Plasma processing apparatus

By using the lifting mechanism of the mounting table and the ring member in the plasma processing device, the plasma distribution density is controlled, and the difficulty in removing deposits of the mounting table and the ring member is solved, and an efficient and safe cleaning effect is achieved.

CN118901122APending Publication Date: 2024-11-05TOKYO ELECTRON LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380028914.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-12-22
Filing Date
2023-06-15
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

When the existing plasma treatment device removes deposits on the outer peripheral, inner peripheral and lower surface of the mounting table and ring member, it is easy to damage the mounting table, resulting in a shortening of its life and making it difficult to effectively remove deposits.

Method used

A plasma treatment device is designed. By setting up a lifting mechanism of a mounting table and an ring member in the processing container, the plasma is used to clean the plasma on different mounting surfaces, and the distribution density of the plasma is controlled to efficiently remove deposits. At the same time, protect the mounting table.

Benefits of technology

While suppressing damage to the mounting table, the deposits on the outer peripheral part of the mounting table, the inner peripheral part of the ring member and the lower surface of the mounting table are efficiently removed, extending the life of the mounting table, and improving cleaning efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118901122A_ABST
    Figure CN118901122A_ABST
Patent Text Reader

Abstract

The plasma processing apparatus includes: a processing container; a mounting table provided in the processing container, the mounting table having a substrate mounting surface and a ring member mounting surface surrounding an outer periphery of the substrate mounting surface; a ring mounted on the ring member mounting surface; a first lifting mechanism provided with a first lifting pin for supporting the substrate; a second lifting mechanism provided with a second lifting pin for supporting the ring; and a control unit. The control unit is configured to execute a process (a) and a process (b). In the process (a), the inside of the processing container is cleaned using plasma in a state in which the first elevating mechanism is controlled to support the dummy substrate by the first elevating pin. In the process (b), the inside of the processing container is cleaned using plasma in a state in which the second lifting mechanism is controlled to support the ring by means of the second lifting pin.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to a plasma processing apparatus. Background Art

[0002] Conventionally, there is known a technique in which, in a plasma processing apparatus, an edge ring surrounding the outer periphery of a substrate mounting surface is separated from a mounting table on which the edge ring is mounted, and deposits deposited on the mounting table and the edge ring mounted on the mounting table are removed using plasma.

[0003] Prior art literature

[0004] Patent Literature

[0005] Patent Document 1: Japanese Patent Application Publication No. 2012-146743

[0006] Patent Document 2: Japanese Patent Application Publication No. 2019-201047 Summary of the invention

[0007] Problem that the invention aims to solve

[0008] The present disclosure provides a technology capable of removing deposits deposited on the outer peripheral portion of a mounting table, the inner peripheral portion of a ring member, and the lower surface of the ring member while suppressing damage to the mounting table.

[0009] Solutions for solving problems

[0010] A plasma processing device according to one embodiment of the present disclosure comprises: a processing container; a loading table disposed in the processing container, the loading table having a substrate loading surface and a ring member loading surface surrounding the outer periphery of the substrate loading surface; a ring mounted on the ring member loading surface; a first lifting mechanism having a first lifting pin for supporting the substrate; a second lifting mechanism having a second lifting pin for supporting the ring; and a control unit. The control unit is configured to perform processing (a) and processing (b). In processing (a), the processing container is cleaned using plasma while the first lifting mechanism is controlled to support the substrate dummy by the first lifting pin. In processing (b), the processing container is cleaned using plasma while the second lifting mechanism is controlled to support the ring by the second lifting pin.

[0011] Effects of the Invention

[0012] According to the present disclosure, it is possible to remove deposits deposited on the outer peripheral portion of the mounting table, the inner peripheral portion of the ring member, and the lower surface of the ring member while suppressing damage to the mounting table. BRIEF DESCRIPTION OF THE DRAWINGS

[0013] Figure 11 is a system configuration diagram showing an example of a substrate processing system in the first embodiment of the present disclosure.

[0014] Figure 2 This is a schematic cross-sectional view showing the structure of the PM according to the first embodiment.

[0015] Figure 3 This is a flowchart showing an example of the flow of the cleaning process according to the first embodiment.

[0016] Figure 4 This is a diagram showing an example of distribution of plasma generated when high-frequency power is supplied in a state where the edge ring is placed on the second placement surface.

[0017] Figure 5 This is a diagram showing an example of distribution of plasma generated when high-frequency power is supplied in a state where the edge ring is separated from the second mounting surface.

[0018] Figure 6 This is a graph showing the relationship between the height of the lower surface of the edge ring relative to the first mounting surface and the etching rate of the resist film at each position of the mounting table and the edge ring when the edge ring is separated from the second mounting surface.

[0019] Figure 7 This is a flowchart showing an example of the flow of the cleaning process according to Modification 1 of the first embodiment.

[0020] Figure 8 This is a flowchart showing an example of the flow of the cleaning process according to Modification 2 of the first embodiment.

[0021] Fig. 9 This is a schematic cross-sectional view showing an example of the structure of a PM in the second embodiment.

[0022] Fig.10 This is an enlarged cross-sectional view showing an example of the structure near the edge of the electrostatic holding disk.

[0023] Fig.11 This is a flowchart showing an example of the flow of the cleaning process according to the second embodiment.

[0024] Fig.12 This is a flowchart showing an example of the flow of the cleaning process according to the first modification of the second embodiment.

[0025] Fig.13 This is a flowchart showing an example of the flow of the cleaning process according to Modification 2 of the second embodiment.

[0026] Fig.14 This is a flowchart showing an example of the flow of the cleaning process according to Modification 3 of the second embodiment.

[0027] Fig.15 This is a flowchart showing an example of the flow of the cleaning process according to Modification 4 of the second embodiment.

[0028] Fig.16 This is a flowchart showing an example of the flow of the cleaning process according to the fifth modification of the second embodiment.

[0029] Fig.17 This is a flowchart showing an example of the flow of the cleaning process according to Modification 6 of the second embodiment.

[0030] Fig.18 This is a flowchart showing an example of the flow of the cleaning process according to Modification 7 of the second embodiment.

[0031] Fig.19 This is a flowchart showing an example of the flow of the cleaning process according to Modification 8 of the second embodiment.

[0032] Fig. 20 This is a flowchart showing an example of the flow of the cleaning process according to Modification 9 of the second embodiment.

[0033] Fig.21 This is a flowchart showing an example of the flow of the cleaning process according to Modification 10 of the second embodiment. DETAILED DESCRIPTION

[0034] Hereinafter, embodiments of the plasma processing apparatus and cleaning method disclosed in the present application will be described in detail with reference to the accompanying drawings. In addition, the present disclosure is not limited by this embodiment. Each embodiment can be appropriately combined within the scope that does not cause contradiction in the processing content.

[0035] In a plasma processing device, a deposit composed of reaction products such as CF-based polymers is deposited on the substrate mounting surface of a mounting table by performing plasma processing. Due to the deposition of the deposit on the substrate mounting surface, abnormalities such as poor adsorption of the substrate may occur. Therefore, in the plasma processing device, dry cleaning is performed to remove the deposit deposited on the substrate mounting surface by plasma processing.

[0036] Here, for example, when the diameter of the substrate mounting surface is smaller than the diameter of the substrate, the reaction product of the processing gas used in the plasma treatment enters between the outer periphery of the mounting table and the back side of the wafer, so that the deposit is sometimes partially deposited on the outer periphery of the mounting table. In addition, a ring member such as an edge ring that surrounds the substrate mounting surface in a manner separated from the outer periphery of the mounting table by a small interval is arranged around the outer periphery of the mounting table. Therefore, since the reaction product enters the area between the outer periphery of the mounting table and the inner periphery of the ring member, the deposit is sometimes partially deposited on the outer periphery of the mounting table, the inner periphery of the ring member, and the lower surface of the ring member. However, since the area between the outer periphery of the mounting table and the inner periphery of the ring member is narrow, it is difficult for plasma to enter the area between the outer periphery of the mounting table and the inner periphery of the ring member and the lower surface of the ring member compared to other areas. Therefore, the deposit is easy to remain on the outer periphery of the mounting table after dry cleaning, the inner periphery of the ring member, and the lower surface of the ring member.

[0037] As described above, deposits tend to be more likely to accumulate on the outer peripheral portion of the mounting table, the inner peripheral portion of the ring member, and the lower surface of the ring member than on other regions.

[0038] In order to remove the deposits deposited on the outer periphery of the mounting table, the inner periphery of the ring member and the lower surface of the ring member, for example, it is considered to extend the dry cleaning time. However, when the dry cleaning time is extended, the damage to the mounting table becomes greater, which may shorten the life of the mounting table.

[0039] Therefore, it is expected to remove the deposits deposited on the outer peripheral portion of the mounting table, the inner peripheral portion of the ring member, and the lower surface of the ring member while suppressing damage to the mounting table.

[0040] (First Embodiment)

[0041] [Structure of Substrate Processing System 50]

[0042] Figure 1 1 is a system configuration diagram showing an example of a substrate processing system 50 in the first embodiment of the present disclosure. The substrate processing system 50 includes a VTM (Vacuum Transfer Module) 51, a storage device 52, a plurality of LLMs (Load Lock Modules) 53, an EFEM (Equipment Front End Module) 54, and a plurality of PMs (Process Modules) 1. A plurality of PMs 1 are connected to the side wall of the VTM 51 via a gate valve G1. Figure 1In the example of FIG. 5 , six PMs 1 are connected to the VTM 51. However, the number of PMs 1 connected to the VTM 51 may be more than six or less than six. The VTM 51 is an example of a vacuum transfer device.

[0043] Each PM 1 performs a process such as etching or film formation using plasma on a wafer W (an example of a substrate) as a processing target. A plurality of LLMs 53 are connected to the other side wall of the VTM 51 via a gate valve G2. Figure 1 In the example, two LLMs 53 are connected to the VTM 51, but the number of LLMs 53 connected to the VTM 51 may be more than two or may be only one.

[0044] A transport robot 510 is disposed in the VTM 51. The transport robot 510 is an example of a transport device. The transport robot 510 has an arm 511 and a fork 512. The fork 512 is provided at the front end of the arm 511. The fork 512 carries a wafer W, an edge ring, and a wafer dummy (an example of a substrate dummy). The transport robot 510 transports the wafer W between PM 1 and other PM 1s, and between PM 1 and LLM 53. In addition, the transport robot 510 transports an edge ring and a wafer dummy between PM 1 and a storage device 52. The interior of the VTM 51 is maintained at a predetermined pressure atmosphere lower than the atmospheric pressure.

[0045] One side wall of each LLM 53 is connected to the VTM 51 via a gate valve G2, and the other side wall is connected to the EFEM 54 via a gate valve G3. When the wafer W is carried into the LLM 53 from the EFEM 54 via the gate valve G3, the gate valve G3 is closed, and the pressure in the LLM 53 is reduced to the same level as the pressure in the VTM 51. Then, the gate valve G2 is opened, and the wafer W in the LLM 53 is carried out into the VTM 51 by the transfer robot 510.

[0046] In addition, when the pressure in the LLM 53 is equal to the pressure in the VTM 51, the wafer W is carried into the LLM 53 from the VTM 51 via the gate valve G2 by the transfer robot 510, and the gate valve G2 is closed. Furthermore, the pressure in the LLM 53 is increased to the same level as the pressure in the EFEM 54. Then, the gate valve G3 is opened, and the wafer W in the LLM 53 is carried out into the EFEM 54.

[0047] A plurality of loading ports 55 are provided on the side wall of the EFEM 54 opposite to the side wall provided with the gate valve G3. A container such as a FOUP (Front Opening Unified Pod) capable of accommodating a plurality of wafers W is connected to each loading port 55.

[0048] The inside of the EFEM 54 is, for example, at atmospheric pressure. A transfer robot 540 is provided in the EFEM 54. The transfer robot 540 moves in the EFEM 54 along a guide rail 541 provided in the EFEM 54 to transfer the wafer W between the LLM 53 and the container connected to the load port 55. An FFU (Fan Filter Unit) or the like is provided in the upper portion of the EFEM 54 to supply dry air from which particles and the like have been removed from the upper portion into the EFEM 54 and form a downward flow in the EFEM 54. In addition, in the present embodiment, the inside of the EFEM 54 is at atmospheric pressure, but as another mode, the pressure in the EFEM 54 may also be controlled to be a positive pressure. Thus, it is possible to suppress the intrusion of particles and the like into the EFEM 54 from the outside.

[0049] The EFEM 54 is connected to an aligner AN. The aligner AN is configured to adjust the position of the wafer W. The aligner AN may also be configured to adjust the position of the edge ring. The aligner AN may be provided inside the EFEM 54 .

[0050] The other side wall of the VTM 51 is connected to a receiving device 52 via a gate valve G4. The receiving device 52 is used to receive edge rings and wafer dummy sheets. In the present embodiment, the receiving device 52 receives edge rings for replacement, edge rings after use, and wafer dummy sheets. The receiving device 52 has a function of switching the pressure in the receiving device 52 between atmospheric pressure and the same pressure as that in the VTM 51. In addition, the edge ring for replacement can be a new edge ring or an edge ring that has been used but has a small consumption.

[0051] For example, when the pressure in the storage device 52 is equal to that in the VTM 51, the gate valve G4 is opened, and the used edge ring is stored in the storage device 52 from the PM 1 via the VTM 51 by the transport robot 510. Then, the edge ring for replacement is carried from the storage device 52 to the PM 1 via the VTM 51 by the transport robot 510. Then, the gate valve G4 is closed, and the pressure in the storage device 52 is switched from the pressure equal to that in the VTM 51 to the atmospheric pressure, and then the gate valve G5 is opened, and the used edge ring is carried out to the outside of the storage device 52 via the gate valve G5. Then, the edge ring for replacement is carried into the storage device 52 via the gate valve G5.

[0052] In addition, for example, when the pressure in the storage device 52 is equal to that in the VTM 51, the gate valve G4 is opened, and the dummy wafer is moved into the PM 1 through the VTM 51 by the transfer robot 510. Then, after the cleaning in the PM 1 is completed, the dummy wafer is returned to the storage device 52 by the transfer robot 510. When replacing the dummy wafer, for example, after the pressure in the storage device 52 is switched from the pressure equal to that in the VTM 51 to the atmospheric pressure, the gate valve G5 is opened, and the dummy wafer is moved out of the storage device 52 through the gate valve G5. Then, the dummy wafer for replacement is moved into the storage device 52 through the gate valve G5. The dummy wafer for replacement can be a new dummy wafer or a dummy wafer that has been used but has a small consumption.

[0053] In addition, Figure 1 In the example of the embodiment, the storage device 52 is connected to the outer side of the side wall of the VTM 51, but the disclosed technology is not limited thereto. For example, as another example, the storage device 52 may be connected to the outer side of the side wall of the EFEM 54, or may be arranged inside the EFEM 54. In addition, in this case, the wafer dummy may be stored in the storage device 52, or may be stored in a container such as a FOUP connected to the load port 55.

