Plastic package mold

By designing a plastic packaging mold with bumps, the end of the extruded connection part away from the accommodation cavity forms a protruding part, which solves the problem of lead breakage caused by overflow of plastic packaging material, improves the yield rate of semiconductor products, and reduces manufacturing costs.

CN118737843APending Publication Date: 2024-10-01GREAT TEAM BACKEND FOUNDRY (DONGGUAN) LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310335285.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-03-30
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

During the plastic packaging process of semiconductor chips, the plastic packaging material overflows and remains on the edge of the lead frame, which may cause pin breakage and affect product yield.

Method used

Design a plastic sealing mold, including a first sub-mold and a second sub-mold. The first sub-mold has a bump. After the mold is closed, the bump squeezes the end of the connecting part away from the accommodation cavity, so that it extends in the away direction to form a bump. outlet to prevent the plastic material from flowing into the gap between the connecting part and the recess.

Benefits of technology

It effectively prevents plastic packaging materials from flowing into gaps, reduces product scrap rates, improves product yields, reduces lead frame dimensional accuracy requirements, and reduces manufacturing costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118737843A_ABST
    Figure CN118737843A_ABST
Patent Text Reader

Abstract

The invention provides a plastic package mold which is used for carrying out plastic package on a semiconductor structure. The semiconductor structure comprises an electrical element and a lead frame, the lead frame comprises a connecting part and a plurality of pins connected with the connecting part, and the pins are electrically connected with the electrical element. The plastic packaging mold comprises a first sub-mold and a second sub-mold, the first sub-mold comprises a first sub-mold body and protruding blocks, a groove is formed in the first butt joint face of the first sub-mold body, and the protruding blocks are arranged on the two sides of the groove respectively. And the second butt joint surface of the second sub-mold is provided with a recess. One of the first butt joint face and the second butt joint face is provided with a containing groove, and the other is provided with an abutting portion. After the first sub-mold and the second sub-mold are closed, the first butt joint face abuts against the second butt joint face to form a containing cavity for containing the electrical element, a runner communicated with the containing cavity and a containing part for containing part of the lead frame, and the protruding block is located in the containing part and located at the end, away from the containing cavity, of the containing part. The connecting part extends to form a convex part. The end part of the connecting part deviates from the accommodating cavity.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of semiconductor technology, and in particular to a plastic packaging mold. Background Art

[0002] Common semiconductor packaging technologies, such as chip packaging processes, may include the following steps: first, a lead frame is set on the front side of the chip, and the pins of the lead frame are electrically connected to the pads on the front side of the chip; then, the chip is plastic-sealed to form a plastic layer that encapsulates the chip, thereby obtaining a semiconductor structure including the chip, the lead frame and the plastic layer.

[0003] In the process of encapsulating the chip, a plastic encapsulation mold is usually used to encapsulate the chip. However, in the process of encapsulating the chip with the mold, a small amount of plastic encapsulation material will overflow and remain on the edge of the lead frame. In the subsequent cutting process of the semiconductor structure, the plastic encapsulation material on the edge of the lead frame may fall off and adhere to the pin of the lead frame. When there is plastic encapsulation material above the pin, the mold used for cutting presses on the plastic encapsulation material above the pin, which will cause the pin to break, thereby causing the product to be scrapped and affecting the product yield. Summary of the invention

[0004] The embodiment of the present application provides a plastic encapsulation mold. The plastic encapsulation mold is used to encapsulate a semiconductor structure; the semiconductor structure includes an electrical component and a lead frame located on one side of the electrical component, the lead frame includes a connecting portion and a plurality of pins, the plurality of pins are connected to the connecting portion, and the pins are electrically connected to the electrical component; the orthographic projection of the connecting portion on the plane where the surface of the electrical component is located is located outside the surface of the electrical component;

