An outdoor full-color LED display module and its production process
Through the combination of flip-chip and a whole piece of bowl and cup plastic parts, combined with ultra-thin prefabricated membrane and waterproof rubber ring, the problems of complex process and poor waterproof effect of traditional module are solved, and an efficient and energy-saving outdoor full-color LED display is realized. Screen module production improves product performance and production efficiency.
Patent Information
- Application Number
- CN202210435063.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-04-24
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2042-04-24
AI Technical Summary
The production process of traditional outdoor full-color LED display modules is complex and time-consuming, resulting in low production efficiency, and the waterproof effect and light extraction efficiency of the modules are not ideal.
It uses flip-chip R, G, and B chips for direct packaging, combines the entire bowl plastic part and ultra-thin prefabricated film, and uses a high-precision dot matrix die-bonding machine and UV curing technology to improve packaging efficiency and waterproof performance, and integrates the PCB and bottom Add waterproof rubber rings between the shells.
The production process is simplified, the waterproof level and light extraction efficiency of the module are improved, the cost is reduced, the service life of the module is extended, and the reliability and visual effects are improved.
Smart Images

Figure CN115019674B_ABST
Abstract
Description
Technical Field
[0001] The invention provides an outdoor full-color LED display screen module and a manufacturing process thereof, belonging to the technical field of outdoor full-color LED display screen modules. Background Art
[0002] The main components of the traditional outdoor full-color LED display module are plastic bottom shell, PCB, RGB lamp beads, plastic mask, and various driver ICs, capacitors, resistors, power sockets, connectors and other electronic components that make up the drive circuit. The structure diagram is as follows Figure 1-3 The main production process is as follows:
[0003] 1. Various electronic components 102 are mounted on the back of the PCB board 103 through a solder paste printer, a mounter, and a reflow soldering device;
[0004] 2. Use the same method to mount the RGB lamp beads 104 on the front of the PCB through a solder paste printer, a mounter, and a reflow soldering device. In order to make the ink color of the module consistent, this PCB is mainly made of black copper clad laminate;
[0005] 3. The back of the PCB is sprayed with conformal coating to achieve IP54 waterproof rating;
[0006] 4. Use screws to fix the PCB to the bottom case 101. There will be vertical walls around the front of the bottom case, the height of which is slightly higher than the height of the PCB plus the RGB lamp bead pins;
[0007] 5. Use a glue filling machine to fill the front of the PCB with black glue 105 until it covers all the pins of the RGB lamp beads, so that the front side reaches the IP65 waterproof level. In addition, the glue will also flow into the gap between the PCB and the bottom shell wall to prevent rainwater from flowing from the front of the module to the back of the module when used outdoors;
[0008] 6. Use screws 107 to fix the plastic mask 106 to the surface of the module.
[0009] When the module is used outdoors, a waterproof rubber ring will be installed at the bottom, which can play a good waterproof role at the junction of the module and the box, so that the module as a whole reaches the IP65 waterproof level and meets the requirements of outdoor use. However, traditional module RGB lamp beads need to use bracket raw materials and some packaging processes, including welding wires, dispensing, light splitting, braiding, etc., as well as auxiliary processes such as dehumidification and baking. Not only is the process complicated and time-consuming, but the production efficiency is low. Summary of the invention
[0010] In order to overcome the deficiencies in the prior art, the present invention aims to solve the technical problem of providing an improvement in the hardware structure of an outdoor full-color LED display screen module.
[0011] In order to solve the above technical problems, the technical solution adopted by the present invention is: an outdoor full-color LED display screen module, including a plastic bottom shell, a PCB, and a prefabricated film, the back of the PCB is mounted with electronic components and copper pillars, the front of the PCB is provided with pads for flip-chip R, G, and B chips, the upper surface of the plastic bottom shell is provided with a groove for laying a waterproof rubber ring, the back of the PCB is placed on the plastic bottom shell with the waterproof rubber ring installed, and the plastic bottom shell is connected and locked with the copper pillars on the back of the PCB by screws;
[0012] A whole cup plastic part is fixed on the front of the PCB, and the whole cup plastic part includes a plurality of plastic cups, each plastic cup is aligned with a group of R, G, B chips, and the whole cup plastic part is aligned with the plastic cup position of a group of R, G, B chips by degassing mixed epoxy resin glue, and the glue covers all R, G, B chips and their bottom pads;
[0013] The prefabricated film is attached to the surface of the module, and covers the edge and surrounding of the plastic bottom shell.
