A preparation method of alpha-ketoleucine
By using the solid base catalyst PDVB-SO3Na in the preparation of α-ketoleucine, the problems of large alkali consumption, large acid consumption and low yield in the existing processes are solved, and an efficient and low-cost preparation process is achieved, which is suitable for industrialization application.
Patent Information
- Application Number
- CN202310774316.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-06-28
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2043-06-28
AI Technical Summary
In the existing α-ketoleucine preparation process, the large amount of alkali, the large amount of acid, the low yield and the high cost.
Using the solid base catalyst PDVB-SO3Na, the reflux reaction of isobutylenehein and sodium hydroxide in deionized water, combined with sulfuric acid acidification, extraction and drying, α-ketoleucine is prepared, reducing the amount of sodium hydroxide and increasing the amount of sodium hydroxide. Yield rate.
It effectively reduces the amount of sodium hydroxide and sulfuric acid, increases the yield of α-ketoleucine, simplifies the reaction steps, reduces the preparation cost, and achieves high-purity products, suitable for industrial production.
Smart Images

Figure CN116891406B_ABST
Abstract
Description
Technical Field
[0001] The invention provides a method for preparing alpha-ketoleucine, and belongs to the technical field of drug production process innovation (organic compounds). Background Art
[0002] α-Ketoleucine, also known as 4-methyl-2-oxovaleric acid, plays an irreplaceable role in the synthesis of medicines and pesticides. It is an important raw material and intermediate for organic synthesis and is widely used in the synthesis of drugs for the treatment of tumors, hypertension, depression, glaucoma, sedatives, antibacterial agents and plant germination promoters. In recent years, chronic kidney disease (CKD) has shown a high incidence rate and a trend of younger patients, and has received increasing attention. The course of CKD progresses insidiously. Once it enters the late stage, the cost of treatment drugs and nursing will surge. Compound α-ketoacid tablets combined with a low-protein diet can delay the progression of renal failure. It has important value in the treatment of CKD and has gradually become the core means of CKD treatment. At present, in the market, compound α-ketoacid tablets are used as one of the drugs for the treatment of uremia. They provide essential amino acids for patients with kidney disease and minimize the intake of amino nitrogen. They have played a good role in slowing down the deterioration of renal function and have significant medical efficacy in the treatment of uremia. α-Ketoleucine is an important intermediate of calcium ketoleucine, which is one of the main components of compound α-ketoacid tablets. The currently disclosed α-ketoleucine preparation schemes are as follows: Keisuke Furukawa et al. mentioned in Org.Lett.2016,18,4230-4233 that α-hydroxy acid was used to prepare α-ketoleucine under the action of TEMPO, with a yield of 89%; CN104313071A mentioned a method of preparing α-ketoleucine by first reacting glycine with isobutyraldehyde and then regulating it with enzyme and ammonia water; CN 113735776 A mentioned a method of preparing α-ketoleucine under the action of a strong base (KOH, NaOH, LiOH) with twice the molar amount of isobutylene hydantoin under slight negative pressure; Ding Wei mentioned in his master's thesis "Synthesis of Several α-keto acids and α-keto acid salts by hydantoin method" a method of preparing α-ketoleucine with 20% of 5 times the molar amount of isobutylene hydantoin NaOH solution hydrolysis to obtain α-ketoleucine, the yield is 76.55%; in the current industrial production process, isobutylene hydantoin is still mainly hydrolyzed under alkaline conditions. This process has certain defects, such as excessive use of alkali, large amount of three wastes in the reaction, and high cost. Therefore, it is urgent to find a catalytic system to reduce the amount of alkali, simplify the reaction steps, and increase the yield of phenylpyruvic acid. Summary of the invention
[0003] In view of the problems in the prior art, the purpose of the present invention is to provide a method for preparing α-ketoleucine by using a solid base catalyst (PDVB-SO3Na) to reduce the amount of sodium hydroxide (NaOH) used, thereby reducing the amount of sulfuric acid (H2SO4) used during post-treatment.
[0004] The technical solution adopted by the present invention is as follows:
[0005] A method for preparing α-ketoleucine is characterized by comprising the following steps: using isobutylene hydantoin and sodium hydroxide as raw materials, using solid base PDVB-SO3Na as catalyst, using deionized water as solvent, reacting for 2 to 6 hours under reflux, acidifying with sulfuric acid after the reaction, extracting, and drying to obtain α-ketoleucine.
