Inward-shrinkage mold and injection molding method

By setting up inner and outer runners and circulating cooling systems in small volume internal shrink molds, the problem of insufficient heat dissipation of the mold is solved, constant temperature cooling at the injection molding end of the mold is achieved, and the molding efficiency and yield of the product are improved.

CN118906404APending Publication Date: 2024-11-08江苏新劢德医疗器械科技有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411288199.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-14
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

Small volume internal shrinkage molds are difficult to dissipate heat during injection molding, resulting in an increase in temperature, affecting product molding efficiency and yield, and the existing cooling methods are not effective.

Method used

Design the inner and outer runner structure, combine the circulating cooling system, cool the mold through cooling medium, maintain the constant temperature at the injection molding end, and realize continuous product production.

Benefits of technology

It effectively reduces the mold temperature and improves the product forming efficiency and yield, and is especially suitable for molds with limited volume.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118906404A_ABST
    Figure CN118906404A_ABST
Patent Text Reader

Abstract

The invention discloses an inward shrinkage mold and an injection molding method, the inward shrinkage mold comprises an inward shrinkage piece, an insertion core and a binding sleeve, the inward shrinkage piece is arranged on a top plate, and an outer runner is arranged on the periphery of the inward shrinkage piece and used for cooling the inward shrinkage piece; the insertion core is arranged on the fixed mold base and is in sliding fit with the inner shrinkage piece, and an inner flow channel is formed in the insertion core and is used for cooling the insertion core; the binding sleeve is arranged on the internal contraction piece and is used for selectively controlling the internal contraction piece to be folded or unfolded; and the ejector plate can move up and down relative to the fixed mold base, so that the inward shrinkage movable mold is switched between an injection molding state and a demolding state. According to the internal shrinkage mold, the mold is cooled, so that the injection molding end of the mold is kept at a constant temperature in the injection molding process, continuous production of products is realized, and the yield of the products is improved; and aiming at a mold with a limited volume, an inner and outer runner collaborative cooling mode is adopted, so that the cooling effect is better.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of molds, and in particular to an inner shrink mold and an injection molding method. Background Art

[0002] Injection molding refers to a method in which completely molten material is injected into a mold cavity under high pressure at a certain temperature, and a molded product is obtained after cooling and solidification. For some products with undercut structures, the existing technology generally uses a mold with an indented structure for injection molding, so that the molded product can be ejected smoothly to achieve the demoulding effect.

[0003] However, for some smaller products (such as Figure 8 The kit shown has a diameter of about 1 cm and an undercut structure needs to be formed on the inside. Since the mold volume of the matching inward-shrinking structure is small, the injection end of the mold cannot dissipate heat well during the long-term injection molding process, causing the injection temperature to continue to rise, which not only affects the product molding efficiency, but also may cause product defects, such as uneven filling, bubbles and flow marks on the surface, or dimensional changes and warping, reducing the product yield.

[0004] There are two main ways to solve the above problems: 1. Stop the machine when the temperature at the injection end of the mold reaches the warning line, and continue production after the temperature drops, but this seriously affects production efficiency. 2. Use a fan to cool the injection end of the mold after demoulding, but it still cannot change the impact of high temperature on product molding during injection molding, and the cooling effect is poor.

[0005] Therefore, how to keep the small-volume shrink mold at a constant temperature during the injection molding process and improve product production efficiency and yield is an urgent problem to be solved. Summary of the invention

[0006] The object of the present invention is to provide an inward shrink mold and an injection molding method, by arranging internal and external flow channels to cool the mold, so that the injection end of the mold maintains a constant temperature during the injection molding process, thereby realizing continuous production of products and improving product yield.

[0007] The purpose of the present invention is achieved by the following technical solutions: A shrink mold, comprising: The retracted part is arranged on the top plate, and an outer flow channel is arranged on the outer periphery of the retracted part for cooling the retracted part; An insert core is arranged on the fixed mold base and is slidably matched with the retracted part, and an inner flow channel is arranged inside the insert core for cooling the insert core; A collar, disposed on the retractable member, for selectively controlling the retraction or expansion of the retractable member; The top plate can move up and down relative to the fixed mold base, so that the shrink mold can be switched between the injection state and the demoulding state.

