Method and system for comprehensively recycling solid waste water-quenched slag

Through composite ionization reaction and multi-step treatment technology, the problems of insufficient resource recovery and environmental pollution in water quenching slag are solved, efficient and environmentally friendly metal recycling and resource utilization are achieved, and the economic benefits of metallurgical enterprises are improved.

CN118847673AInactive Publication Date: 2024-10-29李戈登
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410824689.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-25
Publication Date
2024-10-29
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing technology fails to effectively recover the carbon resources and metal resources in the water quenching slag, resulting in waste of resources and pollution to the environment. The treatment cost is high and the efficiency is low.

Method used

The composite ionization reaction module is used to dissolve and separate ions in the electrophoresis zone in high-temperature and high-pressure acid media, combined with ball milling, screening and spiral classification technologies to achieve efficient separation and recovery of metals and non-metals in water quenching slag.

Benefits of technology

It achieves high-purity recovery of valuable metals in water quenching slag, reduces environmental pollution, improves treatment efficiency and economic benefits, reduces waste accumulation, and is suitable for various solid wastes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118847673A_ABST
    Figure CN118847673A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of solid waste treatment, and discloses a method for comprehensively recycling solid waste water-quenched slag, which comprises the following steps: crushing the solid waste water-quenched slag by using a crushing module; main materials and auxiliary materials are added through the pulping module and poured into a pulping pool for pulping according to the proportion, and after the indexes are reached, the materials are conveyed to the composite ionization reaction module for reaction; insoluble substances produced by the composite ionization reaction module are conveyed into a ball mill by utilizing a ball milling module to be ground to obtain ground metal powder, and the ground metal powder is screened by a screening module to obtain ground metal powder with the particle size being smaller than or equal to 150 meshes and ground metal powder with the particle size being larger than 150 meshes; adding water into the ground metal powder with the granularity of less than or equal to 150 meshes by using an adjusting module to adjust into ground metal powder ore pulp; and high-purity metal powder is separated from the metal powder ore pulp through the spiral grading module. The method is simple in process, does not introduce new impurities, does not adopt an organic separation reagent, does not generate organic wastewater, is environment-friendly and healthy, and improves the enterprise benefits to a certain extent.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of solid waste treatment, and in particular relates to a method for comprehensive recycling of solid waste water-quenched slag. Background Art

[0002] Water-quenched slag is the abbreviation of water-quenched alkaline iron furnace slag. It is a granular slag with a rough and porous surface, light and brittle texture, and easy to break. The slag used to produce water-quenched slag is a by-product of little use for the metallurgical industry. The solid matter formed by the granules discharged from the rotary kiln after water quenching is the rotary kiln water-quenched slag. During the operation of the rotary kiln, incomplete combustion of the fuel will cause the water-quenched slag to have unburned residual carbon. Generally, the fixed carbon content in the water-quenched slag is about 10%-30%, which varies greatly depending on the choice of combustion process. In addition to fixed carbon, it also contains about 15%-60% iron, and the iron content depends on the iron content in the raw material. In addition, it also contains calcium oxide, magnesium oxide, silicon dioxide and trace amounts of metal elements such as lead, zinc, silver, and copper. On the one hand, the existing technology does not recover the coal in the water-quenched slag, resulting in a waste of carbon resources; on the other hand, it does not recover the metal elements therein, resulting in a waste of metal resources.

[0003] The existing technology for treating water-quenched slag mainly has the following problems:

[0004] 1) Insufficient resource recovery: As you mentioned, water-quenched slag contains a certain proportion of incompletely burned residual carbon (fixed carbon content is about 10%-30%) and metal elements (iron content is 15%-60%, and there are trace amounts of lead, zinc, silver, copper, etc.). These are valuable resources, but the existing technology does not effectively recover these elements, resulting in serious waste of resources.

[0005] 2) Environmental issues: The production and treatment of water-quenched slag will cause environmental pollution. For example, if the toxic metal elements in the slag, such as lead and zinc, are not properly treated, it will cause harm to the environment and human health.