[0054] The control unit 9 processes computer executable commands for causing the substrate processing system 50 to execute various processes described in the present disclosure. The control unit 9 can be configured to control the various elements of the substrate processing system 50 to execute the various processes described herein. In one embodiment, a part or all of the control unit 9 can be included in the substrate processing system 50. The control unit 9 can include a processing unit 9a1, a storage unit 9a2, and a communication interface 9a3. The control unit 9 is implemented, for example, by a computer 9a. The processing unit 9a1 can be configured to read a program from the storage unit 9a2 and execute the read program, thereby performing various control actions. The program can be stored in the storage unit 9a2 in advance, or it can be obtained via a medium when necessary. The obtained program is stored in the storage unit 9a2, and the processing unit 9a1 reads the program from the storage unit 9a2 and executes it. The medium can be various storage media that can be read by the computer 9a, or it can be a communication line connected to the communication interface 9a3. The processing unit 9a1 can be a CPU (Central Processing Unit: Central Processing Unit). The storage unit 9a2 may include a RAM (Random Access Memory), a ROM (Read Only Memory), a HDD (Hard Disk Drive), an SSD (Solid State Drive), or a combination thereof. The communication interface 9a3 may communicate with the substrate processing system 50 via a communication line such as a LAN (Local Area Network).

[0055] [Structure of plasma processing apparatus]

[0056] Figure 2 : is a schematic cross-sectional view showing the structure of PM 1 involved in the first embodiment. PM 1 is an example of a plasma processing device. In the present embodiment, PM 1 is a capacitively coupled plasma processing device. PM 1 is airtightly constructed and has a processing container (also appropriately referred to as a "plasma processing chamber") 10 that is set to an electrical ground potential. The processing container 10 is cylindrical and is made of, for example, aluminum. The processing container 10 divides a processing space for generating plasma. A mounting table 2 that horizontally supports a semiconductor wafer (hereinafter referred to as a "wafer") W serving as a substrate (work-piece) is provided in the processing container 10. The mounting table 2 is constructed to include a substrate (base) 2a and an electrostatic holding disk (ESC: Electrostatic chuck) 6.

[0057] The substrate 2a is made of a conductive metal such as aluminum and functions as a lower electrode. The substrate 2a is supported by an insulating support 4. The support 4 is supported by a support member 3 made of, for example, quartz.

[0058] The electrostatic holding disk 6 is in the shape of a disk with a flat upper surface, and the upper surface constitutes a first mounting surface 6e for mounting the wafer W. The electrostatic holding disk 6 is disposed at the center of the mounting table 2 in a plan view. The electrostatic holding disk 6 is configured such that an electrode 6a is disposed between the insulators 6b, and a DC power supply 17 is connected to the electrode 6a. Furthermore, the configuration is such that a DC voltage is applied from the DC power supply 17 to the electrode 6a, so that the wafer W is electrostatically adsorbed by the Coulomb force.

[0059] In addition, in the present embodiment, the diameter of the first mounting surface 6 e is set to be slightly smaller than the diameter of the wafer W as an example.

[0060] The outer periphery above the mounting table 2 forms a second mounting surface 6f. The second mounting surface 6f surrounds the first mounting surface 6e and is formed at a position lower than the first mounting surface 6e. An edge ring 5 formed of, for example, single crystal silicon is arranged on the second mounting surface 6f. The edge ring 5 is formed in a ring shape and is arranged on the second mounting surface 6f in a manner surrounding the outer periphery of the first mounting surface 6e in the mounting table 2. In addition, a cylindrical inner wall member 3a made of, for example, quartz is provided in the processing container 10 in a manner surrounding the mounting table 2 and the support table 4.

[0061] The substrate 2a is connected to the first RF power supply 14a via the first matching device 15a, and is also connected to the second RF power supply 14b via the second matching device 15b. The first RF power supply 14a is used to generate plasma, and is configured to supply a high-frequency power of a predetermined frequency from the first RF power supply 14a to the substrate 2a of the stage 2. In addition, the second RF power supply 14b is used to attract ions (for generating bias), and is configured to supply a high-frequency power of a predetermined frequency lower than the frequency of the first RF power supply 14a from the second RF power supply 14b to the substrate 2a of the stage 2. In this way, the stage 2 is configured to be able to apply a voltage. On the other hand, above the stage 2, a shower head 16 is provided in a manner parallel to the stage 2, and the shower head 16 has a function as an upper electrode. The shower head 16 and the stage 2 function as a pair of electrodes (upper electrode and lower electrode).

[0062] A temperature control medium flow path 2d is formed inside the mounting table 2, and an inlet pipe 2b and an outlet pipe 2c are connected to the temperature control medium flow path 2d. Moreover, the structure is such that the mounting table 2 can be controlled to a predetermined temperature by circulating an appropriate temperature control medium, such as cooling water, in the temperature control medium flow path 2d. In addition, a gas supply pipe 130 for supplying a heat transfer gas (back side gas) such as helium to the back side of the wafer W is provided in a manner penetrating the mounting table 2, etc., and the gas supply pipe 130 is connected to a gas supply source not shown. Through these structures, the wafer W adsorbed and held on the upper surface of the mounting table 2 by the electrostatic holding disk 6 is controlled to a predetermined temperature.

[0063] The mounting table 2 is provided with a plurality of, for example, three, pin through holes 200 (in Figure 2 Only one is shown in the figure. ), lift pins 161 are respectively arranged inside these pin through holes 200. The lift pins 161 are connected to the lift mechanism 162. The lift mechanism 162 lifts and lowers the lift pins 161 so that the lift pins 161 can move freely to protrude and retract relative to the first loading surface 6e of the loading table 2. When the lift pins 161 are raised, the front ends of the lift pins 161 protrude from the first loading surface 6e of the loading table 2 to hold the wafer W above the first loading surface 6e of the loading table 2. On the other hand, when the lift pins 161 are lowered, the front ends of the lift pins 161 are accommodated in the pin through holes 200 to load the wafer W on the first loading surface 6e of the loading table 2. In this way, the lift mechanism 162 lifts and lowers the wafer W relative to the first loading surface 6e of the loading table 2 through the lift pins 161. In addition, the lifting mechanism 162 holds the wafer W above the first mounting surface 6 e of the mounting table 2 via the lifting pins 161 in a state where the lifting pins 161 are lifted.

[0064] In addition, the mounting table 2 is provided with a plurality of, for example, three, pin through holes 300 (in Figure 2Only one is shown in the figure. ), lift pins 163 are respectively arranged inside these pin through holes 300. The lift pins 163 are connected to the lift mechanism 164. The lift mechanism 164 lifts and lowers the lift pins 163 so that the lift pins 163 can freely move to protrude and retract relative to the second loading surface 6f of the loading table 2. When the lift pins 163 are raised, the front ends of the lift pins 163 protrude from the second loading surface 6f of the loading table 2 to hold the edge ring 5 above the second loading surface 6f of the loading table 2. On the other hand, when the lift pins 163 are lowered, the front ends of the lift pins 163 are accommodated in the pin through holes 300 so that the edge ring 5 is loaded on the second loading surface 6f of the loading table 2. In this way, the lift mechanism 164 lifts and lowers the edge ring 5 relative to the second loading surface 6f of the loading table 2 through the lift pins 163. In addition, the lifting mechanism 164 holds the edge ring 5 above the second mounting surface 6 f of the mounting table 2 via the lifting pins 163 in a state in which the lifting pins 163 are lifted.

[0065] The shower head 16 is provided on the top wall of the processing container 10. The shower head 16 includes a main body 16a and an upper top plate 16b constituting an electrode plate, and the shower head 16 is supported on the upper part of the processing container 10 via an insulating member 95. The main body 16a is made of a conductive material, such as aluminum with an anodized surface, and the main body 16a is configured to be able to detachably support the upper top plate 16b at its lower part.

[0066] A gas diffusion chamber 16c is provided inside the main body 16a. In addition, a large number of gas flow holes 16d are formed at the bottom of the main body 16a so as to be located below the gas diffusion chamber 16c. In addition, a gas introduction hole 16e is provided on the upper top plate 16b so as to penetrate the upper top plate 16b in the thickness direction, and the gas introduction hole 16e is provided so as to overlap with the above-mentioned gas flow hole 16d. With such a structure, the processing gas supplied to the gas diffusion chamber 16c is dispersed and supplied to the processing container 10 in a spray-like manner through the gas flow hole 16d and the gas introduction hole 16e.

[0067] A gas inlet port 16g for introducing a processing gas into the gas diffusion chamber 16c is formed in the main body 16a. One end of a gas supply pipe 18a is connected to the gas inlet port 16g. A gas supply source (gas supply unit) 15 for supplying a processing gas is connected to the other end of the gas supply pipe 18a. A mass flow controller (MFC) 18b and an opening and closing valve V2 are provided in the gas supply pipe 18a in sequence from the upstream side. A processing gas for plasma etching is supplied from the gas supply source 18 to the gas diffusion chamber 16c via the gas supply pipe 18a. The processing gas is supplied in a spray-like manner to the processing container 10 via the gas flow hole 16d and the gas inlet hole 16e.

[0068] The shower head 16 as the upper electrode is electrically connected to the variable DC power supply 72 via a low pass filter (LPF) 71. The variable DC power supply 72 is configured to be able to turn on / off the power supply by using an on / off switch 73. The current / voltage of the variable DC power supply 72 and the on / off of the on / off switch 73 are controlled by the control unit 100 described later. In addition, as described later, when a high frequency is applied from the first RF power supply 14a and the second RF power supply 14b to the mounting table 2 to generate plasma in the processing space, the on / off switch 73 is turned on by the control unit 100 as needed. Thus, a predetermined DC voltage is applied to the shower head 16 as the upper electrode.

[0069] A cylindrical ground conductor 10c is provided so as to extend from the side wall of the processing container 10 to a position above the height position of the shower head 16. The cylindrical ground conductor 10c has a ceiling wall at its upper portion.

[0070] An exhaust port 81 is formed at the bottom of the processing container 10. The exhaust port 81 is connected to a first exhaust device 83 via an exhaust pipe 82. The first exhaust device 83 has a vacuum pump, and is configured to reduce the pressure in the processing container 10 to a predetermined vacuum level by operating the vacuum pump. On the other hand, a wafer W loading and unloading port 84 is provided on the side wall of the processing container 10, and a gate valve 85 is provided at the loading and unloading port 84 to open and close the loading and unloading port 84. The gate valve 85 is connected to the first exhaust device 83. Figure 1 Corresponding to gate valve G1.

[0071] A sediment shield 86 is provided along the inner wall surface on the inner side of the processing container 10. The sediment shield 86 is used to prevent etching byproducts (sediments) from being deposited on the processing container 10. A conductive member (GND block) 89 connected in a manner that can control the potential relative to the ground is provided at a height position substantially the same as that of the wafer W of the sediment shield 86, thereby preventing abnormal discharge. In addition, a sediment shield 87 extending along the inner wall member 3a is provided at the lower end of the sediment shield 86. The sediment shields 86 and 87 are provided to be detachable.

[0072] The operation of the PM 1 having the above configuration is centrally controlled by the control unit 100. The control unit 100 is provided with a process controller 101, a user interface 102, and a storage unit 103. The process controller 101 includes a CPU for controlling each unit of the PM 1.

[0073] The user interface 102 is composed of a keyboard for the process manager to input commands to manage the PM 1 , a display that visually displays the operating status of the PM 1 , and the like.

[0074] The storage unit 103 stores control programs (software) for realizing various processes executed by the PM 1 under the control of the process controller 101, and processes storing processing condition data, etc. Furthermore, as required, any process is called out from the storage unit 103 according to instructions from the user interface 102, etc., and the process controller 101 is caused to execute the process, thereby performing the desired process by the PM 1 under the control of the process controller 101. In addition, regarding the processes such as the control program and the processing condition data, it is possible to use the programs and processes in a state stored in a computer storage medium (e.g., a hard disk, a CD, a floppy disk, a semiconductor memory, etc.) that can be read by a computer. In addition, the processes such as the control program and the processing condition data can also be used online by being transmitted in real time from other devices via, for example, a dedicated line.

[0075] In addition, in the above example, the case where PM 1 is controlled by the control unit 100 is illustrated, but PM 1 may be connected to the control unit 9 of the substrate processing system 50 and controlled by the control unit 9. In this case, the control unit 9 may be integrally formed with the control unit 100 or may be separately formed from the control unit 100. In addition, PM 1 may be controlled by the cooperation of the control unit 100 and the control unit 9.

[0076] [An Example of a Cleaning Process Flow According to the First Embodiment]

[0077] Next, refer to Figure 3 The flow of the cleaning process performed by the PM 1 according to the first embodiment will be described. Figure 31 is a flowchart showing an example of the flow of the cleaning process according to the first embodiment. The cleaning process is mainly realized by the PM 1 operating according to the control of the control unit 100. Figure 3 In addition, the cleaning process is performed in a state where no wafer W is contained in the processing container 10. Figure 3 Illustrated cleaning process.

[0078] First, the control unit 100 determines whether it is time to perform the cleaning process (S100). The timing for performing the cleaning process includes, for example, the timing for performing a process such as plasma etching of a predetermined number of wafers W. If it is not time to perform the cleaning process (S100: No), the process of step S100 is performed again.

[0079] On the other hand, when the timing for executing the cleaning process has come (S100: Yes), the edge ring 5 is separated from the second mounting surface 6f by raising the lifting pins 163 (raising the pins) (S101). Information on the separation distance between the edge ring 5 and the second mounting surface 6f is pre-stored in the storage unit 103, for example, and the control unit 100 raises the lifting pins 163 based on the information stored in the storage unit 103.

[0080] Next, after the processing container 10 is depressurized to a predetermined vacuum degree by the first exhaust device 83, a reaction gas is supplied from the gas supply source 18 to the processing container 10 via the gas supply pipe 18a (S102). In the present embodiment, when the deposit to be cleaned is a CF-based polymer, the reaction gas supplied from the gas supply source 18 is O2 gas. In addition, the reaction gas is not limited to O2 gas, and may also be other oxygen-containing gases such as CO gas, CO2 gas, and O3 gas. In addition, when the deposit contains silicon and metal in addition to the CF-based polymer, a halogen-containing gas, for example, may be added to the reaction gas O2 gas. The halogen-containing gas is, for example, a fluorine-based gas such as CF4 gas and NF3 gas. In addition, the halogen-containing gas may be a chlorine-based gas such as Cl2 gas, or a bromine-based gas such as HBr gas. In this way, an oxygen-containing gas is used as a reaction gas in the cleaning process.

[0081] Next, high-frequency power is supplied to the mounting table 2 as the lower electrode (S103). In step S103, the control unit 100 controls the first RF power supply 14a and the second RF power supply 14b to generate high-frequency power, thereby supplying high-frequency power to the substrate 2a of the mounting table 2. In addition, the control unit 100 applies the DC power supplied from the variable DC power supply 72 to the shower head 16 by turning on the on-off switch 73. As a result, a plasma of oxygen-containing gas is generated in the processing container 10. In addition, there is no particular limitation on the frequency of the high-frequency power generated by the first RF power supply 14a and the second RF power supply 14b. In addition, an example in which PM 1 has the first RF power supply 14a and the second RF power supply 14b is shown here, but PM 1 does not necessarily have the second RF power supply 14b. In addition, an example in which PM 1 has the variable DC power supply 72 is shown here, but PM 1 does not necessarily have the variable DC power supply 72.

