Gallium nitride device with improved linearity and preparation method thereof

By designing a dual-crystalline gallium nitride device with a V-shaped structure on the m-crystal plane GaN, the nonlinearity problem of gallium nitride devices in high-frequency applications is solved, and higher linearity and signal fidelity are achieved, avoiding the etching damage reduces epitaxial design costs.

CN118919562AActive Publication Date: 2024-11-08SOUTHERN UNIVERSITY OF SCIENCE AND TECHNOLOGY +1
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202410441529.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-04-12
Publication Date
2024-11-08
Estimated Expiration
2044-04-12

AI Technical Summary

Technical Problem

Existing GaN high-electron mobility field effect tube devices have nonlinear problems in high-frequency and high-power applications, resulting in spectrum leakage, premature output power saturation and signal distortion, and existing methods to improve linearity usually require complexity. The epitaxial structure design or etching process increases costs and may introduce etching damage.

Method used

By preparing bi-crystalline gallium nitride devices on m-crystalline GaN, using V-shaped structure and multi-layer barrier layer design, a dual-crystalline channel is formed, transconductance flatness modulation is achieved, and the linearity of the device is improved, and the linearity of the device is avoided. The damage introduced by barrier layer etching is performed.

Benefits of technology

It achieves higher linearity, reduces epitaxial design costs, improves the signal transmission fidelity of the device in RF applications, and avoids the problem of nonlinear distortion.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118919562A_ABST
    Figure CN118919562A_ABST
Patent Text Reader

Abstract

The invention discloses a gallium nitride device with improved linearity. The gallium nitride device with improved linearity comprises an electrode extension part, a V-shaped structure and a substrate structure from top to bottom. According to the gallium nitride device with the improved linearity, the transconductance flatness modulation of the device can be realized by utilizing the property that the mobility of double crystal orientations is different from the concentration of two-dimensional electron gas, so that the higher linearity is realized; specifically, high linearity can be realized by directly extending a conventional AlxGa1-xN / GaN heterojunction on an m crystal face GaN epitaxial wafer and then preparing a gallium nitride device with double crystal orientation channels, and a special epitaxial structure is not needed, so that the cost of epitaxial design is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of semiconductor devices, and in particular to a gallium nitride device with improved linearity and a preparation method thereof. Background Art

[0002] With the continuous development of the wireless communication market and the progress in the military and defense fields, the requirements for the performance of microwave power devices are also increasing, which has promoted the rapid development of microwave power devices. Third-generation semiconductor materials, such as gallium nitride (GaN) and silicon carbide (SiC), play an important role in this process and show excellent high-power application characteristics. Gallium nitride (GaN) has excellent physical properties such as large bandgap, high electron saturation rate, high voltage resistance, high temperature resistance and good thermal stability. It is considered to be an ideal material for applications in high voltage, high frequency, high temperature and radiation resistance. In the fields of optoelectronics, high-temperature high-power devices and RF microwave device applications, gallium nitride has broad prospects.

[0003] The transconductance (G m ) with gate voltage (V gs ) The change curve is as shown in the attached Figure 1 As shown, with V gs Increase, G m It will rise first and then fall. m ) represents the relationship between the change in output current and the change in input voltage. The nonlinear nature of the power amplifier (PA) leads to a series of problems, such as spectrum leakage, premature saturation of output power, and signal distortion. These problems not only affect system performance, but also increase the difficulty of system design. In addition, in the process of audio and video file transmission in the field of wireless communication, the nonlinearity of PA will cause distortion of sound and image information. In order to obtain better signal transmission fidelity, GaN devices are required to have high linearity.

[0004] The method to improve the linearity of GaN devices is generally to design a more complex epitaxial structure or to etch the device structure to achieve a special structure. The former solution has higher requirements for device epitaxy and the cost will also increase, while the latter solution uses etching to achieve the structure. Etching will introduce more etching damage and other problems, thus affecting the reliability and yield of the device, and the process technology is also more complicated.

[0005] In the prior art, the patent document CN111969046A discloses a high linearity enhanced gallium nitride high electron mobility transistor and a preparation method thereof, which realizes the depletion of the two-dimensional electron gas of the group III nitride heterojunction by the p-type group III nitride region by providing a nanochannel strip structure under the gate electrode, thereby improving the flatness and linearity of the transistor's transconductance curve. The method relies on an inductively coupled plasma etching process (ICP) to etch the barrier layer, which causes a large amount of etching damage in the barrier layer region, thereby reducing the performance of the device.

