Method for improving width difference between upper and lower surfaces of steel plate

By optimizing the slab heating and rolling process, controlling the slab outlet temperature and rolling roll diameter difference, the width difference caused by uneven end surfaces of the steel plate thickness is solved, and the material yield and surface quality of the steel plate are improved.

CN118926308AInactive Publication Date: 2024-11-12BAOTOU IRON & STEEL (GROUP) CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202411185574.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-27
Publication Date
2024-11-12
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

During the steel plate rolling process, due to the uneven end surface of the slab thickness, the width difference between the upper and lower surfaces of the steel plate is large, resulting in an increase in the width margin of the steel plate to ensure shear quality, resulting in waste and loss of material yield.

Method used

By optimizing the slab heating and rolling process, it includes controlling the upper and lower surface temperature difference of the slab outlet temperature, adjusting the upper and lower roller diameter difference of the rough rolling mill working roller, and controlling the sled value to reduce the inverted trapezoidal shape of the steel plate.

Benefits of technology

It effectively reduces the width difference between the upper and lower surfaces of the steel plate, reduces the cutting amount of the edges of the steel plate, improves the yield rate, and ensures the surface quality of the steel plate.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a method for improving the width difference between the upper and lower surfaces of a steel plate, which comprises the following steps of: 1) controlling the temperature difference between the upper and lower surfaces of a plate blank, namely enhancing the lower heating of the plate blank and increasing the heating temperature of the lower surface to ensure that the temperature difference between the upper and lower surfaces of the discharged plate blank is less than or equal to 20 DEG C; 2) controlling the diameter difference of the upper and lower working rollers of the roughing mill: controlling the diameter difference of the upper and lower working rollers of the roughing mill within 40mm; and (3) sled control during rolling of the steel plate: when the steel plate is rolled in the broadening sequence of the roughing mill, the sled value is controlled to be 3-8%. According to the method for improving the width difference between the upper surface and the lower surface of the steel plate, by optimizing the heating and rolling processes, the risk that the width of the steel plate is short due to the fact that the cutting amount of the edge of the steel plate is increased due to uneven end faces of wide and thick plates in a factory is solved, and the yield of the steel plate is increased.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of hot rolling, and in particular relates to a method for improving the width difference between the upper and lower surfaces of a steel plate. Background Art

[0002] When casting wide and thick slabs, the casting machine generally uses light pressure to improve the internal quality of the slabs. The continuous casting slabs will have uneven thickness end faces, wide upper surface width and narrow lower surface width. When the steel plate is rolled, after widening and rolling, due to the influence of the width ratio, the width difference between the upper and lower surfaces of the steel plate is further increased. The thicker the steel plate, the wider the width, and the larger the width ratio, the more obvious this phenomenon is, showing an "inverted trapezoidal" phenomenon. The width of the upper surface of the steel plate is generally about 30mm larger than the lower surface, and the maximum reaches more than 50mm. Wide and thick plates are generally delivered by four-cutting, and the steel plates need to be cut on both sides. Since the width of the lower surface is narrower than the width of the upper surface, in order to ensure the shearing quality of the lower surface of the steel plate, the width margin of the rolled large plate must be increased, which will cause waste and loss of yield. At the same time, since the thickness end face of the steel plate is inverted trapezoidal, it cannot be cut off on the shearing line, and can only be added with a fire cutting process. In serious cases, it will cause the contract to be broken, resulting in greater losses. Therefore, how to reduce the width difference between the upper and lower surfaces of the rolled large plate, reduce the width margin of the rolled large plate, and reduce the number of unqualified products is an urgent problem that needs to be solved in the production of wide and thick steel plates.

[0003] The document "Slab Width Deviation Control Practice" improves the slab width control accuracy by adjusting the chemical composition, determining the steel grade width shrinkage coefficient and dynamically controlling the cooling intensity of the casting. This patent effectively improves the width difference problem of the upper and lower surfaces of the steel plate and improves the steel plate yield rate by optimizing the slab heating and rolling process.

[0004] The document "Improvement and Application of Hot-rolled Strip Width Exceeding Tolerance Control Technology" mainly solves the problem of steel plate width exceeding tolerance by optimizing rolling models and equipment accuracy. This patent effectively improves the problem of width difference between the upper and lower surfaces of the steel plate and improves the steel plate yield rate by optimizing the slab heating and rolling process. Summary of the invention

[0005] The purpose of the present invention is to provide a method for improving the width difference between the upper and lower surfaces of a steel plate. By optimizing the heating and rolling processes, the method solves the risk of increasing the cutting amount of the edge of the steel plate caused by the uneven thickness end faces of the wide and thick plates in our factory, thereby improving the yield rate of the steel plate.

