Method for recycling aggregate from waste concrete and high temperature strengthening device
By adopting high-temperature waste heat heating device and multi-step treatment in the treatment of waste concrete recycled aggregate, the problems of poor quality, high cost and high energy consumption in the prior art are solved, and high quality, low energy consumption and low pollution are achieved. production of recycled aggregates.
Patent Information
- Application Number
- CN202211099237.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-09-08
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2042-09-08
AI Technical Summary
In the prior art, waste concrete recycled aggregate has poor quality and high cost, and has problems such as secondary pollution and high energy consumption.
Using waste concrete regenerated aggregate method including rotatable cylindrical structure and high-temperature waste heat heating device, the high-temperature waste heat resources are used to heat by pre-decomposition treatment, crushing, high-temperature reinforcement, milling and screening steps to avoid direct consumption of fossil fuels and electricity, reducing energy consumption and pollution.
It improves the quality of recycled aggregates, reduces energy consumption and pollution, and achieves efficient production of recycled aggregates, which has the advantages of high quality, low energy consumption and low pollution.
Smart Images

Figure CN116283011B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of building material processing, and more specifically, to a method for recycling aggregate from waste concrete and a high-temperature strengthening device. Background Art
[0002] With the process of urbanization and industrialization, the construction industry has developed rapidly, and natural sand and gravel aggregates have been consumed in large quantities. The annual consumption of engineering construction is about 7 billion tons, which has caused the natural aggregate resources to become increasingly scarce and the ecological environment to be seriously damaged. On the other hand, the demolition and reconstruction of concrete buildings such as bridges and houses in the process of urban renewal and transformation have generated hundreds of millions of tons of waste concrete, and the amount is increasing day by day with the acceleration of urbanization. The simple landfill or open-air storage of waste concrete not only occupies a large amount of land and has high transportation costs, but also brings potential harm to the ecological environment such as soil and water sources. Carrying out the recycling of waste concrete, such as the production of recycled aggregates and recycled concrete, has significant economic, social and environmental benefits.
[0003] At present, the methods of recycling aggregate from discarded concrete include simple mechanical crushing and screening method (patent CN111825360A), chemical strengthening treatment method (patent CN108298849A, CN111747668A), high temperature strengthening treatment method (patent CN103626413B, CN209854006U), etc. The recycled aggregate obtained by the simple mechanical crushing and screening method has many edges and corners, contains cement mortar that is difficult to separate in the components, has high porosity, high water absorption rate, and many fine cracks, resulting in its performance being significantly lower than that of natural aggregates. The prepared recycled concrete has low strength and can only be used for low-grade concrete preparation. The chemical strengthening treatment method uses chemical reagents to soak for strengthening treatment, thereby improving the quality of recycled aggregates, but the cost is high and there are secondary pollutants produced. The high temperature strengthening treatment method grinds and screens the concrete after preliminary crushing after high temperature treatment such as high temperature oven heating or microwave heating, which greatly improves the quality of recycled aggregates, but there is a problem of high energy consumption. Summary of the invention
[0004] In view of the above problems, the purpose of the present invention is to provide a method for recycling aggregate from waste concrete and a high-temperature strengthening device to solve the problems existing in the current prior art of poor quality of aggregate recycled from waste concrete, high cost, secondary pollution and high energy consumption.
[0005] The present invention provides a high-temperature strengthening device for recycled concrete aggregate, comprising a rotatable cylindrical structure and a high-temperature waste heat heating device; wherein:
[0006] The cylindrical structure is a horizontal cylindrical structure arranged obliquely or a vertical cylindrical structure arranged vertically;
[0007] When the cylindrical structure is a horizontal cylindrical structure, a feed port is provided at the top of one end of the horizontal cylindrical structure that is inclined upward, and a discharge port is provided at the bottom of one end of the horizontal cylindrical structure that is inclined downward; when the cylindrical structure is a vertical cylindrical structure, a feed port is provided at the top of the vertical cylindrical structure, and a discharge port is provided at the bottom of the vertical cylindrical structure;
[0008] The high-temperature waste heat heating device comprises a first high-temperature waste heat heating structure and / or a second high-temperature waste heat heating structure; wherein,
[0009] The first high-temperature waste heat heating structure comprises a sleeve arranged inside the cylindrical structure; a high-temperature waste heat channel is formed between the outer wall of the sleeve and the inner wall of the cylindrical structure; a first high-temperature waste heat inlet is arranged at the upper end of the high-temperature waste heat channel close to the discharge port; a first high-temperature waste heat outlet is arranged at the bottom of the lower end of the high-temperature waste heat channel close to the feed port;
[0010] The second high-temperature waste heat heating structure includes a hollow turntable arranged in the middle of the cylindrical structure, and a second high-temperature waste heat inlet and a second high-temperature waste heat outlet are respectively provided at both ends of the turntable; the second high-temperature waste heat inlet is close to the first high-temperature waste heat inlet, and the second high-temperature waste heat outlet is close to the first high-temperature waste heat outlet.