[0082] Next, the control unit 100 determines whether a preset processing time has elapsed since the start of supply of high-frequency power in step S103 (S104). If the preset processing time has not elapsed (S104: No), the process of step S104 is executed again.

[0083] On the other hand, when the set processing time has elapsed (S104: Yes), the supply of high frequency power to the mounting table 2 is stopped (S105). In addition, the supply of the reaction gas into the processing container 10 is stopped (S106). Thus, the generation of the plasma of the oxygen-containing gas in the processing container 10 is stopped.

[0084] Then, after exhausting the reaction gas in the processing container 10 , the edge ring 5 is placed on the second placement surface 6 f by lowering the lift pins 163 . At this point, the cleaning method shown in this flowchart is completed.

[0085] [Regarding Plasma Generated in Cleaning Process in First Embodiment]

[0086] Figure 4 This is a diagram showing an example of distribution of plasma generated when high-frequency power is supplied in a state where the edge ring 5 is placed on the second placement surface 6f. Figure 5 This is a diagram showing an example of distribution of plasma generated when high-frequency power is supplied in a state where the edge ring 5 is separated from the second mounting surface 6 f.

[0087] like Figure 4 As shown, when high frequency power is supplied from the first RF power supply 14 a to the mounting table 2 with the edge ring 5 mounted on the second mounting surface 6 f, the plasma P is uniformly distributed in the in-plane direction of the mounting table 2 in the reduced pressure space between the mounting table 2 and the shower head 16 .

[0088] On the other hand, the inventors of the present application have found that by separating the edge ring 5 from the second mounting surface 6f and appropriately setting the separation distance, it is possible to Figure 5 As shown in the figure, the plasma P is unevenly distributed around a specific area above the mounting table 2. Specifically, the inventors of the present application found that by separating the edge ring 5 from the second mounting surface 6f and appropriately setting the separation distance, the plasma P can be unevenly distributed around the area between the outer edge of the first mounting surface 6e and the inner edge of the lower surface of the edge ring 5.

[0089] For example, this mechanism can be described as follows. That is, when the edge ring 5 is separated from the second mounting surface 6f, a decompression space is also formed between the edge ring 5 and the second mounting surface 6f. This decompression space can be regarded as a capacitor on the path of the high-frequency power from the first RF power source 14a to the ground connected to the shower head 16 via the mounting table 2. This capacitor becomes a part of the synthetic impedance on the path of the high-frequency power from the first RF power source 14a to the ground.

[0090] Here, consider the path of the high-frequency power from the mounting table 2 to the shower head 16 divided into the path above the first mounting surface 6e and the path above the second mounting surface 6f (hereinafter referred to as "the path of the first mounting surface" and "the path of the second mounting surface"). Figure 4 As shown in FIG. 1 , when the edge ring 5 is placed on the second placement surface 6f, the synthetic impedance per unit area in the in-plane direction of the placement table 2 is almost the same in the path on the first placement surface and the path on the second placement surface. Figure 5 As shown, when the edge ring 5 is separated from the second mounting surface 6f, the path on the second mounting surface becomes a parallel path of a path passing through the edge ring 5 and a path at a position outside the edge ring 5 and not passing through the edge ring 5. The path passing through the edge ring 5 is a path passing through a capacitor of a decompression space formed between the edge ring 5 and the second mounting surface 6f, and the path not passing through the edge ring 5 is a path not passing through the above-mentioned capacitor.

[0091] Therefore, the combined impedance per unit area formed by the two parallel high-frequency power paths above the second placement surface 6f is lower than the combined impedance per unit area formed above the first placement surface 6e.

[0092] The high-frequency power flows intensively in the area above the second mounting surface 6f where the synthetic impedance is relatively low. Moreover, when the separation distance between the second mounting surface 6f and the edge ring 5 is appropriately set, the high-frequency power flows intensively in the area between the outer edge of the first mounting surface 6e and the inner edge of the lower surface of the edge ring 5 in the area above the second mounting surface 6f. As a result, the density of the plasma P in the area between the outer edge of the first mounting surface 6e and the inner edge of the lower surface of the edge ring 5 is higher than the density of the plasma P in other areas, and a ring-shaped plasma P is formed around the area between the outer edge of the first mounting surface 6e and the inner edge of the lower surface of the edge ring 5.

[0093] In the cleaning process according to the first embodiment, by using the plasma P unevenly distributed around the area between the outer edge of the first mounting surface 6e and the inner edge of the lower surface of the edge ring 5, the deposits can be removed intensively at a position where the density of the plasma is relatively high. That is, according to the cleaning process according to the first embodiment, the plasma P can be concentrated around the area between the outer edge of the first mounting surface 6e and the inner edge of the lower surface of the edge ring 5, thereby improving the removal force of the deposits at the outer periphery of the mounting table 2, the inner periphery of the edge ring 5, and the lower surface of the edge ring 5. Therefore, the deposits deposited on the outer periphery of the mounting table 2, the inner periphery of the edge ring 5, and the lower surface of the edge ring 5 can be reliably removed in a short time. In addition, in other areas other than the area between the outer edge of the first mounting surface 6e and the inner edge of the lower surface of the edge ring 5, the density of the plasma P is relatively low, so it is possible to suppress the parts of the mounting table 2 corresponding to other areas from being damaged by the plasma P. For example, the density of plasma P formed in the area above the first mounting surface 6e is lower than the density of plasma P formed in the area between the outer edge of the first mounting surface 6e and the inner edge of the lower surface of the edge ring 5, thereby suppressing damage to the first mounting surface 6e.

[0094] As described above, according to the cleaning process according to the first embodiment, deposits deposited on the outer periphery of the mounting table 2 , the inner periphery of the edge ring 5 , and the lower surface of the edge ring 5 can be removed while suppressing damage to the mounting table 2 .

[0095] Furthermore, according to the cleaning process according to the first embodiment, deposits can be removed efficiently without preparing electrodes of a special structure for generating local plasma on the outer periphery of the mounting table 2 , the inner periphery of the edge ring 5 , and the lower surface of the edge ring 5 .

[0096] In addition, the CF-based polymer deposits in the deposits deposited on the outer periphery of the mounting table 2, the inner periphery of the edge ring 5, and the lower surface of the edge ring 5 can be removed by the plasma of an oxygen-containing gas such as O2 gas. In addition, Si-based or metal-based deposits can be removed by the plasma of a halogen-containing gas such as CF4 gas, NF3 gas, Cl2 gas, HBr gas, etc. In addition, mixed deposits of CF-based polymers and at least one of Si-based and metal-based deposits can be removed by the plasma of a mixed gas of an oxygen-containing gas and a halogen-containing gas. In addition, the CF-based polymer deposits can also be removed by a hydrogen-containing gas such as H2 gas, or a nitrogen-containing gas such as N2. In addition, rare gases such as argon and helium can also be added.

[0097] (Removal force based on cleaning process)

[0098] The inventors of the present application conducted an experiment to investigate the removal power of the cleaning process involved in the first embodiment against CF-based polymer deposits. In the experiment, a test piece coated with an anti-etching film that is an organic film similar to the CF-based polymer deposits was set at multiple positions on the stage 2 and the edge ring 5 instead of the CF-based polymer deposits. In addition, in the experiment, the etching rate of the anti-etching film at each position of the stage 2 and the edge ring 5 after performing the cleaning process involved in the first embodiment was measured as the removal power of the CF-based polymer deposits. Figure 6 The experimental results are shown in FIG. Figure 6 It is a graph showing the relationship between the height of the lower surface of the edge ring 5 relative to the first mounting surface 6 e and the etching rate of the resist film at each position of the mounting table 2 and the edge ring 5 when the edge ring 5 is separated from the second mounting surface 6 f.

[0099] Figure 6 The processing conditions for the experimental results shown are as follows.

[0100] Pressure in the processing container 10: 400mT

[0101] High frequency power (first RF power source 14a / second RF power source 14b): 600W / 0W

[0102] DC voltage (variable DC power supply 72): 0V

[0103] Gas type and flow rate: O2 gas = 700 sccm

[0104] Diameter of wafer W: 300 mm (wafer W is not contained in the processing container 10)

[0105] Processing time: 60 seconds

[0106] in addition, Figure 6The illustration in FIG. 1 shows the placement of the test piece coated with the anti-corrosion film. Figure 6 In the legend of FIG. 1 , “ER upper surface” indicates the upper surface of the edge ring 5 , and “ER lower surface” indicates the lower surface of the edge ring 5 .

[0107] like Figure 6 As shown in the figure, when the height of the lower surface of the edge ring 5 is less than 1.4 mm, the etching rate at the outer edge of the first mounting surface 6e and the lower surface of the edge ring 5 is reduced. From this result, it can be seen that when the height of the lower surface of the edge ring 5 is less than 1.4 mm, the difference between the density of plasma generated around the area between the outer edge of the first mounting surface 6e and the inner edge of the lower surface of the edge ring 5 and the density of plasma generated in other areas is not so large.

[0108] In addition, if Figure 6 As shown in FIG. 1 , when the height of the lower surface of the edge ring 5 is greater than 4.4 mm, the etching rate at the outer edge of the first mounting surface 6e and the lower surface of the edge ring 5 is reduced. From this result, it can be seen that when the height of the lower surface of the edge ring 5 is greater than 4.4 mm, the difference between the density of plasma generated around the area between the outer edge of the first mounting surface 6e and the inner edge of the lower surface of the edge ring 5 and the density of plasma generated in other areas is not that large.

[0109] According to the above results, it is preferable that the height of the lower surface of the edge ring 5 relative to the first mounting surface 6e is set to be greater than 1.4 mm and less than 4.4 mm when the edge ring 5 is separated from the second mounting surface 6f. By setting the height of the lower surface of the edge ring 5 within this range, the plasma can be appropriately unevenly distributed around the area between the outer edge of the first mounting surface 6e and the inner edge of the lower surface of the edge ring 5. That is, it is possible to generate annular plasma around the area between the outer edge of the first mounting surface 6e of the mounting table 2 and the inner edge of the lower surface of the edge ring 5 while protecting the first mounting surface 6e of the mounting table 2 from the influence of the plasma.

[0110] In addition, if Figure 6 As shown in FIG. 1 , when the height of the lower surface of the edge ring 5 is 2.4 mm, the etching rate of the outer edge of the first mounting surface 6e is the highest. Based on this result, it is preferable that the height of the lower surface of the edge ring 5 relative to the first mounting surface 6e when the edge ring 5 is separated from the second mounting surface 6f is 1.6 mm or more and 3.4 mm or less, and more preferably 2.0 mm or more and 2.8 mm or less. By setting the height of the lower surface of the edge ring 5 within this range, the deposits deposited on the outer periphery of the mounting table 2, the inner periphery of the edge ring 5, and the lower surface of the edge ring 5 can be reliably removed in a short time.

[0111] [Modification of the first embodiment]

[0112] In the above cleaning process, PM 1 can further separate the edge ring 5 from the second mounting surface 6f after stopping the generation of plasma, and then generate plasma in the processing container 10 to clean the mounting table 2 and the edge ring 5. Figure 7 The cleaning process will be described below.

[0113] Figure 7 This is a flowchart showing an example of a cleaning process flow according to Modification 1 of the first embodiment. The cleaning process is mainly realized by PM1 operating under the control of the control unit 100. Figure 7 In addition, the cleaning process is performed in a state where no wafer W is contained in the processing container 10. Figure 7 In addition, Figure 7 Steps S200 to S206 and Figure 3 The steps S100 to S106 shown are the same, so their detailed description is omitted here.

[0114] When the supply of high frequency power and the supply of reaction gas are stopped to stop generating plasma (S205, S206), the edge ring 5 is further separated from the second mounting surface 6f by further raising the lifting pins 163 (S207). Information on the separation distance between the edge ring 5 and the second mounting surface 6f is pre-stored in the storage unit 103, for example, and the control unit 100 raises the lifting pins 163 based on the information stored in the storage unit 103. The separation distance in step S207 is greater than the separation distance in step S201.

[0115] Next, after the interior of the processing container 10 is depressurized to a predetermined vacuum level by the first exhaust device 83 , a reaction gas is supplied from the gas supply source 18 through the gas supply pipe 18 a into the processing container 10 ( S208 ).

[0116] Next, high frequency power is supplied to the mounting table 2 as the lower electrode (S209). In step S209, the control unit 100 controls the first RF power supply 14a and the second RF power supply 14b to generate high frequency power, thereby supplying high frequency power to the substrate 2a of the mounting table 2. In addition, the control unit 100 applies the direct current supplied from the variable direct current power supply 72 to the shower head 16 by turning on the on-off switch 73. As a result, plasma of the oxygen-containing gas is generated in the processing container 10.

[0117] Next, the control unit 100 determines whether a preset processing time has elapsed since the high-frequency power supply was started in step S103 (S210). If the preset processing time has not elapsed (S210: No), the process of step S210 is executed again.

[0118] On the other hand, when the set processing time has elapsed (S210: Yes), the supply of high frequency power to the mounting table 2 is stopped (S211). In addition, the supply of the reaction gas into the processing container 10 is stopped (S212). Thus, the generation of the plasma of the oxygen-containing gas in the processing container 10 is stopped.

[0119] After the reaction gas in the processing container 10 is exhausted, the edge ring 5 is placed on the second placement surface 6f by lowering the lift pins 163 (S213). At this point, the cleaning method shown in this flowchart is completed.

[0120] By cleaning the mounting table 2 and the edge ring 5 after further separating the edge ring 5 from the second mounting surface 6 f in this manner, plasma diffuses to the vicinity of the second mounting surface 6 f , and as a result, deposits deposited on the second mounting surface 6 f can be removed.

[0121] In addition, Figure 7 In the cleaning process shown, the following Figure 8 The processing of steps S221 to S223 shown in the figure replaces the processing of step S213. That is, the edge ring 5 can be replaced after the stage 2 and the edge ring 5 are cleaned. This can suppress the contamination caused by the sediment attached to the edge ring 5 being carried out to the VTM 51.

[0122] Here, when referring to Figure 6 According to the experimental results shown, when the height of the lower surface of the edge ring 5 is 6.4 mm or more and 32.4 mm or less, the etching rate of the second mounting surface 6f increases. On the other hand, when the height of the lower surface of the edge ring 5 is 6.4 mm or more and 32.4 mm or less, the etching rates at the first mounting surface 6e and the lower surface of the edge ring 5 are almost unchanged and maintained at a fixed value. According to this result, it is preferable to set the height of the lower surface of the edge ring 5 relative to the first mounting surface 6e when the edge ring 5 is separated from the second mounting surface 6f to 6.4 mm or more and 32.4 mm or less, and more preferably to 12.4 mm or more and 32.4 mm or less. By setting the height of the lower surface of the edge ring 5 within this range, the density of the plasma in the in-plane direction of the mounting table 2 can be equalized, so that the deposits deposited on the second mounting surface 6f can be efficiently removed while suppressing damage to the first mounting surface 6e and the lower surface of the edge ring 5.

