Humic acid-containing water-soluble fertilizer and preparation method thereof
By cross-linking modified colloids with polyurethane materials and adding surfactants, the problem of moisture absorption and agglomeration in salt-resistant polymer fertilizer coatings has been solved, achieving efficient release and utilization of fertilizers, and enhancing structural stability and microbial growth environment.
Patent Information
- Application Number
- CN202411137912.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-19
- Publication Date
- 2024-10-01
AI Technical Summary
Existing salt-resistant polymeric fertilizer coatings are prone to moisture absorption and agglomeration, resulting in bonding between fertilizer particles and salt-based ions, reducing fertilizer utilization.
Modified colloids are cross-linked with polyurethane materials to form a coating, and surfactants, biosurfactants and anti-sticking agents are added to the coating to control the contact between fertilizer particles and water to prevent moisture absorption and agglomeration. Improve the gradient sustained release performance of nutrients.
It effectively prevents the adhesion between fertilizer particles and salt-based ions, improves fertilizer utilization, enhances structural stability, reduces dust generation and environmental pollution, and promotes microbial growth and gradient release of nutrients.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of fertilizers, in particular to a water-soluble fertilizer containing humic acid and a preparation method thereof. Background Art
[0002] After water-soluble fertilizers are applied to the soil, part of the nutrients can be absorbed by crops, but the rest of the fertilizers are lost due to runoff, volatilization or mineralization, resulting in low fertilizer utilization. The result is not only a waste of resources, but also pollution of the soil, water and atmospheric environment.
[0003] At present, the main method to reduce fertilizer loss is to prepare slow-release fertilizers by coating and making large-particle compound fertilizers. Coated slow-release fertilizers are mainly made by granulating fertilizers and then wrapping them with a film. When the film dissolves or degrades, the release rate of the fertilizer gradually increases, thereby providing the nutrients needed by crops.
[0004] The Chinese invention patent with publication date of June 9, 2020 and publication number of CN107011058B proposes a salt-resistant functional coated slow / controlled release fertilizer and a preparation method thereof, wherein the fertilizer is composed of a core and a coating layer wrapped on the surface of the core. The core includes fertilizer particles; the coating layer includes a polyurethane material containing an acid group, a carboxylic acid, a sulfonic acid group, a sulfuric acid group or a sulfurous acid group, an isocyanate, a polyol, a catalyst and a cross-linking agent, etc. The polyurethane material containing an acid group is at least one of a carboxylic acid polyurethane, a sulfonate group polyurethane, a sulfate group polyurethane and a sulfite polyurethane material.
[0005] According to the above technical solution, the salt-resistant polymer fertilizer coating is prone to moisture absorption and agglomeration, resulting in adhesion between the fertilizer particles and the base ions, which limits the effective release of the fertilizer and reduces the utilization rate of the fertilizer. Summary of the invention
[0006] In order to improve the utilization rate of fertilizers, the present invention provides a water-soluble fertilizer containing humic acid and a preparation method thereof.
[0007] In a first aspect, the present invention provides a water-soluble fertilizer containing humic acid, which adopts the following technical scheme: A water-soluble fertilizer containing humic acid, comprising fertilizer particles and a coating wrapped on the surface of the fertilizer particles, wherein the coating accounts for 2% to 8% of the mass of the fertilizer particles; The fertilizer granules include the following raw materials in parts by weight: 20 to 40 parts of water-soluble humic acid, 1 to 40 parts of nitrogen fertilizer, 1 to 40 parts of phosphorus fertilizer, 1 to 40 parts of potassium fertilizer, 0.1 to 5 parts of microbial agent, 0.1 to 5 parts of trace elements, and 0.1 to 5 parts of amino acids; The coating includes a polyurethane material, a modified colloid, a catalyst and a cross-linking agent, wherein the modified colloid accounts for 6 to 9% of the mass of the polyurethane material, the polyurethane material is at least one of carboxylic acid polyurethane, olefinic acid polyurethane, carbonated polyurethane and polyamide ester, and the modified colloid is at least one of alkenyl alkane modified gelatin, alkenyl ketone modified gelatin and alkenyl ester modified gelatin.
[0008] By adopting the above technical solution, modified colloids are cross-linked with polyurethane materials, which helps prevent moisture absorption and agglomeration of the fertilizer coating after contact with water, thereby preventing adhesion between the fertilizer particles and the base ions. The gradient slow-release performance of nutrients in the fertilizer is effectively controlled, which is beneficial to the effective release of the fertilizer, thereby improving the utilization rate of the fertilizer.
