Calcium exchange carbon-molecular sieve composite material and preparation method thereof

By performing absorption calcination and hydrothermal reaction on coal gangue, combined with calcium chloride ion exchange modification, calcium exchange carbon-molecular sieve composite material is prepared, which solves the problems of low adsorption amount and poor stability of the existing CO2 capture method. , achieving low-cost and environmentally friendly CO2 adsorption effect, and effectively utilizes coal gangue resources.

CN118892810APending Publication Date: 2024-11-05CHINA UNIV OF MINING & TECH (BEIJING)
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202411123701.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-15
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

The existing CO2 capture methods have problems such as low adsorption, poor stability, high cost and difficulty in recycling. At the same time, coal gangue cannot be effectively utilized as solid waste, resulting in environmental pollution and waste of resources.

Method used

Carbon-molecular sieve was prepared by calcining the coal gangue powder at an oxygen and mixing it with alkali and melting it with alkali, followed by hydrothermal reaction, and ion exchange modification in calcium chloride solution to prepare the calcium exchange carbon-molecular sieve composite material. Improve its CO2 adsorption capacity and stability.

Benefits of technology

It has achieved low-cost, environmentally friendly CO2 adsorption materials, with good thermal stability and cyclic renewable properties, significantly reducing carbon capture costs, and solving the problems of coal gangue accumulation and pollution.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118892810A_ABST
    Figure CN118892810A_ABST
Patent Text Reader

Abstract

The invention discloses a calcium exchange carbon-molecular sieve composite material and a preparation method thereof. The calcium exchange carbon-molecular sieve composite material is applicable to the fields of high-value utilization of coal-based solid wastes, preparation of solid adsorbents and CO2 trapping. The preparation method comprises the following steps: placing coal gangue in a tubular furnace for anoxic calcination, then uniformly mixing with sodium hydroxide, and calcining and activating in an anoxic atmosphere; and further adding water, stirring and aging, transferring to a hydrothermal reaction kettle, carrying out hydrothermal reaction, washing with deionized water, drying, grinding, and carrying out ion exchange in a calcium chloride solution to finally obtain the calcium exchange carbon-molecular sieve composite material. The invention has the following beneficial effects: (1) the coal gangue is used as a raw material, the cost is low, and high-valued utilization of the coal gangue can be realized; (2) the adsorption material is simple in preparation process and free of secondary pollution; and (3) the material has good thermal stability and cyclic reusability, and the carbon capture cost can be remarkably reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a calcium exchange carbon-molecular sieve composite material and a preparation method thereof, which is applicable to the fields of high-value utilization of coal-based solid waste, preparation of solid adsorbent and CO2 capture. Background Art

[0002] With the development of industry and technological progress, energy demand has increased dramatically, resulting in a continuous increase in CO2 emissions. The increase in carbon emissions has led to global warming, causing a series of problems such as glacier melting and seawater acidification, which has had a serious impact on the ecological environment and economic development. In order to cope with a series of hazards brought about by global warming, countries around the world have pledged in the Paris Agreement to control the global temperature rise within 1.5°C this century. The International Energy Agency estimates that to achieve this goal, global carbon dioxide emissions must be zero by 2050. Therefore, it is urgent to take effective measures to control CO2 emissions. At present, the main methods for capturing CO2 are: absorption, adsorption, cryogenic distillation and membrane separation, but overall there are shortcomings such as low adsorption capacity, poor stability, high cost and difficulty in recycling.

[0003] Gangue is a solid waste discharged during coal mining and washing. It is a black-gray rock with a low carbon content and harder than coal that accompanies coal seams during the coal formation process. Gangue is currently one of the largest solid wastes discharged in China, accounting for more than one-tenth of coal production. The long-term storage of large quantities of gangue that cannot be effectively utilized not only occupies land and arable land, but also easily spontaneously combusts and releases toxic and harmful gases during storage. After long-term weathering and rainwater leaching, the harmful substances in the gangue will pollute groundwater and soil, and at the same time cause geological disasters such as landslides and mud-rock flows, seriously affecting the ecological environment and human production and life. Therefore, the management of large quantities of solid waste from gangue is of great significance.

[0004] Zeolite molecular sieve is a nano-aluminosilicate microporous material with a three-dimensional structure. It has the advantages of uniform pore structure, large specific surface area, strong adsorption capacity, high cation exchange capacity (CEC), and good hydrothermal stability. In recent years, it has been widely used in adsorption, catalysis, drying, ion exchange and other fields. The mineral components of coal gangue are mainly quartz and clay minerals, such as kaolinite, feldspar, montmorillonite, illite, quartz sand, mica and chlorite. The chemical composition is mainly SiO2 and Al2O3. In addition, it contains a small amount of residual carbon. It is an ideal raw material for synthesizing zeolite molecular sieves. The preparation of molecular sieves can not only alleviate the problem of coal gangue accumulation occupying land and polluting the environment, but also further realize the high added value of coal gangue and reduce the cost of molecular sieve preparation. The preparation methods of gangue molecular sieve include alkali melting hydrothermal method, hydrothermal synthesis method, seed introduction method, ultrasound-assisted method and microwave-assisted method. The most commonly used one is alkali melting hydrothermal method, which mixes gangue or calcined activated gangue with alkali, and synthesizes zeolite molecular sieve through high-temperature melting calcination and hydrothermal reaction. However, the thermal activation pretreatment and alkali melting treatment currently used are mostly high-temperature calcination in air atmosphere, which cannot effectively utilize the residual carbon components in the gangue, thus resulting in waste of carbon components.

