Device and method for preparing 1,5-pentanediisocyanate by non-phosgene method

Through simplified non-phosgene device and method, the pyrolysis reactor and protective gas purging technology are used to solve the problems of low yield and safety hazards of phosgene, and the efficient and environmentally friendly 1,5-Pulmonary 1,5-Pulmonary 2 is achieved. Isocyanate preparation improves yield and avoids the use of highly toxic substances.

CN115350660BActive Publication Date: 2024-11-12INSTITUTE OF PROCESS ENGINEERING CHINESE ACADEMY OF SCIENCES
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210792820.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-07-05
Publication Date
2024-11-12
Estimated Expiration
2042-07-05

AI Technical Summary

Technical Problem

In the prior art, the yield of phosgene preparation of 1,5-pentadiisocyanate is low and the use of highly toxic raw materials has poses a safety hazard. The industrial application of non-phosgene method has not yet been realized, and the yield of pyrolysis method is Only 65%-75%.

Method used

Provided is an apparatus and method for preparing 1,5-pentadiisocyanate for non-phosgene method, including feed unit, reaction unit, condensation unit and cooling unit, reacting through a pyrolysis reactor, purging and catalyst using protective gas , control reaction temperature and pressure to achieve efficient preparation.

Benefits of technology

PDI is prepared efficiently and stably geothermal decomposition under lower temperature pressure, which improves the yield to more than 76.8%, up to 99.2%, and is green and environmentally friendly, and does not use highly toxic substances.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115350660B_ABST
    Figure CN115350660B_ABST
Patent Text Reader

Abstract

The invention provides a device and method for preparing 1,5-pentane diisocyanate by a non-phosgene method. The device consists of a feeding unit, a reaction unit, a condensing unit, a collecting unit and a cooling unit; the feeding unit, the reaction unit, the condensing unit and the collecting unit are connected in sequence; the reaction unit is also connected to the cooling unit; the method passes a raw material into the reaction unit, performs pyrolysis under a protective atmosphere, refluxes a part of the obtained light components after condensation, and collects the other part after condensation, so as to obtain a 1,5-pentane diisocyanate product; the device structure of the invention is simple, the method conditions are mild, the yield of 1,5-pentane diisocyanate can be effectively improved, and there is no highly toxic reagent, it is green and environmentally friendly, and has good industrial application prospects.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of non-phosgene synthesis of isocyanate, and specifically relates to a device and method for preparing 1,5-pentane diisocyanate by a non-phosgene method. Background Art

[0002] Cyanate esters are the main raw materials for the production of polyurethane and are widely used in industries such as elastomers, coatings, plastics, pesticides and leather.

[0003] At present, there are mainly phosgene method and non-phosgene method for synthesizing isocyanate, and phosgene method is the mainstream process for industrial preparation of isocyanate. CN112457217A is a method for preparing 1,5-pentanediisocyanate (PDI), the steps of which are: using o-dichlorobenzene as solvent and trimethylsilyl chloride as catalyst, 1,5-pentanediamine and phosgene react at 15℃-30℃ and normal pressure to generate diaminoformyl chloride; after the reaction is completed, the reaction material is heated to 110℃120℃, a small amount of solvent and all catalysts are evaporated for recycling; a certain amount of phosgene is continuously introduced into diaminoformyl chloride, the temperature is raised to 150℃-170℃, and a thermal photochemical reaction occurs until the material is clear and transparent; after the photochemical reaction is completed, the solvent is removed by vacuum distillation, and 1,5-pentanediisocyanate product can be obtained by continuing vacuum distillation. The yield of PDI using this method is only 84%-85%, and the raw material phosgene in this process is a highly toxic raw material, which poses a major safety hazard.

[0004] The research progress report on non-phosgene method is as follows: Monsanto has developed a process route for producing MDI using aniline and carbon dioxide as raw materials. This method finally synthesizes MDI through N-phenylcarbamate methyl ester and MDU, but it has not been industrialized.

