A special gas for protecting vehicle lights and its preparation process

Through the special gas formula and the purification treatment of high-purity xenon and krypton, the problems of tungsten filament evaporation and bulb deposition at high temperatures are solved, extending the service life of the lamp and reducing energy consumption.

CN115513040BActive Publication Date: 2024-10-29FOSHAN SANSHUI DELI MESSER GAS CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202211158178.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-09-22
Publication Date
2024-10-29
Estimated Expiration
2042-09-22

AI Technical Summary

Technical Problem

Tungsten filament easily evaporates at high temperatures in automotive lighting bulbs, causing tungsten to deposit on the bulb shell, causing the bulb shell to turn black and affecting its service life.

Method used

Special gas formulas are used, including dibromomethane, nitrogen, xenon and krypton. Through specific filling processes and purification treatments, high-purity xenon and krypton are prepared to reduce the evaporation of tungsten wire and inhibit tungsten deposition.

Benefits of technology

Effectively reduce the evaporation of tungsten filament, prevent the bulb from turning black, extend the service life of the lamp, and save energy consumption.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0003859766740000081
    Figure BDA0003859766740000081
  • Figure BDA0003859766740000091
    Figure BDA0003859766740000091
  • Figure BDA0003859766740000092
    Figure BDA0003859766740000092
Patent Text Reader

Abstract

The present application discloses a special gas for protecting headlights and a preparation process thereof, and relates to the field of special gases. The special gas for protecting headlights is made of 0.029-0.031wt% dibromomethane, 0.013-0.016wt% dichloromethane, 4-6wt% nitrogen, 28-32wt% xenon and the remainder of krypton. The special gas for protecting headlights can not only reduce the evaporation of tungsten filaments, but also inhibit the deposition of tungsten on the bulb shell, thereby improving the problem that the bulb shell is easy to blacken, and further extending the service life of the headlights.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of special gases, and in particular to a special gas for protecting vehicle lights and a preparation process thereof. Background Art

[0002] Tungsten filaments are mainly used in electric light sources such as incandescent lamps and halogen tungsten lamps. Among them, tungsten filaments used as various luminous bodies in bulbs for automobile lighting also need to be doped with oxides such as potassium, silicon, and aluminum during the smelting process to improve the high-temperature anti-drooping ability of the tungsten filaments to ensure the luminous effect of the bulbs.

[0003] However, although the anti-sagging ability of the tungsten filament is improved, the temperature of the tungsten filament is extremely high during the lighting process of the bulb, making the tungsten easy to evaporate.

[0004] Among them, the gas filling can inhibit the evaporation of tungsten. At present, the protective gas in the automotive lighting bulbs is usually argon or a mixture of argon and nitrogen, which reduces the evaporation of the tungsten filament and prolongs the service life of the tungsten filament. However, the evaporated tungsten is easy to deposit on the bulb shell, resulting in the bulb shell being prone to blackening after long-term use. Summary of the invention

[0005] In order to reduce the evaporation of tungsten filament and further improve the problem that the bulb shell of automobile lighting bulbs is prone to blackening after long-term use, the present application provides a special gas for protecting automobile lights and its preparation process.

[0006] In the first aspect, the present application provides a special gas for protecting vehicle lights using the following technical solution:

[0007] A special gas for car lamp protection, made from the following raw materials in percentage by weight:

[0008] Dibromomethane: 0.029-0.031%

[0009] Dichloromethane: 0.013-0.016%

[0010] Nitrogen: 4-6%

[0011] Xenon: 28-32%

[0012] Krypton: Balance

[0013] The purity of the xenon gas and krypton gas is above 99.9%.

[0014] Preferably, the special gas for headlight protection is made of the following raw materials in weight percentage:

[0015] Dibromomethane: 0.03%

[0016] Dichloromethane: 0.015%

[0017] Nitrogen: 5%

[0018] Xenon: 30%

[0019] Krypton: Balance

[0020] The purity of the xenon gas and the krypton gas is above 99.9%.

[0021] The special gas made according to the above formula can not only reduce the evaporation of tungsten filament, but also inhibit the deposition of tungsten on the bulb, thereby improving the problem of the bulb turning black easily and further extending the service life of the car lamp.

[0022] Preferably, the purity of the xenon gas and krypton gas is above 99.999%.