[0008] In some embodiments, the retracted part and the insert are both made of heat-conductive metal material.

[0009] In some embodiments, the outer flow channel is located in the top plate, and a first inlet and a first outlet communicating with the outer flow channel are provided in the top plate.

[0010] In some embodiments, a first sealing ring is respectively provided between the first inlet and the outer flow channel, and between the first outlet and the outer flow channel.

[0011] In some embodiments, the inner flow channel is partially located in the fixed mold base, and a second inlet and a second outlet communicating with the inner flow channel are provided in the fixed mold base.

[0012] In some embodiments, a second sealing ring is respectively provided between the second inlet and the outer flow channel, and between the second outlet and the outer flow channel.

[0013] In some embodiments, a flow partition is disposed in the inner flow channel, one end of the flow partition is sealed with one end of the inner flow channel, and the other end of the flow partition is spaced apart from the other end of the inner flow channel.

[0014] In some embodiments, the retracted member includes a first seat portion, a first connecting portion, and a gathering portion arranged sequentially from bottom to top; Wherein, the first seat portion is partially fixed in the top plate, a convex bump is arranged on the first connecting portion, and a molding feature is arranged on the gathering portion.

[0015] In some embodiments, a heat-conducting layer is disposed on the surface of the molding feature, the heat-conducting layer extends to the outer flow channel, and the thermal conductivity of the material of the heat-conducting layer is greater than the thermal conductivity of the material of the shrink part.

[0016] In some embodiments, the insert core includes a second seat portion, a second connecting portion and an inner core portion arranged sequentially from bottom to top; Wherein, the second seat portion is partially fixed in the fixed mold seat, and the inner core portion corresponds to and matches the gathering portion.

[0017] In some embodiments, the inner flow channel is located in the second seat portion, a heat conductor is disposed in the inner core portion, the heat conductor extends to the inner flow channel, and the thermal conductivity of the heat conductor material is greater than the thermal conductivity of the core material.

[0018] In some embodiments, a circulating cooling system is further included, wherein the circulating cooling system connects the inner flow channel and the outer flow channel, and the temperature and flow rate of the cooling medium output by the circulating cooling system are adjustable.

[0019] In some embodiments, the first inlet connected to the outer flow channel is provided with a heat insulation layer, and / or the second inlet connected to the inner flow channel is provided with a heat insulation layer. An injection molding method, using any of the above-mentioned inner shrink molds, comprises the following steps: S1, moving the inner shrinkage part downward to make it cooperate with the insert to form the injection end of the mold; S2, injecting cooling medium into the inner flow channel and the outer flow channel respectively; S3, mold closing, molding the target product at the injection end of the mold, during which the temperature of the injection end of the mold is monitored and the temperature and flow rate of the cooling medium are adjusted accordingly; S4, mold opening, first control the inner shrinkage part to move upward to decompose the injection end of the mold, and then control the sleeve to move upward to close the inner shrinkage part, so as to demould the target product; S5. Repeat steps S1, S3 and S4 in sequence to achieve continuous production of the target product.

[0020] In some embodiments, in step S2, the cooling medium is cooling liquid or cooling gas.

[0021] In some embodiments, in step S3, the temperature of the injection end of the mold is maintained at 120°-140°.

[0022] Compared with the prior art, the beneficial effects of the present invention include at least: 1. By cooling the mold, the injection end of the mold can maintain a constant temperature during the injection process, thereby achieving continuous production of products and improving product yield.

[0023] 2. For molds with limited volume, the internal and external runners are used for collaborative cooling, which has a better cooling effect. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 It is a schematic diagram of the connection between the inner shrink mold and the circulating cooling system of the present invention.

[0025] Figure 2 It is a cross-sectional view of the inner shrink mold of the present invention.

[0026] Figure 3 It is a three-dimensional structural schematic diagram of the inner shrink mold of the present invention.

[0027] Figure 4 yes Figure 3 sectional view of .

[0028] Figure 5It is a three-dimensional structural schematic diagram of the retracted part of the present invention.

[0029] Figure 6 It is a cross-sectional view of the ferrule of the present invention.

