledge in the relevant technical field can make various modifications without departing from the technical spirit of the present invention.
[0034] Figure 1 This is a block diagram schematically illustrating a manufacturing process of a packaging film manufacturing method according to an embodiment of the present invention.
[0035] A method for manufacturing a packaging film according to an embodiment of the present invention is as follows Figure 1 As shown, it generally includes: a) a forming film manufacturing step (hereinafter referred to as "step a)"), b) a lower side film joining step (hereinafter referred to as "step b)"), c) a fluid filling step (hereinafter referred to as "step c)"), d) an air chamber sealing step (hereinafter referred to as "step d)") and e) an upper side film joining step (hereinafter referred to as "step e)").
[0036] Figure 2 This is a side view schematically illustrating a manufacturing process of a method for manufacturing a packaging film according to one embodiment of the present invention. Figure 3 This is a perspective view schematically illustrating an example of bonding a molded film and a lower film using an embossing roller and a lower film roller in one embodiment. Figure 4 This is a perspective view schematically illustrating another example of joining a molded film and a lower film using an embossing roller and a lower film roller in one embodiment.
[0037] First, the above step a) is as Figure 3 as well as Figure 4 1 and 2 , which are steps for manufacturing a molded film 10 in which a plurality of air cells 110 are formed at predetermined intervals.
[0038] The plurality of air cells 110 protruding toward the upper portion of the molding film 10 may be formed at a predetermined interval from the front side to the rear side of the molding film 10 .
[0039] As an example, Figure 2 As shown, the molded film 10 can be manufactured by supplying a thermoplastic synthetic resin melt-extruded from a T-die (not shown) to an embossing roll 100 having molded grooves 111 having a shape corresponding to the air cells 110 formed at regular intervals on its outer circumference.
[0040] Next, the above step b) is Figure 3 as well as Figure 4 As shown, the lower film 20 is melt-bonded to the lower side of the molded film 10 in a manner that the plurality of air cells 110 of the molded film 10 are open.
[0041] In order to more conveniently equip one side of the lower side membrane 20 with the check valve 40 described later, one end of the lower side membrane 20 is extended longer toward the outside of one side of the molding membrane 10 relative to one end of the molding membrane 10, so that the left-right length from one side of the lower side membrane 20 to the other side is greater than the left-right length from one side of the molding membrane 10 to the other side.
[0042] As an example, Figure 3 As shown, in the step b), the lower film 20 may be welded and joined to the lower side of the molded film 10 in such a manner that the other side of the plurality of air cells 110 of the molded film 10 is closed and one side of the plurality of air cells 110 is open.
[0043] As another example, Figure 4 As shown, the lower film 20 may be welded and joined to the lower side of the molded film 10 in such a manner that one side and the other side of the plurality of air cells 110 of the molded film 10 are completely open.
[0044] In addition, the lower film 20 in the above step b) is as follows Figure 2 As shown, the lower film 10 can be welded and joined to the lower side of the molded film 10 by using a lower film roll (not shown) and a lower film squeezing roll 240 .
[0045] The lower film 20 may be rolled up on the outer side of the lower film roll (not shown).
[0046] The lower film pressing roller 240 may press the lower film 20 rolled out from the lower film roller (not shown) toward the embossing roller 100 onto the molded film 10 on the outer side of the embossing roller 100 .
[0047] Next, the step c) is a step of filling the interior of the plurality of air cells 110 of the molded film 10 with fluid.
[0048] Figure 5 The present invention schematically illustrates an example of a process of sealing a plurality of air chambers while the plurality of air chambers are filled with fluid. Figure 3 Cross-sectional view along line AA.
[0049] As an example, Figure 2 As shown, in the process where the molded film 10 and the lower film 20 pass through between the embossing roller 100 and the lower film squeezing roller 240 in a mutually engaged state, as shown in FIG. Figure 5 As shown, the fluid may be temporarily filled into the plurality of gas chambers 110 using a fluid injector 120 for injecting the fluid into the plurality of gas chambers 110 .
[0050] The fluid filled into the multiple air chambers 110 can be composed of various types. As an example, it can be composed of gases such as air or inert gas. The fluid injector 120 can be composed of various types such as a compressor for temporarily filling air into the multiple air chambers 110 or an inert gas injector for temporarily injecting inert gas into the multiple air chambers 110.