[0006] The reaction process involved in the present invention is as follows:
[0007]
[0008] Further preferred settings are:
[0009] In the reaction, the molar ratio of sodium hydroxide to isobutylene hydantoin is 1.1 to 2:1. Since the solid base (PDVB-SO3Na) is used as a catalyst to prepare α-ketoleucine, the yield of α-ketoleucine can be effectively improved while the amount of sodium hydroxide used can be greatly reduced.
[0010] The reaction conditions are as follows: the reaction is refluxed for 2 to 6 hours under magnetic stirring;
[0011] After the reaction is completed, the mixture is cooled to room temperature, filtered, acidified, extracted, concentrated and dried to obtain a white solid product, α-ketoleucine;
[0012] After the reaction is completed, the mixture is acidified with dilute sulfuric acid.
[0013] The catalyst in the reaction is solid base PDVB-SO3Na, and its usage is 3.0% to 6.5% of the mass of isobutylene hydantoin.
[0014] After the reaction is completed, the filtered solid base (PDVB-SO3Na) can be reused.
[0015] The solid base PDVB-SO3Na of the present invention is prepared by the following method:
[0016] (1) Polymerization: divinylbenzene and azobisisobutyronitrile are mixed and added into an autoclave, and then an appropriate amount of solvent is added, and the mixture is stirred thoroughly and then reacted at 80 to 120° C. for 12 to 36 hours. After the reaction is completed, the mixture is dried at room temperature to obtain a porous polymer;
[0017] (2) Sulfonation: After the porous polymer obtained in step (1) is fully expanded in dichloromethane, chlorosulfonic acid is added, and the reaction is carried out at 60-100° C. for 12-24 hours. After the reaction is completed, the mixture is filtered, washed and dried to obtain a sulfonated solid acid;
[0018] The preferred dosage of chlorosulfonic acid is 2-10 ml.
[0019] (3) Alkalization: adding the solid acid obtained in step (2) into a sodium hydroxide solution, reacting at 60-80° C. for 8 h, filtering and drying after the reaction to obtain a solid base.
[0020] The beneficial effects of the present invention are as follows:
[0021] 1. The present invention prepares a new solid base PDVB-SO3Na, which is used as a catalyst to prepare α-ketoleucine and has a very good catalytic effect. Compared with other catalysts, the solid base catalyst has better stability and reusability. In industrial production, the solid base catalyst is also widely used.
[0022] 2. Through experiments, it is found that the aforementioned solid base PDVB-SO3Na is used as a catalyst to prepare α-ketoleucine, which can be well recycled, thereby increasing the yield of α-ketoleucine and reducing the amount of sodium hydroxide and sulfuric acid used in the post-treatment process. The present invention solves the technical difficulties of large alkali and acid usage and low yield in the existing process.
[0023] 3. The present invention carries out the reaction at a relatively low temperature, thus avoiding the potential safety hazards caused by high temperature reactions, making it easy to control the reaction, and at the same time, the reaction operation process and post-processing are simple;
[0024] 4. The process provided by the invention is simple, the conditions are mild, the catalyst can be recycled, and the preparation cost is reduced while obtaining high-yield, high-purity products, showing better reaction advantages and economic advantages, and is more suitable for industrial production.
[0025] The present invention is further described below through the accompanying drawings and specific embodiments. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 This is a scanning electron microscope image of the solid acid PDVB-SO3H prepared in Example 1.
[0027] Figure 2 This is the infrared spectrum of the solid base PDVB-SO3Na catalyst prepared in Example 1 before and after alkalization.
[0028] Figure 3 This is the thermogravimetric analysis diagram of the solid base PDVB-SO3Na catalyst prepared in Example 1.
[0029] Figure 4 The hydrogen nuclear magnetic resonance spectrum of α-ketoleucine in Application Example 1 is shown in FIG. DETAILED DESCRIPTION
[0030] Example 1: Preparation of solid base (PDVB-SO3Na) catalyst
[0031] (1) Preparation of porous polymers
[0032] 2.0 g of divinylbenzene and 0.05 g of azobisisobutyronitrile were dissolved in 20 ml of tetrahydrofuran at room temperature, stirred thoroughly, and reacted at 100° C. for 24 h. After the reaction, the solid was filtered out and dried at room temperature to obtain 1.56 g of a porous polymer.