[0005] The plastic encapsulation mold includes a first sub-mold and a second sub-mold, the first sub-mold includes a first sub-mold body and a convex block, the first sub-mold body includes a first docking surface, the first docking surface is provided with a groove, and the two sides of the groove are respectively provided with the convex blocks; the second sub-mold includes a second sub-mold body, the second sub-mold body includes a second docking surface, and the second docking surface is provided with a recess; one of the first docking surface and the second docking surface is provided with a receiving groove, and the other is provided with an abutting portion; after the first sub-mold and the second sub-mold are molded together, the first docking surface abuts against the second docking surface, the edge of the receiving groove abuts against the abutting portion to form an accommodating cavity for accommodating the electrical component, a flow channel connected to the accommodating cavity is formed between the groove and the second docking surface, and an accommodating portion for accommodating part of the lead frame is formed between the recess and the first docking surface, the convex block is located in the accommodating portion and at one end of the accommodating portion away from the accommodating cavity, and is used to squeeze the end of the connecting portion away from the accommodating cavity so that the connecting portion extends in a direction away from the accommodating cavity to form a convex portion abutting against the side of the recess.

[0006] In one embodiment, the cross-sectional area of ​​the protrusion gradually decreases in a direction away from the first mating surface.

[0007] In one embodiment, the end surface of the protrusion facing away from the first butt joint surface is a curved surface, or the end surface of the protrusion facing away from the first butt joint surface is a flat surface.

[0008] In one embodiment, after the first sub-mold and the second sub-mold are molded together, there is a gap between the protrusion and the side of the recess facing away from the accommodating cavity.

[0009] In one embodiment, the protrusion is detachably disposed on the first sub-mold body.

[0010] In one embodiment, the first sub-mold body is provided with a slot, and the first sub-mold further comprises a connecting portion connected to the protrusion, and the connecting portion is embedded in the slot.

[0011] In one embodiment, in a direction perpendicular to the first docking surface, the difference between the size of the protrusion and the thickness of the end of the connecting portion away from the accommodating cavity is less than or equal to 0.1 mm, and the size of the protrusion is smaller than the thickness of the end of the connecting portion away from the accommodating cavity.

[0012] In one embodiment, in the direction in which the protrusion points to the groove, the size of the protrusion ranges from 0.5 mm to 1.2 mm.

[0013] In one embodiment, the distance between the protrusion and the adjacent groove is less than 0.2 mm.

[0014] In one embodiment, the semiconductor structure includes a plurality of the electrical components; the lead frame includes a plurality of pin groups, each of the pin groups includes a plurality of the pins, and each of the pins in the same pin group is electrically connected to the same electrical component;

[0015] The second docking surface is provided with a plurality of recesses arranged at intervals and a docking portion located between adjacent recesses; the plastic encapsulation mold is provided with a plurality of the accommodating grooves, a plurality of the grooves and a plurality of the docking portions; after the first module and the second sub-mold are molded together, a flow channel is formed between a docking portion and a groove, and the plastic encapsulation mold forms a plurality of the accommodating cavities, a plurality of the flow channels and a plurality of the accommodating portions.

[0016] The main technical effects achieved by the embodiments of the present application are:

[0017] The plastic encapsulation mold provided in the embodiment of the present application has protrusions on both sides of the groove in the first sub-mold. After the first sub-mold and the second sub-mold are closed, the protrusions squeeze the end of the connecting part away from the accommodating cavity so that the end of the connecting part away from the accommodating cavity extends in a direction away from the accommodating cavity to form a protrusion, and the protrusion abuts against the side of the recess away from the accommodating cavity. The protrusion can prevent the plastic encapsulation material in the flow channel from flowing to the gap between the end of the connecting part away from the accommodating cavity and the recess, thereby causing the product to be scrapped, which helps to improve the yield of the product. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 is a schematic structural diagram of a semiconductor structure provided by an exemplary embodiment of the present application;

[0019] Figure 2 is a top view of a first sub-mold provided by an exemplary embodiment of the present application;

[0020] Figure 3 yes Figure 2 The partial cross-sectional view of the first sub-mold shown is obtained by cutting along AA;

[0021] Figure 4 is a top view of a second sub-mold provided by an exemplary embodiment of the present application;

[0022] Figure 5 yes Figure 4 The partial cross-sectional view of the second sub-mold shown is obtained by cutting along BB;

[0023] Figure 6 is a top view of a semiconductor structure provided by an exemplary embodiment of the present application placed on a second sub-mold;

[0024] Figure 7 is a partial cross-sectional view of a first sub-mold and a second sub-mold after being molded together, provided by an exemplary embodiment of the present application;

