Composite film layer structure and manufacturing method thereof, and magnetic storage device

By employing a composite film structure in a spin orbital magnetic memory, including a first magnetic layer, a lattice separation layer, an induction layer, and a second magnetic layer, the problem of balancing thermal stability and write power consumption is solved, achieving both high thermal stability and low write power consumption.

CN118574503BActive Publication Date: 2024-11-19青岛海存微电子有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411046646.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-01
Publication Date
2024-11-19
Estimated Expiration
2044-08-01

AI Technical Summary

Technical Problem

Existing spin-orbit magnetic memory (SOT-MRAM) struggles to balance improving thermal stability and reducing write power consumption, especially the MTJs of perpendicular magnetic anisotropy (PMA) and in-plane magnetic anisotropy (IMA) types, which present challenges in simultaneously achieving both thermal stability and write power efficiency.

Method used

A composite film structure is adopted, including a first magnetic layer, a lattice separation layer, an induction layer, and a second magnetic layer. The thermal stability is improved by increasing the thickness of the second magnetic layer, the write power consumption is reduced by decreasing the thickness of the first magnetic layer, and the coupling and synchronous flipping are enhanced by the design of the induction layer, thereby reducing the equivalent magnetization.

Benefits of technology

This achieves improved thermal stability and reduced write power consumption in spin orbital magnetic memories, enhancing write efficiency and improving device performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118574503B_ABST
    Figure CN118574503B_ABST
Patent Text Reader

Abstract

The present application provides a composite film layer structure and a manufacturing method thereof, and a magnetic memory, which relates to the field of semiconductor technology and is used to solve the technical problem that it is difficult to simultaneously improve thermal stability and reduce write power. The composite film layer structure includes a first magnetic layer, a lattice separation layer, an induction layer, and a second magnetic layer; the first magnetic layer, the lattice separation layer, and the second magnetic layer are stacked in sequence, the induction layer includes at least one island-shaped split or the induction layer is a continuous film layer with different thicknesses at both ends, the induction layer is arranged on the first magnetic layer, and / or, is arranged on the side of the first magnetic layer facing the lattice separation layer. The induction layer and the lattice separation layer cooperate to enhance the coupling between the first magnetic layer and the second magnetic layer, and reduce the influence of the lattice structure between the two, so that the first magnetic layer and the second magnetic layer can be flipped more synchronously, thereby improving the writing efficiency. The contact between the induction layer and the lattice separation layer can alleviate the unevenness of the surface of the induction layer and further improve the performance of the device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of semiconductor technology, and in particular to a composite film layer structure and a manufacturing method thereof, and a magnetic memory. Background Art

[0002] Spin Orbit Torque-Magnetic Random Access Memory (SOT-MRAM) has the advantages of non-volatility, high-speed and low-power data writing (<1 ns, <~0.1 pJ / bit) and high device durability. It is a key technology that is expected to break through the power consumption bottleneck of integrated circuits in the post-Moore era.

[0003] The spin-orbit torque magnetic memory includes a magnetic tunnel junction (MTJ) for storing data and a spin-orbit torque (SOT) bottom electrode layer for providing a spin-orbit torque (SOT) to write data. Among them, the core structure of the MTJ includes a fixed layer formed by a ferromagnetic (FM) metal, a barrier layer formed by an oxide, and a free layer formed by a ferromagnetic metal. The direction of the magnetic moment of the free layer can be changed by external excitation (such as the SOT bottom electrode layer), thereby switching in the two directions of the easy magnetization axis. The direction of the magnetic moment of the fixed layer is not easily changed by external excitation, so it is fixed in a certain direction. When the free layer is parallel to the direction of the magnetic moment of the fixed layer, the MTJ presents a low resistance state; when the free layer is antiparallel to the direction of the magnetic moment of the fixed layer, the MTJ presents a high resistance state. In this way, the high and low resistance states of the MTJ can be used to store data "1" and "0" accordingly.

[0004] The free layer of MTJ can be perpendicular magnetic anisotropy (PMA) or in-plane magnetic anisotropy (IMA). Magnetic memories with the above two forms of free layers have the problem of difficulty in taking both thermal stability and writing power into consideration at the same time. Summary of the invention

[0005] In view of the above problems, the embodiments of the present application provide a composite film layer structure and a manufacturing method thereof, and a magnetic memory to improve thermal stability and reduce write power consumption.

[0006] According to some embodiments, the present application provides a composite film layer structure, which includes: a first magnetic layer, a lattice separation layer, an induction layer, and a second magnetic layer;

[0007] The first magnetic layer, the lattice separation layer and the second magnetic layer are stacked in sequence, the induction layer includes at least one island-shaped split body or the induction layer is a continuous film layer with different thicknesses at both ends; the induction layer is arranged in the first magnetic layer, and / or, is arranged on the side of the first magnetic layer facing the lattice separation layer.

[0008] In some possible implementations, the thickness of the first magnetic layer is smaller than the thickness of the second magnetic layer.

[0009] In some possible implementations, a lattice structure of the first magnetic layer is different from a lattice structure of the second magnetic layer.

[0010] In some possible implementations, at least a portion of the induction layer is in contact with the lattice separation layer.

[0011] In some possible implementations, the thicknesses of the lattice separation layer at two ends are different.

[0012] In some possible implementations, the induction layer includes at least two island-shaped splits, at least some of the island-shaped splits are arranged in parallel, and among the island-shaped splits arranged in parallel, the two island-shaped splits located at two ends have different thicknesses.

[0013] The composite film structure provided by the embodiment of the present application has at least the following advantages:

[0014] The composite film layer structure provided in the embodiment of the present application includes a first magnetic layer, a lattice separation layer, an induction layer and a second magnetic layer. The first magnetic layer, the lattice separation layer and the second magnetic layer are stacked in sequence. By increasing the thickness of the second magnetic layer, the thermal stability can be improved, and by reducing the thickness of the first magnetic layer, the write power consumption can be reduced. The induction layer includes at least one island-shaped split or the induction layer is a continuous film layer with different thicknesses at both ends. On the one hand, it can reduce the influence on the lattice structure of the second magnetic layer, and on the other hand, it makes the second magnetic layer and the first magnetic layer closer in some places, which can enhance the coupling between the first magnetic layer and the second magnetic layer, so that the first magnetic layer and the second magnetic layer can be more synchronously flipped, thereby improving the write efficiency. The induction layer is arranged on the first magnetic layer, and / or, on the side of the first magnetic layer facing the lattice separation layer. The induction layer is in contact with the first magnetic layer, which can reduce the equivalent magnetization of the first magnetic layer, thereby further reducing the write power consumption; the induction layer is in contact with the lattice separation layer, which can alleviate the unevenness of the surface of the induction layer, thereby further improving the device performance.

