Resonator, resonance device, and resonator manufacturing method
Patent Information
- Application Number
- CN202280092684.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-02-28
- Filing Date
- 2022-09-02
- Publication Date
- 2024-10-11
AI Technical Summary
[0007]然而,在现有的方法中,存在以下担心:很难比以往更多地提高杂质的浓度,或者由于残留于硅晶片的表面的碳(C)等污染物质而使杂质失活,从而妨碍电阻率的降低
[0014] According to the present invention, the resistivity of the vibrating part can be reduced compared with the conventional ones.
Smart Images

Figure CN118765485A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a resonator, a resonant device and a method for manufacturing the resonator. Background Art
[0002] In the past, resonant devices using MEMS (Micro Electro Mechanical Systems) technology were used, for example, as timing devices. The resonant device is mounted on a printed circuit board assembled in electronic devices such as smartphones. The resonant device includes: a lower substrate; an upper substrate, a cavity formed between the lower substrate and the upper substrate; and a resonator, which is arranged in the cavity between the lower substrate and the upper substrate.
[0003] Resonators are generally manufactured from semiconductor wafers such as silicon (Si) wafers. For example, Patent Document 1 discloses the following method for manufacturing semiconductor wafers: the diffusion source of N-type impurities of the wafer in the first diffusion process is phosphorus of phosphorus oxychloride, the vapor of phosphorus oxychloride is continuously supplied together with Ar gas containing 0.5% or more O2 gas, the temperature is maintained between 1100°C and 1300°C, and the time required for diffusion is continued.
[0004] Patent Document 1: Japanese Patent Application Laid-Open No. 11-8201
[0005] However, it is known that by using a silicon substrate having a low electrical resistivity (hereinafter simply referred to as “resistivity”) for the vibration portion of the resonator, the resonant frequency of the resonator can have a so-called frequency-temperature characteristic that is improved, in which the rate of change of the resonant frequency with respect to temperature change is reduced.
[0006] In order to form a silicon substrate with low resistivity, there is known a method of doping a silicon wafer with impurities (dopant) such as phosphorus (P).
[0007] However, in the conventional methods, there is a concern that it is difficult to increase the concentration of impurities more than before, or that contaminants such as carbon (C) remaining on the surface of the silicon wafer may inactivate the impurities and hinder the reduction of resistivity. Summary of the invention
[0008] The present invention has been made in view of the above circumstances, and one object of the present invention is to provide a resonator, a resonator device, and a resonator manufacturing method capable of reducing the resistivity of a vibrating portion compared with conventional ones.
[0009] A resonator according to one aspect of the present invention includes a vibrating portion configured to vibrate in a predetermined vibration mode as a main vibration, and formed on a silicon substrate containing phosphorus, wherein the concentration of phosphorus in the silicon substrate is 1.1×10 20 [1 / cm 3 ], the carbon concentration of the silicon substrate is 1.1×1018 [1 / cm 3 ]the following.
[0010] A resonator according to another aspect of the present invention includes a vibrating portion configured to vibrate in a predetermined vibration mode as a main vibration, and formed on a silicon substrate containing phosphorus, wherein the concentration of phosphorus in the silicon substrate is 110 times or more the concentration of carbon.
[0011] A resonator according to still another aspect of the present invention includes a vibrating portion configured to vibrate in a predetermined vibration mode as a main vibration, and formed on a silicon substrate containing phosphorus, wherein the resistivity of the silicon substrate is 0.60 [mΩ·cm] or less.
[0012] A resonance device according to one aspect of the present invention includes a cover and the above-described resonator.
[0013] A resonator manufacturing method according to one aspect of the present invention includes: a process of preparing a silicon wafer to which phosphorus is added; a process of heating the silicon wafer in an oxygen atmosphere to form a silicon oxide film; a process of removing the silicon oxide film from the silicon wafer; a process of forming a silicon substrate by performing the process of forming the silicon oxide film and the process of removing the silicon oxide film one or more times; and a process of forming a vibration portion on the silicon substrate that is configured to vibrate in a predetermined vibration mode as a main vibration.
[0014] According to the present invention, the resistivity of the vibration portion can be lowered compared with the related art. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 It is a perspective view schematically showing the appearance of the resonance device according to the first embodiment.
[0016] Figure 2 It is a rough representation Figure 1 An exploded perspective view of the structure of the resonance device shown.
[0017] Figure 3 It is a rough representation Figure 2 A top view of the resonator configuration is shown.
[0018] Figure 4 It is a rough representation Figures 1 to 3 The structure of the resonant device shown is a cross-sectional view taken along line IV-IV.
[0019] Figure 5 1 is a flowchart showing the resonator manufacturing method according to the first embodiment.
[0020] Figure 6 It is used for Figure 5 A conceptual diagram for explaining an example of the process is shown.
[0021] Figure 7 It is used for Figure 5 A conceptual diagram for explaining another example of the process shown.
[0022] Figure 8 It is used for Figure 5 A conceptual diagram for explaining the process shown.
[0023] Fig. 9 Is used for not Figure 5 A conceptual diagram for explaining the process conditions shown.
[0024] Fig.10 It is used for Figure 5 A conceptual diagram for explaining the process shown.
[0025] Fig.11 It is used for Figure 5 A conceptual diagram for explaining the process shown.
[0026] Fig.12 It is used for Figure 5 A conceptual diagram for explaining the process shown.
[0027] Fig.13 This is a graph showing the concentrations of phosphorus (P) and carbon (C) in the silicon substrate in the first embodiment.
[0028] Fig.14 The silicon substrate and Figure 6 A graph of the resistivity of a silicon wafer is shown.
[0029] Fig.15 The silicon substrate and Figure 6 A table of silicon wafers for comparison is shown.
[0030] Fig.16 1 is a flowchart showing a method for manufacturing a resonator according to the second embodiment.
[0031] Fig.17 It is used for Fig.16 The steps shown are cross-sectional views for explaining the process.
[0032] Fig.18 It is used for Fig.16 The steps shown are cross-sectional views for explaining the process.
[0033] Fig.19 It is used for Fig.16 A cross-sectional view illustrating an example of the process shown.
[0034] Fig. 20 It is used for Fig.16 A cross-sectional view illustrating another example of the process is shown. DETAILED DESCRIPTION
[0035] The following is an explanation of the embodiments of the present invention. In the following drawings, the same or similar reference numerals are used to represent the same or similar structural elements. The drawings are illustrative, and the size and shape of each part are schematic, and the technical scope of the present invention should not be limited to the embodiments.