[0023] The purity of xenon and krypton reaches more than 99.999%, which can effectively reduce the evaporation of tungsten filament at high working temperature, which is beneficial to prolong the service life of tungsten filament at high working temperature.

[0024] In the second aspect, the present application provides a preparation process of a special gas for protecting vehicle lights, which adopts the following technical solution:

[0025] A process for preparing special gas for protecting vehicle lamps comprises the following steps:

[0026] S1. Under the vacuum state of the cylinder, pressurize the saturated dichloromethane vapor into the cylinder according to the proportion;

[0027] S2. When the cylinder is in vacuum state, charge the saturated dibromomethane vapor into the cylinder according to the proportion;

[0028] S3. Fill the cylinder with nitrogen according to the proportion;

[0029] S4. Fill the cylinder with xenon gas according to the proportion;

[0030] S5. Fill the cylinder with krypton gas according to the ratio.

[0031] The preparation process for preparing special gases for protecting vehicle lamps has the advantages of simple process steps and high production efficiency.

[0032] Preferably, before filling the xenon gas and the krypton gas, the xenon gas and the krypton gas are first purified by a purifier, and the purification method is as follows:

[0033] The purifier in the adsorber is activated under vacuum at 300-600°C for 5-6 hours;

[0034] Xenon or krypton gas is introduced into the adsorber at a rate of 500-600 mL / min.

[0035] Before filling xenon and krypton, the xenon and krypton are purified with a purifier to make the purity of xenon and krypton reach more than 99.999%, which can further reduce the evaporation of tungsten filament at high working temperature and extend the service life of tungsten filament at higher working temperature.

[0036] Preferably, the purifier is made of the following raw materials in parts by weight:

[0037] Zirconium metal powder: 550-600 parts

[0038] Strontium oxide powder: 8-12 parts

[0039] Titanium powder: 3-5 parts

[0040] Calcium oxide powder: 5-10 parts

[0041] Aluminum powder: 10-20 parts

[0042] Iron powder: 4-8 parts.

[0043] The activation temperature of the purifier prepared by the above formula is about 300° C., which can increase the purity of xenon and krypton to more than 99.999%, greatly saving energy consumption.

[0044] Preferably, the preparation method of the purifier comprises the following steps:

[0045] Metal zirconium powder, strontium oxide powder, metal titanium powder, calcium oxide powder, aluminum powder and iron powder are smelted in a vacuum, and the temperature is controlled at 900-1000°C during the smelting process. After smelting evenly, the temperature is lowered to 400-500°C, and then kept at this temperature for 2-3 hours, and then lowered to room temperature to obtain a zirconium alloy;

[0046] The zirconium alloy is ball-milled, and a zirconium alloy with a particle size range of 40-50 μm and a zirconium alloy with a particle size range of 1-2 mm are selected as purifiers, and the weight ratio of the zirconium alloy with a particle size range of 40-50 μm to the zirconium alloy with a particle size range of 1-2 mm is 1:(3-4).

[0047] The purifier prepared by the above method has uniform pore size and large micropore internal surface area, which increases the contact area between the gas and the purifier; secondly, the contact area between the gas and the purifier is further increased by compounding zirconium alloys of different particle sizes, which is conducive to improving the gas purification efficiency. In addition, the activation temperature of the purifier prepared by the above method is about 300°C, which can increase the purity of xenon and krypton to more than 99.999%, greatly saving energy consumption.

[0048] Preferably, the metal zirconium powder is pretreated before smelting, and the pretreatment of the metal zirconium powder comprises the following steps:

[0049] Adding 2-4 parts by weight of polyvinyl alcohol to 100 parts by weight of deionized water to prepare a polyvinyl alcohol aqueous solution;

[0050] 1-2 parts by weight of metal zirconium powder is added to a polyvinyl alcohol aqueous solution, subjected to ultrasonic treatment for 1-2 hours, filtered, and dried at 50-60° C. to obtain pretreated metal zirconium powder.

[0051] Using polyvinyl alcohol to pre-treat the metal zirconium powder before smelting is beneficial to reducing the pulverization rate of the purifier after multiple cycles of use.

[0052] Preferably, the average molecular weight of the polyvinyl alcohol is 40,000-50,000.