[0015] According to some embodiments, the present application also provides a magnetic memory, comprising: a free layer, a reference layer, and a barrier layer disposed between the free layer and the reference layer;

[0016] At least one of the free layer and the reference layer includes the composite film layer structure as described above, and the second magnetic layer of the composite film layer structure is adjacent to the barrier layer.

[0017] In some possible implementations, the lattice structure of the first magnetic layer of the composite film layer structure is different from the lattice structure of the barrier layer.

[0018] The magnetic memory provided by the embodiment of the present application includes: a free layer, a reference layer and a barrier layer. The barrier layer is arranged between the free layer and the reference layer. At least one of the free layer and the reference layer includes the above-mentioned composite film layer structure, and the second magnetic layer of the composite film layer structure is adjacent to the barrier layer. The magnetic memory includes the composite film layer structure, which has at least the advantages of good thermal stability and low write power consumption.

[0019] According to some embodiments, the present application also provides a method for manufacturing a composite film layer structure, which includes:

[0020] forming a first magnetic layer, a lattice separation layer, an induction layer, and a second magnetic layer, wherein the lattice separation layer is formed on a side of the second magnetic layer close to the induction layer, the induction layer includes at least one island-shaped split body or the induction layer is a continuous film layer with different thicknesses at both ends, and the induction layer is formed in the first magnetic layer and / or formed on a side of the first magnetic layer facing the lattice separation layer;

[0021] The first magnetic layer, the lattice separation layer, the induction layer and the second magnetic layer form the composite film layer structure;

[0022] In some possible implementations, the induction layer is formed by a sputtering process, and at least one of a sputtering time and a sputtering angle is controlled so that the thickness of the induction layer at two ends is different.

[0023] The method for manufacturing the composite film layer structure provided in the embodiment of the present application has at least the following advantages:

[0024] In the method for manufacturing the composite film layer structure provided in the embodiment of the present application, a first magnetic layer, a lattice separation layer, an induction layer and a second magnetic layer are formed. By increasing the thickness of the second magnetic layer, the thermal stability can be improved, and by reducing the thickness of the first magnetic layer, the write power consumption can be reduced. The lattice separation layer is arranged on the first magnetic layer, and the induction layer includes at least one island-shaped split or the induction layer is a continuous film layer with different thicknesses at both ends, which can reduce the influence on the lattice structure of the second magnetic layer, and make the second magnetic layer closer to the first magnetic layer in some places, which can enhance the coupling between the first magnetic layer and the second magnetic layer, so that the first magnetic layer and the second magnetic layer can be more synchronously flipped, and the write efficiency is improved. The induction layer is arranged in the first magnetic layer, and / or, arranged on the side of the first magnetic layer facing the lattice separation layer. The induction layer is in contact with the first magnetic layer, which can reduce the equivalent magnetization of the first magnetic layer, thereby further reducing the write power consumption. The induction layer is in contact with the lattice separation layer, which can alleviate the unevenness of the surface of the induction layer and further improve the performance of the device. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 A schematic diagram of a magnetic storage device in the related art;

[0026] Figure 2 for Figure 1 A top view of

[0027] Figure 3 Another schematic diagram of a magnetic storage device in the related art;

[0028] Figure 4 for Figure 3 A top view of

[0029] Figure 5 A schematic diagram of a first structure of a magnetic memory in an embodiment of the present application;

[0030] Figure 6 A second structural schematic diagram of a magnetic memory in an embodiment of the present application;

[0031] Figure 7 A comparison diagram of the write voltages of a magnetic memory in an embodiment of the present application and a magnetic memory with a traditional structure;

[0032] Figure 8 A third structural schematic diagram of a magnetic memory in an embodiment of the present application;

[0033] Fig. 9 A fourth structural schematic diagram of a magnetic memory in an embodiment of the present application;

[0034] Fig.10 A fifth structural schematic diagram of a magnetic memory in an embodiment of the present application;

[0035] Fig.11 A sixth structural schematic diagram of a magnetic memory in an embodiment of the present application;

[0036] Fig.12 Schematic diagram of the seventh structure of the magnetic memory in one embodiment of the present application;

[0037] Fig.13 The figure is a comparison diagram of the tunnel magnetoresistance of the magnetic memory in one embodiment of the present application and the magnetic memory with a traditional structure.

[0038] Description of reference numerals:

[0039] 1-MTJ; 10-SOT layer;

[0040] 20-free layer; 30-barrier layer;

[0041] 40-reference layer; 51-first magnetic layer;

[0042] 52- lattice separation layer; 53- induction layer;

[0043] 54-a second magnetic layer; 60-a synthetic antiferromagnetic layer;

[0044] 70-pinning layer; 80-top electrode. DETAILED DESCRIPTION

[0045] There is a problem in the related technology that it is difficult to balance improving thermal stability and reducing writing power consumption. After research, it was found that: Figure 1 and Figure 2 When the free layer 20 has PMA, the magnetic moment of the free layer 20 is in the vertical direction ( Figure 1 At this time, the thermal stability of the free layer 20 (also the MTJ) is provided by PMA, such as Figure 2 As shown, the MTJ can be prepared into a cylindrical shape. In order to ensure the thermal stability of the PMA-MTJ, the PMA strength of the free layer 20 needs to be enhanced, which will increase the write power consumption.

[0046] See also Figure 3 and Figure 4 When the free layer 20 has IMA, the magnetic moment of the free layer 20 is in the in-plane direction ( Figure 3 In order to make the free layer 20 have sufficient thermal stability, the MTJ needs to be prepared into an elliptical column or a rectangular parallelepiped. Figure 4As shown, when the MTJ is an elliptical column, the easy magnetization axis of the magnetic moment of the free layer 20 is the long axis of the ellipse. In order to ensure the thermal stability of the IMA-MTJ, on the one hand, the ratio of the length of the long and short axes of the ellipse or the aspect ratio of the rectangle needs to reach 3~4, or even larger, which limits the miniaturization capability of the IMA-MTJ. On the other hand, the thickness of the free layer 20 needs to be thickened, which will also increase the write power consumption.