[0123] In addition, in the above-mentioned cleaning process, the PM 1 can replace the edge ring 5 after stopping the generation of plasma. Figure 8 The cleaning process will be described below.

[0124] Figure 8This is a flowchart showing an example of a cleaning process according to Modification 2 of the first embodiment. The PM 1 is mainly operated under the control of the control unit 100 to achieve Figure 8 In addition, the cleaning process is performed in a state where no wafer W is contained in the processing container 10. Figure 8 In addition, Figure 8 Steps S100 to S106 and Figure 3 The steps S100 to S106 shown are the same, so their detailed description is omitted here.

[0125] When the supply of high frequency power and the supply of reaction gas are stopped to stop the generation of plasma ( S105 , S106 ), the edge ring 5 is carried out ( S221 ). That is, the edge ring 5 is carried out from the PM 1 by the transport robot 510 and returned to the storage device 52 .

[0126] In addition, after executing the processing of steps S105 and S106 and before executing step S221, the edge ring 5 may be placed on the second mounting surface 6f for a predetermined time. Thus, the edge ring 5 heated by cleaning can be cooled before the edge ring 5 is carried out in step S221. In addition, while the lifting pins 163 are raised to clean the edge ring 5, the temperature of the temperature control medium flowing in the temperature control medium flow path 2d may be controlled so that the temperature of the second mounting surface 6f is lowered. Thus, when the edge ring 5 is placed on the second mounting surface 6f, the edge ring 5 can be efficiently cooled. In addition, a heat transfer gas such as helium can be supplied between the back surface of the edge ring 5 and the second mounting surface 6f. Thus, the edge ring 5 can be cooled more efficiently.

[0127] Next, the edge ring 5 for replacement is carried into the PM 1 (S222). That is, the edge ring 5 for replacement is carried out from the storage device 52 by the transport robot 510, carried into the PM 1, and delivered to the lifting pin 163. In addition, in step S222, the edge ring 5 that has been used but has a small consumption can be carried into the PM 1.

[0128] Next, the lifting pins 163 are lowered by driving the lifting mechanism 164, so that the edge ring 5 for replacement is placed on the second placement surface 6f (step S223).

[0129] By unloading the edge ring 5 to the VTM 51 after cleaning the mounting table 2 and the edge ring 5 in this manner, it is possible to suppress contamination caused by carrying out the deposits attached to the edge ring 5 to the VTM 51 .

[0130] [other]

[0131] In the first embodiment described above, the case where the stage 2 has the first mounting surface 6e and the second mounting surface 6f is shown as an example, but the disclosed technology is not limited to this. For example, the stage 2 can also be configured to be divided into a first stage having the first mounting surface 6e and a second stage having the second mounting surface 6f. In addition, in the case where the stage 2 is configured to be divided into the first stage and the second stage, the second stage can be configured to include a substrate and an electrostatic holding disk. In this case, the electrostatic holding disk of the second stage is annular with a flat upper surface, and the upper surface constitutes the second mounting surface 6f for mounting the edge ring 5.

[0132] [Effect]

[0133] As described above, the plasma processing device involved in the first embodiment (e.g., PM 1) includes a mounting table (e.g., mounting table 2), a lifting mechanism (e.g., lifting mechanism 164), a high-frequency power supply (e.g., a first RF power supply 14a), and a control unit (e.g., control unit 100). The mounting table has a first mounting surface (e.g., a first mounting surface 6e) and a second mounting surface (e.g., a second mounting surface 6f), a substrate (e.g., a wafer W) is mounted on the first mounting surface, and a ring member (e.g., an edge ring 5) surrounding the outer periphery of the first mounting surface is mounted on the second mounting surface. The lifting mechanism lifts and lowers the ring member relative to the second mounting surface. The high-frequency power supply is connected to the mounting table. The control unit is configured to execute a cleaning method, which includes a separation process and a removal process. In the separation process, the second mounting surface is separated from the ring member using the lifting mechanism. In the process of removing, after the process of separating, plasma is generated by supplying high-frequency power to the stage from the high-frequency power supply to remove the deposits deposited on the stage and the ring member. In addition, in the process of separating, the separation distance between the second stage and the ring member is set so that the density of the plasma generated in the area between the outer edge of the first stage and the inner edge of the lower surface of the ring member is higher than the density of the plasma generated in other areas. Thus, according to the plasma processing device involved in the embodiment, it is possible to remove the deposits deposited on the outer periphery of the stage, the inner periphery of the ring member, and the lower surface of the ring member while suppressing damage to the stage.

[0134] In addition, in the separation process, the height of the lower surface of the ring member relative to the first mounting surface can be greater than 1.4 mm and less than 4.4 mm. Thus, according to the plasma processing device involved in the first embodiment, an annular plasma can be generated around the area between the outer edge of the first mounting surface of the mounting table and the inner edge of the lower surface of the ring member while protecting the first mounting surface of the mounting table from the influence of plasma.

[0135] In addition, in the separation process, the height of the lower surface of the ring member relative to the first mounting surface is preferably 1.6 mm to 3.4 mm, and more preferably 2.0 mm to 2.8 mm. Thus, according to the plasma processing apparatus involved in the first embodiment, the deposits deposited on the outer periphery of the mounting table, the inner periphery of the ring member, and the lower surface of the ring member can be reliably removed in a short time.

[0136] In addition, the cleaning method may further include a process of further separation and a process of further removal. In the process of further separation, after the process of removal, the second mounting surface and the ring member may be further separated using a lifting mechanism. In the process of further removal, after the process of further separation, plasma may be generated by supplying high-frequency power from a high-frequency power supply to the mounting table to further remove the deposits deposited on the mounting table and the ring member. Thus, according to the plasma processing device involved in the first embodiment, the plasma can diffuse to the vicinity of the second mounting surface, and as a result, the deposits deposited on the second mounting surface can be removed.

[0137] In addition, in the further separation process, the height of the lower surface of the ring member relative to the first mounting surface is preferably 6.4 mm or more and 32.4 mm or less, and more preferably 12.4 mm or more and 32.4 mm or less. Thus, according to the plasma processing device involved in the first embodiment, the density of the plasma in the plane direction of the mounting table can be equalized, so that the deposits deposited on the second mounting surface can be efficiently removed while suppressing damage to the first mounting surface and the lower surface of the edge ring.

[0138] In addition, the plasma processing apparatus according to the first embodiment may further include a processing container (e.g., processing container 10) for accommodating the mounting table. The cleaning method may be performed in a state where no substrate is accommodated in the processing container. Thus, according to the plasma processing apparatus according to the first embodiment, deposits deposited on the outer periphery of the mounting table, the inner periphery of the ring member, and the lower surface of the ring member may be efficiently removed while the first mounting surface of the mounting table is exposed.

[0139] In addition, in the removal process, a plasma containing an oxygen-containing gas (for example, O2 gas or a reaction gas in which a halogen gas is added to O2 gas) can be generated. Thus, according to the plasma processing apparatus involved in the first embodiment, carbon-based deposits deposited on the outer periphery of the mounting table, the inner periphery of the ring member, and the lower surface of the ring member can be appropriately removed.

[0140] In addition, the ring member may be an edge ring. Thus, according to the plasma processing apparatus according to the embodiment, it is possible to remove deposits deposited on the outer periphery of the mounting table, the inner periphery of the edge ring, and the lower surface of the edge ring while suppressing damage to the mounting table.

[0141] (Second Embodiment)

[0142] Next, the second embodiment will be described. The structure of the substrate processing system 50 in the second embodiment is similar to Figure 1 The structure of the substrate processing system 50 shown is the same, so its description is omitted.

[0143] [Structure of plasma processing apparatus]

[0144] Fig. 9 1 is a schematic cross-sectional view showing an example of the structure of PM 1 in Embodiment 2. PM 1 is an example of a plasma processing apparatus.

[0145] In the present embodiment, PM 1 is a capacitively coupled plasma processing apparatus. PM 1 includes a plasma processing chamber 10, a gas supply unit 20, a power supply 30, and an exhaust system 40. In addition, PM 1 includes a substrate support unit 11 and a gas inlet unit. The plasma processing chamber 10 is an example of a processing container. The gas inlet unit is configured to introduce at least one processing gas into the plasma processing chamber 10. The gas inlet unit includes a shower head 13. The substrate support unit 11 is disposed in the plasma processing chamber 10. The shower head 13 is disposed above the substrate support unit 11. In one embodiment, the shower head 13 constitutes at least a portion of the top (Ceiling) of the plasma processing chamber 10. The plasma processing chamber 10 has a plasma processing space 10s defined by the shower head 13, the side wall 10a of the plasma processing chamber 10, and the substrate support unit 11. The plasma processing chamber 10 has at least one gas supply port for supplying at least one processing gas to the plasma processing space 10s, and at least one gas exhaust port for exhausting gas from the plasma processing space. The plasma processing chamber 10 is grounded. The shower head 13 and the substrate support 11 are electrically insulated from the housing of the plasma processing chamber 10. An opening 10b for carrying the wafer W into and out of the plasma processing chamber 10 is formed on the side wall 10a of the plasma processing chamber 10. The opening 10b is opened and closed by a gate valve G1.

[0146] The substrate support portion 11 includes a main body 111 and a ring assembly 112. The main body 111 is an example of a mounting table. The main body 111 has a central area 111a for supporting a wafer W, and an annular area 111b for supporting the ring assembly 112. The central area 111a is an example of a first mounting surface, and the annular area 111b is an example of a second mounting surface. Wafer W is an example of a substrate. The annular area 111b of the main body 111 surrounds the central area 111a of the main body 111 when viewed from above. Wafer W is arranged on the central area 111a of the main body 111, and the ring assembly 112 is arranged on the annular area 111b of the main body 111 in a manner that surrounds the wafer W on the central area 111a of the main body 111. Therefore, the central area 111a is also referred to as a substrate supporting surface for supporting wafer W, and the annular area 111b is also referred to as a ring supporting surface for supporting the ring assembly 112.

[0147] In one embodiment, the main body 111 includes a base 1110 and an electrostatic holding disk 1111. The base 1110 includes a conductive component. The conductive component of the base 1110 can function as a lower electrode. The electrostatic holding disk 1111 is arranged on the base 1110. The electrostatic holding disk 1111 includes a ceramic component 1111a and a first electrode 1111b arranged in the ceramic component 1111a. The ceramic component 1111a has a central area 111a. In one embodiment, the ceramic component 1111a also has an annular area 111b. In addition, other components surrounding the electrostatic holding disk 1111, such as an annular electrostatic holding disk or an annular insulating component, may also have an annular area 111b. In this case, the ring assembly 112 may be arranged on the annular electrostatic holding disk or the annular insulating component, or on both the electrostatic holding disk 1111 and the annular insulating component. In addition, at least one RF / DC electrode coupled to the RF (Radio Frequency) power supply 31 and / or the DC (Direct Current) power supply 32 described later may be configured in the ceramic component 1111a. In this case, at least one RF / DC electrode functions as a lower electrode. In the case where a bias RF signal and / or a DC signal described later is provided to at least one RF / DC electrode, the RF / DC electrode is also referred to as a bias electrode. In addition, the conductive component of the base 1110 and at least one RF / DC electrode may function as a plurality of lower electrodes. In addition, the first electrode 1111b may function as a lower electrode. Thus, the substrate support portion 11 includes at least one lower electrode.

[0148] The ring assembly 112 includes one or more ring-shaped members. In one embodiment, the one or more ring-shaped members include one or more edge rings and at least one cover ring. The edge ring is formed of a conductive material or an insulating material, and the cover ring is formed of an insulating material.

[0149] In addition, the substrate support portion 11 may include a temperature control module configured to adjust at least one of the electrostatic holding disk 1111, the ring assembly 112, and the substrate to a target temperature. The temperature control module may include a heater, a heat transfer medium, a flow path 1110a, or a combination thereof. A heat transfer fluid such as brine or gas flows through the flow path 1110a. In one embodiment, the flow path 1110a is formed in the base 1110, and one or more heaters are arranged in the ceramic component 1111a of the electrostatic holding disk 1111. In addition, the substrate support portion 11 may include a heat transfer gas supply portion configured to supply a heat transfer gas to the gap between the back side of the wafer W and the central area 111a. In addition, the substrate support portion 11 includes a heat transfer gas supply portion configured to supply a heat transfer gas to the gap between the back side of the edge ring and the annular area 111b, but in Figure 2 In addition, a plurality of lifting pins are provided on the substrate support portion 11, but Figure 2 Omitted in .

[0150] The showerhead 13 is configured to introduce at least one processing gas from the gas supply unit 20 into the plasma processing space 10s. The showerhead 13 has at least one gas supply port 13a, at least one gas diffusion chamber 13b, and a plurality of gas introduction ports 13c. The processing gas supplied to the gas supply port 13a passes through the gas diffusion chamber 13b and is introduced into the plasma processing space 10s from the plurality of gas introduction ports 13c. In addition, the showerhead 13 includes at least one upper electrode. In addition, the gas introduction unit may include one or more side gas injection units (SGI: Side Gas Injector) in addition to the showerhead 13, and the one or more side gas injection units are installed in one or more openings formed in the side wall 10a.

[0151] The gas supply unit 20 may include at least one gas source 21 and at least one flow controller 22. In one embodiment, the gas supply unit 20 is configured to supply at least one process gas from the respective gas sources 21 to the shower head 13 via the respective flow controllers 22. Each flow controller 22 may include, for example, a mass flow controller or a pressure-controlled flow controller. In addition, the gas supply unit 20 may include one or more flow modulation devices for modulating or pulsing the flow of at least one process gas.

[0152] The power supply 30 includes an RF power supply 31 coupled to the plasma processing chamber 10 via at least one impedance matching circuit. The RF power supply 31 is configured to provide at least one RF signal (RF power) to at least one lower electrode and / or at least one upper electrode. Thus, plasma is formed from at least one processing gas supplied to the plasma processing space 10s. Therefore, the RF power supply 31 can function as at least a part of a plasma generating unit configured to generate plasma from one or more processing gases in the plasma processing chamber 10. In addition, by providing a bias RF signal to at least one lower electrode, a bias potential can be generated on the wafer W to attract ion components in the formed plasma to the wafer W.

[0153] In one embodiment, the RF power supply 31 includes a first RF generating unit 31a and a second RF generating unit 31b. The first RF generating unit 31a is configured to be coupled to at least one lower electrode and / or at least one upper electrode via at least one impedance matching circuit, and to generate a source RF signal (source RF power) for generating plasma. In one embodiment, the source RF signal has a frequency in the range of 10 MHz to 150 MHz. In one embodiment, the first RF generating unit 31a may be configured to generate a plurality of source RF signals having different frequencies. The generated one or more source RF signals are provided to at least one lower electrode and / or at least one upper electrode.