[0051] As the inert gas, a stable gas having excellent heat insulation properties and not easily disappearing, such as nitrogen, argon, krypton, helium, neon, xenon, radon, etc., can be used.
[0052] Next, the step d) is a step of temporarily sealing the plurality of air chambers 110 filled with fluid.
[0053] like Figure 2 as well as Figure 5 As shown, in a state where the molding film 10 and the lower film 20 pass through the fluid injector 120 , the plurality of air chambers 110 may be temporarily closed by the pressing portion 130 .
[0054] As an example, Figure 5 As shown, when the interior of the multiple air chambers 110 opened to one side by the fluid injector 120 is temporarily filled with fluid, one side of the molding film 10 and one side of the lower film 20 can pass through the extrusion portion 130 located on one side of the molding film 10 and one side of the lower film 20.
[0055] The extrusion portion 130 is as follows Figure 2 as well as Figure 5 As shown, it can be generally composed of a flatbed conveyor including: an upper flatbed conveyor 131; and a lower flatbed conveyor 132, which is equipped at the lower part of the upper flatbed conveyor 131 in a state of being connected to the lower part of the upper flatbed conveyor 131;
[0056] In the process that one side of the molded film 10 passing through the fluid injector 120 and one side of the lower film 20 pass between the upper flatbed conveyor 131 and the lower flatbed conveyor 132 , one side of the multiple air chambers 110 can be squeezed toward the inner side of the multiple air chambers 110 .
[0057] Figure 6 The present invention schematically illustrates another example of a process for sealing a plurality of air chambers while the plurality of air chambers are filled with fluid. Figure 4 Cross-sectional view along line BB in FIG.
[0058] As another example, in a state where the fluid is temporarily filled in the plurality of gas chambers 110 that are fully opened on one side and the other side by the fluid injector 120, as shown in FIG. Figure 6 As shown, one side and the other side of the molded film 10 and one side and the other side of the lower film 20 can all pass through the pressing parts 130 located on one side and the other side of the molded film 10 and one side and the other side of the lower film 20 respectively.
[0059] Figure 7 Each of the perspective views schematically illustrates a state in which an upper film is bonded to a plurality of air cells of a molded film in one embodiment.
[0060] Next, the above step e) is Figure 7 As shown, it is a step of welding and joining the upper film 30 to the upper parts of the plurality of air cells 110 .
[0061] When the multiple air chambers 110 are temporarily closed by utilizing the extrusion portion 130, the fluid in the multiple air chambers 110 can be temporarily prevented from being discharged to the outside, thereby making it easier to maintain the bulging state of the multiple air chambers 110 and thereby making it easier to weld and join the upper side membrane 30 to the upper portion of the multiple air chambers 110.
[0062] As an example of the upper film 30 in the above step e), Figure 2 As shown, the upper film extrusion roller 330 can be used to extrude the thermoplastic synthetic resin melt-extruded from other T-type dies (not shown) for manufacturing the upper film onto the upper portions of the plurality of air chambers 110 to melt-join the resin in a state where the resin is extruded onto the upper portions of the plurality of air chambers 110 .
[0063] like Figure 2 As shown, guide rollers 700 for placing the lower film 20 engaged with the molding film 10 on the upper portion can be respectively provided between the fluid injector 120 and the embossing roller 100 and below the upper film squeezing roller 330 .
[0064] Next, if Figure 1 As shown, it can also include: f) a fluid discharge step (hereinafter referred to as "step f)"); and g) a winding step (hereinafter referred to as "step g)").
[0065] Figure 8 This is a partially enlarged side view showing an enlarged process of winding the molded film, the lower film, and the upper film on a winding roll in a squeezed state.
[0066] The step f) is a step of discharging fluid from the interior of the plurality of air chambers 110 .
[0067] After the molding film 10 , the lower film 20 , and the upper film 30 pass through the pressing portion 130 , the closed state of the air cells 110 may be released, so that the fluid is discharged from the inside of the air cells 110 to the outside.
[0068] In order to more easily discharge the fluid inside the plurality of air chambers 110 to the outside of the air chambers 110, as Figure 8 As shown, the molding film 10, the lower film 20 and the upper film 30 can be passed through a pair of rotating rollers 400 and squeezed, so that the fluid inside the multiple air chambers 110 is discharged to the outside of the air chambers 110.