[0047] The embodiments of the present application provide a composite film layer structure, a method for manufacturing the same, and a magnetic memory. The composite film layer structure includes a first magnetic layer, a lattice separation layer, and a second magnetic layer that are stacked. The thermal stability can be improved by increasing the thickness of the second magnetic layer, and the write power consumption can be reduced by reducing the thickness of the first magnetic layer.

[0048] The composite film layer structure also includes an induction layer, which includes at least two island-shaped splits arranged in parallel or the induction layer is a continuous film layer with different thicknesses at both ends. On the one hand, it can reduce the impact on the lattice structure of the second magnetic layer, and on the other hand, it makes the second magnetic layer and the first magnetic layer closer in some places, which can enhance the coupling between the first magnetic layer and the second magnetic layer, so that the first magnetic layer and the second magnetic layer can be flipped more synchronously, thereby improving writing efficiency.

[0049] The induction layer is arranged on the first magnetic layer, and / or arranged on the side of the first magnetic layer facing the lattice separation layer. The induction layer is in contact with the first magnetic layer, and the induction layer can be used to reduce the equivalent magnetization intensity of the first magnetic layer, thereby further reducing the write power consumption. The induction layer is in contact with the lattice separation layer, which can alleviate the unevenness of the surface of the induction layer and further improve the device performance.

[0050] In order to make the above-mentioned purposes, features and advantages of the embodiments of the present application more obvious and understandable, the technical solutions in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work belong to the scope of protection of this application.

[0051] See also Figures 5 to 12 The embodiment of the present application provides a composite film structure, which includes: a first magnetic layer 51, a lattice separation layer 52, an induction layer 53 and a second magnetic layer 54. The first magnetic layer 51, the lattice separation layer 52 and the second magnetic layer 54 are stacked in sequence, the lattice separation layer 52 is arranged on a surface of one side of the first magnetic layer 51, and the second magnetic layer 54 is arranged on a surface of the lattice separation layer 52 away from the first magnetic layer 51.

[0052] In the above composite film layer structure, the second magnetic layer 54 provides high thermal stability, and the first magnetic layer 51 reduces write power consumption. In some possible implementation methods, the thickness of the first magnetic layer 51 is less than the thickness of the second magnetic layer 54. Increasing the thickness of the second magnetic layer 54 can improve thermal stability, and reducing the thickness of the first magnetic layer 51 can reduce write power consumption. The thickness direction of the second magnetic layer 54 and the first magnetic layer 51 is the stacking direction of the second magnetic layer 54, the lattice separation layer 52 and the second magnetic layer 54 ( Figure 5 Z direction as shown).

[0053] The lattice structures of the first magnetic layer 51 and the second magnetic layer 54 are different. In order to achieve a high read margin, that is, to achieve a high tunnel magnetoresistance (TMR), the second magnetic layer 54 needs to form a specific lattice structure, which is different from the lattice structure of the SOT layer 10. The lattice structure of the first magnetic layer 51 will be affected by the lattice structure of the SOT layer 10, so that the lattice structure of the first magnetic layer 51 is different from the lattice structure of the second magnetic layer 54. Among them, the materials of the first magnetic layer 51 and the second magnetic layer 54 both include ferromagnetic materials, such as one or more combinations of Co, Fe, Ni, CoFe, CoFeB, FeB, CoB, NiFe, Co / Ni, Co / Pt, etc.

[0054] Continue reading Figures 5 to 12 The lattice separation layer 52 is disposed between the first magnetic layer 51 and the second magnetic layer 54, and is in contact with the first magnetic layer 51 and the second magnetic layer 54, respectively. By disposing the lattice separation layer 52, the mutual influence between the lattice of the first magnetic layer 51 and the lattice of the second magnetic layer 54 can be isolated, thereby improving the thermal stability and read margin of the MTJ.

[0055] The thickness of the two ends of the lattice separation layer 52 may be different, that is, the thickness of one end of the lattice separation layer 52 is greater than the thickness of the other end. Fig. 9 As shown, the thickness of the lattice separation layer 52 gradually increases from one end to the other end of the lattice separation layer 52. In this way, the lattice separation layer 52 is adapted to the induction layer 53, so that the lattice separation layer 52 is away from the surface level of the first magnetic layer 51, so that other film layers formed on the lattice separation layer 52 remain horizontal, thereby improving the performance of the entire film stack.

[0056] The material of the lattice separation layer 52 may include an amorphous material, such as TaB, WB, or Ta, etc. Alternatively, the material of the lattice separation layer 52 may be a material having the same lattice structure as the second magnetic layer 54, that is, the lattice structure of the lattice separation layer 52 is the same as the lattice structure of the second magnetic layer 54, but the material is different, so that the lattice separation layer 52 serves as a sacrificial layer of the second magnetic layer 54, alleviating the influence of the lattice structure of the first magnetic layer 51 on the lattice structure of the second magnetic layer 54.

[0057] Continue reading Figures 5 to 12 The induction layer 53 includes at least one island-shaped body or the induction layer 53 is a continuous film layer with different thicknesses at both ends. The induction layer 53 is arranged on the first magnetic layer 51, and / or, is arranged on the side of the first magnetic layer 51 facing the lattice separation layer 52. The material of the induction layer 53 is a material with strong anisotropy, such as metals such as Ta, W, Ru, and Mo.

[0058] By providing the induction layer 53 and the induction layer 53 being in contact with the first magnetic layer 51, the equivalent magnetization intensity of the first magnetic layer 51 can be reduced, thereby further reducing the write power consumption. The induction layer 53 is in contact with the lattice separation layer 52, which can alleviate the unevenness of the surface of the induction layer 53 and further improve the device performance.

[0059] There are many options for the position of the induction layer 53 relative to the first magnetic layer 51. For example, Figure 5 and Fig.11 As shown, the induction layer 53 can be disposed on the first magnetic layer 51. As another example, Figure 6 , Fig. 9 , Fig.10 and Fig.12 As shown, the induction layer 53 can be disposed on the side of the first magnetic layer 51 facing the lattice separation layer 52. As another example, Figure 8 As shown, the induction layer 53 can be disposed on the first magnetic layer 51 and on a side of the first magnetic layer 51 facing the lattice separation layer 52 , that is, the induction layer 53 can be disposed in multiple locations.