[0025] Figure 8 yes Figure 1 A cross-sectional view of the protrusion shown is obtained by cutting along CC;

[0026] Fig. 9 yes Figure 1 Another cross-sectional view of the protrusion shown is obtained along CC. Specific embodiments

[0027] Exemplary embodiments will be described in detail herein, examples of which are shown in the accompanying drawings. When the following description refers to the drawings, unless otherwise indicated, the same numbers in different drawings represent the same or similar elements. The embodiments described in the following exemplary embodiments do not represent all embodiments consistent with the present application. Instead, they are merely examples of devices and methods consistent with some aspects of the present application as detailed in the appended claims.

[0028] The terms used in this application are for the purpose of describing specific embodiments only and are not intended to limit this application. The singular forms of "a", "said" and "the" used in this application and the appended claims are also intended to include plural forms unless the context clearly indicates other meanings. It should also be understood that the term "and / or" used herein refers to and includes any or all possible combinations of one or more associated listed items.

[0029] It should be understood that although the terms first, second, third, etc. may be used in the present application to describe various information, these information should not be limited to these terms. These terms are only used to distinguish the same type of information from each other. For example, without departing from the scope of the present application, the first information may also be referred to as the second information, and similarly, the second information may also be referred to as the first information. Depending on the context, the word "if" as used herein may be interpreted as "at the time of" or "when" or "in response to determining".

[0030] Some embodiments of the present application are described in detail below in conjunction with the accompanying drawings. In the absence of conflict, the following embodiments and features in the embodiments can be combined with each other.

[0031] The present application embodiment provides a plastic encapsulation mold. The plastic encapsulation mold is used to encapsulate a semiconductor structure. Figure 1 As shown, the semiconductor structure includes an electrical component 10 and a lead frame 20 located on one side of the electrical component 10, the lead frame 20 includes a connecting portion 21, a base island 23 and a plurality of pins 22, the plurality of pins 22 are connected to the connecting portion 21, and the pins 22 are electrically connected to the electrical component 10. The base island 23 is connected to the ends of the pins 22, and the base island 23 is used to carry the electrical component. The orthographic projection of the connecting portion 21 on the plane where the surface of the electrical component 10 is located is located outside the surface of the electrical component 10. The electrical component 10 can be a chip, the lead frame is located on the front side of the chip, and the pins 22 are electrically connected to the pads on the front side of the chip. In some embodiments, the lead frame 20 may not include the base island 23.

[0032] See again Figure 1, the semiconductor structure may include a plurality of electrical components 10 arranged in parallel. The connecting portion 21 includes a plurality of first connecting rods 211 and a plurality of second connecting rods 212. The extension direction of the first connecting rod 211 is the same as the extension direction of the pin 22, and the extension direction of the second connecting rod 212 may be perpendicular to the extension direction of the first connecting rod 211. The plurality of first connecting rods 211 divide the plurality of pins 22 into a plurality of pin groups, and each pin of a pin group is located between two adjacent first connecting rods 211. Each pin 22 in each pin group is electrically connected to the same electrical component 10. The pins 22 in a pin group are connected to two second connecting rods 212, one of the second connecting rods 212 is close to the electrical component 10, and the other second connecting rod 212 is connected to the end of the pin 22 away from the electrical component 10, and the two second connecting rods 212 are connected to the same first connecting rod 211.

[0033] like Figures 2 to 6 As shown, the plastic encapsulation mold includes a first sub-mold 30 and a second sub-mold 40. The first sub-mold 30 includes a first sub-mold body 31 and a protrusion 32. The first sub-mold body 31 includes a first docking surface 311. The first docking surface 311 is provided with a groove 312. The protrusions 32 are respectively provided on both sides of the groove 312. The second sub-mold 40 includes a second sub-mold body 41. The second sub-mold body 41 includes a second docking surface 411. The second docking surface 411 is provided with a recess 412. One of the first docking surface 311 and the second docking surface 411 is provided with a receiving groove 413, and the other is provided with an abutting portion 313. After the first sub-mold 30 and the second sub-mold 40 are molded together, the first docking surface 311 abuts against the second docking surface 411, and the edge of the accommodating groove 413 abuts against the abutting portion 313 to form an accommodating cavity for accommodating the electrical component 10, a flow channel connected to the accommodating cavity is formed between the groove 312 and the second docking surface 411, and an accommodating portion for accommodating part of the lead frame 20 is formed between the recess 412 and the first docking surface 311; the protrusion 32 is located in the accommodating portion and at one end of the accommodating portion away from the accommodating cavity, and is used to squeeze the end of the connecting portion 21 away from the accommodating cavity so that the connecting portion 21 extends in a direction away from the accommodating cavity to form a protrusion 213 abutting against the side of the recess 412.