[0006] Patent document CN101488457A discloses a method for improving the linearity of a gallium nitride high electron mobility transistor by x Ga 1-x Insert an Al layer between N / GaN heterojunction y Ga 1-y N insertion layer, forming AlxGa 1-x N / AlyGa 1-y N / GaN. By optimizing the barrier layer Al x Ga 1-x The thickness of N and the value of Al component x can make Al x Ga 1-x N / A y Ga 1-y The lateral electric field ET in the 2DEG formed between N is reduced to a moderate value, thereby obtaining the maximum linearity of the device; this method requires the design of a more complex epitaxial structure, so the quality requirements for the device epitaxial structure are higher and the manufacturing cost is higher.

[0007] Therefore, it is urgent to develop a gallium nitride device to solve the above problems. Summary of the invention

[0008] Based on the defects and shortcomings of the prior art, the present invention provides a gallium nitride device with improved linearity. By utilizing the different properties of the mobility of the dual crystal directions and the two-dimensional electron gas (2DEG) concentration, the transconductance flatness modulation of the device can be realized, thereby achieving higher linearity while avoiding the etching damage introduced by the barrier layer etching. Specifically, the present invention directly epitaxies conventional Al on the m-plane GaN. x Ga 1-x The N / GaN heterojunction and then the preparation of a dual-channel GaN device can achieve high linearity without the need for a special epitaxial structure, thereby reducing the cost of epitaxial design.

[0009] In the present invention, linearity refers to the degree of change of the output signal of a device when the input signal changes.

[0010] An object of the present invention is to provide a gallium nitride device with improved linearity, wherein the gallium nitride device with improved linearity comprises the following structures from top to bottom: an electrode extension portion, a V-shaped structure and a substrate structure;

[0011] in

[0012] Base structure: The base structure includes a buffer layer and a substrate from top to bottom;

[0013] The buffer layer includes a second buffer layer and a first buffer layer from top to bottom;

[0014] V-shaped structure: the V-shaped structure is arranged on the first buffer layer, the V-shaped structure is a multilayer structure with a V-shaped cross-section, and the V-shaped structure comprises an electrode layer, a barrier layer and a second buffer layer from top to bottom;

[0015] The second buffer layer is an extension of the first buffer layer on the V-shaped structure;

[0016] The entire surface of the electrode layer of the V-shaped structure and the outer side of the second buffer layer are covered with Si 3 N 4 Covered by the formed passivation layer;

[0017] The electrode layer is composed of a source electrode, a drain electrode and a gate electrode, wherein

[0018] The gate is deposited at the center of the V-shaped structure, the source and drain are deposited at both ends of the V-shaped structure, and there are gaps between the source and drain and the gate;

[0019] Electrode extension portion: The source, drain and gate are partially extended upward from the device to form electrode extension portions of the source, drain and gate, respectively.

[0020] Furthermore, materials of the first buffer layer and the second buffer layer are both m-plane GaN materials.

[0021] Furthermore, the length of the source-gate gap between the source electrode and one end of the adjacent gate electrode is 1-3 um.

[0022] Furthermore, the length of the drain-gate gap between the drain electrode and one end of the adjacent gate electrode is 3-6 um.

[0023] Furthermore, the length of the drain-gate gap is greater than the length of the source-gate gap.

[0024] Furthermore, the material of the substrate is selected from one or more of silicon, sapphire, silicon carbide, and diamond.

[0025] Furthermore, the gate, source and drain are independently multi-layer metal electrodes, and the material of the multi-layer metal electrode, each layer is independently selected from one or more of gold, aluminum, titanium, silver, copper, platinum and nickel.

[0026] Furthermore, the barrier layer material is Al x Ga 1-x N material, wherein the value range of X is 0.2-0.34.

[0027] The present invention also provides a method for preparing the gallium nitride device with improved linearity, and the method for preparing the gallium nitride device with improved linearity comprises the following steps:

[0028] S1. preparing a substrate with a multilayer structure, wherein the substrate with the multilayer structure comprises a barrier layer, a buffer layer and a substrate from top to bottom;

[0029] S2, etching the substrate to etch the barrier layer and a portion of the buffer layer into a V-shaped structure, so that the buffer layer is etched into a first buffer layer located in the substrate structure and a second buffer layer located in the V-shaped structure;

[0030] S3, depositing a gate, a source and a drain on the barrier layer of the V-shaped structure respectively to form an electrode layer;

[0031] S4, on the outer surface of the electrode layer and part of the first buffer layer, Si 3 N 4 Passivation treatment and control of Si 3 N 4 The thickness of the passivation layer is formed;

[0032] S5, etching the interconnection through holes between the passivation layer and the source, drain and gate, and completing the preparation of the electrode extension parts of the source, drain and gate.