[0036] <First embodiment>
[0037] First, refer to Figure 1 as well as Figure 2 , a schematic structure of a resonance device according to a first embodiment of the present invention is described. Figure 1 It is a perspective view schematically showing the appearance of the resonance device 1 according to the first embodiment. Figure 2 It is a rough representation Figure 1 The structure of the resonance device 1 is shown in an exploded perspective view.
[0038] The resonance device 1 includes a lower cover 20, a resonator 10 (hereinafter, the lower cover 20 and the resonator 10 are also collectively referred to as a "MEMS substrate 50"), and an upper cover 30. That is, the resonance device 1 is formed by sequentially stacking the MEMS substrate 50, the bonding portion 60, and the upper cover 30. The upper cover 30 is an example of the "cover body" of the present invention.
[0039] Hereinafter, each structure of the resonance device 1 will be described. In the following description, the side of the resonance device 1 provided with the upper cover 30 is referred to as the upper side (or the front side), and the side provided with the lower cover 20 is referred to as the lower side (or the back side).
[0040] The resonator 10 is a MEMS vibrator manufactured using MEMS technology. The resonator 10 is bonded to the lower cover 20 and the upper cover 30 so as to seal the resonator 10 and form a vibration space of the resonator 10. In addition, the resonator 10, the lower cover 20, and the upper cover 30 are respectively formed using a silicon (Si) substrate (hereinafter referred to as a "Si substrate"), and the Si substrates are bonded to each other. In addition, the resonator 10, the lower cover 20, and the upper cover 30 can also be formed using an SOI (Silicon On Insulator) substrate stacked with a silicon layer and a silicon oxide film. In particular, the resonator 10 and the lower cover 20 can also be formed integrally using a CSOI (Cavity SOI) substrate.
[0041] The upper cover 30 includes a bottom plate 32 in a rectangular flat plate shape arranged along the XY plane, and a side wall 33 extending from the peripheral edge of the bottom plate 22 in the Z-axis direction. In the upper cover 30, a recess 31 is formed on the surface facing the resonator 10, which is divided by the surface of the bottom plate 32 and the inner surface of the side wall 23. The recess 31 forms at least a part of the vibration space, which is a space for the resonator 10 to vibrate. In addition, a getter layer 34 described later is formed on the surface of the recess 31 of the upper cover 30 on the side of the resonator 10. In addition, the upper cover 30 may not have the recess 31, but may have a flat plate-like structure.
[0042] The lower cover 20 has a bottom plate 22 in the shape of a rectangular plate arranged along the XY plane, and a side wall 23 extending from the peripheral edge of the bottom plate 22 in the Z-axis direction, that is, the stacking direction of the lower cover 20 and the resonator 10. In the lower cover 20, a recess 21 formed by the surface of the bottom plate 22 and the inner surface of the side wall 23 is formed in the surface opposite to the resonator 10. The recess 21 forms at least a part of the vibration space of the resonator 10. In addition, the lower cover 20 may not have the recess 21, but may have a flat plate-like structure. In addition, a getter layer may be formed on the surface of the recess 21 of the lower cover 20 on the resonator 10 side.
[0043] By bonding the upper cover 30, the resonator 10, and the lower cover 20, the vibration space of the resonator 10 is hermetically sealed and maintained in a vacuum state. The vibration space may be filled with a gas such as an inert gas, for example.
[0044] Next, refer to Figure 3 , a schematic structure of a resonator included in the resonance device according to the first embodiment of the present invention is described. Figure 3 It is a rough representation Figure 2 The structure of the resonator 10 is shown in a top view.
[0045] like Figure 3 As shown, the resonator 10 is a MEMS vibrator manufactured using MEMS technology. Figure 3Out-of-plane vibration is performed in the XY plane of the orthogonal coordinate system. In addition, the resonator 10 is not limited to a resonator using an out-of-plane bending vibration mode, and can be constructed to vibrate in a specified vibration mode as a main vibration (hereinafter, also referred to as a "main mode"). The resonator of the resonance device 1 can also use, for example, an extended vibration mode, a thickness longitudinal vibration mode, a Lamb wave vibration mode, an in-plane bending vibration mode, and a surface wave vibration mode. These vibrators are used in, for example, timing devices, RF filters, duplexers, ultrasonic transducers, angular velocity sensors (gyro sensors), acceleration sensors, etc. In addition, it can also be used for piezoelectric mirrors with actuator functions, piezoelectric gyroscopes, piezoelectric microphones with pressure sensor functions, ultrasonic vibration sensors, etc. Furthermore, it can also be applied to electrostatic MEMS elements, electromagnetically driven MEMS elements, and piezoresistive MEMS elements.
[0046] The resonator 10 includes a vibrating portion 120 , a holding portion 140 , and a supporting arm 110 .
[0047] The holding part 140 is formed in a rectangular frame shape so as to surround the outer side of the vibration part 120 along the XY plane. For example, the holding part 140 is formed integrally with a prism-shaped frame body. In addition, the holding part 140 can be provided at least partially around the vibration part 120, and is not limited to a frame shape.
[0048] The support arm 110 is provided inside the holding portion 140 , and connects the vibration portion 120 and the holding portion 140 .
[0049] The vibration part 120 is provided inside the holding part 140, and a space is formed at a predetermined interval between the vibration part 120 and the holding part 140. Figure 3 In the example shown, the vibration part 120 includes a base 130 and four vibration arms 135A to 135D (hereinafter collectively referred to as "vibration arms 135"). The number of vibration arms is not limited to four, and may be set to any number of one or more, for example. In the present embodiment, each vibration arm 135A to 135D is formed integrally with the base 130.
[0050] In a plan view, the base 130 has long sides 131a and 131b in the X-axis direction and short sides 131c and 131d in the Y-axis direction. The long side 131a is one side of the surface of the front end of the base 130 (hereinafter, also referred to as "front end 131A"), and the long side 131b is one side of the surface of the rear end of the base 130 (hereinafter, also referred to as "rear end 131B"). In the base 130, the front end 131A and the rear end 131B are arranged to face each other.
[0051] The base 130 is connected to the vibration arm 135 at the front end 131A and to the support arm 110 described later at the rear end 131B. Figure 3In the example shown, the base 130 has a substantially rectangular shape when viewed from above, but is not limited thereto. The base 130 may be formed to be substantially plane-symmetrical with respect to a virtual plane P defined by a perpendicular bisector along the long side 131a. For example, the base 130 may be a trapezoid in which the long side 131b is shorter than 131a, or may be in the shape of a semicircle with the long side 131a as the diameter. In addition, the surfaces of the base 130 are not limited to flat surfaces, but may be curved surfaces. In addition, the virtual plane P is a plane passing through the center of the direction in which the vibration arms 135 in the vibration portion 120 are arranged.