[0009] Optionally, the modified colloid is made of gelatin through a modifier, and the modifier is at least one of alkenyl acid, alkenyl ketone, and alkenyl acid ester that can react with amino groups or hydroxyl groups in gelatin.
[0010] By adopting the above technical scheme, cross-linking points are introduced through modification reaction, which is beneficial to increase the cross-linking structure between gelatin molecules and enhance its mechanical strength, thermal stability and gelling properties; functional groups, such as hydrophobic groups or hydrophilic groups, are introduced through modification reaction, thereby improving the specific properties of gelatin, such as enhancing solubility, adjusting viscosity, improving emulsification, etc.; in this way, the gradient slow-release performance of nutrients in the fertilizer is effectively controlled, which is beneficial to the effective release of the fertilizer, thereby improving the utilization rate of the fertilizer.
[0011] Optionally, the coating further comprises a surfactant, and the surfactant is at least one of fatty acid salts, fatty acid glycerides, alkyl sulfates, imidazole derivatives, and halogenated pyridines.
[0012] By adopting the above technical solution, adding a surfactant to the coating is beneficial to reducing the surface tension of water, making the fertilizer more soluble in water and forming a stable mixture with water, which is not easy to absorb moisture and agglomerate, thereby realizing water-fertilizer integration, which is beneficial to the effective release of fertilizer, thereby improving the utilization rate of fertilizer. At the same time, it is beneficial to enhance the structural stability of fertilizer particles, reduce the breakage and pulverization of particles during transportation, storage and application, reduce the dust generated during the transportation of fertilizers, and reduce pollution to operators and the environment.
[0013] Optionally, the fertilizer particles further include 0.01 to 0.5 parts by weight of a biosurfactant, and the biosurfactant is at least one of a Lactobacillus propionate bioactive agent, a Bacillus subtilis lysine surfactant, a green algae bioactive agent, and a fungal bio-glue.
[0014] By adopting the above technical scheme, since the colloid has gelling properties, the viscosity of the fertilizer can be increased, and a certain protective effect can be played on the fertilizer particles in the soil, which is beneficial to the growth and long-term release of microbial agents; with the degradation of the high molecular polymer coating, micropores are gradually formed on the surface of the coating, and as the pores gradually expand, the biosurfactant is simultaneously decomposed by the microorganisms in the soil, making it easier for the microorganisms to invade the inside of the fertilizer particles from the surface of the coating, thereby forming a plurality of through-type holes in the fertilizer particles, accelerating the degradation of the fertilizer until the fertilizer is completely decomposed; with such a configuration, the gradient slow-release performance of the nutrients in the fertilizer is effectively controlled, which is beneficial to the effective release of the fertilizer, thereby improving the utilization rate of the fertilizer.
[0015] Optionally, the fertilizer granules further include 1 to 10 parts by weight of a filler, and the filler is at least one of silicate, calcium carbonate, bentonite, and cellulose.
[0016] By adopting the above technical solution, adding fillers to fertilizer particles is beneficial to increasing the physical stability of the fertilizer, improving the strength of the fertilizer particles, and providing the spatial density and support structure required for microbial growth, while providing the biological matrix required for microbial growth and promoting the attachment and growth of microorganisms.
[0017] Optionally, the coating further includes an anti-sticking agent, which is at least one of stearate, silicone, and polyvinyl alcohol.
[0018] By adopting the above technical solution, since polyurethane materials and surfactants have certain adhesion, especially in the case of high concentration or high molecular weight, which may cause adhesion between particles, a certain amount of anti-sticking agent is added to the surface of the capsule to prevent the capsule from sticking together during storage or use, thereby maintaining its surface flatness and aesthetics, which is conducive to the effective release of fertilizers, thereby improving the utilization rate of fertilizers.
[0019] In a second aspect, the present invention provides a method for preparing a water-soluble fertilizer containing humic acid, which adopts the following technical scheme: A method for preparing a water-soluble fertilizer containing humic acid, which is used to prepare a water-soluble fertilizer containing humic acid as described in the first aspect, comprises the following steps: a. Powder the raw materials into powder and add them into a blender, and mix them evenly to obtain fertilizer granules; b. Preparation of polyurethane materials and modified colloids; c. Under the action of a catalyst and a cross-linking agent, the polyurethane material and the modified colloid are cross-linked and cured to obtain a composite material, and the composite material is preheated to a molten state to obtain a coating liquid; d. Preheat the fertilizer particles in a drum or fluidized bed; e. After the coating liquid is atomized, it is evenly sprayed on the surface of the preheated fertilizer particles, cooled, and the coated fertilizer is made.
