Circuit integration method and device based on thin film circuit substrate

By making a sandwich structure of the buffer layer and the protective layer on the thin-film circuit substrate, the problem of rupture or ripping up of the thin-film circuit substrate or integrated circuit layer in the flexible display panel is solved, and stress relief and stability improvement are achieved.

CN118921877AInactive Publication Date: 2024-11-08ZHONGJIANG LIJIANG ELETRONICS CO LTD
View PDF 14 Cites 0 Cited by

Patent Information

Application Number
CN202411083910.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-08
Publication Date
2024-11-08
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

During the production and use of flexible display panels, thin-film circuit substrates or integrated circuit layers are prone to rupture or cause problems.

Method used

By making a buffer layer and a protective layer on the thin film circuit substrate, the buffer layer covers the surface of the thin film circuit substrate, the thickness of the protective layer is 2 to 3 times the thickness of the buffer layer, and the thickness of the integrated circuit layer is smaller than the thickness of the buffer layer, forming a sandwich structure to release stress.

Benefits of technology

It effectively avoids the cracking or lifting of thin-film circuit substrates and integrated circuit layers during production and use, ensuring their stability and flexibility, releasing stress to the greatest extent and preventing damage.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118921877A_ABST
    Figure CN118921877A_ABST
Patent Text Reader

Abstract

The invention provides a circuit integration method and device based on a thin film circuit substrate, and relates to the technical field of thin film substrates. Firstly, a thin film circuit substrate is provided, and a buffer layer is manufactured based on the thin film circuit substrate; wherein the buffer layer covers the surface of the thin film circuit substrate, and then the integrated circuit layer is manufactured based on the surface of the buffer layer; wherein the integrated circuit layer comprises an electronic element; manufacturing a protection layer based on the surface of the integrated circuit layer; wherein the thickness of the protection layer is 2-3 times that of the buffer layer, and the thickness of the integrated circuit layer is smaller than that of the buffer layer. The circuit integration method and device based on the thin film circuit substrate have the advantages of being high in stress release capacity and capable of effectively preventing the thin film circuit substrate and the integrated circuit layer from being damaged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of thin film substrates, and in particular to a circuit integration method and device based on a thin film circuit substrate. Background Art

[0002] In today's display technology, flexible display panels have become a new generation of forward-looking display technology due to their excellent properties such as high lightness, impact resistance, flexibility, wearability and portability.

[0003] At present, flexible display panels are generally prepared by thin film circuit substrates. After the thin film circuit substrates are prepared, integrated circuits need to be further manufactured on their surface to drive the display of the corresponding display panel. In the prior art, the corresponding circuits are generally directly manufactured on the thin film circuit substrates.

[0004] However, in actual applications, it is found that during preparation and subsequent applications, the thin film circuit substrate or the integrated circuit layer is prone to cracking or lifting. Summary of the invention

[0005] The purpose of the present application is to provide a circuit integration method and device based on a thin film circuit substrate to solve the problem that the thin film circuit substrate or the integrated circuit layer is prone to cracking or lifting.

[0006] In order to achieve the above purpose, the technical solution adopted in the embodiment of the present application is as follows:

[0007] On the one hand, an embodiment of the present application provides a circuit integration method based on a thin film circuit substrate, the method comprising:

[0008] Providing a thin film circuit substrate;

[0009] A buffer layer is manufactured based on the thin film circuit substrate; wherein the buffer layer covers the surface of the thin film circuit substrate;

[0010] An integrated circuit layer is fabricated based on the surface of the buffer layer; wherein the integrated circuit layer includes electronic components;

[0011] A protective layer is manufactured based on the surface of the integrated circuit layer; wherein the thickness of the protective layer is 2 to 3 times the thickness of the buffer layer, and the thickness of the integrated circuit layer is less than the thickness of the buffer layer.

[0012] Optionally, the step of manufacturing a buffer layer based on the thin film circuit substrate includes:

[0013] A multi-layer buffer layer is manufactured based on the surface of the thin film circuit substrate, wherein the refractive index of the multi-layer buffer layer gradually decreases along the epitaxial direction of the thin film circuit substrate.