[0060] In some possible examples, the induction layer 53 includes at least two island-shaped splits, and at least some of the island-shaped splits are arranged in parallel so that they are arranged in the same layer, for example, all the island-shaped splits are arranged in parallel. In order to achieve a high reading margin, the second magnetic layer 54 must form a specific lattice structure, and the lattice structure of the induction layer 53 is different. At least some of the island-shaped splits are arranged in parallel, which can reduce the impact on the upper lattice structure (i.e., the lattice structure of the second magnetic layer 54) on the one hand, and make the second magnetic layer 54 and the first magnetic layer 51 closer in some places on the other hand, which can enhance the coupling between the first magnetic layer 51 and the second magnetic layer 54. When the current is written, the first magnetic layer 51 and the second magnetic layer 54 can be flipped more synchronously, thereby improving the writing efficiency.

[0061] In some possible implementations, such as Figure 5 As shown, the induction layer 53 includes at least two island-shaped segments, all of which are arranged in parallel, and these island-shaped segments can all be set on the first magnetic layer 51.

[0062] In some other possible implementations, such as Figure 6 As shown, the induction layer 53 includes at least two island-shaped segments, all of which are arranged in parallel. These island-shaped segments can be arranged on the side of the first magnetic layer 51 facing the lattice separation layer 52. Figure 7 , "1" in the horizontal axis represents a magnetic memory with a conventional structure, and "2" represents a magnetic memory with a composite film layer structure according to an embodiment of the present application. The composite film layer structure of the magnetic memory is as shown in FIG. Figure 6 As shown. Figure 7 As shown, compared with the magnetic memory of the conventional structure, the write voltage V C reduce.

[0063] In another possible implementation, Figure 8 As shown, the induction layer 53 includes at least four island-shaped splits, some of which are arranged on the side of the first magnetic layer 51 facing the lattice separation layer 52 and are arranged in parallel on the corresponding side of the first magnetic layer 51, and another part of the island-shaped splits are arranged in the first magnetic layer 51 and are arranged in parallel on the first magnetic layer 51.

[0064] Specifically, at least two island-shaped bodies are arranged in parallel on the side of the first magnetic layer 51 facing the lattice separation layer 52. The surface of the lattice separation layer 52 facing away from the first magnetic layer 51 is higher than the surface of these island-shaped bodies facing away from the first magnetic layer 51, so that the lattice separation layer 52 is isolated between these island-shaped bodies and the second magnetic layer 54, and these island-shaped bodies are prevented from contacting the second magnetic layer 54. At least two island-shaped bodies are arranged in parallel on the first magnetic layer 51, and the first magnetic layer 51 covers these island-shaped bodies.

[0065] It can be understood that the number and arrangement of the island-like splits can have various forms. Exemplarily, the induction layer 53 includes at least three island-like splits, one of which is arranged between the first magnetic layer 51 and the lattice separation layer 52, and the remaining island-like splits are arranged in parallel in the first magnetic layer 51; or, one of the island-like splits is arranged in the first magnetic layer 51, and the remaining island-like splits are arranged in parallel between the first magnetic layer 51 and the lattice separation layer 52.

[0066] In the above example, at least part of the induction layer 53 is also in contact with the lattice separation layer 52. The lattice separation layer 52 can alleviate the unevenness of the surface of the induction layer, so that the device performance is further improved. The induction layer 53 is located on the side of the first magnetic layer 51 facing the lattice separation layer 52, and the induction layer 53 is located between the first magnetic layer 51 and the lattice separation layer 52, and is in contact with both the first magnetic layer 51 and the lattice separation layer 52. At this time, all the induction layers 53 are in contact with the lattice separation layer 52.

[0067] When the induction layer 53 is located on the first magnetic layer 51, the surface of the induction layer 53 is exposed to the corresponding surface of the first magnetic layer 51, so that the induction layer 53 can contact the lattice separation layer 52. At this time, at least part of the induction layer 53 is in contact with the lattice separation layer 52. Exemplarily, the induction layer 53 includes at least one island-shaped split body, all the island-shaped split bodies are in contact with the lattice separation layer 52, or part of the island-shaped split bodies are in contact with the lattice separation layer 52.

[0068] When the induction layer 53 is located at the first magnetic layer 51 and the side of the first magnetic layer 51 facing the lattice separation layer 52 , the induction layer 53 in the first magnetic layer 51 may be exposed or not. At this time, at least part of the induction layer 53 is in contact with the lattice separation layer 52 .

[0069] In some possible examples, the induction layer 53 includes at least two island-shaped splits, at least some of which are arranged in parallel, for example, all of the island-shaped splits are arranged in parallel, or at least two of all the island-shaped splits are arranged in parallel. Among the island-shaped splits arranged in parallel, the thickness of the two island-shaped splits at the two ends is different.

[0070] For example, Fig.10 and Fig.11 As shown, along the arrangement direction of the island-shaped splits, that is, along the direction from one end to the other end of the induction layer 53, the thickness of these island-shaped splits increases successively, so that the thickness of the island-shaped splits at both ends is different. In this way, at least two island-shaped splits form a slope, so that the components of the island-shaped splits at one end are more, and the components of the island-shaped splits at the other end are less, so that the end of the first magnetic layer 51 corresponding to the island-shaped split with a smaller thickness is easier to flip, thereby driving the other end to flip, and further reducing the write power consumption.

[0071] By controlling the growth process of the island-like bodies, the thickness of the island-like bodies can be controlled. Fig.10 and Fig.11 As shown, the induction layer 53 is formed by a magnetron sputtering process, and the thickness of each island-shaped body can be controlled by controlling at least one of the sputtering time and / or the sputtering angle. For example, the longer the sputtering time, the greater the thickness of the island-shaped body.

[0072] In other possible examples, such as Fig. 9 As shown, the induction layer 53 is a continuous film layer, and the thickness of the two ends is different. Exemplarily, the thickness of the continuous film layer gradually increases from one end to the other end of the continuous film layer, that is, the continuous film layer is wedge-shaped. In this way, the induction layer 53 has a certain slope, and the thickness of the induction layer 53 at different positions is different, so that the equivalent anisotropy field and equivalent magnetization of the first magnetic layer 51 are different. The end with a smaller equivalent magnetization is easier to flip, thereby driving the other end to flip, further reducing the write power consumption.

