Long film and method for manufacturing connection structure

By giving identification markers on the long strip film and using image recognition technology to identify poor monoliths, the problems of degraded adhesive film performance and foreign matter residues are solved, productivity and product quality are improved, and efficient manufacturing of connecting structures is achieved.

CN118923217APending Publication Date: 2024-11-08DEXERIALS CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380029549.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-03-31
Filing Date
2023-03-17
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

When manufacturing long strip films and connecting structures, it is difficult for the prior art to effectively avoid the influence of poor monoliths, resulting in reduced performance of the adhesive film and foreign matter residues, affecting productivity and product quality.

Method used

By assigning identification markers on the substrate film and adhesive film monoliths of the strip film, and using image recognition technology to identify poor monoliths, combined with a laser marker, quickly and accurately assigning identification markers without stopping delivery without stopping. , ensure the quality and productivity of the monolithic.

Benefits of technology

Effectively avoid bad monoliths, maintain the performance of the adhesive film, improve productivity, and ensure excellent crimping characteristics and reliability of the connecting structure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118923217A_ABST
    Figure CN118923217A_ABST
Patent Text Reader

Abstract

Provided are a long film capable of maintaining the performance of a single adhesive film, and a method for manufacturing a connected structure. The long film (10) has a long substrate film (11) and single pieces (21) to (25) of an adhesive film disposed along the longitudinal direction of the substrate film (11), and an identification marker (30) is applied to a predetermined single piece or / and the substrate film on which the predetermined single piece is disposed. Therefore, when the single sheet is used, the identification marker is identified, so that the bad single sheet can be avoided, and the performance of the single sheet of the adhesive film can be maintained.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This technology relates to a method for manufacturing a long film and a connected structure in which a single piece of film is arranged along the long side of a substrate film. This application claims priority based on Japanese Patent Application No. 2022-061427 filed in Japan on March 31, 2022, and is incorporated herein by reference. Background Art

[0002] In recent years, adhesive films such as anisotropic conductive film (ACF), conductive film, and adhesive film (NCF) are punched into single pieces of arbitrary shapes, and long strips of film with the single pieces arranged along the long side direction of the base film are wound on a reel and shipped (for example, see Patent Document 1).

[0003] However, for example, during punching, broken pieces may remain, broken pieces may be transferred to individual sheets, or individual sheets may curl up, and therefore, it is necessary to inspect and pick up defective individual sheets from each individual sheet of the long film.

[0004] Because defective sheets are removed after inspection, there's a risk of affecting the sheets at either end of the defective sheet. Furthermore, there's a risk of tiny fragments of adhesive film remaining on the base film, becoming foreign matter in the manufacturing line for the connected structure. Thus, when removing defective sheets, it's difficult to maintain the performance of the long film sheets. Prior art literature Patent Literature

[0005] Patent Document 1: Japanese Patent Application Laid-Open No. 2020-198422. Summary of the Invention Problems to be solved by the invention

[0006] The present technology has been proposed in view of such conventional actual conditions, and provides a method for producing a long film and a connection structure that can maintain the performance of a single sheet of adhesive film. Solutions to Problems

[0007] The long film according to the present technology comprises a long base film and a single piece of adhesive film arranged along the longitudinal direction of the base film, and an identification marker is provided to a predetermined single piece or at least one of the base films on which the predetermined single piece is arranged. Effects of the Invention

[0008] According to this technology, when using a sheet, the identification mark is image-recognized, thereby avoiding defective sheets and maintaining the performance of the sheet of adhesive film. BRIEF DESCRIPTION OF THE DRAWINGS

[0009] Figure 1 This is a diagram showing an example of a long film. Figure 2 FIG. 1 is a schematic diagram showing an example of a defective single piece having a window frame portion. Figure 2 (A) shows a state where foreign matter is mixed in. Figure 2 (B) shows a state where wrinkles are generated. Figure 2 (C) shows a state where a notch has occurred. Figure 3 FIG. 1 is a diagram showing an example of an identification marker. Figure 4 1 is a diagram showing a configuration example of an inspection mark device. Figure 5 is a diagram for explaining the operation of the detection sensor. Figure 5 (A) shows a detection sensor for detecting each piece of the transported long film. Figure 5 (B) shows the detection signal of a single chip detected by the detection sensor. Figure 6 It is a diagram for explaining the detection timing of the detection sensor. Figure 7 This is a diagram for explaining the NG signal and the OK signal in inspection and judgment. Figure 8 This is an example of assigning an identification marker using a laser marker. Figure 9 This is a diagram showing an example of acceleration and deceleration waveforms of a supply motor or a recovery motor for a long film. Figure 10 This is a flowchart showing a method for inspecting a long film. DETAILED DESCRIPTION

[0010] Hereinafter, embodiments of the present invention will be described in detail in the following order while referring to the accompanying drawings. 1. Long strip film 2. Check the marking device 3. Manufacturing method of long film 4. Method for manufacturing a connection structure

[0011] <1. Long strip film> The long film according to this embodiment comprises a long base film and a sheet of adhesive film disposed along the long side of the base film. An identification mark is assigned to a given sheet or at least one side of the base film on which the given sheet is disposed, so that defective sheets can be identified. Thus, when the sheets are used, the identification mark can be identified, for example, through image recognition, thereby avoiding defective sheets and maintaining the performance of the adhesive film sheet.

