Machining method for forged aluminum alloy milling wheel

By adopting a multi-step milling and setting specific structural features during the machining process of forged aluminum alloy wheels, the problem of deformation and size changes of aluminum alloy wheels after milling is solved, and the yield rate and product quality are improved. stability.

CN118926843AActive Publication Date: 2024-11-12TIANJIN NANUO MACHINERY MFG
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411187860.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-28
Publication Date
2024-11-12
Estimated Expiration
2044-08-28

AI Technical Summary

Technical Problem

Forged aluminum alloy wheels are prone to deformation after milling, resulting in the finished product size exceeding the product drawing requirements and low yield.

Method used

A machining method is adopted, including turning the blank to obtain the blank material, then milling to obtain the milling material, then turning the blank to obtain the rough material, and drilling the bolt hole and valve hole at the end. Ensure the product meets the size requirements. Specific dimensional retention and structural features, such as weight reduction holes and mounting surface drainage tanks, can be set in this method to reduce deformation and dimensional changes.

Benefits of technology

Effectively reduce or avoid deformation of forged aluminum alloy wheels after milling, ensure that the product size meets the requirements, improves yield, and simplify operations to improve the stability and reliability of product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118926843A_ABST
    Figure CN118926843A_ABST
Patent Text Reader

Abstract

The invention discloses a machining method for a forged aluminum alloy milling wheel, which comprises the following steps of: turning a blank to obtain a smooth blank material; the polished blank material is milled, and a milled material is obtained; turning the milling material to obtain a rough turning material; bolt hole and valve hole drilling is conducted on the rough turning material, and a product meeting the product drawing size requirement is obtained; the deformation of the forged aluminum alloy milling wheel after milling can be reduced or avoided, the size change of a part of a product is reduced or avoided, and the yield is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of wheel machining production, and in particular relates to a machining method for forged aluminum alloy milling wheels. Background Art

[0002] In the production process of forged aluminum alloy milling wheels, the machining method of the prior art is: according to the product drawing size, the rough turning material is turned from the blank; then the milling material is milled, and finally the finished product is drilled.

[0003] Due to the thin wall thickness of the forged aluminum alloy wheel rim and the large internal stress of the forged aluminum alloy wheel, the above-mentioned machining method of the prior art easily causes deformation of the product after milling, and the final size of the finished product exceeds the requirements of the product drawing, resulting in a low yield rate. Summary of the invention

[0004] The purpose of the present invention is to provide a machining method for forged aluminum alloy milled wheels, reduce or avoid deformation of forged aluminum alloy milled wheels after milling, reduce or avoid partial dimensional changes of products, and improve the yield rate.

[0005] In order to achieve the above object, the present invention adopts the following technical solutions:

[0006] The present invention provides a machining method for a forged aluminum alloy wheel by milling, comprising the following steps:

[0007] The blank is turned to obtain a rough blank material;

[0008] Milling the blank material to obtain a milled material;

[0009] Turning the milled material to obtain a rough-turned material;

[0010] The rough-turned material is subjected to drilling processing for bolt holes and valve holes to obtain a product that meets the size requirements of the product drawing.

[0011] Preferably, when the blank is turned to obtain the rough blank material, the dimensional margin Da between position A and the finished product is set to 0.6 mm.

[0012] Preferably, the dimensional allowance Dd between position D and the finished product is set to 0.

[0013] Preferably, the dimensional margin De between the mounting surface at position E and the finished product is set to 1 mm.

[0014] Preferably, the radius of the center hole, the cover and the stop at position F and the dimension Df allowed between the finished product is set to 2 mm.

[0015] Preferably, a dimensional margin is set between the radius of the rim and the finished product.

[0016] Preferably, the rough-turned material is provided with weight-reducing holes.

[0017] Preferably, the number of the weight-reducing holes is at least two and they are evenly distributed along the circumference.

[0018] Preferably, the rough-turned material is provided with a mounting surface drainage groove.

[0019] Preferably, the number of drainage grooves on the mounting surface is at least two and they are evenly distributed along the circumference.

[0020] The machining method of forged aluminum alloy wheel milling provided by the present invention has the following beneficial effects:

[0021] The machining method of the forged aluminum alloy milled wheel of the present invention can reduce or avoid deformation of the forged aluminum alloy milled wheel after milling due to the thin wall thickness of the forged aluminum alloy wheel rim and the large internal stress of the forged aluminum alloy wheel, reduce or avoid changes in part dimensions of the product, avoid part dimensions exceeding the requirements of the product drawings, and improve the yield rate; the operation is simple and the quality of the obtained products is stable and reliable. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 The invention is a structural schematic diagram of a rough turning material of a machining method of a forged aluminum alloy wheel milling process in the prior art.