[0073] The continuous film layer is arranged on the side of the first magnetic layer 51 facing the lattice separation layer 52, that is, the continuous film layer is arranged between the first magnetic layer 51 and the lattice separation layer 52, so as to facilitate the production of the composite film layer structure. Among them, the thickness of the lattice separation layer 52 is also different to adapt to the continuous film layer. Fig. 9 As shown, the total thickness of the lattice separation layer 52 and the continuous film layer is consistent.

[0074] It can be understood that in the above two examples, the use of the lattice separation layer 52 can alleviate the unevenness and unevenness of the surface of the induction layer 53, so that the performance of the entire composite film layer structure is better. In addition, the lattice separation layer 52 combined with the induction layer 53 can improve thermal stability while reducing write power consumption, that is, it can reduce the write voltage of the magnetic memory and improve tunneling magnetoresistance.

[0075] In summary, the composite film layer structure in the embodiment of the present application includes a first magnetic layer 51, a lattice separation layer 52, an induction layer 53 and a second magnetic layer 54. The first magnetic layer 51, the lattice separation layer 52 and the second magnetic layer 54 are stacked in sequence. By increasing the thickness of the second magnetic layer 54, the thermal stability can be improved, and by reducing the thickness of the first magnetic layer 51, the write power consumption can be reduced. The induction layer 53 includes at least one island-shaped split arranged in parallel or the induction layer 53 is a continuous film layer with different thicknesses at both ends. On the one hand, it can reduce the influence on the lattice structure of the second magnetic layer 54, and on the other hand, it makes the second magnetic layer 54 and the first magnetic layer 51 closer in some places, which can enhance the coupling between the first magnetic layer 51 and the second magnetic layer 54, so that the first magnetic layer 51 and the second magnetic layer 54 can be more synchronously flipped, thereby improving the write efficiency. The induction layer 53 is arranged in the first magnetic layer 51, and / or, it is arranged on the side of the first magnetic layer 51 facing the lattice separation layer 52. The induction layer 53 contacts the first magnetic layer 51, which can reduce the equivalent magnetization intensity of the first magnetic layer 51, thereby further reducing the write power consumption. The induction layer 53 contacts the lattice separation layer 52, which can alleviate the unevenness of the surface of the induction layer 53, thereby further improving the device performance.

[0076] See also Figures 5 to 12The embodiment of the present application further provides a magnetic memory, which includes a free layer 20, a reference layer 40, and a barrier layer 30 disposed between the free layer 20 and the reference layer 40. At least one of the free layer 20 and the reference layer 40 includes the above-mentioned composite film layer structure, and the second magnetic layer 54 of the composite film layer structure is adjacent to the barrier layer 30.

[0077] The free layer 20, the barrier layer 30 and the reference layer 40 are stacked in sequence, and the material of the barrier layer 30 can be an oxide. At least one of the free layer 20 and the reference layer 40 includes a composite film layer structure to improve the thermal stability of the magnetic memory and reduce write power consumption. Preferably, at least the free layer 20 includes a composite film layer structure, so that the free layer 20 is easier to flip, further reducing write power consumption.

[0078] In some possible examples, the free layer 20 includes a composite film layer structure, and the material of the reference layer 40 can be one or more combinations of Co, Fe, Ni, CoFe, CoFeB, FeB, CoB, NiFe, Co / Ni, Co / Pt, etc.

[0079] For other possible examples, see Fig.12 The reference layer 40 includes a composite film structure, and the material of the free layer 20 can be one or more combinations of Co, Fe, Ni, CoFe, CoFeB, FeB, CoB, NiFe, Co / Ni, Co / Pt, etc. Fig.13 , "1" in the horizontal axis represents a magnetic memory with a conventional structure, and "2" represents a magnetic memory with a composite film layer structure according to an embodiment of the present application. The composite film layer structure of the magnetic memory is as shown in FIG. Fig.12 Compared with the magnetic memory of the conventional structure, the tunnel magnetoresistance (TMR) of the magnetic memory having the composite film layer structure of the embodiment of the present application is increased.

[0080] The lattice structure of the first magnetic layer 51 in the composite film layer structure is different from the lattice structure of the barrier layer 30, wherein the lattice structure of the second magnetic layer 54 is specific to improve the tunneling magnetic resistance, the barrier layer 30 is in contact with the second magnetic layer 54, and the lattice structure of the barrier layer 30 and the lattice structure of the second magnetic layer 54 influence each other, which is different from the lattice structure of the first magnetic layer 51.

[0081] Continue reading Figures 5 to 12 The magnetic memory further includes a SOT layer 10 disposed on the side of the free layer 20 away from the barrier layer 30. The SOT layer 10 may be a single layer or a multilayer. The material of the SOT layer 10 includes heavy metal materials such as platinum, palladium, hafnium, gold, tantalum, tungsten, iridium, and their alloys, oxides, nitrides, borides, etc. The material of the SOT layer 10 may also include Bi x Se1-x 、Bi x Sb 1-x , topological insulators such as (Bi,Sb)2Te3, and two-dimensional materials such as MoS2 and WTe2.

[0082] In some possible examples, the magnetic memory further includes a synthetic antiferromagnetic layer 60 disposed on the side of the reference layer 40 away from the barrier layer 30. The synthetic antiferromagnetic layer 60 includes two ferromagnetic layers and a coupling layer disposed between the two ferromagnetic layers, and the magnetization directions of the two ferromagnetic layers are arranged in antiparallel. The material of the coupling layer may include metals such as Ta, Ir, W, Ru, and Pt. The material of the ferromagnetic layer includes one or more combinations of Co, Fe, Ni, CoFe, CoFeB, FeB, CoB, NiFe, Co / Ni, and Co / Pt, for example, the ferromagnetic layer is a Co / Pt multilayer film. The material of the coupling layer includes a manganese alloy, such as IrMn, PtMn, NiMn, FeMn, and the like.

[0083] The magnetic memory may further include a pinning layer 70 disposed on the side of the synthetic antiferromagnetic layer 60 away from the barrier layer 30, for pinning the ferromagnetic layer in the synthetic antiferromagnetic layer 60 in a fixed direction. For example, the pinning layer 70 pins the magnetization direction of the ferromagnetic layer adjacent to the pinning layer 70 in the direction of its long axis. The pinning layer 70 may be a laminate, including a ferromagnetic material layer and a non-ferromagnetic material layer, and the ferromagnetic material layer and the non-ferromagnetic material layer are alternately stacked. For example, the pinning layer 70 includes two opposite ferromagnetic material layers, and a non-ferromagnetic material layer disposed between the two ferromagnetic material layers.