[0006] In order to solve the above technical problems, the present invention adopts the following technical solutions:

[0007] The present invention provides a method for improving the width difference between the upper and lower surfaces of a steel plate, comprising:

[0008] 1) Control of the temperature difference between the upper and lower surfaces of the slab out of the furnace: If the upper surface temperature of the slab out of the furnace is higher than the lower surface temperature, the upper surface will be pressed more than the lower surface during widening rolling, and the steel plate will appear in an inverted trapezoid after rolling. The greater the temperature difference between the upper and lower surfaces, the more serious the inverted trapezoid after widening rolling. Therefore, by strengthening the heating of the slab below and increasing the heating temperature of the lower surface, the temperature difference between the upper and lower surfaces of the slab out of the furnace is less than or equal to 20°C;

[0009] 2) Control of the difference in roll diameter between the upper and lower working rolls of the roughing mill: Under a constant rolling force, the smaller the roll diameter, the greater the reduction. The roll diameter of the lower working roll is reduced, the roll diameter of the upper working roll is increased, and the reduction of the lower surface during widening rolling is increased, so that the extension deformation of the lower surface of the steel plate is greater than that of the upper surface, which will reduce the width difference between the upper and lower surfaces of the steel plate and reduce the inverted trapezoid of the steel plate; when matching the working rolls of the roughing mill, it is required that the roll diameter of the lower working roll is smaller than that of the upper roll; adjust the matching rolls of the roughing mill to control the difference in the upper and lower roll diameters of the working rolls of the roughing mill within 40 mm;

[0010] 3) Sled control during steel plate rolling: Since warping or buckling is inevitable during the rolling of the intermediate billet, if the billet buckles during widening rolling, the upper surface width of the steel plate will be greater than the lower surface width after rolling, presenting an inverted trapezoidal phenomenon; in order to reduce the buckling phenomenon during steel plate rolling, the sled value of the steel plate during widening sequence rolling is controlled to a positive value, that is, the linear speed of the lower working roll is required to be greater than that of the upper working roll during rolling, so that the steel plate is straight or slightly warped after widening rolling; when the steel plate is rolled in the widening sequence of the roughing mill, the sled value is controlled between 3% and 8%.

[0011] Furthermore, in 1), the temperature difference between the upper and lower surfaces of the slab out of the furnace is less than or equal to 18°C.

[0012] Furthermore, the temperature difference between the upper and lower surfaces of the slab out of the furnace is made less than or equal to 15°C.

[0013] Furthermore, in the above 2), the diameter difference between the upper and lower rolls of the roughing mill working rolls is controlled within 30 mm.

[0014] Furthermore, in the above 2), the diameter difference between the upper and lower rolls of the roughing mill working rolls is controlled within 25 mm.

[0015] Furthermore, in the above 3), when the steel plate is rolled in the widening sequence of the roughing mill, the sled value is controlled between 5% and 6%.

[0016] Furthermore, the upper surface of the continuous casting billet cross-sectional width is 11mm wider than the lower surface, the lower heating is strengthened when the slab is heated, the temperature difference between the upper and lower surfaces of the slab out of the furnace is 20°C, the roller diameter difference between the upper and lower working rolls of the roughing mill is 38mm, and the sled value is 8% when the roughing mill is rolling in a widening sequence; the upper surface of the rolled steel plate is 4mm wider than the lower surface, and the inverted trapezoid is small. After the steel plate is cut, the surface quality of the edge of the steel plate is checked, and the surface quality is normal and can be delivered normally.

[0017] Furthermore, the upper surface of the continuous casting billet cross-sectional width is 10mm wider than the lower surface, the lower heating is strengthened when the slab is heated, the temperature difference between the upper and lower surfaces of the slab out of the furnace is 16°C, the roller diameter difference between the upper and lower working rolls of the roughing mill is 32mm, and the sled value is 4% when the roughing mill is rolling in a widening sequence; the upper surface of the rolled steel plate is 3.5mm wider than the lower surface, and the inverted trapezoid is small. After the steel plate is cut, the surface quality of the edge of the steel plate is checked, and the surface quality is normal and can be delivered normally.

