Preparation method of water-based iron oxide red primer
By setting strain gauge on the stirring impeller to collect stress data and compare the characteristic models, the precise control problem of water-based iron red primer mixing process is solved, product quality and production efficiency are improved, and paint stability and application performance are ensured. .
Patent Information
- Application Number
- CN202410929912.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-11
- Publication Date
- 2024-11-05
AI Technical Summary
During the preparation of water-based iron red primer, it is difficult to accurately control the stirring process, which affects the uniform dispersion of raw materials and the rate of chemical reaction, resulting in poor stability and application performance of the final paint.
By setting a strain gauge on the stirring impeller, collecting force data and comparing it with the characteristic model, the completion status of the stirring and dispersion process is judged, and the precise control of the stirring process is ensured.
Accurate control of the preparation process of water-based iron red primer is achieved, product quality and production efficiency are improved, and local overheating or reaction prolongation problems caused by uneven stirring are avoided.
Smart Images

Figure CN118895073A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of primer preparation, and in particular to a method for preparing a water-based iron red primer. Background Art
[0002] In the coatings industry, iron red primer is a widely used anti-rust coating, and its performance is directly related to the corrosion resistance and service life of the coated object. Traditional iron red primers mostly use solvent-based systems, but with the improvement of environmental protection requirements and the deepening of the concept of sustainable development, water-based iron red primers have gradually become the mainstream of the industry due to their low VOC (volatile organic compound) emissions and superior environmental performance. The preparation of water-based iron red primers involves the precise proportions of multiple raw materials and complex chemical reactions. Among them, accurate control of the stirring process is the key link to ensure product quality and production efficiency.
[0003] In the preparation process of water-based iron red primer, the main technical challenge is how to achieve precise control of the stirring process. Stirring not only affects the uniform dispersion of raw materials, the rate and completeness of chemical reactions, but is also directly related to the stability and application performance of the final paint. Specifically, the technical issues include: 1. Uniform mixing of materials: Ensure that various solid particles (such as red iron oxide, fillers, etc.), liquid raw materials (such as water-based resins, solvents, additives) and possible powdered zinc powder are evenly dispersed to avoid agglomeration and sedimentation. 2. Reaction control: In steps involving chemical reactions, such as the cross-linking reaction of epoxy resin and curing agent, the stirring rate needs to be moderate. Too fast may cause local overheating or uneven reaction, and too slow may prolong the reaction time, affecting efficiency and product performance.
[0004] In the prior art, the control is usually achieved by limiting the stirring time and stirring speed, but such a method is obviously a rough estimate and cannot be actually controlled according to the actual stirring conditions. In view of this, a preparation method of a water-based iron red primer is proposed. Summary of the invention
[0005] The purpose of the present invention is to provide a method for preparing a water-based iron red primer, which can achieve accurate control of the preparation process of the iron red primer.
[0006] The above technical objectives of the present invention are achieved through the following technical solutions:
[0007] A method for preparing a water-based iron red primer comprises the following steps:
[0008] S1, take 35-40 parts by weight of water-based acrylic emulsion, 5-10 parts by weight of water-based alkyd resin, 0.5-1 parts by weight of dispersant, 20-30 parts by weight of deionized water, 10-15 parts by weight of iron oxide red powder, 5-10 parts by weight of zinc phosphate, 15-25 parts by weight of barium sulfate, 0.5-1 parts by weight of DMEA and 2-4 parts by weight of water-based additive;
[0009] S2, adding water-based alkyd resin, DMEA and deionized water into a dispersion tank, stirring and dispersing;
[0010] S3, add iron red powder, zinc phosphate and barium sulfate, and stir and disperse in a dispersion tank;
[0011] S4, put it into the grinding cylinder and grind it to a fineness less than 30um;
[0012] S5, adding water-based acrylic emulsion and water-based film-forming aid, stirring and dispersing in a dispersion tank;
[0013] S6, add water-based thickener, and stir and disperse in a dispersion tank;
[0014] Among them, during the stirring and dispersing process of S2, S3, S5, and S6, the force data of the stirring impeller are collected, and the change characteristics of the force data per unit time are compared with the characteristic model. When the comparison is consistent with the characteristic model, it is judged that the stirring and dispersing process is completed.
[0015] In a preferred embodiment, in S1, 37 parts by weight of aqueous acrylic emulsion, 7 parts by weight of aqueous alkyd resin, 0.6 parts by weight of dispersant, 25 parts by weight of deionized water, 13 parts by weight of iron ore red, 7 parts by weight of zinc phosphate, 20 parts by weight of barium sulfate, 0.6 parts by weight of DMEA and 3 parts by weight of aqueous additive are taken.
[0016] In a preferred embodiment, the feature model is obtained through model training.
[0017] In a preferred embodiment, the stirring impeller is provided with a strain gauge for collecting force data.