[0014] The whole piece of bowl and cup plastic part is made of high temperature resistant nylon material or high temperature resistant metal material, wherein high temperature resistance means that it can withstand a minimum thermal deformation temperature of 300°C, and the minimum high temperature resistance of the whole piece of bowl and cup plastic part for continuous use is 170°C.
[0015] The plastic bowl cup is configured as a trumpet-mouth structure that is small inside and large outside, wherein the opening angle of the trumpet-mouth interface is 20-45°, and the inner wall of the plastic bowl cup is white, and the surface is ink-sprayed.
[0016] The prefabricated film is an ultra-thin film with a thickness of 0.05-0.5 mm, and is cured by UV. The prefabricated film specifically adopts a black semi-cured prefabricated film with a frosted microstructure on the surface or a semi-cured prefabricated film with a textured microstructure on the surface.
[0017] The mixed epoxy resin glue specifically adopts A / B component epoxy resin glue or single component phenolic resin or light-transmitting resin glue.
[0018] The production process of outdoor full-color LED display modules includes the following steps:
[0019] S1: Mount electronic components and copper pillars on the back of the PCB through solder paste printer, placement machine, and reflow soldering equipment;
[0020] S2: Spray conformal coating on the back of the PCB to achieve IP54 waterproof rating;
[0021] S3: Flip the pads of R, G, and B chips on the front side of the PCB;
[0022] S4: Print solder paste on the R, G, and B chip pads on the front of the PCB, or dot-print conductive glue on the pads;
[0023] S5: Use a high-precision dot matrix die bonding machine to fix the flip-chip R, G, and B chips on the corresponding pad positions on the front side of the PCB;
[0024] S6: Put the PCB with R, G, B chips fixed into reflow soldering or heating oven for soldering and curing, so that the R, G, B chips are firmly bonded to the PCB pads;
[0025] S7: Lay a waterproof rubber ring in the groove reserved on the upper surface of the plastic bottom shell;
[0026] S8: Place the PCB on the plastic bottom case with the waterproof rubber ring installed, and use screws to connect and lock the plastic bottom case with the copper pillars on the back of the PCB;
[0027] S9: Adhere the whole plastic bowl with adhesive backing to the front of PCB, and align each plastic bowl with a group of R, G, and B chips;
[0028] S10: Mix the epoxy resin glue and the filler in a certain proportion and then put them into a vacuum box for vacuum degassing. The vacuum degree is 80MPa-85MPa and the time is 3-5min.
[0029] S11: Use a dispensing machine to inject the degassed mixed epoxy resin glue into the cup position of a group of R, G, and B chips of the entire cup plastic part. The amount of glue should be enough to fill the cup and slightly convex. The glue will cover all R, G, and B chips and their bottom pads.
[0030] S12: The entire module with glue injected is placed in a 130-140°C environment and baked until the glue is completely cured;
[0031] S13: Use a film laminating machine to attach the semi-cured prefabricated film to the surface of the module with the glue injected. The prefabricated film needs to cover the edge of the plastic bottom shell and extend about 5 to 10 mm around it. Then put it into a high temperature condition of 120 to 150°C for hot pressing, and simultaneously evacuate it under a negative pressure of not less than 80MPa, so that the prefabricated film is tightly attached to the surface of the module. Then use a 350 to 375nm UV curing furnace to re-cure the prefabricated film after hot pressing. The curing power is 2500 to 4000mJ and the curing time is 3 to 5 minutes.
[0032] S14: The cured module is removed, and the excess prefabricated film at the edge of the plastic bottom shell is cut off with a cutting knife to form a finished module.