[0033] Furthermore, the thickness of the passivation layer is 100-300 nm.

[0034] Furthermore, in the V-shaped structure, the angle between the two sides is 60-80°.

[0035] Furthermore, the passivation layer is prepared by a CVD process.

[0036] Furthermore, the gate, source, drain and the barrier layer form an ohmic contact.

[0037] The beneficial effects of the present invention are as follows:

[0038] 1. This structure can make the GaN device achieve better transconductance flatness, thereby achieving higher linearity. The improved linearity of the GaN RF device means that within its operating range, the device's response is closer to the linear relationship of the input signal. Higher linearity usually means that the device can more accurately and reliably maintain the original shape of the signal when processing complex RF signals without introducing nonlinear distortion.

[0039] 2. Surprisingly, it was found that the method requires the preparation of GaN devices with a specific crystal orientation angle on the m-plane GaN epitaxial wafer. However, the two-dimensional electron gas density and electron mobility on the GaN epitaxial wafers with other polar planes, such as the Ga plane, do not change significantly with the crystal orientation. Therefore, the dual-crystal orientation channel device on the polar plane GaN cannot achieve improved linearity. However, the present invention can make the GaN device have better transconductance flatness by arranging a barrier layer and a second buffer layer with a V-shaped structure on the m-plane GaN epitaxial wafer, thereby achieving higher linearity. When the angle of the V-shaped structure is 60°, the difference in the two-dimensional electron gas density and the electron mobility between the two crystal orientations is the largest. The preparation of the GaN device with a dual-crystal orientation channel can achieve the maximum device linearity. BRIEF DESCRIPTION OF THE DRAWINGS

[0040] Figure 1 In the background technology, the transconductance (G m ) with gate voltage (V gs ) Schematic diagram of the change curve;

[0041] FIG2(a)-(f) are schematic flow diagrams of a method for preparing a gallium nitride device with improved linearity in Examples 1-3;

[0042] Figure 3 is a schematic diagram of a gallium nitride device proposed in Comparative Example 1;

[0043] In the figure: 1. source; 2. drain; 3. gate; 4. passivation layer (covering the surface); 5. barrier layer; 6. buffer layer; 61. first buffer layer; 62. second buffer layer; 7. substrate. DETAILED DESCRIPTION

[0044] In order to more clearly illustrate the technical solution of the present invention, the following examples are listed. Unless otherwise stated, the raw materials, reactions and post-treatment methods shown in the examples are common raw materials on the market and technical methods well known to those skilled in the art.

[0045] The words "preferred", "preferably", "more preferably", etc. in the present invention refer to embodiments of the present invention that can provide certain beneficial effects in certain circumstances. However, other embodiments may also be preferred under the same circumstances or other circumstances. In addition, the description of one or more preferred embodiments does not imply that other embodiments are not applicable, nor is it intended to exclude other embodiments from the scope of the present invention.

[0046] It should be understood that, except in any operating examples, or where otherwise indicated, all numbers expressing, for example, the amounts of ingredients used in the specification and claims should be understood to be modified in all instances by the term "about". Therefore, unless indicated to the contrary, the numerical parameters set forth in the following specification and the appended claims are approximate values ​​that vary depending on the desired properties to be obtained by the present invention.

[0047] The m crystal plane is a type of specific crystal plane in the hexagonal crystal system. For details, please refer to "Nitride Wide Bandgap Semiconductor Materials and Electronic Devices", author: Hao Yue, publisher: Science Press, page 20.

[0048] Example 1

[0049] A gallium nitride device with improved linearity, the structure of the gallium nitride device with improved linearity is shown in FIG. 2( a ) to ( f ), an electrode extension portion, a V-shaped structure and a substrate structure;

[0050] in

[0051] Substrate structure: The substrate structure includes, from top to bottom, a buffer layer 6 (1000 nm) of m-plane GaN and a sapphire substrate 7 (650 μm);

[0052] The buffer layer 6 includes a second buffer layer 62 (100 nm) and a first buffer layer 61 (900 nm) from top to bottom;

[0053] V-shaped structure: The V-shaped structure is arranged on the first buffer layer 61. The V-shaped structure is a multilayer structure with a V-shaped cross-section (the angle is 60°). The V-shaped structure is composed of an electrode layer, an Al 0.25 Ga 0.75 N barrier layer 5 (20 nm) and second buffer layer 62 (100 nm);

[0054] The second buffer layer 62 is an extension of the first buffer layer 61 on the V-shaped structure, and this special shape is achieved by the following etching;

[0055] The entire surface of the V-shaped electrode layer and the outer side of the second buffer layer 62 are covered with Si 3 N 4The formed passivation layer 4 is covered (100 nm);

[0056] The electrode layer is composed of a source electrode 1, a drain electrode 2 and a gate electrode 3.

