Packaging structure manufacturing method and chip anti-warping device

By applying pressure to the upper chip using the weight of the cover plate in the chip anti-warping device, the problem of soldering performance failure caused by warping in the 3D stacked chip is solved, and the soldering quality of the 3D package is improved.

CN115101434BActive Publication Date: 2024-12-06JCET GROUP CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210863313.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-07-21
Publication Date
2024-12-06
Estimated Expiration
2042-07-21

AI Technical Summary

Technical Problem

In 3D stacked chips, TSV chips are prone to warping problems in room temperature or high temperature environments, especially when the upper chip size is small, resulting in failure of soldering performance and difficulty in completing effective packaging.

Method used

Provide a chip anti-warping device, including a base, support and cover plate, by fixing the product packaging structure, and applying pressure to the upper chip using the weight of the cover plate in the reflow process to prevent the lower chip from warping and ensure welding. quality.

Benefits of technology

It effectively suppresses the warpage of the lower chip during the reflow soldering process of the chip package structure, improves the welding quality of the 3D package, and ensures effective welding between the upper and lower chips.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115101434B_ABST
    Figure CN115101434B_ABST
Patent Text Reader

Abstract

The present invention discloses a packaging structure manufacturing method and a chip anti-warping device, the manufacturing method includes the steps of: providing a test substrate and a test stacked chipset to form a test packaging structure; subjecting the test packaging structure to a reflow soldering process; testing the welding performance of the packaging structure after the reflow soldering process; when the welding performance fails, providing a chip anti-warping device and a product packaging structure identical to the test packaging structure, fixing the product packaging structure in the chip anti-warping device, and then subjecting the reflow soldering process. The method can effectively prevent and inhibit the lower chip from warping to a large extent during the reflow soldering process, reduce the risk of welding failure between the upper chip and the lower chip, and improve the welding quality of 3D packaging.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of semiconductor packaging, and in particular to a packaging structure manufacturing method and a chip anti-warping device. Background Art

[0002] TSV (Through Silicon Via) technology is a high-density packaging technology that is gradually replacing the current more mature wire bonding technology and is considered the fourth generation packaging technology. TSV technology is to make vertical conduction between chips and wafers, and to achieve vertical electrical interconnection of silicon vias by filling with conductive materials such as copper, tungsten, and polysilicon. Vertical interconnection can reduce the interconnection length, reduce signal delay, and reduce capacitance / inductance, thereby achieving low power consumption between chips, high-speed communication, increased bandwidth, and miniaturization of device integration.

[0003] As electronic products develop in the direction of miniaturization, no matter how the stacking form and connection method change, the thickness of each layer of chips used in the stack will inevitably need to be thinned as the overall thickness of the package remains unchanged or even decreases. In 3D stacking projects, the thickness of TSV chips is between 100 and 200μm. Compared with conventional chips, warping problems will occur at room temperature or high temperature, and the degree of warping increases with the size of the chip. Under the current conventional process, after the TSV chip is flipped and reflowed and the bottom is filled, its warping can reach more than 200μm. In the case of large warping of the TSV chip, it will be difficult to mount the chip on the TSV chip, especially when the top chip is small, it is difficult to complete the overall chip packaging. Summary of the invention

[0004] The object of the present invention is to provide a packaging structure manufacturing method and a chip anti-warping device.

[0005] To achieve one of the above-mentioned purposes of the invention, an embodiment of the present invention provides a method for manufacturing a packaging structure, the manufacturing method comprising the steps of:

[0006] Providing a test substrate and a test stacked chip set, wherein the test stacked chip set at least includes an upper test chip and a lower test chip, and the lower test chip is formed between the test substrate and the upper test chip to form a test package structure;

[0007] Performing a reflow process on the test package structure;

[0008] Testing the welding performance between the upper test chip and the lower test chip after the reflow process;

[0009] When the welding performance fails, a chip anti-warping device and a product packaging structure identical to the test packaging structure are provided, wherein the chip anti-warping device comprises a base, at least two supporting members and a cover plate, the product packaging structure is fixedly placed on the base, the supporting members are respectively placed on both sides of the product packaging structure, the cover plate is covered on the upper surface of the product packaging structure, and is mounted on the supporting members;

[0010] The product packaging structure fixedly loaded in the chip anti-warping device is subjected to a reflow soldering process.

[0011] As a further improvement of an embodiment of the present invention, the lower test chip is formed between the test substrate and the upper test chip to form a test package structure, which specifically includes:

[0012] Flip-chip soldering the functional surface of the lower test chip to the upper surface of the test substrate through solder balls;

[0013] The functional surface of the upper test chip is flip-chip soldered to the upper surface of the lower test chip through solder balls.

[0014] As a further improvement of an embodiment of the present invention, the welding performance between the upper test chip and the lower test chip in the packaging structure after the reflow process is tested specifically includes:

[0015] Testing the electrical conductivity between the upper test chip and the lower test chip;

[0016] The welding quality of the solder balls is detected using X-Ray technology.

[0017] As a further improvement of an embodiment of the present invention, the providing of a product packaging structure that is completely identical to the test packaging structure specifically includes:

[0018] Providing a substrate identical to the test substrate and a stacked chipset identical to the test stacked chipset, the stacked chipset comprising at least an upper chip identical to the upper test chip and a lower chip identical to the lower test chip;

[0019] The lower chip is formed between the substrate and the upper chip to form a product packaging structure.

[0020] As a further improvement of an embodiment of the present invention, the step of fixing the product packaging structure on the base specifically includes:

[0021] The device also includes a substrate fixing member, and the substrate fixing member is placed above the base;

[0022] The substrate is fixedly clamped in the substrate fixing member.