[0033] The front of the plastic bottom shell is surrounded by vertical walls, the height of which is consistent with the thickness of the PCB5 plus the entire bowl and cup plastic part.
[0034] The single cup of the whole cup plastic part is a square trumpet-shaped structure with a small inside and a large outside, and the opening angle of the cup is 20-45 degrees;
[0035] The entire bowl and cup plastic part is made of high-temperature resistant nylon material or high-temperature resistant metal material. The lowest thermal deformation temperature of the entire bowl and cup plastic part can withstand 300°C, and the lowest continuous use temperature can withstand 170°C. The inner wall of the bowl and cup is white and the surface is inkjet.
[0036] The prefabricated film is an ultra-thin film with a thickness of 0.05-0.5 mm, and is cured by UV. The prefabricated film specifically adopts a black semi-cured prefabricated film with a frosted microstructure on the surface or a semi-cured prefabricated film with a textured microstructure on the surface.
[0037] When the finished module is used outdoors, a waterproof rubber ring is installed on the plastic bottom shell to play a waterproof role at the junction of the module and the box body, so that the module as a whole reaches the IP65 waterproof level.
[0038] The beneficial effects of the present invention compared with the prior art are as follows:
[0039] 1. Direct mounting of flip-chip R, G, and B chips eliminates the raw materials of the bracket of the traditional module RGB lamp beads and some of the packaging processes, including welding wires, dispensing, splitting, taping, etc., as well as auxiliary processes such as dehumidification and baking, saving a lot of labor, equipment, raw materials and consumables;
[0040] 2. Use flip chip to directly package into outdoor display module. Since there is no electrode blocking the light-emitting surface of flip chip, the brightness of the chip itself is higher than that of the regular chip. This packaging process can greatly improve the light-emitting efficiency of R, G, and B chips, making the display module save energy by more than 20% under the same brightness;
[0041] 3. Using PCB with bright tin or silver plating on the front can also improve the light output efficiency of R, G, and B chips;
[0042] 4. A waterproof rubber ring is added between the PCB and the bottom shell to improve the overall waterproof effect of the module;
[0043] 5. The use of a whole piece of bowl-cup plastic parts improves production efficiency. A single bowl-cup is a square trumpet-shaped structure with a small inside and a large outside. The inner surface is white, which can further improve the light output efficiency of the R, G, and B chips. The outer surface is black, which can increase the contrast and improve the viewing visual effect of the module.
[0044] 6. The module adopts the overall glue filling method, which improves the consistency of the module's glue surface and ink color;
[0045] 7. A frosted microstructured black film is mounted on the outer surface, which not only removes the screws used to fix the mask in the traditional module, but also improves the consistency and flatness of the module surface. It looks matte to the human eye and is not dazzling. It also makes the module surface extremely waterproof, scratch-resistant, bump-resistant, and UV-resistant, greatly improving the reliability and service life of the module.