[0023] Figure 2 The invention is a structural schematic diagram of the milling material of the machining method of forged aluminum alloy milling wheel in the prior art.

[0024] Figure 3 The figure is a flow chart of a machining method for a forged aluminum alloy wheel milling process provided by one embodiment of the present invention.

[0025] Figure 4 It is a schematic structural diagram of a blank of a machining method for a forged aluminum alloy wheel milling process provided by an embodiment of the present invention.

[0026] Figure 5 It is a structural schematic diagram of a blank material of a machining method for a forged aluminum alloy wheel milling process provided by an embodiment of the present invention.

[0027] Figure 6 It is a structural schematic diagram of a milling material in a machining method for a forged aluminum alloy wheel milling provided by an embodiment of the present invention.

[0028] Figure 7 It is a structural schematic diagram of a rough turning material of a machining method for a forged aluminum alloy wheel milling process provided by an embodiment of the present invention.

[0029] Figure 8 It is a schematic diagram of the finished product structure of a machining method for forged aluminum alloy milling wheel provided in one embodiment of the present invention.

[0030] Fig. 9 It is a product cross-sectional structural diagram of a machining method for a forged aluminum alloy wheel milling process provided by one embodiment of the present invention.

[0031] Fig.10 yes Fig. 9 A partial enlarged view of point I in the middle.

[0032] Fig.11 yes Fig. 9 A partial enlarged view of point II in the middle.

[0033] Fig.12 yes Fig. 9 A partial enlarged view of point III in the middle.

[0034] Reference numerals in the figures:

[0035] 1 is the blank, 2 is the polished material, 3 is the milled material, 310 is the window molding position, 320 is the rim, 4 is the rough-turned material, 401 is the bolt hole, 402 is the valve hole, 410 is the center hole, 420 is the cover, 430 is the stop, 440 is the weight reduction hole, 450 is the drainage groove of the installation surface, and 5 is the finished product. DETAILED DESCRIPTION

[0036] The present invention is further described in detail below through the accompanying drawings and specific embodiments.

[0037] Example

[0038] Please refer to Figures 3 to 12 The present embodiment provides a machining method for a forged aluminum alloy wheel by milling. The machining method for a forged aluminum alloy wheel by milling comprises the following steps:

[0039] Step S1, lathe the blank 1 to obtain a rough blank material 2;

[0040] Step S2, milling the blank material 2 to obtain a milled material 3;

[0041] Step S3, turning the milled material 3 to obtain a rough-turned material 4;

[0042] Step S4, drilling the bolt hole 401 and the valve hole 402 of the rough-turned material 4 to obtain a product that meets the size requirements of the product drawing.

[0043] In the machining method of forged aluminum alloy milling wheel of this embodiment, the bare blank material 2 is milled to obtain the milled material 3, which is convenient for forming the window shape position 310, and the window shape is used for heat dissipation and aesthetics; please refer to Figure 1 and Figure 2 Compared with the prior art in which the window shape is formed when the blank is turned into a rough-turned material, this embodiment is beneficial to reducing the deformation of the forged aluminum alloy milling wheel after milling, reducing or avoiding the change of part size of the product, and improving the yield rate.

[0044] The drilling of the bolt hole 401 and the valve hole 402 can be performed in a machining center. The bolt hole 401 is set as a light hole, which is used to install the wheel on the car through the bolt set in the bolt hole 401. The valve hole 402 is used to install the valve core.

[0045] Please refer to Figure 5 , Figures 10 to 12 In some embodiments, in step S1, when the blank 1 is turned to obtain the bare blank material 2, the dimension allowance Da between position A and the finished product 5 is set to 0.6 mm. Among them, position A is located at the window molding position 310, and the dimension allowance Da refers to the single-side wall thickness allowance. The dimension allowance Dd between position D and the finished product 5 is set to 0. Among them, position D is located at the window molding position 310, and the dimension allowance Dd refers to the single-side wall thickness allowance. The dimension allowance De between the mounting surface at position E and the finished product 5 is set to 1 mm. Among them, position E is located at the position of the mounting surface drainage groove 450, and the dimension allowance De refers to the single-side wall thickness allowance. The dimension allowances Db and Dc between positions B and C on the rim 320 and the finished product 5 are set to 0.6 mm respectively, and the dimension allowances Db and Dc refer to the single-side wall thickness allowances.