[0057] The gate 3 is deposited at the center of the V-shaped structure, the source 1 and the drain 2 are deposited at the two ends of the V-shaped structure, and there are gaps between the source 1 and the drain 2 and the gate 3. 3 N 4 The formed passivation layer 4 is filled;

[0058] Electrode extension part: The source 1, drain 2 and gate 3 are partially extended upwards of the device to form electrode extension parts of the source 1, drain 2 and gate 3. The electrode extension part formed can be specifically divided into two parts. The first part is a columnar structure (height of 100nm) extending from the electrode layer for support, and a metal plate (area of ​​80um*80um) of a planar structure extending horizontally from each columnar structure part for needle puncture test.

[0059] The method for preparing the gallium nitride device with improved linearity is as follows, and the related drawings are as follows: Figure 2(a)-2(f) shown.

[0060] S1, prepare a multi-layer structure substrate, the multi-layer structure epitaxial wafer is Al 0.25 Ga 0.75 N barrier layer 5 (20 nm), m-plane GaN buffer layer 6 (1000 nm) and sapphire substrate 7 (650 μm), as shown in FIG2(a);

[0061] S2, using ICP process to etch the upper part of the barrier layer 5 and the buffer layer 6 to form a columnar V-shaped structure (including the etched barrier layer 5 and the second buffer layer 62); in the V-shaped structure, an active area of ​​a dual crystal channel can be formed. It should be noted that in order to ensure the device isolation effect, the two-dimensional electron gas in the non-active area of ​​the device needs to be completely cut off, because the barrier layer 5 in the non-active area needs to be completely etched, and the upper part of the buffer layer 6 is etched to form a second buffer layer 62 (100nm), and the unetched part forms a first buffer layer 61 (900nm), as shown in Figure 2 (b);

[0062] S3. Ti / Al / Ti / Au (20nm / 110nm / 40nm / 50nm) is deposited on one end of the V-shaped barrier layer 5 as the source 1, and Ti / Al / Ti / Au (20nm / 110nm / 40nm / 50nm) is deposited on the other end as the drain 2 using an electron beam evaporation device, and then rapidly thermally annealed at 830°C for 45s to form an ohmic contact, thereby obtaining the source 1 and the drain 2, as shown in FIG2(c);

[0063] S4, at the center point of the V-shape, the gate length is designed to be 250nm, and then the gate 3 metal Ni / Au (20nm / 130nm) is deposited by electron beam evaporation equipment to obtain the gate 3. The shape of the gate 3 is a small V-shape, and the angle between the two sides is also 60°, and there is a gap between the source 1 and the drain 2, as shown in Figure 2(d);

[0064] The length of the source-gate gap between the source electrode 1 and one end of the adjacent gate electrode 3 is 2 um; the length of the drain-gate gap between the drain electrode 2 and one end of the adjacent gate electrode 3 is 4 um;

[0065] S5, using CVD process to perform surface Si on the barrier layer 5 3 N 4 The passivation layer 4 is grown to fill the gaps and wrap the electrode layer on the surface, and its surface thickness is controlled to be 100 nm;

[0066] Surface Si is performed on the first buffer layer 61 3 N 4 The growth of the passivation layer 4 is controlled to have a surface thickness of 100 nm, so that the outer side of the second buffer layer 62 is covered with Si 3 N 4 The formed passivation layer 4 is covered, as shown in FIG2(e);

[0067] S6. The passivation layer 4 on the surface of the barrier layer 5 is etched with a photolithography machine and an ICP process to form gate-source-drain electrode interconnection through holes, the etching depth of the through holes being 100 nm, and then Ni / Au (20 nm / 180 nm) is deposited using an electron beam evaporation device to form a columnar structure with a height of 100 nm, and a Ni / Au (20 nm / 180 nm) metal plate (with an area of ​​80 um*80 um) is formed to obtain the gallium nitride device with improved linearity, as shown in FIG2(f).