[0046] In summary, the new outdoor full-color LED display screen module of the present invention not only improves product performance, but also saves a lot of labor, equipment, and materials, greatly reduces costs, creates benefits for enterprises, and can also reduce environmental pollution and benefit society. BRIEF DESCRIPTION OF THE DRAWINGS
[0047] The present invention will be further described below in conjunction with the accompanying drawings:
[0048] Figure 1 This is an exploded view of a traditional outdoor full-color LED display module;
[0049] Figure 2 This is a partial enlarged picture of the plastic mask of the traditional outdoor full-color LED display module;
[0050] Figure 3 This is a partial enlarged picture of the neatly arranged RGB lamp beads of the traditional outdoor full-color LED display module;
[0051] Figure 4 This is an exploded view of the outdoor full-color LED display module of the present invention;
[0052] Figure 5 This is a partial enlarged view of the semi-cured prefabricated film with a frosted microstructure of the outdoor full-color LED display screen module of the present invention;
[0053] Figure 6 This is a partial enlarged view of the microstructured semi-cured prefabricated film with textures of the outdoor full-color LED display module of the present invention;
[0054] Figure 7 This is a partial enlarged view of the entire bowl-cup plastic part of the outdoor full-color LED display module of the present invention;
[0055] Figure 8 This is a partial enlarged view of the flip-chip R, G, and B chips of the outdoor full-color LED display module of the present invention;
[0056] Fig. 9 This is a cross-sectional view of an outdoor full-color LED display screen module of the present invention;
[0057] In the figure: 1 is a plastic bottom shell, 2 is a waterproof rubber ring, 3 is a copper column, 4 is an electronic component, 5 is a PCB, 6 is a flip-chip R, G, B chip, 7 is a whole piece of bowl and cup plastic parts, 8 is mixed epoxy resin glue, 9 is a prefabricated film, 101 is a bottom shell, 102 are various electronic components, 103 is a PCB board, 104 is an RGB lamp bead, 105 is a filled black glue, 106 is a plastic mask, and 107 is a screw. DETAILED DESCRIPTION
[0058] like Figures 4 to 9 As shown, an outdoor full-color LED display screen module of the present invention includes a plastic bottom shell 1, a PCB5, and a prefabricated film 9. The back of the PCB5 is mounted with electronic components 4 and copper pillars 3. The front of the PCB5 is provided with pads for flip-chip R, G, and B chips 6. The upper surface of the plastic bottom shell 1 is provided with a groove for laying a waterproof rubber ring 2. The back of the PCB5 is placed on the plastic bottom shell 1 with the waterproof rubber ring 2 installed. The plastic bottom shell 1 is connected and locked with the copper pillars 3 on the back of the PCB5 by screws;
[0059] A whole cup plastic part 7 is fixed on the front of the PCB 5. The whole cup plastic part 7 includes a plurality of plastic cups. Each plastic cup is aligned with a group of R, G, and B chips 6. The whole cup plastic part 7 is aligned with the plastic cup position of a group of R, G, and B chips 6 by degassing the mixed epoxy resin glue 8. The glue covers all R, G, and B chips 6 and their bottom pads.
[0060] The prefabricated film 9 is attached to the surface of the module, and covers the edge and surrounding of the plastic bottom shell 1 .
[0061] The whole bowl and cup plastic part 7 is made of high temperature resistant nylon material or high temperature resistant metal material, wherein high temperature resistance means that it can withstand a minimum thermal deformation temperature of 300°C, and the minimum high temperature resistance of the whole bowl and cup plastic part 7 for continuous use is 170°C.
[0062] The plastic bowl cup is configured as a trumpet-mouth structure that is small inside and large outside, wherein the opening angle of the trumpet-mouth interface is 20-45°, and the inner wall of the plastic bowl cup is white, and the surface is ink-sprayed.
[0063] The prefabricated film 9 is an ultra-thin film with a thickness of 0.05-0.5 mm, and is cured by UV. The prefabricated film 9 is specifically a black semi-cured prefabricated film with a frosted microstructure on the surface or a semi-cured prefabricated film with a textured microstructure on the surface.
[0064] The mixed epoxy resin glue 8 specifically adopts A / B component epoxy resin glue or single component phenolic resin or light-transmitting resin glue.
[0065] The production process of outdoor full-color LED display modules includes the following steps:
[0066] S1: Mount the electronic components 4 and the copper pillars 3 on the back of the PCB 5 through a solder paste printer, a placement machine, and a reflow soldering device;
[0067] S2: Spray conformal coating on the back of PCB5 to make it reach IP54 waterproof grade;
[0068] S3: flip-mount the pads of the R, G, and B chips 6 on the front side of the PCB 5;
[0069] S4: Print solder paste on the R, G, and B chip pads on the front of PCB5, or dot-print conductive glue on the pads;
[0070] S5: Use a high-precision dot matrix die bonding machine to fix the flip-chip R, G, and B chips 6 on the corresponding pad positions on the front side of the PCB 5;
[0071] S6: Put the PCB5 with R, G, B chips fixed into a reflow oven or a heating oven for soldering and curing, so that the R, G, B chips are firmly bonded to the PCB pads;
[0072] S7: Laying the waterproof rubber ring 2 in the groove reserved on the upper surface of the plastic bottom shell 1;
[0073] S8: Place the PCB 5 on the plastic bottom shell 1 with the waterproof rubber ring 2 installed, and connect and lock the plastic bottom shell 1 and the copper pillar 3 on the back of the PCB 5 with screws;
[0074] S9: The whole cup plastic part 7 with adhesive backing is bonded and fixed to the front of PCB 5, and each plastic cup is aligned with a group of R, G, and B chips;
[0075] S10: Mix the epoxy resin glue 8 and the filler in a certain proportion and then put them into a vacuum box for vacuum degassing. The vacuum degree is 80MPa to 85MPa and the time is 3 to 5 minutes.