[0034] Figures 2 to 5 In the illustrated embodiment, the receiving groove 413 is provided on the second docking surface 411 of the second sub-mold 40, and the abutting portion 313 is provided on the first docking surface 311 of the first sub-mold 30. In other embodiments, the receiving groove 413 may be provided on the first docking surface 311 of the first sub-mold 30, and the abutting portion 313 is provided on the second docking surface 411 of the second sub-mold 40.

[0035] When using a plastic encapsulation mold to encapsulate a semiconductor structure, if Figure 4 and Figure 5 As shown, the receiving groove 413 is provided on the second docking surface 411 of the second sub-mold 40, and the second docking surface 411 of the second sub-mold 40 can be directed upward. Figure 6 As shown, the semiconductor structure is placed on the second docking surface 411 of the second sub-mold 40, so that the electrical component 10 of the semiconductor structure is located in the receiving groove 413, a part of the pin 22 and the second connecting rod 212 are located in the recess 412, and the first connecting rod 211 of the connecting portion 21 is arranged on one side of the recess 412. Then, the first sub-mold 30 and the second sub-mold 40 are molded together, and the first docking surface 311 and the second docking surface 411 are abutted to form a receiving cavity, a flow channel and a receiving portion, and the electrical component 10 is located in the receiving cavity, and a part of the pin 22 and the second connecting rod 212 are located in the receiving portion. In order to enable a part of the pin 22 and the second connecting rod 212 to be smoothly placed in the recess 412 of the second sub-mold 40, considering the alignment deviation, in the length direction of the first connecting rod 211, the size of the recess 412 is usually larger than the size of the first connecting rod 211, so there is a gap between the end of the second connecting rod 212 away from the receiving cavity and the side of the recess 412 away from the receiving cavity.

[0036] like Figure 7 As shown, after the first sub-mold 30 and the second sub-mold 40 are molded together, the second abutting surface 411 of the second sub-mold 40 abuts against the edge of the groove 312 of the first sub-mold 30 through the first connecting rod 211, and there is no first connecting rod 211 below a small section of the groove 312, resulting in a leakage hole formed in the formed flow channel at this position. If the first sub-mold 30 is not provided with a protrusion 32, the gap between the second connecting rod 212 and the recess 212 is connected to the leakage hole, then when the plastic encapsulation material is injected into the accommodating cavity through the flow channel to encapsulate the electrical component 10, the plastic encapsulation material will flow through the leakage hole of the flow channel to the gap between the second connecting rod 212 and the recess 412 and remain on the edge of the second connecting rod 212.

[0037] In the plastic encapsulation mold provided in the embodiment of the present application, since the two sides of the groove 312 in the first sub-mold 30 are respectively provided with protrusions 32, after the first sub-mold 30 and the second sub-mold 40 are molded together, the protrusions 32 squeeze the end of the connecting portion 21 away from the accommodating cavity 51 (that is, the second connecting rod 212 in the connecting portion 21 away from the electrical component 10) to cause it to deform, such as Figure 6As shown, the end of the connecting portion 21 away from the accommodating cavity 51 extends in a direction away from the accommodating cavity 51 to form a protrusion 213, and the protrusion 213 abuts against the side of the recess 412 away from the accommodating cavity 51, which can prevent the plastic encapsulation material in the flow channel 52 from flowing to the gap between the end of the connecting portion 21 away from the accommodating cavity 51 and the side of the recess 412, thereby preventing the product from being scrapped, which helps to improve the yield of the product. In addition, the plastic encapsulation mold provided in the embodiment of the present application has a lower requirement for the width of the connecting portion of the lead frame. In the process of processing the lead frame, the dimensional accuracy of the lead frame can be appropriately reduced, which helps to reduce the manufacturing cost of the lead frame.