[0052] In the base 130, the longest distance between the front end 131A and the rear end 131B in the direction from the front end 131A to the rear end 131B, that is, the base length, is about 35 μm. In addition, in the width direction orthogonal to the base length direction, the longest distance between the side ends of the base 130, that is, the base width, is about 265 μm.
[0053] The vibration arms 135 extend in the Y-axis direction and have the same size. The vibration arms 135 are respectively arranged between the base 130 and the holding portion 140 in parallel with the Y-axis direction, one end of which is connected to the front end 131A of the base 130 to become a fixed end, and the other end becomes an open end. In addition, the vibration arms 135 are respectively arranged in parallel at a predetermined interval in the X-axis direction. In addition, for example, the width of the vibration arm 135 in the X-axis direction is about 50 μm, and the length in the Y-axis direction is about 465 μm.
[0054] The width of each vibration arm 135 in the X-axis direction is wider than that of other parts of the vibration arm 135, for example, at a portion of about 150 μm from the open end. The portion with the wider width is called a weight portion G. In the weight portion G, for example, the width is wider by 10 μm to the left and right along the X-axis direction compared to other parts of the vibration arm 135, and the width in the X-axis direction is about 70 μm. The weight portion G is formed integrally with the vibration arm 135 through the same process. By forming the weight portion G, the weight per unit length of the vibration arm 135 is heavier on the open end side than on the fixed end side. Therefore, by having the weight portion G on the open end side of each vibration arm 135, the amplitude of the vibration in the up and down directions of each vibration arm can be increased.
[0055] A protective film 235 described later is formed on the surface of the vibration part 120 (the surface facing the upper cover 30) so as to cover the entire surface. In addition, a frequency adjustment film 236 is formed on the surface of the protective film 235 at the front end of the open end side of the vibration arms 135A to 135D. The resonant frequency of the vibration part 120 can be adjusted by the protective film 235 and the frequency adjustment film 236.
[0056] In addition, in the present embodiment, substantially the entire surface of the resonator 10 (the surface on the side facing the upper cover 30) is covered by the protective film 235. Furthermore, substantially the entire surface of the protective film 235 is covered by the parasitic capacitance reducing film 240. However, the protective film 235 only needs to cover at least the vibration arm 135, and is not limited to a structure that covers substantially the entire surface of the resonator 10.
[0057] Next, refer to Figure 4 , the stacked structure of the resonance device 1 according to the first embodiment of the present invention will be described. Figure 4 It is a rough representation Figures 1 to 3 The structure of the resonance device 1 shown is a cross-sectional view taken along line IV-IV.
[0058] like Figure 4 As shown, the resonator device 1 is formed by joining the holding portion 140 of the resonator 10 to the side wall 23 of the lower cover 20, and further joining the holding portion 140 of the resonator 10 to the side wall 33 of the upper cover 30. In this way, the resonator 10 is held between the lower cover 20 and the upper cover 30, and a vibration space for the vibration portion 120 to vibrate is formed by the lower cover 20, the upper cover 30, and the holding portion 140 of the resonator 10. In addition, a terminal T4 is formed on the upper surface of the upper cover 30 (the surface opposite to the surface facing the resonator 10). The terminal T4 and the resonator 10 are electrically connected by the through electrode V3, the connection wiring 70, and the contact electrodes 76A and 76B.
[0059] The upper cover 30 is formed of a Si substrate L3 having a predetermined thickness. The upper cover 30 is bonded to the holding portion 140 of the resonator 10 at its peripheral edge portion (side wall 33) through a bonding portion 60 described later. The surface of the upper cover 30 that faces the resonator 10 is covered with a silicon oxide film L31. The silicon oxide film L31 is, for example, silicon dioxide (SiO2), and is formed on the surface of the Si substrate L3 by oxidation of the surface of the Si substrate L3 and chemical vapor deposition (CVD: Chemical Vapor Deposition). In addition, it is preferred that the back surface of the upper cover 30 and the side surface of the through electrode V3 are also covered with the silicon oxide film L31.
[0060] In addition, a getter layer 34 is formed on the surface of the concave portion 31 of the upper cover 30 on the side facing the resonator 10. The getter layer 34 is formed of, for example, titanium (Ti) or the like, and absorbs exhaust gas generated in the vibration space. In the upper cover 30 of the present embodiment, the getter layer 34 is formed on substantially the entire surface of the surface facing the resonator 10 in the concave portion 31, so that the reduction in the vacuum degree of the vibration space can be suppressed.
[0061] In addition, a conductive material is filled in the through hole formed in the upper cover 30 to form a through electrode V3 of the upper cover 30. The conductive material filled is, for example, polysilicon (Poly-Si) doped with impurities, copper (Cu), gold (Au), single crystal silicon doped with impurities, etc. The through electrode V3 functions as a wiring that electrically connects the terminal T4 to the connection wiring 70.
[0062] The bottom plate 22 and the side wall 23 of the lower cover 20 are integrally formed by the Si wafer L1. In addition, the lower cover 20 is bonded to the holding portion 140 of the resonator 10 through the upper surface of the side wall 23. The thickness of the lower cover 20 specified in the Z-axis direction is, for example, 150 μm, and the depth of the recess 21 is, for example, 50 μm. In addition, the Si wafer L1 is formed of non-degenerate silicon, and its resistivity is, for example, 16 mΩ·cm or more.
[0063] The vibration part 120, the holding part 140 and the support arm 110 in the resonator 10 are integrally formed by the same process. The resonator 10 has a piezoelectric film F3 formed on a Si substrate F2 so as to cover the Si substrate F2, and a metal layer E2 is further stacked on the piezoelectric film F3. Moreover, a piezoelectric film F3 is stacked on the metal layer E2 so as to cover the metal layer E2, and a metal layer E1 is further stacked on the piezoelectric film F3. A protective film 235 is stacked on the metal layer E1 so as to cover the metal layer E1, and a parasitic capacitance reduction film 240 is stacked on the protective film 235. For example, by dry etching by irradiating an argon (Ar) ion beam, the stack composed of the above-mentioned Si substrate F2, the piezoelectric film F3, the metal layer E2, the metal layer E1, the protective film 235, etc. is removed and patterned, thereby forming the outer shapes of the holding part 140, the base 130, the vibration arm 135 and the support arm 110.
[0064] The Si substrate F2 may be formed of a degenerate n-type silicon (Si) semiconductor having a thickness of about 6 μm, for example. Degenerate silicon (Si) contains phosphorus (P) as an n-type dopant. In this embodiment, the Si substrate F2 is an example of a silicon substrate described later, and the details are described later.
