Method for preparing tetrahydropyrrole through tetrahydrofuran amination
By using the reaction of molded ZSM-5/ZSM-11 eutectic molecular sieve catalyst with tetrahydrofuran and ammonia, the problem of difficult industrial preparation of powder catalysts in the prior art is solved, and the high selectivity and yield of tetrahydropyrrole is achieved, which simplifies the The reaction device is reduced and the cost is reduced.
Patent Information
- Application Number
- CN202310537621.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-12
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2043-05-12
AI Technical Summary
The existing catalysts are powdery, making it difficult to achieve industrial preparation of tetrahydropyrrole, and have high requirements for reactors.
The preparation of tetrahydropyrrole is achieved by reacting with tetrahydrofuran and ammonia by using the molded ZSM-5/ZSM-11 eutectic molecular sieve catalyst, and the reaction device is simplified.
While maintaining high selectivity and yield, industrial production of tetrahydropyrrole is achieved, reducing catalyst costs and simplifying the operation process.
Smart Images

Figure BDA0004227638980000051 
Figure BDA0004227638980000061
Abstract
Description
Technical Field
[0001] The present application relates to a method for preparing tetrahydropyrrole by amination of tetrahydrofuran, belonging to the field of preparation of tetrahydropyrrole. Background Art
[0002] Tetrahydropyrrole is an important intermediate of fine chemicals, which is widely used in organic synthesis, medicine, pesticides, coatings, daily chemicals and other fields. Tetrahydropyrrole can be used to synthesize dozens of drugs such as buflomedil, dextromorphamide tartrate, procyclidine, procyclidine, and carmatelin; Tetrahydropyrrole can be used to synthesize insecticides such as dicamba; Tetrahydropyrrole reacts with aldehydes, ketones and other compounds to generate enamine compounds; Tetrahydropyrrole is an important solvent in the fine chemical and pharmaceutical industries; Tetrahydropyrrole is an organic template for synthesizing molecular sieves such as ZSM-5, ZSM-35, and ZSM-48; In addition, tetrahydropyrrole can also be used as a desulfurizer, additive and other fine chemical raw materials.
[0003] Tetrahydropyrrole can be synthesized from raw materials such as 1,4-butanediol, 1,4-succinonitrile, 1,4-butanediamine, and tetrahydrofuran. Among them, the synthesis of tetrahydropyrrole by catalytic amination of 1,4-butanediol and tetrahydrofuran has the advantages of simple reaction process, low raw material cost, and high atomic utilization rate, and has high industrial application value.
[0004] However, the existing catalysts are all powdered catalysts, which have high requirements on the reactor during the preparation of tetrahydropyrrole and are difficult to achieve industrialization. Summary of the invention
[0005] The present application provides a method for preparing tetrahydropyrrole by amination of tetrahydrofuran, which uses a formed ZSM-5 / ZSM-11 eutectic molecular sieve catalyst, and can industrialize the process of preparing tetrahydropyrrole by amination of tetrahydrofuran while maintaining a high tetrahydropyrrole selectivity and yield.
[0006] According to one aspect of the present application, a method for preparing tetrahydropyrrole by amination of tetrahydrofuran is provided, comprising the following steps:
[0007] The raw material containing tetrahydrofuran and ammonia is contacted with a catalyst for reaction to obtain a tetrahydropyrrole product;
[0008] The catalyst is a ZSM-5 / ZSM-11 eutectic molecular sieve catalyst.
[0009] Optionally, the reaction pressure is 0-3 MPa; the reaction temperature is 150-450°C.
[0010] In the present application, "0 MPa" means a normal pressure state.
[0011] Optionally, the reaction pressure is selected from any value of 0 MPa, 0.5 MPa, 1.0 MPa, 1.5 MPa, 2.0 MPa, 2.5 MPa, 2.8 MPa, 3.0 MPa, or a range between two values.
[0012] Optionally, the reaction temperature is selected from any value of 150°C, 200°C, 220°C, 260°C, 310°C, 320°C, 360°C, 380°C, 400°C, 450°C, or a range between two values.
[0013] Optionally, the space velocity of tetrahydrofuran is 0.02 to 2.0 h -1 .
[0014] Optionally, the space velocity of the tetrahydrofuran is selected from 0.02h -1 、0.08h -1 、0.5h -1 , 1.0h -1 , 1.5h -1 , 1.8h -1 , 2.0h -1 Any value or a range of values between .