[0033] (2) Preparation of sulfonated solid acid PDVB-SO3H
[0034] Place 1 g of the porous polymer obtained in step (1) in a 250 ml three-necked flask, add 100 ml of dichloromethane, and after it is fully expanded, add 5 ml of chlorosulfonic acid (pure) and react at 80°C for 12 h. After the reaction is completed, filter out the solid, wash it with ethanol solution, and dry it to obtain 1.08 g of sulfonated solid acid (PDVB-SO3H).
[0035] (3) Preparation of solid base PDVB-SO3Na
[0036] 1 g of the sulfonated solid acid obtained in step (2) was added into a 50 ml three-necked flask, and then 20 ml of a 20% sodium hydroxide solution was added, and the mixture was reacted at 60° C. for 8 h. After the reaction was completed, the solid base was filtered, washed and dried to obtain a solid base.
[0037] Product characterization:
[0038] like Figure 1 The figure shows the SEM image of solid acid (PDVB-SO3H). Figure 2 This is a comparison of the infrared spectra of the solid base PDVB-SO3Na before and after alkalization; Figure 3 This is the thermogravimetric analysis diagram of the solid base PDVB-SO3Na.
[0039] Example 2-4: Preparation of sulfonated solid acid using different volumes of chlorosulfonic acid
[0040] The preparation method according to Example 1 is different in that in the preparation of the sulfonated solid acid (PDVB-SO3H) in step (2), the volume of 5 ml of chlorosulfonic acid is replaced by 2 ml, 3 ml, and 10 ml, and the other conditions remain unchanged. The solid base catalysts prepared with 2 ml, 3 ml, 5 ml, and 10 ml of chlorosulfonic acid are marked as PDVB-SO3Na-1, PDVB-SO3Na-2, PDVB-SO3Na-3, and PDVB-SO3Na-4, respectively.
[0041] Application Example 1: Application of Solid Base (PDVB-SO3Na) in the Preparation of α-Ketoleucine
[0042] In a 100ml three-necked flask, add 75mg of the solid base (PDVB-SO3Na-3) prepared in Example 1, then add 20ml of deionized water, and then add 0.6g (0.015mol) of sodium hydroxide and 1.54g (0.01mol) of isobutylene hydantoin in sequence, heat to reflux under magnetic stirring, and react for 4h. After the reaction is completed, cool to room temperature, filter with a Buchner funnel to obtain a solid base (PDVB-SO3Na-3), and recover the precipitated solid base for repeated use; the crude filtrate is acidified to pH 3 with dilute sulfuric acid, and filtered again with a Buchner funnel to remove impurities. The filtrate after the secondary filtration is extracted with ethyl acetate / water, the organic phases are combined, concentrated and dried to obtain a white solid product, namely α-ketoleucine, and the product is characterized as follows Figure 4 As shown: 1 H NMR (400MHz, DeuteriumOxide) δ2.54 (d, J = 7.0Hz, 2H), 2.03 (dh, J = 13.6, 6.8Hz, 1H), 0.86 (d, J = 6.7Hz, 6H).
[0043] Replacement Example 1-13
[0044] The preparation method is based on the application example 1, except that the NaOH dosage, catalyst dosage and catalyst type are adjusted, and their effects on the reaction are tested respectively, as shown in Table 1.
[0045] Table 1
[0046]
[0047]
[0048] According to Table 1, it can be seen that the comprehensive cost and yield situation show that the solid base (PDVB-SO3Na-3) has the best catalytic performance, and when the amount of the solid base (PDVB-SO3Na-3) is 5% (75 mg) of the mass of isobutylene hydantoin and the molar ratio of sodium hydroxide to isobutylene hydantoin is (1.5:1), the reaction yield is the highest, which is 91.8%.