[0023] As a further improvement of an embodiment of the present invention, the supporting members are respectively placed on both sides of the product packaging structure, the cover plate is covered on the upper surface of the product packaging structure, and is mounted on the supporting members, specifically including:

[0024] The support members placed on one side of the substrate include a group of first support members and two groups of second support members, the first support members are placed on opposite sides of the cover plate along the length direction, and the two groups of second support members are placed on opposite sides of the cover plate along the width direction, and the first support members and the second support members placed on the same side of the substrate form a triangular structure on a plane;

[0025] The cover plate is covered on the upper surface of the upper chip and is simultaneously mounted on the first support member and the second support member.

[0026] As a further improvement of an embodiment of the present invention, the manufacturing method further includes:

[0027] A step is formed at the top of the first support member and the second support member, which is recessed inward toward one side of the cover plate. The height of the upper surface of the step is consistent with the height of the upper surface of the upper chip. The cover plate is placed on the upper surfaces of the steps of the first support member and the second support member at both ends in its length direction. The cover plate is fixedly clamped in the steps of the first support member and the second support member.

[0028] As a further improvement of an embodiment of the present invention, the manufacturing method further includes:

[0029] An elastic member is installed at a partial area of ​​the support member, and the elastic member can enable the support member to perform telescopic movement in its height direction.

[0030] The present invention also provides a chip anti-warping device, the chip anti-warping device comprises a base and at least two supporting members arranged on the base, the base is used to place a substrate and a stacked chipset arranged on the substrate, the stacked chipset comprises at least an upper chip and a lower chip, the lower chip is arranged between the substrate and the upper chip, and the supporting members are respectively arranged on both sides of the substrate;

[0031] The device further comprises a cover plate, which is arranged on the upper surface of the upper chip and mounted on the support member.

[0032] As a further improvement of one embodiment of the present invention, the support members arranged on both sides of the substrate include a first support member and a second support member, the first support member is arranged on opposite sides of the cover plate along the length direction, and the second support member is arranged on opposite sides of the cover plate along the width direction.

[0033] As a further improvement of one embodiment of the present invention, the support members arranged on one side of the substrate include a group of first support members and two groups of second support members, the two groups of second support members are respectively arranged on opposite sides of the cover plate along the width direction, and the first support members and the second support members located on the same side of the substrate form a triangular structure on the plane.

[0034] As a further improvement of one embodiment of the present invention, the top of the first support member and the second support member are recessed inward toward the side of the substrate to form a step, and the height of the upper surface of the step is consistent with the height of the upper surface of the upper chip. The cover plate is simultaneously mounted on the upper surface of the steps of the first support member and the second support member at both ends in its length direction, and the cover plate is fixedly clamped in the steps of the first support member and the second support member.

[0035] As a further improvement of one embodiment of the present invention, the functional surface of the lower chip is flip-chip welded to the upper surface of the substrate through solder balls, and the functional surface of the upper chip is flip-chip welded to the upper surface of the lower chip through solder balls.

[0036] As a further improvement of an embodiment of the present invention, the device further includes a substrate fixing member, the substrate fixing member is arranged above the base, and the substrate is fixedly clamped in the substrate fixing member.

[0037] As a further improvement of an embodiment of the present invention, the top end height of the substrate fixing member is lower than the upper surface height of the step.

[0038] As a further improvement of an embodiment of the present invention, an elastic member is provided in a partial area of ​​the support member, and the elastic member can enable the support member to perform telescopic movement in its height direction.

[0039] The beneficial effect of the present invention is that: the formed test packaging structure is subjected to a reflow soldering process once, and if the welding performance of the test packaging structure is normal after the reflow soldering process, the chip that is the same as the test packaging structure in the subsequent product manufacturing process can adopt a manufacturing process of first welding and then reflowing once; however, when the welding performance of the test packaging structure fails after the reflow soldering process, in the subsequent product manufacturing process, the product packaging structure that is the same as the test packaging structure is fixedly installed in the chip anti-warping device provided by the present invention, and then the reflow soldering process is performed. Even when the upper chip is small in size and light in weight, the weight of the cover plate is used to apply pressure to the upper chip, which can well suppress the chip packaging structure from generating a large degree of warping of the lower chip during the reflow soldering process, prevent welding problems between the upper chip and the lower chip, and improve the 3D packaging welding quality. BRIEF DESCRIPTION OF THE DRAWINGS

[0040] Figure 1 Schematic diagram of a method for manufacturing a packaging structure in one embodiment of the present invention.

[0041] 2( a ) to ( h ) are diagrams showing steps of manufacturing a packaging structure in one embodiment of the present invention.

[0042] Figure 3 FIG. 4 is a structural side view of a chip anti-warping device in one embodiment of the present invention.

[0043] Figure 4 FIG. 4 is a top view of the structure of a chip anti-warping device in one embodiment of the present invention.

[0044] Figure 5 FIG. 4 is a structural side view of a chip anti-warping device in another embodiment of the present invention. DETAILED DESCRIPTION

[0045] In order to make the purpose, technical solution and advantages of the present invention clearer, the technical solution of the present invention will be clearly and completely described below in combination with the specific implementation methods of the present invention and the corresponding drawings. Obviously, the described implementation methods are only part of the implementation methods of the present invention, not all implementation methods. Based on the implementation methods of the present invention, all other implementation methods obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0046] The embodiments of the present invention are described in detail below, and examples of the embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.