[0065] The Si substrate F2 is degenerate silicon (Si), and by using a degenerate silicon substrate with a low resistance value, for example, the Si substrate F2 itself can also function as the lower electrode of the resonator 10. In this case, the above-mentioned metal layer E2 is omitted.
[0066] A silicon oxide layer F21 of silicon dioxide (SiO2) is formed on the lower surface of the Si substrate F2 as an example of a temperature characteristic correction layer. Thus, the temperature characteristics can be improved. In addition, the silicon oxide layer F21 can also be formed on the upper surface of the Si substrate F2, or on both the upper surface and the lower surface of the Si substrate F2.
[0067] The thickness of the metal layers E1 and E2 is, for example, about 0.1 μm or more and 0.2 μm or less. After film formation, the metal layers E1 and E2 are patterned into a desired shape by etching or the like. The metal layers E1 and E2 use a metal having a body-centered cubic crystal structure. Specifically, the metal layers E1 and E2 are formed using Mo (molybdenum), tungsten (W), or the like.
[0068] The metal layer E1 is formed on the vibration part 120 to function as an upper electrode, for example. Also, the metal layer E1 is formed on the support arm 110 and the holding part 140 to function as a wiring for connecting the upper electrode to an AC power source provided outside the resonator 10 .
[0069] On the other hand, the metal layer E2 is formed on the vibration part 120 to realize the function of the lower electrode. In addition, the metal layer E2 is formed on the support arm 110 and the holding part 140 to realize the function of the wiring for connecting the lower electrode to the circuit provided outside the resonator 10.
[0070] The piezoelectric film F3 is a piezoelectric film that converts an applied voltage into vibration. The piezoelectric film F3 is formed of a material having a wurtzite-type hexagonal crystal structure, and can be composed of nitrides and oxides such as aluminum nitride (AlN), scandium aluminum nitride (ScAlN), zinc oxide (ZnO), gallium nitride (GaN), and indium nitride (InN) as main components. In addition, scandium aluminum nitride is obtained by replacing part of the aluminum in aluminum nitride with scandium, and scandium can also be replaced by two elements such as magnesium (Mg) and niobium (Nb), magnesium (Mg) and zirconium (Zr). In addition, the piezoelectric film F3 has a thickness of 1 μm, for example, but a thickness of about 0.2 μm to 2 μm can also be used.
[0071] The piezoelectric film F3 expands and contracts in the in-plane direction of the XY plane, i.e., in the Y-axis direction, according to the electric field applied to the piezoelectric film F3 by the metal layers E1 and E2. Due to the expansion and contraction of the piezoelectric film F3, the vibration arm 135 displaces its free end toward the inner surface of the lower cover 20 and the upper cover 30, and vibrates in an out-of-plane bending vibration mode.
[0072] In the present embodiment, the phase of the electric field applied to the outer vibration arms 135A and 135D is set to be opposite to the phase of the electric field applied to the inner vibration arms 135B and 135C. As a result, the outer vibration arms 135A and 135D and the inner vibration arms 135B and 135C are displaced in opposite directions. For example, if the free ends of the outer vibration arms 135A and 135D are displaced toward the inner surface of the upper cover 30, the free ends of the inner vibration arms 135B and 135C are displaced toward the inner surface of the lower cover 20.
[0073] The protective film 235 prevents oxidation of the upper electrode for piezoelectric vibration, that is, the metal layer E2. The protective film 235 is preferably formed of a material whose mass reduction rate caused by etching is slower than that of the frequency adjustment film 236. The mass reduction rate is represented by the etching rate, that is, the product of the thickness removed per unit time and the density. In addition to being formed of piezoelectric films such as aluminum nitride (AlN), scandium aluminum nitride (ScAlN), zinc oxide (ZnO), gallium nitride (GaN), and indium nitride (InN), the protective film 235 is also formed of insulating films such as silicon nitride (SiN), silicon dioxide (SiO2), and aluminum oxide (Al2O3). The thickness of the protective film 235 is, for example, about 0.2μm.
[0074] The frequency adjustment film 236 is formed on substantially the entire surface of the vibration part 120 and then formed only in a predetermined region by etching or the like. The frequency adjustment film 236 is formed of a material whose mass decreases faster than the protective film 235 due to etching. Specifically, the frequency adjustment film 236 is made of a metal such as molybdenum (Mo), tungsten (W), gold (Au), platinum (Pt), nickel (Ni), or titanium (Ti).
[0075] In addition, as long as the relationship between the mass reduction rates of the protective film 235 and the frequency adjustment film 236 is as described above, the magnitude relationship of the etching rates is arbitrary.
[0076] The parasitic capacitance reduction film 240 is formed of tetraethylorthosilicate (TEOS). The thickness of the parasitic capacitance reduction film 240 is about 1 μm. It reduces the parasitic capacitance in the routing wiring portion, and has the function of an insulating layer when wirings of different potentials cross each other, and a function as a support for expanding the vibration space.
[0077] The connection wiring 70 is electrically connected to the terminal T4 via the through electrode V3 , and is also electrically connected to the contact electrodes 76A and 76B.
[0078] The contact electrode 76A is formed to contact the metal layer E1 of the resonator 10, and electrically connects the connection wiring 70 to the resonator 10. The contact electrode 76B is formed to contact the metal layer E2 of the resonator 10, and electrically connects the connection wiring 70 to the resonator 10. Specifically, when the contact electrode 76A is connected to the metal layer E1, a part of the piezoelectric film F3, the protective film 235, and the parasitic capacitance reduction film 240 stacked on the metal layer E1 is removed to expose the metal layer E1, and the via hole V1 is formed. The inside of the formed via hole V1 is filled with the same material as the contact electrode 76A, and the metal layer E1 is connected to the contact electrode 76A. Similarly, when the contact electrode 76B is connected to the metal layer E2, a part of the piezoelectric film F3 and the parasitic capacitance reduction film 240 stacked on the metal layer E2 is removed to expose the metal layer E2, and the via hole V2 is formed. The contact electrode 76B is filled in the formed via hole V2, and the metal layer E2 is connected to the contact electrode 76B. The contact electrodes 76A and 76B are made of metals such as aluminum (Al), gold (Au), and tin (Sn). In addition, the connection portion between the metal layer E1 and the contact electrode 76A, and the connection portion between the metal layer E2 and the contact electrode 76B are preferably in the area outside the vibration part 120, and are connected at the holding part 140 in this embodiment.