[0069] The above step g) is as follows Figure 8The illustrated method is a step of rolling up the molded film 10 , the lower film 20 , and the upper film 30 , which are squeezed while passing between the pair of rotating rollers 400 , onto the outer surface of a winding roller 500 .
[0070] Through the above step g), the packaging film can be stored and transported in a state of minimizing the volume by discharging the fluid inside the above air chamber 110, thereby significantly saving logistics costs.
[0071] Fig. 9 This is a side view schematically showing a manufacturing process of a method for manufacturing a packaging film according to another embodiment of the present invention.
[0072] Next, the manufacturing method of the packaging film of another embodiment of the present invention is the same as that of the first embodiment. The molded film 10 in the above step a) is as follows: Fig. 9 As shown, the film can be rolled onto the outer peripheral surface of a film forming roll (not shown) and unrolled toward the embossing roller 100, so that the film can be manufactured by forming a plurality of the air cells 110 at a certain interval using the embossing roller 100.
[0073] In the step b), the lower film 20 may be bonded to the lower side of the molded film 10 by the lower film roller (not shown), the adhesive coating unit 220 , the lower film guide roller 230 , and the lower film squeezing roller 240 .
[0074] The adhesive coating unit 220 may include an adhesive storage bucket 221 , an adhesive transfer roller 222 , and a blade 223 .
[0075] The adhesive 2 to be applied to the lower film 20 can be stored at a certain height inside the adhesive storage barrel 221 .
[0076] The adhesive transfer roller 222 may be axially coupled to the upper side of the adhesive storage barrel 221 in a state where the lower portion of the adhesive transfer roller 222 is immersed in the adhesive 2 stored in the adhesive storage barrel 221 .
[0077] The upper portion of the adhesive transfer roller 222 can be in contact with the lower film 20 wound around the lower film roller (not shown).
[0078] A plurality of receiving grooves 222 a for receiving a portion of the adhesive 2 received in the adhesive receiving barrel 221 may be formed at a predetermined interval in a matrix on the outer side of the adhesive transfer roller 222 .
[0079] Fig.10This is a perspective view schematically illustrating a molded film and a lower film that are joined to each other by an embossing roller and a lower film roller in another embodiment. Fig.11 This is a perspective view schematically illustrating a molded film and a lower film that are joined to each other by an embossing roll and a lower film roll in another embodiment.
[0080] A portion of the adhesive is received in a plurality of the receiving grooves 222a formed in a matrix at a certain interval on the outer surface of the adhesive transfer roller 222, such as Fig.10 as well as Fig.11 As shown, the adhesive 2 can be applied in a matrix form at a certain interval on the upper surface of the lower film 20 rolled out from the lower film roll (not shown).
[0081] The blade 223 is in contact with the outer side surface of the adhesive transfer roller 222 to remove the adhesive 2 attached to the outer side surface of the adhesive transfer roller 222 .
[0082] The lower film guide roller 230 may guide the lower film 20 onto the embossing roller 100 in a state where the lower film 20 rolled out from the lower film roller (not shown) is placed on the rear side of the lower film guide roller 230 .
[0083] In addition, in another embodiment, the upper film 30 in the above step e) is as follows Fig. 9 As shown, the upper portion of the plurality of air cells 110 can be bonded to the upper portion of the plurality of air cells 110 by using an upper film roller (not shown), an adhesive coating unit 310 , an upper film guide roller 320 , and the upper film pressing roller 330 .
[0084] The upper film 30 may be rolled up on the outer side of the upper film roll (not shown).
[0085] The adhesive coating unit 310 may include an adhesive storage bucket 311 , an adhesive transfer roller 312 , and a blade 313 .
[0086] The adhesive 2 to be applied to the upper film 30 may be stored at a certain height inside the adhesive storage barrel 311 .
[0087] The adhesive transfer roller 312 may be axially coupled to the upper side of the adhesive storage barrel 311 in a state where the lower portion of the adhesive transfer roller 312 is immersed in the adhesive 2 stored in the adhesive storage barrel 311 .
[0088] The upper portion of the adhesive transfer roller 312 may be in contact with the upper film 30 wound around the upper film roller (not shown).
[0089] A plurality of receiving grooves 312 a for receiving a portion of the adhesive 2 received in the adhesive receiving barrel 311 may be formed at regular intervals in a matrix on the outer side of the adhesive transfer roller 312 .