[0012] Figure 1FIG is a diagram showing an example of a long film. Figure 1 As shown, the long film 10 has a long base film 11 and single pieces 21 to 25 of adhesive film arranged along the long side direction of the base film 11, and an identification mark 30 is given to the single piece 23 as a defective single piece and the base film 11 where the single piece 23 as a defective single piece is arranged.

[0013] The long strip film 10 is preferably provided with an end region composed of a substrate film 11 at the end in the width direction. The length W in the width direction of the end region composed of the substrate film 11 is preferably 100 μm or more, more preferably 500 μm or more, and further preferably 1000 μm or more. As a result, it is possible to give an identification mark to the end region composed of the substrate film 11, and compared with the case where the identification mark is given to a single piece, the decline in printing quality can be suppressed. In addition, by having such an end region, it is difficult for the adhesive to overflow, which is easy to occur in the case of a long strip. This is because it is difficult for the adhesive to reach the end of the substrate film, and since it is difficult to produce so-called blockage, the convenience in actual use is improved. As described later, when the single piece is separated from the end of the substrate film, it is difficult to produce blockage, which can also contribute to productivity.

[0014] The long strip film 10 can also be a long strip film in which single pieces 21 to 25 are continuously arranged for each unit area along the long side direction and wound on a reel. Here, the so-called "unit area" has a predetermined length along the length direction of the substrate, for example, a rectangular area is shown, and it can also be considered as the area between the center line between the single pieces and the center line between the adjacent single pieces or the area between a single piece and the center line between the single pieces. The adhesive film is peeled off from the base film and separated. In the present technology, there is no corresponding support body in the single piece adhesive film, but it is composed only of a layer composed of an adhesive (sometimes a covering film with a width roughly the same as the base material is laminated).

[0015] The base film 11 is a support film that supports the multiple individual sheets. Examples of the base film 11 include PET (PolyEthylene Terephthalate), OPP (Oriented Polypropylene), PMP (Poly-4-methylpentene-1), and PTFE (Polytetrafluoroethylene). Furthermore, the base film 11 can be suitably one in which at least the individual sheet side has been subjected to a release treatment, such as with silicone resin.

[0016] The thickness of the base film 11 is not particularly limited. From the perspective of peeling, the lower limit of the thickness of the base film 11 is preferably 10 μm or greater, more preferably 25 μm or greater, and even more preferably 38 μm or greater. If the upper limit of the base film thickness is too great, there is concern that excessive pressure may be applied to the adhesive film. Therefore, it is preferably 200 μm or less, more preferably 100 μm or less, even more preferably 75 μm or less, and may be 50 μm or less. Furthermore, when a cover film is provided on a single sheet of adhesive film, the thickness of the cover film also falls within the same range, but the cover film is preferably thinner than the base film.

[0017] The width of the substrate film 11 is also not particularly limited. From the perspective of winding, the lower limit of the width of the substrate film 11 is preferably 1 mm or greater, more preferably 2 mm or greater, and even more preferably 4 mm or greater. If the upper limit of the width of the substrate film 11 is too large, it may be difficult to transport or handle. Therefore, it is preferably 500 mm or less, more preferably 250 mm or less, and even more preferably 120 mm or less.

[0018] The adhesive film is not particularly limited, and examples thereof include anisotropic conductive film (ACF), conductive film containing conductive particles in an adhesive, adhesive film (NCF: non-conductive film), and solder-containing film containing solder particles. The binder of the adhesive film may be either thermosetting or thermoplastic.

[0019] When conductive particles such as metal particles, resin-core metal-coated particles, or solder particles are contained, the single sheet may have regions containing conductive particles and regions not containing conductive particles. Furthermore, the single sheet may have a structure of two or more layers, a structure of two or more layers consisting of a layer containing conductive particles or solder particles and a layer not containing conductive particles or solder particles, a structure of two or more layers containing conductive particles, or a structure of two or more layers not containing conductive particles.