[0011] In addition, a preferred solution is that when the cylindrical structure is a horizontal cylindrical structure arranged obliquely, an inlet and an outlet communicating with the feed port and the discharge port are respectively arranged on the sleeve.
[0012] In addition, a preferred solution is that an evaporated water outlet is provided at the top of the horizontal cylindrical structure.
[0013] The present invention provides a method for recycling aggregate from waste concrete, comprising the following steps:
[0014] S1, performing a pre-impurity removal treatment on the waste concrete to remove iron impurities and non-iron impurities in the waste concrete to obtain the impurity-removed waste concrete;
[0015] S2, crushing the waste concrete after impurities removal to obtain waste concrete blocks with a particle size of 40 mm to 80 mm;
[0016] S3, adding the waste concrete blocks into the above-mentioned concrete recycled aggregate high temperature strengthening device for high temperature strengthening treatment to obtain high temperature strengthened waste concrete blocks;
[0017] S4, placing the high temperature strengthened waste concrete block in a grinding device, grinding and crushing it to obtain aggregate with a particle size of less than 40 mm;
[0018] S5. Screening the aggregate through a vibrating screen to obtain classified recycled aggregate.
[0019] In addition, a preferred solution is that the waste concrete is pre-processed to remove iron impurities and non-iron impurities in the waste concrete to obtain the waste concrete after impurities removal, which comprises:
[0020] The waste concrete is crushed by impact hammering, and the steel bars in the waste concrete are divided to obtain large blocks of concrete;
[0021] The iron impurities in the bulk concrete are sorted and removed by a magnetic separator to obtain the bulk concrete from which the iron impurities are removed;
[0022] The non-iron impurities in the bulk concrete from which the iron impurities have been removed are sorted and removed to obtain the waste concrete after the impurities have been removed.
[0023] In addition, a preferred solution is that the waste concrete after impurities removal is crushed to obtain waste concrete blocks with a particle size of 40 mm to 80 mm, which comprises:
[0024] The waste concrete after impurities removal is added to a jaw crusher or a cone crusher for crushing to obtain waste concrete blocks with a particle size of 40 mm to 80 mm; wherein,
[0025] The minimum feed particle size of the jaw crusher is 350mm, the processing capacity is 20-65t / h, and the power is 30kw.
[0026] In addition, a preferred solution is that the waste concrete blocks are added to the concrete recycled aggregate high temperature strengthening device for high temperature strengthening treatment to obtain the high temperature strengthened waste concrete blocks, which comprises:
[0027] A heat source of high-temperature waste heat is introduced from the first high-temperature waste heat inlet and / or the second high-temperature waste heat inlet of the recycled aggregate high-temperature strengthening device, and waste concrete blocks are added from the feed inlet of the recycled aggregate high-temperature strengthening device, and the waste concrete blocks are subjected to high-temperature strengthening by the heat source of high-temperature waste heat;
[0028] The waste concrete blocks strengthened by high temperature move downwards and slide to the discharge port of the recycled aggregate high temperature strengthening device as the cylindrical structure rotates, and flow out from the discharge port.
[0029] In addition, a preferred solution is that the heat source of the high-temperature waste heat is a waste heat resource; and / or the temperature of the heat source of the high-temperature waste heat is 300°C to 1000°C; and / or the temperature of the waste concrete blocks after high-temperature strengthening is 200°C to 800°C; the heating time of the waste concrete blocks in the recycled aggregate high-temperature strengthening device is 40 to 80 minutes.
[0030] In addition, a preferred solution is that in the process of placing the high temperature strengthened waste concrete blocks in a grinding device for grinding and crushing to obtain aggregates with a particle size of less than 40 mm,
[0031] The high temperature strengthened waste concrete blocks are placed in a grinding device and ground and crushed 2 to 3 times, each grinding and crushing time is 60 to 120 minutes, to obtain aggregates with a particle size of less than 40 mm.
[0032] In addition, a preferred solution is that the aggregate is screened through a vibrating screen to obtain the graded recycled aggregate, which comprises:
[0033] The aggregate is sieved by a double-layer vibrating screen to obtain first-level recycled aggregate particles with a particle size of 25 to 40 mm, second-level recycled aggregate particles with a particle size of 5 to 25 mm, and third-level recycled aggregate particles with a particle size of less than 5 mm;
[0034] The third-level recycled aggregate particles are subjected to wind classification treatment to obtain fourth-level recycled aggregate particles with a particle size of 0.15 to 5 mm and fine powder with a particle size of less than 0.15 mm.