[0154] The second RF generating unit 31b is configured to be coupled to at least one lower electrode via at least one impedance matching circuit and generate a bias RF signal (bias RF power). The frequency of the bias RF signal may be the same as or different from the frequency of the source RF signal. In one embodiment, the bias RF signal has a frequency lower than the frequency of the source RF signal. In one embodiment, the bias RF signal has a frequency in the range of 100kHz to 60MHz. In one embodiment, the second RF generating unit 31b may also be configured to generate a plurality of bias RF signals having different frequencies. The generated one or more bias RF signals are provided to at least one lower electrode. In addition, in various embodiments, at least one of the source RF signal and the bias RF signal may also be pulsed.

[0155] In addition, the power supply 30 may include a DC power supply 32 coupled to the plasma processing chamber 10. The DC power supply 32 includes a first DC generating unit 32a and a second DC generating unit 32b. In one embodiment, the first DC generating unit 32a is configured to be connected to at least one lower electrode and generate a first DC signal. The generated first bias DC signal is applied to at least one lower electrode. In one embodiment, the second DC generating unit 32b is configured to be connected to at least one upper electrode and generate a second DC signal. The generated second DC signal is applied to at least one upper electrode.

[0156] In various embodiments, at least one of the first DC signal and the second DC signal may also be pulsed. In this case, a sequence of voltage pulses is applied to at least one lower electrode and / or at least one upper electrode. The voltage pulse may have a rectangular, trapezoidal, triangular, or a pulse waveform of a combination of these shapes. In one embodiment, a waveform generator for generating a sequence of voltage pulses from a DC signal is connected between the first DC generator 32a and at least one lower electrode. Thus, the first DC generator 32a and the waveform generator constitute a voltage pulse generator. In the case where the second DC generator 32b and the waveform generator constitute a voltage pulse generator, the voltage pulse generator is connected to at least one upper electrode. The voltage pulse may have a positive polarity or a negative polarity. In addition, the sequence of voltage pulses may include one or more positive polarity voltage pulses and one or more negative polarity voltage pulses in one cycle. In addition, the first DC generator 32a and the second DC generator 32b may be provided in addition to the RF power supply 31, or the first DC generator 32a may be provided to replace the second RF generator 31b.

[0157] The exhaust system 40 can be connected to a gas outlet 10e, for example, provided at the bottom of the plasma processing chamber 10. The exhaust system 40 can include a pressure regulating valve and a vacuum pump. The pressure in the plasma processing space 10s is adjusted by the pressure regulating valve. The vacuum pump can include a turbomolecular pump, a dry pump, or a combination thereof.

[0158] Fig.101 is an enlarged cross-sectional view showing an example of a structure near the edge of the electrostatic holding disk 1111. The base 1110 is supported by an insulating member 1110b formed in an annular shape. The ring assembly 112 has an edge ring ER and a cover ring CR. The edge ring ER has an inner portion ER-1 and an outer portion ER-2, and the thickness of the inner portion ER-1 is thinner than the thickness of the outer portion ER-2. The inner portion ER-1 of the edge ring ER and a part of the outer portion ER-2 are arranged on the annular area 111b. In addition, the outer peripheral portion of the outer portion ER-2 of the edge ring ER overlaps with the inner peripheral portion of the cover ring CR when viewed from above. The edge ring ER is formed of a conductive material such as silicon or carbon. The cover ring CR is arranged on the insulating member 1110b. The cover ring CR is formed of an insulating material such as quartz, and is used to protect the upper surface of the insulating member 1110b from the influence of plasma. In addition, the edge ring ER can be an insulating material such as quartz. In addition, the cover ring CR can also be a conductive material such as silicon or silicon carbide.

[0159] In the electrostatic holding disk 1111, a first electrode 1111b is buried under the central region 111a, and a second electrode 1111c is buried under the annular region 111b. The first electrode 1111b electrostatically adsorbs the wafer W or the wafer dummy to the central region 111a by generating an electrostatic force corresponding to the applied voltage. The second electrode 1111c electrostatically adsorbs the edge ring ER to the annular region 111b by generating an electrostatic force corresponding to the applied voltage. Fig.10 In the example, the first electrode 1111b is a monopolar electrode, but as another example, the first electrode 1111b may be a bipolar electrode. Fig.10 In the example, the second electrode 1111c is a bipolar electrode, but as another example, the second electrode 1111c may be a monopolar electrode.

[0160] Below the central region 111a, a through hole H1 is formed in the electrostatic holding disk 1111, and a through hole H2 is formed in the base 1110. The lifting pins 60 are inserted into the through holes H1 and H2. The lifting pins 60 are lifted and lowered by the lifting mechanism 62. The lifting pins 60 are lifted and lowered, thereby enabling the wafer W or the wafer dummy placed on the central region 111a to be lifted and lowered. In this embodiment, three lifting pins 60 are provided in the central region 111a.

[0161] Below the region where the edge ring ER overlaps the cover ring CR when viewed from above, a through hole H3 is formed in the cover ring CR, a through hole H4 is formed in the insulating member 1110b, and a through hole H5 is formed in the base 1110. The lift pins 61 are inserted into the through holes H3 to H5. The lift pins 61 are lifted and lowered by the lifting mechanism 63. The lift pins 61 are lifted and lowered, thereby enabling the edge ring ER on the cover ring CR to be lifted and lowered. In the present embodiment, three lift pins 61 are provided in the annular region 111b. In addition, a recess ERr is formed on the lower surface of the edge ring ER corresponding to the position of the through hole H3, and as the lift pins 61 are lifted, the front end 61a of the lift pin 61 abuts against the recess ERr. Thus, the lift pins 61 can stably support the edge ring ER through the front end 61a.

[0162] Below the annular region 111b, a gas supply pipe 70 is provided between the electrostatic holding disk 1111 and the base 1110 in such a manner as to penetrate the electrostatic holding disk 1111 and the base 1110. The gas supply pipe 70 is connected to a gas supply source (not shown) and is used to supply a heat transfer gas such as helium to the gap between the back side of the edge ring ER and the annular region 111b. The gas supply pipe 70 is an example of a heat transfer gas supply unit. The gas supply pipe 70 can also be connected to other gas supply sources (not shown) via a branch pipe (not shown) to supply a cleaning gas instead of a heat transfer gas to the gap between the back side of the edge ring ER and the annular region 111b.

[0163] [An Example of a Cleaning Process Flow According to the Second Embodiment]

[0164] Next, refer to Fig.11 The flow of the cleaning process performed by the PM 1 according to the second embodiment will be described. Fig.11 The control unit 9 controls each part of the substrate processing system 50 to achieve Fig.11 In addition, the steps are performed in a state where no wafer W is accommodated in the plasma processing chamber 10. Fig.11 Illustrated cleaning process.

[0165] First, the control unit 9 determines whether it is time to perform the cleaning process (S230). As the timing for performing the cleaning process, for example, the timing for performing the plasma etching process of a predetermined number of wafers W is listed. If it is not time to perform the cleaning process (S230: No), the process of step S230 is performed again.

[0166] When the timing for executing the cleaning process has come (S230: YES), the application of voltage to the second electrode 1111c is stopped, thereby releasing the electrostatic attraction of the edge ring ER to the annular region 111b (S231).

[0167] Next, the lifting pins 61 are lifted (raised) by driving the lifting mechanism 63, thereby separating the edge ring ER from the annular region 111b (S232). Information on the separation distance between the edge ring ER and the annular region 111b is pre-stored in the storage unit 9a2, for example, and the control unit 9 raises the lifting pins 61 based on the information stored in the storage unit 9a2.

[0168] Next, after the interior of plasma processing chamber 10 is depressurized to a predetermined vacuum level by exhaust system 40 , reaction gas (cleaning gas) is supplied from gas supply unit 20 into plasma processing chamber 10 ( S233 ).

[0169] The cleaning gas supplied into the plasma processing chamber 10 in step S233 includes, for example, a cleaning gas containing at least one gas selected from the group consisting of O2 gas, O3 gas, CO gas, CO2 gas, COS gas, N2 gas, and H2 gas. In addition, the cleaning gas may further contain a halogen-containing gas such as CF4 gas, NF3 gas, SF6 gas, Cl2 gas, or HBr gas.

[0170] In step S233, a cleaning gas may be supplied from the gas supply unit 20 to the plasma processing chamber 10, and a cleaning gas may be supplied from the gas supply pipe 70 to the plasma processing chamber 10 instead of the heat transfer gas. As a result, the plasma concentration above the annular region 111b becomes high, and the deposits deposited on the outer periphery of the electrostatic holding disk 1111, the inner periphery of the edge ring ER, and the lower surface of the edge ring ER can be removed efficiently. In addition, the deposits attached to the inside of the gas supply pipe 70 can also be removed.

[0171] In addition, the cleaning gas supplied from the gas supply pipe 70 to the plasma processing chamber 10 may also contain halogen-containing gases such as CF4 gas, NF3 gas, SF6 gas, Cl2 gas or HBr gas. As a result, the plasma concentration above the annular region 111b becomes higher, and the silicon-containing and metal-containing deposits can be removed efficiently. In addition, the silicon-containing and metal-containing deposits attached to the inside of the gas supply pipe 70 can also be removed.

[0172] Next, high frequency power is supplied to the base 1110 as the lower electrode (S234). In step S234, the control unit 9 controls the RF power supply 31 to generate high frequency power, thereby supplying high frequency power to the conductive member of the base 1110. In addition, the control unit 9 controls the DC power supply 32 to apply direct current power to the shower head 13. Thus, plasma of the cleaning gas is generated in the plasma processing chamber 10, and cleaning in the plasma processing chamber 10 is performed by the plasma generated from the cleaning gas.

[0173] Next, the control unit 9 determines whether a preset processing time (cleaning time) has passed since the high-frequency power supply started in step S234 (S235). If the preset processing time has not passed (S235: No), the process of step S235 is executed again.

[0174] On the other hand, when the set processing time has passed (S235: Yes), the supply of high frequency power to the base 1110 is stopped (S236). In addition, the supply of the reaction gas (cleaning gas) into the plasma processing chamber 10 is stopped (S237). Thus, the generation of the plasma of the cleaning gas in the plasma processing chamber 10 is stopped.

[0175] After the reaction gas in the plasma processing chamber 10 is exhausted, the lifting pins 61 are lowered by driving the lifting mechanism 63 , thereby placing the edge ring ER on the annular region 111 b .

[0176] Next, the edge ring ER is electrostatically adsorbed to the annular region 111b (step S239). In step S239, the edge ring ER is adsorbed and held to the annular region 111b by the electrostatic force generated in accordance with the voltage applied to the second electrode 1111c. The cleaning method shown in this flowchart is now completed.

[0177] In the above steps S232 to S237, the density of the plasma generated in the region between the outer edge of the central region 111a and the inner edge of the lower surface of the edge ring ER is set higher than the density of the plasma generated in other regions. Thus, the deposits deposited on the outer periphery of the main body 111, the inner periphery of the edge ring ER, and the lower surface of the edge ring ER can be removed efficiently while suppressing damage to the main body 111.

[0178] In addition, in the above-mentioned steps S232 to S237, the cleaning can be performed while the height position of the edge ring ER is maintained so that the lower surface of the edge ring ER is higher than the upper surface of the cover ring CR. Thus, the deposits volatilized by the plasma can be smoothly exhausted from the gap between the edge ring ER and the cover ring CR, thereby improving the removal efficiency of the deposits.

[0179] [Modification of the Second Embodiment]

[0180] In the above cleaning process, PM 1 can replace the edge ring ER after stopping the generation of plasma. Fig.12 The cleaning process will be described below.

[0181] Fig.12This is a flowchart showing an example of the flow of the cleaning process according to the modification 1 of the second embodiment. The PM 1 is mainly operated under the control of the control unit 9 to achieve Fig.12 The cleaning process is performed in the plasma processing chamber 10 without accommodating the wafer W. Fig.12 In addition, Fig.12 Steps S230 to S237 and Fig.11 The steps S230 to S237 shown are the same, so detailed description is omitted here.

[0182] When the supply of high frequency power and the supply of reaction gas are stopped to stop the generation of plasma ( S236 , S237 ), the edge ring ER is carried out ( S241 ). That is, the edge ring ER is carried out from the PM 1 by the transport robot 510 and returned to the storage device 52 .

[0183] In addition, after executing the processing of steps S236 and S237 and before executing step S241, the edge ring ER may be placed in the annular region 111b for a predetermined time. Thus, the edge ring ER heated by cleaning can be cooled before the edge ring ER is carried out in step S241. In addition, during the period when the lifting pins 61 are raised to clean the edge ring ER, the temperature control module included in the substrate support part 11 may be controlled so that the temperature of the annular region 111b is lowered. Thus, when the edge ring ER is placed in the annular region 111b, the edge ring ER can be efficiently cooled. In addition, when the edge ring ER is placed in the annular region 111b after executing the processing of steps S236 and S237, the pressure of the heat transfer gas supplied between the back surface of the edge ring ER and the annular region 111b may be increased. Thus, the edge ring ER can be cooled more efficiently.

[0184] Next, the edge ring ER for replacement is carried into the PM 1 (S242). That is, the edge ring ER for replacement is carried out from the storage device 52 by the transport robot 510, carried into the PM 1, and delivered to the lifting pin 61. In addition, in step S242, the edge ring ER that has been used but has a small consumption can be carried into the PM 1.

[0185] Next, the lifting pins 61 are lowered by driving the lifting mechanism 63, thereby placing the edge ring ER for replacement on the annular region 111b and electrostatically adsorbing it to the annular region 111b (step S243). That is, the edge ring ER is adsorbed and held on the annular region 111b by the electrostatic force generated in accordance with the voltage applied to the second electrode 1111c.

[0186] As described above, in Modification 1, by replacing the edge ring ER after cleaning the stage and the edge ring ER, contamination of the replaced edge ring ER can be suppressed. In addition, in Modification 1, by unloading the edge ring ER to the VTM 51 after cleaning the stage and the edge ring ER, contamination caused by carrying sediment attached to the edge ring ER to the VTM 51 can be suppressed.

[0187] Fig.13 This is a flowchart showing an example of a cleaning process according to Modification 2 of the second embodiment. The PM 1 is mainly operated under the control of the control unit 9 to achieve Fig.13 The cleaning process is performed in the plasma processing chamber 10 without accommodating the wafer W. Fig.13 In addition, Fig.13 Steps S230 to S239 and Fig.11 The steps S230 to S239 shown are the same, so their detailed description is omitted here.

[0188] exist Fig.13 In the cleaning process shown, when the timing for performing the cleaning process has arrived (S230: "Yes"), cleaning (S301) is performed in the plasma processing chamber 10 before performing the cleaning of steps S231 to S239. In step S301, cleaning is performed in the plasma processing chamber 10 in a state where no wafer W is placed in the central area 111a. In step S301, a reaction gas (cleaning gas) is supplied from the gas supply unit 20 into the plasma processing chamber 10, and high-frequency power is supplied to the base 1110. Thus, in step S301, plasma of the cleaning gas is generated in the plasma processing chamber 10, and cleaning is performed in the plasma processing chamber 10 by the plasma generated from the cleaning gas.

[0189] The cleaning gas supplied into the plasma processing chamber 10 in step S301 may be the same as or different from the cleaning gas supplied into the plasma processing chamber 10 in step S233. The cleaning performed in step S301 is an example of the first cleaning.