[0030] Figures 7a to 7d The present invention is a schematic diagram of the injection molding process using the inner shrink mold of the present invention.

[0031] Figure 8 It is a structural diagram of the target product.

[0032] In the figure: 1, retracted part; 11, first seat; 12, first connecting part; 121, convex hull; 13, gathering part; 131, molding feature; 14, outer flow channel; 15, heat conducting layer; 2. Insert core; 21. Second seat portion; 22. Second connection portion; 23. Inner core portion; 24. Inner flow channel; 25. Heat conductor; 3. Harness; 4. Top plate; 41. First inlet; 42. First outlet; 5. Fixed die base; 51. Second inlet; 52. Second outlet; 6. The first sealing ring; 7. Second sealing ring; 8. Flow divider; 9. Circulating cooling system; 10. Thermal insulation layer. DETAILED DESCRIPTION

[0033] Example embodiments will now be described more fully with reference to the accompanying drawings. However, example embodiments can be implemented in a variety of forms and should not be construed as limited to the embodiments set forth herein; rather, these embodiments are provided to make the present invention more comprehensive and complete and to fully convey the concepts of example embodiments to those skilled in the art. The same reference numerals in the figures represent the same or similar structures, and thus their repeated description will be omitted.

[0034] The words expressing positions and directions described in the present invention are all explained with reference to the accompanying drawings as examples, but they can be changed as needed, and all such changes are included in the protection scope of the present invention.

[0035] See also Figures 1 to 6 As shown, the present invention discloses an inner shrink mold, comprising an inner shrink part 1, an insert core 2 and a sleeve 3.

[0036] Among them, Figure 2 As shown, the retracted part 1 is arranged on the top plate 4, and can move up and down with the top plate 4, so as to realize the formation and decomposition of the injection end of the mold. In addition, an outer flow channel 14 is arranged on the outer periphery of the retracted part 1 for cooling the retracted part 1.

[0037] See also Figure 5 As shown, in the present application, the retractable part 1 is roughly cylindrical, and includes a first seat portion 11, a first connecting portion 12 and a gathering portion 13 arranged in sequence from bottom to top. Among them, the first seat portion 11 is partially fixed in the top plate 4, so that the retractable part 1 and the top plate 4 form an integral structure, and a convex bump 121 is provided on the first connecting portion 12, which is used to cooperate with the vertical sleeve, so as to control the gathering portion 13 to gather or open, and a molding feature 131 is provided on the gathering portion 13, which is used to mold the undercut structure of the target product. In a more specific structure, the first seat portion 11 is continuous in the circumference, and the first connecting portion 12 and the gathering portion 13 are spaced in the circumference, so as to form a retractable petal-type structure for demoulding. Considering that only the first seat portion 11 of the retractable part 1 has the groove condition, and because the diameter of the first seat portion 11 is larger than that of the other parts, the outer flow channel 14 is preferably arranged on the outer periphery of the first seat portion 11, so that the retractable part 1 can obtain a better cooling effect.

[0038] Or Figure 2 As shown, the insert core 2 is arranged on the fixed mold base 5 and slidably cooperates with the retracted part 1 to realize the formation and decomposition of the injection end of the mold, and an inner flow channel 24 is arranged inside the insert core 2 for cooling the insert core 2.

[0039] See also Figure 6 As shown, in the present application, the insert 2 includes a second seat portion 21, a second connecting portion 22 and an inner core portion 23 arranged in sequence from bottom to top. Among them, the second seat portion 21 is partially fixed in the fixed mold seat 5, so that the insert 2 and the fixed mold seat 5 form an integrated structure, and the inner core portion 23 corresponds to and matches the gathering portion 13, and the combination of the two can form the desired mold injection end (see Figure 4 ). In a more specific structure, the second seat portion 21 is cylindrical, the second connection portion 22 is more slender rod-shaped, and the inner core portion 23 is star-shaped and completely matches the inner side of the gathering portion 13. Considering the structural strength and processing technology of the core 2, the inner flow channel 24 is preferably located inside the second connection portion 22, so that the core 2 can obtain a better cooling effect.