[0005] CN108689884A discloses a method for preparing 1,5-pentanediisocyanate, comprising: (1) extracting 1,5-pentanediamine by mixing a 1,5-pentanediamine conversion solution and an extraction solvent, and then dehydrating the extraction solution to obtain a mixture of 1,5-pentanediamine and the extraction solvent; (2) adding a catalyst and urea to the mixture of 1,5-pentanediamine and the extraction solvent, supplementing an appropriate amount of the extraction solvent to form a reaction system, esterifying 1,5-pentanediamine and recovering the excess extraction solvent in the reaction system by reduced pressure distillation to obtain PDU; (3) mixing PDU with a heat carrier and a catalyst for a thermal cracking reaction, and separating to obtain the extraction solvent and PDI. However, the yield of PDI obtained by the thermal decomposition method is only 65%-75%.

[0006] In summary, it is of great significance to provide a method with mild production conditions, simple equipment and the ability to effectively improve the PDI yield. Summary of the invention

[0007] In view of the problems existing in the prior art, the object of the present invention is to provide a device and method for preparing 1,5-pentanediisocyanate by a non-phosgene method. The device has a simple structure, and the method has mild conditions. PDI can be prepared by pyrolysis efficiently. The process flow is environmentally friendly and is conducive to industrial production.

[0008] To achieve this object, the present invention adopts the following technical solutions:

[0009] In a first aspect, the present invention provides a device for preparing 1,5-pentanediisocyanate by a non-phosgene method, the device comprising a feeding unit, a reaction unit, a condensation unit, a collection unit and a cooling unit;

[0010] The feeding unit, the reaction unit, the condensation unit and the collection unit are connected in sequence;

[0011] The reaction unit is also connected to the cooling unit.

[0012] In the present invention, the device greatly simplifies the equipment required for the reaction, and the preparation of 1,5-pentanediisocyanate can be achieved only through a feeding unit, a reaction unit, a condensation unit and a collection unit, and the product yield can be effectively improved; the cooling unit can process the reaction liquid after the reaction to achieve reasonable utilization.

[0013] The following are preferred technical solutions of the present invention, but are not intended to be limitations of the technical solutions provided by the present invention. Through the following technical solutions, the technical objectives and beneficial effects of the present invention can be better achieved and realized.

[0014] As a preferred technical solution of the present invention, the feeding unit includes a raw material feeding pipe and a protective gas purge pipe.

[0015] Preferably, the protective gas purge pipe is inserted into the lower middle part of the reactor.

[0016] As a preferred technical solution of the present invention, the reaction unit includes a pyrolysis reactor.

[0017] Preferably, the top of the pyrolysis reactor is connected to the condensation unit via a steam outlet pipe and a condensation reflux pipe, respectively.

[0018] As a preferred technical solution of the present invention, the condensing unit includes a condenser.

[0019] Preferably, the top of the condenser is connected to the collection unit via a non-condensable gas extraction pipe.

[0020] As a preferred technical solution of the present invention, the collection unit includes a collection tank.

[0021] Preferably, a protective gas exhaust pipe is connected to the top of the collection tank.

[0022] As a preferred technical solution of the present invention, the bottom of the reaction unit is connected to the cooling unit;

[0023] Preferably, the cooling unit comprises a cooler.

[0024] In a second aspect, the present invention provides a method for preparing 1,5-pentanediisocyanate using the device described in the first aspect, the method comprising the following steps:

[0025] The 1,5-pentanedicarbamate solution, solvent and catalyst are introduced into the reaction unit to react under a protective atmosphere, and the obtained light components enter the condensation unit, and a part of the light components are returned to the reaction unit after condensation; the other part of the light components are condensed and enter the collection unit to obtain 1,5-pentanediisocyanate;

[0026] After the reaction, the reaction liquid in the reaction unit is collected after being cooled.

[0027] As a preferred technical solution of the present invention, the 1,5-pentanediaminocarbamate includes any one of 1,5-pentanediaminocarbamate methyl ester, 1,5-pentanediaminocarbamate ethyl ester, 1,5-pentanediaminocarbamate propyl ester or 1,5-pentanediaminocarbamate butyl ester, or a combination of at least two of them. Typical but non-limiting examples of the combination include: a combination of 1,5-pentanediaminocarbamate methyl ester and 1,5-pentanediaminocarbamate ethyl ester, a combination of 1,5-pentanediaminocarbamate methyl ester and 1,5-pentanediaminocarbamate ethyl ester, a combination of 1,5-pentanediaminocarbamate propyl ester and 1,5-pentanediaminocarbamate butyl ester, and the like.