[0014] Optionally, the step of manufacturing a buffer layer based on the thin film circuit substrate includes:

[0015] A multi-layer buffer layer is manufactured based on the surface of the thin film circuit substrate, wherein the thickness of the multi-layer buffer layer gradually decreases along the epitaxial direction of the thin film circuit substrate.

[0016] Optionally, the thin film circuit substrate includes a bending region, and before the step of manufacturing an integrated circuit layer based on the surface of the buffer layer, the method further includes:

[0017] A bending protection layer is manufactured based on the bending area.

[0018] Optionally, the bending region includes a first bending point and a second bending point, and before the step of manufacturing an integrated circuit layer based on the surface of the buffer layer, the method further includes:

[0019] A first bending protection layer is manufactured based on the first bending point, and a second protection layer is manufactured based on the second bending point.

[0020] Optionally, the thin film circuit substrate includes a display area and a non-display area, and after the step of manufacturing a protective layer based on the surface of the integrated circuit layer, the method further includes:

[0021] A blocking plate is arranged on the surface of the protection layer to isolate the display area from the non-display area.

[0022] Optionally, the material of the thin film circuit substrate is a combination of one or more of polyimide, polyetherimide, polyphenylene sulfide and polyarylate, and the material of the blocking plate is nitride silicon.

[0023] Optionally, before the step of providing a thin film circuit substrate, the method further comprises:

[0024] Providing a carrier plate, wherein the carrier plate is provided with a clamping groove;

[0025] The steps of providing a thin film circuit substrate include:

[0026] A thin film circuit substrate is manufactured based on the clamping groove; wherein the thin film circuit substrate is located in the clamping groove and on the table surface of the carrier, and the difference in thermal expansion coefficient between the carrier and the thin film circuit substrate is less than 10 ppm / °C.

[0027] Optionally, the buffer layer includes at least one of silicon oxide, silicon nitride, niobium oxide, aluminum oxide or an organic material.

[0028] On the other hand, an embodiment of the present application provides a circuit integration device based on a thin film circuit substrate, and the circuit integration device based on a thin film circuit substrate is used to execute the above method.

[0029] Compared with the prior art, the embodiments of the present application have the following beneficial effects:

[0030] The embodiment of the present application provides a circuit integration method and device based on a thin film circuit substrate, first providing a thin film circuit substrate, making a buffer layer based on the thin film circuit substrate; wherein the buffer layer covers the surface of the thin film circuit substrate, and then making an integrated circuit layer based on the surface of the buffer layer; wherein the integrated circuit layer includes electronic components; and then making a protective layer based on the surface of the integrated circuit layer; wherein the thickness of the protective layer is 2 to 3 times the thickness of the buffer layer, and the thickness of the integrated circuit layer is less than the thickness of the buffer layer. Since the present application first makes a buffer layer to relieve stress when making the integrated circuit layer, there will be no cracking or lifting when making the integrated circuit layer. Moreover, since the thickness of the protective layer is 2 to 3 times the thickness of the buffer layer, and the thickness of the integrated circuit layer is less than the thickness of the buffer layer, the integrated circuit layer is clamped by the buffer layer and the protective layer to form a "sandwich" structure, which can release stress to the greatest extent, so that in the subsequent use process, even if the thin film circuit substrate and the integrated circuit layer are bent, it can quickly release stress to avoid damage to the thin film circuit substrate and the integrated circuit layer.

[0031] In order to make the above-mentioned objects, features and advantages of the present application more obvious and easy to understand, preferred embodiments are specifically cited below and described in detail with reference to the attached drawings. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the drawings required for use in the embodiments will be briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present application and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without paying creative work.

[0033] Figure 1 An exemplary flow chart of a circuit integration method based on a thin film circuit substrate provided in an embodiment of the present application.

[0034] Figure 2 A schematic diagram of the structure based on a thin film circuit substrate and an integrated circuit layer provided in an embodiment of the present application.