[0040] See you next Figure 3 and Figure 4 The sleeve 3 is arranged on the retracted part 1. By controlling its up and down movement, the retracted part 1 can be selectively controlled to be retracted or opened, thereby switching between injection molding and demolding.

[0041] In the present application, an extrusion portion is provided on the inner side of the sleeve 3, and the extrusion portion is slidably matched with the first connecting portion 12 of the retracted part 1. After the injection molding is completed, the sleeve 3 is controlled to move upward so that it contacts the convex bump 121. The convex bump 121 is squeezed and deflected radially inward, causing the retracted portion 13 of the retracted part 1 to gather, thereby facilitating the demolding of the target product.

[0042] When the inner shrink mold is in use, the top plate 4 can move up and down relative to the fixed mold base 5, so that the inner shrink mold is switched between the injection state and the demoulding state.

[0043] Specifically, the top plate 4 is controlled to drive the inner shrinking part 1 to move downward, so that its retracted part 13 cooperates with the inner core part 23 of the plug 2 to form the injection end of the mold. Then the mold is closed for injection molding, during which cooling medium is injected into the inner runner 24 and the outer runner 14 respectively, so that the inner shrinking part 1 and the plug 2 are cooled by heat conduction. Through the coordinated cooling method of the inside and outside, the inner shrinking mold can have a better cooling effect as a whole, and the temperature of the injection end of the mold can also be stabilized within a suitable range. After the injection molding, the mold is opened, and the top plate 4 is controlled to drive the inner shrinking part 1 to move upward, so that its retracted part 13 is separated from the inner core part 23 of the plug 2 by a certain distance. At this time, the injection end of the mold is decomposed, and the top plate 4 is continued to be controlled to move upward until the sleeve 3 contacts the convex 121 on the first connecting part 12 of the inner shrinking part 1, and the retracted part 13 of the inner shrinking part 1 is forced to retract. At this time, the target product with the undercut structure can be smoothly demolded from the inner shrinking part 1.

[0044] In the above process, in order to realize the cooling function, the inner shrink mold needs to be connected to the circulating cooling system 9, which connects the inner flow channel 24 and the outer flow channel 14, and the temperature and flow rate of the cooling medium output by the circulating cooling system 9 are adjustable, so as to meet the temperature control requirements of the injection molding process of different materials. In this application, the cooling medium output by the circulating cooling system 9 is cooling water, and the temperature control of the cooling water is relatively stable, which can make the injection end of the mold constant temperature within a certain range, such as floating around 130°, and the cooling water can be recycled, which is energy-saving and environmentally friendly.

[0045] In some embodiments, the inner shrink piece 1 and the insert 2 are both made of heat-conducting metal materials to ensure that the inner shrink mold has good thermal conductivity, and the heat accumulated at the injection end of the mold can be well transferred to the inner flow channel 24 and the outer flow channel 14, and cooled down under the action of the cooling medium, thereby avoiding high temperature affecting the injection molding. Exemplarily, the heat-conducting metal material of the present application can be copper, aluminum and its alloys or low-carbon steel and other materials.

[0046] See also Figure 2 As shown, in some embodiments, the outer flow channel 14 is located in the top plate 4, and the top plate 4 is provided with a first inlet 41 and a first outlet 42 connected to the outer flow channel 14, so as to realize the inlet and outlet functions of the cooling medium in the outer flow channel 14. In the present application, the first inlet 41 and the first outlet 42 are hidden in the top plate 4, and the outer flow channel 14 can be connected by inserting the two. Compared with the external inlet and outlet, it reduces the additional pipeline configuration, which is not only convenient to connect, but also has lower cost. On the other hand, since the additional pipeline configuration is reduced, the inlet and outlet design does not take up a lot of space, which is particularly suitable for dense and small-volume molds.

[0047] Furthermore, a first sealing ring 6 is provided between the first inlet 41 and the outer flow channel 14, and between the first outlet 42 and the outer flow channel 14, respectively, to improve the sealing performance at the inlet and outlet of the outer flow channel 14, prevent leakage of the cooling medium, and improve reliability. In the present application, first sealing grooves are provided on both sides of the first seat 11, and the first sealing ring 6 is installed in the first sealing groove. The first sealing ring 6 can be an O-shaped rubber ring, which has low cost and good sealing performance.