[0035] From the above technical scheme, it can be seen that the waste concrete regeneration aggregate method and high temperature strengthening device provided by the present invention removes iron impurities and non-iron impurities in the waste concrete through pre-impurity removal treatment, crushes the waste concrete into waste concrete blocks with a particle size of 40mm to 80mm through crushing treatment, and then adopts the concrete regeneration aggregate high temperature strengthening device to use high temperature waste heat to perform high temperature strengthening on the waste concrete blocks to obtain high-quality regenerated aggregate; after grinding, crushing and screening, different levels of regenerated aggregate can be obtained; because the heat source used by the concrete regeneration aggregate high temperature strengthening device is a high temperature waste heat resource, it is different from the microwave heating, high temperature oven drying, fossil fuel combustion flue gas heating and other technical means used in the prior art, and does not consume precious fossil gas and electricity, and has low energy consumption; the high temperature waste heat resource does not directly contact the waste concrete blocks, and is heated by heat conduction, and the tail gas treatment is simple, with less secondary pollution. The present invention has the advantages of high quality of regenerated aggregate, low energy consumption, and low pollution.
[0036] In order to achieve the above and related purposes, one or more aspects of the present invention include the features that will be described in detail later. The following description and the accompanying drawings describe some exemplary aspects of the present invention in detail. However, these aspects indicate only some of the various ways in which the principles of the present invention can be used. In addition, the present invention is intended to include all these aspects and their equivalents. BRIEF DESCRIPTION OF THE DRAWINGS
[0037] By referring to the following description in conjunction with the accompanying drawings, and with a more comprehensive understanding of the present invention, other objects and results of the present invention will become more clear and easy to understand. In the accompanying drawings:
[0038] Figure 1 is a flow chart of a method for recycling aggregate from waste concrete according to an embodiment of the present invention;
[0039] Figure 2 A schematic diagram of a process flow of a method for recycling aggregate from waste concrete according to an embodiment of the present invention;
[0040] Figure 3 This is a schematic structural diagram of a high-temperature strengthening device for recycled aggregate of concrete according to Example 1 of the present invention;
[0041] Figure 4 This is a schematic structural diagram of a high-temperature strengthening device for recycled aggregate of concrete according to Example 2 of the present invention;
[0042] Figure 5 This is a schematic structural diagram of a high-temperature strengthening device for recycled aggregate of concrete according to Example 3 of the present invention;
[0043] Figure 6 Schematic diagram of the structure of a high-temperature strengthening device for recycled aggregate of concrete according to Example 4 of the present invention.
[0044] In the accompanying drawings, 1-cylindrical structure, 11-feed port, 12-discharge port, 13-evaporated water outlet, 2-sleeve, 21-inlet, 22-outlet, 3-high-temperature waste heat channel, 31-first high-temperature waste heat inlet, 32-first high-temperature waste heat outlet, 4-turntable, 41-second high-temperature waste heat inlet, 42-second high-temperature waste heat outlet, 5-insulation layer.
[0045] The same reference numerals throughout the drawings indicate similar or corresponding features or functions. DETAILED DESCRIPTION
[0046] In the following description, for the purpose of explanation, numerous specific details are set forth in order to provide a thorough understanding of one or more embodiments. However, it is apparent that these embodiments may also be implemented without these specific details.
[0047] In view of the above-mentioned problems in the current prior art, such as poor quality, high cost, secondary pollution and high energy consumption of aggregates recycled from waste concrete, a method for recycling aggregates from waste concrete and a high-temperature strengthening device are proposed.
[0048] The specific embodiments of the present invention will be described in detail below with reference to the accompanying drawings.
[0049] In order to illustrate the method for recycling aggregate from waste concrete and the high temperature strengthening device provided by the present invention, Figure 1 The process of the method for recycling aggregate from waste concrete according to an embodiment of the present invention is shown; Figure 2 The process flow of the method for recycling aggregate from waste concrete according to an embodiment of the present invention is shown; Figure 3 The structure of the high temperature strengthening device for recycled aggregate of concrete according to Example 1 of the present invention is shown; Figure 4 The structure of the high temperature strengthening device for recycled aggregate of concrete according to the second embodiment of the present invention is shown; Figure 5 The structure of the high temperature strengthening device for recycled aggregate of concrete according to Example 3 of the present invention is shown; Figure 6 The structure of the high-temperature strengthening device for recycled aggregate of concrete according to Example 4 of the present invention is shown.
