A method for manufacturing fine inner-layer circuits of a hard circuit board with blind buried holes
By using RTF copper foil and laser direct imaging exposure technology, the production path is adjusted, and the problem that the existing technology cannot produce 36.8/36.8um fine lines is solved, and the stable production of high-density interconnected PCBs and the satisfaction of copper thickness requirements is achieved, reducing the need for stable production of high-density interconnected PCBs. Production difficulty and short circuit risk.
Patent Information
- Application Number
- CN202210834710.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-07-16
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2042-07-16
AI Technical Summary
The prior art cannot effectively produce 36.8/36.8um fine lines of 18/18um based copper, resulting in the inability of the inner layer lines of high-density interconnected PCBs to achieve constant and stable production, mainly due to the equipment exposure capability and material characteristics.
Use RTF inverted copper foil as raw material, use thin dry film and laser direct imaging exposure machine, and adjust the production path through micro-etching, film compression, exposure, development, electroplating and flash etching, to ensure copper thickness and line accuracy. Reduce the risk of short circuit after etching.
The copper thickness of base copper 18/18um is achieved to meet the minimum requirements specified in IPC-6012C, reducing the difficulty of fine line production, ensuring constant and stable production of high-density interconnected PCB, and avoiding short circuit problems after etching.
Smart Images

Figure CN115279058B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of circuit board production and processing, and in particular to a method for manufacturing fine inner-layer circuits of a blind buried-hole rigid circuit board. Background Art
[0002] Circuit board, also known as PCB board, circuit board, etc., plays an important role in the mass production of fixed circuits and the optimization of electrical appliance layout. It has the characteristics of high wiring density, light weight, thin thickness, good bending, and soft-hard combination board. Therefore, the soft-hard combination board is a flexible circuit board and a rigid circuit board. After pressing and other processes, they are combined together according to relevant process requirements to form a circuit board with FPC characteristics and PCB characteristics.
[0003] In real life, people have never stopped pursuing high-quality consumer electronic products, such as ultra-thin laptops, ultra-thin smart phones, smart home appliances, etc., all of which have light, thin, dense blind and buried via PCB products, and have the characteristics of high wiring density, high reliability, and complex manufacturing process. A large part of this type of PCB is used in portable electronic products. To realize the production of such blind and buried via PCB products, it is necessary to complete the process of inner layer circuit production first, and the production of fine circuits is a very important link, making the inner layer fine circuit a technology that needs to be focused on development.
[0004] At present, the production of inner fine circuits is mainly limited by the exposure capability of current equipment and the characteristics of materials, such as the influence of dry film and ink on the resolution of fine circuits or the limitation of copper thickness. If 36.8 / 36.8um fine circuits are to be produced with 18 / 18um base copper, with the current common inner circuit production process technology: inner layer pre-treatment to drying to lamination or wet film coating plus drying to exposure to static to development to acid etching to film stripping, the conventional inner layer exposure machine with 18um HTE ordinary copper foil base copper has a limit production capacity of 45um / 45um for inner layer circuits, which is impossible to produce such HDI (high density interconnect circuit board) inner fine circuits;
[0005] This conventional production process has defects: the ordinary etching solution used in the inner layer etching machine will corrode the edge of the circuit, and the side etching amount will reach: 12.5um, then the line width is too small, which has exceeded the tolerance requirement of plus or minus 20%; in addition, considering the copper thickness of the PCB substrate, the copper thickness of the PCB substrate is 18 / 18um. Because the copper thickness exceeds the energy resolution capability of the exposure machine and the resolution of the dry film, it is impossible to resolve the 36.8um fine circuit. In addition, due to the edge corrosion of the etching, it is impossible to produce the 36.8 / 36.8um fine circuit of this type of HDI (high-density interconnect PCB), and thus it is impossible to meet the constant stable production needs of high-density interconnect PCB products.