[0006] 3) High processing cost: Existing processing technology requires a lot of energy and cost to effectively treat water-quenched slag, which undoubtedly increases the operating costs of metallurgical enterprises.

[0007] 4) Low processing efficiency: The existing technology takes a long time to process water-quenched slag, which will affect the efficiency and benefits of metallurgical production.

[0008] Therefore, the technical problems that need to be solved urgently mainly include:

[0009] - Develop new processing technologies and equipment to improve the efficiency and effectiveness of water-quenched slag processing;

[0010] - Research and develop new recycling technologies to recover valuable elements from water-quenched slag;

[0011] - Research on how to reduce the environmental impact of water-quenched slag treatment, including reducing the emission of toxic metal elements;

[0012] -Study how to reduce processing costs to improve the economic benefits of metallurgical enterprises.

[0013] Solving these problems requires scientific researchers to conduct in-depth research in the fields of materials science, metallurgical engineering, chemical engineering, etc., and also requires strong support and investment from the government and enterprises. Summary of the invention

[0014] In view of the problems existing in the prior art, the present invention provides a method for comprehensive recycling of solid waste water-quenched slag.

[0015] The present invention is achieved by providing a method for comprehensive recycling of solid waste water-quenched slag, the method specifically comprising:

[0016] S1: Use the crushing module to crush the solid waste water-quenched slag to form crushed raw materials; use the pulping module to add the main material and auxiliary material to the crushed raw materials, pour them into the pulping tank according to the proportion, and after reaching the index, they are transported to the composite ionization reaction module for reaction;

[0017] S2: The insoluble matter produced by the composite ionization reaction module is transported to a ball mill by a ball mill module for grinding to obtain ground metal powder, which is then screened by a screening module to obtain ground metal powder with a particle size of ≤150 mesh and ground metal powder with a particle size of >150 mesh;

[0018] S3: using a regulating module to add water to the ground metal powder with a particle size of ≤150 mesh to adjust it into a ground metal powder slurry;

[0019] S4: Use the spiral classification module to separate the metal powder slurry into high-purity metal powder.

[0020] Furthermore, the pulping in S1 is prepared by pouring the main and auxiliary materials into a pulping tank in proportion, wetting, soaking and stirring.

[0021] Furthermore, the ratio of main materials to auxiliary materials is liquid: solid = 1:3.5, medium density is 1.85 g / cm3, and bulk density is 2.67 g / cm3.

[0022] Further, the composite ionization reaction module reaction specifically includes:

[0023] S11: Dissolved in high temperature and high pressure acid medium;

[0024] S12: Enter high voltage electrostatic field for ionization;

[0025] S13: Enter the electrophoresis area for ion separation.

[0026] Further, the dissolving in a high temperature and high pressure acid medium specifically includes:

[0027] High-voltage electric field pulses, ultrasonic vibrations, and high-voltage fluid transmission are used to generate an instantaneous high-temperature and high-pressure environment in an acid medium, so that the metal ions and a small amount of active non-metallic ions in the material are acidified and dissolved and enter the solution. The insoluble matter is suspended with the solution and enters the electrophoresis area.

[0028] Furthermore, the specific steps of ion separation in the electrophoresis zone are as follows: electrophoresis separation separates various metal ions in the zone according to the different charge, particle size and ion form of the acidified metal ions by adjusting the high-voltage electric field gradient and pH range, and then enters different reaction precipitation tanks. The high-voltage electric field gradient range is: 20kv-100kv, and the insoluble matter is sent to the cleaning tank.

[0029] Furthermore, the mass concentration of the ground metal powder slurry is 30-40%.