[0053] The coating effect of the metal zirconium powder can be further improved by selecting polyvinyl alcohol with an average molecular weight of 40,000-50,000.

[0054] In summary, the technical solution of the present application includes at least the following beneficial effects:

[0055] (1) The special gas used for protecting the headlights in the present application can not only reduce the evaporation of the tungsten filament at a higher working temperature, but also inhibit the deposition of tungsten on the bulb, thereby improving the problem that the bulb tends to turn black after a long time.

[0056] (2) Before filling xenon and krypton, the xenon and krypton are purified by a purifier to make the purity of xenon and krypton reach above 99.999%, which can further reduce the evaporation of tungsten filament at higher working temperature.

[0057] (3) The activation temperature of the purifier used to purify xenon and krypton in the present application is relatively low, which can effectively reduce energy consumption. DETAILED DESCRIPTION

[0058] The present application discloses a special gas for protecting a headlight, which can reduce the evaporation of tungsten filament and inhibit the deposition of tungsten on the bulb, thereby improving the problem of the bulb being easy to turn black and further extending the service life of the headlight. The special gas for protecting a headlight is made of the following raw materials in percentage by weight:

[0059] Dibromomethane: 0.029-0.031%

[0060] Dichloromethane: 0.013-0.016%

[0061] Nitrogen: 4-6%

[0062] Xenon: 28-32%

[0063] Krypton: Balance

[0064] The purity of xenon gas and krypton gas is 99.9% or more, and preferably, the purity of xenon gas and krypton gas is 99.999% or more.

[0065] More preferably, the weight percentage of dibromomethane is 0.03%, the weight percentage of dichloromethane is 0.015%, the weight percentage of nitrogen is 5%, the weight percentage of xenon is 30%, and the weight percentage of krypton is 64.955%.

[0066] In addition, the present application also discloses a preparation process of the above-mentioned special gas for protecting vehicle lights, comprising the following steps:

[0067] S1. Under the vacuum state of the cylinder, pressurize the saturated dichloromethane vapor into the cylinder according to the proportion;

[0068] S2. When the cylinder is in vacuum state, charge the saturated dibromomethane vapor into the cylinder according to the proportion;

[0069] S3. Fill the cylinder with nitrogen according to the proportion;

[0070] S4. Fill the cylinder with xenon gas according to the proportion;

[0071] S5. Fill the cylinder with krypton gas according to the ratio.

[0072] In order to further reduce the evaporation of the tungsten filament at high working temperature, it is preferred to purify the xenon gas and krypton gas respectively before filling the xenon gas and krypton gas. The purification method is as follows:

[0073] The purifier in the adsorber is activated under vacuum at 300-600°C for 5-6 hours;

[0074] Xenon or krypton gas is introduced into the adsorber at a rate of 500-600 mL / min.

[0075] Wherein, the purifying agent is preferably made of the following raw materials in parts by weight:

[0076] Zirconium metal powder: 550-600 parts

[0077] Strontium oxide powder: 8-12 parts

[0078] Titanium powder: 3-5 parts

[0079] Calcium oxide powder: 5-10 parts

[0080] Aluminum powder: 10-20 parts

[0081] Iron powder: 4-8 parts.

[0082] The activation temperature of the purifier prepared by the above formula is about 600° C., which can increase the purity of xenon and krypton to more than 99.999%, greatly saving energy consumption.

[0083] In addition, the preparation method of the above-mentioned purifier is preferably the following preparation method, and the activation temperature of the purifier prepared by the method can increase the purity of xenon and krypton to more than 99.999% at about 600°C, which greatly saves energy consumption. Among them, the preferred preparation method of the purifier includes the following steps:

[0084] Metal zirconium powder, strontium oxide powder, metal titanium powder, calcium oxide powder, aluminum powder and iron powder are smelted in a vacuum, and the temperature is controlled at 900-1000°C during the smelting process. After smelting evenly, the temperature is lowered to 400-500°C, and then kept at this temperature for 2-3 hours, and then lowered to room temperature to obtain a zirconium alloy;

[0085] The zirconium alloy is ball-milled, and a zirconium alloy with a particle size range of 40-50 μm and a zirconium alloy with a particle size range of 1-2 mm are selected as purifiers, and the weight ratio of the zirconium alloy with a particle size range of 40-50 μm to the zirconium alloy with a particle size range of 1-2 mm is 1:(3-4).