[0038] The encapsulation mold provided in the embodiment of the present application can be used to encapsulate the semiconductor structure and then cut to obtain a semiconductor product. During the cutting process, the connection portion of the lead frame is removed, and the semiconductor product finally obtained may include an electrical component. Although the width of the lead frame increases after the semiconductor structure is encapsulated, the mold used to cut the semiconductor structure can accommodate the lead frame with increased width, so the encapsulation process does not affect the subsequent cutting operation.

[0039] In one embodiment, the abutting portion 313 may be a plane. In other embodiments, the abutting portion 313 may be an annular convex structure. After the first sub-mold 30 and the second sub-mold 40 are molded together, the convex structure abuts against the edge area of ​​the receiving groove 413.

[0040] In one embodiment, Figure 4 and Figure 5 As shown, the second docking surface 411 is also provided with a docking portion 414, and the docking portion 414 is higher than the bottom surface of the recess 412. After the first sub-mold 30 and the second sub-mold 40 are molded together, a flow channel is formed between the docking portion 414 and the groove 312. Specifically, the first connecting rod 211 of the connecting portion 21 is located on the docking portion 414, and the first connecting rod 211 located on the docking portion 414 and a partial area of ​​the groove 312 are abutted to form a part of the flow channel, and a partial area of ​​the docking portion 414 where the first connecting rod 211 is not provided is abutted against other areas of the groove 312 to form a part of the flow channel. Figure 4 The dotted line in the figure is the docking portion 414. At least part of the area of ​​the second docking surface 411 where the recess 412 and the receiving groove 413 are not provided is a plane, the area of ​​the docking portion 414 between adjacent grooves 312 may be lower than the plane, and other areas of the docking portion 414 may be part of the plane.

[0041] Furthermore, if Figure 4 As shown, the second docking surface 411 is provided with a plurality of recesses 412 arranged at intervals and a plurality of docking portions 414, wherein the docking portion 414 is located between two adjacent recesses 412. Figure 2As shown, the first sub-mold 30 is provided with a plurality of grooves 312. The plurality of grooves 312 may correspond to the plurality of docking portions 414 one by one. After the first sub-mold 30 and the second sub-mold 40 are molded together, a flow channel is formed between each docking portion 414 and the corresponding groove 312; the plurality of recesses 412 are respectively in contact with the first docking surface 311 to form a plurality of accommodating portions.

[0042] In one embodiment, Figure 4 As shown, the recess 412 includes a first sub-recess 4121 and a second sub-recess 4122 located on the side of the first sub-recess 4121 away from the receiving groove 413, and the depth of the first sub-recess 4121 is greater than the depth of the second sub-recess 4122. When the connecting portion 21 is placed in the second sub-mold 40, the end of the connecting portion 21 away from the receiving cavity 51 (that is, the second connecting rod 212 in the connecting portion 21 away from the electrical component 10) is located in the second sub-recess 4122. The bottom surface of the second sub-recess 4122 and the area of ​​the docking portion 414 located before the adjacent recess 412 can be in the same plane.

[0043] In one embodiment, Figure 2 As shown, the first butting surface 311 of the first sub-mold 30 is provided with a plurality of abutting portions 313. Figure 4 As shown, the second docking surface 411 is provided with a plurality of receiving grooves 413. The plurality of abutting portions 313 may correspond to the plurality of receiving grooves 413 one by one. After the first sub-mold 30 and the second sub-mold 40 are molded together, each abutting portion 313 abuts against the edge of the corresponding receiving groove 413, thereby forming a plurality of receiving cavities.

[0044] In one embodiment, Figure 2 As shown, the groove 312 includes a first sub-groove 3121 and two second sub-grooves 3122. The two second sub-grooves 3122 are located on the side of the first sub-groove 3121 away from the bump 32, and the two sub-grooves 3122 are connected to the end of the first sub-groove 3121 away from the bump 32. After the first sub-mold 30 and the second sub-mold 40 are molded together, the two sub-grooves 3122 of the same groove 312 are respectively connected to one accommodating cavity, and the two accommodating cavities connected to the same groove are adjacent.