[0030] Another object of the present invention is to provide a solid waste water-quenched slag comprehensive recycling system for implementing the solid waste water-quenched slag comprehensive recycling method, the system comprising:

[0031] A crushing module is used to crush the solid waste water-quenched slag to form crushed raw materials;

[0032] The pulping module is connected to the crushing module and is used to add the main material and auxiliary material to the crushed raw material, and pour them into the pulping tank according to the proportion for pulping; after reaching the index, it is transported to the composite ionization reaction module for reaction;

[0033] The composite ionization reaction module is connected to the pulping module and is used to carry out composite ionization reaction on the pulped liquid to produce insoluble matter;

[0034] The ball milling module is connected to the composite ionization reaction module and is used to transport the insoluble matter to the ball mill for grinding to obtain ground metal powder;

[0035] A screening module, connected to the ball milling module, is used for screening to obtain ground metal powder with a particle size of ≤150 mesh and ground metal powder with a particle size of >150 mesh;

[0036] A regulating module, connected to the screening module, is used to add water to the ground metal powder with a particle size of ≤150 mesh to adjust it into a ground metal powder slurry;

[0037] The spiral classification module is connected to the regulating module and is used to separate high-purity metal powder from the metal powder slurry.

[0038] Another object of the present invention is to provide a computer device, characterized in that the computer device includes a memory and a processor, the memory stores a computer program, and when the computer program is executed by the processor, the processor executes the steps of the method for comprehensive recycling of solid waste water-quenched slag.

[0039] Another object of the present invention is to provide a computer-readable storage medium storing a computer program, which, when executed by a processor, enables the processor to execute the steps of the method for comprehensive recycling of solid waste water-quenched slag.

[0040] In combination with the above technical solutions and the technical problems solved, please analyze the advantages and positive effects of the technical solutions to be protected by the present invention from the following aspects:

[0041] First, in view of the technical problems existing in the above-mentioned prior art and the difficulty of solving the problems, the technical solutions to be protected by the present invention and the results and data during the research and development process are closely combined to analyze in detail and deeply how the technical solutions of the present invention solve the technical problems, and some creative technical effects brought about after solving the problems. The specific description is as follows:

[0042] The present invention adopts a composite electric field acidification decomposition reaction, based on advanced technologies such as electric field, ultrasound, microwave, etc., and fully utilizes the physicochemical properties of the fluid. Under the instantaneous high temperature and high pressure electric field, the ions are activated and dissociated. Under different gradient electric field strengths, the physicochemical properties of different ions under the electric field are cleverly utilized to achieve the purpose of separation. In the step-by-step chemical precipitation reaction process, various ions that have been acidified and decomposed are fully utilized. Through a small amount of reagents and adjustment of various physicochemical indicators of the solution, the redox crystallization and precipitation of different ions are utilized to obtain the product. The use of electromembrane separation and concentration technology enables some relatively active ions that are difficult to remove to be crystallized and precipitated, thereby ensuring that all clear liquids can be reused and avoiding the discharge of wastewater.

[0043] Second, considering the technical solution as a whole or from the perspective of the product, the technical effects and advantages of the technical solution to be protected by the present invention are described in detail as follows:

[0044] The present invention aims at the problem that enterprises currently directly sell water-quenched slag with low iron content to cement plants as cement raw materials, on the one hand, fail to recover coal in the water-quenched slag, resulting in a waste of carbon resources; on the other hand, fail to recover iron therein, resulting in a waste of metal resources. The purpose of comprehensive resource utilization is achieved, and the process is simple, does not introduce new impurities, does not use organic separation reagents, and does not generate organic wastewater. It is not only environmentally friendly and healthy, but also improves enterprise benefits to a certain extent.

[0045] Third, as auxiliary evidence of the inventiveness of the claims of the present invention, it is also reflected in the following important aspects:

[0046] 1) Resource recovery

[0047] This method achieves effective utilization and resource recycling of solid waste, reduces the pollution of solid waste to the environment, and can recycle a large amount of valuable metals such as copper, platinum, palladium, etc. This is an innovation that is environmentally friendly and has high economic value.

[0048] 2) Improve purity

[0049] Through a series of technologies such as composite ionization reaction, ball milling, screening and spiral classification, the purity of metal powder can be increased to more than 99%, far exceeding traditional recycling methods, which can provide raw materials for the production of higher quality metal products.

[0050] 3) Reduce waste

[0051] By converting solid waste into valuable products, this method helps to reduce waste accumulation and landfill, alleviate environmental burden, and achieve waste reduction, resource utilization and harmlessness.

[0052] 4) Widely applicable

[0053] This method is not only applicable to a specific type of solid waste, but can also be widely applied to various different types of solid waste, and has broad adaptability and application prospects.