[0028] Preferably, the solvent comprises one or a combination of two or more of alkanes, halogenated alkanes, benzene, toluene, xylene, chlorobenzene, o-dichlorobenzene, p-dichlorobenzene, monochlorobiphenyl, diphenylmethane, dialkyl terephthalate, diethyl phthalate, cyclohexane oil, decalin, etc. Typical but non-limiting examples of the combination include: a combination of benzene and toluene, a combination of o-dichlorobenzene, p-dichlorobenzene and monochlorobiphenyl, a combination of alkanes and halogenated alkanes, etc., wherein the alkanes include straight-chain alkanes and / or cycloalkanes.

[0029] In the present invention, the catalyst includes metal, metal oxide or organic matter.

[0030] Among them, the metal includes any one of iron, chromium, manganese, aluminum, magnesium, barium, copper, lead, zinc, tin, cobalt, nickel, antimony, cadmium, bismuth, gold, silver, platinum, ruthenium, rhodium, palladium, osmium, iridium, beryllium, titanium, zirconium, hafnium, vanadium, niobium, tantalum, tungsten, molybdenum, rhenium, lanthanum or cerium; the metal oxide is the oxide corresponding to the above metals.

[0031] Preferably, the mass ratio of the catalyst to the 1,5-pentanedicarbamate is 1:(10-200), such as 1:10, 1:20, 1:50, 1:80, 1:100, 1:150 or 1:200, etc., but is not limited to the listed values. Other unlisted values ​​within the numerical range are also applicable, preferably 1:(50-100).

[0032] Preferably, the concentration of the 1,5-pentanedicarbamate solution is 2-50wt%, for example 2wt%, 5wt%, 8wt%, 10wt%, 20wt%, 30wt%, 40wt% or 50wt%, etc., but is not limited to the listed values, and other unlisted values ​​within the numerical range are also applicable, preferably 2-15wt%, and more preferably 2-10wt%.

[0033] As a preferred technical solution of the present invention, the reaction temperature is 160-350°C, for example, 160°C, 180°C, 200°C, 250°C, 300°C or 350°C, but is not limited to the listed values. Other unlisted values ​​within the numerical range are also applicable, preferably 210-280°C.

[0034] Preferably, the reaction pressure is 0.1-3.0 MPa, such as 0.1 MPa, 0.5 MPa, 1.0 MPa, 1.5 MPa, 2.0 MPa, 2.5 MPa or 3.0 MPa, but is not limited to the listed values. Other unlisted values ​​within the numerical range are also applicable, preferably 0.3-0.8 MPa.

[0035] Preferably, the reaction time is 60-360 min, for example 60 min, 90 min, 120 min, 150 min, 180 min, 210 min, 240 min, 270 min, 300 min, 330 min or 360 min, but is not limited to the listed values, and other unlisted values ​​within the numerical range are also applicable, preferably 240-300 min.

[0036] As a preferred technical solution of the present invention, the temperature of the reaction solution after cooling is 20-150°C, for example, 20°C, 40°C, 60°C, 80°C, 100°C, 120°C or 150°C, but is not limited to the listed values, and other unlisted values ​​within the numerical range are also applicable, preferably 30-50°C.

[0037] Compared with the prior art, the present invention has the following beneficial effects:

[0038] (1) The device of the present invention has a simple structure and can efficiently and stably prepare PDI by pyrolysis at a relatively low temperature and pressure. The yield of PDI can be increased to more than 76.8%. By further controlling the concentration of the 1,5-pentanedicarbamate solution, the yield of PDI can reach more than 90.0%, and the highest can reach 99.2%;

[0039] (2) The method of the present invention does not use any highly toxic substances during the preparation process, and is green and environmentally friendly. BRIEF DESCRIPTION OF THE DRAWINGS

[0040] Figure 1 The invention discloses a device for preparing 1,5-pentanediisocyanate by a non-phosgene method.