[0076] S11: Use a dispensing machine to inject the degassed mixed epoxy resin glue 8 into the cup position of a group of R, G, and B chips of the entire cup plastic part 7. The amount of glue is enough to fill the cup and slightly convex. The glue will cover all R, G, and B chips and their bottom pads.
[0077] S12: The entire module with glue injected is placed in a 130-140°C environment and baked until the glue is completely cured;
[0078] S13: Use a film laminating machine to attach the semi-cured prefabricated film 9 to the surface of the module with the glue injected. The prefabricated film 9 needs to cover the edge of the plastic bottom shell 1 and extend about 5 to 10 mm around it. Then put it into a high temperature condition of 120 to 150°C for hot pressing, and evacuate it at a negative pressure of not less than 80MPa at the same time, so that the prefabricated film 9 is tightly attached to the surface of the module. Then use a 350 to 375nm UV curing furnace to re-cure the prefabricated film 9 after hot pressing. The curing power is 2500 to 4000mJ and the curing time is 3 to 5 minutes.
[0079] S14: The cured module is removed, and the excess prefabricated film 9 at the edge of the plastic bottom shell 1 is cut off with a cutting knife to form a finished module.
[0080] The front of the plastic bottom shell 1 is surrounded by vertical walls, the height of which is consistent with the thickness of the PCB 5 plus the entire bowl and cup plastic part 7.
[0081] The single cup of the whole cup plastic part 7 is a square trumpet-shaped structure with a small inside and a large outside, and the opening angle of the cup is 20-45°;
[0082] The whole bowl and cup plastic part 7 is made of high temperature resistant nylon material or high temperature resistant metal material. The thermal deformation temperature of the whole bowl and cup plastic part 7 can be as low as 300°C, and the continuous use temperature can be as low as 170°C. The inner wall of the bowl and cup is white and the surface is inkjet.
[0083] The prefabricated film 9 is an ultra-thin film with a thickness of 0.05-0.5 mm, and is cured by UV. The prefabricated film specifically adopts a black semi-cured prefabricated film with a frosted microstructure on the surface or a semi-cured prefabricated film with a textured microstructure on the surface.
[0084] When the finished module is used outdoors, a waterproof rubber ring is installed on the plastic bottom shell 1 to play a waterproof role at the junction of the module and the box body, so that the entire module reaches the IP65 waterproof level.