[0006] Therefore, it is necessary to provide a method for manufacturing fine inner-layer circuits of a rigid circuit board with blind buried vias to solve the above-mentioned technical problems. Summary of the invention
[0007] The present invention provides a method for manufacturing inner-layer fine circuits of a hard circuit board with blind buried holes, which solves the technical bottleneck that it is impossible to manufacture 36.8 / 36.8um fine circuits with 18 / 18um base copper according to the current conventional PCB inner-layer circuit manufacturing process technology; and also solves the problem of realizing the constant stable production demand of the inner-layer fine circuits of HDI high-density interconnection PCB.
[0008] In order to solve the above technical problems, the present invention provides a method for manufacturing fine inner-layer circuits of a rigid circuit board with blind buried vias, comprising the following steps:
[0009] S1, cutting process, and then use drying equipment to bake the plate, using RTF reverse copper foil as raw material, cutting the raw material according to production requirements, and then use drying equipment to bake the plate;
[0010] S2, pre-micro-etching treatment, the copper foil 18 / 18um surface is etched to 7-9um, and then washed and dried respectively;
[0011] S3, lamination treatment, using lamination equipment to stack the copper foil, dielectric layer, and copper foil in sequence to obtain a dry film with a thickness of 25um;
[0012] S4, exposure processing, using a laser direct imaging exposure machine to expose the dry film laminate, using a positive image pattern to expose the unnecessary circuit pattern, and then developing to reveal the circuit pattern;
[0013] S5, developing treatment, using alkali solution to wash away the dry film part on the surface of the circuit board after exposure treatment that has not undergone chemical reaction;
[0014] S6, pattern electroplating and tinning treatment, using electroplating and tinning processes to add 4um to the circuit copper thickness, so that the copper thickness of the circuit board is 13.8um, meeting the IPC-6012C requirement that the inner layer with a base copper of 18 / 18um must have a copper thickness of ≥11.4um;
[0015] S7, film stripping treatment, using a strong alkaline solution to peel off the anti-corrosion layer protecting the copper surface, so that the circuit pattern is exposed;
[0016] S8, flash etching treatment, use vacuum flash etching equipment to flash etch the circuit board, the etching edge bite amount is 1-2um, which does not affect the line accuracy of the fine line;
[0017] S9, then carry out the tin stripping and inner layer AOI scanning process on the circuit board in turn.
[0018] Preferably, in S1, in order to avoid the quality being affected by the edge baring of the board after cutting, the board needs to be ground and rounded after cutting. During the edge grinding and rounding process, the glass fiber left at the right angles of the four sides of the board when cutting is mainly removed by mechanical grinding, so as to reduce the scratches / scratches on the board surface in the subsequent production process, thereby causing quality risks.
[0019] Preferably, when baking the plate in S1, the temperature is set at 40-50° C. and the time is set at 5-7 min.
[0020] Preferably, during the exposure treatment in S4, the exposure energy is 10-30 mj and the dwell time is 5-10 min.
[0021] Preferably, during the development treatment in S5, the alkali solution used is a Na2CO3 solution, which washes away the dry film that has not undergone polymerization reaction, while the dry film that has undergone polymerization reaction is retained on the board surface as an anti-corrosion protective layer during etching.
[0022] Preferably, in S1, the drying equipment for drying the plate includes a machine body, a baffle structure is provided on the machine body, the baffle structure includes an electric telescopic rod, a movable plate, and two sliding rods, the movable plate is horizontally arranged on the machine body, and the telescopic end of the electric telescopic rod is fixedly installed on one side of the movable plate.
[0023] Preferably, the two sliding rods are fixedly installed between two sides of the inner wall of the machine body, and two sides of the outer side of the movable plate are respectively slidably connected to the outer sides of the two sliding rods.
[0024] Preferably, rectangular grooves are provided on both sides of the machine body, the electric telescopic rod is horizontally fixedly mounted on the rectangular grooves through mounting parts, and the movable plate is aligned front and back with the rectangular grooves.
[0025] Preferably, a drying box is arranged in the middle of the top of the machine body, a dryer is arranged in the middle of the bottom of the inner wall of the machine body, and the movable plate is located between the drying box and the dryer. A conveying component for driving the circuit board to move horizontally is arranged on the machine body.