[0048] See also Figure 2 As shown, in some embodiments, the inner flow channel 24 is partially located in the fixed mold base 5, and the fixed mold base 5 is provided with a second inlet 51 and a second outlet 52 connected to the inner flow channel 24, so as to realize the inlet and outlet function of the cooling medium in the inner flow channel 24. In the present application, the second inlet 51 and the second outlet 52 are hidden in the fixed mold base 5, and the inner flow channel 24 can be connected by inserting the inner flow channel 24 between the two. Compared with the external inlet and outlet, it also reduces the additional pipeline configuration, which is not only convenient for connection, but also has lower cost. On the other hand, since the additional pipeline configuration is reduced, the inlet and outlet design does not take up a lot of space, which is particularly suitable for dense and small-volume molds.

[0049] Furthermore, a second sealing ring 7 is provided between the second inlet 51 and the outer flow channel 14, and between the second outlet 52 and the outer flow channel 14. It is used to improve the sealing performance at the inlet and outlet of the inner flow channel 24, prevent leakage of the cooling medium, and improve reliability. In the present application, second sealing grooves are provided on both sides of the second seat 21, and the second sealing ring 7 is installed in the second sealing groove. The second sealing ring 7 can also be an O-shaped rubber ring.

[0050] See also Figure 4 and Figure 6 As shown, in some embodiments, a flow partition 8 is provided in the inner flow channel 24, one end of the flow partition 8 is sealed with one end of the inner flow channel 24, and a distance is provided between the other end of the flow partition 8 and the other end of the inner flow channel 24, so as to extend the path of the cooling medium in the inner flow channel 24 and increase the contact area with the second seat 21, so as to fully exchange heat and improve the cooling effect on the core 2.

[0051] Due to the volume limitation of the inner shrink mold, the inner flow channel 24 in the second seat 21 is a narrow and long strip hole structure. The cooling medium (such as cooling water) may have scale and crystallization during the long-term cooling process, resulting in blockage of the inner flow channel 24 and affecting the cooling effect. Therefore, in the present application, one end of the flow divider 8 is detachably sealed and connected to one end of the inner flow channel 24. For example, the lower end of the flow divider 8 is sealed and connected to the bottom thread of the second seat.

[0052] See also Figure 4 and Figure 5As shown, in the inward-shrinking mold, the molding feature 131 is a concave structure, which is used to mold the undercut structure of the target product. Due to its concave design, the molding feature 131 is more difficult to cool down and dissipate heat than the rest of the gathering portion 13. Therefore, when demolding, the undercut structure of the target product is softer than the rest, and there is a risk of deformation, which affects the yield.

[0053] To this end, in some embodiments, a heat-conducting layer 15 is provided on the surface of the molding feature 131, and the heat-conducting layer 15 extends to the outer flow channel 14, and the thermal conductivity of the material of the heat-conducting layer 15 is greater than the thermal conductivity of the material of the shrink part 1, so as to enhance the cooling effect at the molding feature 131 and ensure the reliability of the undercut structure molding of the target product. Exemplarily, in the present application, the heat-conducting layer 15 is preferably a silver-plated layer, which has excellent thermal conductivity and can cool the surface of the molding feature 131 well, thereby improving the yield of injection molding. In addition, the silver-plated layer has a smooth texture, and the undercut structure of the target product is not easy to adhere to the molding feature 131, further improving the smoothness of demolding.

[0054] See also Figure 4 As shown, in the inner shrink mold, the second connecting part 22 is in the shape of a slender rod, and its thermal conductivity is relatively poor, which may cause a difference in cooling temperature between the inner core part 23 and the gathering part 13, and also affect the demolding yield of the target product. If the second connecting part 22 directly adopts a material with a high thermal conductivity coefficient, the cost will be high and the structural strength will be difficult to guarantee.