[0046] Please refer to Figure 6 , Fig.10 and Fig.12 In some embodiments, in step S1, when the blank 1 is turned to obtain the bare blank material 2, the radius of the center hole 410, the cover 420 and the stop 430 at position F and the finished product 5 are set to a size allowance Df of 2 mm, and the size allowance Df refers to the radius allowance.

[0047] In addition, the radius of the rim 320 can also be set with a size margin between the finished product 5, and the size margin can be a radius margin, and is greater than 0. This is more conducive to reducing or avoiding the deformation of the forged aluminum alloy milling wheel after milling, reducing or avoiding the change of the product size, and improving the yield rate. Figure 2The milled material obtained by milling the rough-turned material in the prior art method shown has a rim, a center hole diameter, a cover and a stopper diameter that are consistent with the product drawing. The rim 320 is used to mount the tire. The center hole 410 is used to penetrate and connect the axle. The cover 420 and the stopper 430 are used to clamp the cap and the wheel.

[0048] Please refer to Figure 7 In some embodiments, in step S3, the milling material 3 is turned to obtain the rough-turned material 4, and a center hole 410 is formed. In addition, the rough-turned material 4 can be provided with a weight-reducing hole 440. The weight-reducing holes 440 are set to at least two and are evenly distributed along the circumference. The rough-turned material 4 can be provided with a mounting surface drainage groove 450. The mounting surface drainage groove 450 is set to at least two and is evenly distributed along the circumference. It can be seen that the rough-turned material 4 of this embodiment is different from the rough-turned material 4 of this embodiment. Figure 1 Compared with the rough-turned material obtained by turning the blank in the prior art method shown, weight-reducing holes 440 and mounting surface drainage grooves 450 are added, which is conducive to reducing weight and improving drainage effect and efficiency.

[0049] The above embodiments are merely examples for the purpose of clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection of the invention.

[0050] It should be noted that, in the absence of conflict, the embodiments of the present invention and the features in the embodiments may be combined with each other.

Claims

1. A machining method for forged aluminum alloy wheel milling, characterized in that: The following steps are involved: The blank is turned to obtain a rough blank material; Milling the blank material to obtain a milled material; Turning the milled material to obtain a rough-turned material; The rough-turned material is subjected to drilling processing for bolt holes and valve holes to obtain a product that meets the size requirements of the product drawing.

2. The machining method of forged aluminum alloy wheel milling according to claim 1, characterized in that: When the blank is turned to obtain the rough blank material, the dimension margin Da between position A and the finished product is set to 0.6 mm.

3. The machining method of forged aluminum alloy wheel by milling according to claim 2, characterized in that: The dimension allowance Dd between position D and the finished product is set to 0.

4. The machining method of forged aluminum alloy wheel milling according to claim 3, characterized in that: The dimensional margin De between the mounting surface at position E and the finished product is set to 1 mm.

5. The machining method of forged aluminum alloy wheel by milling according to claim 4, characterized in that: The dimension margin Df between the radius of the center hole, the cover and the stop at position F and the finished product is set to 2 mm.

6. The machining method of forged aluminum alloy wheel by milling according to claim 5, characterized in that: A dimensional margin is set between the radius of the rim and the finished product.

7. The machining method of forged aluminum alloy wheel by milling according to any one of claims 1 to 6, characterized in that: The rough turning material is provided with weight reduction holes.

8. The machining method of forged aluminum alloy wheel by milling according to claim 7, characterized in that: The number of the weight-reducing holes is at least two and they are evenly distributed along the circumference.

9. The machining method of forged aluminum alloy wheel by milling according to claim 7, characterized in that: The rough-turned material is provided with a mounting surface drainage groove.

10. The machining method of forged aluminum alloy wheel by milling according to claim 9, characterized in that: The number of drainage grooves on the mounting surface is at least two and they are evenly distributed along the circumference.

Citation Information

Patent Citations

  • System for charging and securing an electronic device in a vehicle

    CN105916738A

  • Process for forging hub

    CN110561052A

  • Machining technology and manufacturing technology of hub

    CN110666188A

  • Machining method of high-strength forged hub

    CN112643287A