[0085] The difference between the present invention and the traditional outdoor full-color LED display module lies mainly in the front of the PCB. Instead of using packaged RGB lamp beads for patching, a high-precision patch machine is used to directly mount the flipped R, G, and B chips, and a special whole bowl-cup plastic part 7 is used to replace the bowl of a single RGB lamp bead. The positive and negative electrodes of the flipped R, G, and B chips 6 are at the bottom of the chip and can be directly connected to the PCB pads through solder paste or other solder. The main production process of the new outdoor full-color LED display module of the present invention is as follows:
[0086] 1. Various electronic components 4 such as driver ICs, capacitors, resistors, power sockets, connectors, and copper pillars 3 are mounted on the back of PCB 5 through solder paste printers, mounters, and reflow soldering equipment;
[0087] 2. The back of the PCB is sprayed with three-proof paint to achieve the IP54 waterproof level;
[0088] 3. The 6 pads of the R, G, B chips on the front of the PCB are plated with bright tin or silver, with a thickness of about 20 to 60 marks, which can reflect the light emitted by the R, G, B chips very well, thereby improving the light output efficiency of the R, G, B chips;
[0089] 4. Print 5#~7# powder solder paste on the R, G, B chip pads on the front of the PCB, or print conductive glue on the pads;
[0090] 5. Use a high-precision dot matrix die bonding machine to fix the flip-chip R, G, and B chips 6 on the corresponding pad positions on the front of the PCB;
[0091] 6. Put the PCB with R, G, B chips fixed into reflow soldering or heating oven for soldering and curing, so that the R, G, B chips are firmly bonded to the PCB pads;
[0092] 7. Lay the waterproof rubber ring 2 in the groove reserved on the upper surface of the plastic bottom shell 1;
[0093] 8. Place the PCB on the plastic bottom shell 1 with the waterproof rubber ring installed, and use screws to connect and lock the plastic bottom shell 1 with the copper pillars 3 on the back of the PCB. A wall will also be erected around the front of the plastic bottom shell 1, and the height is consistent with the thickness of the PCB board plus the entire bowl plastic part 7, so that the glue can be prevented from flowing out during the glue filling;
[0094] 9. The whole plastic cup 7 with adhesive backing is fixed on the front of PCB by positioning and mounting equipment. Each plastic cup is aligned with a group of R, G, B chips. A single cup is a square trumpet structure with small inside and large outside. The cup angle is 20-45° (such as Figure 7 ), which is the most suitable light-emitting structure for R, G, and B chips, the whole bowl cup plastic part is made of high-temperature resistant nylon (PPA) material (in this case, high-temperature resistant nylon material is used, and metal materials such as aluminum alloy can also be used), with a thermal deformation temperature of up to 300°C and a continuous use temperature of up to 170°C. The inner wall of the bowl cup is white and the surface is inkjet. The purpose of this is that the inner wall of the bowl cup can reflect light and improve the light-emitting efficiency of the R, G, and B chips, and the second is that the white inside and the black outside can increase the overall contrast of the module;
[0095] 10. Mix the A / B component epoxy resin glue (in this case, two-component epoxy resin is used for filling, and single-component phenolic resin or other light-transmitting resin can also be used) with filler in a certain proportion and then put it into a vacuum box for vacuum degassing. The vacuum degree is 80MPa~85MPa and the time is 3~5min;
[0096] 11. Use a dispensing machine to inject the degassed mixed epoxy resin glue 8 into the cup position of a group of R, G, and B chips on the entire cup plastic part 7. The amount of glue should be enough to fill the cup and slightly convex. The glue will cover all R, G, and B chips and their bottom pads.
[0097] 12. Bake the whole module with glue at 130-140℃ for 3 hours until the glue is completely cured. The cured glue has a good protective effect, which can protect the chip from external erosion and bumps, and can also emit the light from the R, G, and B chips out of the cup.
[0098] 13. Use a film laminating machine to apply a black semi-cured prefabricated film with a frosted microstructure on the surface (in this example, a black semi-cured prefabricated film with a frosted microstructure is used, such as Figure 5 ; Other color semi-cured prefabricated films with textured microstructures can also be used, such as Figure 6 ) is attached to the surface of the module with glue injection. The prefabricated film 9 needs to cover the edge of the plastic bottom shell 1 and extend about 5 to 10 mm around it. Then it is placed in a high temperature condition of 120 to 150 ° C for hot pressing, and vacuumed at a negative pressure of not less than 80 MPa at the same time. The prefabricated film 9 is tightly attached to the surface of the module, and then a 350 to 375 nm UV curing furnace is used to re-cur the prefabricated film after hot pressing. The curing power is 2500 to 4000 mJ and the curing time is 3 to 5 minutes.