[0190] When the cleaning of step S301 is completed, the cleaning of steps S231 to S239 is performed. The cleaning performed in steps S231 to S239 is an example of the second cleaning.

[0191] As described above, in Modification 2, cleaning of the plasma processing chamber 10 is performed before the cleaning of steps S231 to S239. Thus, the deposits deposited on the outer periphery of the electrostatic holding disk 1111, the inner periphery of the edge ring ER, and the lower surface of the edge ring ER can be removed more efficiently while suppressing damage to the electrostatic holding disk 1111.

[0192] In addition, Fig.13 The cleaning process shown can be Figure 8 The processing of steps S221 to S223 replaces the processing of steps S238 and S239, and after the processing of step S223, the edge ring ER for replacement is electrostatically adsorbed to the annular region 111b.

[0193] In addition, step S301 and step S231 may be performed at the same time. That is, the electrostatic adsorption of the edge ring ER to the annular region 111b may be released while the plasma processing chamber 10 is being cleaned in a state where no wafer W is placed on the central region 111a. In this case, for example, the second electrode 1111c (see FIG. 14 ) may be simultaneously cleaned while the plasma processing chamber 10 is being cleaned. Fig.10 ) applies a voltage having a polarity opposite to that of the voltage used for electrostatic attraction to release the electrostatic attraction of the edge ring ER relative to the annular region 111b.

[0194] Fig.14 This is a flowchart showing an example of a cleaning process according to Modification 3 of the second embodiment. The PM 1 is mainly operated under the control of the control unit 9 to achieve Fig.14 In addition, Fig.14 Steps S230 to S239 and Fig.11 Steps S230 to S239 are the same as those shown in the figure, so their detailed description is omitted here. Fig.14 Step S301 and Fig.13 The step S301 shown is the same, so its detailed description is omitted here.

[0195] exist Fig.14In the cleaning process shown, when the cleaning of step S301 is completed, the dummy wafer is moved into the plasma processing chamber 10 (S302). In step S302, the gate valve G4 is opened, and the dummy wafer is moved out of the storage device 52 by the transfer robot 510. Then, the gate valve G1 is opened, the dummy wafer is moved into PM 1, and handed over to the lifting pin 60. Moreover, the lifting pin 60 is lowered by the driving of the lifting mechanism 62, thereby placing the dummy wafer on the central area 111a of the electrostatic holding disk 1111. Here, the diameter of the dummy wafer placed in the central area 111a in step S302 is smaller than the inner diameter of the edge ring ER. Therefore, even when the dummy wafer is placed in the central area 111a, the edge ring ER can be separated from the annular area 111b without causing interference between the dummy wafer and the edge ring ER.

[0196] Next, the dummy wafer is electrostatically attached to the central region 111a (S303). Then, the cleaning (second cleaning) of steps S231 to S239 is performed. In steps S231 to S239, the plasma processing chamber 10 is cleaned with the dummy wafer placed on the central region 111a.

[0197] In addition, the processing conditions in the cleaning of steps S231 to S239 may be changed by at least one parameter relative to the processing conditions in the cleaning of step S301. The processing conditions in the cleaning of steps S231 to S239 and the cleaning of step S301 include, for example, at least one parameter selected from the group consisting of gas species, gas flow ratio, gas flow rate, pressure, bias power, plasma generation power, temperature of the electrostatic holding disk 1111, and cleaning time.

[0198] Here, in steps S231 to S239, it is preferable to perform cleaning under conditions with higher cleaning performance than that performed in step S301. Thus, the deposits attached to the edge ring ER after use can be sufficiently removed, so that the deposits can be suppressed from falling during the conveyance of the edge ring ER after use. For example, the plasma generation power supplied to the upper electrode and / or the lower electrode in the cleaning in steps S231 to S239 can be greater than the plasma generation power supplied in the first cleaning. In addition, the cleaning in steps S231 to S239 can be performed with a bias power greater than that in the cleaning in step S301. Alternatively, the bias power may not be supplied in the cleaning in step S301, and the bias power may be supplied in the cleaning in steps S231 to S239. In addition, the cleaning in steps S231 to S239 can be performed with a higher pressure than that in the cleaning in step S301. In addition, the cleaning in steps S231 to S239 can be performed with a higher pressure and a larger bias power than that in the cleaning in step S301. In addition, the temperature of the electrostatic holding disk 1111 in the cleaning of steps S231 to S239 may be higher than the temperature of the electrostatic holding disk 1111 in the cleaning of step S301. For example, the temperature of the electrostatic holding disk 1111 may be controlled by controlling the temperature of the temperature regulating medium (heat transfer fluid) flowing in the flow path 1110a and / or controlling the heater not shown in the electrostatic holding disk 1111. In addition, the temperature control of the electrostatic holding disk 1111 may be started after the end of step S301. In addition, the cleaning in steps S231 to S239 may be performed for a longer time than the cleaning in step S301. In addition, in steps S231 to S239, a gas (e.g., a halogen-containing gas) having a stronger corrosiveness than the gas used in the cleaning performed in step S301 may be used for cleaning. In addition, a gas (e.g., a halogen-containing gas) having a stronger corrosiveness may also be used in the cleaning in step S301. In this case, the flow rate of the highly corrosive gas in the cleaning of steps S231 to S239 may be greater than the flow rate of the highly corrosive gas in the cleaning of step S301 .

[0199] As described above, in Modification 3, cleaning of the plasma processing chamber 10 is performed before the cleaning of steps S231 to S239. Thus, the deposits deposited on the outer periphery of the electrostatic holding disk 1111, the inner periphery of the edge ring ER, and the lower surface of the edge ring ER can be removed more efficiently while suppressing damage to the electrostatic holding disk 1111.

[0200] In Modification 3, the cleaning of steps S231 to S239 is performed with a dummy wafer placed on central region 111a. Thus, even when the plasma processing chamber 10 is cleaned under high cleaning performance conditions, damage to central region 111a can be reduced.

[0201] In addition, Fig.14 The cleaning process shown can be Figure 8 The processing of steps S221 to S223 replaces the processing of steps S238 and S239, and after the processing of step S223, the edge ring ER for replacement is electrostatically adsorbed to the annular region 111b.

[0202] In addition, step S303 and step S231 may be executed at the same timing. That is, the electrostatic adsorption of the edge ring ER relative to the annular region 111b may be released in parallel when the dummy wafer is electrostatically adsorbed to the central region 111a. In this case, for example, after the dummy wafer is placed in the central region 111a, nitrogen, oxygen or other gas may be supplied to the plasma processing chamber 10 and controlled to a predetermined pressure, and the first electrode 1111b (see FIG. 1 ) may be electrically adsorbed to the central region 111a by supplying high frequency power to the plasma processing chamber 10 to generate plasma. Fig.10 ) to electrostatically adsorb the dummy wafer to the central region 111a, and apply a voltage having a polarity opposite to that of the voltage used for electrostatic adsorption to the second electrode 1111c to release the electrostatic adsorption of the edge ring ER relative to the annular region 111b. In addition, although plasma is generated, the electrostatic adsorption of the dummy wafer and the release of the electrostatic adsorption of the edge ring may be performed in a state where an inert gas (nitrogen, etc.) is supplied into the plasma processing chamber 10 and controlled to a predetermined pressure (without generating plasma).

[0203] Fig.15 This is a flowchart showing an example of the flow of the cleaning process according to the modification 4 of the second embodiment. The PM 1 is mainly operated according to the control of the control unit 9 to achieve Fig.15 In addition, Fig.15 Steps S230 to S239 and Fig.11 Steps S230 to S239 are the same as those shown in the figure, so their detailed description is omitted here. Fig.15 Steps S301 to S303 and Fig.14 The steps S301 to S303 shown are the same, so their detailed description is omitted here.

[0204] exist Fig.15In the cleaning process shown, when the dummy wafer is electrostatically adsorbed on the central area 111a (S303), cleaning (S304) is performed in the plasma processing chamber 10. In step S304, cleaning is performed in the plasma processing chamber 10 in a state where the dummy wafer is placed on the central area 111a. Here, the diameter of the dummy wafer placed on the central area 111a can be the same as the diameter of the wafer W, or it can be smaller than the diameter of the wafer W and the inner diameter of the edge ring ER. In step S304, a reaction gas (cleaning gas) is supplied from the gas supply unit 20 into the plasma processing chamber 10, and high-frequency power is supplied to the base 1110. Thus, in step S304, plasma of the cleaning gas is generated in the plasma processing chamber 10, and cleaning of the plasma processing chamber 10 is performed by the plasma generated from the cleaning gas.

[0205] The cleaning gas supplied into the plasma processing chamber 10 in step S304 may be the same as or different from the cleaning gas supplied into the plasma processing chamber 10 in step S233. The cleaning performed in step S304 is an example of the first cleaning.

[0206] When the cleaning of step S304 is completed, the dummy wafer is unloaded (S305). In step S305, the lifting pins 60 are raised by driving the lifting mechanism 62, thereby lifting the dummy wafer. Then, the gate valve G1 is opened, and the dummy wafer is unloaded from PM 1 by the transfer robot 510.

[0207] Next, cleaning of steps S231 to S239 is performed. The cleaning performed in steps S231 to S239 is an example of the second cleaning.

[0208] As described above, in Modification 4, cleaning of the plasma processing chamber 10 is performed before the cleaning of steps S231 to S239. Thus, the deposits deposited on the outer periphery of the electrostatic holding disk 1111, the inner periphery of the edge ring ER, and the lower surface of the edge ring ER can be removed more efficiently while suppressing damage to the electrostatic holding disk 1111.

[0209] In addition, Fig.15 The cleaning process shown can be Figure 8 The processing of steps S221 to S223 replaces the processing of steps S238 and S239, and after the processing of step S223, the edge ring ER for replacement is electrostatically adsorbed to the annular region 111b.

[0210] Fig.16 This is a flowchart showing an example of the flow of the cleaning process according to the modification 5 of the second embodiment. The PM 1 is mainly operated under the control of the control unit 9 to achieve Fig.16In addition, Fig.16 Steps S230 to S239 and Fig.11 Steps S230 to S239 are the same as those shown in the figure, so their detailed description is omitted here. Fig.16 Steps S301 to S302 and Fig.15 The steps S301 to S302 shown are the same, so their detailed description is omitted here.

[0211] exist Fig.16 In the cleaning process shown, after the dummy wafer is moved into the plasma processing chamber 10 (S302), the following process is performed. That is, the lifting pins 60 are raised (lifting pins) by driving the lifting mechanism 62, thereby keeping the dummy wafer at a position separated from the central area 111a by a predetermined distance (for example, 1 to 5 mm) (S312). The information of the separation distance between the dummy wafer and the central area 111a is pre-stored in the storage unit 9a2, for example, and the control unit 9 raises the lifting pins 60 according to the information stored in the storage unit 9a2.

[0212] Next, cleaning of the plasma processing chamber 10 is performed (S313). In step S313, cleaning of the plasma processing chamber 10 is performed in a state where the wafer dummy is separated from the central area 111a. In step S313, a reaction gas (cleaning gas) is supplied from the gas supply unit 20 into the plasma processing chamber 10, and high-frequency power is supplied to the base 1110. Thus, in step S313, plasma of the cleaning gas is generated in the plasma processing chamber 10, and cleaning of the plasma processing chamber 10 is performed by the plasma generated from the cleaning gas. The cleaning performed in step S313 is an example of the third cleaning.

[0213] The cleaning gas supplied into the plasma processing chamber 10 in step S313 may be the same as or different from the cleaning gas supplied into the plasma processing chamber 10 in step S233 .

[0214] When the cleaning of step S313 is completed, the dummy wafer is removed (S314). In step S314, the lifting pins 60 are raised by driving the lifting mechanism 62, thereby lifting the dummy wafer. Then, the gate valve G1 is opened, and the dummy wafer is removed from PM 1 by the transfer robot 510.

[0215] In addition, after performing the cleaning of step S313 and before the dummy wafer is moved out by step S314, the dummy wafer may also be placed in the central area 111a for a predetermined time. Thus, the dummy wafer heated by cleaning can be cooled before the dummy wafer is moved out by step S314. In addition, during the period when the lifting pins 60 are raised to clean the plasma processing chamber 10, the temperature control module included in the substrate support 11 may also be controlled to reduce the temperature of the central area 111a. Thus, when the dummy wafer is placed in the central area 111a, the dummy wafer can be efficiently cooled. In addition, when the dummy wafer is placed in the central area 111a after performing the cleaning of step S313, the pressure of the heat transfer gas supplied between the back of the dummy wafer and the central area 111a may also be increased. Thus, the dummy wafer can be cooled more efficiently.

[0216] Next, cleaning of steps S231 to S239 is performed. The cleaning performed in steps S231 to S239 is an example of the second cleaning.

[0217] Thus, in the fifth modification, the cleaning of the plasma processing chamber 10 is performed before the cleaning of steps S231 to S239. Thus, the connection surface 111c (see FIG. 11A ) deposited on the substrate mounting surface (central region 111a) and the ring mounting surface (annular region 111b) can be cleaned while suppressing damage to the electrostatic holding disk 1111. Fig.10 ), the inner periphery of the edge ring ER and the deposits on the lower surface of the edge ring ER are more effectively removed.

[0218] In Modification 5, cleaning in the plasma processing chamber 10 is performed in a state where the dummy wafer is separated from the central region 111a. Thus, deposits deposited on the connection surface between the substrate mounting surface and the ring mounting surface can be efficiently removed.

[0219] In addition, Fig.16 The cleaning process shown can be Figure 8 The processing of steps S221 to S223 replaces the processing of steps S238 and S239, and after the processing of step S223, the edge ring ER for replacement is electrostatically adsorbed to the annular region 111b.

[0220] Fig.17 This is a flowchart showing an example of the flow of the cleaning process according to the modification 6 of the second embodiment. The PM 1 is mainly operated under the control of the control unit 9 to achieve Fig.17 In addition, Fig.17 Steps S230 to S239 and Fig.11 Steps S230 to S239 are the same as those shown in the figure, so their detailed description is omitted here. Fig.17Step S301 and Fig.13 The step S301 shown is the same, so its detailed description is omitted here.

[0221] exist Fig.17 In the cleaning process shown, when the timing for performing the cleaning process is reached (S230: "Yes"), a dummy wafer is moved into the plasma processing chamber 10 (S321). In step S321, the gate valve G4 is opened, and the dummy wafer is moved out of the storage device 52 by the transfer robot 510. Then, the gate valve G1 is opened, the dummy wafer is moved into PM 1, and is handed over to the lifting pin 60. Then, the lifting pin 60 is lowered by driving the lifting mechanism 62, thereby placing the dummy wafer on the central area 111a of the electrostatic holding disk 1111. Here, in step S321, the diameter of the dummy wafer placed in the central area 111a is the same as the diameter of the wafer W, which is larger than the inner diameter of the edge ring ER.