[0041] Among them, 1-feeding unit, 11-raw material feeding pipe, 12-protective gas purge pipe, 2-reaction unit, 21-steam outlet pipe, 3-condensation unit, 31-condensation reflux pipe, 32-non-condensable gas extraction pipe, 4-collection unit, 41-protective gas exhaust pipe, 5-cooling unit. DETAILED DESCRIPTION

[0042] In order to better illustrate the present invention and facilitate understanding of the technical solution of the present invention, the present invention is further described in detail below. However, the following embodiments are only simple examples of the present invention and do not represent or limit the scope of protection of the present invention. The scope of protection of the present invention shall be subject to the claims.

[0043] In a specific embodiment, the present invention provides a device for preparing 1,5-pentanediisocyanate by a non-phosgene method, the structural schematic diagram of the device is as follows: Figure 1 As shown;

[0044] The device is composed of a feeding unit 1, a reaction unit 2, a condensation unit 3, a collection unit 4 and a cooling unit 5;

[0045] The feed unit 1, the reaction unit 2, the condensation unit 3 and the collection unit 4 are connected in sequence;

[0046] The reaction unit 2 is also connected to the cooling unit 5 .

[0047] Furthermore, the feeding unit 1 comprises a raw material feeding pipe 11 and a protective gas purge pipe 12; the protective gas purge pipe 12 is inserted into the middle and lower part of the reactor.

[0048] Furthermore, the reaction unit 2 comprises a pyrolysis reactor; preferably, the top of the pyrolysis reactor is connected to the condensation unit 3 via a steam outlet pipe 21 and a condensation reflux pipe 31 respectively.

[0049] Furthermore, the condensing unit 3 includes a condenser; the top of the condenser is connected to the collecting unit 4 via a non-condensable gas extraction pipe 32.

[0050] Furthermore, the collecting unit 4 comprises a collecting tank; a protective gas exhaust pipe 41 is connected to the top of the collecting tank.

[0051] Furthermore, the bottom of the reaction unit 2 is connected to the cooling unit 5; the cooling unit 5 includes a cooler.

[0052] The following are typical but non-limiting embodiments of the present invention:

[0053] Embodiment 1:

[0054] This embodiment provides a device and method for preparing 1,5-pentane diisocyanate by a non-phosgene method, and the device is the same as the device in the specific embodiment.

[0055] The method is carried out using the above-mentioned device, and the method comprises:

[0056] A 2 wt % 1,5-pentanedicarbamate solution, o-dichlorobenzene and magnesium oxide (the mass ratio of magnesium oxide to 1,5-pentanedicarbamate is 1:100) are introduced into a pyrolysis reactor, and nitrogen is introduced for purging. The reaction is carried out at 265±5° C. and 0.5 MPa for 300 min. The obtained light components enter a condenser, and a part of the light components is returned to the pyrolysis reactor after condensation; the other part of the light components enters a collecting tank after condensation to obtain 1,5-pentanediisocyanate, and the nitrogen is discharged from the protective gas exhaust pipe 41;

[0057] After the reaction, the reaction liquid in the pyrolysis reaction kettle enters the cooler for cooling, and is collected after being cooled to 30° C. for standby use.

[0058] Embodiment 2:

[0059] This embodiment provides a device and method for preparing 1,5-pentane diisocyanate by a non-phosgene method, and the device is the same as the device in the specific embodiment.

[0060] The method is carried out using the above-mentioned device, and the method comprises:

[0061] A 2 wt % 1,5-pentanedicarbamate solution, o-dichlorobenzene and magnesium oxide (the mass ratio of magnesium oxide to 1,5-pentanedicarbamate is 1:50) are introduced into a pyrolysis reactor, and nitrogen is introduced for purging. The reaction is carried out at 265±5° C. and 0.6 MPa for 300 min. The obtained light components enter a condenser, and a part of the light components is returned to the pyrolysis reactor after condensation; the other part of the light components enters a collecting tank after condensation to obtain 1,5-pentanediisocyanate, and the nitrogen is discharged from the protective gas exhaust pipe 41;

[0062] After the reaction, the reaction liquid in the pyrolysis reaction kettle enters the cooler for cooling, and is collected after being cooled to 50° C. for standby use.

[0063] Embodiment 3:

[0064] This embodiment provides a device and method for preparing 1,5-pentane diisocyanate by a non-phosgene method, and the device is the same as the device in the specific embodiment.

[0065] The method is similar to that in Example 1, except that the concentration of the 1,5-pentanedicarbamate solution is 5 wt %.