[0047] For ease of explanation, this document uses terms that represent relative positions in space for description, such as "above", "below", "back", "front", etc., to describe the relationship of one unit or feature shown in the drawings relative to another unit or feature. Terms of relative positions in space can include different orientations of the device in use or operation other than the orientation shown in the figure. For example, if the device in the figure is turned over, the unit described as being "below" or "above" other units or features will be located "below" or "above" the other units or features. Therefore, the exemplary term "below" can encompass both the spatial orientations of below and above.

[0048] An embodiment of the present invention further provides a method for manufacturing a packaging structure, such as Figure 1 As shown, the steps include:

[0049] S1: providing a test substrate and a test stacked chipset, wherein the test stacked chipset comprises at least an upper test chip and a lower test chip, and forming the lower test chip between the test substrate and the upper test chip to form a test package structure.

[0050] S2: Perform a reflow process on the test package structure.

[0051] S3: Testing the welding performance between the upper test chip and the lower test chip after the reflow process.

[0052] S4: When the welding performance fails, a chip anti-warping device and a product packaging structure identical to the test packaging structure are provided, wherein the chip anti-warping device comprises a base, at least two supporting members and a cover plate, the product packaging structure is fixedly placed on the base, the supporting members are respectively placed on both sides of the product packaging structure, the cover plate is covered on the upper surface of the product packaging structure, and is mounted on the supporting members.

[0053] S5: Perform a reflow process on the product packaging structure fixedly loaded in the chip anti-warping device.

[0054] In step S1, a test substrate 1' and a test stacked chip set 2' are provided. The test stacked chip set 2' includes at least an upper test chip 21' and a lower test chip 22'. The lower test chip 22' is formed between the test substrate 1' and the upper test chip 21' to form a test package structure A', which specifically includes:

[0055] As shown in Fig. 2(a) to (c), a test substrate 1' is provided, and a plurality of electrical pads are arranged on the upper surface of the test substrate 1'. The functional surface of the lower test chip 22' is welded to the upper surface of the test substrate 1' through the solder ball 6 by the flip-chip ball welding process, so that the lower test chip 22' and the test substrate 1' are electrically connected. The functional surface of the upper test chip 21' is flip-chip welded to the upper surface of the lower test chip 22' through the solder ball 6, so that the upper test chip 21' and the lower test chip 22' are electrically connected. In this embodiment, the lower test chip 22' is preferably a TSV chip, and its thickness can be selected to be 100 to 200 μm. The upper test chip 21' is other functional chips, and the chip thickness can be selected according to actual design requirements. The solder ball 6 is a tin ball, which can be melted at high temperature for welding and is solid at room temperature, and plays a certain supporting role for the lower test chip 22' and the upper test chip 21'.

[0056] Of course, this step also includes coating flux on the functional surfaces of the lower test chip 22' and the upper test chip 21'. This is the prior art and the present invention will not be elaborated on here. However, it should be emphasized that in a specific embodiment of the present invention, a flux with high viscosity and good temperature resistance, such as a resin-activated series flux, is used to prevent the risk of displacement between the upper test chip 21', the lower test chip 22' and the test substrate 1' during the reflow process of the packaging structure.

[0057] In one embodiment of the present invention, the upper test chip 21' is two chips welded side by side on the lower test chip 22', as shown in Figure 2(c). In other embodiments of the present invention, the upper test chip 21' may also be multiple chips welded side by side on the lower test chip 22', or multiple layers of chips welded in a vertical direction, which can be set according to actual design requirements, and the present invention is not limited here.

[0058] In step S3, the welding performance between the upper test chip 21' and the lower test chip 22' after the reflow process is tested, specifically including:

[0059] The conductive performance of the test package structure A' after step S2 is tested. Specifically, the conductive performance between the upper test chip 21' and the lower test chip 22' is tested. If there is an electrical connection between the upper test chip 21' and the lower test chip 22', the test result is normal. For each chip that is the same as the upper test chip 21' and the lower test chip 22', the process can be carried out according to steps S1-S2, and the chip welding and assembly are first performed, and then the reflow process is performed again; if the test result of the conductive performance between the upper test chip 21' and the lower test chip 22' is an open circuit or a short circuit, step S4 is performed.

[0060] In another embodiment of the present invention, the test package structure A' after step S2 can also be inspected by X-Ray technology for the welding quality of the solder balls 6. Specifically, the welding quality of each solder ball 6 between the upper test chip 21' and the lower test chip 22' is inspected to observe whether there are voids, solder bridges, too large solder joints, insufficient solder joints, etc. in the solder balls 6 after the reflow process. Similarly, if the inspection result is normal, the same chips as the upper test chip 21' and the lower test chip 22' can be manufactured according to steps S1-S2, firstly performing chip welding and assembly, and then reflowing the manufacturing process; if abnormal conditions are detected in the solder balls 6, step S4 is performed.

[0061] Of course, in other embodiments of the present invention, the conductive performance of the package structure A' can be detected, and the welding quality of the solder ball 6 can be detected by X-Ray technology to ensure the accuracy of whether the solderability of the package structure is effective. Specifically, the detection can be carried out based on the actual manufacturing process, and the present invention does not limit the specific technical means for detecting the welding performance.

[0062] In step S4, a product package structure A identical to the test package structure A' is provided, specifically including:

[0063] As shown in FIG. 2( d ), a substrate 1 identical to a test substrate 1 ′ and a stacked chipset 2 identical to a test stacked chipset 2 ′ are provided, the stacked chipset 2 comprising at least an upper chip 21 identical to an upper test chip 21 ′ and a lower chip 22 identical to a lower test chip 22 ′.