[0020] The shape of the adhesive film is not particularly limited. For example, as described in Japanese Patent Application Laid-Open No. 2020-198422, it may be a U-shaped film with two horizontal sides and one vertical side, a square-shaped film with two horizontal sides and two vertical sides, an L-shaped film, a U-shaped film, a C-shaped film, etc. In addition, when conductive particles are contained, as described in Japanese Patent Application No. 6187665, the conductive particles may be embedded in the insulating resin. In addition, the conductive particles may be randomly or regularly arranged, and the conductive particles are preferably aligned in the film thickness direction. When solder particles are included, as described in Japanese Patent No. 6898413, it is preferred to prepare a thermoplastic resin that is solid at room temperature and has a melt flow rate of 10 g / 10 min or higher, as measured at 190°C and a load of 2.16 kg. The thickness should be at least 50% and no more than 300% of the average particle size of the solder particles. As described in Japanese Patent No. 7032367, the minimum melt viscosity of the adhesive film is preferably less than 100 Pa·s. The adhesive of the adhesive film may be either thermosetting or thermoplastic. The adhesive may be a single layer or a multilayered layer.

[0021] The thickness of the single sheet is not particularly limited. The lower limit of the thickness of the single sheet is preferably 1 μm or more, more preferably 3 μm or more, and further preferably 4 μm or more. The upper limit of the thickness of the single sheet is preferably 50 μm or less, more preferably 20 μm or less, and further preferably 10 μm or less.

[0022] The thickness of the monolithic sheet can be measured using a well-known micrometer or digital thickness gauge (e.g., with a minimum display of 0.0001 mm). However, when the thickness of the monolithic sheet is thinner than the particle size of the conductive particles, a contact-type thickness gauge is not suitable, and thus a laser displacement meter (e.g., a spectral interference displacement type, etc.) is preferably used. Here, the thickness of the monolithic sheet refers to the thickness of the adhesive resin layer only, and does not include the particle size of the conductive particles.

[0023] In addition, if Figure 1 As shown, the sheet may have a window frame portion where the base film 11 is exposed, and the base film of the window frame portion is provided with an identification marker 30. Sheets having a window frame portion are prone to becoming defective sheets, and therefore application of this technology is particularly useful.

[0024] Figure 2 FIG. 1 is a schematic diagram showing an example of a defective single piece having a window frame portion. Figure 2 (A) shows a state where foreign matter is mixed in. Figure 2 (B) shows a state where wrinkles are generated. Figure 2 (C) shows the state where a notch is generated. Figure 2As shown in (A), if the foreign matter H1 mixed into the wafer or the base film is a metal or non-metal object with a size larger than the particle size of the conductive particles during the appearance inspection, it is judged as a defective wafer. Figure 2 As shown in (B), when wrinkles H2 are generated on the outer shape of the single piece, for example, if the wrinkles are more than ±50 μm during the appearance inspection, the single piece is judged as a defective single piece. Figure 2 As shown in (C), when a chip H3 is formed in the outer shape of the chip and the chip is judged as a defective chip in a visual inspection, for example, if the chip H3 is larger than ±50 μm.

[0025] The identification marker 30 can be imparted using a laser marker, inkjet, punching, etc., and among these, laser printing using a laser marker is particularly preferred. For example, when using an inkjet to impart the identification marker 30, the ink scatters to the surrounding area, which may misjudge a defective single piece or produce a new defect caused by contamination. In addition, when the defective part is marked by punching without stopping the conveyance, when the long strip film with the single piece is wound on the reel, the shape change caused by the punching hole may cause the winding quality to deteriorate or the punching mark to be transferred to the single piece in the adjacent winding layer, and the waste caused by the punching needs to be recycled. In addition, the vibration of the film caused by the punching has an adverse effect on the focus of the inspection camera in the front section, making it difficult to mark without stopping the conveyance. These possibilities can be eliminated by imparting the identification marker 30 with a laser marker.

[0026] When conductive particles are included, the width of the identification marker 30 is equal to or greater than the particle diameter of the conductive particles, preferably equal to or greater than 20 μm, more preferably equal to or greater than 50 μm, and even more preferably equal to or greater than 100 μm.

[0027] Furthermore, the printing position of the identification marker 30 is not limited as long as it can identify defective sheets. For example, if a base film region is provided at the end of the width direction of the long film, the identification marker 30 may be printed only on the base film at the end of the defective sheet, or only on the defective sheet, or both. Furthermore, for example, if a base film region is provided at the end of the width direction of the long film, the identification marker 30 may be printed only on the base film at the end of a normal sheet, or on the base film at the end of the sheet preceding the defective sheet.

[0028] Figure 3 is a diagram showing an example of an identification marker. Figure 3 As shown in (A), the identification mark M1 may be a line in the width direction from the center of the window frame portion of the single piece to the end area formed by the base film. Figure 3As shown in (B), the identification mark M2 may be a line printed on the end area of ​​the substrate film in the conveying direction. Figure 3 As shown in (C), the identification mark M3 may also be a line printed on the conveying direction of the window frame portion of the single piece. Figure 3 As shown in (D), the identification mark M4 may be a zigzag line printed on the end area of ​​the substrate film in the conveying direction. Figure 3 As shown in (E), the identification mark M5 may also be a circle that is printed from the center of the window frame portion of a single piece to the end area formed by the base film. Figure 3 As shown in (F), the identification mark M6 may also be a slant line printed on the inner side of both ends of the sheet in the conveying direction. Figure 3 As shown in (G), the identification mark M7 is not particularly limited as long as it is not printed on adjacent wafers and can identify defective wafers.