[0086] More preferably, the metal zirconium powder is pretreated before smelting, and the pretreatment of the metal zirconium powder comprises the following steps:

[0087] Adding 2-4 parts by weight of polyvinyl alcohol to 100 parts by weight of deionized water to prepare a polyvinyl alcohol aqueous solution;

[0088] 1-2 parts by weight of metal zirconium powder is added to a polyvinyl alcohol aqueous solution, subjected to ultrasonic treatment for 1-2 hours, filtered, and dried at 50-60° C. to obtain pretreated metal zirconium powder.

[0089] Among them, using polyvinyl alcohol to coat the metal zirconium powder before smelting is beneficial to reduce the powdering rate of the purifier after multiple cycles of use. Preferably, the polyvinyl alcohol used in the pretreatment step is preferably polyvinyl alcohol with an average molecular weight of 40,000-50,000, which can further improve the coating effect of the metal zirconium powder.

[0090] The present application is further described in detail below in conjunction with embodiments and comparative examples.

[0091] Example

[0092] Examples 1-3

[0093] The formulation of the special gas used for vehicle lamp protection in Examples 1-3 is shown in Table 1 below.

[0094] Table 1 Proportions of special gases used for lamp protection in Examples 1-3 (unit / kg)

[0095] raw material Example 1 Example 2 Example 3 Dibromomethane 0.029 0.031 0.030 Dichloromethane 0.016 0.013 0.015 Nitrogen 4 6 5 Xenon 32 28 30 Krypton 63.955 65.956 64.955

[0096] The purity of the xenon gas and krypton gas in the above-mentioned embodiments 1-3 is 99.9%.

[0097] In addition, the preparation process of the special gas for protecting the vehicle lamp in the above-mentioned embodiments 1-3 comprises the following steps:

[0098] S1. Under the vacuum state of the cylinder, pressurize the saturated dichloromethane vapor into the cylinder according to the proportion;

[0099] S2. When the cylinder is in vacuum state, charge the saturated dibromomethane vapor into the cylinder according to the proportion;

[0100] S3. Fill the cylinder with nitrogen according to the proportion;

[0101] S4. Fill the cylinder with xenon gas according to the proportion;

[0102] S5. Fill the cylinder with krypton gas according to the ratio.

[0103] Embodiment 4-5

[0104] A special gas for protecting vehicle lights, which differs from Example 1 in that the preparation process is different.

[0105] Specifically, when preparing the special gas for protecting the headlights in this embodiment, before filling the xenon gas and the krypton gas, the xenon gas and the krypton gas are first purified by a purifier, and the purification method is as follows:

[0106] The purifier in the adsorber was activated under vacuum at 600°C for 5.5 hours, wherein the inner diameter of the adsorber was 25 cm and the length was 80 cm;

[0107] Xenon or krypton gas is introduced into the adsorber at a rate of 550 mL / min.

[0108] Among them, the purity of xenon and krypton after purification is more than 99.999%.

[0109] In addition, the difference between Example 4 and Example 5 is that the purifier is different.

[0110] The raw materials of the medium purifier are shown in Table 2.

[0111] Table 2 Component ratio of the purifier in Examples 4-5 (unit / g)

[0112] project Example 4 Example 5 Zirconium metal powder 550 600 Strontium oxide powder 8 12 Titanium powder 3 5 Calcium oxide powder 5 10 Aluminum powder 10 20 Iron Fan 4 8

[0113] In addition, the preparation method of the purifier in Example 4-5 comprises the following steps:

[0114] Metal zirconium powder, strontium oxide powder, metal titanium powder, calcium oxide powder, aluminum powder and iron powder are smelted in a vacuum, and the temperature is controlled at 950°C during the smelting process. The smelting is carried out for 30 minutes, and then the temperature is reduced to 450°C, and then the temperature is kept for 2.5 hours, and then the temperature is reduced to room temperature to obtain a zirconium alloy;

[0115] The zirconium alloy is ball-milled, and a zirconium alloy with a particle size range of 40-50 μm and a zirconium alloy with a particle size range of 1-2 mm are selected as purifiers, and the weight ratio of the zirconium alloy with a particle size range of 40-50 μm to the zirconium alloy with a particle size range of 1-2 mm is 1:3.5.