[0045] In one embodiment, Figure 2 As shown, the first sub-mold 30 is provided with a plurality of first material channels 314; Figure 4As shown, the second sub-mold 40 is provided with a plurality of second material channels 415. The plurality of first material channels 314 may correspond to the plurality of second material channels 415 one by one. After the first sub-mold 30 and the second sub-mold 40 are molded together, each first material channel 314 is connected with the corresponding second material channel 415 to form a raw material cavity, and the raw material cavity is connected with the flow channel. The plastic encapsulation mold also includes an extruder rod. After the first sub-mold 30 and the second sub-mold 40 are molded together, the extruder rod squeezes the plastic encapsulation material in the raw material cavity into the flow channel, so that the plastic encapsulation material enters the accommodating cavity through the flow channel to form a plastic encapsulation layer that encapsulates the electrical component 10.

[0046] In one embodiment, Figure 8 and Fig. 9 As shown, in the direction away from the first docking surface 311, the cross-sectional area of ​​the protrusion 32 gradually decreases. When the semiconductor structure is encapsulated by the encapsulation mold, the semiconductor structure is first placed on the second docking surface of the second sub-mold 40, and then the first sub-mold 30 and the second sub-mold 40 are molded together. At this time, the protrusion 32 abuts against the end of the connecting portion 21 away from the accommodating cavity, and squeezes the end of the connecting portion 21 away from the accommodating cavity, so that the end of the connecting portion 21 away from the accommodating cavity extends in the direction away from the accommodating cavity to form a protrusion 213. By setting the cross-sectional area of ​​the protrusion 32 to gradually decrease in the direction away from the first docking surface 311, the contact area between the protrusion 32 and the connecting portion 21 gradually increases during the process of the first sub-mold 30 and the second sub-mold 40 being molded together, which is more conducive to the protrusion 32 to squeeze and deform the end of the connecting portion 21 away from the accommodating cavity.

[0047] In one embodiment, Figure 8 As shown, the end surface of the protrusion 32 away from the first docking surface 311 is an arc surface. By setting the end surface of the protrusion 32 away from the first docking surface 311 as an arc surface, it is more helpful for the protrusion 32 to press the end of the connecting part 21 away from the accommodating cavity to form a protrusion 213.

[0048] In another embodiment, Fig. 9 As shown, the end surface of the protrusion 32 facing away from the first docking surface 311 is a plane.

[0049] In one embodiment, after the first sub-mold 30 and the second sub-mold 40 are molded together, there is a gap between the protrusion 32 and the side of the recess 412 away from the accommodating cavity. In this way, the contact area between the protrusion 32 and the connecting portion 21 can be ensured to be large, thereby ensuring that the end of the connecting portion 21 away from the accommodating cavity is squeezed to form a protrusion 213.

[0050] Furthermore, after the first sub-mold 30 and the second sub-mold 40 are molded together, the distance between the protrusion 32 and the side of the recess 412 away from the protrusion 32 is less than or equal to the width of the connecting portion 21. The width of the connecting portion 21 refers to the dimension in the extension direction of the pin 22. Such an arrangement can ensure that after the first sub-mold 30 and the second sub-mold 40 are molded together, the end of the protrusion 32 away from the first docking surface 311 is all in contact with the connecting portion 21, which is more conducive to the end of the connecting portion 21 away from the accommodating cavity being squeezed to form a protrusion 213.

[0051] In one embodiment, the protrusion 32 is detachably disposed on the first sub-mold body 31. After the protrusion 32 is used for a large number of times, the end of the protrusion 32 away from the first docking surface 311 will be worn, which will result in a poor squeezing effect of the protrusion 32 on the connecting portion 21, and the formed protrusion 213 cannot effectively prevent the plastic packaging material from entering the gap between the connecting portion 21 and the side of the recess 412. Since the protrusion 32 is detachably disposed on the first sub-mold body 31, the above problem can be solved by replacing the protrusion 32, which helps to ensure the squeezing effect of the protrusion 32 on the connecting portion 21.