[0005] In recent years, zeolite molecular sieves have been widely used in CO2 adsorption due to their pore structure and stability. However, their adsorption capacity is limited. In order to further increase the adsorption capacity of the molecular sieve, it is necessary to further modify the molecular sieve to increase its specific surface area and pore volume, and then improve its CO2 adsorption capacity. In summary, the residual carbon components in coal gangue can be utilized through the two processes of carbonization and activation. At the same time, with the help of inorganic modification, the pore structure and chemical stability of the material can be further adjusted, which is expected to significantly improve the comprehensive performance of the material. Summary of the invention

[0006] The technical scheme of the present invention is as follows: firstly, coal gangue powder is calcined in anoxic conditions, then the calcined material is mixed with an appropriate amount of alkali, and further alkali melting and calcining is carried out in anoxic conditions, the melt is ground, an appropriate amount of water is added, stirred and aged, and then transferred to a hydrothermal reactor for hydrothermal reaction, after the reaction is completed, the product is filtered and washed to neutrality, and dried to obtain a carbon-molecular sieve material. The carbon-molecular sieve is further placed in a calcium chloride solution for ion exchange modification, and a calcium exchange carbon-molecular sieve composite material is obtained after washing and drying.

[0007] The specific preparation process of the prepared calcium exchange carbon-molecular sieve composite material is as follows:

[0008] (1) Weigh a certain amount of coal gangue powder and place it in a tube furnace for calcination. The calcination time is 30 to 150 minutes and the calcination temperature is 500 to 900°C;

[0009] (2) according to the set alkali-ash ratio, weigh the corresponding mass of sodium hydroxide and the coal gangue obtained in step (1), mix and grind them, place them in a tube furnace and roast them at a temperature of 500 to 800° C. for 30 to 150 min;

[0010] (3) weighing a corresponding mass of the calcined product in step (2) according to the set alkali concentration, adding 60 mL of water, and stirring at room temperature for 0 to 120 min;

[0011] (4) transferring the aged product in step (3) into a reactor, placing the reactor in an oven for hydrothermal reaction, the hydrothermal temperature being 60 to 110° C., the hydrothermal time being 3 to 15 h, and washing, drying, and grinding after the reaction to obtain a carbon-molecular sieve composite material;

[0012] (5) placing the carbon-molecular sieve composite adsorbent material in step (3) in a 0.1-0.5 mol / L CaCl2 solution, stirring for 30-150 min, filtering, washing to neutrality, drying, and grinding to obtain a calcium-exchanged carbon-molecular sieve composite material.

[0013] The present invention also provides an application of the calcium exchange carbon-molecular sieve composite adsorption material to adsorb CO2, the method is as follows:

[0014] The CO2 adsorption capacity of the sample was tested using a specific surface area and pore size analyzer. A certain amount of molecular sieve was weighed and placed in a sample tube. The sample was degassed at a degassing temperature of 250°C and a degassing time of 2h. After degassing, the CO2 adsorption capacity of the calcium exchange carbon-molecular sieve composite adsorbent material was tested at 25°C under 100kPa.

[0015] The beneficial effects of the present invention are as follows:

[0016] (1) Using coal gangue as raw material is low-cost and can solve the environmental problems caused by large-scale storage of coal gangue;

[0017] (2) The preparation process of the adsorbent material is simple, the raw materials are pollution-free, and it is an environmentally friendly green adsorbent;

[0018] (3) The adsorbent material has good thermal stability and recyclability, which can significantly reduce the cost of carbon capture. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 It is a schematic diagram of the preparation of the calcium exchange carbon-molecular sieve composite material of the present invention.

[0020] Figure 2 The XRD spectra of coal gangue and the calcium exchange carbon-molecular sieve composite material of the present invention are shown.

[0021] Figure 3It is the FT-IR spectra of coal gangue and the calcium exchange carbon-molecular sieve composite material of the present invention.

[0022] Table 1 shows the CO2 adsorption capacity of Examples 1 to 3 and Comparative Examples 1 to 3 of the calcium exchange carbon-molecular sieve composite adsorption material. DETAILED DESCRIPTION

[0023] Embodiment 1:

[0024] (1) Weigh 20 g of coal gangue powder and calcine it in a tube furnace at a temperature of 800°C for 1 h;

[0025] (2) setting the alkali-ash ratio to 1.6, weighing 16 g of sodium hydroxide and 10 g of the coal gangue obtained in step (1), mixing and grinding, placing in a tubular furnace for calcination at a temperature of 700° C. for 1 h;

[0026] (3) Weigh 10 g of the calcined product in step (2), add 60 mL of water, and stir at room temperature for 90 min;

[0027] (4) transferring the aged product in step (3) into a reactor, placing the reactor in an oven for hydrothermal reaction at a temperature of 80° C. for a time of 9 h, and washing, drying, and grinding after the reaction to obtain a carbon-molecular sieve composite material;

[0028] (5) placing the carbon-molecular sieve composite adsorbent material in step (3) in a 0.2 mol / L CaCl2 solution, stirring for 1 h, filtering, washing, drying, and grinding to obtain a calcium-exchanged carbon-molecular sieve composite material.