[0026] Compared with the related art, the method for manufacturing fine inner-layer circuits of a hard circuit board with blind buried vias provided by the present invention has the following beneficial effects:
[0027] The present invention provides a method for manufacturing inner-layer fine circuits of a blind buried hole rigid circuit board. The present invention mainly uses RTF copper foil as a raw material, uses a thin dry film with a laser direct imaging exposure machine, and adjusts the production raw materials and technical paths respectively to ensure that after the inner-layer pattern transfer production is completed with a base copper thickness of 18 / 18um, the copper thickness of the conductor meets the minimum copper thickness requirement specified in IPC-6012C, thereby greatly reducing the production difficulty of the fine circuits, and can well meet the constant stable production requirements of such fine circuits;
[0028] When using RTF copper foil as the raw material, the copper teeth of this copper foil are small. When it is bonded to the dielectric layer, the copper teeth will partially penetrate the dielectric layer. On the one hand, it can effectively ensure the bonding strength between the copper foil and the dielectric layer. On the other hand, it can appropriately increase the line spacing between adjacent wires, thereby greatly reducing the risk of short circuits between adjacent wires after etching, which can effectively avoid the problem of short circuits after etching.
[0029] By using a thin dry film in combination with a laser direct imaging exposure machine, the resolution of fine lines transferred from the inner layer graphics is improved, and etching technology for making fine lines is realized. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 A schematic diagram of the structure inside the substrate in the method for manufacturing the inner fine circuit of the hard circuit board with blind buried holes provided by the present invention;
[0031] Figure 2 A schematic diagram of the structure of the outer portion of the substrate in the method for manufacturing the inner fine circuit of a hard circuit board with blind buried vias provided by the present invention;
[0032] Figure 3 A schematic diagram of the external structure of the drying equipment provided by the present invention;
[0033] Figure 4 for Figure 3 A cross-sectional view of the AA surface shown;
[0034] Figure 5 for Figure 3 A cross-sectional view of the BB surface shown;
[0035] Figure 6 for Figure 3 Schematic diagram of the structure of the exterior of the baffle structure shown.
[0036] Numbers in the figure
[0037] 10, copper foil, 20, dielectric layer, 30, copper teeth;
[0038] 1. Body;
[0039] 2. Baffle structure;
[0040] 21. Electric telescopic rod, 22. movable plate, 23. sliding rod;
[0041] 3. Rectangular slot;
[0042] 4. Drying box;
[0043] 5. Dryer;
[0044] 6. Transmission components. DETAILED DESCRIPTION
[0045] First embodiment
[0046] The present invention will be further described below in conjunction with the accompanying drawings and implementation modes.
[0047] Please refer to Figure 1 , Figure 2 , Figure 3 , Figure 4 Figure 5 and Figure 6 ,in, Figure 1 A schematic diagram of the structure inside the substrate in the method for manufacturing the inner fine circuit of the hard circuit board with blind buried holes provided by the present invention; Figure 2 A schematic diagram of the structure of the outer portion of the substrate in the method for manufacturing the inner fine circuit of a hard circuit board with blind buried vias provided by the present invention; Figure 3 A schematic diagram of the external structure of the drying equipment provided by the present invention; Figure 4 for Figure 3 A cross-sectional view of the AA surface shown; Figure 5 for Figure 3 A cross-sectional view of the BB surface shown; Figure 6 for Figure 3 The schematic diagram of the structure of the outer baffle structure is shown. The method for making fine circuits in the inner layer of a hard circuit board with blind buried holes includes the following steps:
[0048] S1. Cutting, and then use drying equipment to bake the board. RTF reverse copper foil is used as raw material. The raw material is cut according to production requirements, and then the board is baked using drying equipment. In order to avoid the edge of the board affecting the quality after cutting, it is necessary to grind and fillet the edges after cutting. During the grinding and filleting process, the glass fiber left at the right angles of the four sides of the board during cutting is mainly removed by mechanical grinding to reduce the scratches / scratches on the board surface during the post-production process, which may cause quality risks. When baking the board, the temperature is set at 40°C and the time is set at 5 minutes;
[0049] S2, pre-micro-etching treatment, the copper foil 18 / 18um surface copper is bitten to 7um, and then washed and dried respectively;
[0050] S3, lamination treatment, using lamination equipment to stack the copper foil, dielectric layer, and copper foil in sequence to obtain a dry film with a thickness of 25um;
[0051] S4, exposure treatment, using a laser direct imaging exposure machine to expose the dry film laminate, using a positive image pattern to expose the unnecessary circuit pattern, and then developing to expose the circuit pattern. The exposure energy during exposure is 10mj, and the dwell time is 5min;
[0052] S5, development treatment, using alkali solution to wash away the dry film part of the circuit board surface that has not undergone chemical reaction after exposure treatment. During the development treatment, the alkali solution used is Na2CO3 solution, which washes away the dry film that has not undergone polymerization reaction, while the dry film that has undergone polymerization reaction is retained on the board surface as an anti-corrosion protective layer during etching;
[0053] S6, pattern electroplating and tinning treatment, using electroplating and tinning processes to add 4um to the circuit copper thickness, so that the copper thickness of the circuit board is 13.8um, meeting the IPC-6012C requirement that the inner layer with a base copper of 18 / 18um must have a copper thickness of ≥11.4um;
[0054] S7, film stripping treatment, using a strong alkaline solution to peel off the anti-corrosion layer protecting the copper surface, so that the circuit pattern is exposed;
[0055] S8, flash etching treatment, using vacuum flash etching equipment to flash etch the circuit board;
[0056] S9, then carry out the tin stripping and inner layer AOI scanning process on the circuit board in turn.
[0057] In S1, the drying equipment for drying the plate includes a body 1, a baffle structure 2 is provided on the body 1, the baffle structure 2 includes an electric telescopic rod 21, a movable plate 22, and two sliding rods 23, the movable plate 22 is horizontally arranged on the body 1, the telescopic end of the electric telescopic rod 21 is fixedly installed on one side of the movable plate 22, the two sliding rods 23 are fixedly installed between the two sides of the inner wall of the body 1, and the two sides of the outside of the movable plate 22 are respectively slidably connected to the outside of the two sliding rods 23.
[0058] The electric telescopic rod 21 is connected to the power supply unit on the body 1, and its extension and retraction are controlled by an external switch. By connecting to the movable plate 22, the movable plate 22 can be driven to move horizontally on the body 1. The two sliding rods 23 are slidably connected to the left and right sides of the movable plate 22, which can limit the movable plate 22 and enable it to slide stably in the horizontal direction.
[0059] Rectangular grooves 3 are formed on both sides of the machine body 1 , and the electric telescopic rod 21 is horizontally fixedly mounted on the rectangular groove 3 through a mounting member, and the movable plate 22 is aligned with the rectangular groove 3 in the front and rear direction.
[0060] On the one hand, the rectangular groove 3 can serve as vents on the front and rear sides of the machine body, facilitating the rapid discharge of wind generated by the dryer 5 and the drying box 4. On the other hand, it can allow the movable plate 22 to extend from the inside of the machine body 1 to its outside, serving as an outlet for the movable plate 22.
[0061] A drying box 4 is arranged in the middle of the top of the machine body 1, a dryer 5 is arranged in the middle of the bottom of the inner wall of the machine body 1, and the movable plate 22 is located between the drying box 4 and the dryer 5. A conveying component 6 for driving the circuit board to move horizontally is arranged on the machine body 1.