[0020] By adopting the above technical solution, modified colloids are cross-linked with polyurethane materials, which helps prevent moisture absorption and agglomeration of the fertilizer coating after contact with water, thereby preventing adhesion between the fertilizer particles and the base ions. The gradient slow-release performance of nutrients in the fertilizer is effectively controlled, which is beneficial to the effective release of the fertilizer, thereby improving the utilization rate of the fertilizer.
[0021] Optionally, in step b, the preparation method of the modified colloid is: dissolving gelatin in water, adjusting the pH to less than 4, adding a modifier, stirring for 8 to 12 hours, and after the reaction is completed, adjusting the system to neutral, and drying to obtain a modified colloid.
[0022] By adopting the above technical scheme, after adjusting to the specified pH value, a modifier is added, and gelatin dissolved in water is used as a carrier, which is conducive to the reaction or combination of the modifier and the gelatin molecules to achieve the change of the properties of the gelatin, which is conducive to improving the reaction efficiency, promoting the modifier to fully react with the gelatin, and facilitating the effective release of the fertilizer, thereby improving the utilization rate of the fertilizer.
[0023] Optionally, step a further comprises: powdering the raw materials into powder, adding the powder into a blender, mixing evenly, crushing to 60-80 mesh, adding an acidulant, stirring evenly, acidifying at room temperature, and adding a filler to adjust the viscosity and density of the system to obtain water-soluble fertilizer granules, wherein the acidulant is at least one of boric acid, phosphoric acid, and ethylene glycol.
[0024] By adopting the above technical scheme, humic acid is prone to aggregation at high temperature, and acidification treatment can destroy the ionic bonds and hydrogen bonds between humic acid molecules, making its molecular structure looser, causing the charge balance between humic acid molecules to be unbalanced, increasing its hydrophilicity, thereby improving its solubility and dispersibility, which is beneficial to improving the effectiveness of humic acid fertilizer and enabling it to be fully decomposed and utilized in the soil.
[0025] Optionally, in step c, after the polyurethane material and the modified colloid are cross-linked, UV is used for curing.
[0026] By adopting the above technical scheme, the modified colloid and the polyurethane material form a composite material through chemical crosslinking and covalent bonding under the action of ultraviolet light curing. Compared with other curing methods, this method is more environmentally friendly and clean, does not introduce other harmful substances, is beneficial to enhancing biodegradability, and at the same time, is beneficial to improving the thermal stability and mechanical properties of the composite material.
[0027] In summary, the present invention includes at least one of the following beneficial technical effects: 1. By cross-linking modified colloids with polyurethane materials, it is helpful to prevent the fertilizer coating from absorbing moisture and agglomerating after contacting with water, so that the fertilizer particles and the base ions are not easy to stick together. The gradient slow-release performance of nutrients in the fertilizer is effectively controlled, which is conducive to the effective release of the fertilizer, thereby improving the utilization rate of the fertilizer.
[0028] 2. Introducing cross-linking points through modification reaction is beneficial to increase the cross-linking structure between gelatin molecules, enhancing its mechanical strength, thermal stability and gelling properties; introducing functional groups, such as hydrophobic groups or hydrophilic groups, through modification reaction can improve the specific properties of gelatin, such as enhancing solubility, adjusting viscosity, improving emulsification, etc.; in this way, the gradient slow-release performance of nutrients in the fertilizer is effectively controlled, which is beneficial to the effective release of the fertilizer, thereby improving the utilization rate of the fertilizer.
[0029] 3. Through the setting of biological surfactants and fillers, as the polymer coating degrades, microorganisms can more easily invade the inside of fertilizer particles from the surface of the coating, accelerating the degradation of the fertilizer until the fertilizer is completely decomposed. The gradient slow release performance of nutrients in the fertilizer is effectively controlled, which is conducive to the effective release of fertilizer, thereby improving the utilization rate of fertilizer. Adding fillers to fertilizer particles is conducive to increasing the physical stability of fertilizers, improving the strength of fertilizer particles, and providing the spatial density and support structure required for microbial growth. At the same time, it provides the biological matrix required for microbial growth and promotes the attachment and growth of microorganisms.