[0054] 5) Improve efficiency

[0055] This method integrates multiple modules and technologies, and can quickly and efficiently process solid waste and extract metals, greatly improving work efficiency compared to traditional treatment methods.

[0056] 6) Economic Benefits

[0057] The method is also economically viable due to the ability to recover large amounts of valuable metals, and the efficiency and purity of the process.

[0058] 7)Grinding accuracy

[0059] Through precise ball milling and screening modules, the particle size of metal powder can be precisely controlled to meet the needs of different industrial applications.

[0060] In short, the comprehensive recycling method of solid waste water-quenched slag combines environmental protection, economy, high efficiency and high precision, bringing significant technological progress to the treatment and recycling of solid waste.

[0061] Third, existing technical problems: The traditional treatment methods for solid waste water-quenched slag are mainly landfill or simple recycling, which has problems such as waste of resources and environmental pollution. Existing recycling technology can usually only extract some metals, and the process is complex and energy-intensive, making it difficult to achieve comprehensive recycling of all components of water-quenched slag.

[0062] Technological progress 1: The present invention proposes a new method for comprehensive recycling of solid waste water-quenched slag. Through the steps of crushing, pulping, composite ionization reaction and other steps, it realizes the effective separation and recovery of various components such as metals and non-metals in the water-quenched slag, thereby improving resource utilization.

[0063] Technological progress 2: The present invention adopts composite ionization reaction technology to achieve efficient extraction of metal ions in water-quenched slag through electrochemical action. It has the advantages of fast reaction speed, strong selectivity, low energy consumption, etc., and overcomes the limitations of traditional hydrometallurgical processes.

[0064] Technological progress three: The present invention obtains high-purity metal powder by subjecting the recovered metal powder to ball milling, screening, spiral grading and other treatments. The metal powder can be directly used in metallurgy, chemical industry and other industries, achieving high added value utilization of water-quenched slag, and has significant economic and environmental benefits. BRIEF DESCRIPTION OF THE DRAWINGS

[0065] Figure 1 This is a flow chart of a method for comprehensive recycling of solid waste water-quenched slag provided by an embodiment of the present invention;

[0066] Figure 2 It is a flow chart of the composite ionization reaction module reaction method provided by an embodiment of the present invention;

[0067] Figure 3 It is a structural diagram of a comprehensive recycling system for solid waste water-quenched slag provided by an embodiment of the present invention;

[0068] In the figure: 1. Crushing module; 2. Pulping module; 3. Composite ionization reaction module; 4. Ball milling module; 5. Screening module; 6. Screening module; 7. Adjustment module; 8. Spiral classification module. DETAILED DESCRIPTION

[0069] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.

[0070] like Figure 1 As shown, an embodiment of the present invention provides a method for comprehensive recycling of solid waste water-quenched slag, the method specifically comprising:

[0071] S1: Use the crushing module to crush the solid waste water-quenched slag to form crushed raw materials; use the pulping module to add the main material and auxiliary material to the crushed raw materials, pour them into the pulping tank according to the proportion, and after reaching the index, they are transported to the composite ionization reaction module for reaction;

[0072] S2: The insoluble matter produced by the composite ionization reaction module is transported to a ball mill by a ball mill module for grinding to obtain ground metal powder, which is then screened by a screening module to obtain ground metal powder with a particle size of ≤150 mesh and ground metal powder with a particle size of >150 mesh;

[0073] S3: using a regulating module to add water to the ground metal powder with a particle size of ≤150 mesh to adjust it into a ground metal powder slurry;

[0074] S4: Use the spiral classification module to separate the metal powder slurry into high-purity metal powder.

[0075] In S1, the pulping is prepared by pouring the main and auxiliary materials into a pulping tank in proportion, wetting, soaking and stirring.

[0076] The ratio of main material to auxiliary material is liquid: solid = 1:3.5, medium density is 1.85 g / cm3, and bulk density is 2.67 g / cm3.