[0050] like Figures 1 to 6 As shown together, the method for recycling aggregate from waste concrete provided by the present invention comprises the following steps:
[0051] S1, pre-impurity treatment is performed on the waste concrete to remove iron impurities and non-iron impurities in the waste concrete to obtain the waste concrete after impurity removal;
[0052] S2, crushing the waste concrete after impurities removal to obtain waste concrete blocks with a particle size of 40 mm to 80 mm;
[0053] S3, adding the waste concrete blocks into a concrete recycled aggregate high temperature strengthening device for high temperature strengthening treatment to obtain high temperature strengthened waste concrete blocks;
[0054] The high-temperature strengthening device for recycled aggregate of concrete comprises a rotatable cylindrical structure 1 and a high-temperature waste heat heating device; wherein the cylindrical structure 1 is an inclined horizontal cylindrical structure or a vertical cylindrical structure; when the cylindrical structure 1 is a horizontal cylindrical structure, a feed port 11 is arranged at the top of one end of the horizontal cylindrical structure inclined upward, and a discharge port 12 is arranged at the bottom of one end of the horizontal cylindrical structure inclined downward; when the cylindrical structure is a vertical cylindrical structure, a feed port 11 is arranged at the top of the vertical cylindrical structure, and a discharge port 12 is arranged at the bottom of the vertical cylindrical structure; the high-temperature waste heat heating device comprises a first high-temperature waste heat heating structure and / or a second high-temperature waste heat heating structure; wherein the first high-temperature waste heat heating The thermal structure includes a sleeve 2 arranged inside the cylindrical structure 1; a high-temperature waste heat channel 3 is formed between the outer wall of the sleeve 2 and the inner wall of the cylindrical structure 1; a first high-temperature waste heat inlet 31 is arranged at the upper end of the high-temperature waste heat channel 3 close to the discharge port 12; a first high-temperature waste heat outlet 32 is arranged at the bottom of the lower end of the high-temperature waste heat channel 3 close to the feed port 11; the second high-temperature waste heat heating structure includes an internal hollow turntable 4 arranged in the middle of the cylindrical structure 1, and a second high-temperature waste heat inlet 41 and a second high-temperature waste heat outlet 42 are respectively arranged at both ends of the turntable 4; the second high-temperature waste heat inlet 41 is close to the first high-temperature waste heat inlet 31, and the second high-temperature waste heat outlet 42 is close to the first high-temperature waste heat outlet 32.
[0055] S4. Place the high temperature strengthened waste concrete blocks in a grinding device for grinding and crushing to obtain aggregates with a particle size of <40 mm; wherein the grinding device can be a horizontal rotary grinding device.
[0056] S5. The aggregate is screened through a vibrating screen to obtain graded recycled aggregate.
[0057] The iron impurities and non-iron impurities in the waste concrete are removed by pre-impurity removal, and the waste concrete is crushed into waste concrete blocks with a particle size of 40mm to 80mm by crushing. Then, a high-temperature strengthening device for concrete recycled aggregate is used to strengthen the waste concrete blocks with high temperature using high-temperature waste heat to obtain high-quality recycled aggregate; recycled aggregates of different levels can be obtained after grinding, crushing and screening; since the heat source used by the high-temperature strengthening device for concrete recycled aggregate is a high-temperature waste heat resource, it is different from the technical means such as microwave heating, high-temperature oven drying, and fossil fuel combustion flue gas heating used in the prior art, and does not consume precious fossil gas and electricity, and has low energy consumption; the high-temperature waste heat resource does not directly contact the waste concrete blocks, and is heated by heat conduction, and the tail gas treatment is simple, with less secondary pollution. The present invention has the advantages of high quality of recycled aggregate, low energy consumption, and low pollution.
[0058] As a preferred embodiment of the present invention, pre-impurity removal treatment is performed on waste concrete to remove iron impurities and non-iron impurities in the waste concrete, and the waste concrete after impurity removal is obtained includes:
[0059] The waste concrete is crushed by impact hammering, and the steel bars in the waste concrete are divided to obtain large blocks of concrete;
[0060] The iron impurities in the bulk concrete are sorted and removed by a magnetic separator to obtain the bulk concrete without the iron impurities;
[0061] The non-ferrous impurities in the large concrete blocks with iron impurities removed are sorted and removed to obtain the waste concrete after impurities removal.
[0062] The collected large pieces of concrete are crushed by impact hammering and the steel bars are separated. Then, a magnetic separator and a separation table are used to remove and sort iron impurities such as steel bars and non-iron impurities such as glass, wood, and plastic, thereby obtaining the waste concrete after impurities are removed.
[0063] As a preferred embodiment of the present invention, the waste concrete after impurities removal is crushed to obtain waste concrete blocks with a particle size of 40 mm to 80 mm, including:
[0064] The waste concrete after impurities removal is added to a jaw crusher or a cone crusher for crushing to obtain waste concrete blocks with a particle size of 40 mm to 80 mm; wherein,
[0065] The minimum feed particle size of the jaw crusher is 350mm, the processing capacity is 20-65t / h, and the power is 30kw.
[0066] After the waste concrete is removed from the waste concrete, it can be processed by a jaw crusher or a cone crusher to obtain waste concrete blocks with a particle size of 40mm to 80mm. Among them, the jaw crusher is preferably a jaw crusher of model PE-400X600; its minimum feed particle size is 350mm, the discharge particle size is set to 40mm to 80mm, the processing capacity is 20 to 65t / h, and the power is 30kw.