[0030] 4. The setting of surfactants and anti-sticking agents is helpful to reduce the surface tension of water, making the fertilizer more soluble in water and forming a stable mixture with water, preventing the film from sticking together during storage or use, maintaining its surface flatness and aesthetics, and making it less likely to absorb moisture and agglomerate, which is conducive to the effective release of fertilizers, thereby improving the utilization rate of fertilizers. DETAILED DESCRIPTION
[0031] The present invention is further described in detail below with reference to the embodiments.
[0032] Example 1: This example discloses a water-soluble fertilizer containing humic acid, which is composed of fertilizer particles and a coating wrapped on the surface of the fertilizer particles, wherein the coating accounts for 2% to 8% of the mass of the fertilizer particles; The fertilizer granules are composed of the following raw materials in parts by weight: 20 to 40 parts of water-soluble humic acid, 1 to 40 parts of nitrogen fertilizer, 1 to 40 parts of phosphorus fertilizer, 1 to 40 parts of potash fertilizer, 1 to 10 parts of filler, 0.1 to 5 parts of microbial agent, 0.01 to 0.5 parts of biological surfactant, 0.1 to 5 parts of trace elements, and 0.1 to 5 parts of amino acids; The biosurfactant is at least one of a Lactobacillus propionate bioactive agent, a Bacillus subtilis lysine surfactant, a green algae bioactive agent, and a fungal bioglue; the filler is at least one of a silicate, calcium carbonate, bentonite, and cellulose; the trace element is selected from at least one of zinc, iron, manganese, copper, boron, molybdenum, calcium, magnesium, and selenium; and the crosslinking agent is selected from at least one of diethylene glycol, propylene oxide, melamine formaldehyde resin, hexamethylene diisocyanate, and polymaleic acid.
[0033] The coating is composed of a polyurethane material, a modified colloid, a catalyst, a cross-linking agent, a surfactant, and an anti-sticking agent, wherein the polyurethane material is at least one of carboxylic acid polyurethane, olefinic acid polyurethane, carbonate polyurethane, and polyamide ester; The modified colloid is 6-9% of the mass of the polyurethane material, the modified colloid is at least one of alkenyl alkane modified gelatin, alkenyl ketone modified gelatin, and alkenyl ester modified gelatin, the modified colloid is made of gelatin through a modifier, and the modifier is at least one of alkenyl acid, alkenyl ketone, and alkenyl ester that can react with amino groups or hydroxyl groups in gelatin; The surfactant is at least one of fatty acid salts, fatty acid glycerides, alkyl sulfates, imidazole derivatives, and halogenated pyridines, and the anti-sticking agent is at least one of stearates, silicones, and polyvinyl alcohols.
[0034] The implementation principle of a water-soluble fertilizer containing humic acid in this embodiment is: The use of modified colloids and polyurethane materials for cross-linking helps the fertilizer coating to be less likely to absorb moisture and agglomerate after contact with water, thereby making it less likely for the fertilizer particles to adhere to the base ions. Cross-linking points and functional groups are introduced through the modification reaction, thereby improving the specific properties of gelatin. In this way, the gradient slow-release performance of nutrients in the fertilizer is effectively controlled, which is conducive to the effective release of the fertilizer, thereby improving the utilization rate of the fertilizer.
[0035] Adding surfactants to the coating helps to reduce the surface tension of water, making the fertilizer more soluble in water and less likely to absorb moisture and clump, thereby achieving water-fertilizer integration. At the same time, it helps to enhance the structural stability of the fertilizer particles, reduce the breakage and pulverization of the particles during transportation, storage and application, and reduce the dust generated during the transportation of fertilizers.
[0036] Since polyurethane materials and surfactants have certain adhesion, especially in the case of high concentration or high molecular weight, which may cause adhesion between particles, a certain amount of anti-sticking agent is added to the surface of the coating to prevent the coating from sticking together during storage or use.
[0037] Due to the gelling properties of the colloid, the viscosity of the fertilizer can be increased, and it can protect the fertilizer particles in the soil to a certain extent, which is beneficial to the growth and long-term release of microbial agents. With the degradation of the high molecular polymer coating, micropores are gradually formed on the surface of the coating. As the pores gradually expand, the biosurfactant is also decomposed by the microorganisms in the soil, making it easier for the microorganisms to invade the inside of the fertilizer particles from the surface of the coating, thereby forming multiple through-holes in the fertilizer particles, accelerating the degradation of the fertilizer until the fertilizer is completely decomposed.