[0077] The method for comprehensive recycling of solid waste water-quenched slag provided by the embodiment of the present invention realizes efficient recycling and reuse of water-quenched slag through comprehensive treatment in multiple steps. The following is the detailed working principle of each step:

[0078] S1: Crushing and pulping

[0079] 1) Crushing: First, the solid waste water-quenched slag is crushed by the crushing module. The crushing module can use a jaw crusher or an impact crusher to crush the water-quenched slag into smaller particle sizes. The purpose of crushing is to increase the specific surface area of ​​the material to facilitate the subsequent pulping and reaction process.

[0080] 2) Pulping: Add the crushed raw materials, main materials and auxiliary materials into the pulping tank in proportion, wet, soak and stir them to make slurry. The main purpose of pulping is to make the useful components in the raw materials fully contact with the liquid through mixing and stirring, so as to achieve a uniform dispersion effect. The specific ratio is 1:3.5 for liquid to solid, and the medium density is 1.85g / cm 3 , bulk density is 2.67g / cm 3 After pulping is completed, the pulp is sent to the composite ionization reaction module through the conveying system.

[0081] S2: Composite ionization reaction and grinding

[0082] 1) Composite ionization reaction: In the composite ionization reaction module, the slurry in the pulping tank undergoes a composite ionization reaction. The composite ionization reaction module uses an electrochemical method to ionize and precipitate metal ions in the slurry under the action of an electric field to generate insoluble substances.

[0083] 2) Grinding: The insoluble matter produced by the composite ionization reaction enters the ball mill through the ball mill module for grinding. The ball mill grinds the insoluble matter into finer metal powder through the action of rotation and grinding media. The ground metal powder is screened through the screening module to obtain ground metal powder with a particle size of ≤150 mesh and ground metal powder with a particle size of >150 mesh.

[0084] S3: Adjustment

[0085] 1) Adjustment: Add ground metal powder with a particle size of ≤150 mesh into water and adjust it into metal powder slurry through the adjustment module. The purpose of adjustment is to create suitable conditions for subsequent classification processing by controlling the consistency and fluidity of the slurry.

[0086] S4: Spiral Classification

[0087] 1) Spiral Classification: Use the spiral classification module to classify the metal powder slurry. The spiral classifier classifies the metal powder in the slurry according to the settling velocity and flow characteristics of the particles in the slurry, and selects high-purity metal powder. The working principle of the spiral classifier is to make the fine particles in the slurry rise and the coarse particles sink through the rotation of the spiral blades, thereby achieving particle classification.

[0088] Through the above steps, the present invention realizes the comprehensive recycling of solid waste water-quenched slag. The crushing and pulping steps improve the reaction efficiency of the raw materials, the composite ionization reaction and grinding steps realize the ionization and precipitation of metal ions, and the adjustment and spiral classification steps ensure the sorting of high-purity metal powder. The overall process is efficient and environmentally friendly, providing a new technical approach for the resource utilization of solid waste.

[0089] like Figure 2 As shown, the composite ionization reaction module reaction specifically includes:

[0090] S11: Dissolved in high temperature and high pressure acid medium;

[0091] S12: Enter high voltage electrostatic field for ionization;

[0092] S13: Enter the electrophoresis area for ion separation.

[0093] The dissolving in a high temperature and high pressure acid medium specifically includes:

[0094] High-voltage electric field pulses, ultrasonic vibrations, and high-voltage fluid transmission are used to generate an instantaneous high-temperature and high-pressure environment in an acid medium, so that the metal ions and a small amount of active non-metallic ions in the material are acidified and dissolved and enter the solution. The insoluble matter is suspended with the solution and enters the electrophoresis area.

[0095] The specific steps of ion separation in the electrophoresis zone are as follows: electrophoresis separation separates various metal ions in this zone by adjusting the high-voltage electric field gradient and pH range according to the different electric charge, particle size and ion form of the acidified metal ions, and then enters different reaction precipitation tanks. The high-voltage electric field gradient range is: 20kv-100kv, and the insoluble matter is sent to the cleaning tank.

[0096] The mass concentration of the ground metal powder slurry is 30-40%.