[0064] The lower chip 22 is formed between the substrate 1 and the upper chip 21 to form a product packaging structure A. Specifically, a plurality of electrical pads are provided on the upper surface of the substrate 1. The functional surface of the lower chip 22 is welded to the upper surface of the substrate 1 through the solder balls 6 by a flip-chip ball welding process, so that the lower chip 22 and the substrate 1 are electrically connected. The functional surface of the upper chip 21 is flip-chip welded to the upper surface of the lower chip 22 through the solder balls 6, so that the upper chip 21 and the lower chip 22 are electrically connected. Here, the chip type selection of the upper chip 21 and the lower chip 22 and the specific arrangement of the upper chip 21 are the same as those in the test packaging structure A', and will not be described in detail here. The packaging structure in which the upper chip 21 is welded side by side on the lower chip 22 as shown in Figure 2 (d) is used as an example for explanation below.

[0065] In step S4, a chip anti-warping device is provided to fix the product package structure A on the base 3, which specifically includes:

[0066] As shown in FIG. 2(e), a substrate fixing member 7 is also provided in the chip anti-warping device in the specific embodiment of the present invention. The product packaging structure A and the substrate fixing member 7 are placed above the base 3. The substrate fixing member 7 is placed at least at one corner of the substrate 1. Two substrate fixing members 7 are placed on both sides of the corner ends of one corner of the substrate 1. The substrate 1 is fixed by the two substrate fixing members 7 placed on both sides of the diagonal corner ends. Specifically, two substrate fixing members 7 are placed on both sides of each corner end of the two diagonal corners of the substrate 1. The substrate 1 is fixedly clamped in the substrate fixing member 7 to fix the substrate 1 in the subsequent packaging process.

[0067] In a specific embodiment of the present invention, the height of the substrate fixing member 7 provided may be slightly higher than the height of the upper surface of the substrate 1 to ensure that it can better fix the substrate 1. However, the present invention does not limit the specific height of the substrate fixing member 7, as long as the top height of the substrate fixing member 7 is lower than the height of the upper surface of the upper chip 21, the substrate 1 can be fixed without interfering with the lower surface of the cover plate 5 placed above the upper chip 21 in the subsequent process.

[0068] Preferably, the substrate fixing member 7 is a Pin. Of course, in some other embodiments of the present invention, the substrate fixing member 7 may also be a fixing member made of other high temperature resistant materials, which can still fix the substrate 1 at high temperatures.

[0069] In some other embodiments of the present invention, the substrate 1 may be first fixed on the base 3, and then a chip welding process may be performed on the upper surface of the substrate 1 to form a product packaging structure A. The present invention does not limit the order of these two processes.

[0070] In step S4, the support members 4 are respectively placed on both sides of the product packaging structure A, and the cover plate 5 is covered on the upper surface of the product packaging structure A and mounted on the support members 4, which specifically includes:

[0071] As shown in FIG. 2( f), the cover plate 5 is a rectangular silicon wafer. The cover plate 5 is placed on the upper surface of the upper chip 21, that is, its lower surface is in contact with the upper surface of the upper chip 21, and is used to apply a certain pressure to the upper chip 21. The greater its weight, the greater the pressure applied to the upper chip 21. The size of the cover plate 5 can be designed according to the specific arrangement of the upper chip 21. Preferably, the cover plate 5 is arranged to fully cover the upper surface of each upper chip 21 to ensure that each point of each upper chip 21 is uniformly stressed. The thickness of the cover plate 5 can be determined according to actual design requirements. In the subsequent reflow soldering process, the pressure applied by the cover plate 5 to the upper chip 21 can prevent the lower chip 22 from warping and will not affect the effective welding between the upper chip 21 and the lower chip 22. At the same time, it can also ensure that the pressure applied to the upper chip 21 does not collapse the solder ball 6. Of course, in some other embodiments, the material of the cover plate 5 can also be other high-temperature resistant materials, such as glass sheets, etc.

[0072] As shown in FIG. 2( g), the support member 4 provided in the specific embodiment of the present invention and placed on one side of the substrate 1 includes a group of first support members 41 and two groups of second support members 42. The first support members 41 are placed on opposite sides of the cover plate 5 along the length direction, and the two groups of second support members 42 are placed on opposite sides of the cover plate 5 along the width direction. The first support members 41 and the second support members 42 placed on the same side of the substrate 1 form a triangular structure on the plane.

[0073] Specifically, the top of the first support member 41 and the second support member 42 are provided to be recessed inward toward one side of the cover plate 5 to form a step 43, and the height of the upper surface of the step 43 is consistent with the height of the upper surface of the upper chip 21. The cover plate 5 is placed on the upper surfaces of the steps 43 of the first support member 41 and the second support member 42 at both ends in the length direction, and the cover plate 5 can be fixedly clamped in the steps of the first support member 41 and the second support member 42. In this way, the step surfaces of the first support members 41 placed on the opposite sides in the length direction of the cover plate 5 fix the cover plate 5 in the length direction, and the step surfaces of the second support members 42 located on the opposite sides in the width direction of the cover plate 5 fix the cover plate 5 in the width direction.

[0074] Preferably, the first support member 41 and the second support member 42 are pins. Of course, the present invention does not limit the materials used to make the first support member 41 and the second support member 42. A material that can withstand high temperatures and has a certain supporting force at high temperatures can be selected.

