Welding deformation prevention manufacturing method for thick-plate octagonal-section box type steel column

By adopting double-sided V-shaped grooves and optimizing the welding sequence during the welding process of thick plate octagonal section box steel columns, the problem of welding deformation is solved, material loss is reduced, processing efficiency is improved, and high-quality welding results are achieved.

CN118720485APending Publication Date: 2024-10-01MCC (SHANGHAI) STEEL STRUCTURE TECHNOLOGY CORP LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411022891.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-29
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

Thick plate octagonal cross-section box steel columns are prone to deformation during the welding process, resulting in high material loss and low processing efficiency.

Method used

The welding groove form of double-sided V-shaped groove is adopted, the angle of the cutting gun nozzle is adjusted, the welding sequence of the main weld is optimized, and the gas shielded welding is used as the base and the submerged arc welding is filled in steps to reduce the amount of welding filling and deformation.

Benefits of technology

It reduces material loss, improves processing efficiency, effectively prevents welding deformation, and improves the welding quality of thick plate octagonal section box steel columns.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118720485A_ABST
    Figure CN118720485A_ABST
Patent Text Reader

Abstract

The invention relates to a welding deformation prevention manufacturing method for a thick-plate octagonal-section box type steel column. The welding deformation prevention manufacturing method comprises the steps that firstly, wall plate blanking is manufactured; 2, arranging and blanking the wallboards; 3, assembling and welding a cross part body; fourthly, a cross-shaped column is manufactured; and 5, assembling and welding the rest wall plates of the octagonal column. The welding deformation preventing effect of the thick-plate octagonal-section box type steel column is achieved by formulating the reasonable groove angle and optimizing the welding sequence of the main weld joints.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of steel structure construction, in particular to a method for manufacturing a thick plate octagonal cross-section box-type steel column to prevent welding deformation. Background Art

[0002] With the development of steel structure manufacturing technology, thick polygonal steel columns with high rigidity, high strength and beautiful appearance have appeared in some buildings such as airport terminals and libraries. The main type of steel columns is octagonal columns with a plate thickness of 50~100mm. The proportion of full penetration welds exceeds 50%, and the huge welding filling volume is prone to welding deformation. Summary of the invention

[0003] The present invention aims to overcome the defects of the prior art and provide a method for manufacturing a thick plate octagonal cross-section box-type steel column to prevent welding deformation, thereby solving the problem that the thick plate octagonal cross-section box-type steel column is easily deformed during welding.

[0004] In order to solve the above-mentioned technical problems, the present invention is achieved as follows: A method for preventing welding deformation of thick plate octagonal cross-section box-shaped steel columns, characterized in that it comprises the following steps: Step 1: Make the wall panel blanks; Step 2: Layout and cutting of wall panels; Step 3: Assemble and weld the cross body; Step 4: Making the cross column; Step 5: Assemble and weld the remaining wall panels of the octagonal column.

[0005] The method for preventing welding deformation of a thick plate octagonal cross-section box-type steel column is characterized in that: step one specifically includes: formulating the octagonal column welding groove as a double-sided V-shaped groove, the welding gap takes a large gap, the welding gap value L3 is generally 10-12mm, the welding angle takes a small angle, and the welding angle value is generally between 22°-28°.

[0006] The method for preventing welding deformation of thick plate octagonal cross-section box-type steel columns is characterized in that: step two specifically includes: the wall panel has a trapezoidal cross-section, the cutting gun nozzle angle is adjusted, the wall panel is cut and the groove is opened to share the same edge, and the two processes are completed simultaneously.

[0007] The method for preventing welding deformation of a thick plate octagonal cross-section box-shaped steel column is characterized in that: step three specifically includes: completing the assembly and welding of BH-shaped steel and T-shaped steel respectively.

[0008] The method for preventing welding deformation of a thick plate octagonal cross-section box-type steel column is characterized in that: step four specifically includes: assembling and welding the BH steel, T-steel and stiffening plate to form an integral cross part.

[0009] The method for preventing welding deformation of a thick plate octagonal cross-section box-type steel column is characterized in that: step five specifically includes: during welding, eight longitudinal main welds are primed with gas shielded welding in sequence, at least 2-3 times. After the prime is completed, the upper weld is first filled with submerged arc welding for about 1 / 3 of the workload; then the components are turned over in sequence and the welds on the adjacent two sides are filled and welded to 1 / 3 of the workload, and then the weld on the last side is fully welded; the components are turned over again and the above welds are welded in reverse order.

[0010] The beneficial effects of the present invention are as follows: It can be seen from the above technical scheme that the present application provides a method for preventing welding deformation of thick plate octagonal cross-section box-type steel columns, which greatly reduces material loss and improves processing efficiency by making the cutting and groove share the same edge; by formulating a reasonable groove angle and optimizing the welding sequence of the main welds, an effect of preventing welding deformation of thick plate octagonal cross-section box-type steel columns is achieved. BRIEF DESCRIPTION OF THE DRAWINGS

[0011] The present invention is further described in detail below in conjunction with the accompanying drawings and embodiments: Figure 1 It is a schematic diagram of the cross section of a thick plate octagonal box-type steel column; Figure 2 It is a schematic diagram of the process of the present invention.

[0012] Figure 3 Schematic diagram of assembly groove angle.