[0035] Figure 3 A schematic diagram of the structure of the buffer layer provided in an embodiment of the present application.

[0036] Figure 4 A schematic diagram of the relationship between the thickness of the buffer layer and the chromaticity b* provided in an embodiment of the present application.

[0037] Figure 5 A schematic diagram of the partitioning of the thin film circuit substrate provided in an embodiment of the present application.

[0038] Figure 6 A structural schematic diagram after a bending protection layer is formed in the bending area is provided for an embodiment of the present application.

[0039] Figure 7 Provided in the embodiments of this application Figure 6 Schematic diagram of the corresponding structure after bending.

[0040] Figure 8 Another structural schematic diagram after a bending protection layer is formed in the bending area provided in an embodiment of the present application.

[0041] In the figure: 110 - thin film circuit substrate; 120 - buffer layer; 121 - first buffer layer; 122 - second buffer layer; 123 - third buffer layer; 130 - integrated circuit layer; 140 - protective layer; 150 - bending protective layer; 151 - first bending protective layer; 152 - second bending protective layer. DETAILED DESCRIPTION

[0042] In order to make the purpose, technical solution and advantages of the embodiments of the present application clearer, the technical solution in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, rather than all the embodiments. The components of the embodiments of the present application described and shown in the drawings here can be arranged and designed in various different configurations.

[0043] Therefore, the following detailed description of the embodiments of the present application provided in the accompanying drawings is not intended to limit the scope of the present application for which protection is sought, but merely represents selected embodiments of the present application. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in the field without creative work are within the scope of protection of the present application.

[0044] It should be noted that similar reference numerals and letters represent similar items in the following drawings, so once an item is defined in one drawing, it does not need to be further defined and explained in subsequent drawings. At the same time, in the description of this application, the terms "first", "second", etc. are only used to distinguish the description and cannot be understood as indicating or implying relative importance.

[0045] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Some embodiments of the present application are described in detail below in conjunction with the accompanying drawings. The following embodiments and features in the embodiments may be combined with each other without conflict.

[0046] As described in the background art, currently, in the process of manufacturing and using the flexible display panel, the thin film circuit substrate or the integrated circuit layer is prone to cracking or lifting.

[0047] In view of this, in order to solve the above problems, an embodiment of the present application provides a circuit integration method based on a thin film circuit substrate, which realizes stress buffering by setting a buffer layer, thereby effectively protecting the thin film circuit substrate and the integrated circuit layer.

[0048] The circuit integration method based on the thin film circuit substrate 110 provided in the present application is exemplarily described below:

[0049] As an implementation, see Figure 1 , the method comprising:

[0050] S102, providing a thin film circuit substrate 110.

[0051] S104 , manufacturing a buffer layer 120 based on the thin film circuit substrate 110 ; wherein the buffer layer 120 covers the surface of the thin film circuit substrate 110 .

[0052] S106 , manufacturing an integrated circuit layer 130 based on the surface of the buffer layer 120 ; wherein the integrated circuit layer 130 includes electronic components.

[0053] S108 , manufacturing a protection layer 140 based on the surface of the integrated circuit layer 130 ; wherein the thickness of the protection layer 140 is 2 to 3 times the thickness of the buffer layer 120 , and the thickness of the integrated circuit layer 130 is less than the thickness of the buffer layer 120 .

[0054] Among them, the thin film circuit substrate 110 and the integrated circuit layer 130 provided in the embodiment of the present application are both flexible and bendable, and the present application does not limit the material of the thin film circuit substrate 110. In an optional implementation, the material of the thin film circuit substrate 110 is a combination of one or more of polyimide, polyetherimide, polyphenylene sulfide and polyarylate. Of course, it is not limited to this. For example, the material of the thin film circuit substrate 110 can also be polyethylene terephthalate (PET), cycloolefin polymer (COP), polycarbonate (PC), polymethylmethacrylate (PMMA), cycloolefin copolymer (COC), triacetyl cellulose (TAC), polypropylene (PP), polystyrene (PS), glass, etc.