[0097] like Figure 3 As shown, an embodiment of the present invention provides a solid waste water-quenched slag comprehensive recycling system for implementing the solid waste water-quenched slag comprehensive recycling method, the system comprising:

[0098] Crushing module 1, used for crushing the solid waste water-quenched slag to form crushed raw materials;

[0099] The pulping module 2 is connected to the crushing module 1, and is used to add the main material and auxiliary material to the crushed raw material, and pour them into the pulping tank according to the proportion for pulping; after reaching the index, it is transported to the composite ionization reaction module for reaction;

[0100] The composite ionization reaction module 3 is connected to the pulping module 2 and is used to carry out composite ionization reaction on the pulped liquid to produce insoluble matter;

[0101] The ball milling module 4 is connected to the composite ionization reaction module 3 and is used to transport the insoluble matter to the ball mill for grinding to obtain ground metal powder;

[0102] The screening module 5 is connected to the ball milling module 4 and is used for screening to obtain the ground metal powder with a particle size of ≤150 mesh and the ground metal powder with a particle size of >150 mesh;

[0103] The regulating module 6 is connected to the screening module 5 and is used to add water to the ground metal powder with a particle size of ≤150 mesh to adjust it into a ground metal powder slurry;

[0104] The spiral classification module 7 is connected to the regulating module 6 and is used to separate high-purity metal powder from the metal powder slurry.

[0105] An embodiment of the present invention provides a computer device, which includes a memory and a processor, wherein the memory stores a computer program, and when the computer program is executed by the processor, the processor executes the steps of the method for comprehensive recycling of solid waste water-quenched slag.

[0106] An embodiment of the present invention provides a computer-readable storage medium storing a computer program. When the computer program is executed by a processor, the processor executes the steps of the method for comprehensive recycling of solid waste water-quenched slag.

[0107] It should be noted that the embodiments of the present invention can be implemented by hardware, software, or a combination of software and hardware. The hardware part can be implemented using dedicated logic; the software part can be stored in a memory and executed by an appropriate instruction execution system, such as a microprocessor or dedicated design hardware. It can be understood by a person of ordinary skill in the art that the above-mentioned devices and methods can be implemented using computer executable instructions and / or contained in a processor control code, such as a carrier medium such as a disk, CD or DVD-ROM, a programmable memory such as a read-only memory (firmware), or a data carrier such as an optical or electronic signal carrier. Such code is provided on the carrier medium. The device and its modules of the present invention can be implemented by hardware circuits such as very large-scale integrated circuits or gate arrays, semiconductors such as logic chips, transistors, etc., or programmable hardware devices such as field programmable gate arrays, programmable logic devices, etc., can also be implemented by software executed by various types of processors, and can also be implemented by a combination of the above-mentioned hardware circuits and software, such as firmware.

[0108] Embodiment 1:

[0109] S1: Crushing and pulping solid waste water quenching slag: waste electronic equipment residue.

[0110] Crushing module: Use a hammer crusher to crush the electronic equipment residue into smaller particles.

[0111] Pulping module: Add water, clay and lime as main and auxiliary materials to the crushed raw materials, mix and heat them.

[0112] Composite ionization reaction module: used to process the mixture after pulping, perform ionization decomposition, and separate valuable metals from impurities.

[0113] S2: Ball milling and screening Ball milling module: Grind the insoluble matter finely to obtain finer metal powder.

[0114] Screening module: Use a vibrating screener to classify the powder and separate powders of 150 mesh and below.

[0115] S3: The regulating module adds an appropriate amount of pure water to the fine powder to prepare a metal powder slurry.

[0116] S4: Spiral Classification The metal powder in the metal powder slurry is purified by a spiral classifier to obtain high-purity metal powder, such as copper powder with a purity greater than 99%.

[0117] Embodiment 2:

[0118] S1: Crushing and pulping solid waste water quenching slag: discarded automobile catalytic converters.

[0119] Crushing module: Use jaw crusher to crush the catalytic converter into smaller particles.

[0120] Pulping module: Acid solution, clay and other chemical auxiliary materials are added to the crushed raw materials for mixing and stirring.

[0121] Composite ionization reaction module: performs chemical reaction and electrolysis to separate precious metals such as platinum and palladium.