[0052] In one embodiment, the first sub-mold body 31 is provided with a slot, and the first sub-mold 30 further includes a connecting portion connected to the protrusion 32, and the connecting portion is embedded in the slot. With such a configuration, when the protrusion 32 needs to be replaced, the connecting portion can be taken out of the slot, and the replacement of the protrusion 32 is easy and easy to operate. For example, the slot of the first sub-mold body 31 can be in a cubic shape, and the connecting portion can also be in a cubic shape.

[0053] In one embodiment, in a direction perpendicular to the first butting surface 311, the difference between the size of the protrusion 32 and the thickness of the end of the connecting portion 21 away from the accommodating cavity is less than or equal to 0.1 mm, and the size of the protrusion 32 is smaller than the thickness of the end of the connecting portion 21 away from the accommodating cavity. This arrangement can prevent the size of the protrusion 32 from being too small, resulting in the protrusion 213 formed by the protrusion 32 squeezing the end of the connecting portion 21 unable to abut against the side of the recess 412 away from the accommodating cavity, and can also prevent the size of the protrusion 32 from being too large, resulting in serious deformation of the connecting portion 21, or even the disconnection of the protrusion 213 from the connecting portion 21.

[0054] In one embodiment, the projection 32 points to the groove 312, that is, Figure 3In the X direction shown, the size of the protrusion 32 ranges from 0.5 mm to 1.2 mm. This arrangement can prevent the size of the protrusion 32 from being too small, resulting in a small degree of extrusion deformation of the end of the connecting portion 21, and the formed protrusion 213 cannot effectively prevent the plastic packaging material from entering the gap between the connecting portion 21 and the side of the recess 412. It can also prevent the size of the protrusion 32 from being too large, resulting in serious deformation of the connecting portion 21. In some embodiments, in the direction in which the protrusion 32 points to the recess 312, the size of the protrusion 32 can be 0.5 mm, 0.7 mm, 0.9 mm, 1.0 mm, 1.2 mm, etc.

[0055] In one embodiment, in a direction perpendicular to the direction in which the protrusion 32 points to the groove 312 and parallel to the first docking surface 311, that is, in a direction perpendicular to the direction in which the protrusion 32 points to the groove 312 and parallel to the first docking surface 311, Figure 3 In the Y direction shown, the size of the protrusion 32 ranges from 0.2 mm to 0.6 mm. This arrangement can prevent the end of the connection portion 21 from being squeezed and deformed to a lesser extent, and the formed protrusion 213 cannot effectively prevent the plastic packaging material from entering the gap between the connection portion 21 and the side of the recess 412. It can also prevent the size of the protrusion 32 from being too large, resulting in serious deformation of the connection portion 21. In some embodiments, in the direction perpendicular to the direction in which the protrusion 32 points to the recess 312, the size of the protrusion 32 can be 0.2 mm, 0.25 mm, 0.3 mm, 0.35 mm, 0.4 mm, 0.45 mm, 0.5 mm, 0.55 mm, 0.6 mm, etc.

[0056] In one embodiment, the distance between the protrusion 32 and the adjacent groove 312 is less than 0.2 mm. This arrangement can avoid the problem that the distance between the protrusion 32 and the adjacent groove 312 is too large, the plastic encapsulation material in the flow channel enters the gap between the protrusion 32 and the groove 312 and adheres to the connecting portion 21, thereby causing the yield of the product to decrease. In some embodiments, the distance between the protrusion 32 and the adjacent groove 312 can be 0, 0.05 mm, 0.1 mm, 0.15 mm, 0.2 mm, etc.

[0057] It should be noted that in the accompanying drawings, the sizes of layers and regions may be exaggerated for clarity of illustration. It is also understood that when an element or layer is referred to as being "on" another element or layer, it may be directly on the other element, or there may be an intermediate layer. In addition, it is understood that when an element or layer is referred to as being "under" another element or layer, it may be directly under the other element, or there may be more than one intermediate layer or element. In addition, it is also understood that when a layer or element is referred to as being "between" two layers or two elements, it may be the only layer between the two layers or two elements, or there may also be more than one intermediate layer or element. Similar reference numerals throughout the text indicate similar elements.

[0058] Those skilled in the art will readily appreciate other embodiments of the present application after considering the description and practicing the contents disclosed herein. The present application is intended to cover any variations, uses or adaptations of the present application, which follow the general principles of the present application and include common knowledge or customary techniques in the art that are not disclosed in the present application. The description and examples are intended to be exemplary only, and the true scope and spirit of the present application are indicated by the following claims.