[0222] Next, the dummy wafer is electrostatically adsorbed on the central area 111a (S322). Then, the plasma processing chamber 10 is cleaned (S323). In step S323, the plasma processing chamber 10 is cleaned with the dummy wafer placed on the central area 111a. In step S323, a reaction gas (cleaning gas) is supplied from the gas supply unit 20 to the plasma processing chamber 10, and high-frequency power is supplied to the base 1110. Thus, in step S323, a plasma of the cleaning gas is generated in the plasma processing chamber 10, and the plasma processing chamber 10 is cleaned by the plasma generated from the cleaning gas.

[0223] The cleaning gas supplied into the plasma processing chamber 10 in step S323 may be the same as or different from the cleaning gas supplied into the plasma processing chamber 10 in step S233. The cleaning performed in step S323 is an example of the first cleaning.

[0224] When the cleaning of step S323 is completed, the electrostatic adsorption of the dummy wafer relative to the central region 111 a is released by stopping the application of voltage to the first electrode 1111 b ( S324 ).

[0225] Next, the dummy wafer is unloaded ( S325 ). In step S325 , the lifting pins 60 are raised by driving the lifting mechanism 62 , thereby lifting the dummy wafer. Then, the gate valve G1 is opened, and the transfer robot 510 unloads the dummy wafer from PM 1 .

[0226] Next, cleaning is performed in step S301. The cleaning performed in step S301 is an example of the first cleaning.

[0227] When the cleaning of step S301 is completed, the cleaning of steps S231 to S239 is performed. The cleaning performed in steps S231 to S239 is an example of the second cleaning.

[0228] As described above, in Modification 6, cleaning of the plasma processing chamber 10 is performed before the cleaning of steps S231 to S239. Thus, the deposits deposited on the outer periphery of the electrostatic holding disk 1111, the inner periphery of the edge ring ER, and the lower surface of the edge ring ER can be removed more efficiently while suppressing damage to the electrostatic holding disk 1111.

[0229] In addition, Fig.17 The cleaning process shown can be Figure 8 The processing of steps S221 to S223 replaces the processing of steps S238 and S239, and after the processing of step S223, the edge ring ER for replacement is electrostatically adsorbed to the annular region 111b.

[0230] Fig.18 This is a flowchart showing an example of a cleaning process according to Modification 7 of the second embodiment. The PM 1 is mainly operated under the control of the control unit 9 to achieve Fig.18 In addition, Fig.18 Steps S230 to S239 and Fig.11 Steps S230 to S239 are the same as those shown in the figure, so their detailed description is omitted here. Fig.18 Step S301 and Fig.13 The step S301 shown in FIG. 1 is the same as the step S301 shown in FIG. 1 , so the detailed description thereof is omitted here. Fig.18 Steps S321 to S325 and Fig.17 The steps S321 to S325 shown are the same, so their detailed description is omitted here.

[0231] exist Fig.18 In the cleaning process shown, when the cleaning of step S301 is completed, the dummy wafer is moved into the plasma processing chamber 10 (S331). In step S331, the gate valve G4 is opened, and the dummy wafer is moved out of the storage device 52 by the transfer robot 510. Then, the gate valve G1 is opened, the dummy wafer is moved into PM 1, and handed over to the lifting pin 60. Then, the lifting pin 60 is lowered by driving the lifting mechanism 62, thereby placing the dummy wafer on the central area 111a of the electrostatic holding disk 1111. Here, in step S331, the diameter of the dummy wafer placed in the central area 111a is smaller than the inner diameter of the edge ring ER. Therefore, even when the dummy wafer is placed in the central area 111a, the edge ring ER can be separated from the annular area 111b without causing interference between the dummy wafer and the edge ring ER.

[0232] Next, the dummy wafer is electrostatically attached to the central region 111a (S332). Then, the cleaning (second cleaning) of steps S231 to S239 is performed. In steps S231 to S239, the plasma processing chamber 10 is cleaned with the dummy wafer placed on the central region 111a.

[0233] As described above, in Modification 7, cleaning of the plasma processing chamber 10 is performed before the cleaning of steps S231 to S239. Thus, the deposits deposited on the outer periphery of the electrostatic holding disk 1111, the inner periphery of the edge ring ER, and the lower surface of the edge ring ER can be removed more efficiently while suppressing damage to the electrostatic holding disk 1111.

[0234] In Modification 7, the cleaning of steps S231 to S239 is performed with a dummy wafer placed on the central region 111a. Thus, even when the cleaning in the plasma processing chamber 10 is performed under high cleaning performance conditions, damage to the central region 111a can be reduced.

[0235] In addition, Fig.18 The cleaning process shown can be Figure 8 The processing of steps S221 to S223 replaces the processing of steps S238 and S239, and after the processing of step S223, the edge ring ER for replacement is electrostatically adsorbed to the annular region 111b.

[0236] In addition, step S332 and step S231 may be executed at the same timing. That is, the electrostatic adsorption of the edge ring ER relative to the annular region 111b may be released in parallel when the dummy wafer is electrostatically adsorbed to the central region 111a. In this case, for example, after the dummy wafer is placed in the central region 111a, nitrogen, oxygen or other gases may be supplied to the plasma processing chamber 10 and controlled to a predetermined pressure, and high-frequency power may be supplied to the plasma processing chamber 10 to generate plasma, and then the first electrode 1111b (see FIG. 1 ) may be charged with a charge. Fig.10 ) is applied with a voltage to electrostatically adsorb the dummy wafer to the central region 111a, and a voltage having a polarity opposite to that of the voltage used for electrostatic adsorption is applied to the second electrode 1111c to release the electrostatic adsorption of the edge ring ER relative to the annular region 111b. In addition, although plasma is generated, the electrostatic adsorption of the dummy wafer and the release of the electrostatic adsorption of the edge ring may be performed in a state where an inert gas (nitrogen, etc.) is supplied into the plasma processing chamber 10 and controlled to a predetermined pressure (without generating plasma).

[0237] Fig.19This is a flowchart showing an example of the flow of the cleaning process according to the modification 8 of the second embodiment. The PM 1 is mainly operated under the control of the control unit 9 to achieve Fig.19 In addition, Fig.19 Steps S230 to S239 and Fig.11 Steps S230 to S239 are the same as those shown in the figure, so their detailed description is omitted here. Fig.19 Steps S302 to S303 and Fig.14 The steps S302 to S303 shown are the same, so their detailed description is omitted here.

[0238] exist Fig.19 In the cleaning process shown, when the dummy wafer is electrostatically adsorbed on the central area 111a (S303), cleaning (S304) is performed in the plasma processing chamber 10. In step S304, cleaning is performed in the plasma processing chamber 10 in a state where the dummy wafer is placed on the central area 111a. Here, the diameter of the dummy wafer placed on the central area 111a is smaller than the inner diameter of the edge ring ER. In step S304, a reaction gas (cleaning gas) is supplied from the gas supply unit 20 to the plasma processing chamber 10, and high-frequency power is supplied to the base 1110. Thus, in step S304, plasma of the cleaning gas is generated in the plasma processing chamber 10, and cleaning is performed in the plasma processing chamber 10 by the plasma generated from the cleaning gas.

[0239] The cleaning gas supplied into the plasma processing chamber 10 in step S304 may be the same as or different from the cleaning gas supplied into the plasma processing chamber 10 in step S233. The cleaning performed in step S304 is an example of the first cleaning.

[0240] When the cleaning of step S304 is completed, the cleaning of steps S231 to S239 is performed. The cleaning performed in steps S231 to S239 is an example of the second cleaning. In steps S231 to S239, the cleaning of the plasma processing chamber 10 is performed with the wafer dummy placed on the central area 111a.

[0241] Thus, in Modification 8, cleaning of the plasma processing chamber 10 is performed before the cleaning of steps S231 to S239. Thus, the deposits deposited on the outer periphery of the electrostatic holding disk 1111, the inner periphery of the edge ring ER, and the lower surface of the edge ring ER can be efficiently removed while suppressing damage to the electrostatic holding disk 1111.

[0242] In Modification 8, the cleaning of steps S231 to S239 is performed with a dummy wafer placed on central region 111a. Thus, even when the plasma processing chamber 10 is cleaned under high cleaning performance conditions, damage to central region 111a can be reduced.

[0243] In addition, Fig.19 The cleaning process shown can be Figure 8 The processing of steps S221 to S223 replaces the processing of steps S238 and S239, and after the processing of step S223, the edge ring ER for replacement is electrostatically adsorbed to the annular region 111b.

[0244] Fig. 20 This is a flowchart showing an example of a cleaning process according to a modification 9 of the second embodiment. The PM 1 is mainly operated under the control of the control unit 9 to achieve Fig. 20 In addition, Fig. 20 Steps S230 to S239 and Fig.11 Steps S230 to S239 are the same as those shown in the figure, so their detailed description is omitted here. Fig. 20 Steps S302 to S303 and Fig.14 The steps S302 to S303 shown are the same, so their detailed description is omitted here.

[0245] exist Fig. 20 In the cleaning process shown, when the dummy wafer is electrostatically attached to the central region 111a (S303), the cleaning (second cleaning) of steps S231 to S239 is performed. In steps S231 to S239, the plasma processing chamber 10 is cleaned with the dummy wafer placed on the central region 111a.

[0246] In Modification 9, the cleaning of steps S231 to S239 is performed with a dummy wafer placed on the central region 111a. Thus, even when the plasma processing chamber 10 is cleaned under high cleaning performance conditions, damage to the central region 111a can be reduced.

[0247] In addition, Fig. 20 The cleaning process shown can be Figure 8 The processing of steps S221 to S223 replaces the processing of steps S238 and S239, and after the processing of step S223, the edge ring ER for replacement is electrostatically adsorbed to the annular region 111b.

[0248] In addition, step S303 and step S231 may be executed at the same timing. That is, the electrostatic adsorption of the edge ring ER relative to the annular region 111b may be released in parallel when the dummy wafer is electrostatically adsorbed to the central region 111a. In this case, for example, after the dummy wafer is placed in the central region 111a, nitrogen, oxygen or other gases may be supplied to the plasma processing chamber 10 and controlled to a predetermined pressure, and in a state where plasma is generated by supplying high-frequency power to the plasma processing chamber 10, the first electrode 1111b (see Fig.10 ) to electrostatically adsorb the dummy wafer to the central region 111a, and apply a voltage having a polarity opposite to that of the voltage used for electrostatic adsorption to the second electrode 1111c to release the electrostatic adsorption of the edge ring ER relative to the annular region 111b. In addition, although plasma is generated, the electrostatic adsorption of the dummy wafer and the release of the electrostatic adsorption of the edge ring may be performed in a state where an inert gas (nitrogen, etc.) is supplied into the plasma processing chamber 10 and controlled to a predetermined pressure (without generating plasma).

[0249] Fig.21 This is a flowchart showing an example of the flow of the cleaning process according to the modification 10 of the second embodiment. The PM 1 is mainly operated under the control of the control unit 9 to achieve Fig.21 In addition, Fig.21 Steps S230 to S239 and Fig.11 Steps S230 to S239 are the same as those shown in the figure, so their detailed description is omitted here. Fig. 20 Steps S302 to S303 and Fig.14 The steps S302 to S303 shown are the same, so their detailed description is omitted here.

[0250] exist Fig.21 In the cleaning process shown, after the edge ring ER is separated from the annular region 111b by the lifting pins 61 (S232), a dummy wafer is moved into the plasma processing chamber 10 (S302). Here, the diameter of the dummy wafer moved into the plasma processing chamber 10 in step S302 is smaller than the inner diameter of the edge ring ER.

[0251] Next, the lifting pins 60 are lifted by driving the lifting mechanism 62 (elevating the pins), whereby the dummy wafer is transferred to the lifting pins 60 .

[0252] Next, the lifting pins 60 are lowered by driving the lifting mechanism 62, thereby placing the dummy wafer on the central region 111a and electrostatically adsorbing the dummy wafer on the central region 111a (S303). Furthermore, after adjusting the separation distance between the edge ring ER and the annular region 111b as needed, the process from step S233 is performed. That is, in the process from step S233, the cleaning of the plasma processing chamber 10 is performed with the dummy wafer placed on the central region 111a.

[0253] In Modification 10, the processing from step S233 onwards is performed with a dummy wafer placed on central region 111a. Thus, even when the plasma processing chamber 10 is cleaned under high cleaning performance conditions, damage to central region 111a can be reduced.

[0254] In addition, assuming that the edge ring ER is separated from the annular region 111b after the dummy wafer is placed in the central region 111a, the dummy wafer and the edge ring ER may interfere with each other depending on the placement position of the dummy wafer in the central region 111a. In this regard, in Modification 10, the dummy wafer is placed in the central region 111a after the edge ring ER is separated from the annular region 111b, thereby preventing the dummy wafer from interfering with the edge ring ER.

[0255] [other]

[0256] In addition, the technology disclosed in the present application is not limited to the above-mentioned embodiment, and various modifications can be made within the scope of the gist of the technology.

[0257] For example, in the above-mentioned modification 6 of the second embodiment (see Fig.16 ), after the dummy wafer is cleaned in a state where the dummy wafer is raised by pins, the edge ring ER is cleaned in a state where the edge ring ER is raised by pins, but the disclosed technology is not limited to this. For example, as another example, after the edge ring ER is cleaned in a state where the edge ring ER is raised by pins, the dummy wafer is cleaned in a state where the dummy wafer is raised by pins. More specifically, after the edge ring ER is cleaned in a state where the edge ring ER is raised by pins, the edge ring ER is placed in the annular area 111b, the dummy wafer is moved into the plasma processing chamber 10, and the dummy wafer is cleaned in a state where the dummy wafer is raised by pins. In addition, the diameter of the dummy wafer used in this case may be smaller than the inner diameter of the edge ring ER.

[0258] Alternatively, in the variation 6 of the second embodiment described above, both the wafer dummy and the edge ring ER may be cleaned in a state where both are raised by the pins. The timing of raising the wafer dummy and the edge ring ER by the pins may be simultaneous or staggered. For example, in the case where the edge ring ER is raised first by the pins, after the edge ring ER is raised by the pins, a wafer dummy having a diameter smaller than the inner diameter of the edge ring ER is moved into the plasma processing chamber 10. Then, the wafer dummy may be lowered by the lifting pins 60 until the wafer dummy is slightly above the central area 111a, thereby creating a state where both the wafer dummy and the edge ring ER are raised by the pins. Alternatively, the wafer dummy is moved into the plasma processing chamber 10, and the wafer dummy is lowered by the lifting pins 60 until the wafer dummy is slightly above the central area 111a. Then, the edge ring ER may be raised by the pins, thereby creating a state where both the wafer dummy and the edge ring ER are raised by the pins. Furthermore, the lower surface of the dummy wafer may be higher than the upper surface of the inner peripheral portion of the edge ring ER, and the lower surface of the edge ring ER may be higher than the upper surface of the dummy wafer.