[0015] Optionally, the molar ratio of ammonia to tetrahydrofuran in the raw material is 2-20.
[0016] Optionally, the molar ratio of ammonia to tetrahydrofuran in the raw material is selected from any value among 2, 4, 6, 8, 10, 14, 18, 20 or a range value between two values.
[0017] Optionally, the preparation method of the ZSM-5 / ZSM-11 eutectic molecular sieve catalyst comprises the following steps:
[0018] The mixed raw material containing eutectic molecular sieve raw powder, adhesive and sesbania powder is mixed with an acid solution, molded, calcined I, ion exchanged, and calcined II to obtain the ZSM-5 / ZSM-11 eutectic molecular sieve catalyst.
[0019] Optionally, the content of ZSM-5 molecular sieve in the ZSM-5 / ZSM-11 eutectic molecular sieve catalyst is 0 to 99.5 wt %, and the content of ZSM-11 molecular sieve is 0.5 to 100 wt %.
[0020] Optionally, the molar ratio of silicon dioxide to aluminum oxide in the eutectic molecular sieve raw powder is 15-500.
[0021] Optionally, the mass ratio of the eutectic molecular sieve raw powder to the adhesive is 0.05 to 19:1.
[0022] Optionally, the mass of the sesbania powder accounts for 0.1 to 15.0 wt % of the total mass of the eutectic molecular sieve raw powder and the adhesive.
[0023] Optionally, the mass of the acid solution accounts for 10 to 70 wt % of the total mass of the eutectic molecular sieve raw powder and the adhesive.
[0024] Optionally, the concentration of the acid solution is 1-8 wt %.
[0025] Optionally, the adhesive is pseudo-boehmite.
[0026] Optionally, the acid solution is a nitric acid solution.
[0027] Optionally, the forming method is extrusion or ball rolling.
[0028] Optionally, the calcination conditions I are: in an oxygen-containing atmosphere, heating the temperature to 440-600° C. at a heating rate of 0.5-3.0° C. / min, and keeping the temperature for 3-24 hours.
[0029] Optionally, the calcination II conditions are: in an oxygen-containing atmosphere, heating the temperature to 420-550° C. at a heating rate of 0.5-3.0° C. / min, and keeping the temperature for 1-5 hours.
[0030] Optionally, the ion exchange conditions are: temperature 50-95° C., time 0.5-24 h.
[0031] Optionally, the exchange solution for the ion exchange is selected from at least one of oxalic acid, hydrochloric acid, ammonium chloride and ammonium nitrate.
[0032] As a specific method for preparing a ZSM-5 / ZSM-11 eutectic molecular sieve catalyst, the method comprises the following steps:
[0033] 1) The raw materials containing ZSM-5 / ZSM-11 eutectic molecular sieve powder, pseudo-boehmite, and sesbania powder are fully mixed with dilute nitric acid to form a mixture, wherein the content of each component is:
[0034] a) The mass ratio of ZSM-5 / ZSM-11 eutectic molecular sieve raw powder to pseudo-boehmite is (0.05-19):1;
[0035] b) the mass of sesbania powder is 0.1 to 15.0 wt% of the total mass of ZSM-5 / ZSM-11 eutectic molecular sieve powder and binder;
[0036] c) the mass of the dilute nitric acid solution is 10-70wt% of the total mass of the ZSM-5 / ZSM-11 eutectic molecular sieve powder and the binder;
[0037] d) the concentration of the dilute nitric acid solution is 1 to 8 wt%;
[0038] e) The content of ZSM-5 molecular sieve in the ZSM-5 / ZSM-11 eutectic molecular sieve is 0% to 99.5%, the content of ZSM-11 molecular sieve is 0.5% to 100%, and the sum of the content of ZSM-5 molecular sieve and the content of ZSM-11 molecular sieve is 100%.
[0039] f) The molar ratio of silicon dioxide to aluminum oxide in the ZSM-5 / ZSM-11 eutectic molecular sieve raw powder is 15-500.
[0040] 2) slowly raising the temperature (0.5-3°C / min) to 440-600°C under flowing air and maintaining it for 3-24 hours to remove the organic template;
[0041] 3) The calcined sample is exchanged with oxalic acid, hydrochloric acid, ammonium chloride or ammonium nitrate solution and then dried at 60-130°C for 6-12 hours;
[0042] 4) The exchanged sample is slowly heated (0.5-3°C / min) to 420-550°C under a flowing air atmosphere and maintained for 1-5 hours to obtain a hydrogenated ZSM-5 / ZSM-11 eutectic molecular sieve catalyst.