[0018] In a preferred embodiment, the stirring impeller is provided with stirring blades, and the strain gauges are provided on multiple stirring blades. The multiple strain gauges collect force data during the stirring and dispersing process. When the force data per unit time collected by more than 90% of the strain gauges are consistent with the characteristic model comparison results, the stirring and dispersing process is judged to be completed.
[0019] In a preferred embodiment, the stirring blades are arranged in two rows, the force data collected by the strain gauges arranged on the upper and lower rows of the stirring blades correspond to different characteristic models respectively, and when the respective models are matched, it is judged that the stirring and dispersing process is completed.
[0020] In a preferred embodiment, an electrode is arranged on the stirring blade, and before adding the iron ore red powder, zinc phosphate and barium sulfate, the iron ore red powder, zinc phosphate and barium sulfate are charged with opposite charges to those of the electrode.
[0021] In a preferred embodiment, during the stirring and dispersing process, when the force exceeds a preset threshold, the stirring is stopped.
[0022] Compared with the prior art, the present invention provides a method for preparing a water-based iron red primer. In the process of stirring and dispersing in each step, force data of the force on the stirring impeller is collected, and by comparing the force data with the characteristic model, it is judged whether the stirring and dispersing process is completed. The characteristic model is a model trained by big data, and its model state is a characteristic state that reaches a qualified state in the corresponding step, that is, when the collected data is compared with the characteristic model, the result is consistent, indicating that the stirring and dispersing state has reached a qualified state, so that it can be judged that the stirring and dispersing process is completed. Compared with the method of limiting the stirring time and rotation speed in the prior art, this method directly evaluates the fluid state in the dispersion tank, and the result is more intuitive and accurate, so that the primer preparation process can be more controllable and the quality is better. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 The invention relates to a schematic flow chart of a method for preparing a water-based iron red primer.
[0024] Figure 2 The invention relates to a statistical schematic diagram of force data of a single strain gauge in a method for preparing a water-based iron red primer.
[0025] Figure 3 The invention relates to a schematic structural diagram of a stirring impeller used in a method for preparing a water-based iron red primer.
[0026] Figure 4 yes Figure 3 Schematic diagram of the enlarged structure of part A.
[0027] In the figure
[0028] Stirring impeller 1; stirring blade 2; strain gauge 3; electrode 4. DETAILED DESCRIPTION
[0029] The present invention is further described in detail below in conjunction with the accompanying drawings.
[0030] This specific embodiment is merely an explanation of the present invention and is not a limitation of the present invention. After reading this specification, those skilled in the art may make non-creative modifications to the present embodiment as needed. However, as long as they are within the scope of the claims of the present invention, they are protected by the patent law.
[0031] like Figures 1 to 4 As shown, a method for preparing a water-based iron red primer comprises the steps of:
[0032] S1, take 35-40 parts by weight of water-based acrylic emulsion, 5-10 parts by weight of water-based alkyd resin, 0.5-1 parts by weight of dispersant, 20-30 parts by weight of deionized water, 10-15 parts by weight of iron oxide red powder, 5-10 parts by weight of zinc phosphate, 15-25 parts by weight of barium sulfate, 0.5-1 parts by weight of DMEA and 2-4 parts by weight of water-based additive;
[0033] S2, adding water-based alkyd resin, DMEA and deionized water into a dispersion tank, stirring and dispersing;
[0034] S3, add iron red powder, zinc phosphate and barium sulfate, and stir and disperse in a dispersion tank;
[0035] S4, put it into the grinding cylinder and grind it to a fineness less than 30um;
[0036] S5, adding water-based acrylic emulsion and water-based film-forming aid, stirring and dispersing in a dispersion tank;
[0037] S6, add water-based thickener, and stir and disperse in a dispersion tank;
[0038] Among them, during the stirring and dispersing process of S2, S3, S5, and S6, the force data of the stirring impeller 1 is collected, and the change characteristics of the force data per unit time are compared with the characteristic model. When the comparison is consistent with the characteristic model, it is judged that the stirring and dispersing process is completed.
[0039] The present invention provides a method for preparing a water-based iron red primer. In the process of stirring and dispersing in each step, force data of the force of the stirring impeller 1 is collected, and by comparing the force data with a characteristic model, it is judged whether the stirring and dispersing process is completed. The characteristic model is a model trained by big data, and its model state is a characteristic state that reaches a qualified state in the corresponding step, that is, when the collected data is compared with the characteristic model, the result is consistent, indicating that the stirring and dispersing state has reached a qualified state, so that it can be judged that the stirring and dispersing process is completed. Compared with the method of limiting the stirring time and rotation speed in the prior art, this method directly evaluates the fluid state in the dispersion cylinder, and the result is more intuitive and accurate, so that the primer preparation process can be more controllable and the quality is better.