[0067] As a preferred embodiment of the present invention, waste concrete blocks are added into a concrete recycled aggregate high temperature strengthening device for high temperature strengthening treatment, and the waste concrete blocks after high temperature strengthening are obtained, which include:
[0068] The heat source of high-temperature waste heat is introduced from the first high-temperature waste heat inlet 21 and / or the second high-temperature waste heat inlet 41 of the recycled aggregate high-temperature strengthening device, and the waste concrete blocks are added from the feed inlet 11 of the recycled aggregate high-temperature strengthening device, and the waste concrete blocks are subjected to high-temperature strengthening by the heat source of high-temperature waste heat;
[0069] The waste concrete blocks strengthened by high temperature move downwards and slide down to the discharge port 12 of the recycled aggregate high temperature strengthening device as the cylindrical structure 1 rotates, and flow out from the discharge port 12 .
[0070] The heat source of high-temperature waste heat is introduced from the first high-temperature waste heat inlet 21 or the second high-temperature waste heat inlet 41, and is selected according to the specific structure of the high-temperature waste heat heating device in the device. At this time, the heat source is located inside the high-temperature waste heat channel 3 or inside the turntable 4, and will not directly contact the waste concrete blocks. It is heated by heat conduction, and the tail gas treatment is simple, and there is less secondary pollution; when the cylindrical structure 1 is a horizontal cylindrical structure, since the horizontal cylindrical structure is inclined and can rotate, the waste concrete blocks located in the concrete channel 3 slide down along the inclined surface inside it as the horizontal cylindrical structure rotates, and are continuously heated during the sliding process. The heating time and temperature of the internal waste concrete blocks can be controlled by adjusting the length of the sleeve 2 and the inclination angle of the horizontal cylindrical structure. When the cylindrical structure 1 is a vertical cylindrical structure, the waste concrete blocks located in the concrete channel 3 slide down under the action of gravity, and are continuously heated during the sliding process, and the heating is uniform through the rotating cylindrical structure.
[0071] As a preferred embodiment of the present invention, the heat source of the high-temperature waste heat is a waste heat resource; for example, waste heat flue gas or waste steam; and / or the temperature of the heat source of the high-temperature waste heat is 300°C to 1000°C; and / or the temperature of the waste concrete blocks after high-temperature strengthening is 200°C to 800°C; the heating time of the waste concrete blocks in the recycled aggregate high-temperature strengthening device is 40 to 80 minutes.
[0072] The heat source of high-temperature waste heat can be obtained from waste incineration plants, cement plants, and smelters. In particular, waste incineration plants and waste concrete recycling can be processed in coordination and are relatively close. The waste concrete blocks are heated to 200°C to 800°C using high-temperature waste heat of 300°C to 1000°C. The cement stone in the concrete blocks is dehydrated and brittle, making it very easy to remove the cement stone in the subsequent grinding process. The heating time is about 40 to 80 minutes. If the time is too long, the aggregate performance is likely to deteriorate; if the time is too short, the cement stone cannot be dehydrated and brittle, resulting in poor aggregate quality.
[0073] As a preferred embodiment of the present invention, the inclination angle of the horizontal cylindrical structure is 0-8°; and / or the rotation speed of the horizontal cylindrical structure is 0.5-2 r / min. The rotation speed and the inclination angle can be adjusted according to the residence time control.
[0074] As a preferred embodiment of the present invention, a vaporized water outlet 13 is provided at the top of the horizontal cylindrical structure. The vaporized water outlet 13 can be provided to quickly discharge the water vapor inside the horizontal cylindrical structure.
[0075] As a preferred embodiment of the present invention, in the process of placing the high temperature strengthened waste concrete blocks in a grinding device for grinding and crushing to obtain aggregates with a particle size of less than 40 mm,
[0076] The waste concrete blocks after high temperature strengthening are placed in a grinding device and ground and crushed 2 to 3 times, each grinding and crushing time is 60 to 120 minutes, to obtain aggregates with a particle size of <40 mm.
[0077] After high temperature strengthening treatment, the waste concrete blocks enter the grinding device. In the horizontal rotary grinding device, the waste concrete blocks are subjected to the impact and grinding of the steel ball grinding blocks and different waste concrete blocks. After grinding and crushing, the aggregates and fine powders with a particle size of <40mm are sent to the next level for screening and grading. The grinding and crushing treatment is performed 2 to 3 times. The aggregates obtained by one grinding treatment cannot meet the high quality requirements (the cement mortar adhesion rate is high). The grinding time is about 60 to 120 minutes. If the time is too long or too short, high-quality recycled concrete aggregates cannot be obtained.