[0055] Furthermore, the material of the buffer layer 120 is not limited. For example, the material of the buffer layer 120 is silicon oxide, silicon nitride, niobium oxide, aluminum oxide, an organic material, or a combination or stack of the above materials.

[0056] In one implementation, the buffer layer 120 may cover the entire surface of the thin film circuit substrate 110 . Of course, the area of ​​the buffer layer 120 may also be smaller than that of the thin film circuit substrate 110 , that is, the edge of the buffer layer 120 is at a certain distance from the edge of the thin film circuit substrate 110 .

[0057] Among them, the integrated circuit layer 130 includes a variety of electronic components to drive the display device to display. For example, the integrated circuit layer 130 may include touch electrodes, thin film transistors, pixel electrodes, common electrodes, light-emitting diodes (such as organic light-emitting diodes or inorganic light-emitting diodes), wires, insulating layers or combinations or stacks of the above.

[0058] Regarding the production of the integrated circuit layer 130, the integrated circuit layer 130 may be first produced on other carriers and then transferred to the buffer layer 120. Alternatively, the integrated circuit layer 130 may be directly produced on the buffer layer 120, for example, by vapor phase epitaxy, metal deposition or other processes.

[0059] During the process of manufacturing the integrated circuit layer 130, the temperature may be high, generally reaching above 200°C. At this temperature, the thin film circuit substrate 110 or the integrated circuit layer 130 may be easily cracked or lifted. Through research, it is found that this situation mainly occurs due to excessive stress.

[0060] In the present application, when making the integrated circuit layer 130, a buffer layer 120 is first made to relieve stress. Therefore, when making the integrated circuit layer 130, it is possible to avoid cracking or lifting as much as possible. At the same time, since the thickness of the protective layer 140 is 2 to 3 times the thickness of the buffer layer 120, and the thickness of the integrated circuit layer 130 is less than the thickness of the buffer layer 120, the thickness of the integrated circuit layer 130 located in the middle is the smallest. The buffer layer 120 and the protective layer 140 are used to clamp the integrated circuit layer 130 to form a "sandwich" structure. This structure can release stress to the greatest extent, so that in the subsequent use process, even if the thin film circuit substrate 110 and the integrated circuit layer 130 are bent, it can quickly release stress to avoid damage to the thin film circuit substrate 110 and the integrated circuit layer 130.

[0061] Moreover, the applicant has discovered that by setting the thickness of the protective layer 140 to 2 to 3 times the thickness of the buffer layer 120, it is possible to ensure that the stress is extended as much as possible toward the protective layer 140, so that the stress of the thin film circuit substrate 110, the buffer layer 120 and the integrated circuit layer 130 will not be concentrated inside as much as possible, thereby ensuring the stability of the thin film circuit substrate 110 and the integrated circuit layer 130.

[0062] It should be noted that the thickness of the buffer layer 120 and the thickness of the integrated circuit layer 130 described in the present application are their own heights, and the thickness of the protective layer 140 described in the present application is the height between the surface and the bottom of the protective layer 140. Figure 2 In the figure, the lowest point of the protection layer 140 extends to the surface of the buffer layer 120 , so the thickness of the protection layer 140 is h1 as shown in the figure.

[0063] It can be understood that, through the above configuration, the protection layer 140 can not only provide insulation protection for the integrated circuit layer 130 , but also achieve stress release.

[0064] In one implementation, the buffer layer 120 can not only achieve stress buffering, but also serve as an optical matching layer to adjust the color of the entire display panel. Of course, it can also adjust the color of light penetrating the thin film circuit substrate 110 and the integrated circuit layer 130 .

[0065] In order to better adjust the chromaticity, a multi-layer buffer layer 120 can be fabricated on the surface of the thin film circuit substrate 110, wherein the refractive index of the multi-layer buffer layer 120 gradually decreases along the epitaxial direction of the thin film circuit substrate 110 and the thickness of the multi-layer buffer layer 120 gradually increases along the epitaxial direction of the thin film circuit substrate 110. For example, see Figure 3 The buffer layer 120 includes a first buffer layer 121, a second buffer layer 122 and a third buffer layer 123, the thicknesses of the first buffer layer 121, the second buffer layer 122 and the third buffer layer 123 gradually decrease, and the refractive indices of the first buffer layer 121, the second buffer layer 122 and the third buffer layer 123 gradually decrease.