[0066] Embodiment 4:

[0067] This embodiment provides a device and method for preparing 1,5-pentane diisocyanate by a non-phosgene method, and the device is the same as the device in the specific embodiment.

[0068] The method is similar to that in Example 1, except that the concentration of the 1,5-pentanedicarbamate solution is 8 wt %.

[0069] Embodiment 5:

[0070] This embodiment provides a device and method for preparing 1,5-pentane diisocyanate by a non-phosgene method, and the device is the same as the device in the specific embodiment.

[0071] The method is similar to that in Example 1, except that the concentration of the 1,5-pentanedicarbamate solution is 10 wt %.

[0072] Embodiment 6:

[0073] This embodiment provides a device and method for preparing 1,5-pentane diisocyanate by a non-phosgene method, and the device is the same as the device in the specific embodiment.

[0074] The method is similar to that in Example 1, except that the concentration of the 1,5-pentanedicarbamate solution is 15 wt %.

[0075] Embodiment 7:

[0076] This embodiment provides a device and method for preparing 1,5-pentane diisocyanate by a non-phosgene method, and the device is the same as the device in the specific embodiment.

[0077] The method is similar to that in Example 1, except that the reaction temperature is 165±10°C.

[0078] The yield of the product PDI was measured after the reaction for 300 min. The results are shown in Table 1.

[0079] Table 1

[0080]

[0081]

[0082] It can be seen from the above embodiments that the device of the present invention has a simple structure and can prepare PDI by pyrolysis efficiently and stably at a relatively low temperature and pressure. At the same time, the yield of PDI can be increased to more than 76.8%, and by further controlling the concentration of the 1,5-pentanedicarbamate solution, the yield of PDI can reach more than 90.0%, and up to 99.2%; the method does not use highly toxic substances in the preparation process, and is green and environmentally friendly.

[0083] The present invention illustrates the device and detailed method of the present invention through the above embodiments, but the present invention is not limited to the above devices and detailed methods, that is, it does not mean that the present invention must rely on the above devices and detailed methods to be implemented. Those skilled in the art should understand that any improvement of the present invention, equivalent replacement of the operation of the present invention, addition of auxiliary operations, selection of specific methods, etc., all fall within the protection scope and disclosure scope of the present invention.

Claims

1. A device for preparing 1,5-pentanediisocyanate by a non-phosgene method, It is characterized in that The device consists of a feeding unit, a reaction unit, a condensation unit, a collection unit and a cooling unit; The feeding unit, the reaction unit, the condensation unit and the collection unit are connected in sequence; The reaction unit is also connected to the cooling unit; The method for preparing 1,5-pentanediisocyanate using the device comprises the following steps: The 1,5-pentanedicarbamate solution, solvent and catalyst are introduced into the reaction unit to react under a protective atmosphere, and the obtained light components enter the condensation unit, and a part of the light components are returned to the reaction unit after condensation; the other part of the light components are condensed and enter the collection unit to obtain 1,5-pentanediisocyanate; After the reaction, the reaction liquid in the reaction unit is collected after being cooled.

2. The device for preparing 1,5-pentanediisocyanate by a non-phosgene method according to claim 1, It is characterized in that The feeding unit comprises a raw material feeding pipe and a protective gas purge pipe.

3. The device for preparing 1,5-pentanediisocyanate by non-phosgene method according to claim 2, It is characterized in that The protective gas purge pipe is inserted into the middle and lower part of the reactor.

4. The device for preparing 1,5-pentanediisocyanate by a non-phosgene method according to claim 1, It is characterized in that The reaction unit comprises a pyrolysis reactor.

5. The device for preparing 1,5-pentanediisocyanate by non-phosgene method according to claim 4, It is characterized in that The top of the pyrolysis reactor is connected to the condensation unit through a steam outlet pipe and a condensation reflux pipe respectively.

6. The device for preparing 1,5-pentanediisocyanate by non-phosgene method according to claim 1, It is characterized in that The condensing unit includes a condenser.

7. The device for preparing 1,5-pentanediisocyanate by non-phosgene method according to claim 6, It is characterized in that The top of the condenser is connected to the collection unit through a non-condensable gas extraction pipe.

8. The device for preparing 1,5-pentanediisocyanate by a non-phosgene method according to claim 1, It is characterized in that The collecting unit includes a collecting tank.