[0078] As a preferred embodiment of the present invention, the aggregate is screened through a vibrating screen to obtain the classified recycled aggregate, which includes:
[0079] The aggregate is sieved by a double-layer vibrating screen to obtain first-level recycled aggregate particles with a particle size of 25 to 40 mm, second-level recycled aggregate particles with a particle size of 5 to 25 mm, and third-level recycled aggregate particles with a particle size of less than 5 mm;
[0080] The third-level recycled aggregate particles are subjected to wind classification treatment to obtain fourth-level recycled aggregate particles with a particle size of 0.15 to 5 mm and fine powder with a particle size of less than 0.15 mm.
[0081] The concrete blocks after grinding can be screened by vibrating screen to obtain recycled concrete aggregate particles with particle sizes of 25-40mm, 5-25mm, and <5mm. The particles less than 5mm can be processed by wind classification to obtain recycled concrete aggregate particles of 0.15-5mm and fine powder of <0.15mm. Aggregate particles of different particle sizes can be used later as needed.
[0082] The high-temperature strengthening device for recycled aggregate of concrete provided by the present invention is used in the above-mentioned method for recycling aggregate of waste concrete, and comprises a rotatable cylindrical structure 1 and a high-temperature waste heat heating device; wherein the cylindrical structure 1 is an inclined horizontal cylindrical structure or a vertical cylindrical structure; when the cylindrical structure 1 is a horizontal cylindrical structure, a feed port 11 is arranged at the top of one end of the horizontal cylindrical structure inclined upward, and a discharge port 12 is arranged at the bottom of one end of the horizontal cylindrical structure inclined downward; when the cylindrical structure is a vertical cylindrical structure, a feed port 11 is arranged at the top of the vertical cylindrical structure, and a discharge port 12 is arranged at the bottom of the vertical cylindrical structure; the high-temperature waste heat heating device comprises a first high-temperature waste heat heating structure and / or a second high-temperature waste heat heating structure Structure; wherein, the first high-temperature waste heat heating structure includes a sleeve 2 arranged inside the cylindrical structure 1; a high-temperature waste heat channel 3 is formed between the outer wall of the sleeve 2 and the inner wall of the cylindrical structure 1; a first high-temperature waste heat inlet 31 is arranged at the upper port of the high-temperature waste heat channel 3 close to the discharge port 12; a first high-temperature waste heat outlet 32 is arranged at the bottom of the lower port of the high-temperature waste heat channel 3 close to the feed port 11; the second high-temperature waste heat heating structure includes an internally hollow turntable 4 arranged in the middle of the cylindrical structure 1, and a second high-temperature waste heat inlet 41 and a second high-temperature waste heat outlet 42 are respectively arranged at both ends of the turntable 4; the second high-temperature waste heat inlet 41 is close to the first high-temperature waste heat inlet 31, and the second high-temperature waste heat outlet 42 is close to the first high-temperature waste heat outlet 32.
[0083] As a preferred embodiment of the present invention, when the cylindrical structure 1 is an inclined horizontal cylindrical structure, the sleeve 2 is provided with an inlet 21 and an outlet 22 connected with the feed port 11 and the discharge port 12, respectively, to facilitate the entry and exit of raw materials.
[0084] As a preferred embodiment of the present invention, the inclination angle of the horizontal cylindrical structure is 0-8°; and / or the rotation speed of the horizontal cylindrical structure is 0.2-2 r / min. The rotation speed and the inclination angle can be adjusted according to the residence time control.
[0085] As a preferred embodiment of the present invention, an evaporation water outlet 13 is provided at the top of the horizontal cylindrical structure to allow the water vapor inside to be quickly discharged.
[0086] As a preferred embodiment of the present invention, a feed pipe is provided between the feed port 11 and the inlet 21, and a feed end of the feed pipe is provided on the outer side wall of the horizontal cylindrical structure.
[0087] As a preferred embodiment of the present invention, a discharge pipe is provided between the discharge port 12 and the outlet 22, and the discharge end of the discharge pipe is provided on the outer side wall of the horizontal cylindrical structure.
[0088] As a preferred embodiment of the present invention, a first waste heat inlet pipe is connected to the first high-temperature waste heat inlet 31, and a second waste heat inlet pipe is connected to the second high-temperature waste heat inlet 41; the first waste heat inlet pipe and the second waste heat inlet pipe are both connected to the heat source pipeline of the high-temperature waste heat.
[0089] As a preferred embodiment of the present invention, a first waste heat outlet pipe is connected to the first high-temperature waste heat outlet 32, and a second waste heat outlet pipe is connected to the second high-temperature waste heat inlet 41; the first waste heat outlet pipe and the second waste heat outlet pipe are both connected to the waste heat treatment device.
[0090] As a preferred embodiment of the present invention, the turntable 4 is a spiral turntable with a spiral structure.
[0091] As a preferred embodiment of the present invention, an anti-corrosion layer is provided on the inner side wall of the horizontal cylindrical structure to prevent corrosion.