[0055] To this end, in some embodiments, the inner flow channel 24 is located in the second seat 21, and a heat conductor 25 is provided in the inner core 23, the heat conductor 25 extends to the inner flow channel 24, and the thermal conductivity of the material of the heat conductor 25 is greater than the thermal conductivity of the material of the plug 2, so as to enhance the cooling effect on the inner core 23 and ensure that the temperature of the inner core 23 and the gathered portion 13 are consistent. Exemplarily, in the present application, the heat conductor 25 is preferably a silver core, which has excellent thermal conductivity and can cool the inner core 23 well. The thermal conductivity of the plug 2 is enhanced by the core wrapping method, which is low in cost and does not affect the structural strength of the plug 2.

[0056] See also Figure 2As shown, in some embodiments, the first inlet 41 connected to the outer flow channel 14 is provided with a heat insulation layer 10, and / or the second inlet 51 connected to the inner flow channel 24 is provided with a heat insulation layer 10. In the present application, the heat insulation layer 10 can be a synthetic resin layer, a nano-ceramic layer, etc., and there is no specific limitation. The heat insulation layer 10 can alleviate the temperature rise of the cooling medium in the first inlet 41 and / or the second inlet 51, so that the cooling medium can fully absorb heat and cool the retracted part 1 and / or the plug 2, thereby improving the cooling effect. At the same time, because the first outlet 42 and / or the second outlet 52 are not provided with a heat insulation layer 10, the heated cooling medium can directly contact the top plate 4 and / or the fixed mold seat 5, both of which are made of metal and have a large surface area, and can dissipate the heat of the heated cooling medium, so that it has been cooled once when it flows back to the circulating cooling system 9, thereby reducing the refrigeration energy consumption. The shrink mold can effectively reduce energy consumption and be more energy-saving and environmentally friendly by enhancing the cooling effect on the inlet side and the heat dissipation effect on the outlet side.

[0057] See also Figures 7a to 7d As shown, the present invention also discloses an injection molding method, which adopts any of the above-mentioned shrink molds and includes steps S1 to S5.

[0058] S1, moving the retracted part 1 downward to make it cooperate with the insert 2 to form the injection end of the mold; S2, injecting cooling medium into the inner flow channel 24 and the outer flow channel 14 respectively; S3, mold closing, molding the target product at the injection end of the mold, during which the temperature of the injection end of the mold is monitored and the temperature and flow rate of the cooling medium are adjusted accordingly; S4, mold opening, first control the inner shrinkage part 1 to move upward to decompose the injection end of the mold, and then control the bundle sleeve 3 to move upward to shrink the inner shrinkage part 1, so as to demould the target product; S5. Repeat steps S1, S3 and S4 in sequence to achieve continuous production of the target product.

[0059] In some embodiments, in step S2, the cooling medium is a cooling liquid or a cooling gas. For example, the cooling liquid may be cooling water or cooling oil, etc., and the cooling gas may be nitrogen, carbon dioxide, etc.

[0060] In some embodiments, in step S3, the temperature of the injection end of the mold is maintained at 120°-140°. Too high or too low temperature can easily reduce the yield of the target product, for example, causing it to have a tendency to deteriorate mechanical properties such as warping, cracking, and thermal stability. In the present application, the internal and external collaborative cooling method can be used to make the overall shrink mold have a better cooling effect, and the temperature of the injection end of the mold can also be stabilized at 120°-140°. Within this range, the injection efficiency of the target product is high and the molding yield is good.

[0061] Although the embodiments of the present invention have been shown and described above, it is to be understood that the above embodiments are exemplary and are not to be construed as limitations on the present invention. A person skilled in the art may change, modify, substitute and modify the above embodiments within the scope of the invention without departing from the principles and purpose of the present invention. All such changes should fall within the scope of protection of the claims of the present invention.

Claims

1. A shrink mold, characterized in that: include: The retracted part (1) is arranged on the top plate (4), and an outer flow channel (14) is arranged on the outer periphery of the retracted part (1) for cooling the retracted part (1); The insert core (2) is arranged on the fixed mold base (5) and is slidably matched with the retracted part (1); an inner flow channel (24) is arranged inside the insert core (2) for cooling the insert core (2); A sleeve (3) is arranged on the retractable member (1) and is used to selectively control the retraction or expansion of the retractable member (1); The top plate (4) can move up and down relative to the fixed mold base (5), so that the shrink mold can be switched between an injection state and a demoulding state.