[0029] With this long film, when using individual sheets, identification marks can be identified through, for example, image recognition, thereby avoiding defective sheets and maintaining the performance of the individual adhesive film sheets. Furthermore, individual sheets can be managed for safe use by the user, and the product's bonding properties (conductivity, bonding strength, insulation, reliability, etc.) can be more stably maintained.

[0030] <2. Check the marking device> The inspection marking device according to this embodiment includes: a conveying unit that conveys a long film having an adhesive film disposed along its longitudinal direction; a detecting unit that detects each of the conveyed long film sheets; an inspecting unit that inspects each of the conveyed long film sheets; an applying unit that applies an identification mark to a given piece of the conveyed long film sheet or to at least one of the base films on which the given piece of film is disposed; and a control unit that obtains positional information including the detected position of each piece of the long film sheet along its longitudinal direction from the detecting unit, obtains inspection information for each piece from the inspecting unit based on the positional information for each piece of film sheet, and instructs the applying unit to apply the identification mark based on the positional information and the inspection information for each piece of film sheet. This allows for high-speed inspection of the adhesive film sheets, thereby improving productivity. Furthermore, when the sheets are used, image recognition of the identification mark is performed, thereby preventing defective sheets from being processed.

[0031] Furthermore, it is preferred that the control unit records the position of each sheet being applied by the applying unit together with the detected position of each sheet in the position information, and the applying unit applies the identification mark based on the position of each sheet being applied. This facilitates outputting a printing trigger and stabilizes the position of the identification mark even when the conveying speed is increased.

[0032] Furthermore, it is preferred that the control unit record the inspection position of each sheet of the inspection unit together with the detection position of each sheet in the position information, and the inspection unit inspects each sheet of the conveyed long film based on the inspection position of each sheet. This makes it easy to output a camera trigger, and even if the conveying speed is increased, the inspection position of the sheet can be stabilized.

[0033] Furthermore, it is preferable that the control unit controls the timing of applying the identification marker by the applying unit based on the conveyance speed of the long film. This can suppress, for example, deviation of the printing position during acceleration or deceleration.

[0034] In addition, the imparting unit can use a laser marker, inkjet, punching, etc., among which it is particularly preferred to impart the identification mark by a laser marker. For example, when using inkjet to impart the identification mark, the ink scatters to the surrounding area, and sometimes there is a concern that a defective single piece may be misjudged or a new defect may be caused by contamination. In addition, when the defective part is marked by punching without stopping the conveyance, when the long strip film with the single piece is wound on the reel, the shape change caused by the punching hole may cause the winding quality to deteriorate or the punching mark may be transferred to the single piece in the adjacent winding layer, and the waste caused by the punching needs to be recycled. In addition, the vibration of the film caused by the punching has an adverse effect on the focus of the inspection camera in the front section, and sometimes it affects the conveying speed and has an adverse effect on productivity. For such reasons, as the imparting unit, a laser marker is used, so that these concerns can be avoided.

[0035] Figure 4 : is a diagram showing an example of the structure of the inspection mark device. Figure 4 As shown, the inspection and marking device 40 includes an unwinding mechanism 41, a detection sensor 42, an inspection camera 43, a laser marker 44, and a winding mechanism 45. Furthermore, the appearance inspection and marking device includes a control unit that controls the unwinding mechanism 41, the detection sensor 42, the inspection camera 43, the laser marker 44, and the winding mechanism 45. Here, the unwinding mechanism 41 and the winding mechanism 45 correspond to the aforementioned conveying unit, the detection sensor 42 corresponds to the aforementioned detection unit, the inspection camera 43 corresponds to the aforementioned inspection unit, and the laser marker 44 corresponds to the aforementioned applying unit.

[0036] The unwinding mechanism 41, although not shown, comprises, for example, a supply reel for accommodating the long film, a supply motor for rotating the supply reel to unwind the long film from the supply reel, and rollers for supporting the long film in a rolling contact state. The long film is unwound from the supply reel and transported in the longitudinal direction. Furthermore, although not shown, the long film from the unwinding mechanism 41 to the winding mechanism 45 is subjected to tension in the longitudinal direction of the long film, for example, by the action of the rollers.

[0037] The detection sensor 42 can be composed of, for example, a line sensor camera or a zone line camera, and detects each piece of the conveyed long film. For example, the line sensor camera can be used to capture images of the width of the conveyed long film and detect the difference in reflected light between when a piece of film is present and when it is not present on the base film, thereby enabling detection of the piece of film.

[0038] Figure 5 is a diagram for explaining the operation of the detection sensor. Figure 5 (A) shows a detection sensor for detecting each piece of the transported long film. Figure 5 (B) shows the detection signal of a single chip detected by the detection sensor. Figure 5 (A) and Figure 5 As shown in (B), the detection sensor 42 outputs a detection signal when there is a single piece of the conveyed long film as Hi and when there is no single piece as Lo. The control unit detects each single piece 50 when the detection signal changes from Lo to Hi.