[0075] In some possible embodiments of the present invention, the first support member 41, the second support member 42 and the substrate fixing member 7 in the chip anti-warping device provided can be movably fixed to any position on the base 3, and the specific position where the first support member 41 and the second support member 42 are fixed on the base 3 can be determined according to the specific length of the cover plate 5 and the specific position where it is placed on the upper surface of the upper chip 21. The steps of the first support member 41 and the second support member 42 placed on both sides of the cover plate 5 can limit the movement of the cover plate 5 in its length direction and width direction. The specific number and arrangement of the support members 4 provided for supporting and fixing the cover plate 5 are specifically adjusted according to factors such as the size of the cover plate 5. The specific position where the substrate fixing member 7 is fixed on the base 3 is specifically adjusted according to the specific size of the substrate 1, and the substrate fixing members 7 placed on both sides of each corner end of the two diagonal corners of the substrate 1 can limit the movement of the substrate 1 in its length direction and width direction.

[0076] Finally, step S5 is performed to perform a reflow soldering process on the product packaging structure fixedly loaded in the provided chip anti-warping device. Since the cover plate 5 exerts a certain pressure on the upper chip 21 and can relatively avoid the horizontal movement of the upper chip 21 and the lower chip 22 under high temperature, it can also prevent the problem of welding failure between the upper chip 21 and the lower chip 22 caused by large warping of the lower chip 22 due to temperature changes during the reflow soldering process.

[0077] However, since the solder ball 6 is in a melted state at high temperature, the size, thickness and weight design of the cover plate 5 are very important for the pressure applied to the upper chip 21 and the lower chip 22. Excessive pressure can easily lead to bridging between the upper chip 21 and the lower chip 22, and between the lower chip 22 and the substrate 1. Therefore, the selection of the size, thickness and weight of the cover plate 5 needs to be very precise, and the process is difficult.

[0078] Therefore, in step S4 of the method for manufacturing the packaging structure of the present invention, another chip anti-warping device structure is also provided, as shown in FIG2(h), before the first support member 41 and the second support member 42 are fixedly placed on the base 3, an elastic member 8 is first installed at a partial area of ​​the support member 4. Specifically, an elastic member 8 is installed at the bottom end of each of the first support member 41 and the second support member 42, and the elastic member 8 can enable the first support member 41 and the second support member 42 to perform telescopic movement in their height direction.

[0079] When the solder ball 6 is in a melted state at high temperature, its support force on the upper chip 21 and the lower chip 22 is reduced. When the pressure of the cover plate 5 on the upper chip 21 and the lower chip 22 is greater than the support force of the solder ball 6 on the upper chip 21 and the lower chip 22 at high temperature, the elastic member 8 gradually contracts, that is, the elastic member 8 moves downward in its height direction, and the support force of the elastic member 8 on the cover plate 5 increases, avoiding the bridge phenomenon between the upper chip 21 and the lower chip 22, and between the lower chip 22 and the substrate 1. Of course, in this embodiment, the weight of the cover plate 5 and the elastic strength of the elastic member 8 are designed according to different products, and the present invention is not limited here. In the chip anti-warping device equipped with the elastic member 8, the selection of the size, thickness and weight of the cover plate does not need to be precisely controlled, which greatly reduces the process difficulty.

[0080] Of course, in the chip anti-warping device equipped with the elastic member 8, the elastic member 8 is not limited to being installed at the bottom end of the support member 4, and it can also be fixedly installed on the upper surface of the step 43 of each support member, and the cover plate 5 is placed above the elastic member 8 at both ends in its length direction, and is fixedly clamped in the step 43 of each support member. It should be noted that when the elastic member 8 is installed on the upper surface of the step 43 of each support member, the height of the upper surface of the step 43 at this time needs to be lower than the height of the upper surface of the upper chip 21, and the height of the upper surface of the elastic member 8 installed on the step 43 needs to be consistent with the height of the upper surface of the upper chip 21.

[0081] Alternatively, in other possible embodiments of the present invention, the support member 4 is integrally supported as an elastic member, a circular hole matching the size of the support member 4 is made on the lower surface of the cover plate 5, and the top end of the support member 4 can be fixedly engaged in the circular hole to support and fix the cover plate 5.

[0082] The present invention is not limited to the specific structural relationship between the support member 4, the elastic member 8 and the cover plate 5 in the chip anti-warping device provided. It only needs to be able to support and fix the cover plate 5 and enable the cover plate 5 to move in its height direction.

[0083] The packaging structure fixedly loaded in the chip anti-warping device equipped with an elastic member 8 as shown in Figure 2 (h) is carried out to step S5. The elastic member 8 installed at the bottom of the support member 4 can prevent the solder balls from melting at high temperatures during the reflow process, thereby reducing the supporting force on the upper chip 21 and the lower chip 22. At this time, the elastic member 8 can provide a certain supporting force for the cover plate 5 to avoid bridging between the upper chip 21 and the lower chip 22, and between the lower chip 22 and the substrate 1.

[0084] like Figure 3 and 4As shown, the present invention also provides a chip anti-warping device, which is applied to the manufacturing method of the packaging structure. In the 3D stacking project, the lower chip is relatively thin. At room temperature or high temperature, the lower chip is prone to large warping. When the welding performance between the chips cannot be guaranteed after the reflow process of the completed test packaging structure, the chip anti-warping device provided by the present invention is needed. Especially when the upper chip is small in size, the pressure on the lower chip cannot suppress the warping of the lower chip, which easily leads to the problem of welding failure between the upper chip and the lower chip. Therefore, the chip anti-warping device provided by the present invention is applied to the case where the upper chip is small in size and light in weight.

