Method for removing reaction by-products

By stabilizing the etching chamber environment after etching and increasing the electrostatic suction cup temperature, combined with helium sweeping technology, the insufficient charge release and wafer defects caused by the accumulation of reaction by-products is solved, and the product yield and stability are improved .

CN118919449APending Publication Date: 2024-11-08HUA HONG SEMICON WUXI LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411003334.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-24
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

During the manufacturing process of semiconductor devices and integrated circuits, reaction by-products generated during etching are easily accumulated on the electrostatic suction cup, resulting in insufficient charge release, increasing the risk of wafer scratches and debris, and may fall on the wafer surface. Defects, reduce product yield.

Method used

Plasma ignition is performed by stabilizing the pressure and gas flow of the etching chamber within a preset range after etching, increasing the electrostatic suction cup temperature and helium flow to remove reaction by-products, and preventing by-products from blowing through helium sweep Scan to the front of the wafer to ensure the stability of the charge release and wafer transfer process.

Benefits of technology

Effectively remove reaction by-products on wafers and electrostatic suction cups, reduce product defect rate, improve product yield, and reduce the risk of wafer position offset and scratches.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118919449A_ABST
    Figure CN118919449A_ABST
Patent Text Reader

Abstract

The invention discloses a method for removing reaction by-products, and the method is used for etching a wafer, and then the wafer is used for manufacturing a semiconductor device product. The method comprises the following steps: stabilizing the pressure in an etching chamber of an etching machine table within a preset pressure range and stabilizing the gas flow in the etching chamber within a preset flow range; performing plasma ignition; removing reaction by-products on the back surface of the wafer by increasing the temperature of the electrostatic chuck and increasing the flow of helium; performing charge release to enable the wafer not to be adsorbed on the electrostatic chuck any more; the wafer is jacked up through an ejector pin, reaction by-products on the back face of the wafer are flushed through helium, and the flow of argon above the wafer is kept within a preset flow range for preset time; and grabbing the wafer through a mechanical arm and conveying the wafer to a wafer box. According to the invention, reaction byproducts on the wafer and the electrostatic chuck can be effectively removed, the defect rate of products is reduced, and the product yield is improved to a certain extent.