[0259] Alternatively, after the edge ring ER is raised by the pins, a dummy wafer having a diameter larger than the inner diameter of the edge ring ER is moved into the plasma processing chamber 10, and the dummy wafer is lowered by the lifting pins 60 until the dummy wafer is slightly above the central area 111a, thereby creating a state in which both the dummy wafer and the edge ring ER are raised by the pins (first mode). Alternatively, a dummy wafer having a diameter larger than the inner diameter of the edge ring ER is moved into the plasma processing chamber 10, and the dummy wafer is lowered by the lifting pins 60 until the dummy wafer is slightly above the central area 111a, and the edge ring ER is raised by the pins, thereby creating a state in which both the dummy wafer and the edge ring ER are raised by the pins (second mode). In addition, in the first mode and the second mode, the lower surface of the dummy wafer is higher than the upper surface of the inner peripheral portion of the edge ring ER.

[0260] In addition, in step S301 of the variation 6 of the second embodiment described above, the cleaning of the plasma processing chamber 10 is performed in a state where no dummy wafer exists in the central region 111a, but the disclosed technology is not limited thereto. For example, as another example, a dummy wafer may be moved into the plasma processing chamber 10 before step S301, and in step S301, the cleaning of the plasma processing chamber 10 may be performed in a state where a dummy wafer is placed in the central region 111a. Then, after the cleaning of step S301 is completed, the dummy wafer may be raised by pins, and the cleaning of step S313 may be performed.

[0261] In the above-mentioned modification 6 of the second embodiment, after cleaning is performed in a state where the dummy wafer is raised by the pins, the dummy wafer is removed, and cleaning is performed in a state where the edge ring ER is raised by the pins without the dummy wafer in the central area 111a, but the disclosed technology is not limited thereto. For example, as another example, after cleaning is performed in a state where the dummy wafer is raised by the pins, the dummy wafer is not removed, the dummy wafer is placed in the central area 111a, and cleaning is performed in a state where the edge ring ER is raised by the pins. In this case, a dummy wafer having a diameter smaller than the inner diameter of the edge ring ER can be used.

[0262] In the above-mentioned modification 6 of the second embodiment, the cleaning is performed with the edge ring ER separated from the annular region 111b by a predetermined distance, but the disclosed technology is not limited thereto. For example, as another example, the modification 1 of the first embodiment (see Figure 7 ), after cleaning is performed in a state where the edge ring ER is raised by the pins, further cleaning is performed in a state where the distance between the edge ring ER and the annular region 111b is increased.

[0263] In addition, in the above-mentioned variation 6 of the second embodiment, after cleaning is performed in a state where no dummy wafer exists in the central area 111a, the dummy wafer is moved into the plasma processing chamber 10, and further cleaning is performed in a state where the dummy wafer is raised by the pins, but the disclosed technology is not limited thereto. As another example, after cleaning is performed in a state where the dummy wafer is raised by the pins, the dummy wafer is moved out of the plasma processing chamber 10, and further cleaning is performed in a state where no dummy wafer exists in the central area 111a.

[0264] In addition, the cleaning performed in the state where the wafer dummy is raised by the pins and the cleaning performed in the state where the edge ring ER is raised by the pins can be performed every time a predetermined number of product wafers are processed, or every time the cumulative time of processing product wafers reaches a predetermined time. In addition, the cleaning performed in the state where the wafer dummy is raised by the pins and the cleaning performed in the state where the edge ring ER is raised by the pins can be performed at a timing immediately before replacing the edge ring ER.

[0265] In addition, in the above-mentioned embodiment, the dummy wafer is accommodated in the accommodation device 52 separate from the VTM 51, but the disclosed technology is not limited to this. As another embodiment, the dummy wafer can also be accommodated in a space provided in the VTM 51. Moreover, the edge ring ER for replacement can also be accommodated in the space. Alternatively, the dummy wafer can also be accommodated in a container such as a FOUP connected to the load port 55.

[0266] In the above embodiment, PM 1 that processes wafer W using plasma is described as an example, but the disclosed technology is not limited thereto. Any device that can perform processes such as film formation and heat treatment on wafer W may be used, and the disclosed technology may also be applied to a device that does not use plasma.

[0267] In addition, in the above-mentioned embodiment, as an example of a plasma source used in PM 1, a capacitively coupled plasma is described, but the plasma source is not limited thereto. As plasma sources other than the capacitively coupled plasma, for example, inductively coupled plasma (ICP), microwave-excited surface wave plasma (SWP), electron cyclotron resonance plasma (ECP), and helicon wave excited plasma (HWP) are listed. The microwave used in the microwave-excited surface wave plasma (SWP) is an example of an electromagnetic wave.

[0268] The embodiments disclosed herein are to be considered as illustrative in all respects and not restrictive. In fact, the above embodiments can be implemented in a variety of ways. In addition, the above embodiments can be omitted, replaced, and changed in various ways without departing from the attached claims and their gist.

[0269] In addition, regarding the above-mentioned embodiment, the following supplementary notes are disclosed.

[0270] (Note 1)

[0271] A plasma processing device, comprising:

[0272] Handling containers;

[0273] a mounting table disposed in the processing container, the mounting table having a substrate mounting surface and a ring member mounting surface surrounding the outer periphery of the substrate mounting surface;

[0274] a ring placed on the ring member placing surface;

[0275] a first lifting mechanism including first lifting pins for supporting the substrate;

[0276] a second lifting mechanism having second lifting pins for supporting the ring; and

[0277] Control Department,

[0278] The control unit is configured to perform the following processing:

[0279] Process (a), cleaning the inside of the processing container using plasma while controlling the first lifting mechanism to support the dummy substrate through the first lifting pins; and

[0280] In the process (b), the inside of the processing container is cleaned using plasma while the second lifting mechanism is controlled so that the ring is supported by the second lifting pins.

[0281] (Note 2)

[0282] In the plasma processing apparatus described in Supplementary Note 1,

[0283] The control unit is configured to further execute process (c) of cleaning the inside of the processing container in a state where no substrate is in the processing container.

[0284] (Note 3)

[0285] In the plasma processing apparatus described in Supplement 1 or 2,

[0286] The control unit is configured to further execute a process (d) of cleaning the inside of the processing container in a state where a dummy substrate is placed on the substrate placement surface in the processing container.

[0287] (Note 4)

[0288] In the plasma processing apparatus described in Supplementary Note 1,

[0289] The control unit is configured to execute the process (a) and the process (b) simultaneously.

[0290] (Note 5)

[0291] In the plasma processing apparatus described in any one of Supplementary Notes 1 to 4,

[0292] The control unit is configured to execute a process of cleaning the inside of the processing container in the process (b) in a state where a dummy substrate is placed on the substrate placement surface.

[0293] (Note 6)

[0294] In the plasma processing apparatus described in Supplementary Note 5,

[0295] In the process (b), the diameter of the dummy substrate placed on the substrate placement surface is smaller than the inner diameter of the ring.

[0296] (Note 7)

[0297] In the plasma processing apparatus described in Supplementary Note 6,

[0298] The control unit is configured to perform the following processing in the processing (b):

[0299] Process (b-1), controlling the first lifting mechanism to raise the first lifting pin to receive the dummy substrate carried into the processing container;

[0300] Process (b-2), controlling the first lifting mechanism to lower the first lifting pins to place the dummy substrate on the substrate placing surface;

[0301] Process (b-3), controlling the second lifting mechanism to raise the second lifting pins, so as to hold the ring by the second lifting pins; and

[0302] Process (b-4): cleaning the inside of the processing container using plasma.

[0303] (Note 8)

[0304] In the plasma processing apparatus described in any one of Supplementary Notes 1 to 7,

[0305] The control unit is configured to perform the following processing in the processing (a):

[0306] Process (a-1), controlling the first lifting mechanism to raise the first lifting pin to receive the dummy substrate carried into the processing container;

[0307] Process (a-2), controlling the first lifting mechanism so that the front end of the first lifting pin is located above the mounting table and lower than the position where the dummy substrate is received;

[0308] Process (a-3), after the process (a-2), cleaning the inside of the processing container by using plasma; and

[0309] Process (a-4), controlling the first lifting mechanism to raise the first lifting pins to move the dummy substrate out of the processing container.

[0310] (Note 9)

[0311] In the plasma processing apparatus described in Supplementary Note 8,

[0312] The control unit is configured to execute the process (a-2) after the process (a-1).

[0313] (Note 10)

[0314] In the plasma processing apparatus described in Supplementary Note 9,

[0315] The control unit is configured to perform processing (a-5) after processing (a-1) to lower the first lifting pin to place the substrate dummy piece on the substrate mounting surface, and the control unit is configured to raise the first lifting pin in processing (a-2) after processing (a-5) to position the first lifting pin lower than the position where the first lifting pin receives the substrate dummy piece.

[0316] (Note 11)

[0317] In the plasma processing apparatus described in Supplementary Note 10,

[0318] The control unit is configured to perform process (a-6) after process (a-5) and before process (a-2), and clean the inside of the processing container using plasma while the substrate dummy is placed on the substrate placement surface.

[0319] (Note 12)

[0320] In the plasma processing apparatus described in Supplementary Note 8,

[0321] The control unit is configured to execute the process (a-4) after the process (a-3).

[0322] Description of Reference Numerals

[0323] 2: mounting table; 2a: substrate; 2b: inlet piping; 2c: outlet piping; 2d: temperature control medium flow path; 3: support member; 3a: inner wall member; 4: support table; 5: edge ring; 6: electrostatic holding disk; 6a: electrode; 6b: insulator; 6e: first mounting surface; 6f: second mounting surface; 9: control unit; 9a: computer; 9a1: processing unit; 9a2: storage unit; 9a3: communication interface; 10: plasma processing chamber (processing container); 10a: side wall; 10b: opening; 10c: grounding conductor; 10e: gas exhaust port; 10s: plasma processing space; 11: substrate support; 13: shower head; 13a: gas supply port; 13b: gas diffusion chamber; 13c: Gas inlet port; 14a: first RF power supply; 14b: second RF power supply; 15a: first matching device; 15b: second matching device; 16: shower head; 16a: main body; 16b: upper top plate; 16c: gas diffusion chamber; 16d: gas flow hole; 16e: gas inlet hole; 16g: gas inlet port; 17: DC power supply; 18: gas supply source; 18a: gas supply piping; 20: gas supply unit; 21: gas source; 22: flow controller; 30: power supply; 31: RF power supply; 31a: first RF generator; 31b: second RF generator; 32: DC power supply; 32a: first DC generator; 32b: second DC generator; 40: exhaust system; 50: substrate Processing system; 52: Accommodation device; 55: Loading port; 60: Lifting pin; 61: Lifting pin; 61a: Front end; 62: Lifting mechanism; 63: Lifting mechanism; 70: Gas supply pipe; 72: Variable DC power supply; 73: On / off switch; 81: Exhaust port; 82: Exhaust pipe; 83: First exhaust device; 84: Loading and unloading port; 85: Gate valve; 86: Sediment shield; 87: Sediment shield; 95: Insulating member; 100: Control unit; 101: Process controller; 102: User interface; 103: Storage unit; 111: Main body; 111a: Central area; 111b: Ring area; 112: Ring assembly; 130: Gas supply pipe; 161: Lifting pin; 162: Lifting pin Mechanism; 163: lifting pin; 164: lifting mechanism; 200: through hole for pin; 300: through hole for pin; 510: transport robot; 511: arm; 512: fork; 540: transport robot; 541: guide rail; 1110: base; 1110a: flow path; 1110b: insulating component; 1111: electrostatic holding disk; 1111a: ceramic component; 1111b: first electrode; 1111c: second electrode; CR: cover ring; ER: edge ring; ERr: recess; G1: gate valve; G2: gate valve; G3: gate valve; G4: gate valve; G5: gate valve; H1: through hole; H2: through hole; H3: through hole; H4: through hole; H5: through hole; P: plasma; W: wafer.

Claims

1. A plasma processing device, comprising: Handling containers; a mounting table disposed in the processing container, the mounting table having a substrate mounting surface and a ring member mounting surface surrounding the outer periphery of the substrate mounting surface; a ring placed on the ring member placing surface; a first lifting mechanism including first lifting pins for supporting the substrate; a second lifting mechanism having a second lifting pin for supporting the ring; as well as Control Department, in, The control unit is configured to execute the following processing: Process (a), cleaning the inside of the processing container using plasma while controlling the first lifting mechanism to support the dummy substrate through the first lifting pins; as well as In the process (b), the inside of the processing container is cleaned using plasma while the second lifting mechanism is controlled so that the ring is supported by the second lifting pins.

2. The plasma processing apparatus according to claim 1, wherein: The control unit is configured to further execute process (c) of cleaning the inside of the processing container in a state where no substrate is in the processing container.

3. The plasma processing apparatus according to claim 1, wherein: The control unit is configured to further execute a process (d) of cleaning the inside of the processing container in a state where a dummy substrate is placed on the substrate placement surface in the processing container.

4. The plasma processing apparatus according to claim 1, wherein: The control unit is further configured to execute the following processing: Process (c), cleaning the processing container in a state where there is no substrate in the processing container; and Process (d) is to clean the inside of the processing container while a dummy substrate is placed on the substrate placement surface in the processing container.

5. The plasma processing apparatus according to claim 1, wherein: The control unit is configured to execute the process (a) and the process (b) simultaneously.

6. The plasma processing apparatus according to claim 1, wherein: The control unit is configured to execute a process of cleaning the inside of the processing container in the process (b) in a state where a dummy substrate is placed on the substrate placement surface.

7. The plasma processing apparatus according to claim 6, wherein: In the process (b), the diameter of the dummy substrate placed on the substrate placement surface is smaller than the inner diameter of the ring.

8. The plasma processing apparatus according to claim 7, wherein: The control unit is configured to perform the following processing in the processing (b): Process (b-1), controlling the first lifting mechanism to raise the first lifting pin to receive the dummy substrate carried into the processing container; Process (b-2), controlling the first lifting mechanism to lower the first lifting pins to place the dummy substrate on the substrate placing surface; Process (b-3), controlling the second lifting mechanism to raise the second lifting pins, so as to hold the ring by the second lifting pins; and Process (b-4): cleaning the inside of the processing container using plasma.

9. The plasma processing apparatus according to claim 1, wherein: The control unit is configured to perform the following processing in the processing (a): Process (a-1), controlling the first lifting mechanism to raise the first lifting pin to receive the dummy substrate carried into the processing container; Process (a-2), controlling the first lifting mechanism so that the front end of the first lifting pin is located above the mounting table and lower than the position where the dummy substrate is received; Process (a-3), after the process (a-2), cleaning the inside of the processing container by using plasma; and Process (a-4), controlling the first lifting mechanism to raise the first lifting pins to move the dummy substrate out of the processing container.

10. The plasma processing apparatus according to claim 9, wherein: The control unit is configured to execute the process (a-2) after the process (a-1).

11. The plasma processing apparatus according to claim 10, wherein: The control unit is configured to perform processing (a-5) after processing (a-1) to lower the first lifting pin to place the substrate dummy piece on the substrate mounting surface, and the control unit is configured to raise the first lifting pin in processing (a-2) after processing (a-5) to position the first lifting pin lower than the position where the first lifting pin receives the substrate dummy piece.

12. The plasma processing apparatus according to claim 11, wherein: The control unit is configured to perform process (a-6) after process (a-5) and before process (a-2), and clean the inside of the processing container using plasma while the substrate dummy is placed on the substrate placement surface.