[0066] See also Figure 4 , a schematic diagram of the relationship between the thickness of the buffer layer 120 and the chromaticity b*, wherein the thickness of the buffer layer 120 is in nanometers. It can be seen from the figure that when the buffer layer 120 is 20 to 100 nanometers, as the thickness of the buffer layer 120 continues to increase, the chromaticity b* continues to decrease. However, since an excessively thick buffer layer 120 will affect stress, the total thickness of the buffer layer 120 provided in the present application is 20 to 100 nanometers, which not only makes the buffer chromaticity value smaller, but also reduces the stress effect.

[0067] At the same time, by providing multiple buffer layers 120 instead of a single layer, the effect on chromaticity can be relatively flexible when different colors of light penetrate. In addition, the light incident from above can be gradually refracted outward, reducing the impact of noise light incident from above.

[0068] Also, see Figure 5 The thin film circuit substrate 110 provided in the present application includes a display area and a non-display area, and the non-display area includes a bending area. Before the step of manufacturing the integrated circuit layer 130 based on the surface of the buffer layer 120, the method further includes:

[0069] The bending protection layer 150 is manufactured based on the bending area.

[0070] The display area described in the present application refers to the area used for display in the display device, and on this area, devices such as a display panel may also be included. On this basis, the integrated circuit layer 130 may include a pixel circuit. In one implementation, the pixel circuit includes: an active layer located on the flexible substrate, a gate insulating layer located on the active layer, a plurality of gates located on the gate insulating layer, and an interlayer insulating layer, wherein the interlayer insulating layer covers the plurality of gates, a plurality of source electrodes and a plurality of drain electrodes are prepared on the interlayer insulating layer, a plurality of vias are provided on the interlayer insulating layer and the gate insulating layer, and the plurality of source electrodes and the plurality of drain electrodes are connected to the active layer through the plurality of vias. The display of the display panel can be controlled by the pixel circuit.

[0071] Currently, for a foldable display device, the thin film circuit substrate 110 includes a display area and a non-display area, and can be folded along the boundary between the display area and the non-display area.

[0072] The applicant has found that the most prone to failure is the folding area of ​​the foldable display device. It is further found that the cause of the failure is that after multiple foldings, the folding area accumulates too much stress, causing the thin film circuit substrate 110 or the integrated circuit layer 130 in the folding area to break or be damaged.

[0073] For this reason, as an implementation, see Figure 6 , a bending protection layer 150 may be formed in the bending area, and the integrated circuit layer 130 covers the buffer layer 120 and the bending protection layer 150 .

[0074] This arrangement ensures that stress buffering is further achieved in the bending area, effectively preventing damage to the bending area.

[0075] And, for further stress relief, see Figure 7 The edge of the bending protection layer 150 is set to be arc-shaped, that is, the thickness of the middle of the bending protection layer 150 is the largest, and its thickness gradually decreases when extending along both sides.

[0076] Figure 7 In the figure, only the structure of the buffer layer 120 and the bending protection layer 150 after bending is shown. In the figure, B represents the bending area, and a represents the edge of the bending protection layer 150. It can be seen that the thickness of this area is smaller than that of other areas and gradually decreases. Through this setting, the stress generated during the bending process can be dissipated along the direction of the arrow A in the figure, rather than accumulated inside the bending area, which can effectively protect the bending area from damage.

[0077] The applicant further discovered that after the thickness relationship of the buffer layer 120 and the protective layer 140 is set based on the present application, stress is easily accumulated at the first bending point and the second bending point of the bending area. On this basis, before the step of manufacturing the integrated circuit layer 130 based on the surface of the buffer layer 120, the method further includes:

[0078] The first bending protection layer 151 is manufactured based on the first bending point, and the second protection layer 140 is manufactured based on the second bending point.