[0038] Adding fillers to fertilizer granules is beneficial to increase the physical stability of the fertilizer, improve the strength of the fertilizer granules, and provide the spatial density and support structure required for microbial growth. At the same time, it provides the biological matrix required for microbial growth and promotes the attachment and growth of microorganisms.
[0039] Example 2: This example discloses a method for preparing a water-soluble fertilizer containing humic acid, comprising the following steps: a. Powder the raw materials into a blender, mix evenly, crush to 60-80 mesh, add an acidulant, stir evenly, acidify at room temperature, add a filler to adjust the viscosity and density of the system, and obtain water-soluble fertilizer granules. The acidulant is at least one of boric acid, phosphoric acid, and ethylene glycol.
[0040] b. Prepare polyurethane materials and modified colloids. The preparation method of the modified colloid is as follows: dissolve gelatin in water, adjust the pH to less than 4, add a modifier, stir for 8 to 12 hours, adjust the system to neutral after the reaction is completed, and dry to obtain a modified colloid.
[0041] c. Under the action of a catalyst and a cross-linking agent, the polyurethane material and the modified colloid are cross-linked, and UV is used for curing to obtain a composite material, and the composite material is preheated to a molten state to obtain a coating liquid; d. Preheat the fertilizer particles in a drum or fluidized bed; e. After the coating liquid is atomized, it is evenly sprayed on the surface of the preheated fertilizer particles, cooled, and the coating is formed.
[0042] The implementation principle of the method for preparing a water-soluble fertilizer containing humic acid in this embodiment is as follows: The use of modified colloids and polyurethane materials for cross-linking helps prevent the fertilizer coating from absorbing moisture and agglomerating after contact with water, thereby preventing the fertilizer particles from sticking to the base ions. The gradient slow-release performance of nutrients in the fertilizer is effectively controlled, which is beneficial for the effective release of the fertilizer, thereby improving the utilization rate of the fertilizer.
[0043] Humic acid tends to aggregate at high temperatures. Acidification treatment can destroy the ionic bonds and hydrogen bonds between humic acid molecules, making its molecular structure looser, causing an imbalance in the charge balance between humic acid molecules and increasing its hydrophilicity, thereby improving its solubility and dispersibility, which is beneficial to improving the effectiveness of humic acid fertilizers and enabling them to be fully decomposed and utilized in the soil. After adjusting to the specified pH value, a modifier is added, and gelatin dissolved in water is used as a carrier, which is beneficial for the modifier to react or combine with the gelatin molecules to achieve a change in the properties of the gelatin, which is beneficial to improving the reaction efficiency and promoting the modifier to fully react with the gelatin.
[0044] Under the action of ultraviolet light curing, the modified colloid and polyurethane material form a composite material through chemical crosslinking and covalent bonding. Compared with other curing methods, this method is more environmentally friendly and clean, does not introduce other harmful substances, is beneficial to enhancing biodegradability, and at the same time, is beneficial to improving the thermal stability and mechanical properties of the composite material.
[0045] Example 3: The raw materials are 40 parts of lignite humic acid, 20 parts of ammonium sulfate, 15 parts of calcium phosphate, 15 parts of potassium chloride, 5 parts of microbial agent jelly-like bacillus, 0.3 parts of trace elements, and 4.7 parts of amino acids, which are made into powder, stirred and crushed, acidified with boric acid at room temperature, and added with filler silicate to make fertilizer particles. Preparation of polyurethane material polyadipate-1,4-butylene glycol ester. Gelatin is dissolved in water, pH=4 is adjusted, and methyl methacrylate is added as a modifier. After the reaction is completed, the system is adjusted to neutral and dried to obtain modified colloid alkenyl alkane modified gelatin. Under the action of a catalyst and a crosslinking agent, the polyurethane material is crosslinked with the modified colloid, UV cured, and a composite material is obtained. The composite material is preheated to a molten state to obtain a coating liquid. The fertilizer particles are placed in a drum or a fluidized bed for preheating, and the coating liquid is atomized and evenly sprayed on the surface of the preheated fertilizer particles, cooled, and a coated fertilizer is obtained.