[0068] Example 2

[0069] A gallium nitride device with improved linearity, the structure of the gallium nitride device with improved linearity is shown in FIG. 2( a ) to ( f ), an electrode extension portion, a V-shaped structure and a substrate structure;

[0070] in

[0071] Substrate structure: The substrate structure includes, from top to bottom, a buffer layer 6 (1000 nm) of GaN of the m-crystal plane and a sapphire substrate 7 (650 μm);

[0072] The buffer layer 6 includes a second buffer layer 62 (100 nm) and a first buffer layer 61 (900 nm) from top to bottom;

[0073] V-shaped structure: The V-shaped structure is arranged on the first buffer layer 61. The V-shaped structure is a multilayer structure with a V-shaped cross-section (the angle is 60°). The V-shaped structure is composed of an electrode layer, an Al 0.25 Ga 0.75 N barrier layer 5 (10 nm) and second buffer layer 62 (100 nm);

[0074] The second buffer layer 62 is an extension of the first buffer layer 61 on the V-shaped structure, and this special shape is achieved by the following etching;

[0075] The entire surface of the V-shaped electrode layer and the outer side of the second buffer layer 62 are covered with Si 3 N 4 The formed passivation layer 4 is covered (100 nm);

[0076] The electrode layer is composed of a source electrode 1, a drain electrode 2 and a gate electrode 3.

[0077] The gate 3 is deposited at the center of the V-shaped structure, the source 1 and the drain 2 are deposited at the two ends of the V-shaped structure, and there are gaps between the source 1 and the drain 2 and the gate 3. 3 N 4 The formed passivation layer 4 is filled;

[0078] Electrode extension part: The source 1, drain 2 and gate 3 are partially extended upwards of the device to form electrode extension parts of the source 1, drain 2 and gate 3. The electrode extension part formed can be specifically divided into two parts. The first part is a columnar structure (height of 100nm) extending from the electrode layer for support, and a metal plate (area of ​​80um*80um) of a planar structure extending horizontally from each columnar structure part for needle puncture test.

[0079] The method for preparing the gallium nitride device with improved linearity is as follows, and the related drawings are as follows: Figure 2(a)-2(f) shown.

[0080] S1, prepare a multi-layer structure substrate, the multi-layer structure epitaxial wafer is Al 0.25 Ga 0.75 N barrier layer 5 (10 nm), m-plane GaN buffer layer 6 (1000 nm) and sapphire substrate 7 (650 μm), as shown in FIG2(a);

[0081] S2, using ICP process to etch the upper part of the barrier layer 5 and the buffer layer 6 to form a columnar V-shaped structure (including the etched barrier layer 5 and the second buffer layer 62); in the V-shaped structure, an active area of ​​a dual crystal channel can be formed. It should be noted that in order to ensure the device isolation effect, the two-dimensional electron gas in the non-active area of ​​the device needs to be completely cut off, because the barrier layer 5 in the non-active area needs to be completely etched, and the upper part of the buffer layer 6 is etched to form a second buffer layer 62 (100nm), and the unetched part forms a first buffer layer 61 (900nm), as shown in Figure 2 (b);

[0082] S3. Ti / Al / Ti / Au (20nm / 110nm / 40nm / 50nm) is deposited on one end of the V-shaped barrier layer 5 as the source 1, and Ti / Al / Ti / Au (20nm / 110nm / 40nm / 50nm) is deposited on the other end as the drain 2 using an electron beam evaporation device, and then rapidly thermally annealed at 830°C for 45s to form an ohmic contact, thereby obtaining the source 1 and the drain 2, as shown in FIG2(c);

[0083] S4, at the center point of the V-shape, the gate length is designed to be 250nm, and then the gate 3 metal Ni / Au (20nm / 130nm) is deposited by electron beam evaporation equipment to obtain the gate 3. The shape of the gate 3 is a small V-shape, and the angle between the two sides is also 60°, and there is a gap between the source 1 and the drain 2, as shown in Figure 2(d);

[0084] The length of the source-gate gap between the source electrode 1 and one end of the adjacent gate electrode 3 is 2 um; the length of the drain-gate gap between the drain electrode 2 and one end of the adjacent gate electrode 3 is 4 um;

[0085] S5, using CVD process to perform surface Si on the barrier layer 5 3 N 4 The passivation layer 4 is grown to fill the gaps and wrap the electrode layer on the surface, and its surface thickness is controlled to be 100 nm;

[0086] Surface Si is performed on the first buffer layer 61 3 N 4 The growth of the passivation layer 4 is controlled to have a surface thickness of 100 nm, so that the outer side of the second buffer layer 62 is covered with Si 3 N 4 The formed passivation layer 4 is covered, as shown in FIG2(e);

[0087] S6. The passivation layer 4 on the surface of the barrier layer 5 is etched with a photolithography machine and an ICP process to form gate-source-drain electrode interconnection through holes, the etching depth of the through holes being 100 nm, and then Ni / Au (20 nm / 180 nm) is deposited using an electron beam evaporation device to form a columnar structure with a height of 100 nm, and a Ni / Au (20 nm / 180 nm) metal plate (with an area of ​​80 um*80 um) is formed to obtain the gallium nitride device with improved linearity, as shown in FIG2(f).