[0085] The chip anti-warping device provided in one embodiment of the present invention includes a base 3 and at least two support members 4 arranged on the base 3 . The base 3 is used to place a substrate 1 and a stacked chipset 2 arranged on the substrate 1 .

[0086] The stacked chipset 2 includes at least an upper chip 21 and a lower chip 22, and the lower chip 22 is arranged between the substrate 1 and the upper chip 21. The lower chip 22 is preferably a TSV chip, and its thickness can be selected to be 100-200 μm. The upper chip 21 is other functional chips, and the chip thickness can be selected according to actual design requirements. In one embodiment of the present invention, the upper chip 21 is two chips welded side by side on the lower chip 22, as shown in the figure. Of course, in other embodiments of the present invention, the upper chip 21 can also be a plurality of chips welded side by side on the lower chip 22, or a plurality of chips welded in a vertical direction, which can be arranged according to actual design requirements. The present invention is not limited here. The following is explained by taking the packaging structure of the upper chip 21 as two chips welded side by side on the lower chip 22 as an example.

[0087] Specifically, the lower chip 22 has a functional surface provided with a pad and a non-functional surface opposite to the functional surface. The functional surface of the lower chip 22 is arranged toward the substrate 1, and is flip-chip soldered to the upper surface of the substrate 1 through the solder ball 6 to achieve electrical connection with the substrate 1. Similarly, the upper chip 21 has a functional surface provided with a pad and a non-functional surface opposite to the functional surface. The functional surface of the upper chip 21 is arranged toward the lower chip 22, and is flip-chip soldered to the upper surface of the lower chip 22 through the solder ball 6 to achieve electrical connection with the lower chip 22. In this embodiment, the solder ball 6 is specifically a tin ball, which can be melted at high temperature for welding and is solid at room temperature, and plays a certain supporting role for the lower chip 22 and the upper chip 21.

[0088] The support members 4 are respectively arranged on both sides of the substrate 1, and the chip anti-warping device also includes a cover plate 5, which is covered on the upper surface of the upper chip 21 and mounted on the support member 4. Specifically, the cover plate 5 is a rectangular silicon wafer, and its lower surface is in contact with the upper surface of the upper chip 21, which is used to apply a certain pressure to the upper chip 21. The greater its weight, the greater the pressure applied to the upper chip 21. The size of the cover plate 5 can be designed according to the specific arrangement of the upper chip 21. Preferably, the cover plate 5 is arranged to fully cover the upper surface of each upper chip 21 to ensure that each point of each upper chip 21 is uniformly stressed. The thickness of the cover plate 5 can be determined according to actual design requirements. In the subsequent reflow soldering process, the pressure applied by the cover plate 5 to the upper chip 21 can prevent the lower chip 22 from warping, and will not affect the effective welding between the upper chip 21 and the lower chip 22, and can also ensure that the pressure applied to the upper chip 21 does not collapse the solder ball 6. Of course, in some other embodiments, the cover plate 5 may also be made of other high temperature resistant materials, such as glass sheets and the like.

[0089] Specifically, the support members 4 disposed on both sides of the substrate 1 include a first support member 41 and a second support member 42 . The first support member 41 is disposed on opposite sides of the cover plate 5 along the length direction, and the second support member 42 is disposed on opposite sides of the cover plate 5 along the width direction.

[0090] The support member 4 disposed on one side of the substrate 1 includes a group of first support members 41 and two groups of second support members 42. The two groups of second support members 42 are respectively disposed on opposite sides of the cover plate 5 along the width direction. The first support members 41 and the second support members 42 located on the same side of the substrate 1 form a triangular structure on the plane.

[0091] More specifically, the tops of the first support member 41 and the second support member 42 are recessed inward toward one side of the cover plate 5 to form a step 43, the upper surface height of the step 43 is consistent with the upper surface height of the upper chip 21, and the cover plate 5 is mounted on the upper surfaces of the steps 43 of the first support member 41 and the second support member 42 at both ends in the length direction, and the cover plate 5 is fixedly clamped in the steps of the first support member 41 and the second support member 42. That is, the step surfaces of the first support member 41 located on the opposite sides in the length direction of the cover plate 5 fix the cover plate 5 in the length direction, and the step surfaces of the second support member 42 located on the opposite sides in the width direction of the cover plate 5 fix the cover plate 5 in the width direction.

[0092] In a specific embodiment of the present invention, the first support member 41 and the second support member 42 are pins. Of course, the present invention does not limit the materials used to make the first support member 41 and the second support member 42. Materials that can withstand high temperatures and have a certain supporting force at high temperatures can be selected.

[0093] Furthermore, the chip anti-warping device further includes a substrate fixing member 7, which is disposed above the base 3, and the substrate fixing member 7 is disposed at least at one corner of the substrate 1, and two substrate fixing members 7 are respectively disposed on both sides of the corner ends of one corner of the substrate 1, and the substrate 1 is fixedly clamped in the substrate fixing member 7. In this embodiment, two substrate fixing members 7 are respectively disposed on both sides of each corner end of the two diagonal corners of the substrate 1, so as to fix the substrate 1 in a fixed position during the subsequent packaging process.

[0094] Specifically, the top height of the substrate fixing member 7 may be slightly higher than the top surface height of the substrate 1 to ensure that it can better fix the substrate 1. However, the present invention does not limit the specific height of the substrate fixing member 7, as long as the top height of the substrate fixing member 7 is lower than the top surface height of the step 43, the substrate 1 can be fixed without interfering with the bottom surface of the cover plate 5.