[0079] The joint portion 60 is formed in a rectangular ring shape along the XY plane around the vibration portion 120 in the resonator 10, for example, on the holding portion 140, between the MEMS substrate 50 (the resonator 10 and the lower cover 20) and the upper cover 30. The joint portion 60 joins the MEMS substrate 50 and the upper cover 30 to seal the vibration space of the resonator 10. Thus, the vibration space is hermetically sealed and a vacuum state is maintained.
[0080] In this embodiment, the bonding portion 60 includes an aluminum (Al) layer 61 formed on the MEMS substrate 50 and a germanium (Ge) layer 62 formed on the upper cover 30 , and the MEMS substrate 50 and the upper cover 30 are bonded by eutectic bonding of the aluminum (Al) layer 61 and the germanium (Ge) layer 62 .
[0081] exist Figure 4 In the example shown, the aluminum (Al) layer 61 and the germanium (Ge) layer 62 are described as independent layers, but in fact, their interfaces are eutectic. In addition, the joint 60 can also be formed by a gold (Au) film and a tin (Sn) film, or a combination of gold (Au) and silicon (Si), gold (Au) and gold (Au), copper (Cu) and tin (Sn), etc. In addition, in order to improve the adhesion, the joint 60 can also be thinly sandwiched between the stacked layers with titanium (Ti), titanium nitride (TiN), tantalum nitride (TaN), etc.
[0082] In addition, in this embodiment, the example in which the joint portion 60 is provided around the entire vibrating portion 120 in the resonator 10 to seal the vibration space of the resonator 10 is described, but the present invention is not limited thereto. As long as the joint portion 60 joins the MEMS substrate 50 and the upper cover 30, for example, the joint portion 60 may be formed on a portion around the vibrating portion 120 in the resonator 10.
[0083] Next, refer to Figures 5 to 12 , a resonator manufacturing method according to a first embodiment of the present invention is described. Figure 5 1 is a flowchart showing a method for manufacturing the resonator 10 according to the first embodiment. Figure 6 It is used for Figure 5 A conceptual diagram for explaining an example of step S301 is shown. Figure 7 It is used for Figure 5 A conceptual diagram for explaining another example of step S301 is shown. Figure 8 It is used for Figure 5 A conceptual diagram for explaining step S302 is shown. Fig. 9 Is used for not Figure 5 A conceptual diagram for explaining the situation of step S303 is shown. Fig.10 It is used for Figure 5 A conceptual diagram for explaining step S303 is shown. Fig.11 It is used for Figure 5 A conceptual diagram for explaining step S304 is shown. Fig.12 It is used for Figure 5 A conceptual diagram for explaining step S305 is shown.
[0084] like Figure 5 As shown, initially, a silicon wafer 250 is prepared (S301). Specifically, as Figure 6 As shown, a silicon wafer 250 to which phosphorus (P) is added is prepared. The silicon wafer 250 is obtained by growing a single crystal of silicon (Si) and doping phosphorus (P) as an impurity to produce an ingot, and slicing the ingot into a predetermined thickness. The thickness of the silicon wafer 250 is, for example, about 500 μm.
[0085] In addition, in step S301, it is also possible to prepare Figure 6 The silicon wafer 250 shown in FIG. 1 is processed to produce an SOI wafer 260. Figure 7 As shown, the SOI wafer 260 includes a support layer 261 , an insulating layer 262 , and a silicon active layer 263 .
[0086] The support layer 261 supports the silicon active layer 263 and the insulating layer 262 in order to facilitate the handling of the silicon active layer 263. The support layer 261 is composed of single crystal silicon (Si), and its thickness is, for example, about 500 μm. The insulating layer 262 electrically insulates the silicon active layer 263. The insulating layer 262 is composed of silicon dioxide (SiO2), and its thickness is about 1 μm to 20 μm. The silicon active layer 263 is the above-mentioned silicon wafer 250, to which phosphorus (P) is added. The thickness of the silicon active layer 263 is, for example, about 10 μm to 50 μm. The silicon active layer 263 is supported by the support layer 261, so even if it is formed thinner than the silicon wafer 250, it is easy to handle.
[0087] Hereinafter, unless otherwise specified, an example in which the SOI wafer 260 including the silicon active layer 263 is prepared as the silicon wafer 250 will be described.
[0088] Back to Figure 5 Next, the SOI wafer 260 is heated in an oxygen atmosphere to form a silicon oxide film (SiO 2 film) 264 ( S302 ).
[0089] Specifically, if Figure 8 As shown, the surface of the silicon active layer 263 of the SOI wafer 260 is oxidized by thermal oxidation under an oxygen atmosphere, and is changed into a silicon oxide film (SiO2 film) 264 of silicon dioxide. In the thermal oxidation, the heating temperature is about 1100° C. and the heating time is about 3 hours. The thickness of the formed silicon oxide film (SiO2 film) 264 is about 1 μm to 2 μm.
[0090] Here, when a part of the silicon active layer 263 is changed into the silicon oxide film (SiO2 film) 264 by thermal oxidation, the silicon (Si) in the silicon active layer 263 is consumed as silicon dioxide (SiO2). In fact, in the formed silicon oxide film (SiO2 film) 264, 45 vol% is silicon (Si). On the other hand, phosphorus (P) has the property of not being easily dissolved in silicon dioxide (SiO2), so the phosphorus (P) added to the silicon active layer 263 is accumulated inside the silicon active layer 263. As a result, the concentration of phosphorus (P) in the silicon active layer 263 can be increased compared with before the formation of the silicon oxide film (SiO2 film) 264.
[0091] In addition, the silicon active layer 263 can be formed thinner than the silicon wafer 250 , and therefore the concentration of phosphorus (P) can be easily increased in the SOI wafer 260 compared to the silicon wafer 250 .
[0092] Back to Figure 5Next, the thermally oxidized SOI wafer 260 is further heated to diffuse phosphorus (P) (S303). More specifically, the SOI wafer 260 formed with the silicon oxide film (SiO2 film) 264 is subjected to a heat treatment in which the SOI wafer 260 is heated at a high temperature for a long time in a nitrogen gas (N2 gas) atmosphere to diffuse phosphorus (P) into the silicon active layer 263. This method is sometimes referred to as thermal diffusion or drive-in. In this heat treatment, the heating temperature is about 1100°C and the heating time is about 7 to 10 hours.
[0093] Here, without performing the heat treatment of step S303, Fig. 9 As shown, the distribution of phosphorus (P) in the silicon active layer 263 sometimes deviates, and phosphorus (P) segregates at the boundary, that is, the interface, or near the interface between the silicon active layer 263 and the silicon oxide film (SiO 2 film) 264 .
[0094] Thus, in step S303, the SOI wafer 260 is heated to diffuse phosphorus (P), thereby Fig.10 As shown, phosphorus (P) in the silicon active layer 263 can be distributed uniformly or substantially uniformly.
