High-wear-resistance artificial leather and preparation method thereof

Through the coating liquid composed of polyurethane resin and other materials and the method of controlling the thickness of the coating liquid, the wastewater, waste gas and solid waste treatment problems in the production of high wear-resistant artificial leather are solved, and environmentally friendly and highly wear-resistant artificial leather is prepared, which improves product performance and service life.

CN118895672APending Publication Date: 2024-11-05SHAOXING FURUITE NEW MATERIAL TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411173958.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-26
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

The wastewater, waste gas and solid waste treatment generated by the existing high wear-resistant artificial leather during the production process have environmental protection problems, which limits its development.

Method used

The coating liquid composed of polyurethane resin, plasticizer, filler, pigment, antioxidant and ultraviolet absorber is uniformly coated on the substrate through a coating machine, and is dried and cross-linked to prepare high-quality Wear-resistant artificial leather, controlling the thickness of the coating liquid to ensure product quality.

Benefits of technology

It realizes the preparation of environmentally friendly and highly wear-resistant artificial leather, improves the flexibility, hardness, aging resistance and chemical resistance of the material, while reducing production costs and extending the service life of the product.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0005010178420000021
    Figure BDA0005010178420000021
  • Figure BDA0005010178420000031
    Figure BDA0005010178420000031
  • Figure FDA0005010178410000011
    Figure FDA0005010178410000011
Patent Text Reader

Abstract

The invention relates to the field of artificial leather, in particular to a preparation method of artificial leather with high wear resistance. The artificial leather with high wear resistance comprises a coating liquid, and the coating liquid comprises 50-70% of polyurethane resin, 10-20% of a plasticizer, 5-15% of a filler, 2-5% of a pigment, 0.5-2% of an antioxidant and 0.5-2% of an ultraviolet light absorber. The polyurethane resin is used as a base material, so that the artificial leather is endowed with good physical properties and wear resistance; by adding the plasticizer, the flexibility of the material can be improved, and the texture of the material is closer to that of natural leather; the filler is used for improving the hardness and wear resistance of the artificial leather and reducing the cost; the pigment is used for endowing the artificial leather with required colors; the antioxidant and the ultraviolet light absorber are used for improving the aging resistance of the artificial leather and prolonging the service life of the artificial leather; the cross-linking agent is used for improving the cross-linking density of the material and enhancing the wear resistance and chemical resistance of the material; and the solvent is used for adjusting the viscosity of the material to facilitate processing and forming.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of artificial leather, and in particular to a method for preparing highly wear-resistant artificial leather. Background Art

[0002] Although the existing high wear-resistant artificial leather has significantly improved its wear resistance, there is still room for improvement. And with the increasing global awareness of environmental protection, the problem of wastewater, waste gas and solid waste treatment that may be generated during the production process of high wear-resistant artificial leather has become another major problem restricting its development.

[0003] Therefore, it is important to provide an environmentally friendly, wear-resistant artificial leather. Summary of the invention

[0004] The present invention hopes to provide a method for preparing highly wear-resistant artificial leather, and the specific scheme is as follows:

[0005] A highly wear-resistant artificial leather, characterized in that it comprises a coating liquid, wherein the coating liquid comprises 50-70% polyurethane resin, 10-20% plasticizer, 5-15% filler, 2-5% pigment, 0.5-2% antioxidant and 0.5-2% ultraviolet absorber.

[0006] The plasticizer is a phthalate plasticizer, a terephthalate plasticizer or a trimellitate plasticizer, the filler is nano calcium carbonate or silicon dioxide, the antioxidant is trioctyl phosphite or tridecyl phosphite, and the ultraviolet absorber is Tinuvin-1130.

[0007] First, the polyurethane resin is evenly mixed with a plasticizer, a filler, a pigment, an antioxidant and a UV absorber, and then a solvent is added for dilution. After stirring evenly, an artificial leather coating liquid is obtained, and the coating liquid is evenly coated on a substrate through a coating machine. After drying and cross-linking and curing, a highly wear-resistant artificial leather product is finally obtained.

[0008] The substrate is a polyurethane substrate.

[0009] When the coating liquid is evenly coated on the substrate by the coating machine, the coating liquid thickness conforms to the following formula:

[0010] Wherein T is the thickness, η is the viscosity coefficient, r is the nozzle radius, h is the nozzle height, t is the time, ρ is the coating liquid density, and SC% is the solid content of the coating liquid.

[0011] The present invention has the following advantages:

[0012] 1. Polyurethane resin is used as the matrix material to give artificial leather good physical properties and wear resistance; the addition of plasticizer can improve the flexibility of the material, making it closer to the texture of natural leather; filler is used to improve the hardness and wear resistance of artificial leather while reducing costs; pigment is used to give artificial leather the desired color; antioxidant and ultraviolet absorber are used to improve the aging resistance of artificial leather and extend its service life; cross-linking agent is used to increase the cross-linking density of the material (this formula is the preferred option, and whether it is a condition is confirmed based on the final performance required by the product) and enhance its wear resistance and chemical resistance; solvent is used to adjust the viscosity of the material to facilitate processing and molding.