[0062] The drying box 4 and the dryer 5 are symmetrically arranged up and down, and are both used to quickly dry the outside of the circuit board on the conveying component 6, so as to realize the function of drying both sides of the circuit board simultaneously, without the need to flip the circuit board. By arranging the movable plate 22 between the two, the two are mainly protected from each other. When it is necessary to dry the top and bottom of the circuit board at the same time, the drying box 4 and the dryer 5 need to be turned on at the same time. Since the two are in a relative state, the hot air generated will blow against each other, resulting in a counter-blowing situation. At this time, by setting the baffle structure 2, the two can be separated when the circuit board has not passed through the drying box 4 and the dryer 5, and then the electric The intermittent telescopic operation of the telescopic rod 21 can drive the movable plate 22 to slide horizontally on the body 1. When the circuit board passes through, the movable plate 22 is in an outwardly extended state. When the circuit board does not pass through, the movable plate 22 is in a retracted state, thereby achieving a good protection effect on the drying box 4 and the dryer 5, avoiding long-term blowing of the two and causing mutual damage. At the same time, the drying box 4, the dryer 5 and the baffle structure 2 are arranged, so that the drying equipment has the function of drying both sides of the circuit board at the same time, and can also dry one side. It is more flexible to use, and changes the existing form of flipping the circuit board by setting a flip mechanism, eliminating the flipping operation of the circuit board and reducing damage to it.
[0063] Compared with the related art, the method for manufacturing fine inner-layer circuits of a hard circuit board with blind buried vias provided by the present invention has the following beneficial effects:
[0064] The present invention mainly uses RTF copper foil as a raw material, uses a thin dry film with a laser direct imaging exposure machine, and adjusts the production raw materials and technical paths respectively to ensure that the copper thickness of the base copper is 18 / 18um after the inner layer pattern transfer is completed. The copper thickness of the conductor meets the minimum copper thickness requirement specified in IPC-6012C, thereby greatly reducing the production difficulty of fine circuits, and can well meet the constant stable production requirements of such fine circuits;
[0065] When using RTF copper foil as the raw material, the copper teeth of this copper foil are small. When it is bonded to the dielectric layer, the copper teeth will partially penetrate the dielectric layer. On the one hand, it can effectively ensure the bonding strength between the copper foil and the dielectric layer. On the other hand, it can appropriately increase the line spacing between adjacent wires, thereby greatly reducing the risk of short circuits between adjacent wires after etching, which can effectively avoid the problem of short circuits after etching.
[0066] By using a thin dry film in combination with a laser direct imaging exposure machine, the resolution of fine lines transferred from the inner layer graphics is improved, and etching technology for making fine lines is realized.
[0067] Second embodiment
[0068] Based on the first embodiment of the present invention, a method for manufacturing fine inner layer circuits of a rigid circuit board with blind buried vias, the second embodiment of the present invention provides another method for manufacturing fine inner layer circuits of a rigid circuit board with blind buried vias, wherein the second embodiment does not hinder the independent implementation of the technical solution of the first embodiment.
[0069] Specifically, the present invention provides another method for manufacturing inner fine circuits of a rigid circuit board with blind buried vias, which is different in that:
[0070] S1. Cutting, and then use drying equipment to bake the board. RTF reverse copper foil is used as raw material. The raw material is cut according to production requirements, and then the board is baked using drying equipment. In order to avoid the board edge barri affecting the quality after cutting, it is necessary to grind and fillet after cutting. During the grinding and filleting process, the glass fiber left at the right angles of the four sides of the board during cutting is mainly removed by mechanical grinding to reduce the scratches / scratches on the board surface during the post-production process, causing quality risks. When baking the board, the temperature is set at 45℃ and the time is set at 6min.