[0084] The magnetic memory may further include a top electrode 80 disposed on the side of the pinned layer 70 away from the barrier layer 30. The top electrode 80 serves as a reading channel and may be a single layer or a plurality of stacked film layers. Exemplarily, the top electrode 80 is a metal layer, or the top electrode 80 includes a plurality of film layers of tantalum / ruthenium / tantalum (Ta / Ru / Ta), or a plurality of film layers of tantalum / copper nitride / tantalum (Ta / CuN / Ta).

[0085] The magnetic memory in the embodiment of the present application includes: a free layer 20, a reference layer 40 and a barrier layer 30, wherein the barrier layer 30 is disposed between the free layer 20 and the reference layer 40. At least one of the free layer 20 and the reference layer 40 includes the above-mentioned composite film layer structure, and the second magnetic layer 54 of the composite film layer structure is adjacent to the barrier layer 30. The magnetic memory includes a composite film layer structure, which has at least the advantages of good thermal stability and low write power consumption.

[0086] The embodiment of the present application also provides a method for manufacturing a composite film layer structure, at least the free layer 20 includes the composite film layer structure. The method for manufacturing the composite film layer structure specifically includes the following steps: forming a first magnetic layer 51, a lattice separation layer 52, an induction layer 53, and a second magnetic layer 54; the lattice separation layer 52 is formed on a side of the second magnetic layer 54 close to the induction layer 53, and the induction layer 53 includes at least one island-shaped split body or the induction layer 53 is a continuous film layer with different thicknesses at both ends; the induction layer 53 is formed in the first magnetic layer 51, and / or, is formed on a side of the first magnetic layer 51 facing the lattice separation layer 52; the first magnetic layer 51, the lattice separation layer 52, the induction layer 53, and the second magnetic layer 54 form a composite film layer structure.

[0087] The first magnetic layer 51 can reduce the writing power consumption, for example, reducing the thickness of the first magnetic layer 51 can reduce the writing power consumption. The first magnetic layer 51 can be a uniform thickness film layer, and the material of the first magnetic layer 51 includes ferromagnetic materials, such as Co, Fe, Ni, CoFe, CoFeB, FeB, CoB, NiFe, Co / Ni, Co / Pt and one or more combinations thereof.

[0088] The second magnetic layer 54 can provide high thermal stability. For example, increasing the thickness of the second magnetic layer 54 can improve the thermal stability. The thickness of the second magnetic layer 54 can be greater than the thickness of the first magnetic layer 51. The thickness direction of the second magnetic layer 54 and the first magnetic layer 51 is the stacking direction of the second magnetic layer 54, the lattice separation layer 52 and the second magnetic layer 54 ( Figure 5 Z direction as shown).

[0089] The second magnetic layer 54 has a different lattice structure from the first magnetic layer 51. The second magnetic layer 54 is spaced apart from the first magnetic layer 51, for example, a lattice separation layer 52 is provided, or a lattice separation layer 52 and an induction layer 53 are provided. The second magnetic layer 54 can be a uniform thickness film layer. The material of the second magnetic layer 54 includes ferromagnetic materials, such as one or more combinations of Co, Fe, Ni, CoFe, CoFeB, FeB, CoB, NiFe, Co / Ni, Co / Pt, etc.

[0090] The lattice separation layer 52 is formed on the side of the second magnetic layer 54 close to the induction layer 53, that is, the lattice separation layer 52 is located between the first magnetic layer 51 and the second magnetic layer 54, and is used to isolate the first magnetic layer 51 and the film layer above the lattice separation layer 52, so as to reduce the mutual influence of the lattice structure of the film layer on both sides of the lattice separation layer 52, and improve the thermal stability and reading margin. The material of the lattice separation layer 52 may include an amorphous material, such as TaB, WB, or Ta. Alternatively, the material of the lattice separation layer 52 may be a material with the same lattice structure as the film layer on the side of the lattice separation layer 52 away from the first magnetic layer 51.

[0091] The thickness of the two ends of the lattice separation layer 52 may be different, that is, the thickness of one end of the lattice separation layer 52 is greater than the thickness of the other end. Exemplarily, the thickness of the lattice separation layer 52 gradually increases along the direction from one end to the other end of the lattice separation layer 52. In this way, the lattice separation layer 52 is adapted to the induction layer 53, so that the lattice separation layer 52 is away from the surface level of the first magnetic layer 51, so that other film layers formed on the lattice separation layer 52 remain horizontal, thereby improving the performance of the entire film stack.

[0092] See also Figure 5 and Fig.11 The induction layer 53 can be disposed in the first magnetic layer 51, that is, the induction layer 53 is embedded in the middle of the first magnetic layer 51, and the first magnetic layer 51 completely covers the induction layer 53. Figure 6 , Fig. 9 and Fig.10 The induction layer 53 can be disposed on the side of the first magnetic layer 51 facing the lattice separation layer 52, that is, the induction layer 53 is disposed between the first magnetic layer 51 and the lattice separation layer 52. Figure 8 One induction layer 53 can be arranged in the first magnetic layer 51, and another induction layer 53 can be arranged on the side of the first magnetic layer 51 facing the lattice separation layer 52, that is, a plurality of induction layers 53 can be arranged.

[0093] Some possible examples include Figures 5 to 8 As shown, the induction layer 53 includes at least one island-shaped split body, which can reduce the impact on the lattice structure subsequently formed thereon, and can also enhance the coupling between the film layers on both sides of the induction layer 53, so that the first magnetic layer 51 and the corresponding film layer can be flipped more synchronously, thereby improving the writing efficiency. The induction layer 53 can include at least two island-shaped split bodies, at least part of which are arranged in parallel, so that the island-shaped split bodies arranged in parallel are arranged in the same layer for easy formation.

[0094] In other possible examples, such as Fig. 9 As shown, the induction layer 53 is a continuous film layer, and the thickness of the two ends is different. Exemplarily, the thickness of the continuous film layer gradually increases from one end to the other end of the continuous film layer, that is, the continuous film layer is wedge-shaped. In this way, the induction layer 53 has a certain slope, and the thickness of the induction layer 53 at different positions is different, so that the equivalent anisotropy field and equivalent magnetization of the first magnetic layer 51 are different. The end with a smaller equivalent magnetization is easier to flip, thereby driving the other end to flip, further reducing the write power consumption.