[0039] Figure 6 is a diagram for explaining the detection timing of the detection sensor. Figure 6 As shown, the detection sensor 42 captures images at times t=0, t=1, t=2, t=3, t=4, and t=5, and the control unit detects the single chip at times t=1 and t=5 when the detection signal changes from Lo to Hi.

[0040] As described later, when the imaging trigger of the inspection camera 43 and the printing trigger of the laser marker 44 are offset, the imaging interval of the detection sensor 42 is shortened, thereby reducing the error in the detected position and improving the position accuracy of the imaging position of the inspection camera 43 and the position of the laser marker 44. Therefore, the imaging interval of the detection sensor 42 is preferably 1 to 50 milliseconds, more preferably 1 to 10 milliseconds, and even more preferably 1 to 5 milliseconds.

[0041] Inspection camera 43, for example, is comprised of a line camera, and performs visual inspections for, for example, the presence of fragments on the substrate film, transfer of fragments to individual wafers, and wafer curling. The inspection results are recorded in the wafer information memory of the control unit. Preferably, the visual inspection performs two types of inspections: an OK determination for a normal wafer and an NG determination for a defective wafer. Each wafer is inspected and judged to have both an NG signal and an OK signal.

[0042] Figure 7 This is a diagram for explaining the NG signal and OK signal in the inspection judgment. Figure 7As shown, the visual inspection outputs both an NG signal and an OK signal for each wafer. For example, the NG signal is set to Hi for wafer number 3, while the OK signal is set to Hi for normal wafer numbers 1, 2, 4, and 5. Thus, even if the NG determination of wafer number 3 is delayed, or the output of the NG signal is delayed, the NG result for wafer number 3 can be recorded as wafer information in the memory before the defective wafer reaches the printing trigger of the laser marker 44, thereby providing a margin for the inspection process.

[0043] The laser marker 44 irradiates the object with a laser and changes the state of the object surface by oxidation, peeling, coloring, etc., without stopping the conveying. In addition, it will not cause excessive influence (vibration, etc.) on the conveying, and gives an identification mark to at least one side of a predetermined single piece or substrate film. The laser marker 44 is preferably a scanning method of irradiating a laser at one point and printing like a stroke. The laser used by the laser marker 44 can be appropriately selected according to the material of the substrate film, the adhesive film material of the single piece, etc. For example, a fiber laser, UV laser, YVO4 laser, CO2 laser, YAG laser, etc. can be selected. In addition, in order to suppress the influence of dust, the laser marker 44 is preferably provided with a vacuum in the printing part.

[0044] Figure 8 This is an example of assigning an identification mark using a laser marker. Figure 8 As shown, the laser marker 44 assigns identification markers M1 to M3 to defective wafers 52, 54, and 56, respectively, but does not assign identification marker M to normal wafers 51, 53, and 55. The identification marker is preferably assigned within the unit area, and more preferably assigned near the center of the unit area. This can improve the ability to identify defective wafers. Figure 8 In the example of providing the identification mark shown, the mark is printed on both the defective wafer and the base film at the end of the defective wafer, but the present technology is not limited to this.

[0045] The winding mechanism 45, for example, includes a recovery reel for recovering the long film, a recovery motor for rotating the recovery reel so that the recovery reel winds the long film, a roller for supporting the long film in a rolling contact state, etc., and winds the long film after the inspection and marking of a single piece is completed on the recovery reel.

[0046] The control unit, comprised of a device with memory, such as a PLC (Programmable Logic Controller), measures the distance traveled by the long film based on the length of the film pulled from the unwinding mechanism 41 or the length of the film recovered by the winding mechanism 45. Furthermore, the control unit controls the film supply motor and film recovery motor to ensure that the film is conveyed at a predetermined speed. The conveying speed of the long film is preferably 1 to 50 m / min, more preferably 5 to 50 m / min, and even more preferably 10 to 50 m / min.

[0047] The control unit also obtains positional information, including the detected position of each sheet in the longitudinal direction of the long film, from the detection sensor 12 and stores the positional information in the memory as sheet information. Furthermore, based on the positional information of each sheet, the control unit obtains inspection information for each sheet from the inspection camera 43 and stores the inspection information in the memory as sheet information. Furthermore, based on the sheet information for each sheet, the control unit causes the laser marker 44 to assign an identification mark. Furthermore, based on the sheet information, the control unit controls the imaging timing of the inspection camera 43 and the printing timing of the laser marker 44.

[0048] Table 1 shows an example of the chip information stored in the memory. As shown in Table 1, the chip information includes the chip number (chip number), the length measurement value of the chip detected by the detection sensor 42 (detection length measurement), the length measurement value triggered by the inspection camera 43 (camera trigger length measurement), the inspection result based on the inspection judgment (inspection result), and the length measurement value triggered by the printing of the laser marker 44 (laser length measurement).