[0116] Example 6

[0117] A special gas for protecting vehicle lights, which differs from Example 4 in that:

[0118] Strontium oxide powder was replaced by an equal amount of lanthanum oxide powder.

[0119] Example 7

[0120] A special gas for protecting vehicle lights, which differs from Example 4 in that:

[0121] Calcium oxide powder was replaced by an equal amount of lanthanum oxide powder.

[0122] Example 8

[0123] A special gas for protecting vehicle lights, which differs from Example 4 in that:

[0124] Zirconium alloy with a particle size range of 1-2 mm is selected as the purifier.

[0125] Example 9

[0126] A special gas for protecting vehicle lights, which differs from Example 4 in that:

[0127] Metal zirconium powder, strontium oxide powder, metal titanium powder, calcium oxide powder, aluminum powder and iron powder are smelted under vacuum, the temperature is controlled at 450°C during the smelting process, and then kept at this temperature for 2.5 hours, and then cooled to room temperature to obtain a zirconium alloy;

[0128] The zirconium alloy is ball-milled, and a zirconium alloy with a particle size range of 40-50 μm and a zirconium alloy with a particle size range of 1-2 mm are selected as purifiers, and the weight ratio of the zirconium alloy with a particle size range of 40-50 μm to the zirconium alloy with a particle size range of 1-2 mm is 1:3.5.

[0129] Example 10

[0130] A special gas for protecting vehicle lights, which differs from Example 4 in that:

[0131] The metal zirconium powder is pretreated before smelting. The pretreatment steps of the metal zirconium powder are as follows:

[0132] 3 kg of polyvinyl alcohol with an average molecular weight of 40,000 was added to 100 kg of deionized water to prepare a polyvinyl alcohol aqueous solution;

[0133] 1.5 kg of metal zirconium powder was put into a polyvinyl alcohol aqueous solution, ultrasonically treated for 1.5 hours, then filtered and dried at 55° C. to obtain pretreated metal zirconium powder.

[0134] Comparative Example

[0135] Comparative Example 1

[0136] A special gas for protecting vehicle lights, which differs from Example 1 in that:

[0137] Dichloromethane was replaced with an equal amount of dibromomethane.

[0138] Comparative Example 2

[0139] A special gas for protecting vehicle lights, which differs from Example 1 in that:

[0140] Dibromomethane was replaced with an equal amount of dichloromethane.

[0141] Performance test data

[0142] 1. Tungsten evaporation: The data after the lamp has been running for 1000 hours, only the special gas filled is not used.

[0143] 2. Purification effect of the purifier: Xenon and krypton gases doped with equal amounts of impurities were used as experimental objects, and the purification effects of the purifier on xenon and krypton gases were tested under the conditions of the same activation time but different activation temperatures; wherein the impurity concentration was 0.1% and the impurities were fluorocarbons.

[0144] 3. Purifier pulverization rate: the pulverization rate of the purifier after 300 cycles of use. The specific method is to screen out the purifier with a particle size range of 1-2mm in the purifier. The mass change of the purifier with a particle size range of 1-2mm in the purifier before and after the test is the pulverization rate.

[0145] Table 3 Effect data of special gases in Examples 1-10 and Comparative Examples 1-2

[0146]

[0147]

[0148] Table 4 Performance data of the purifier in Examples 4-10

[0149]

[0150] Combining Example 1 with Comparative Examples 1-2 and the data in Table 3, it can be seen that the synergy of dichloromethane and dibromomethane can further reduce the evaporation of tungsten filament at higher operating temperature. At the same time, it can also inhibit the deposition of tungsten on the bulb shell, thereby improving the problem that the bulb shell is easy to blacken after long-term use.

[0151] Combining Example 1 with Examples 4-9 and the data in Table 3, it can be seen that using xenon and krypton gases with a purity of more than 99.999% is beneficial to further reduce the evaporation amount of the tungsten filament at a higher working temperature.

[0152] Combining Examples 4-9 and the data in Table 4, it can be seen that the purifier prepared by the purifier formulation and method claimed in the present application has a low activation temperature, which is beneficial to saving energy consumption.