[0092] As a preferred embodiment of the present invention, an anti-corrosion layer is provided inside the rotating disk 4 to prevent corrosion.
[0093] Among them, the horizontal cylindrical structure is a horizontal cylinder, which is easy to rotate and has a large internal capacity.
[0094] Among them, the horizontal cylindrical structure can be rotated by roller drive (mature mechanical devices are not described here), and the turntable 4 (or propeller plate) is a rotatable mechanism, which is beneficial to enhance heat transfer.
[0095] like Figures 3 to 6 As shown, they are schematic diagrams of three specific embodiments 1, 2, 3 and 4 of the concrete recycled aggregate high temperature strengthening device of the present invention, respectively. Figures 3 to 5 All are high-temperature strengthening devices with a horizontal cylindrical structure, and the high-temperature waste heat heating device includes only the first high-temperature waste heat heating structure, only the second high-temperature waste heat heating structure, and both the first high-temperature waste heat heating structure and the second high-temperature waste heat heating structure. Figure 6 It is a high temperature strengthening device with a vertical cylindrical structure.
[0096] Among them, the vertical cylindrical structure in Example 4 is provided with a feed port 11 (for waste concrete to enter) and a discharge port 12 (for heated waste concrete to discharge), as well as a first high-temperature waste heat inlet 31 and a first high-temperature waste heat outlet 32 for the heat source of high-temperature waste heat to enter and discharge. When the high-temperature strengthening device is as shown in Example 4, the high-temperature waste heat source is high-temperature flue gas, which enters from the lower end of the device and is discharged from the upper end; the waste concrete material enters from the upper end of the device and is discharged from the lower end. The heat source and the material are in direct contact. The device is characterized by high heating efficiency. In order to keep the internal raw materials of the vertical cylindrical structure warm, an insulation layer 5 is provided on the inner side of the vertical cylindrical structure.
[0097] It can be seen from the above specific embodiments that the waste concrete regeneration aggregate method and high temperature strengthening device provided by the present invention removes iron impurities and non-iron impurities in the waste concrete through pre-impurity removal treatment, crushes the waste concrete into waste concrete blocks with a particle size of 40mm to 80mm through crushing treatment, and then adopts the concrete regeneration aggregate high temperature strengthening device to use high temperature waste heat to perform high temperature strengthening on the waste concrete blocks to obtain high-quality regenerated aggregate; after grinding, crushing and screening, different levels of regenerated aggregate can be obtained; because the heat source used by the concrete regeneration aggregate high temperature strengthening device is a high temperature waste heat resource, it is different from the microwave heating, high temperature oven drying, fossil fuel combustion flue gas heating and other technical means used in the prior art, and does not consume precious fossil gas and electricity, and has low energy consumption; the high temperature waste heat resource does not directly contact the waste concrete blocks, and is heated by heat conduction, and the tail gas treatment is simple, with less secondary pollution. The present invention has the advantages of high quality of regenerated aggregate, low energy consumption, and low pollution.
[0098] As described above, the method for recycling aggregate from waste concrete and the high temperature strengthening device proposed in the present invention are described by way of example with reference to the accompanying drawings. However, those skilled in the art should understand that various improvements can be made to the method for recycling aggregate from waste concrete and the high temperature strengthening device proposed in the present invention without departing from the content of the present invention. Therefore, the protection scope of the present invention should be determined by the content of the attached claims.
Claims
1. A high temperature strengthening device for recycled concrete aggregate, characterized in that: It includes a rotatable cylindrical structure and a high-temperature waste heat heating device; wherein, The cylindrical structure is a horizontal cylindrical structure arranged obliquely or a vertical cylindrical structure arranged vertically; When the cylindrical structure is a horizontal cylindrical structure, a feed port is provided at the top of one end of the horizontal cylindrical structure that is inclined upward, and a discharge port is provided at the bottom of one end of the horizontal cylindrical structure that is inclined downward; when the cylindrical structure is a vertical cylindrical structure, a feed port is provided at the top of the vertical cylindrical structure, and a discharge port is provided at the bottom of the vertical cylindrical structure; The high-temperature waste heat heating device comprises a first high-temperature waste heat heating structure and a second high-temperature waste heat heating structure; wherein, The first high-temperature waste heat heating structure comprises a sleeve arranged inside the cylindrical structure; a high-temperature waste heat channel is formed between the outer wall of the sleeve and the inner wall of the cylindrical structure; a first high-temperature waste heat inlet is arranged at the upper end of the high-temperature waste heat channel close to the discharge port; a first high-temperature waste heat outlet is arranged at the bottom of the lower end of the high-temperature waste heat channel close to the feed port; The second high-temperature waste heat heating structure includes an internally hollow turntable arranged in the middle of the cylindrical structure, and a second high-temperature waste heat inlet and a second high-temperature waste heat outlet are respectively arranged at both ends of the turntable; the second high-temperature waste heat inlet is close to the first high-temperature waste heat inlet, and the second high-temperature waste heat outlet is close to the first high-temperature waste heat outlet; wherein the turntable is a spiral turntable with a spiral structure.