[0029] Embodiment 2:

[0030] The steps are the same as those in Example 1, except that in step (4), the hydrothermal temperature is 60° C. and the hydrothermal time is 12 h.

[0031] Embodiment 3:

[0032] The steps are the same as those in Example 1, except that in step (2), the alkali-ash ratio is 2.0 and the calcination temperature is 800°C.

[0033] Comparative Example 1:

[0034] The steps are the same as those in Example 1, except that calcium chloride is not added in step (5).

[0035] Comparative Example 2:

[0036] The steps are the same as those in Example 1, except that the aging time in step (3) is 0 min and the hydrothermal temperature in step (4) is 100°C.

[0037] Comparative Example 3:

[0038] The steps are the same as those in Example 1, except that the calcination atmosphere used in step (2) is air.

[0039] The CO2 adsorption capacity of Examples 1 to 3 and Comparative Examples 1 to 3 was tested in the following manner, and the results are listed in Table 1.

[0040] CO2 adsorption test: The CO2 adsorption of the sample was tested using a specific surface area and pore size analyzer. A certain amount of molecular sieve was weighed and placed in a sample tube. The sample was degassed at a degassing temperature of 250°C and a degassing time of 2h. After degassing, the CO2 adsorption of the calcium exchange carbon-molecular sieve composite adsorbent material was tested at 25°C under 100kPa.

[0041] Table 1 CO2 adsorption at 100 kPa for Examples 1 to 3 and Comparative Examples 1 to 3

[0042]

Claims

1. A calcium exchange carbon-molecular sieve composite material and a preparation method thereof, characterized in that: The following steps are involved: (1) calcining coal gangue powder in a tube furnace; (2) adding sodium hydroxide to the carbonized coal gangue obtained in step (1), mixing and grinding, and calcining in a tubular furnace; (3) Weigh the calcined product in step (2), add 60 mL of water, and stir at room temperature for aging; (4) transferring the aged product in step (3) into a reactor, placing the reactor in an oven for hydrothermal reaction, and washing, drying, and grinding after the reaction to obtain a carbon-molecular sieve composite material; (5) placing the carbon-molecular sieve composite material in step (3) in a CaCl2 solution, stirring thoroughly, filtering, washing to neutrality, drying, and grinding to obtain a calcium-exchanged carbon-molecular sieve composite material.

2. A calcium exchange carbon-molecular sieve composite material and a preparation method thereof according to claim 1, characterized in that: In the step (1), the calcination time is 30 to 150 minutes, and the calcination temperature is 500 to 900°C.

3. A calcium exchange carbon-molecular sieve composite material and a preparation method thereof according to claim 1, characterized in that: The calcination atmosphere in steps (1) and (2) is one of argon, nitrogen and helium.

4. A calcium exchange carbon-molecular sieve composite material and a preparation method thereof according to claim 1, characterized in that: The mass ratio of sodium hydroxide to coal gangue in step (2) is 0.8-2.4, the calcination temperature is 500-900° C., and the calcination time is 30-150 min.

5. A calcium exchange carbon-molecular sieve composite material and a preparation method thereof according to claim 1, characterized in that: The alkali concentration in step (3) is 2.0 to 5.0 mol / L, and the aging time is 0 to 120 min.

6. A calcium exchange carbon-molecular sieve composite material and a preparation method thereof according to claim 1, characterized in that: The hydrothermal time of step (4) is 3 to 15 hours, and the hydrothermal temperature is 60 to 110°C.

7. A calcium exchange carbon-molecular sieve composite material and a preparation method thereof as claimed in claim 1, characterized in that: The calcium chloride concentration in step (5) is 0.1-0.5 mol / L, and the stirring time is 30-150 min.

8. A calcium exchange carbon-molecular sieve composite material, characterized in that: The calcium exchange carbon-molecular sieve composite material is prepared by the preparation method of any one of claims 1 to 7.

Citation Information

Patent Citations

  • Preparation method and application of novel sub-mesoporous zeolite molecular sieve adsorbent

    CN112403433A

  • Coal gangue in-situ carbon activation material as well as preparation method and application thereof

    CN112915990A

  • Carbon-based molecular sieve and 13X zeolite prepared from coal gangue as well as preparation method and application of carbon-based molecular sieve and 13X zeolite

    CN116924428A

  • Coal gangue-based chabazite and preparation method thereof

    CN118343790A

  • Spherical molecular sieve preparation method based on multi-element solid waste sheet layer stacking, corresponding material and application

    CN118439627A