[0079] See also Figure 8The first bending protection layer 151 and the second bending protection layer 152 are arranged on both sides of the bending area to ensure stress buffering in the area. At the same time, the first bending protection layer 151 and the second bending protection layer 152 can also be arranged in an arc shape. On this basis, the stress of the first bending protection layer 151 and the second bending protection layer 152 can be released toward both sides, thereby ensuring that the area is not prone to cracking due to stress accumulation.

[0080] In addition, in order to achieve isolation between the display area and the non-display area, after the step of manufacturing the protection layer 140 based on the surface of the integrated circuit layer 130, the method further includes:

[0081] A blocking plate is disposed on the surface of the protection layer 140 to isolate the display area from the non-display area.

[0082] The present application does not limit the material of the blocking plate. For example, the material of the blocking plate may be silicon nitride.

[0083] Furthermore, since the thin film circuit substrate is relatively thin, before the step of providing a thin film circuit substrate, the method further includes:

[0084] Providing a carrier board, wherein the carrier board is provided with a clamping groove;

[0085] The steps of providing a thin film circuit substrate include:

[0086] A thin film circuit substrate is manufactured based on the clamping groove; wherein the thin film circuit substrate is located in the clamping groove and on the table surface of the carrier plate, and the difference in thermal expansion coefficient between the carrier plate and the thin film circuit substrate is less than 10 ppm / °C.

[0087] That is, in this application, the thin film circuit substrate is made by using the clamping structure of the carrier, and the difference in thermal expansion coefficient between the two is less than 10ppm / ℃, so that during the preparation process, the internal thermal stress is relatively small and can be released through the structure provided by this application to prevent damage during the preparation process. After the production is completed, that is, after the structure including the integrated circuit layer and the protective layer is produced, the thin film circuit substrate can be peeled off from the carrier.

[0088] Based on the above implementation, the embodiment of the present application further provides a circuit integration device based on the thin film circuit substrate 110, and the circuit integration device based on the thin film circuit substrate 110 is used to execute the above method.

[0089] In summary, the embodiment of the present application provides a circuit integration method and device based on a thin film circuit substrate 110, firstly, a thin film circuit substrate 110 is provided, and a buffer layer 120 is manufactured based on the thin film circuit substrate 110; wherein the buffer layer 120 covers the surface of the thin film circuit substrate 110, and then an integrated circuit layer 130 is manufactured based on the surface of the buffer layer 120; wherein the integrated circuit layer 130 includes electronic components; and then a protective layer 140 is manufactured based on the surface of the integrated circuit layer 130; wherein the thickness of the protective layer 140 is 2 to 3 times the thickness of the buffer layer 120, and the thickness of the integrated circuit layer 130 is less than the thickness of the buffer layer 120. Since the present application first manufactures a layer of buffer layer 120 to relieve stress when manufacturing the integrated circuit layer 130, no cracking or lifting will occur when manufacturing the integrated circuit layer 130. Furthermore, since the thickness of the protective layer 140 is 2 to 3 times the thickness of the buffer layer 120 and the thickness of the integrated circuit layer 130 is less than that of the buffer layer 120, the integrated circuit layer 130 is clamped by the buffer layer 120 and the protective layer 140 to form a "sandwich" structure. This structure can release stress to the greatest extent, so that in subsequent use, even if the thin film circuit substrate 110 and the integrated circuit layer 130 are bent, they can quickly release stress to avoid damage to the thin film circuit substrate 110 and the integrated circuit layer 130.

[0090] The above description is only the preferred embodiment of the present application and is not intended to limit the present application. For those skilled in the art, the present application may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present application shall be included in the protection scope of the present application.

[0091] It will be apparent to those skilled in the art that the present application is not limited to the details of the exemplary embodiments described above, and that the present application can be implemented in other specific forms without departing from the spirit or essential features of the present application. Therefore, the embodiments should be considered exemplary and non-limiting in all respects, and the scope of the present application is defined by the appended claims rather than the above description, and it is intended that all changes falling within the meaning and scope of the equivalent elements of the claims be included in the present application. Any reference numeral in a claim should not be considered as limiting the claim to which it relates.