2. The high temperature strengthening device for recycled aggregate of concrete according to claim 1, characterized in that: When the cylindrical structure is a horizontal cylindrical structure arranged obliquely, an inlet and an outlet communicating with the feed port and the discharge port are respectively arranged on the sleeve.
3. The high temperature strengthening device for recycled concrete aggregate according to claim 1, characterized in that: An evaporated water outlet is arranged on the top of the horizontal cylindrical structure.
4. A method for recycling aggregate from waste concrete, characterized in that: The steps include: S1, performing a pre-impurity removal treatment on the waste concrete to remove iron impurities and non-iron impurities in the waste concrete to obtain the impurity-removed waste concrete; S2, crushing the waste concrete after impurities removal to obtain waste concrete blocks with a particle size of 40 mm to 80 mm; S3, adding the waste concrete blocks into the concrete recycled aggregate high temperature strengthening device according to any one of claims 1 to 3 for high temperature strengthening treatment to obtain high temperature strengthened waste concrete blocks; S4, placing the high temperature strengthened waste concrete block in a grinding device, grinding and crushing it to obtain aggregate with a particle size of less than 40 mm; S5. Screening the aggregate through a vibrating screen to obtain classified recycled aggregate.
5. The method for recycling aggregate from waste concrete according to claim 4, characterized in that: The pre-impurity removal treatment of the waste concrete to remove iron impurities and non-iron impurities in the waste concrete to obtain the impurity-removed waste concrete comprises: The waste concrete is crushed by impact hammering, and the steel bars in the waste concrete are divided to obtain large blocks of concrete; The iron impurities in the bulk concrete are sorted and removed by a magnetic separator to obtain the bulk concrete from which the iron impurities are removed; The non-iron impurities in the bulk concrete from which the iron impurities have been removed are sorted and removed to obtain the waste concrete after the impurities have been removed.
6. The method for recycling aggregate from waste concrete according to claim 4, characterized in that: The method of crushing the waste concrete after impurities removal to obtain waste concrete blocks with a particle size of 40 mm to 80 mm comprises: The waste concrete after impurities removal is added to a jaw crusher or a cone crusher for crushing to obtain waste concrete blocks with a particle size of 40 mm to 80 mm; wherein, The minimum feed particle size of the jaw crusher is 350 mm, the processing capacity is 20-65 t / h, and the power is 30 kW.
7. The method for recycling aggregate from waste concrete according to claim 6, characterized in that: The step of adding the waste concrete blocks into the concrete recycled aggregate high temperature strengthening device for high temperature strengthening treatment to obtain the high temperature strengthened waste concrete blocks comprises: A heat source of high-temperature waste heat is introduced from the first high-temperature waste heat inlet and / or the second high-temperature waste heat inlet of the recycled aggregate high-temperature strengthening device, and waste concrete blocks are added from the feed inlet of the recycled aggregate high-temperature strengthening device, and the waste concrete blocks are subjected to high-temperature strengthening by the heat source of high-temperature waste heat; The waste concrete blocks strengthened by high temperature move downwards and slide to the discharge port of the recycled aggregate high temperature strengthening device as the cylindrical structure rotates, and flow out from the discharge port.
8. The method for recycling aggregate from waste concrete according to claim 7, characterized in that: The heat source of the high-temperature waste heat is waste heat resources; and / or, The temperature of the heat source of the high-temperature waste heat is 300° C. to 1000° C.; and / or, The temperature of the waste concrete blocks after high temperature strengthening is 200°C to 800°C; The heating time of the waste concrete blocks in the recycled aggregate high temperature strengthening device is 40 to 80 minutes.
9. The method for recycling aggregate from waste concrete according to claim 4, characterized in that: In the process of placing the high temperature strengthened waste concrete blocks in a grinding device for grinding and crushing to obtain aggregates with a particle size of less than 40 mm, The high temperature strengthened waste concrete blocks are placed in a grinding device and ground and crushed 2 to 3 times, each grinding and crushing time is 60 to 120 minutes, to obtain aggregates with a particle size of less than 40 mm.
10. The method for recycling aggregate from waste concrete according to claim 4, characterized in that: The aggregate is screened through a vibrating screen to obtain the classified recycled aggregate, which comprises: The aggregate is sieved by a double-layer vibrating screen to obtain first-level recycled aggregate particles with a particle size of 25 to 40 mm, second-level recycled aggregate particles with a particle size of 5 to 25 mm, and third-level recycled aggregate particles with a particle size of less than 5 mm; The third-level recycled aggregate particles are subjected to wind classification treatment to obtain fourth-level recycled aggregate particles with a particle size of 0.15 to 5 mm and fine powder with a particle size of less than 0.15 mm.