[0088] Example 3

[0089] A gallium nitride device with improved linearity, the structure of the gallium nitride device with improved linearity is shown in FIG. 2( a ) to ( f ), an electrode extension portion, a V-shaped structure and a substrate structure;

[0090] in

[0091] Substrate structure: The substrate structure includes, from top to bottom, a buffer layer 6 (1000 nm) of m-plane GaN and a sapphire substrate 7 (650 μm);

[0092] The buffer layer 6 includes a second buffer layer 62 (100 nm) and a first buffer layer 61 (900 nm) from top to bottom;

[0093] V-shaped structure: The V-shaped structure is arranged on the first buffer layer 61 of the base structure. The V-shaped structure is a multilayer structure with a V-shaped cross-section (the angle is 60°). The V-shaped structure is composed of an electrode layer, an Al 0.2 Ga 0.8 N barrier layer 5 (20 nm) and second buffer layer 62 (100 nm);

[0094] The second buffer layer 62 is an extension of the first buffer layer 61 on the V-shaped structure, and this special shape is achieved by the following etching;

[0095] The entire surface of the V-shaped electrode layer and the outer side of the second buffer layer 62 are covered with Si 3 N 4 The formed passivation layer 4 is covered (100 nm);

[0096] The electrode layer is composed of a source electrode 1, a drain electrode 2 and a gate electrode 3.

[0097] The gate 3 is deposited at the center of the V-shaped structure, the source 1 and the drain 2 are deposited at the two ends of the V-shaped structure, and there are gaps between the source 1 and the drain 2 and the gate 3. 3 N 4 The formed passivation layer 4 is filled;

[0098] Electrode extension part: The source 1, drain 2 and gate 3 are partially extended upwards of the device to form electrode extension parts of the source 1, drain 2 and gate 3. The electrode extension part formed can be specifically divided into two parts. The first part is a columnar structure (height of 100nm) extending from the electrode layer for support, and a metal plate (area of ​​80um*80um) of a planar structure extending horizontally from each columnar structure part for needle puncture test.

[0099] The method for preparing the gallium nitride device with improved linearity is as follows, and the related drawings are as follows: Figure 2(a)-2(f) shown.

[0100] S1, prepare a multi-layer structure substrate, the multi-layer structure epitaxial wafer is Al 0.2 Ga 0.8 N barrier layer 5 (20 nm), buffer layer 6 (1000 nm) and sapphire substrate 7 (650 μm), as shown in FIG2( a );

[0101] S2, using ICP process to etch the upper part of the barrier layer 5 and the buffer layer 6 to form a columnar V-shaped structure (including the etched barrier layer 5 and the second buffer layer 62); in the V-shaped structure, an active area of ​​a dual crystal channel can be formed. It should be noted that in order to ensure the device isolation effect, the two-dimensional electron gas in the non-active area of ​​the device needs to be completely cut off, because the barrier layer 5 in the non-active area needs to be completely etched, and the upper part of the buffer layer 6 is etched to form a second buffer layer 62 (100nm), and the unetched part forms a first buffer layer 61 (900nm), as shown in Figure 2 (b);

[0102] S3. Ti / Al / Ti / Au (20nm / 110nm / 40nm / 50nm) is deposited on one end of the V-shaped barrier layer 5 as the source 1, and Ti / Al / Ti / Au (20nm / 110nm / 40nm / 50nm) is deposited on the other end as the drain 2 using an electron beam evaporation device, and then rapidly thermally annealed at 830°C for 45s to form an ohmic contact, thereby obtaining the source 1 and the drain 2, as shown in FIG2(c);

[0103] S4, at the center point of the V-shape, the gate length is designed to be 250nm, and then the gate 3 metal Ni / Au (20nm / 130nm) is deposited by electron beam evaporation equipment to obtain the gate 3. The shape of the gate 3 is a small V-shape, and the angle between the two sides is also 60°, and there is a gap between the source 1 and the drain 2, as shown in Figure 2(d);

[0104] The length of the source-gate gap between the source electrode 1 and one end of the adjacent gate electrode 3 is 2 um; the length of the drain-gate gap between the drain electrode 2 and one end of the adjacent gate electrode 3 is 4 um;

[0105] S5, using CVD process to perform surface Si on the barrier layer 5 3 N 4 The passivation layer 4 is grown to fill the gaps and wrap the electrode layer on the surface, and its surface thickness is controlled to be 100 nm;