[0071] S2, pre-micro-etching treatment, the copper foil 18 / 18um surface copper is bitten to 8um, and then washed and dried respectively;
[0072] S3, lamination treatment, using lamination equipment to stack the copper foil, dielectric layer, and copper foil in sequence to obtain a dry film with a thickness of 25um;
[0073] S4, exposure treatment, using a laser direct imaging exposure machine to expose the dry film laminate, using a positive image pattern to expose the unnecessary circuit pattern, and then developing to expose the circuit pattern. The exposure energy during exposure is 20mj, and the dwell time is 7min;
[0074] S5, development treatment, using alkali solution to wash away the dry film part of the circuit board surface that has not undergone chemical reaction after exposure treatment. During the development treatment, the alkali solution used is Na2CO3 solution, which washes away the dry film that has not undergone polymerization reaction, while the dry film that has undergone polymerization reaction is retained on the board surface as an anti-corrosion protective layer during etching;
[0075] S6, pattern electroplating and tinning treatment, using electroplating and tinning processes to add 4um to the circuit copper thickness, so that the copper thickness of the circuit board is 13.8um, meeting the IPC-6012C requirement that the inner layer with a base copper of 18 / 18um must have a copper thickness of ≥11.4um;
[0076] S7, film stripping treatment, using a strong alkaline solution to peel off the anti-corrosion layer protecting the copper surface, so that the circuit pattern is exposed;
[0077] S8, flash etching treatment, using vacuum flash etching equipment to flash etch the circuit board;
[0078] S9, then carry out the tin stripping and inner layer AOI scanning process on the circuit board in turn.
[0079] Third embodiment
[0080] Based on the first embodiment of the present invention, a method for manufacturing fine inner layer circuits of a rigid circuit board with blind buried vias, the third embodiment of the present invention provides another method for manufacturing fine inner layer circuits of a rigid circuit board with blind buried vias, wherein the third embodiment does not hinder the independent implementation of the technical solution of the first embodiment.
[0081] Specifically, the present invention provides another method for manufacturing inner fine circuits of a rigid circuit board with blind buried vias, which is different in that:
[0082] S1. Cutting, and then use drying equipment to bake the board. RTF reverse copper foil is used as raw material. The raw material is cut according to production requirements, and then the board is baked using drying equipment. In order to avoid the board edge barri affecting the quality after cutting, it is necessary to grind and fillet the edges after cutting. During the grinding and filleting process, the glass fiber left at the right angles of the four sides of the board during cutting is mainly removed by mechanical grinding to reduce the scratches / scratches on the board surface during the post-production process, which may cause quality risks. When baking the board, the temperature is set at 50℃ and the time is set at 7min.
[0083] S2. Pre-micro-etching treatment: 18 / 18um copper foil surface is etched to 9um by immersion micro-etching solution. The difference of PCB surface copper distribution uniformity can be + / -1um. The thinner base copper thickness improves the resolution and resolution of the exposure machine, and can achieve 36.8um fine circuit production. After the copper is bitten, it is washed and dried respectively.
[0084] S3, lamination treatment, using lamination equipment to stack the copper foil, dielectric layer, and copper foil in sequence to obtain a dry film with a thickness of 25um;
[0085] S4, exposure treatment, using a laser direct imaging exposure machine to expose the dry film laminate, using a positive image pattern to expose the unnecessary circuit pattern, and then developing to expose the circuit pattern. The exposure energy during exposure is 30mj, and the dwell time is 10min;
[0086] S5, development treatment, using alkali solution to wash away the dry film part of the circuit board surface that has not undergone chemical reaction after exposure treatment. During the development treatment, the alkali solution used is Na2CO3 solution, which washes away the dry film that has not undergone polymerization reaction, while the dry film that has undergone polymerization reaction is retained on the board surface as an anti-corrosion protective layer during etching;
[0087] S6, pattern electroplating and tinning treatment, using electroplating and tinning processes to add 4um to the circuit copper thickness, so that the copper thickness of the circuit board is 13.8um, meeting the IPC-6012C quality requirements of the PCB industry that the inner layer of the base copper is 18 / 18um and the finished copper thickness must reach ≥11.4um;
[0088] S7, film stripping treatment, using a strong alkaline solution to peel off the anti-corrosion layer protecting the copper surface, so that the circuit pattern is exposed;
[0089] S8, flash etching treatment, using vacuum flash etching equipment to flash etch the circuit board;
[0090] S9, then carry out the tin stripping and inner layer AOI scanning process on the circuit board in turn.
[0091] The above descriptions are merely embodiments of the present invention and are not intended to limit the patent scope of the present invention. Any equivalent structure or equivalent process transformation made using the contents of the present invention specification and drawings, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present invention.