[0095] In addition, step S303 is not limited to the case where it is performed separately from step S302. For example, diffusion of phosphorus (P) may be performed as a part of step S302, or may be performed as a part of thermal oxidation in step S302.
[0096] Back to Figure 5 Next, the silicon oxide film (SiO2 film) 264 formed in step S302 is removed (S304).
[0097] Specifically, if Fig.11 As shown, the silicon oxide film (SiO2 film) 264 is removed from the SOI wafer 260 by wet etching. As a result, the thickness of the silicon active layer 263 can be reduced by the thickness of the silicon oxide film (SiO2 film) 264.
[0098] Back to Figure 5 Next, the steps S302 to S304 are repeated for the SOI wafer 260 to form the silicon substrate 270 (S305). Fig.12 As shown, the formed silicon substrate 270 includes a support layer 261, an insulating layer 262, and a silicon active layer 263, similarly to the SOI wafer 260. The silicon substrate 270 is different from the SOI wafer 260 in that the thickness of the silicon active layer 263 is reduced and thinned. As a result, the concentration of phosphorus (P) in the silicon active layer 263 is increased. The details of the silicon active layer 263 in the silicon substrate 270 will be described later.
[0099] In the silicon substrate 270 formed in step S305, the silicon active layer 263 corresponds to Figure 4 The Si substrate F2 shown in the figure, the insulating layer 262 is equivalent to Figure 4 The silicon oxide layer F21 shown, the support layer 261 is equivalent to Figure 4 The Si wafer L1 of the lower cover 20 is shown.
[0100] Furthermore, the steps S302 to S305 are repeated until the silicon substrate 270 reaches a desired phosphorus (P) concentration and resistivity. Specifically, the number of repetitions may be at least one or more, preferably two or more.
[0101] Next, the vibrating portion 120, the holding portion 140, and the supporting arm 110 are formed on the silicon substrate 270 formed in step S305 (S306). As described above, the vibrating portion 120, the holding portion 140, and the supporting arm 110 are integrally formed in the same step. Figure 4 The contact electrodes 76A, 76B and the aluminum (Al) layer 61 are shown. In this way, the resonator 10 is manufactured.
[0102] Next, refer to Figures 13 to 15 , the physical properties of the silicon substrate of the resonator according to the first embodiment of the present invention are described. Fig.13 Graph showing the concentrations of phosphorus (P) and carbon (C) in the silicon substrate 270 in the first embodiment. Fig.14 The silicon substrate 270 and Figure 6 A graph of the resistivity of silicon wafer 250 is shown. Fig.15 The silicon substrate 270 and Figure 6 The silicon wafer 250 is shown in the table for comparison. Fig.13 In FIG. 2 , the horizontal axis is the depth from the surface of the silicon substrate 270, and the vertical axis is the concentration in the silicon substrate 270. Fig.14 In FIG. 1 , the horizontal axis is the thickness of the silicon active layer 263 in the silicon substrate 270 and the thickness of the silicon wafer 250, and the vertical axis is the resistivity of the silicon substrate 270 and the silicon wafer 250. Figures 13 to 15 In the example, the thickness of the silicon active layer 263 in the silicon substrate 270 is 3.09 μm. Fig.14 as well as Fig.15 In FIG. 2 , the thickness of the silicon wafer 250 is 6.07 μm.
[0103] like Fig.13 As shown, within the thickness range of the silicon active layer 263 of the silicon substrate 270, the concentration of phosphorus (P) is 1.1×10 20 [atoms / cm 3] or more. Thus, the concentration of phosphorus (P) is 1.0×10 20 [atoms / cm 3 ] compared to the existing silicon substrate of about 100 nm, the concentration of phosphorus (P) can be increased and the resistivity of the vibration part 120 can be reduced.
[0104] More preferably, the concentration of phosphorus (P) in the silicon substrate 270 within the thickness range of the silicon active layer 263 is 2.0×10 20 [atoms / cm 3 ] and above and 4.0×10 20 [atoms / cm 3 ] or less. In addition, the upper limit of the concentration of phosphorus (P) in the silicon substrate 270 is the solid solubility limit of phosphorus (P) with respect to silicon (Si).
[0105] In addition, the carbon (C) concentration of the silicon substrate 270 within the thickness range of the silicon active layer 263 is 1.1×10 18 [atoms / cm 3 ]the following.
[0106] Here, phosphorus (P) generally has the property of easily bonding with contaminants such as carbon (C) present on the surface of the wafer. Carbon (C) deactivates phosphorus (P) when bonding with phosphorus (P), and thus becomes an important factor that hinders the reduction of resistivity.
[0107] In contrast, the carbon (C) concentration of the silicon substrate 270 is 1.1×10 18 [1 / cm 3 ] or less, thereby suppressing the deactivation of phosphorus (P). Therefore, the resistivity of the vibration part 120 can be lowered than before, and the frequency-temperature characteristic of the resonance frequency can be improved.
[0108] In other words, the concentration of phosphorus (P) in the silicon substrate 270 is 110 times or more the concentration of carbon (C). As a result, the concentration of phosphorus (P) can be increased compared to the conventional silicon substrate, the resistivity of the vibration part 120 can be reduced, and the deactivation of phosphorus (P) can be suppressed. Therefore, the resistivity of the vibration part 120 can be reduced compared to the past, and the frequency-temperature characteristics of the resonance frequency can be improved.
[0109] In addition, from Fig.13 It can be seen that phosphorus (P) is diffused in the silicon substrate 270 by heat treatment, so that the concentration of phosphorus (P) is uniform or substantially uniform within the thickness range of the silicon active layer 263. In this way, by heating the SOI wafer 260 to diffuse phosphorus (P), the segregation of phosphorus (P) on the surface or near the surface of the silicon active layer 263 in the silicon substrate 270 can be suppressed.
[0110] like Fig.14As shown, the resistivity of the silicon wafer 250 in the initial state before the steps S302 to S305 is 0.812 [mΩ·cm] on average. In contrast, the resistivity of the silicon substrate 270 formed by repeatedly performing the steps S302 to S305 is 0.541 [mΩ·cm] on average. Thus, the resistivity of the silicon substrate 270 is [0.60 mΩ·cm] or less, thereby making it possible to reduce the resistivity of the vibration part 120 compared to the past, and improve the frequency-temperature characteristics of the resonance frequency.
[0111] More preferably, the resistivity of the silicon substrate 270 is 0.40 [mΩ·cm] or more and 0.55 [mΩ·cm] or less.