[0049] Application Example 2: Catalyst Recycling
[0050] The solid base catalyst recovered by suction filtration in the application example was simply washed with ethanol and directly added to a 100 ml three-necked flask, and then 20 ml of deionized water, 0.6 g (0.015 mol) of sodium hydroxide, and 1.54 g (0.01 mol) of isobutylene hydantoin were added in sequence. The reaction conditions were consistent with those in application example 1. After the reaction was completed, the solid catalyst was continuously recovered and used for the next reaction. The product purification was consistent with that in application example, and the yield was calculated. This cycle was repeated for the fifth time, and the effects of different cycle times on the product yield were recorded, as shown in Table 2.
[0051] Table 2. Effect of cycle number on product yield
[0052] <![CDATA[Reuse times of solid base (PDVB-SO3Na-3) catalyst / times]]> Yield / % 1 91.8 2 91.3 3 91.0 4 90.2 5 90.3
[0053] As shown in Table 2:
[0054] The solid base (PDVB-SO3Na-3) of the present invention still has a very good catalytic effect after repeated use. After the fifth cycle, the yield can be maintained above 90%. It can be seen that the catalyst of the present invention can be recycled at least 5 times and has a good industrial application prospect.
[0055] Summarize:
[0056] 1. The present invention prepares a new solid base (PDVB-SO3Na), which can be used as a catalyst to prepare α-ketoleucine and has a very good catalytic effect.
[0057] 2. Through experiments, it was found that the aforementioned solid base (PDVB-SO3Na) was used as a catalyst to prepare α-ketoleucine, and it could be well recycled, thereby increasing the yield and reducing the amount of sodium hydroxide used in the reaction process and sulfuric acid used in post-treatment.
[0058] It is understood that the above specific description of the present invention is only used to illustrate the present invention and is not limited to the technical solutions described in the embodiments of the present invention. Those skilled in the art should understand that the present invention can still be modified or replaced by equivalents to achieve the same technical effects; as long as the use requirements are met, they are within the protection scope of the present invention.
Claims
1. A method for preparing α-ketoleucine, characterized in that: The following steps are involved: Using isobutylene hydantoin and sodium hydroxide as raw materials, solid base PDVB-SO3Na as catalyst, deionized water as solvent, reacting under reflux for 2 to 6 hours, and acidifying with sulfuric acid after the reaction to obtain α-ketoleucine; In the reaction, the catalyst is a solid base PDVB-SO3Na, and its amount is 3.0% to 6.5% of the mass of isobutylene hydantoin; After the reaction is completed, the filtered solid base PDVB-SO3Na is reused as a catalyst; The solid base PDVB-SO3Na is prepared by the following method: Polymerization: divinylbenzene and azobisisobutyronitrile are mixed and added into an autoclave, and then an appropriate amount of solvent is added, and the mixture is stirred thoroughly and then reacted at 80-120°C for 12-36 hours. After the reaction is completed, the mixture is dried at room temperature to obtain a porous polymer; Sulfonation: After the porous polymer obtained in step (1) is fully expanded in dichloromethane, chlorosulfonic acid is added, and the reaction is carried out at 60-100° C. for 12-24 hours. After the reaction is completed, the sulfonated solid acid is obtained by filtering, washing and drying; Alkalization: add the sulfonated solid acid obtained in step (2) into a sodium hydroxide solution, react at 60-80°C for 8-12 hours, filter and dry after the reaction to obtain a solid base.
2. The method for preparing α-ketoleucine according to claim 1, characterized in that: In the reaction, the molar ratio of sodium hydroxide to isobutylene hydantoin is 1.1 to 2:
1.
3. The method for preparing α-ketoleucine according to claim 1, characterized in that: In the reaction, the molar ratio of sodium hydroxide to isobutylene hydantoin is 1.5:
1.
4. The method for preparing α-ketoleucine according to claim 1, characterized in that: The reaction conditions are as follows: the reaction is carried out under reflux and magnetic stirring for 2 to 6 hours.
5. The method for preparing α-ketoleucine according to claim 1, characterized in that: After the reaction is completed, the mixture is cooled to room temperature, filtered, acidified with dilute sulfuric acid, extracted, concentrated and dried to obtain a white solid product, α-ketoleucine.
6. The method for preparing α-ketoleucine according to claim 1, characterized in that: In the reaction, the catalyst is solid base PDVB-SO3Na, and its usage is 5% of the mass of isobutylene hydantoin.