[0040] Figure 3 In the figure, the area bounded by the vertical dotted line is the data feature that conforms to the feature model.
[0041] Specifically, in S1, the ingredients are preferably 37 parts by weight of aqueous acrylic emulsion, 7 parts by weight of aqueous alkyd resin, 0.6 parts by weight of dispersant, 25 parts by weight of deionized water, 13 parts by weight of iron ore red, 7 parts by weight of zinc phosphate, 20 parts by weight of barium sulfate, 0.6 parts by weight of DMEA and 3 parts by weight of aqueous additive.
[0042] Furthermore, the characteristic model is obtained through model training, and the characteristic model is obtained through artificial intelligence model training with a large amount of data. After the training is completed, the fluid state in each step can be accurately evaluated, and the data based on it is a large amount of data collected during the primer preparation process. How to implement model training is a relatively mature technology in the existing technology and will not be elaborated here.
[0043] In order to realize the force data collection, the stirring impeller 1 is provided with a strain gauge 3 for collecting force data. During the stirring and dispersing process, the strain gauge 3 collects data on the feedback force during the stirring and dispersing process. Different states of the fluid will feed back different forces to the strain gauge 3, so that the different states of the fluid can be judged by monitoring the force of the strain gauge 3.
[0044] The strain gauge 3 can be directly set as the stirring blade 2 on the stirring impeller 1, or can be set on the stirring blade 2 of the stirring impeller 1. When the strain gauge 3 is directly set as the stirring blade 2, the structure of the stirring impeller 1 can be simplified, and the strain gauge 3 can be manufactured together when the stirring impeller 1 is manufactured. When the strain gauge 3 is set on the stirring blade 2, the structural strength and the stability of the setting of the strain gauge 3 can be effectively guaranteed, and the setting of the strain gauge 3 may also improve the structural strength of the stirring blade 2.
[0045] In this embodiment, the following method is adopted: the stirring impeller 1 is provided with a stirring blade 2, and the plurality of stirring blades 2 are provided with the strain gauges 3, and the plurality of strain gauges 3 collect force data during the stirring and dispersing process, and when the unit time force data collected by more than 90% of the strain gauges 3 are consistent with the characteristic model comparison result, it is judged that the stirring and dispersing process is completed. In the above description, the setting of 90% can be set manually, and the judgment of 90% is a better ratio, which can ensure high accuracy in result judgment and have a certain fault tolerance rate. If the ratio is limited too high, some strain gauges 3 may always fail to meet the requirements of the characteristic model ratio due to the error in their state, and thus cannot judge a qualified result. If the limit is too low, the judgment accuracy will be insufficient.
[0046] Furthermore, the stirring blades 2 are arranged in two rows, one above the other, and the force data collected by the strain gauges 3 arranged on the two rows of stirring blades 2 correspond to different characteristic models, respectively, and when the models are matched, the stirring and dispersing process is judged to be completed. In the above setting, the strain gauges 3 are arranged in two rows, one above the other, so that force detection at different depths can be achieved. By collecting force data at different depths and judging whether the fluid state at different depths is qualified, on the one hand, detection of different height levels inside the fluid can be achieved, so that the detection results have better comprehensiveness. At the same time, calibration can also be achieved through detection at different depths, that is, only when all depth conditions meet the qualified judgment results, the overall qualified judgment result is output, thereby ensuring the accuracy of the output result.
[0047] In order to further improve the accuracy, a multi-layer strain gauge 3 may be provided on the stirring impeller 1 in a gradient manner, thereby further effectively improving the judgment accuracy.
[0048] By collecting force data, in addition to being able to determine whether the fluid state is qualified, the process of material addition can also be judged. When different materials are added, the fluid produces different characteristics. These characteristic data are also trained with the artificial intelligence big data model to obtain the corresponding feature model. Therefore, in the entire primer preparation process, the type of added material can be identified through the collection of force data and the comparison of feature models, which makes it easier for staff to control the process.
[0049] Furthermore, through the analysis of the force data, it is determined that when powder is added, that is, when iron ore red powder, zinc phosphate and barium sulfate are added, a corresponding control strategy can be used to make the powder quickly absorbed by the fluid to prevent the powder from escaping.
[0050] The method of accelerating the absorption speed of the powder is, for example, intermittently increasing the stirring speed of the stirring impeller 1 so that additional gaps appear in the fluid, so that the powder can be quickly coated, or the following method can be adopted: an electrode 4 is set on the stirring blade 2, and before adding iron red powder, zinc phosphate and barium sulfate, the iron red powder, zinc phosphate and barium sulfate are made to have opposite charges with opposite electrical properties to the electrode 4.