Claims
1. A method for manufacturing fine inner-layer circuits of a blind buried hole rigid circuit board, characterized in that: The steps include: S1, cutting process, and then use drying equipment to bake the plate, using RTF reverse copper foil as raw material, cutting the raw material according to production requirements, and then use drying equipment to bake the plate; S2, pre-micro-etching treatment, the copper foil 18 / 18um surface is etched to 7-9um, and then washed and dried respectively; S3, lamination treatment, using lamination equipment to stack the copper foil, dielectric layer, and copper foil in sequence to obtain a dry film with a thickness of 25um; S4, exposure processing, using a laser direct imaging exposure machine to expose the dry film laminate, using a positive image pattern to expose the unnecessary circuit pattern, and then developing to reveal the circuit pattern; S5, developing treatment, using alkali solution to wash away the dry film part on the surface of the circuit board after exposure treatment that has not undergone chemical reaction; S6, pattern electroplating and tinning treatment, using electroplating and tinning processes to add 4um to the circuit copper thickness, so that the copper thickness of the circuit board is 13.8um, meeting the IPC-6012C requirement that the inner layer with a base copper of 18 / 18um must have a copper thickness of ≥11.4um; S7, film stripping treatment, using a strong alkaline solution to peel off the anti-corrosion layer protecting the copper surface, so that the circuit pattern is exposed; S8, flash etching treatment, use vacuum flash etching equipment to flash etch the circuit board, the etching edge bite amount is 1-2um, which does not affect the line accuracy of the fine line; S9, then the circuit board is subjected to tin stripping and inner layer AOI scanning process treatments in sequence. In S1, the drying equipment for drying the plate comprises a body, a baffle structure is arranged on the body, the baffle structure comprises an electric telescopic rod, a movable plate, and two sliding rods, the movable plate is horizontally arranged on the body, the telescopic end of the electric telescopic rod is fixedly installed on one side of the movable plate, the two sliding rods are fixedly installed between the two sides of the inner wall of the body, the two sides of the outer side of the movable plate are respectively slidably connected with the outer sides of the two sliding rods, rectangular grooves are provided on both sides of the body, the electric telescopic rod is horizontally fixedly installed on the rectangular groove by a mounting piece, the movable plate and the rectangular groove are kept aligned front and back, a drying box is arranged in the middle of the top of the body, a dryer is arranged in the middle of the bottom of the inner wall of the body, and the movable plate is located between the drying box and the dryer, and a conveying component for driving the circuit board to move horizontally is arranged on the body.
2. The method for manufacturing inner fine circuits of a hard circuit board with blind buried vias according to claim 1, characterized in that: In S1, in order to avoid the quality of the board after cutting due to barri, it is necessary to grind and fillet the edges after cutting. During the grinding and filleting process, the glass fiber left at the right angles of the four sides of the board when cutting is mainly removed by mechanical grinding, so as to reduce the scratches / scratches on the board surface in the subsequent production process, causing quality risks.
3. The method for manufacturing inner fine circuits of a hard circuit board with blind buried vias according to claim 1, characterized in that: When the baking plate is baked in S1, the temperature is set at 40-50°C and the time is set at 5-7 minutes.
4. The method for manufacturing inner fine circuits of a hard circuit board with blind buried vias according to claim 1, characterized in that: During the exposure treatment in S4, the exposure energy is 10-30 mj and the dwell time is 5-10 min.
5. The method for manufacturing inner fine circuits of a hard circuit board with blind buried vias according to claim 1, characterized in that: During the development treatment in S5, the alkali solution used is a Na2CO3 solution, which washes away the dry film that has not undergone polymerization reaction, while the dry film that has undergone polymerization reaction is retained on the board surface as an anti-corrosion protective layer during etching.
6. The method for manufacturing inner fine circuits of a hard circuit board with blind buried vias according to claim 1, characterized in that: In the S6, when electroplating the circuit board, a new type of electroplating solution additive is used, which contains a diallylamine polymer, and is used to suppress the current distribution between the dry film and the copper, so that the components of the inorganic plating solution are not easily diffused between the fine lines, thereby improving the uniformity of electroplating.