[0153] Combining Example 4 with Example 10 and the data in Table 4, it can be seen that coating the metal zirconium powder with polyvinyl alcohol before smelting the metal zirconium powder is beneficial to reducing the pulverization rate of the purifier after recycling, thereby extending the service life of the purifier.

[0154] This specific embodiment is merely an explanation of the present application and is not a limitation of the present application. After reading this specification, those skilled in the art may make modifications to the present embodiment without any creative contribution as needed. However, as long as it is within the scope of the claims of the present application, it shall be protected by the patent law.

Claims

1. A process for preparing special gas for protecting vehicle lamps, characterized in that: The following steps are involved: S1. Under the vacuum state of the cylinder, pressurize the saturated dichloromethane vapor into the cylinder according to the proportion; S2. When the cylinder is in vacuum state, charge the saturated dibromomethane vapor into the cylinder according to the proportion; S3. Fill the cylinder with nitrogen according to the proportion; S4. Fill the cylinder with xenon gas according to the proportion; S5. Fill the cylinder with krypton gas according to the ratio; The special gas for protecting vehicle lights is made of the following raw materials in percentage by weight: Dibromomethane: 0.029-0.031%; Dichloromethane: 0.013-0.016%; Nitrogen: 4-6%; Xenon: 28-32%; Krypton: Remainder; Before filling xenon and krypton, the xenon and krypton are first purified by a purifier, wherein the purifier is made of the following raw materials in parts by weight: Zirconium metal powder: 550-600 parts; Strontium oxide powder: 8-12 parts; Titanium metal powder: 3-5 parts; Calcium oxide powder: 5-10 parts; Aluminum powder: 10-20 parts; Iron powder: 4-8 parts; The preparation method of the purifier comprises the following steps: Metal zirconium powder, strontium oxide powder, metal titanium powder, calcium oxide powder, aluminum powder and iron powder are smelted in a vacuum, and the temperature is controlled at 900-1000°C during the smelting process. After smelting evenly, the temperature is lowered to 400-500°C, and then kept at this temperature for 2-3 hours, and then lowered to room temperature to obtain a zirconium alloy; The zirconium alloy is ball-milled, and a zirconium alloy with a particle size range of 40-50µm and a zirconium alloy with a particle size range of 1-2mm are selected as purifiers, and the weight ratio of the zirconium alloy with a particle size range of 40-50µm to the zirconium alloy with a particle size range of 1-2mm is 1:(3-4).

2. The process for preparing a special gas for protecting vehicle lights according to claim 1, characterized in that: The special gas for protecting vehicle lights is made of the following raw materials in percentage by weight: Dibromomethane: 0.03% Dichloromethane: 0.015% Nitrogen: 5% Xenon: 30% Krypton: Balance The purity of the xenon gas and krypton gas is above 99.9%.

3. A process for preparing a special gas for protecting vehicle lights according to any one of claims 1 to 2, characterized in that: The purity of the xenon gas and krypton gas is above 99.999%.

4. The process for preparing a special gas for protecting vehicle lights according to claim 1, characterized in that: Before filling xenon and krypton, the xenon and krypton are first purified by a purifier, and the purification method is as follows: The purifier in the adsorber is activated under vacuum at 300-600°C for 5-6 hours; Xenon or krypton gas is introduced into the adsorber at a rate of 500-600 mL / min.

5. The process for preparing special gas for protecting vehicle lamps according to claim 1, characterized in that: The metal zirconium powder is pretreated before smelting, and the pretreatment of the metal zirconium powder includes the following steps: Adding 2-4 parts by weight of polyvinyl alcohol to 100 parts by weight of deionized water to prepare a polyvinyl alcohol aqueous solution; 1-2 parts by weight of metal zirconium powder is added to a polyvinyl alcohol aqueous solution, subjected to ultrasonic treatment for 1-2 hours, filtered, and dried at 50-60° C. to obtain pretreated metal zirconium powder.

6. The process for preparing special gas for protecting vehicle lamps according to claim 5, characterized in that: The average molecular weight of the polyvinyl alcohol is 40,000-50,000.

Citation Information

Patent Citations

  • Krypton-xenon gas purification method and device

    CN104310325A

  • Small-caliber high power lighting tungsten halide lamp and its made method

    CN1071030A