[0049] [Table 1]

[0050] Each time a single sheet is detected by the detection sensor 42, the control unit records the single sheet number and records the single sheet detection length value indicating the detection position of each single sheet in the long side direction of the long film in the single sheet information. In addition, the control unit preferably records the measurement length value of the camera trigger indicating the inspection position of each single sheet by the inspection camera 43 together with the detection position of each single sheet in the single sheet information, and the inspection camera 43 inspects each single sheet of the conveyed long film based on the measurement length value of the camera trigger of each single sheet. That is, the control unit can easily output the camera trigger of the inspection camera 13 by offsetting the distance from the detection sensor 42 to the inspection camera 43 by a predetermined distance (300.00 mm in the example of the single sheet information shown in Table 1).

[0051] Furthermore, the control unit preferably records the measured length value of the printing trigger for each sheet of the laser marker 44, along with the detected position of each sheet, in the sheet information. The laser marker 44 then assigns an identification marker based on the measured length value of the printing trigger for each sheet. Specifically, the control unit can easily output the printing trigger for the laser marker 44 by offsetting the distance from the detection sensor 42 to the laser marker 44 by a predetermined distance (600.00 mm in the example of sheet information shown in Table 1).

[0052] The control unit preferably controls the timing of providing the recognition marker by the laser marker 44 based on the conveyance speed of the long film. For example, the control unit preferably corrects the printing trigger based on the acceleration / deceleration waveform region of the supply motor or the recovery motor.

[0053] Figure 9 : is a diagram showing an example of the acceleration and deceleration waveforms of the supply motor or the recovery motor of the long film. Figure 9 As shown, the acceleration and deceleration waveforms of the supply motor or recovery motor are accelerated by acceleration control and decelerated by deceleration control. Furthermore, the acceleration and deceleration waveforms can be divided into seven speed ranges: a region immediately after the start of acceleration S1, a constant speed increase region S2, a region at the end of acceleration S3, a constant speed region S4, a region immediately after the start of deceleration S5, a constant deceleration region S6, and a region at the end of deceleration S7. The control unit monitors the speed ranges of the supply motor or recovery motor and sets correction values ​​corresponding to speed ranges S1 to S7 for the printing trigger. This, for example, can suppress deviations in the printing position during acceleration and deceleration.

[0054] Then, Figure 4 The following describes the operation of the inspection and marking device shown in FIG. The detection sensor 42 detects a single sheet of adhesive film conveyed from the unwind mechanism 41. Each time a sheet is detected, the measured distance traveled by the long film is recorded in the memory as single-sheet information. Furthermore, each time a sheet is detected, the control unit offsets the single-sheet information by the preset distance from the detection sensor 42 to the inspection camera 43 (the measured value for the imaging trigger) and the preset distance from the detection sensor 42 to the laser marker 44 (the measured value for the printing trigger).

[0055] If a piece has traveled the length measured by the imaging trigger, the control unit outputs a camera trigger to the inspection camera 43 to perform a visual inspection. The inspection result is then added to the sheet information, thereby associating the sheet with the inspection result. Furthermore, if a sheet with an NG inspection result in the sheet information has traveled the length measured by the printing trigger, the control unit outputs a printing trigger to the laser marker 44 to print an identification mark on the defective sheet.

[0056] According to such an inspection marking device, it is possible to inspect the adhesive film sheets at high speed without stopping the conveyance, and to provide an identification mark to at least one of a predetermined sheet or a base film, thereby improving productivity.

[0057] <2. Method for producing long film> The method for manufacturing a long film according to this embodiment includes: a production step of producing a single long film having an adhesive film disposed along the longitudinal direction of a base film; a conveying step of conveying the long film along the longitudinal direction; a detection step of detecting each of the conveyed long film sheets and obtaining positional information including the detected position of each sheet along the longitudinal direction of the long film; an inspection step of inspecting each of the conveyed long film sheets based on the positional information of each sheet and obtaining inspection information for each sheet; and an assigning step of assigning an identification mark to a given sheet of the conveyed long film or to at least one of the base films on which the given sheet is disposed, based on the positional information and the inspection information. This allows for high-speed inspection of the adhesive film sheets, thereby improving productivity.

[0058] Here, it is preferable that, in the detection step, the position of each sheet in the attaching step is recorded in the position information, and in the attaching step, the identification mark is attached based on the attaching position of each sheet. This facilitates outputting the printing trigger and stabilizes the position of the identification mark even when the conveying speed is increased.

[0059] Furthermore, it is preferred that the inspection position of each sheet during the inspection process is recorded in the position information during the detection process, and that each sheet of the conveyed long film be inspected based on the inspection position of each sheet during the inspection process. This facilitates outputting an imaging trigger, and stabilizes the inspection position of each sheet even when the conveying speed is increased.