[0099] 14. Remove the cured module and use a cutting knife to cut off the excess prefabricated film 9 on the edge of the plastic bottom shell 1 to form a finished module. This prefabricated film 9 can not only protect the light-emitting surface for a second time, but also form a secondary seal between the edge of the plastic bottom shell 1 and the internal module to prevent the gap between the edge of the plastic bottom shell 1 and the internal module from being affected by external water vapor. The prefabricated film 9 is an ultra-thin film with a thickness of 0.05-0.5mm. It has excellent UV resistance through UV curing. It looks matte to the human eye and is not dazzling. It can also make the module surface have excellent waterproof, scratch-resistant and bump-resistant effects.
[0100] When the novel module of the present invention is used outdoors, a waterproof rubber ring is also installed on the plastic bottom shell 1, which can play a good waterproof role at the junction of the module and the box body, so that the entire module reaches the IP65 waterproof level and meets the requirements of outdoor use.
[0101] What needs to be explained about the specific structure of the present invention is that the connection relationship between the various component modules adopted in the present invention is definite and feasible. Except for the special instructions in the embodiments, the specific connection relationship can bring about the corresponding technical effects, and solve the technical problems raised by the present invention without relying on the execution of the corresponding software program. Except for the specific instructions, the models and connection methods of the components, modules and specific components appearing in the present invention belong to the existing technologies such as published patents, published journal articles, or common knowledge that can be obtained by technical personnel in this field before the application date, and there is no need to elaborate, so that the technical solution provided in this case is clear, complete and feasible, and the corresponding physical products can be reproduced or obtained according to the technical means.
[0102] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A production process for an outdoor full-color LED display screen module, the outdoor full-color LED display screen module comprising a plastic bottom shell (1) and a PCB (5), characterized in that: It also comprises a prefabricated film (9), the back of the PCB (5) is mounted with electronic components (4) and copper pillars (3), the front of the PCB (5) is provided with pads for flip-chip R, G, and B chips (6), the upper surface of the plastic bottom shell (1) is provided with a groove for laying a waterproof rubber ring (2), the back of the PCB (5) is placed on the plastic bottom shell (1) on which the waterproof rubber ring (2) is installed, and the plastic bottom shell (1) is connected and locked with the copper pillars (3) on the back of the PCB (5) using screws; A whole cup-shaped plastic part (7) is fixed on the front of the PCB (5), wherein the whole cup-shaped plastic part (7) comprises a plurality of plastic cups, each of which is aligned with a group of R, G, and B chips (6), and the whole cup-shaped plastic part (7) is aligned with the plastic cup position of the group of R, G, and B chips (6) by degassed mixed epoxy resin glue (8), and the glue covers all the R, G, and B chips (6) and their bottom pads; The prefabricated film (9) is attached to the surface of the module, and the prefabricated film (9) covers the edge and surrounding of the plastic bottom shell (1); The production process of the outdoor full-color LED display module includes the following steps: S1: mounting the electronic components (4) and the copper pillars (3) on the back of the PCB (5) by means of a solder paste printer, a placement machine, and a reflow soldering device; S2: Spray conformal coating on the back of PCB (5) to achieve IP54 waterproof rating; S3: flip-mount the pads of the R, G, and B chips (6) on the front side of the PCB (5); S4: Print solder paste on the R, G, and B chip pads on the front of the PCB (5), or dot-print conductive glue on the pads; S5: Use a high-precision dot matrix die bonding machine to fix the flip-chip R, G, and B chips (6) at the corresponding pad positions on the front side of the PCB (5); S6: Put the PCB (5) with the R, G, and B chips fixed thereon into a reflow soldering or heating oven for soldering and curing, so that the R, G, and B chips are firmly bonded to the PCB pads; S7: Laying a waterproof rubber ring (2) in a groove reserved on the upper surface of the plastic bottom shell (1); S8: placing the PCB (5) on the plastic bottom shell (1) on which the waterproof rubber ring (2) is installed, and connecting and locking the plastic bottom