Claims

1. A circuit integration method based on a thin film circuit substrate, characterized in that: The method comprises: Providing a thin film circuit substrate; A buffer layer is manufactured based on the thin film circuit substrate; wherein the buffer layer covers the surface of the thin film circuit substrate; An integrated circuit layer is fabricated based on the surface of the buffer layer; wherein the integrated circuit layer includes electronic components; A protective layer is manufactured based on the surface of the integrated circuit layer; wherein the thickness of the protective layer is 2 to 3 times the thickness of the buffer layer, and the thickness of the integrated circuit layer is less than the thickness of the buffer layer.

2. The circuit integration method based on a thin film circuit substrate according to claim 1, characterized in that: The step of manufacturing a buffer layer based on the thin film circuit substrate comprises: A multi-layer buffer layer is manufactured based on the surface of the thin film circuit substrate, wherein the refractive index of the multi-layer buffer layer gradually decreases along the epitaxial direction of the thin film circuit substrate.

3. The circuit integration method based on a thin film circuit substrate according to claim 2, characterized in that: The step of manufacturing a buffer layer based on the thin film circuit substrate comprises: A multi-layer buffer layer is manufactured based on the surface of the thin film circuit substrate, wherein the thickness of the multi-layer buffer layer gradually decreases along the epitaxial direction of the thin film circuit substrate.

4. The circuit integration method based on a thin film circuit substrate according to claim 1, characterized in that: The thin film circuit substrate includes a bending area. Before the step of manufacturing an integrated circuit layer based on the surface of the buffer layer, the method further includes: A bending protection layer is manufactured based on the bending area.

5. The circuit integration method based on a thin film circuit substrate according to claim 4, characterized in that: The bending region includes a first bending point and a second bending point. Before the step of manufacturing an integrated circuit layer based on the surface of the buffer layer, the method further includes: A first bending protection layer is manufactured based on the first bending point, and a second protection layer is manufactured based on the second bending point.

6. The circuit integration method based on a thin film circuit substrate according to claim 1, characterized in that: The thin film circuit substrate comprises a display area and a non-display area. After the step of manufacturing a protective layer based on the surface of the integrated circuit layer, the method further comprises: A blocking plate is arranged on the surface of the protection layer to isolate the display area from the non-display area.

7. The circuit integration method based on a thin film circuit substrate according to claim 6, characterized in that: The material of the thin film circuit substrate is a combination of one or more of polyimide, polyetherimide, polyphenylene sulfide and polyarylate, and the material of the blocking plate is nitride silicon.

8. The circuit integration method based on a thin film circuit substrate according to claim 1, characterized in that: Before the step of providing a thin film circuit substrate, the method further comprises: Providing a carrier plate, wherein the carrier plate is provided with a clamping groove; The steps of providing a thin film circuit substrate include: A thin film circuit substrate is manufactured based on the clamping groove; wherein the thin film circuit substrate is located in the clamping groove and on the table surface of the carrier, and the difference in thermal expansion coefficient between the carrier and the thin film circuit substrate is less than 10 ppm / °C.

9. The circuit integration method based on a thin film circuit substrate according to claim 1, characterized in that: The buffer layer includes at least one of silicon oxide, silicon nitride, niobium oxide, aluminum oxide or an organic material.

10. A circuit integrated device based on a thin film circuit substrate, characterized in that: The circuit integration device based on a thin film circuit substrate is used to execute the circuit integration method based on a thin film circuit substrate as claimed in any one of claims 1 to 9.

Citation Information

Patent Citations

  • Combination of patterned metal wire and substrate

    CN103715177A

  • Flexible display substrate and preparation method thereof, and flexible display device

    CN104022123A

  • Display device

    CN107871751A

  • Flexible panel and method for manufacturing the same

    CN109213347A

  • Light-emitting diode structure with novel transparent conducting layer and production method

    CN109904290A