[0043] The beneficial effects of this application include:
[0044] 1) The method for preparing tetrahydropyrrole by amination of tetrahydrofuran provided in the present application adopts a formed ZSM-5 / ZSM-11 eutectic molecular sieve catalyst, which can not only improve the selectivity and yield of the tetrahydropyrrole product but also simplify the reaction device to realize industrial production.
[0045] 2) The method for preparing tetrahydropyrrole by amination of tetrahydrofuran provided in the present application uses a formed ZSM-5 / ZSM-11 eutectic molecular sieve catalyst, and can achieve high tetrahydropyrrole selectivity and yield within the reaction range of 150 to 450°C.
[0046] 3) The method for preparing tetrahydropyrrole by amination of tetrahydrofuran provided in the present application uses a low-cost catalyst, readily available raw materials, and is simple to operate. DETAILED DESCRIPTION
[0047] The present application is described in detail below with reference to embodiments, but the present application is not limited to these embodiments.
[0048] Unless otherwise specified, the raw materials in the examples of this application were purchased through commercial channels.
[0049] The analysis method in the examples of this application is as follows:
[0050] Tetrahydrofuran conversion rate = (tetrahydrofuran carbon moles in reactants - tetrahydrofuran carbon moles in products) / tetrahydrofuran carbon moles in reactants × 100%
[0051] Tetrahydropyrrole selectivity = mole number of tetrahydropyrrole carbon in the product / (mole number of tetrahydrofuran carbon in the reactant - mole number of tetrahydrofuran carbon in the product) × 100%
[0052] Tetrahydropyrrole yield = mole number of tetrahydropyrrole carbon in the product / mole number of tetrahydrofuran carbon in the reactant × 100%
[0053] In the examples of the present application, the tetrahydrofuran conversion, tetrahydropyrrole selectivity and tetrahydropyrrole yield are all calculated based on the carbon molar number.
[0054] Example 1
[0055] 11.36g ZSM-5 / ZSM-11 eutectic molecular sieve (88% on dry basis, 95% ZSM-5 content, 400 molar ratio of silica to alumina), 116.13g pseudo-boehmite (77.5% on dry basis), 12.00g sesbania powder, and 20.00g dilute nitric acid solution with a mass concentration of 6.5wt% were fully mixed and formed by extrusion. Dry at 80°C for 12h. Then, heat to 580°C at 1.5°C / min and keep for 4h to remove the organic template. Ion exchange was performed with 0.8mol / L ammonium nitrate solution and repeated three times. After drying at 120°C, heat to 530°C at 1.5°C / min and keep for 4h. Thus, a columnar catalyst with a ZSM-5 / ZSM-11 eutectic molecular sieve content of 10% was obtained, which was recorded as catalyst A.
[0056] Example 2
[0057] 51.14g ZSM-5 / ZSM-11 eutectic molecular sieve (dry basis 88%, ZSM-5 content 55%, silica to alumina molar ratio of 25), 70.97g pseudo-boehmite (dry basis 77.5%), 8.00g sesbania powder, 60.00g dilute nitric acid solution with a mass concentration of 2.0wt% were fully mixed and formed by rolling. Dry at 90°C for 8h. Then, heat to 460°C at 2.5°C / min and keep for 20h to remove the organic template. Ion exchange was performed with 0.8mol / L oxalic acid solution and repeated three times. After drying at 80°C, heat to 450°C at 2.5°C / min and keep for 2h. Thus, a spherical catalyst with a ZSM-5 / ZSM-11 eutectic molecular sieve content of 45% was obtained, which was recorded as catalyst B.
[0058] Example 3
[0059] 102.27g ZSM-5 / ZSM-11 eutectic molecular sieve (88% on dry basis, 10% ZSM-5 content, 60 molar ratio of silica to alumina), 12.90g pseudo-boehmite (77.5% on dry basis), 1.50g sesbania powder, 45.00g dilute nitric acid solution with a mass concentration of 4.0wt% were fully mixed and formed by extrusion. Dry at 120°C for 8h. Then, heat to 530°C at 2.0°C / min and keep for 6h to remove the organic template. Ion exchange was performed with 0.8mol / L ammonium chloride solution and repeated three times. After drying at 80°C, heat to 510°C at 2.0°C / min and keep for 3h. Thus, a columnar catalyst with a ZSM-5 / ZSM-11 eutectic molecular sieve content of 90% was obtained, which was recorded as catalyst C.