[0095] The substrate fixing member 7 is also a Pin. Of course, in some other embodiments of the present invention, the substrate fixing member 7 can also be a fixing member made of other high-temperature resistant materials, which can still fix the substrate 1 at high temperatures.

[0096] In some possible embodiments of the present invention, the first support member 41, the second support member 42 and the substrate fixing member 7 can be movably fixed at any position on the base, and the specific position where the first support member 41 and the second support member 42 are fixed on the base 3 can be determined according to the specific length of the cover plate 5 and the specific position where it is placed on the upper surface of the upper chip 21, and the steps of the first support member 41 and the second support member 42 located on both sides of the cover plate 5 can limit the movement of the cover plate 5 in its length direction and width direction. The specific number and arrangement of the support members 4 used to support and fix the cover plate 5 are specifically adjusted according to factors such as the size of the cover plate 5. The specific position where the substrate fixing member 7 is fixed on the base 3 can be determined according to the specific size of the substrate 1, and the substrate fixing members 7 located on both sides of each corner end of the two diagonal corners of the substrate 1 can limit the movement of the substrate 1 in its length direction and width direction.

[0097] At room temperature, since the solder ball 6 is solid, it can support the pressure of the cover plate 5 on the upper chip 21 and the lower chip 22. At high temperature, the solder ball 6 will melt as the temperature rises. The size, thickness, and weight design of the cover plate 5 are very important for the pressure applied to the upper chip 21 and the lower chip 22. Excessive pressure can easily cause bridging between the upper chip 21 and the lower chip 22, and between the lower chip 22 and the substrate 1. Therefore, the selection of the size, thickness and weight of the cover plate 5 in the chip anti-warping device in the above embodiment needs to be very precise, and the process is difficult.

[0098] like Figure 5FIG. 1 is a chip anti-warping device in another embodiment of the present invention, and FIG. Figure 3 The difference between the structures is that, in order to prevent the solder balls 6 on the lower surfaces of the upper chip 21 and the lower chip 22 from melting at high temperature and causing a bridge phenomenon between the upper chip 21 and the lower chip 22, and between the lower chip 22 and the substrate 1, a part of the support member 4 is provided with an elastic member 8, and the elastic member 8 can make the support member 4 perform telescopic movement in its height direction. Specifically, the elastic member 8 is provided at the bottom end of the support member 4, that is, the bottom ends of the first support member 41 and the second support member 42 are both provided with an elastic member 8. Since the solder balls 6 are in a melted state at high temperature, the supporting force on the upper chip 21 and the lower chip 22 is reduced. When the pressure of the cover plate 5 on the upper chip 21 and the lower chip 22 is greater than the supporting force of the solder balls 6 on the upper chip 21 and the lower chip 22 at high temperature, the elastic member 8 gradually contracts, that is, the elastic member 8 moves downward in its height direction, and the supporting force of the elastic member 8 on the cover plate 5 increases, thereby avoiding the bridge phenomenon between the upper chip 21 and the lower chip 22, and between the lower chip 22 and the substrate 1. In this embodiment, the weight of the cover plate 5 and the elastic strength of the elastic member 8 are designed differently according to different products, and the present invention does not limit this.

[0099] Of course, the elastic member 8 in the present invention is not limited to being arranged at the bottom end of the support member 4, and it can also be fixedly arranged on the upper surface of the step 43 of each support member, and the cover plate 5 is placed above the elastic member 8 at both ends in its length direction, and is fixedly clamped in the step 43 of each support member. It should be noted that when the elastic member 8 is arranged on the upper surface of the step 43 of each support member, the height of the upper surface of the step 43 at this time needs to be lower than the height of the upper surface of the upper chip 21, and the height of the upper surface of the elastic member 8 placed on the step 43 needs to meet the consistency with the height of the upper surface of the upper chip 21.

[0100] Alternatively, in other possible embodiments of the present invention, the support member 4 is an elastic member as a whole, and a circular hole matching the size of the support member 4 is provided on the lower surface of the cover plate 5, and the top end of the support member 4 can be fixedly engaged in the circular hole to support and fix the cover plate 5.

[0101] The present invention is not limited to the specific structural relationship between the support member 4, the elastic member 8 and the cover plate 5. It only needs to be able to support and fix the cover plate 5 and enable the cover plate 5 to move in its height direction.

[0102] To sum up, the test packaging structure formed in the present invention is subjected to a reflow soldering process once. If the welding performance of the test packaging structure is normal after the reflow soldering process, the chip that is the same as the test packaging structure in the subsequent product manufacturing process can adopt a manufacturing process of first welding and then reflowing once; however, when the welding performance of the test packaging structure fails after the reflow soldering process, in the subsequent product manufacturing process, the product packaging structure that is the same as the test packaging structure is fixedly installed in the chip anti-warping device provided by the present invention, and then the reflow soldering process is performed. Even if the upper chip is small in size and light in weight, the weight of the cover plate is used to apply pressure to the upper chip, which can well suppress the chip packaging structure from causing a large degree of warping of the lower chip during the reflow soldering process, thereby preventing welding problems between the upper chip and the lower chip, and improving the 3D packaging welding quality.

[0103] It should be understood that although this specification is described according to implementation modes, not every implementation mode contains only one independent technical solution. This description of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each implementation mode may also be appropriately combined to form other implementation modes that can be understood by those skilled in the art.

[0104] The series of detailed descriptions listed above are only specific descriptions of feasible implementation methods of the present invention. They are not intended to limit the scope of protection of the present invention. Any equivalent implementation methods or changes that do not deviate from the technical spirit of the present invention should be included in the scope of protection of the present invention.