[0112] In addition, if Fig.15 As shown in FIG. 1 , the standard deviation of the resistivity of the silicon wafer 250, which indicates the variation of the resistivity, is 0.008. In contrast, the standard deviation of the resistivity of the silicon substrate 270 is 0.005, which is approximately the same. Thus, it can be said that the variation of the resistivity does not change or hardly changes before and after the steps S302 to S305.
[0113] Furthermore, it can be said that the surface roughness of the silicon substrate 270 is 0.3 nm or less, specifically, about 0.25 nm, and surface roughness caused by steps S302 to S305 does not occur or is unlikely to occur.
[0114] <Second embodiment>
[0115] Next, refer to Figures 16 to 20 , a resonator and a resonator manufacturing method according to a second embodiment of the present invention are described. In addition, the same or similar structures as those in the first embodiment are marked with the same or similar reference numerals. The following describes the points that are different from the first embodiment. In addition, the same effects based on the same structure are not mentioned in sequence. Furthermore, the resonator in the second embodiment is substantially the same as the resonator 10 of the first embodiment, so the illustration and description thereof are omitted.
[0116] First, refer to Fig.16 , a resonator manufacturing method according to a second embodiment of the present invention is described. Fig.16 1 is a flowchart showing a method for manufacturing a resonator according to the second embodiment. Fig.17 It is used for Fig.16 The step S352 is shown as a cross-sectional view for explanation. Fig.18 It is used for Fig.16 The cross-sectional view shown is for explaining step S353. Fig.19 It is used for Fig.16 A cross-sectional view illustrating an example of step S356 is shown. Fig. 20 It is used for Fig.16 A cross-sectional view illustrating another example of step S356 is shown.
[0117] Fig.16 The step 351 shown is the same as the step 301 of the first embodiment, and therefore the description thereof is omitted. In addition, in the following, an example of preparing the SOI wafer 260 is described similarly to the first embodiment.
[0118] Next, the SOI wafer 260 is processed to form the recess 265 (S352). Fig.17 As shown, a portion of the surface of the silicon active layer 263 is removed by etching to form one or more recesses 265. As a result, the portion of the surface of the silicon active layer 263 that is not removed, that is, the portion between the recesses 265, is a convex portion 266.
[0119] In addition, step S352 is not limited to the case where it is performed between step S351 and step S352. For example, the recess 265 may be performed as a part of step S351, or may be performed as a pre-treatment of thermal oxidation in step S353.
[0120] Back to Fig.16 Next, the SOI wafer 260 is heated in an oxygen atmosphere to form a silicon oxide film (SiO2 film) 264 (S352).
[0121] More specifically, similarly to the first embodiment, the surface of the silicon active layer 263 of the SOI wafer 260 is oxidized by thermal oxidation under heating in an oxygen atmosphere, and is converted into a silicon oxide film (SiO 2 film) 264 .
[0122] Here, if Fig.18 As shown, the recessed portion 265 and part of the protruding portion 266 formed in step 352 are also transformed into a silicon oxide film (SiO2 film) 264 by thermal oxidation. By including the recessed portion 265 on the surface of the silicon active layer 263, the surface area of the silicon active layer 263 is increased, so that the volume of the silicon oxide film (SiO2 film) 264 formed by thermal oxidation can be increased.
[0123] Fig.16 The steps 354 and 355 shown are respectively the same as the steps 303 and 304 of the first embodiment, and thus description thereof will be omitted.
[0124] Back to Fig.16 Next, the SOI wafer 260 is repeatedly subjected to steps S353 to S355 to form a silicon substrate 280 (S305). Fig.19As shown, the formed silicon substrate 280 includes a support layer 261, an insulating layer 262, and a silicon active layer 263 in the same manner as the silicon substrate 270 of the first embodiment. The silicon substrate 280 is different from the silicon substrate 270 in that the silicon active layer 263 is formed with a concave portion 265 and a convex portion 266. In this way, the silicon substrate 280 includes the concave portion 265 formed in the silicon active layer 263, so that the surface area of the silicon active layer 263 becomes larger, thereby increasing the volume of the silicon oxide film (SiO2 film) 264 formed by thermal oxidation. Therefore, the silicon (Si) of the silicon active layer 263 can be more efficiently consumed as silicon dioxide (SiO2), and the resistivity of the silicon substrate 280 can be more easily reduced.
[0125] In step S356, the silicon substrate 280 having the narrowed convex portion 266 may be formed by repeating steps S353 to S355. Fig. 20 As shown, the protrusion 266 in the silicon active layer 263 is Fig.19 The width of the narrowed convex portion 266 is narrower than that of the convex portion 266 shown in FIG. 2. The narrowed convex portion 266 can be formed by adjusting the heating time of the heat treatment when diffusing phosphorus (P) in step S354. In addition, by adjusting the heating time, the diffusion of phosphorus (P) changes, so the narrowed convex portion 266 has a different resistivity than other parts of the silicon active layer 263. Specifically, the resistivity of the convex portion 266 is smaller than that of the other parts. As a result, the silicon substrate 280 can have multiple regions with different resistivities, and a resonator with multiple frequency-temperature characteristics can be realized.
[0126] Fig.16 The step 357 shown is the same as the step 306 of the first embodiment, and therefore the description thereof is omitted.
[0127] The above is a description of an exemplary embodiment of the present invention. A resonator according to an embodiment of the present invention includes a vibrating portion configured to vibrate in a predetermined vibration mode as a main vibration, and formed on a silicon substrate containing phosphorus (P), wherein the concentration of phosphorus (P) in the silicon substrate is 1.1×10 20 [1 / cm 3 ] or more. Thus, the concentration of phosphorus (P) is 1.0×10 20 [1 / cm 3 ] compared to the existing silicon substrate, the phosphorus (P) concentration can be increased, and the resistivity of the vibration part can be reduced. In addition, the carbon (C) concentration of the silicon substrate is 1.1×10 18 [1 / cm 3 ] or less. Thus, the deactivation of phosphorus (P) can be suppressed. Therefore, the resistivity of the vibration part can be lowered compared with the past, and the frequency-temperature characteristics of the resonance frequency can be improved.
[0128] In addition, a resonator according to an embodiment of the present invention includes a vibration portion, which is configured to vibrate in a predetermined vibration mode as a main vibration, and is formed on a silicon substrate containing phosphorus (P), and the concentration of phosphorus (P) in the silicon substrate is 110 times or more of the concentration of carbon (C) in the silicon substrate. As a result, compared with the existing silicon substrate, the concentration of phosphorus (P) can be increased, the resistivity of the vibration portion 120 can be reduced, and the deactivation of phosphorus (P) can be suppressed. Therefore, the resistivity of the vibration portion can be reduced compared with the past, and the frequency-temperature characteristics of the resonant frequency can be improved.