[0095] The induction layer 53 is formed by a sputtering process, and at least one of the sputtering time and the sputtering angle is controlled to make the thickness of the two ends of the induction layer 53 different. The thickness of the induction layer 53 at different positions is different, so that the equivalent anisotropy field and the equivalent magnetization intensity of the first magnetic layer 51 are different, and the end with a smaller equivalent magnetization intensity is easier to flip, thereby driving the other end to flip, and further reducing the write power consumption.

[0096] In summary, in the method for manufacturing the composite film layer structure in the embodiment of the present application, the first magnetic layer 51, the lattice separation layer 52, the induction layer 53 and the second magnetic layer 54 are formed. By increasing the thickness of the second magnetic layer 54, the thermal stability can be improved, and by reducing the thickness of the first magnetic layer 51, the write power consumption can be reduced. The lattice separation layer 52 is arranged on the first magnetic layer 51, and the induction layer 53 includes at least one island-shaped split arranged in parallel or the induction layer 53 is a continuous film layer with different thicknesses at both ends, which can reduce the influence on the lattice structure of the second magnetic layer 54, and make the second magnetic layer 54 and the first magnetic layer 51 closer in some places, which can enhance the coupling between the first magnetic layer 51 and the second magnetic layer 54, so that the first magnetic layer 51 and the second magnetic layer 54 can be more synchronously flipped, and the write efficiency is improved. The induction layer 53 is arranged in the first magnetic layer 51; and / or, it is arranged on the side of the first magnetic layer 51 facing the lattice separation layer 52. The induction layer 53 is in contact with the first magnetic layer 51, which can reduce the equivalent magnetization intensity of the first magnetic layer 51, thereby further reducing the write power consumption. The induction layer 53 is in contact with the lattice separation layer 52 , which can alleviate the unevenness of the surface of the induction layer 53 and further improve the device performance.

[0097] In the first possible implementation, see Figure 5 , forming a first magnetic layer 51, a lattice separation layer 52, an induction layer 53 and a second magnetic layer 54, including: growing a first portion of the first magnetic layer 51; sputtering to form at least two island-shaped splits arranged in parallel, at least two island-shaped splits forming the induction layer 53; growing a second portion of the first magnetic layer 51, the second portion of the first magnetic layer 51 covering the induction layer 53; growing a lattice separation layer 52; and growing a second magnetic layer 54.

[0098] The first part of the first magnetic layer 51 and the second part of the first magnetic layer 51 are made of the same material, so that the first magnetic layer 51 is an integrated structure. The first magnetic layer 51 is grown in two parts, so that the induction layer 53 is located inside the first magnetic layer 51, and the lattice separation layer 52 is located on the first magnetic layer 51.

[0099] In the second possible implementation, see Figure 6, forming a first magnetic layer 51, a lattice separation layer 52, an induction layer 53 and a second magnetic layer 54, including: growing the first magnetic layer 51; sputtering to form at least two island-shaped splits arranged in parallel, the at least two island-shaped splits forming the induction layer 53; growing the lattice separation layer 52, the lattice separation layer 52 covering the induction layer 53; growing the second magnetic layer 54. Among them, the induction layer 53 is located on the side of the first magnetic layer 51 adjacent to the lattice separation layer 52, that is, the induction layer 53 is located between the first magnetic layer 51 and the lattice separation layer 52. Figure 7 , "1" in the horizontal axis represents a magnetic memory with a conventional structure, and "2" represents a magnetic memory with a composite film layer structure according to an embodiment of the present application. The composite film layer structure of the magnetic memory is as shown in FIG. Figure 6 Compared with the magnetic memory of the conventional structure, the write voltage V C reduce.

[0100] In a third possible implementation, see Figure 8 , forming a first magnetic layer 51, a lattice separation layer 52, an induction layer 53 and a second magnetic layer 54, including: growing a first portion of the first magnetic layer 51; sputtering to form at least two island-shaped splits arranged in parallel, at least two island-shaped splits forming the first induction layer 53; growing a second portion of the first magnetic layer 51, the second portion of the first magnetic layer 51 covering the first induction layer 53; sputtering to form at least two island-shaped splits arranged in parallel, at least two island-shaped splits forming the second induction layer 53; growing a lattice separation layer 52; growing a second magnetic layer 54.

[0101] The first part of the first magnetic layer 51 and the second part of the first magnetic layer 51 are made of the same material, so that the first magnetic layer 51 is an integrated structure. The first induction layer 53 is located inside the first magnetic layer 51, and the second induction layer 53 is located on the side of the first magnetic layer 51 adjacent to the lattice separation layer 52, that is, the second induction layer 53 is located between the first magnetic layer 51 and the lattice separation layer 52.

[0102] In a fourth possible implementation, see Fig. 9 , forming a first magnetic layer 51, a lattice separation layer 52, an induction layer 53 and a second magnetic layer 54, including: growing the first magnetic layer 51; sputtering to form a continuous film layer with different thicknesses at both ends, the continuous film layer forming the induction layer 53; growing the lattice separation layer 52, the lattice separation layer 52 covering the induction layer 53; growing the second magnetic layer 54. The induction layer 53 is located on the side of the first magnetic layer 51 adjacent to the lattice separation layer 52, that is, the induction layer 53 is located between the first magnetic layer 51 and the lattice separation layer 52.

[0103] The thickness of the induction layer 53 at both ends is different. For example, by controlling the sputtering time and / or the sputtering angle, the thickness of the induction layer 53 is gradually increased. In this way, the induction layer 53 has a certain slope, and the thickness of the induction layer 53 at different positions is different, so that the equivalent anisotropy field and equivalent magnetization of the first magnetic layer 51 are different. The end with a smaller equivalent magnetization is easier to flip, thereby driving the other end to flip, and further reducing the write power consumption.

[0104] The thickness of the lattice separation layer 52 at both ends may be different. For example, the thickness of the lattice separation layer 52 gradually increases, and the thickness variation trend of the lattice separation layer 52 is opposite to the thickness variation trend of the induction layer 53. Fig. 9 As shown, from left to right, the thickness of the lattice separation layer 52 gradually decreases, and the thickness of the induction layer 53 gradually increases. In this way, the lattice separation layer 52 is adapted to the induction layer 53, so that the lattice separation layer 52 is away from the surface level of the first magnetic layer 51, so that other film layers formed on the lattice separation layer 52 remain horizontal, thereby improving the performance of the entire film stack.