Claims

1. A method for manufacturing a packaging structure, characterized in that: The production method comprises the steps of: Providing a test substrate and a test stacked chip set, wherein the test stacked chip set at least includes an upper test chip and a lower test chip, and the lower test chip is formed between the test substrate and the upper test chip to form a test package structure; Performing a reflow process on the test package structure; Testing the welding performance between the upper test chip and the lower test chip after the reflow process; When the welding performance fails, a chip anti-warping device and a product packaging structure identical to the test packaging structure are provided, wherein the chip anti-warping device comprises a base, at least two supporting members and a cover plate arranged on the base, the product packaging structure is fixedly placed above the base, the supporting members are respectively placed on both sides of the product packaging structure, the cover plate is covered on the upper surface of the product packaging structure, and is mounted on the supporting members; Performing a reflow soldering process on the product packaging structure fixedly loaded in the chip anti-warping device; The production method further comprises: An elastic member is installed at a partial area of ​​the support member, and the elastic member enables the support member to perform telescopic movement in its height direction.

2. The method for manufacturing a packaging structure according to claim 1, characterized in that: The lower test chip is formed between the test substrate and the upper test chip to form a test package structure, which specifically includes: Flip-chip soldering the functional surface of the lower test chip to the upper surface of the test substrate through solder balls; The functional surface of the upper test chip is flip-chip soldered to the upper surface of the lower test chip through solder balls.

3. The method for manufacturing a packaging structure according to claim 2, characterized in that: Testing the welding performance between the upper test chip and the lower test chip in the packaging structure after the reflow process specifically includes: Testing the electrical conductivity between the upper test chip and the lower test chip; The welding quality of the solder balls is detected using X-Ray technology.

4. The method for manufacturing a packaging structure according to claim 3, characterized in that: Provide a product packaging structure that is identical to the test packaging structure, specifically including: Providing a substrate identical to the test substrate and a stacked chipset identical to the test stacked chipset, the stacked chipset comprising at least an upper chip identical to the upper test chip and a lower chip identical to the lower test chip; The lower chip is formed between the substrate and the upper chip to form a product packaging structure.

5. The method for manufacturing a packaging structure according to claim 4, characterized in that: The product packaging structure is fixedly placed on the base, specifically comprising: The device also includes a substrate fixing member, and the substrate fixing member is placed above the base; The substrate is fixedly clamped in the substrate fixing member.

6. The method for manufacturing a packaging structure according to claim 5, characterized in that: Placing the support members on both sides of the product packaging structure respectively, and covering the cover plate on the upper surface of the product packaging structure and placing it on the support members, specifically including: The support members placed on one side of the substrate include a group of first support members and two groups of second support members, the first support members are placed on opposite sides of the cover plate along the length direction, and the two groups of second support members are placed on opposite sides of the cover plate along the width direction, and the first support members and the second support members placed on the same side of the substrate form a triangular structure on a plane; The cover plate is covered on the upper surface of the upper chip and is simultaneously mounted on the first support member and the second support member.

7. The method for manufacturing a packaging structure according to claim 6, characterized in that: The production method further comprises: A step is formed at the top of the first support member and the second support member, which is recessed inward toward one side of the cover plate. The height of the upper surface of the step is consistent with the height of the upper surface of the upper chip. The cover plate is placed on the upper surfaces of the steps of the first support member and the second support member at both ends in its length direction. The cover plate is fixedly clamped in the steps of the first support member and the second support member.

8. A chip anti-warping device, characterized in that: The chip anti-warping device comprises a base and at least two supporting members arranged on the base, wherein the base is used to place a substrate and a stacked chipset arranged on the substrate, wherein the stacked chipset comprises at least an upper chip and a lower chip, wherein the lower chip is arranged between the substrate and the upper chip, and the supporting members are respectively arranged on both sides of the substrate; The device also includes a cover plate, which is covered on the upper surface of the upper chip and mounted on the support member; an elastic member is provided in a partial area of ​​the support member, and the elastic member enables the support member to perform telescopic movement in its height direction.

9. The chip anti-warping device according to claim 8, characterized in that: The support members arranged on both sides of the substrate include a first support member and a second support member, wherein the first support member is arranged on opposite sides of the cover plate along the length direction, and the second support member is arranged on opposite sides of the cover plate along the width direction.

10. The chip anti-warping device according to claim 9, characterized in that: The support members arranged on one side of the substrate include a group of first support members and two groups of second support members, the two groups of second support members are respectively arranged on opposite sides of the cover plate along the width direction, and the first support members and the second support members located on the same side of the substrate form a triangular structure on the plane.

11. The chip anti-warping device according to claim 10, characterized in that: The tops of the first support member and the second support member are recessed inward toward one side of the substrate to form a step, and the height of the upper surface of the step is consistent with the height of the upper surface of the upper chip. The cover plate is simultaneously mounted on the upper surfaces of the steps of the first support member and the second support member at both ends in its length direction, and the cover plate is fixedly clamped in the steps of the first support member and the second support member.

12. The chip anti-warping device according to claim 11, characterized in that: The functional surface of the lower chip is flip-chip welded to the upper surface of the substrate through solder balls, and the functional surface of the upper chip is flip-chip welded to the upper surface of the lower chip through solder balls.

13. The chip anti-warping device according to claim 12, characterized in that: The device also includes a substrate fixing member, which is arranged above the base, and the substrate is fixedly clamped in the substrate fixing member.

14. The chip anti-warping device according to claim 13, characterized in that: The top end height of the substrate fixing member is lower than the upper surface height of the step.