[0060] Example 4
[0061] The catalytic performance of the prepared catalyst in the amination of tetrahydrofuran to tetrahydropyrrole was evaluated in a fixed bed reactor. The reactor diameter was 13 mm, the catalyst loading was 3 g, the reaction pressure was 0.0-3.0 MPa (0.0 MPa represents normal pressure), the reaction temperature was 160-450°C, and the tetrahydrofuran space velocity was 0.02-2.0 h -1 , the ammonia / tetrahydrofuran molar ratio is 2 to 20.
[0062] The reaction results are shown in Table 1.
[0063] Table 1 Catalytic performance of the catalyst of the present invention in the reaction of tetrahydrofuran amination to tetrahydropyrrole
[0064]
[0065]
[0066] The above are only a few embodiments of the present application and do not constitute any form of limitation to the present application. Although the present application is disclosed as above with preferred embodiments, it is not intended to limit the present application. Any technician familiar with the profession, without departing from the scope of the technical solution of the present application, using the technical content disclosed above to make slight changes or modifications are equivalent to equivalent implementation cases and fall within the scope of the technical solution.
Claims
1. A method for preparing tetrahydropyrrole by amination of tetrahydrofuran, characterized in that: The following steps are involved: The raw material containing tetrahydrofuran and ammonia is contacted with a catalyst for reaction to obtain a tetrahydropyrrole product; The catalyst is a ZSM-5 / ZSM-11 eutectic molecular sieve catalyst.
2. The method according to claim 1, characterized in that The preparation method of the ZSM-5 / ZSM-11 eutectic molecular sieve catalyst comprises the following steps: The mixed raw material containing eutectic molecular sieve raw powder, adhesive and sesbania powder is mixed with an acid solution, molded, calcined I, ion exchanged, and calcined II to obtain the ZSM-5 / ZSM-11 eutectic molecular sieve catalyst.
3. The method according to claim 2, characterized in that The content of ZSM-5 molecular sieve in the ZSM-5 / ZSM-11 eutectic molecular sieve catalyst is 0-99.5wt%, and the content of ZSM-11 molecular sieve is 0.5-100wt%; Preferably, the molar ratio of silicon dioxide to aluminum oxide in the eutectic molecular sieve raw powder is 15-500.
4. The method according to claim 2, characterized in that: The mass ratio of the eutectic molecular sieve raw powder to the adhesive is 0.05 to 19:1; Preferably, the mass of the sesbania powder accounts for 0.1 to 15.0 wt% of the total mass of the eutectic molecular sieve raw powder and the adhesive; Preferably, the mass of the acid solution accounts for 10 to 70 wt% of the total mass of the eutectic molecular sieve raw powder and the adhesive; Preferably, the concentration of the acid solution is 1-8 wt %.
5. The method according to claim 2, characterized in that: The adhesive is pseudo-boehmite; Preferably, the acid solution is a nitric acid solution.
6. The method according to claim 2, characterized in that The forming method is extrusion or ball rolling; Preferably, the calcination conditions are as follows: in an oxygen-containing atmosphere, heating the temperature to 440-600° C. at a heating rate of 0.5-3.0° C. / min, and keeping the temperature for 3-24 hours; Preferably, the calcination II is carried out under the following conditions: in an oxygen-containing atmosphere, heating the temperature to 420-550° C. at a heating rate of 0.5-3.0° C. / min, and keeping the temperature for 1-5 hours.
7. The method according to claim 2, characterized in that The conditions of the ion exchange are: temperature 50-95°C, time 0.5-24h; Preferably, the exchange solution for the ion exchange is selected from at least one of oxalic acid, hydrochloric acid, ammonium chloride and ammonium nitrate.
8. The method according to claim 1, characterized in that The reaction pressure is 0-3.0 MPa, wherein 0 MPa is normal pressure; The reaction temperature is 150-450°C.
9. The method according to claim 1, characterized in that: The space velocity of tetrahydrofuran is 0.02~2.0h -1 .
10. The method according to claim 1, characterized in that The molar ratio of ammonia to tetrahydrofuran in the raw material is 2-20.
Citation Information
Patent Citations
Preparation method of pyrrolidine
CN101948448A
Preparation method of catalyst for synthesizing pyrrolidine from tetrahydrofuran by catalytic amination
CN106693972A
Method for synthesizing tetrahydropyrrole by continuous catalytic amination of tetrahydrofuran
CN112521346A