[0018] Furthermore, the upper surface of the continuous casting billet cross-sectional width is 11mm wider than the lower surface, the lower heating is strengthened when the slab is heated, the temperature difference between the upper and lower surfaces of the slab out of the furnace is 11°C, the roller diameter difference between the upper and lower working rolls of the roughing mill is 23mm, and the sled value is 4.5% when the roughing mill is rolling in a widening sequence; the upper surface of the rolled steel plate is 2mm wider than the lower surface, and the inverted trapezoid is small. After the steel plate is cut, the surface quality of the edge of the steel plate is checked, and the surface quality is normal and can be delivered normally.

[0019] Compared with the prior art, the beneficial technical effects of the present invention are:

[0020] The invention solves the risk of increased edge cutting of steel plates and short width of steel plates caused by uneven end faces of wide and thick plates in our factory by optimizing heating and rolling processes, thereby improving the yield rate of steel plates. DETAILED DESCRIPTION

[0021] The present invention is further described in detail below with reference to specific embodiments.

[0022] The process sequence adopted in the embodiment is: heating - rolling - cutting - product surface quality inspection - warehousing.

[0023] Embodiment 1:

[0024] The upper surface of the continuous casting billet is 11mm wider than the lower surface. The lower heating is strengthened when the billet is heated. The temperature difference between the upper and lower surfaces of the billet out of the furnace is 20℃. The diameter difference between the upper and lower working rolls of the roughing mill is 38mm. When the roughing mill is rolling in a widening sequence, the sled value is 8%. The upper surface of the rolled steel plate is 4mm wider than the lower surface, and the inverted trapezoid is small. After the steel plate is cut, the surface quality of the edge of the steel plate is checked. The surface quality is normal and can be delivered normally.

[0025] Embodiment 2:

[0026] The upper surface of the continuous casting billet is 10mm wider than the lower surface. The lower heating is strengthened when the billet is heated. The temperature difference between the upper and lower surfaces of the billet out of the furnace is 16°C. The diameter difference between the upper and lower working rolls of the roughing mill is 32mm. When the roughing mill is rolling in a widening sequence, the sled value is 4%. The upper surface of the rolled steel plate is 3.5mm wider than the lower surface, and the inverted trapezoid is small. After the steel plate is cut, the surface quality of the edge of the steel plate is checked. The surface quality is normal and can be delivered normally.

[0027] Embodiment 3:

[0028] The upper surface of the continuous casting billet is 11mm wider than the lower surface. The lower heating is strengthened when the billet is heated. The temperature difference between the upper and lower surfaces of the billet out of the furnace is 11°C. The diameter difference between the upper and lower working rolls of the roughing mill is 23mm. When the roughing mill is rolling in a widening sequence, the sled value is 4.5%. The upper surface of the rolled steel plate is 2mm wider than the lower surface, and the inverted trapezoid is small. After the steel plate is cut, the surface quality of the edge of the steel plate is checked. The surface quality is normal and can be delivered normally.

[0029] The embodiments described above are only descriptions of the preferred modes of the present invention, and are not intended to limit the scope of the present invention. Without departing from the design spirit of the present invention, various modifications and improvements made to the technical solutions of the present invention by ordinary technicians in this field should all fall within the protection scope determined by the claims of the present invention.