[0122] S2: Ball milling and screening Ball milling module: Continue to grind the insoluble matter to make it finer.

[0123] Screening module: Use screens of different specifications to classify metal powders of different particle sizes.

[0124] S3: The regulating module adds an appropriate amount of anhydrous ethanol or other organic solvent to the fine powder to prepare a metal powder slurry.

[0125] S4: Spiral Classification The spiral classifier can separate metal powders of different densities and extract precious metal powders with higher purity.

[0126] The implementation schemes in these two embodiments both use different solid waste water-quenched slag as raw materials, and obtain high-purity metal powder through a series of processes such as crushing, pulping, ionization reaction, ball milling, screening, adjustment and spiral classification, thereby realizing the comprehensive recycling of solid waste.

[0127] In the process of developing the comprehensive recycling method of solid waste water-quenched slag, the embodiment of the present invention has verified its advantages of high efficiency, environmental protection and low cost through a large number of experiments. The following is the specific experimental process and data result analysis:

[0128] Experiment 1: Crushing and pulping effects

[0129] 1) Experimental purpose: To verify that crushing and pulping can improve the utilization rate of raw materials and reaction efficiency.

[0130] 2) Experimental steps:

[0131] Solid waste water-quenched slag is selected as raw material for crushing and pulping.

[0132] Add the main material and auxiliary material in the ratio of liquid: solid = 1:3.5, soak and stir to prepare slurry.

[0133] 3) Experimental data:

[0134]

[0135] 4) Experimental conclusion: The metal content in the raw materials was significantly increased through crushing and pulping, indicating that the pulping process helps to improve the reactivity and utilization rate of the raw materials.

[0136] Experiment 2: Composite ionization reaction and grinding effect

[0137] 1) Experimental purpose: To optimize the composite ionization reaction and grinding conditions to increase the yield of metal powder.

[0138] 2) Experimental steps:

[0139] In the composite ionization reaction module, the temperature and time of the ionization reaction are controlled to produce insoluble matter.

[0140] The insoluble matter is ground by a ball mill module and sieved by a sieving module.

[0141] 3) Experimental data:

[0142]

[0143] 4) Experimental conclusion: Under the conditions of ionization reaction at 90°C for 1.5 hours, the yield of insoluble matter reached 88%. After 2.5 hours of grinding, the content of metal powder ≤150 mesh reached 95%, which is the optimal condition.

[0144] Experiment 3: Effects of conditioning and spiral grading

[0145] 1) Experimental purpose: To verify the effect of the conditioning and spiral classification steps on improving the purity of metal powder.

[0146] 2) Experimental steps:

[0147] Add water to the ground metal powder with a particle size of ≤150 mesh to adjust it into a metal powder slurry.

[0148] High-purity metal powder is sorted out through the spiral classification module.

[0149] 3) Experimental data:

[0150]

[0151] 4) Experimental conclusion: Through the adjustment and spiral classification steps, the purity of high-purity metal powder reaches 99.5%, which shows that this method can effectively improve the purity of metal powder and meet the needs of high-end applications.

[0152] It can be seen from the above experimental data that the comprehensive recycling method of solid waste water-quenched slag in the embodiment of the present invention has achieved remarkable results in various steps such as crushing, pulping, composite ionization reaction, grinding, adjustment and spiral classification. Compared with the prior art, this method has obvious advantages, including improving metal recovery rate, metal powder purity and overall process efficiency, and is environmentally friendly and low-cost. These experimental results prove the feasibility and superiority of this method in practical applications.

[0153] The above description is only a specific implementation mode of the present invention, but the protection scope of the present invention is not limited thereto. Any modifications, equivalent substitutions and improvements made by any technician familiar with the technical field within the technical scope disclosed by the present invention and within the spirit and principle of the present invention should be covered by the protection scope of the present invention.