[0060] Furthermore, it is preferable that the timing of applying the identification marker is controlled based on the conveying speed of the long film in the applying step. This can suppress, for example, deviation of the printing position during acceleration or deceleration.

[0061] In addition, in the imparting process, laser markers, inkjet, punching, etc. can be used, and among them, imparting identification markers by laser markers is particularly preferred. For example, when using inkjet to impart identification markers, the ink scatters to the surroundings, and it is possible to misjudge a defective single piece or produce a new defect caused by contamination. In addition, when the defective parts are marked by punching without stopping the conveyance, when the long strip film with a single piece is wound on the reel, the shape change caused by the punching hole may cause the winding quality to deteriorate or the punching mark to be transferred to the single piece in the adjacent winding layer, and the waste caused by the punching needs to be recycled. In addition, the vibration of the film caused by the punching has an adverse effect on the focus of the inspection camera in the front section, making it difficult to mark without stopping the conveyance. As the imparting portion, a laser marker is used, so that these possibilities can be eliminated.

[0062] Hereinafter, the aforementioned Figures 4 to 9 The inspection mark device shown and Figure 10 The following describes the manufacturing step (A), the conveying step (B), the detecting step (C), the inspecting step (D), and the applying step (E) with reference to the flowchart of the inspection method of the long film shown in FIG.

[0063] [Production process (A)] In the production process (A), a long film of a single piece with an adhesive film arranged along the long side direction of the base film is produced. The single piece is preferably formed on the base film by half-cutting, screen printing or inkjet printing. Half-cutting is performed by using a Vick knife to cut only the adhesive film without cutting the base film, and unnecessary parts are removed by cutting. Screen printing uses the pressure caused by a scraper etc. to pass the adhesive relative to the mesh of the screen mask, and prints (applies) it on the base film, for example, using the thickness of the screen mask to produce a single piece of predetermined thickness. The screen mask is a plate with a screen mesh woven from synthetic fibers such as polyester or stainless steel or various metal fibers. When the adhesive contains conductive particles or solder particles, it is sufficient to make the mesh larger than the maximum diameter of the conductive particles or solder particles. Inkjet printing does not require a plate, but directly patterns the data, for example, by controlling the coating amount using the nozzle diameter to produce a single piece of predetermined thickness.

[0064] In addition, the monolithic film can also be a composition of more than 2 layers, or a composition of more than 2 layers of a layer comprising conductive particles or solder particles and a layer not comprising conductive particles or solder particles, or a composition of more than 2 layers of layers comprising conductive particles or solder particles, or a composition of more than 2 layers of layers not comprising conductive particles or solder particles. In the case of constituting a monolithic film by more than 2 layers, it is preferably performed half-cutting after forming a blank (original reverse) of more than 2 layers by coating or lamination. In addition, it is also possible to, after making a monolithic film by screen printing, stack and shape. In addition, it is also possible to, after making a monolithic film by nozzle jet printing (inkjet printing), stack and shape.

[0065] [Conveying process (B)] In the next conveying step (B), the long film is conveyed in the longitudinal direction. In step S11, the control unit unwinds the single long film provided with the adhesive film from the unwinding mechanism 41 and measures the conveying distance indicating the position of the long film in the longitudinal direction.

[0066] [Detection process (C)] In the subsequent detection step (C), each piece of the conveyed long film is detected, and positional information of each piece of the detected position in the longitudinal direction of the long film is obtained. First, in step S12, the control unit uses the detection sensor 42 to determine the presence or absence of the piece of film on the base film, and obtains the measured length value of the conveyed distance as the positional information of each piece of the long film in the longitudinal direction.

[0067] Then, in step S13, the control unit records the single piece number (single piece number) each time a single piece is detected by the detection sensor 42, as in the single piece information shown in Table 1, and records the single piece detection length measurement value (whether or not the detection length measurement is performed) showing the detection position of each single piece in the long side direction of the long strip film in the single piece information.

[0068] Furthermore, the control unit records the length measurement value (camera trigger measurement length) triggered by the imaging, indicating the inspection position of each individual piece by the inspection camera 43, in the individual piece information, as shown in Table 1. Specifically, the control unit offsets the individual piece information by a preset distance from the detection sensor 42 to the inspection camera 43 (300.00 mm in the example of the individual piece information shown in Table 1).

[0069] Furthermore, the control unit records the length measurement value (laser length measurement) used as a printing trigger for the position of each sheet by the laser marker 14, as shown in the sheet information shown in Table 1. Specifically, the control unit offsets the sheet information by a preset distance from the detection sensor 42 to the laser marker 44 (600.00 mm in the example of the sheet information shown in Table 1).

[0070] [Inspection process (D)] In the subsequent inspection step (D), each sheet of the conveyed long film is inspected based on the position information of each sheet, and inspection information for each sheet is obtained. First, in step S14, the control unit determines whether the length measurement value (camera-triggered length measurement) indicating the inspection position of each sheet by the inspection camera 13 has been reached. If the length measurement value is determined to have been reached, the process proceeds to step S15.