[0013] 2. This is another important innovation of the present invention. In actual production, the thickness of the coating liquid has a very important influence on the result. If it is too thin, it will be detrimental to the wear resistance, and if it is too thick, it will easily fall off. Therefore, for different coating liquids, we hope that their thickness is different. After further research, we determined the above formula to ensure that the required thickness is achieved and the product quality is guaranteed. DETAILED DESCRIPTION

[0014] The composition of the coating liquid of a highly wear-resistant artificial leather includes the following components to ensure the comprehensive performance of the final product. Specifically, the coating liquid contains 63% of polyurethane resin, which, as the basic material of artificial leather, provides good physical properties and wear resistance, making it perform well in various applications. In addition, in order to improve the flexibility and feel of the material, 16% of plasticizer is added to the coating liquid, of which dibutyl phthalate (DBP) is mainly used. This plasticizer can make the material softer and closer to the texture of natural leather. In order to enhance the hardness and wear resistance of artificial leather, and considering cost-effectiveness, the coating liquid also contains 9% of filler, and nano calcium carbonate is used as filler here, which can not only improve the hardness of the material, but also reduce the cost to a certain extent. In order to give artificial leather rich colors, 3.8% of pigments are added to the coating liquid, which can meet different design requirements and make the product more diversified. In terms of improving the aging resistance of artificial leather, the coating liquid also contains 1.2% of antioxidants and 1.8% of ultraviolet absorbers. The antioxidant used is tridecyl phosphite, which can effectively prevent the material from aging due to oxidation during use; the ultraviolet absorber uses Tinuvin-1130, which can absorb ultraviolet rays and reduce the damage of ultraviolet rays to the material, thereby extending the service life of artificial leather. In addition, according to the final performance requirements of the product, a cross-linking agent can also be added to increase the cross-linking density of the material and further enhance the wear resistance and chemical resistance. In order to ensure that the viscosity of the coating liquid is moderate and easy to process and shape, the addition of solvents is essential. The use of solvents can adjust the viscosity of the material, making it smoother during coating and processing, ensuring the quality of the final product.

[0015] A method for preparing highly wear-resistant artificial leather comprises the following steps: firstly, uniformly mixing polyurethane resin with plasticizer, filler, pigment, antioxidant and ultraviolet absorber, then adding solvent for dilution, stirring evenly to obtain coating liquid for artificial leather, uniformly coating the coating liquid on a polyurethane substrate through a coating machine, drying, cross-linking and curing, and finally obtaining a highly wear-resistant artificial leather product.

[0016] When the coating liquid is evenly coated on the substrate by the coating machine, the coating liquid thickness conforms to the following formula:

[0017] Wherein T is the thickness, η is the viscosity coefficient, r is the nozzle radius, h is the nozzle height, t is the time, ρ is the coating liquid density, and SC% is the solid content of the coating liquid.

[0018] According to the applicant's multiple tests of several schemes of the present application, it is found that the coating liquid of the present application has a solid content of 63% ± 3 according to different specific formulas, and a density range of about 1-1.36 g / cm 3 The viscosity coefficient has a wide range and needs to be tested separately. The nozzle radius and height, especially the nozzle height, are relatively easy to adjust, so this variable can be adjusted in practice.

[0019] The above content describes the technical principles, beneficial effects and features of the present invention. It should be pointed out that the above is only a preferred implementation mode of the present invention, but is not limited to the above embodiments. For technicians in the technical field to which the present invention belongs, some improvements and optimizations can be made without departing from the content of the present invention, which should be regarded as belonging to the protection scope of the present invention.

Claims

1. A highly wear-resistant artificial leather, characterized in that: The coating liquid comprises 50-70% of polyurethane resin, 10-20% of plasticizer, 5-15% of filler, 2-5% of pigment, 0.5-2% of antioxidant and 0.5-2% of ultraviolet absorber.

2. The highly wear-resistant artificial leather according to claim 1, characterized in that: The plasticizer is a phthalate plasticizer, a terephthalate plasticizer or a trimellitate plasticizer, the filler is nano calcium carbonate or silicon dioxide, the antioxidant is trioctyl phosphite or tridecyl phosphite, and the ultraviolet absorber is Tinuvin-1130.

3. A method for preparing the highly wear-resistant artificial leather as claimed in claim 1, characterized in that: First, the polyurethane resin is evenly mixed with a plasticizer, a filler, a pigment, an antioxidant and a UV absorber, and then a solvent is added for dilution. After stirring evenly, an artificial leather coating liquid is obtained, and the coating liquid is evenly coated on a substrate through a coating machine. After drying and cross-linking and curing, a highly wear-resistant artificial leather product is finally obtained.

4. The method for preparing a highly wear-resistant artificial leather as claimed in claim 3, characterized in that: The substrate is a polyurethane substrate.

5. The method for preparing a highly wear-resistant artificial leather as claimed in claim 3, characterized in that: When the coating liquid is evenly coated on the substrate by the coating machine, the coating liquid thickness conforms to the following formula: Wherein T is the thickness, η is the viscosity coefficient, r is the nozzle radius, h is the nozzle height, t is the time, ρ is the coating liquid density, and SC% is the solid content of the coating liquid.