[0090] Fig.12 This is a perspective view schematically showing a state in which an upper film is bonded to a plurality of air cells of a molded film in another embodiment.
[0091] A portion of the adhesive 2 is received in a plurality of the receiving grooves 312a formed in a matrix at a certain interval on the outer surface of the adhesive transfer roller 312, such as Fig.12 As shown, the adhesive 2 can be applied in a matrix form at a certain interval to the lower surface of the upper film 30 rolled out from the upper film roll (not shown).
[0092] The blade 313 is in contact with the outer side surface of the adhesive transfer roller 312 to remove the adhesive attached to the outer side surface of the adhesive transfer roller 312 .
[0093] The upper film guide roller 320 may be composed of a first upper film guide roller 321 and a second upper film guide roller 322 .
[0094] The upper film 30 rolled out from the upper film roll (not shown) can be placed on the front side of the first upper film guide roll 321 .
[0095] The second upper film guide roller 322 can be located on the opposite side of the front of the first upper film guide roller 321, i.e., at the rear, and when the upper film 30 is placed on the upper part of the second upper film guide roller 322, the upper film 30 can be guided onto the upper film squeezing roller 330.
[0096] Figures 13 to 17 This is a perspective view schematically showing a state in which a molding film, a lower film, and an upper film are joined in a state in which a check valve is provided.
[0097] Next, if Figures 13 to 17 As shown, when one or more check valves 40 are arranged at a certain interval between one side of the lower film 20 and one side of the upper film 30, the edge of the lower film 20 and the edge of the upper film 30 can be welded or bonded.
[0098] An injection space 150 communicating with the plurality of gas cells 110 may be formed between one side of the lower film 20 and one side of the upper film 30 .
[0099] The check valve 40 may be prepared in a state of being previously melt-bonded or adhesively bonded to one upper portion or the other upper portion of the lower film 20 before manufacturing the packaging film to which the present invention is applied.
[0100] Alternatively, the check valve 40 may be prepared in a state of being melt-bonded or adhesively bonded to one lower portion or the other lower portion of the upper film 30 before manufacturing the packaging film to which the present invention is applied.
[0101] Alternatively, after the packaging film applicable to the present invention is manufactured but before the packaging film is used, one or more check valves 40 can be welded or adhesively joined at a certain interval between one side of the lower film 20 rolled out from the winding roller 500 and one side of the upper film 30.
[0102] Alternatively, the check valve 40 can also be melt-bonded or adhesively bonded to one side of the lower film 20 or melt-bonded or adhesively bonded to one side of the upper film 30 before the upper portion of the plurality of air chambers 110 is bonded to the upper portion of the upper film 30 during the manufacturing process of the packaging film applicable to the present invention.
[0103] Alternatively, the check valve 40 can also be joined to the upper side film 30 at the top of the plurality of air chambers 110 and melt-bonded or adhesively bonded to one side of the lower side film 20 or melt-bonded or adhesively bonded to one side of the upper side film 30 before the molding film 10, the lower side film 20 and the upper side film 30 are wound onto the winding roller 500 during the manufacturing process of the packaging film applicable to the present invention.
[0104] An operator can use an injection means such as an injector to inject the fluid into the interior of the air chamber 110 and the space 140 formed between the air chambers 110 through the check valve 40 and the injection space 150 .
[0105] In this case, by injecting a fluid into the space 140 formed between the air chambers 110 , heat exchange caused by the space 140 can be prevented, thereby effectively preventing the thermal insulation of the packaging film of the present invention from being reduced.
[0106] like Fig.14 As shown, a connection air chamber 160 communicating with the plurality of air chambers 110 and the injection space 150 can be formed on one side of the molding film 10 .
[0107] The inner diameter of the connecting air chamber 160 may be smaller than the inner diameter of the air chamber 110 .
[0108] Or, if Fig.15As shown, a plurality of the connection air chambers 160 for connecting one air chamber 110 with another air chamber 110 in a mutually communicating state can be formed at a certain interval between one air chamber 110 and another air chamber 110 .
[0109] Or, if Fig.16 As shown, a plurality of the air cells 110 may be formed in a matrix on the molding film 10 and may be formed in various shapes such as a circle or an ellipse.
[0110] Furthermore, the connecting air chamber 160 for connecting one of the air chambers 110 and another of the air chambers 110 in a mutually communicating state may be arranged at a certain interval from one side to the other side of the molding film 10 in a state of being located between the plurality of air chambers 110 formed in a matrix form.