2. The shrink mold according to claim 1, characterized in that: The retracted part (1) and the insert (2) are both made of heat-conducting metal material.

3. The shrink mold according to claim 1, characterized in that: The outer flow channel (14) is located in the top plate (4), and a first inlet (41) and a first outlet (42) communicating with the outer flow channel (14) are provided in the top plate (4).

4. The shrink mold according to claim 3, characterized in that: A first sealing ring (6) is provided between the first inlet (41) and the outer flow channel (14), and between the first outlet (42) and the outer flow channel (14).

5. The shrink mold according to claim 1, characterized in that: The inner flow channel (24) is partially located in the fixed mold base (5), and a second inlet (51) and a second outlet (52) communicating with the inner flow channel (24) are provided in the fixed mold base (5).

6. The shrink mold according to claim 5, characterized in that: A second sealing ring (7) is provided between the second inlet (51) and the external flow channel (14), and between the second outlet (52) and the external flow channel (14).

7. The shrink mold according to claim 5, characterized in that: A flow partition (8) is provided in the inner flow channel (24); one end of the flow partition (8) is sealed with one end of the inner flow channel (24); and a distance is provided between the other end of the flow partition (8) and the other end of the inner flow channel (24).

8. The shrink mold according to claim 1, characterized in that: The retractable component (1) comprises a first seat portion (11), a first connecting portion (12) and a retracting portion (13) which are arranged in sequence from bottom to top; The first seat portion (11) is partially fixed in the top plate (4), the first connecting portion (12) is provided with a convex bump (121), and the gathering portion (13) is provided with a molding feature (131).

9. The shrink mold according to claim 8, characterized in that: A heat-conducting layer (15) is provided on the surface of the molding feature (131), the heat-conducting layer (15) extends to the outer flow channel (14), and the heat conductivity of the material of the heat-conducting layer (15) is greater than the heat conductivity of the material of the shrinking part (1).

10. The shrink mold according to claim 1, characterized in that: The insert (2) comprises a second seat portion (21), a second connecting portion (22) and an inner core portion (23) which are arranged in sequence from bottom to top; Wherein, the second seat portion (21) is partially fixed in the fixed mold seat (5), and the inner core portion (23) corresponds to and matches the gathering portion (13).

11. The shrink mold according to claim 10, characterized in that: The inner flow channel (24) is located in the second seat portion (21), a heat conductor (25) is arranged in the inner core portion (23), the heat conductor (25) extends to the inner flow channel (24), and the thermal conductivity of the material of the heat conductor (25) is greater than the thermal conductivity of the material of the insert (2).

12. The shrink mold according to claim 1, characterized in that: It also includes a circulating cooling system (9), wherein the circulating cooling system (9) connects the inner flow channel (24) and the outer flow channel (14), and the temperature and flow rate of the cooling medium output by the circulating cooling system (9) are adjustable.

13. The shrink mold according to claim 12, characterized in that: The first inlet (41) connected to the outer flow channel (14) is provided with a heat insulation layer (10), and / or the second inlet (51) connected to the inner flow channel (24) is provided with a heat insulation layer (10).

14. An injection molding method, characterized in that: The shrink mold according to any one of claims 1 to 13 is used, comprising the following steps: S1, moving the retracted part (1) downward so that it cooperates with the insert (2) to form an injection molding end of the mold; S2, injecting cooling medium into the inner flow channel (24) and the outer flow channel (14) respectively; S3, mold closing, molding the target product at the injection end of the mold, during which the temperature of the injection end of the mold is monitored and the temperature and flow rate of the cooling medium are adjusted accordingly; S4, opening the mold, first controlling the inner shrinkage part (1) to move upward to disassemble the injection end of the mold, and then controlling the sleeve (3) to move upward to shrink the inner shrinkage part (1), thereby demoulding the target product; S5. Repeat steps S1, S3 and S4 in sequence to achieve continuous production of the target product.

15. The injection molding method according to claim 14, characterized in that: In the step S2, the cooling medium is cooling liquid or cooling gas.

16. The injection molding method according to claim 14, characterized in that: In step S3, the temperature of the injection end of the mold is maintained at 120°-140°.