Claims

1. A method for improving the width difference between the upper and lower surfaces of a steel plate. Features: include: 1) Control of the temperature difference between the upper and lower surfaces of the slab out of the furnace: If the upper surface temperature of the slab out of the furnace is higher than the lower surface temperature, the upper surface will be pressed more than the lower surface during widening rolling, and the steel plate will appear in an inverted trapezoid after rolling. The greater the temperature difference between the upper and lower surfaces, the more serious the inverted trapezoid after widening rolling. Therefore, by strengthening the heating of the slab below and increasing the heating temperature of the lower surface, the temperature difference between the upper and lower surfaces of the slab out of the furnace is less than or equal to 20°C; 2) Control of the difference in roll diameter between the upper and lower working rolls of the roughing mill: Under a constant rolling force, the smaller the roll diameter, the greater the reduction. The roll diameter of the lower working roll is reduced, the roll diameter of the upper working roll is increased, and the reduction of the lower surface during widening rolling is increased, so that the extension deformation of the lower surface of the steel plate is greater than that of the upper surface, which will reduce the width difference between the upper and lower surfaces of the steel plate and reduce the inverted trapezoid of the steel plate; when matching the working rolls of the roughing mill, it is required that the roll diameter of the lower working roll is smaller than that of the upper roll; adjust the matching rolls of the roughing mill to control the difference in the upper and lower roll diameters of the working rolls of the roughing mill within 40 mm; 3) Sled control during steel plate rolling: Since warping or buckling is inevitable during the rolling of the intermediate billet, if the billet buckles during widening rolling, the upper surface width of the steel plate will be greater than the lower surface width after rolling, presenting an inverted trapezoidal phenomenon; in order to reduce the buckling phenomenon during steel plate rolling, the sled value of the steel plate during widening sequence rolling is controlled to a positive value, that is, the linear speed of the lower working roll is required to be greater than that of the upper working roll during rolling, so that the steel plate is straight or slightly warped after widening rolling; when the steel plate is rolled in the widening sequence of the roughing mill, the sled value is controlled between 3% and 8%.

2. The method for improving the width difference between the upper and lower surfaces of a steel plate according to claim 1, Features: In the above 1), the temperature difference between the upper and lower surfaces of the slab out of the furnace is made less than or equal to 18°C.

3. The method for improving the width difference between the upper and lower surfaces of a steel plate according to claim 2, Features: Make the temperature difference between the upper and lower surfaces of the slab out of the furnace less than or equal to 15℃.

4. The method for improving the width difference between the upper and lower surfaces of a steel plate according to claim 1, Features: In the above 2), the diameter difference between the upper and lower rolls of the roughing mill working rolls is controlled within 30 mm.

5. The method for improving the width difference between the upper and lower surfaces of a steel plate according to claim 4, Features: The diameter difference between the upper and lower rolls of the roughing mill working rolls shall be controlled within 25mm.

6. The method for improving the width difference between the upper and lower surfaces of a steel plate according to claim 1, Features: In the above 3), when the steel plate is rolled in the widening sequence of the roughing mill, the sled value is controlled between 5 and 6%.

7. The method for improving the width difference between the upper and lower surfaces of a steel plate according to claim 1, Features: The upper surface of the continuous casting billet section width is 11mm wider than the lower surface. The lower heating is strengthened when the slab is heated. The temperature difference between the upper and lower surfaces of the slab out of the furnace is 20℃. The diameter difference between the upper and lower working rolls of the roughing mill is 38mm. When the roughing mill is rolling in a widening sequence, the sled value is 8%; the upper surface of the rolled steel plate is 4mm wider than the lower surface, and the inverted trapezoid is small. The surface quality of the edge of the steel plate is checked after cutting. The surface quality is normal and can be delivered normally.

8. The method for improving the width difference between the upper and lower surfaces of a steel plate according to claim 1, Features: The upper surface of the continuous casting billet section width is 10mm wider than the lower surface. The lower heating is strengthened when the slab is heated. The temperature difference between the upper and lower surfaces of the slab out of the furnace is 16°C. The diameter difference between the upper and lower working rolls of the roughing mill is 32mm. When the roughing mill is rolling in a widening sequence, the sled value is 4%; the upper surface of the rolled steel plate is 3.5mm wider than the lower surface, and the inverted trapezoid is small. The surface quality of the edge of the steel plate is checked after cutting. The surface quality is normal and can be delivered normally.

9. The method for improving the width difference between the upper and lower surfaces of a steel plate according to claim 1, Features: The upper surface of the continuous casting billet section width is 11mm wider than the lower surface. The lower heating is strengthened when the slab is heated. The temperature difference between the upper and lower surfaces of the slab out of the furnace is 11°C. The roller diameter difference between the upper and lower working rolls of the roughing mill is 23mm. When the roughing mill is rolling in a widening sequence, the sled value is 4.5%; the upper surface of the rolled steel plate is 2mm wider than the lower surface, and the inverted trapezoid is small. The surface quality of the edge of the steel plate is checked after cutting. The surface quality is normal and can be delivered normally.

Citation Information

Patent Citations

  • Method for improving rectangularity of transverse section of wide and thick steel plate

    CN115463976A

  • Method for eliminating inverted trapezoidal cross section of intermediate blank of wide and thick plate

    CN118385284A