[0111] In addition, if Fig.17 As shown, the connecting air chamber 160 can also be formed between the air chambers 110 in one row and the air chambers 110 in another row.
[0112] Industry availability
[0113] The present invention can not only greatly improve the heat insulation, but also minimize the volume of the air chamber without cutting or opening a part of the air chamber by needle punching, thereby facilitating storage and transportation.
Claims
1. A method for manufacturing a packaging film, characterized in that: include: a) a step of manufacturing a molded film having a plurality of air cells formed at certain intervals, the air cells being open at the bottom and one side and protruding upward; b) a step of joining a lower film having one end portion longer than one end portion of the formed film to the lower side of the formed film in such a manner that one side of the plurality of air cells of the formed film is open; c) a step of filling the interior of the plurality of air cells of the molded film with a fluid in such a manner that the plurality of air cells convexly expand; d) a step of closing one side of the plurality of air cells of the molded film in a manner capable of maintaining a state in which the plurality of air cells are convexly expanded; e) a step of bonding an upper film having an adhesive applied to the lower surface in a matrix form to the upper part of the plurality of air chambers in such a manner that the upper part of the space between the plurality of air chambers that are bulged convexly is closed; f) releasing the sealed state of the plurality of air chambers and discharging fluid from the interior of the plurality of air chambers; as well as, g) A step of rolling the formed film, the lower film and the upper film onto an outer side surface of a winding roller.
2. The method for manufacturing a packaging film according to claim 1, characterized in that: The molded film in step a) is manufactured by melt-extruding a thermoplastic synthetic resin onto an embossing roll having molded grooves having a shape corresponding to the air chamber formed at a certain interval on the outer peripheral surface; The lower film in step b) is joined to the formed film by a lower film roller and a lower film squeezing roller, The lower film roller is wound with the lower film, The lower film squeezing roller squeezes the lower film rolled out from the lower film roller against the embossing roller.
3. The method for manufacturing a packaging film according to claim 1, characterized in that: The molded film in step a) is manufactured by using an embossing roller having molded grooves having shapes corresponding to the air chambers formed at certain intervals on the outer peripheral surface; The lower film of step b) is joined to the molded film by a lower film roller, an adhesive coating unit and a lower film squeezing roller, The lower film roller is wound with the lower film, The adhesive coating section coats the adhesive at a certain interval onto the lower film rolled out from the lower film roll. The lower film squeezing roller squeezes the lower film rolled out from the lower film roller against the embossing roller.
4. The method for manufacturing a packaging film according to claim 1, characterized in that: In the step b), one side and the other side of the plurality of air cells of the formed film are all open; In the step c), the interior of the plurality of air chambers is temporarily filled with fluid using a fluid injector for injecting fluid into the interior of the plurality of air chambers.
5. The method for manufacturing a packaging film according to claim 1, characterized in that: In the step d), the plurality of air chambers are temporarily closed by passing through a pressing portion that presses one side of the plurality of air chambers while the interior of the plurality of air chambers is temporarily filled with a fluid.
6. The method for manufacturing a packaging film according to claim 4, characterized in that: In the step d), the plurality of air chambers are temporarily closed by passing through a pressing portion that presses one side and the other side of the plurality of air chambers while the fluid is temporarily filled inside the plurality of air chambers.
7. The method for manufacturing a packaging film according to claim 5 or 6, characterized in that: The extrusion part is composed of a flatbed conveyor.
8. The method for manufacturing a packaging film according to claim 1, characterized in that: The upper film of step e) is bonded to the plurality of air chambers by an upper film roller, an adhesive coating unit and an upper film squeezing roller, The upper film roll is wound with the upper film, The adhesive coating section coats the adhesive at a predetermined interval onto the upper film rolled out from the upper film roll. The upper film pressing roller presses the upper film rolled out from the upper film roller onto the plurality of air cells.
Citation Information
Patent Citations
St. thermal insulation and storage method for producing improved packaging sheet
KR101752100B1
St. thermal insulation and storage method for producing improved packaging sheet
KR101752101B1
Novel portable device for cell lysis
KR1020160117724A
Flat buffering air bag provided with internal separating air chambers and used for container
CN103538795A
Exhaust valve apparatus and gas filled cushion
CN105383799A