[0046] Embodiment 4: The difference between Embodiment 4 and Embodiment 3 is that the polyurethane material is polycaprolactone ester diol and the modifier is hexadecene.
[0047] Embodiment 5: The difference between Embodiment 5 and Embodiment 3 is that the polyurethane material is polycarbonate diol and the modifier is vinyl trimethoxy silane.
[0048] Example 6: The difference between Example 6 and Example 3 is that after the composite material is preheated to a molten state, a surfactant fatty acid glyceride is added and stirred evenly to obtain a coating liquid.
[0049] Example 7: The difference between Example 7 and Example 3 is that the raw material for preparing the fertilizer granules further includes 0.5 parts by weight of a biosurfactant, and the biosurfactant is a Lactobacillus propionate bioactive agent.
[0050] Example 8: The difference between Example 8 and Example 7 is that the raw material for preparing the fertilizer granules further includes 10 parts by weight of a filler, and the filler is a silicate.
[0051] Example 9: The difference between Example 9 and Example 3 is that after the coating liquid is sprayed on the surface of the fertilizer particles, a layer of anti-sticking agent is also sprayed on the coating surface, and the anti-sticking agent is cyclotetramethylsiloxane.
[0052] Example 10: The difference between Example 10 and Example 3 is that gelatin is dissolved in water, pH is adjusted to 2, and a modifier, alkenyl acid, is added. After the reaction is completed, the system is adjusted to neutral and dried to obtain a modified colloid alkenyl alkane-modified gelatin.
[0053] Embodiment 11: The difference between the embodiment 11 and the embodiment 3 is that the raw materials are made into powder and added into a blender, mixed evenly, crushed into 60-80 mesh, an acidulant is added, stirred evenly, and acidified at room temperature. The coated fertilizers prepared in Examples 3 to 11 were tested for coating hydrolysis rate, fertilizer release rate, agglomeration rate and microbial activity 30 days after release. The results are shown in the following table: Example Encapsulation hydrolysis rate / % Fertilizer release rate / % Agglomeration rate / % Microbial activity / % Example 3 70.4 62.0 0.9 65.6 Example 4 69.3 61.6 0.9 65.1 Example 5 68.8 61.4 0.9 65.3 Example 6 71.2 62.3 0.8 65.4 Example 7 74.3 65.0 0.7 72.1 Example 8 76.5 66.3 0.7 72.6 Example 9 70.5 62.3 0.7 65.7 Example 10 72.2 62.9 0.8 65.5 Embodiment 11 72.5 62.4 0.8 65.6 From the comparison of Example 3, Example 4, and Example 5, it can be seen that by cross-linking the modified colloid with the polyurethane material, the fertilizer is not easy to absorb moisture and agglomerate after contacting with water, the solubility of the fertilizer particles is enhanced, the viscosity between the particles is reduced, and the gradient slow release performance of the nutrients in the fertilizer is effectively controlled.
[0054] From the comparison between Example 3 and Example 6, it can be seen that adding a surfactant to the coating is beneficial to reducing the surface tension of water, making the fertilizer more soluble in water and forming a stable mixture with water, which is less likely to absorb moisture and agglomerate.
[0055] From the comparison between Example 3 and Example 9, it can be seen that wrapping a certain amount of anti-sticking agent on the surface of the film is beneficial to reducing the caking rate of the fertilizer, thereby improving the 30-day release rate of the fertilizer.
[0056] By comparing Example 3, Example 7, and Example 8, it can be seen that by adding a certain amount of biosurfactant, the microbial activity can be regulated to a certain extent, and the release rate of the fertilizer can be accelerated, so that the gradient slow release performance of the nutrients in the fertilizer can be effectively controlled; after the filler is added to the fertilizer particles, it is beneficial to increase the physical structure stability of the fertilizer, provide the spatial density and biological matrix required for microbial growth, and promote the attachment and growth of microorganisms.
[0057] From the comparison between Example 3 and Example 10, it can be seen that adjusting the pH to less than 4 before modification is beneficial to improving the reaction efficiency and promoting the full reaction between the modifier and gelatin. When the pH is further reduced, the hydrolysis rate of the fertilizer particles is improved to a certain extent, and the fertilizer is less likely to agglomerate.
[0058] From the comparison between Example 3 and Example 11, it can be seen that the use of an acidifier to acidify humic acid is beneficial to increase its hydrophilicity, thereby improving its solubility.