[0105] In a fifth possible implementation, see Fig.10 , forming a first magnetic layer 51, a lattice separation layer 52, an induction layer 53 and a second magnetic layer 54, including: growing the first magnetic layer 51; sputtering to form at least two island-shaped splits, the thickness of the two island-shaped splits at both ends are different, at least two island-shaped splits form the induction layer 53; growing the lattice separation layer 52, the lattice separation layer 52 covers the induction layer 53; growing the second magnetic layer 54.

[0106] The induction layer 53 is located on one side of the first magnetic layer 51 adjacent to the lattice separation layer 52, that is, the induction layer 53 is located between the first magnetic layer 51 and the lattice separation layer 52. By controlling the sputtering angle, at least two island-shaped bodies have a slight slope, and the content of the island-shaped body at one end is greater than that of the island-shaped body at the other end, so as to reduce the write power consumption. In the arrangement direction of the island-shaped bodies, that is, along the direction from one end to the other end of the first magnetic layer 51, the thickness of these island-shaped bodies increases successively for easy manufacturing.

[0107] In a sixth possible implementation, see Fig.11 , forming a first magnetic layer 51, a lattice separation layer 52, an induction layer 53 and a second magnetic layer 54, including: growing a first portion of the first magnetic layer 51; sputtering to form at least two island-shaped splits, the thickness of the two island-shaped splits at both ends are different, and at least two island-shaped splits form the induction layer 53; growing a second portion of the second magnetic layer 54, the second portion of the second magnetic layer 54 covers the induction layer 53; growing a lattice separation layer 52; growing a second magnetic layer 54.

[0108] The induction layer 53 is located in the first magnetic layer 51. By controlling the sputtering angle, at least two island-shaped bodies have a slight slope, and the content of the island-shaped body at one end is greater than that of the island-shaped body at the other end, so as to reduce the write power consumption. The thickness of these island-shaped bodies increases in sequence along the arrangement direction of the island-shaped bodies, that is, along the direction from one end to the other end of the first magnetic layer 51, so as to facilitate the manufacturing.

[0109] In the seventh possible implementation, see Fig.12 , forming a first magnetic layer 51, a lattice separation layer 52, an induction layer 53 and a second magnetic layer 54, including: growing the second magnetic layer 54; growing the lattice separation layer 52; sputtering to form at least two island-shaped splits arranged in parallel, at least two island-shaped splits forming the induction layer 53; growing the first magnetic layer 51. The induction layer 53 is located on the side of the lattice separation layer 52 adjacent to the first magnetic layer 51, that is, the induction layer 53 is located between the first magnetic layer 51 and the lattice separation layer 52.

[0110] See also Fig.13 , "1" in the horizontal axis represents a magnetic memory with a conventional structure, and "2" represents a magnetic memory with a composite film layer structure according to an embodiment of the present application. The composite film layer structure of the magnetic memory is as shown in FIG. Fig.12 Compared with the magnetic memory of the conventional structure, the tunnel magnetoresistance of the magnetic memory having the composite film layer structure of the embodiment of the present application is increased.

[0111] In this specification, each embodiment or implementation is described in a progressive manner, and each embodiment focuses on the differences from other embodiments, and the same or similar parts between the embodiments can be referenced to each other. The description of reference terms such as "one implementation", "some implementations", "illustrative implementations", "examples", "specific examples", or "some examples" means that the specific features, structures, materials or characteristics described in conjunction with the implementation or example are included in at least one implementation or example of the present application. In this specification, the schematic representation of the above terms does not necessarily refer to the same implementation or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more implementations or examples in a suitable manner.

[0112] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present application, rather than to limit it. Although the present application has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present application.

Claims

1. A composite film structure, characterized in that: include: a first magnetic layer, a lattice separation layer, an induction layer, and a second magnetic layer; The first magnetic layer, the lattice separation layer and the second magnetic layer are stacked in sequence, the induction layer includes at least one island-shaped split body or the induction layer is a continuous film layer with different thicknesses at both ends; the induction layer is arranged in the first magnetic layer, and / or, arranged on a side of the first magnetic layer facing the lattice separation layer; The material of the lattice separation layer includes an amorphous material, or the material of the lattice separation layer is a material with the same lattice structure as the second magnetic layer; The induction layer is made of a material with strong anisotropy.

2. The composite membrane structure according to claim 1, characterized in that: The thickness of the first magnetic layer is smaller than the thickness of the second magnetic layer.

3. The composite membrane structure according to claim 1, characterized in that: The lattice structure of the first magnetic layer is different from the lattice structure of the second magnetic layer.

4. The composite membrane structure according to claim 1, characterized in that: At least a portion of the induction layer is in contact with the lattice separation layer.

5. The composite membrane structure according to claim 1, characterized in that: The thicknesses of the two ends of the lattice separation layer are different.

6. The composite membrane structure according to claim 1, characterized in that: The induction layer includes at least two island-shaped splits, at least some of which are arranged in parallel, and among the island-shaped splits arranged in parallel, the island-shaped splits at two ends have different thicknesses.

7. A magnetic memory, characterized in that: include: A free layer, a reference layer, and a barrier layer disposed between the free layer and the reference layer; At least one of the free layer and the reference layer comprises the composite film layer structure according to any one of claims 1 to 6, and the second magnetic layer of the composite film layer structure is adjacent to the barrier layer.

8. The magnetic memory according to claim 7, characterized in that: The lattice structure of the first magnetic layer of the composite film layer structure is different from the lattice structure of the barrier layer.

9. A method for manufacturing a composite membrane structure, characterized in that: include: forming a first magnetic layer, a lattice separation layer, an induction layer, and a second magnetic layer; The lattice separation layer is formed on a side of the second magnetic layer close to the induction layer, the induction layer includes at least one island-shaped split body or the induction layer is a continuous film layer with different thicknesses at both ends; the induction layer is formed in the first magnetic layer and / or formed on a side of the first magnetic layer facing the lattice separation layer; The first magnetic layer, the lattice separation layer, the induction layer and the second magnetic layer form the composite film layer structure; The material of the lattice separation layer includes an amorphous material, or the material of the lattice separation layer is a material with the same lattice structure as the second magnetic layer; The induction layer is made of a material with strong anisotropy.

10. The manufacturing method according to claim 9, characterized in that: The induction layer is formed by a sputtering process, and at least one of a sputtering time and a sputtering angle is controlled so that the thickness of the two ends of the induction layer is different.