[0129] In addition, a resonator according to an embodiment of the present invention includes a vibration portion, the vibration portion is configured to vibrate in a predetermined vibration mode as a main vibration, and is formed on a silicon substrate containing phosphorus (P), wherein the resistivity of the silicon substrate is 0.60 [mΩ·cm] or less. Thus, the resistivity of the vibration portion can be reduced compared to the past, and the frequency-temperature characteristics of the resonant frequency can be improved.
[0130] In the resonator described above, a silicon substrate is formed using an SOI wafer including a support layer, an insulating layer, and a silicon active layer to which phosphorus (P) is added. Here, the silicon active layer can be formed thin, so the SOI wafer can easily increase the concentration of phosphorus (P).
[0131] In addition, in the above-mentioned resonator, the silicon substrate includes a recessed portion formed in the silicon active layer. As a result, the surface area of the silicon active layer becomes larger, so that the volume of the silicon oxide film (SiO2 film) formed by thermal oxidation can be increased. Therefore, the silicon (Si) of the silicon active layer can be more efficiently consumed as silicon dioxide (SiO2), and the resistivity of the silicon substrate can be more easily reduced.
[0132] A resonance device according to one embodiment of the present invention includes a cover and the above-mentioned resonator.
[0133] This makes it possible to easily realize a resonance device in which the resistivity of the vibration portion is further reduced.
[0134] According to one embodiment of the present invention, a resonator manufacturing method includes: a process of preparing a silicon wafer to which phosphorus (P) is added; a process of heating the silicon wafer in an oxygen atmosphere to form a silicon oxide film (SiO2 film); a process of removing the silicon oxide film (SiO2 film) from the silicon wafer; a process of performing the process of forming the silicon oxide film and the process of removing the silicon oxide film more than once to form a silicon substrate; and a process of forming a vibration part configured to vibrate in a predetermined vibration mode as a main vibration on the silicon substrate. As a result, compared with the existing manufacturing method, the concentration of phosphorus (P) can be increased, the resistivity of the vibration part can be reduced, and phosphorus (P) can be added in advance, which is not easy to combine with contaminants such as carbon (C), thereby suppressing the deactivation of phosphorus (P). Therefore, the resistivity of the vibration part can be reduced compared with the past, and the frequency-temperature characteristics of the resonant frequency can be improved.
[0135] In addition, in the resonator manufacturing method described above, between the step of forming the silicon oxide film (SiO2 film) and the step of removing the silicon oxide film (SiO2 film), a step of heating the silicon wafer to diffuse phosphorus (P) is included. Thus, the segregation of phosphorus (P) on the surface or near the surface of the silicon substrate can be suppressed.
[0136] In addition, each embodiment described above is used to make the understanding of the present invention easy, and is not used to limit the interpretation of the present invention. The present invention can be changed / improved without departing from its purpose, and its equivalent is also included in the present invention. That is, as long as the content obtained by appropriately applying design changes to each embodiment by those skilled in the art has the characteristics of the present invention, it is included in the scope of the present invention. For example, each element and its configuration, material, condition, shape, size, etc. possessed by the embodiment are not limited to the illustrated content, and can be appropriately changed. In addition, the embodiment is an illustration, and of course, the partial replacement or combination of the structure shown in different embodiments can be performed, as long as they include the characteristics of the present invention, it is included in the scope of the present invention.
[0137] Explanation of reference numerals: 1…resonance device; 10…resonator; 20…lower cover; 21…recess; 22…bottom plate; 23…side wall; 30…upper cover; 31…recess; 32…bottom plate; 33…side wall; 34…getter layer; 50…MEMS substrate; 60…joining portion; 61…aluminum layer; 62…germanium layer; 70…connection wiring; 76A…contact electrode; 76B…contact electrode; 110…support arm; 120…vibration portion; 130…base; 135, 135A, 135B, 135C, 135D…vibration arm; 140…holding portion; 235…protective film; 236… Frequency adjustment film; 240…parasitic capacitance reduction film; 250…silicon wafer; 260…SOI wafer; 261…support layer; 262…insulating layer; 263…silicon active layer; 264 silicon oxide film; 265…concave portion; 266…convex portion; 270…silicon substrate; 280…silicon substrate; E1…metal layer; E2…metal layer; F2…Si substrate; F3…piezoelectric film; F21…silicon oxide layer; G…hammer; L1…Si wafer; L3…Si substrate; L31…silicon oxide film; P…virtual plane; T4…terminal; V1…conductive hole; V2…conductive hole; V3…through electrode
Claims
1. A resonator, wherein: A vibrating portion is provided, the vibrating portion being configured to vibrate in a predetermined vibration mode as a main vibration and being formed on a silicon substrate containing phosphorus, The phosphorus concentration of the silicon substrate is 1.1×10 20 [1 / cm 3 ] above, the carbon concentration of the silicon substrate is 1.1×10 18 [1 / cm 3 ]the following.
2. A resonator, wherein: A vibrating portion is provided, the vibrating portion being configured to vibrate in a predetermined vibration mode as a main vibration and formed on a silicon substrate containing phosphorus, wherein: The concentration of the phosphorus in the silicon substrate is 110 times or more the concentration of carbon in the silicon substrate.
3. A resonator, wherein: A vibrating portion is provided, the vibrating portion being configured to vibrate in a predetermined vibration mode as a main vibration and formed on a silicon substrate containing phosphorus, wherein: The resistivity of the silicon substrate is 0.60 [mΩ·cm] or less.
4. The resonator according to any one of claims 1 to 3, wherein: The silicon substrate is formed using an SOI wafer including a support layer, an insulating layer, and a silicon active layer to which the phosphorus is added.
5. The resonator according to claim 4, wherein The silicon substrate includes a recessed portion formed in the silicon active layer.
6. A resonant device, wherein: have: a cover; and The resonator according to any one of claims 1 to 5.
7. A method for manufacturing a resonator, wherein: include: A process for preparing a silicon wafer to which phosphorus is added; The step of heating the silicon wafer in an oxygen atmosphere to form a silicon oxide film; a step of removing the silicon oxide film from the silicon wafer; a step of forming a silicon substrate by performing the step of forming the silicon oxide film and the step of removing the silicon oxide film one or more times; and The step of forming a vibration portion configured to vibrate in a predetermined vibration mode as a main vibration on the silicon substrate.
8. The resonator manufacturing method according to claim 7, wherein: The method further includes heating the silicon wafer to diffuse the phosphorus between the step of forming the silicon oxide film and the step of removing the silicon oxide film.