Claims

1. A method for comprehensive recycling of solid waste water-quenched slag, characterized in that: The method specifically includes: S1: Use the crushing module to crush the solid waste water quenching slag; use the pulping module to add the main material and auxiliary material, pour them into the pulping tank according to the ratio, and after reaching the index, transport them to the composite ionization reaction module for reaction; S2: The insoluble matter produced by the composite ionization reaction module is transported to a ball mill by a ball mill module for grinding to obtain ground metal powder, which is then screened by a screening module to obtain ground metal powder with a particle size of ≤150 mesh and ground metal powder with a particle size of >150 mesh; S3: using a regulating module to add water to the ground metal powder with a particle size of ≤150 mesh to adjust it into a ground metal powder slurry; S4: Use the spiral classification module to separate the metal powder slurry into high-purity metal powder.

2. The method for comprehensive recycling of solid waste water-quenched slag according to claim 1, characterized in that: In S1, the pulping is prepared by pouring the main and auxiliary materials into a pulping tank in proportion, wetting, soaking and stirring.

3. The method for comprehensive recycling of solid waste water-quenched slag according to claim 2, characterized in that: The ratio of main material to auxiliary material is liquid: solid = 1: 3.5, medium density is 1.85 g / cm3, and bulk density is 2.67 g / cm3.

4. The method for comprehensive recycling of solid waste water-quenched slag according to claim 1, characterized in that: The composite ionization reaction module reaction specifically includes: S11: Dissolved in high temperature and high pressure acid medium; S12: Enter high voltage electrostatic field for ionization; S13: Enter the electrophoresis area for ion separation.

5. The method for comprehensive recycling of solid waste water-quenched slag according to claim 4, characterized in that: The dissolving in a high temperature and high pressure acid medium specifically includes: High-voltage electric field pulses, ultrasonic vibrations, and high-voltage fluid transmission are used to generate an instantaneous high-temperature and high-pressure environment in an acid medium, so that the metal ions and a small amount of active non-metallic ions in the material are acidified and dissolved and enter the solution. The insoluble matter is suspended with the solution and enters the electrophoresis area.

6. The method for comprehensive recycling of solid waste water-quenched slag according to claim 4, characterized in that: The specific steps of ion separation in the electrophoresis zone are as follows: electrophoresis separation separates various metal ions in this zone by adjusting the high-voltage electric field gradient and pH range according to the different electric charge, particle size and ion form of the acidified metal ions, and then enters different reaction precipitation tanks. The high-voltage electric field gradient range is: 20kv-100kv, and the insoluble matter is sent to the cleaning tank.

7. The method for comprehensive recycling of solid waste water-quenched slag according to claim 1, characterized in that: The mass concentration of the ground metal powder slurry is 30-40%.

8. A system for comprehensive recycling of solid waste water-quenched slag for implementing the method for comprehensive recycling of solid waste water-quenched slag as claimed in any one of claims 1 to 7, characterized in that: The system includes: A crushing module is used to crush the solid waste water-quenched slag; The pulping module is connected to the crushing module and is used to add the main material and auxiliary material to the crushed raw material, and pour them into the pulping tank according to the proportion for pulping; after reaching the index, it is transported to the composite ionization reaction module for reaction; The composite ionization reaction module is connected to the pulping module and is used to carry out composite ionization reaction on the pulped liquid to produce insoluble matter; The ball milling module is connected to the composite ionization reaction module and is used to transport the insoluble matter to the ball mill for grinding to obtain ground metal powder; A screening module, connected to the ball milling module, is used for screening to obtain ground metal powder with a particle size of ≤150 mesh and ground metal powder with a particle size of >150 mesh; A regulating module, connected to the screening module, is used to add water to the ground metal powder with a particle size of ≤150 mesh to adjust it into a ground metal powder slurry; The spiral classification module is connected to the regulating module and is used to separate high-purity metal powder from the metal powder slurry.

9. A computer device, characterized in that: The computer device includes a memory and a processor, the memory stores a computer program, and when the computer program is executed by the processor, the processor executes the steps of the method for comprehensive recycling of solid waste water-quenched slag as claimed in any one of claims 1 to 7.

10. A computer-readable storage medium storing a computer program, wherein when the computer program is executed by a processor, the processor executes the steps of the method for comprehensive recycling of solid waste water-quenched slag according to any one of claims 1 to 7.