[0071] Next, in step S15, the control unit uses the inspection camera 13 to capture images of the wafer based on the length measurement value triggered by the image capture, thereby performing a visual inspection. The visual inspection preferably includes two types of inspections: an OK determination for a normal wafer and an NG determination for a defective wafer. For each wafer, an NG signal and an OK signal are output. The control unit stores the inspection information indicating the OK or NG determination result of the visual inspection in memory as wafer information.

[0072] [Providing step (E)] In the subsequent assigning step (E), an identification marker is assigned to a predetermined sheet of the conveyed long film or to at least one of the substrate films on which the predetermined sheet is placed, based on the positional information and inspection information of each sheet. First, in step S16, the control unit determines whether the length measurement value triggered by printing, which is the assigning position of each sheet, has been reached by the laser marker 44. If it is determined that the length measurement value triggered by imaging has been reached, the process proceeds to step S17.

[0073] Next, in step S17 , the control unit determines whether the inspection result of the predetermined wafer is OK based on the wafer information recorded in the memory, and proceeds to step S19 if the inspection result is OK, and proceeds to step S18 if the inspection result is NG.

[0074] In step S18 , the control unit causes the laser marker 44 to mark defective sheets with an NG sheet information inspection result, and the process proceeds to step S19 . In step S19 , the control unit winds the inspected and marked long film onto the recovery reel of the winding mechanism 45 .

[0075] According to such a method for producing a long film, the adhesive film sheets can be inspected at high speed without stopping the conveyance, and an identification mark can be given to at least one of a predetermined sheet or a base film, thereby improving productivity.

[0076] <4. Method for Manufacturing Connected Structure> The manufacturing method of the connection structure involved in this embodiment includes: an attaching process, which uses a long film to attach only a normal single chip to the first electronic component or the second electronic component having a terminal row based on an identification marker, and the long film has a long base film and a single chip of an adhesive film arranged along the long side direction of the aforementioned base film, and an identification marker is given to a predetermined single chip or at least one side of the base film arranged with the predetermined single chip so that a defective single chip can be distinguished; and a connecting process, which connects the terminal of the first electronic component to the terminal of the second electronic component via the normal single chip.

[0077] [Attachment process] In the attaching process, the aforementioned long film strip is used to attach only normal individual chips to the first or second electronic component having a terminal array based on the identification mark. For example, defective individual chips are identified through image recognition and discarded. A attaching device presses the normal individual chips from the base film side and attaches the individual chips to the mounting surface of the first or second electronic component on the stage. The transferred individual chips are wound as only the base film. The defective individual chips can be wound together with the base film, or after being attached to the recovery unit, they can be wound as only the base film.

[0078] [Connection process] In the connection process, the terminals of the first electronic component and the terminals of the second electronic component are connected via a normal sheet. For example, a crimping tool is used to press against the terminal arrays of the first and second electronic components through a cushioning material. Furthermore, the sheet is cured by heating, light irradiation, or other methods depending on the curing type of the adhesive film on the sheet.

[0079] According to such a method for producing a connection structure, the performance of the adhesive film used can be maintained as a single sheet, and excellent pressure-bonding characteristics (conductivity, bonding strength, insulation, reliability, etc.) of the connection structure can be obtained. Description of Reference Numerals

[0080] 10 long film, 11 base film, 21 to 25 single pieces, 30 identification marker, 40 inspection marking device, 41 unwinding mechanism, 42 detection sensor, 43 inspection camera, 44 laser marker, 45 winding mechanism, 50 to 56 single pieces.

Claims

1. A long film having a long base film and a sheet of an adhesive film arranged along the long side direction of the base film, wherein an identification mark is given to a predetermined sheet or at least one of the base films on which the predetermined sheet is arranged so that a defective sheet can be identified.

2. The long film according to claim 1, wherein: An end region formed of the base film is provided at an end portion in the width direction of the long film, and the identification marker is provided in the end region.

3. The long film according to claim 2, wherein: The length of the edge region in the width direction is 100 μm or more.

4. The long film according to any one of claims 1 to 3, wherein The single sheet has a window frame portion where the base film is exposed, and the identification marker is provided on the base film of the window frame portion.

5. The long film according to any one of claims 1 to 4, wherein The identification mark is formed by laser printing.

6. The long film according to any one of claims 1 to 5, wherein: The long film is wound on a reel.

7. A method for manufacturing a connection structure, comprising: A step of attaching only normal chips to a first electronic component or a second electronic component having a terminal array based on an identification mark using a long film strip, the long film strip having a long base film and a chip of an adhesive film arranged along a long side direction of the base film, and giving the identification mark to at least one of a predetermined chip or a base film on which the predetermined chip is arranged so as to be able to distinguish a defective chip; and A connecting step of connecting the terminal of the first electronic component and the terminal of the second electronic component via the normal chip.