[0013] Figure 4 Schematic diagram of muzzle cutting for wall panel blanking.

[0014] Figure 5 Schematic diagram of H-shaped steel and T-shaped steel.

[0015] Figure 6 This is a schematic diagram of the cross section assembly.

[0016] Figure 7 Schematic diagram of octagonal column assembly. DETAILED DESCRIPTION

[0017] The technical solutions of the embodiments of the present application will be described clearly and completely below in conjunction with the accompanying drawings. Obviously, the described embodiments are part of the embodiments of the present application, not all of the embodiments. All other embodiments obtained by ordinary technicians in this field without creative work based on the embodiments in the embodiments of the present application are within the scope of protection requested by the present application. like Figure 1-6 As shown: A method for preventing welding deformation of a thick plate octagonal cross-section box-shaped steel column, comprising the following steps: Step 1: Calculate the size of the wall panel cutting; The octagonal column welding groove form is formulated as a double-sided V-shaped groove, the welding gap is a large gap, the welding gap value L3 is generally 10-12mm, and the welding angle is a small angle, and the welding angle value is generally between 22°-28°. The process of large gap and small groove angle is used to reduce the welding filling amount and thus reduce welding deformation; the outer surface size of the wall panel is calculated to be L1, and the inner surface size is L2, then the outer surface size of the blank is (L1-L3) mm, and the inner surface size of the blank is (L2-L3) mm.

[0018] Step 2: Layout and cutting of wall panels; The wall panel has a trapezoidal cross-section. Cut the panel as shown in the figure and adjust the cutting gun nozzle angle so that the wall panel cutting and beveling can be done on the same edge. The two processes can be completed at the same time, saving materials.

[0019] Step 3: Assemble and weld the cross part body; Complete the assembly and welding of BH steel and T steel respectively.

[0020] Step 4: Making the cross column; Assemble and weld the BH steel, T steel and stiffening plate to form an integral cross part.

[0021] Step 5: Assemble and weld the remaining wall panels of the octagonal column; Finally, the assembly and welding of the octagonal column is completed. When welding, the main welding seam welding sequence is as follows: Figure 7 As shown, the eight longitudinal main welds are primed with gas shielded welding in sequence, at least 2-3 times. After the prime is completed, first, welds ① and ② are filled with submerged arc welding to about 1 / 3 of the workload; then the component is turned over in sequence to fill and weld welds ③ and ④ to 1 / 3 of the workload, and weld welds ⑤ and ⑥ to 1 / 3 of the workload; ensure that the interlayer temperature of welds ⑦ and ⑧ is within the process requirements and fill the welds; turn the component over again and fill the welds in the order of welds ⑤ and ⑥ first, welds ③ and ④, and finally welds ① and ②.

[0022] The present invention greatly reduces material loss and improves processing efficiency by making the cutting and the groove share the same edge; by formulating a reasonable groove angle and optimizing the welding sequence of the main welds, an effect of preventing welding deformation of a thick plate octagonal cross-section box-type steel column is achieved.

[0023] The above are only embodiments provided for the present application and are not intended to limit the present application. Although the present application is described in detail with reference to the embodiments, those skilled in the art can still modify the technical solutions described in the aforementioned embodiments or make equivalent substitutions for some of the technical features therein. However, any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present application should be included in the protection scope of the present application.

Claims

1. A method for preventing welding deformation of thick plate octagonal cross-section box-shaped steel columns, characterized in that It includes the following steps: Step 1: Make the wall panel blanks; Step 2: Layout and cutting of wall panels; Step 3: Assemble and weld the cross body; Step 4: Making the cross column; Step 5: Assemble and weld the remaining wall panels of the octagonal column.

2. The method for preventing welding deformation of a thick plate octagonal cross-section box-shaped steel column according to claim 1 is characterized in that: Step one specifically includes: setting the octagonal column welding groove form as a double-sided V-shaped groove, taking a large gap as the welding gap, the welding gap value L3 is generally 10-12mm, taking a small angle as the welding angle, and the welding angle value is generally between 22°-28°.

3. The method for preventing welding deformation of a thick plate octagonal cross-section box-shaped steel column according to claim 1 is characterized in that: Step 2 specifically includes: the wall panel has a trapezoidal cross-section, the cutting gun nozzle angle is adjusted, the wall panel is cut and the groove is opened to have the same edge, and the two processes are completed simultaneously.

4. The method for preventing welding deformation of a thick plate octagonal cross-section box-shaped steel column according to claim 1 is characterized in that: Step three specifically includes: completing the assembly and welding of BH-shaped steel and T-shaped steel respectively.

5. The method for preventing welding deformation of a thick plate octagonal cross-section box-shaped steel column according to claim 1 is characterized in that: Step 4 specifically includes: assembling and welding the BH steel, T steel and stiffening plate to form an integral cross part.

6. The method for preventing welding deformation of a thick plate octagonal cross-section box-shaped steel column according to claim 1 is characterized in that: Step five specifically includes: during welding, eight longitudinal main welds are primed with gas shielded welding in sequence, at least 2-3 times. After the prime is completed, first fill the upper weld with submerged arc welding to weld about 1 / 3 of the workload; then turn the component over in sequence and fill the adjacent two side welds to 1 / 3 of the workload, and then fill the last side weld; turn the component over again and fill the above welds in reverse order.

Citation Information

Cited By