9. The device for preparing 1,5-pentanediisocyanate by non-phosgene method according to claim 8, It is characterized in that The top of the collecting tank is connected with a protective gas exhaust pipe.

10. The device for preparing 1,5-pentanediisocyanate by non-phosgene method according to claim 1, It is characterized in that The bottom of the reaction unit is connected to the cooling unit.

11. The device for preparing 1,5-pentanediisocyanate by a non-phosgene method according to claim 1, It is characterized in that The cooling unit includes a cooler.

12. A method for preparing 1,5-pentanediisocyanate by a non-phosgene method, It is characterized in that The method is carried out using the device according to any one of claims 1 to 11, and the method comprises the following steps: The 1,5-pentanedicarbamate solution, solvent and catalyst are introduced into the reaction unit to react under a protective atmosphere, and the obtained light components enter the condensation unit, and a part of the light components are returned to the reaction unit after condensation; the other part of the light components are condensed and enter the collection unit to obtain 1,5-pentanediisocyanate; After the reaction, the reaction liquid in the reaction unit is collected after being cooled.

13. The method for preparing 1,5-pentanediisocyanate by a non-phosgene method according to claim 12, It is characterized in that The 1,5-pentanedicarbamate includes any one of 1,5-pentanedicarbamate methyl ester, 1,5-pentanedicarbamate ethyl ester, 1,5-pentanedicarbamate propyl ester or 1,5-pentanedicarbamate butyl ester, or a combination of at least two thereof.

14. The method for preparing 1,5-pentanediisocyanate by a non-phosgene method according to claim 12, It is characterized in that The solvent includes any one of alkanes, halogenated alkanes, benzene, toluene, xylene, chlorobenzene, o-dichlorobenzene, p-dichlorobenzene, monochlorobiphenyl, diphenylmethane, dialkyl terephthalate, diethyl phthalate, cyclohexane oil, and decalin, or a combination of two or more thereof.

15. The method for preparing 1,5-pentanediisocyanate by a non-phosgene method according to claim 12, It is characterized in that The mass ratio of the catalyst to the 1,5-pentanedicarbamate is 1:(10-200).

16. The method for preparing 1,5-pentanediisocyanate by a non-phosgene method according to claim 15, It is characterized in that The mass ratio of the catalyst to the 1,5-pentanedicarbamate is 1:(50-100).

17. The method for preparing 1,5-pentanediisocyanate by a non-phosgene method according to claim 12, It is characterized in that The concentration of the 1,5-pentanedicarbamate solution is 2-50 wt %.

18. The method for preparing 1,5-pentanediisocyanate by a non-phosgene method according to claim 17, It is characterized in that The concentration of the 1,5-pentanedicarbamate solution is 2-15 wt %.

19. The method for preparing 1,5-pentanediisocyanate by a non-phosgene method according to claim 18, It is characterized in that The concentration of the 1,5-pentanedicarbamate solution is 2-10 wt %.

20. The method for preparing 1,5-pentanediisocyanate by a non-phosgene method according to claim 12, It is characterized in that The reaction temperature is 160-350°C.

21. The method for preparing 1,5-pentanediisocyanate by a non-phosgene method according to claim 20, It is characterized in that The reaction temperature is 210-280°C.

22. The method for preparing 1,5-pentanediisocyanate by a non-phosgene method according to claim 12, It is characterized in that The reaction pressure is 0.1-3.0 MPa.

23. The method for preparing 1,5-pentanediisocyanate by a non-phosgene method according to claim 22, It is characterized in that The reaction pressure is 0.3-0.8 MPa.

24. The method for preparing 1,5-pentanediisocyanate by a non-phosgene method according to claim 12, It is characterized in that The reaction time is 60-360 min.

25. The method for preparing 1,5-pentanediisocyanate by a non-phosgene method according to claim 24, It is characterized in that The reaction time is 240-300 min.

26. The method for preparing 1,5-pentanediisocyanate by a non-phosgene method according to claim 12, It is characterized in that The temperature of the reaction solution after cooling is 20-150°C.

27. The method for preparing 1,5-pentanediisocyanate by a non-phosgene method according to claim 26, It is characterized in that The temperature of the reaction solution after cooling is 30-50°C.