[0059] The above are all preferred embodiments of the present invention, and are not intended to limit the protection scope of the present invention. Therefore, any equivalent changes made based on the structure, shape, and principle of the present invention should be included in the protection scope of the present invention.
Claims
1. A water-soluble fertilizer containing humic acid, characterized in that: It comprises fertilizer particles and a coating wrapped on the surface of the fertilizer particles, wherein the coating accounts for 2% to 8% of the mass of the fertilizer particles; The fertilizer granules include the following raw materials in parts by weight: 20 to 40 parts of water-soluble humic acid, 1 to 40 parts of nitrogen fertilizer, 1 to 40 parts of phosphorus fertilizer, 1 to 40 parts of potassium fertilizer, 0.1 to 5 parts of microbial agent, 0.1 to 5 parts of trace elements, and 0.1 to 5 parts of amino acids; The coating includes a polyurethane material, a modified colloid, a catalyst and a cross-linking agent, wherein the modified colloid accounts for 6 to 9% of the mass of the polyurethane material, the polyurethane material is at least one of carboxylic acid polyurethane, olefinic acid polyurethane, carbonated polyurethane and polyamide ester, and the modified colloid is at least one of alkenyl alkane modified gelatin, alkenyl ketone modified gelatin and alkenyl ester modified gelatin.
2. A water-soluble fertilizer containing humic acid according to claim 1, characterized in that: The modified colloid is made of gelatin through a modifier, and the modifier is at least one of alkenyl acid, alkenyl ketone and alkenyl acid ester that can react with amino groups or hydroxyl groups in gelatin.
3. A water-soluble fertilizer containing humic acid according to claim 2, characterized in that: The envelope further comprises a surfactant, and the surfactant is at least one of fatty acid salts, fatty acid glycerides, alkyl sulfates, imidazole derivatives, and halogenated pyridines.
4. A water-soluble fertilizer containing humic acid according to any one of claims 1 to 3, characterized in that: The fertilizer particles also include 0.01 to 0.5 parts by weight of a biosurfactant, wherein the biosurfactant is at least one of a Lactobacillus propionate bioactive agent, a Bacillus subtilis lysine surfactant, a green algae bioactive agent, and a fungal bio-glue.
5. A water-soluble fertilizer containing humic acid according to claim 4, characterized in that: The fertilizer granules further include 1 to 10 parts by weight of a filler, wherein the filler is at least one of silicate, calcium carbonate, bentonite and cellulose.
6. The water-soluble fertilizer containing humic acid according to claim 4, characterized in that: The coating further comprises an anti-sticking agent, which is at least one of stearate, silicone and polyvinyl alcohol.
7. A method for preparing a water-soluble fertilizer containing humic acid, used for preparing a water-soluble fertilizer containing humic acid according to any one of claims 1 to 6, characterized in that: The following steps are involved: a. Powder the raw materials into powder and add them into a blender, and mix them evenly to obtain fertilizer granules; b. Preparation of polyurethane materials and modified colloids; c. Under the action of a catalyst and a cross-linking agent, the polyurethane material and the modified colloid are cross-linked and cured to obtain a composite material, and the composite material is preheated to a molten state to obtain a coating liquid; d. Preheat the fertilizer particles in a drum or fluidized bed; e. After the coating liquid is atomized, it is evenly sprayed on the surface of the preheated fertilizer particles, cooled, and the coated fertilizer is made.
8. The method for preparing a water-soluble fertilizer containing humic acid according to claim 7, characterized in that: In step b, the preparation method of the modified colloid is: dissolving gelatin in water, adjusting the pH to less than 4, adding a modifier, stirring for 8 to 12 hours, adjusting the system to neutral after the reaction is completed, and drying to obtain the modified colloid.
9. The method for preparing a water-soluble fertilizer containing humic acid according to claim 7, characterized in that: Step a further comprises: powdering the raw materials into powder, adding the powder into a blender, mixing evenly, crushing to 60-80 mesh, adding an acidulant, stirring evenly, acidifying at room temperature, and adding a filler to adjust the viscosity and density of the system to obtain water-soluble fertilizer granules, wherein the acidulant is at least one of boric acid, phosphoric acid, and ethylene glycol.
10. The method for preparing a water-soluble fertilizer containing humic acid according to claim 7, characterized in that: In step c, the polyurethane material and the modified colloid are cross-linked and then cured using UV.