[0051] Before the powder is added, the iron ore red powder, zinc phosphate and barium sulfate are brought into contact with a container with opposite charges and are charged with opposite charges. After the powder is added, the charges are detected and the battery charging is controlled. The iron ore red powder, zinc phosphate and barium sulfate are attracted by the electrode 4 so that the iron ore red powder, zinc phosphate and barium sulfate can be quickly incorporated into the fluid system to prevent the powder from scattering. This allows the powder to be added accurately and sufficiently while maintaining a clean environment to ensure the health of the staff.
[0052] In order to effectively monitor the intrusion of foreign matter, during the stirring and dispersing process, when the force exceeds a preset threshold, the stirring is stopped. When foreign matter invades, the force exceeds a preset threshold, and the stirring impeller 1 is controlled to stop stirring.
[0053] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that the process, method, article or terminal device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or terminal device. In the absence of further restrictions, the elements defined by the sentence "include..." or "comprise..." do not exclude the existence of other elements in the process, method, article or terminal device including the elements. In addition, in this article, "greater than", "less than", "exceed" and the like are understood to exclude the number itself; "above", "below", "within" and the like are understood to include the number itself.
[0054] The above description of the embodiments is to facilitate the understanding and use of the present invention by those skilled in the art. It is obvious that those skilled in the art can easily make various modifications to the embodiments and apply the general principles described herein to other embodiments without creative work. Therefore, the present invention is not limited to the above embodiments. Improvements and modifications made by those skilled in the art based on the disclosure of the present invention without departing from the scope of the present invention should be within the protection scope of the present invention.
Claims
1. A method for preparing a water-based iron red primer, characterized in that: Includes steps: S1, take 35-40 parts by weight of water-based acrylic emulsion, 5-10 parts by weight of water-based alkyd resin, 0.5-1 parts by weight of dispersant, 20-30 parts by weight of deionized water, 10-15 parts by weight of iron oxide red powder, 5-10 parts by weight of zinc phosphate, 15-25 parts by weight of barium sulfate, 0.5-1 parts by weight of DMEA and 2-4 parts by weight of water-based additive; S2, adding water-based alkyd resin, DMEA and deionized water into a dispersion tank, stirring and dispersing; S3, add iron red powder, zinc phosphate and barium sulfate, and stir and disperse in a dispersion tank; S4, put it into the grinding cylinder and grind it to a fineness less than 30um; S5, adding water-based acrylic emulsion and water-based film-forming aid, stirring and dispersing in a dispersion tank; S6, add water-based thickener, and stir and disperse in a dispersion tank; Among them, during the stirring and dispersing process of S2, S3, S5, and S6, the force data of the stirring impeller are collected, and the change characteristics of the force data per unit time are compared with the characteristic model. When the comparison is consistent with the characteristic model, it is judged that the stirring and dispersing process is completed.
2. The method for preparing a water-based iron red primer according to claim 1, characterized in that: In S1, 37 parts by weight of aqueous acrylic emulsion, 7 parts by weight of aqueous alkyd resin, 0.6 parts by weight of dispersant, 25 parts by weight of deionized water, 13 parts by weight of iron ore red, 7 parts by weight of zinc phosphate, 20 parts by weight of barium sulfate, 0.6 parts by weight of DMEA and 3 parts by weight of aqueous additive are taken.
3. The method for preparing a water-based iron red primer according to claim 1, characterized in that: The feature model is obtained through model training.
4. The method for preparing a water-based iron red primer according to claim 1, characterized in that: The stirring impeller is provided with a strain gauge for collecting force data.
5. The method for preparing a water-based iron red primer according to claim 4, characterized in that: The stirring impeller is provided with stirring blades, and the plurality of stirring blades are provided with strain gauges. The plurality of strain gauges collect force data during the stirring and dispersing process. When more than 90% of the force data per unit time collected by the strain gauges are consistent with the characteristic model comparison result, it is judged that the stirring and dispersing process is completed.
6. The method for preparing a water-based iron red primer according to claim 5, characterized in that: The stirring blades are arranged in two rows, upper and lower. The force data collected by the strain gauges arranged on the stirring blades in the upper and lower rows correspond to different characteristic models respectively, and when the models are compared and matched, it is judged that the stirring and dispersing process is completed.
7. The method for preparing a water-based iron red primer according to claim 4, characterized in that: An electrode is arranged on the stirring blade, and before adding iron oxide red powder, zinc phosphate and barium sulfate, the iron oxide red powder, zinc phosphate and barium sulfate are charged with opposite charges to those of the electrode.
8. The method for preparing a water-based iron red primer according to claim 1, characterized in that: During the stirring and dispersing process, when the force exceeds a preset threshold, the stirring is stopped.
Citation Information
Patent Citations
Water-based quick-drying weldable pre-coat iron oxide red primer used for steel plates and section steel
CN110343468A
Uniform stirring control method and control device for food stirrer
CN117652902A