[0106] Surface Si is performed on the first buffer layer 61 3 N 4 The growth of the passivation layer 4 is controlled to have a surface thickness of 100 nm, so that the outer side of the second buffer layer 62 is covered with Si 3 N 4 The formed passivation layer 4 is covered, as shown in FIG2(e);

[0107] S6. The passivation layer 4 on the surface of the barrier layer 5 is etched with a photolithography machine and an ICP process to form gate-source-drain electrode interconnection through holes, the etching depth of the through holes being 100 nm, and then Ni / Au (20 nm / 180 nm) is deposited using an electron beam evaporation device to form a columnar structure with a height of 100 nm, and a Ni / Au (20 nm / 180 nm) metal plate (with an area of ​​80 um*80 um) is formed to obtain the gallium nitride device with improved linearity, as shown in FIG2(f).

[0108] Comparative Example 1

[0109] A gallium nitride device, the structure of the gallium nitride device is as follows Figure 3 As shown, the conventional gallium nitride device comprises the following structures from top to bottom: an electrode extension portion, a substrate structure;

[0110] in

[0111] Substrate structure: The substrate structure includes, from top to bottom, a passivation layer 4 (100 nm), an electrode layer, a barrier layer 5 (20 nm), a buffer layer 6 (1000 nm); and a substrate 7 (650 μm);

[0112] The buffer layer 6 includes a second buffer layer 62 (100 nm) and a first buffer layer 61 (900 nm) from top to bottom;

[0113] The electrode layer is composed of a source electrode 1, a drain electrode 2 and a gate electrode 3;

[0114] Electrode extension portion: the source electrode 1 , the drain electrode 2 and the gate electrode 3 are partially extended upward of the device to form electrode extension portions of the source electrode 1 , the drain electrode 2 and the gate electrode 3 , respectively.

[0115] The substrate 7 is Si; the passivation layer 4 is Si 3 N 4 Material; the barrier layer 5 is Al0.25 Ga 0.75 N; the materials of the first buffer layer 61 and the second buffer layer 62 are GaN.

[0116] The conventional method for preparing the gallium nitride device is as follows:

[0117] S1. Soak the GaN epitaxial wafer in acetone for 10 minutes, then take it out and soak it in isopropanol solution for 5 minutes, then wash it in deionized water for 3 minutes, and finally blow it dry with a nitrogen gun to obtain a clean GaN epitaxial wafer, completing the process preparation;

[0118] S1. Using ICP process, grooves are etched on both sides of the GaN epitaxial wafer to form a second buffer layer 62 and a barrier layer 5 of the columnar body to achieve electrical isolation between devices, and the etching depth is 120nm;

[0119] S2. Ti / Al / Ti / Au (20nm / 110nm / 40nm / 50nm) is deposited on the barrier layer 5 using an electron beam evaporation device as the material of the source 1 and the drain 2, and then rapidly thermally annealed at 830°C for 45s to form an ohmic contact to obtain the source 1 and the drain 2;

[0120] S3. The gate region is exposed using an electron beam exposure machine (EBL) process, and the gate length is designed to be 250 nm. Then, gate metal Ni / Au (20 nm / 130 nm) is deposited between the source electrode 1 and the drain electrode 2 using an electron beam evaporation device to obtain a gate 3;

[0121] S4. Surface Si is formed on the first buffer layer 61 by CVD process. 3 N 4 The growth of the passivation layer 4 controls its surface thickness to be 100 nm;

[0122] Surface Si is performed on the barrier layer 5 3 N 4 The passivation layer 4 is grown to fill the gaps and wrap the electrode layer on the surface, and its surface thickness is controlled to be 100 nm;

[0123] S5. Use a photolithography machine and ICP process to etch the interconnection through holes of the source, drain and gate electrodes on the passivation layer 4 on the surface of the barrier layer 5, and then use electron beam evaporation equipment to deposit Ni / Au (20nm / 150nm) to form the electrode extension parts of the source, drain and gate electrodes to obtain the conventional gallium nitride device.

[0124] Test Example 1

[0125] The gallium nitride devices of Example 1 and Comparative Example 1 were tested for transfer characteristic curves.

[0126] Test method: Set the source-drain voltage Vds =1V, the transfer characteristic curves of the gallium nitride devices of Example 1 and Comparative Example 1 were tested.

[0127] Among them, the gate-voltage-swing (GVS) figure of merit is a physical quantity that characterizes linearity. It is specifically defined as the gate voltage swing range that maintains the transconductance at 80% of the transconductance peak value in the transfer characteristic curve. The larger the GVS, the higher the transconductance flatness, that is, the better the device linearity.

[0128] The test results are shown in Table 1.