shell (1) and the copper pillars (3) on the back of the PCB (5) with screws; S9: The whole plastic bowl (7) with adhesive backing is bonded and fixed to the front of the PCB (5), and each plastic bowl is aligned with a group of R, G, and B chips; S10: Mix the mixed epoxy resin glue (8) and the filler in a certain proportion and then put it into a vacuum box for vacuum degassing at a vacuum degree of 80 MPa to 85 MPa for 3 to 5 minutes; S11: Use a dispensing machine to inject the degassed mixed epoxy resin glue (8) into the entire cup plastic part (7) corresponding to the cup position of a group of R, G, and B chips. The amount of glue should be enough to fill the cup and slightly convex. The glue will cover all R, G, and B chips and their bottom pads. S12: The entire module with glue injected is placed in a 130-140°C environment and baked until the glue is completely cured; S13: Using a film laminating machine, attach the semi-cured prefabricated film (9) to the surface of the module that has been injected with glue. The prefabricated film (9) needs to cover the edge of the plastic bottom shell (1) and extend about 5 to 10 mm around it. Then, heat press the prefabricated film (9) at a high temperature of 120 to 150°C, and simultaneously evacuate the prefabricated film (9) at a negative pressure of not less than 80 MPa. Then, use a 350 to 375 nm UV curing furnace to re-cure the prefabricated film (9) that has been heat-pressed and bonded. The curing power is 2500 to 4000 mJ and the curing time is 3 to 5 minutes. S14: The cured module is then removed, and the excess prefabricated film (9) on the edge of the plastic bottom shell (1) is cut off with a cutting knife, thereby forming a finished module.
2. The production process of an outdoor full-color LED display module according to claim 1, characterized in that: The whole bowl and cup plastic part (7) is made of high temperature resistant nylon material or high temperature resistant metal material, wherein high temperature resistance means that it can withstand a minimum thermal deformation temperature of 300° C. The minimum high temperature resistance of the whole bowl and cup plastic part (7) for continuous use is 170° C.
3. The production process of an outdoor full-color LED display module according to claim 2, characterized in that: The plastic bowl cup is configured as a trumpet-mouth structure that is small inside and large outside, wherein the opening angle of the trumpet-mouth interface is 20-45°, and the inner wall of the plastic bowl cup is white, and the surface is ink-sprayed.
4. The production process of an outdoor full-color LED display module according to claim 3, characterized in that: The prefabricated film (9) is an ultra-thin film with a thickness of 0.05-0.5 mm and is cured by UV. The prefabricated film (9) is specifically a black semi-cured prefabricated film with a frosted microstructure on the surface or a semi-cured prefabricated film with a textured microstructure on the surface.
5. The production process of an outdoor full-color LED display module according to claim 1, characterized in that: The mixed epoxy resin glue (8) specifically adopts A / B component epoxy resin glue or single component phenolic resin or light-transmitting resin glue.
6. The production process of the outdoor full-color LED display module according to claim 1 is characterized in that: The front of the plastic bottom shell (1) is provided with vertical walls around it, the height of which is consistent with the thickness of the PCB (5) plus the entire bowl and cup plastic part (7).
7. The production process of the outdoor full-color LED display module according to claim 1 is characterized in that: A single bowl of the whole bowl-cup plastic part (7) is a square trumpet-shaped structure with a small inside and a large outside, and the opening angle of the bowl is 20 to 45 degrees; The whole bowl and cup plastic part (7) is made of high temperature resistant nylon material or high temperature resistant metal material. The whole bowl and cup plastic part (7) can withstand a minimum thermal deformation temperature of 300°C and a minimum continuous use temperature of 170°C. The inner wall of the bowl and cup is white and the surface is inkjet.
8. The production process of the outdoor full-color LED display module according to claim 1, characterized in that: When the finished module is used outdoors, a waterproof rubber ring is installed on the plastic bottom shell (1) to provide a waterproof effect at the junction between the module and the box body, so that the module as a whole reaches the IP65 waterproof level.
Citation Information
Patent Citations
LED display module and manufacturing method thereof
CN113130466A
Exempt from waterproof high density LED display screen of encapsulating
CN208655172U
LED flip support, LED lamp bead and LED lamp
CN212113739U