[0059] It should be understood that the present application is not limited to the precise structures that have been described above and shown in the drawings, and that various modifications and changes may be made without departing from the scope thereof. The scope of the present application is limited only by the appended claims.

Claims

1. A plastic encapsulation mold, It is characterized in that Used for plastic encapsulating a semiconductor structure; the semiconductor structure comprises an electrical component and a lead frame located on one side of the electrical component, the lead frame comprises a connecting portion and a plurality of pins, the plurality of pins are connected to the connecting portion, and the pins are electrically connected to the electrical component; the orthographic projection of the connecting portion on the plane where the surface of the electrical component is located is located outside the surface of the electrical component; The plastic encapsulation mold includes a first sub-mold and a second sub-mold, the first sub-mold includes a first sub-mold body and a convex block, the first sub-mold body includes a first docking surface, the first docking surface is provided with a groove, and the two sides of the groove are respectively provided with the convex blocks; the second sub-mold includes a second sub-mold body, the second sub-mold body includes a second docking surface, and the second docking surface is provided with a recess; one of the first docking surface and the second docking surface is provided with a receiving groove, and the other is provided with an abutting portion; after the first sub-mold and the second sub-mold are molded together, the first docking surface abuts against the second docking surface, the edge of the receiving groove abuts against the abutting portion to form an accommodating cavity for accommodating the electrical component, a flow channel connected to the accommodating cavity is formed between the groove and the second docking surface, and an accommodating portion for accommodating part of the lead frame is formed between the recess and the first docking surface, the convex block is located in the accommodating portion and at one end of the accommodating portion away from the accommodating cavity, and is used to squeeze the end of the connecting portion away from the accommodating cavity so that the connecting portion extends in a direction away from the accommodating cavity to form a convex portion abutting against the side of the recess.

2. The plastic encapsulation mold according to claim 1, It is characterized in that In a direction away from the first butting surface, the cross-sectional area of ​​the protrusion gradually decreases.

3. The plastic encapsulation mold according to claim 2, It is characterized in that The end surface of the protrusion facing away from the first butt joint surface is a curved surface, or the end surface of the protrusion facing away from the first butt joint surface is a flat surface.

4. The plastic encapsulation mold according to claim 1, It is characterized in that After the first sub-mold and the second sub-mold are molded together, a gap exists between the protrusion and the side of the recess facing away from the accommodating cavity.

5. The plastic encapsulation mold according to claim 1, It is characterized in that The protrusion is detachably arranged on the first sub-mold body.

6. The plastic encapsulation mold according to claim 5, It is characterized in that The first sub-mold body is provided with a slot, and the first sub-mold further comprises a connecting portion connected to the protrusion, and the connecting portion is embedded in the slot.

7. The plastic encapsulation mold according to claim 1, It is characterized in that In a direction perpendicular to the first docking surface, the difference between the size of the protrusion and the thickness of the end of the connecting portion away from the accommodating cavity is less than or equal to 0.1 mm, and the size of the protrusion is smaller than the thickness of the end of the connecting portion away from the accommodating cavity.

8. The plastic encapsulation mold according to claim 1, It is characterized in that In the direction in which the protrusion points to the groove, the size of the protrusion ranges from 0.5 mm to 1.2 mm.

9. The plastic encapsulation mold according to claim 1, It is characterized in that The distance between the protrusion and the adjacent groove is less than 0.2 mm.

10. The plastic encapsulation mold according to claim 1, It is characterized in that The semiconductor structure comprises a plurality of the electrical components; the lead frame comprises a plurality of pin groups, each of the pin groups comprises a plurality of the pins, and each of the pins of the same pin group is electrically connected to the same electrical component; The second docking surface is provided with a plurality of recesses arranged at intervals and a docking portion located between adjacent recesses; the plastic encapsulation mold is provided with a plurality of the accommodating grooves, a plurality of the grooves and a plurality of the docking portions; after the first module and the second sub-mold are molded together, a flow channel is formed between a docking portion and a groove, and the plastic encapsulation mold forms a plurality of the accommodating cavities, a plurality of the flow channels and a plurality of the accommodating portions.