[0129] Table 1 Performance test results of gallium nitride devices of Example 1 and Comparative Example 1

[0130] Threshold voltage (V) Maximum transconductance (mS / mm) Gate voltage swing figure of merit (V) Example 1 -4.12 391 5.9 Comparative Example 1 -5.86 445 3.8

[0131] According to the test results in Table 1, the gate voltage swing of the gallium nitride device of Example 1 is significantly higher than that of the device of Comparative Example 1, and the linearity of the device of Example 1 is better.

[0132] It will be apparent to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above and that the present invention can be implemented in other specific forms without departing from the spirit or essential features of the present invention. Therefore, the embodiments should be considered exemplary and non-restrictive in all respects, and the scope of the present invention is defined by the appended claims rather than the above description, and it is intended that all changes falling within the meaning and scope of the equivalent elements of the claims be included in the present invention.

[0133] In addition, it should be understood that although the present specification is described according to implementation modes, not every implementation mode contains only one independent technical solution. This description of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment may also be appropriately combined to form other implementation modes that can be understood by those skilled in the art.

Claims

1. A gallium nitride device with improved linearity, characterized in that: The gallium nitride device with improved linearity comprises the following structures from top to bottom: an electrode extension portion, a V-shaped structure and a substrate structure; in Base structure: The base structure includes a buffer layer and a substrate from top to bottom; The buffer layer includes a second buffer layer and a first buffer layer from top to bottom; V-shaped structure: the V-shaped structure is arranged on the first buffer layer, the V-shaped structure is a multilayer structure with a V-shaped cross-section, and the V-shaped structure comprises an electrode layer, a barrier layer and a second buffer layer from top to bottom; The second buffer layer is an extension of the first buffer layer on the V-shaped structure; The entire surface of the electrode layer of the V-shaped structure and the outer side of the second buffer layer are covered by a passivation layer formed by Si3N4; The electrode layer is composed of a source electrode, a drain electrode and a gate electrode, wherein The gate is deposited at the center of the V-shaped structure, the source and drain are deposited at both ends of the V-shaped structure, and there are gaps between the source and drain and the gate; Electrode extension portion: The source, drain and gate are partially extended upward from the device to form electrode extension portions of the source, drain and gate, respectively.

2. The gallium nitride device with improved linearity according to claim 1, characterized in that: The materials of the first buffer layer and the second buffer layer are both m-plane GaN materials.

3. The gallium nitride device with improved linearity according to claim 1, characterized in that: The length of the source-gate gap between the source electrode and one end of the adjacent gate electrode is 1-3 um.

4. The gallium nitride device with improved linearity according to claim 3, characterized in that: The length of the drain-gate gap between the drain electrode and one end of the adjacent gate electrode is 3-6 um.

5. The gallium nitride device with improved linearity according to claim 4, characterized in that: The length of the drain-gate gap is greater than the length of the source-gate gap.

6. The gallium nitride device with improved linearity according to claim 1, characterized in that: The barrier layer material is Al x Ga 1-x N material, wherein the value range of X is 0.2-0.

34.

7. The method for preparing a gallium nitride device with improved linearity according to any one of claims 1 to 6, characterized in that: The method for preparing the gallium nitride device with improved linearity comprises the following steps: S1. preparing a substrate with a multilayer structure, wherein the substrate with the multilayer structure comprises a barrier layer, a buffer layer and a substrate from top to bottom; S2, etching the substrate to etch the barrier layer and a portion of the buffer layer into a V-shaped structure, so that the buffer layer is etched into a first buffer layer located in the substrate structure and a second buffer layer located in the V-shaped structure; S3, depositing a gate, a source and a drain on the barrier layer of the V-shaped structure respectively to form an electrode layer; S4, performing Si3N4 passivation treatment on the outer surface of the electrode layer and part of the first buffer layer, and controlling the thickness of Si3N4 to form a passivation layer; S5, etching the interconnection through holes between the passivation layer and the source, drain and gate, and completing the preparation of the electrode extension parts of the source, drain and gate.

8. The method for preparing a gallium nitride device with improved linearity according to claim 7, characterized in that: The thickness of the passivation layer is 100-300 nm.

9. The method for preparing a gallium nitride device with improved linearity according to claim 7, characterized in that: In the V-shaped structure, the angle between the two sides is 60-80°.

10. The method for preparing a gallium nitride device with improved linearity according to claim 7, characterized in that: The passivation layer is prepared by CVD process.

Citation Information

Patent Citations

  • Non-planar GaN HEMT transverse power device

    CN116454112A

  • Field effect transistor having an ultra-short gate and a horizontal structure, and process for manufacturing the same

    EP0138638A2