Blast furnace hearth thermocouple adding technology

By adding double couples to the side wall of the blast furnace cylinder and performing precise installation, the problems of hearth cylinder erosion and carbon brick ablation are solved, efficient and safe longevity management of blast furnaces is achieved, and the accident of hearth burning through is avoided and production is improved. Safety and economic benefits.

CN118932129APending Publication Date: 2024-11-12HUNAN VALIN LIANYUAN IRON & STEEL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411264583.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-10
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

The blast furnace cylinder erosion seriously affects the life of the blast furnace. There are safety hazards when carbon bricks are ablated too quickly or sudden furnace cylinder burning accidents. There are blind spots in existing monitoring methods, which are difficult to warn in a timely manner.

Method used

Double galvanized pairs are added to the side wall of the blast furnace cylinder to determine the installation position through cooperation between multiple parties to ensure safe opening and installation, use curable carbon materials to fill the gap, monitor the residual thickness of carbon bricks, avoid blind spots, and ensure the normal operation of the galvanized pair.

Benefits of technology

实现了及时判断碳砖侵蚀情况,采取有效措施,延长高炉寿命,避免事故,确保安全生产,带来经济效益。

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a blast furnace hearth thermocouple adding technology which comprises the following steps: step 1, before damping down, listing a position where a thermocouple needs to be added, and the position of a newly-installed thermocouple and trepanning positioning need to be discussed by a production department, a technical department, a design institute, a technical department, a 6 # blast furnace workshop and a piping workshop together and are determined according to the actual situation in the production process; 2, various obstacles around are cleaned, obstacles outside the furnace are as few as possible, and gaps between the cooling walls can meet the requirement for the hole diameter of the open holes; thirdly, positioning and drilling are conducted after safety is guaranteed; 4, after drilling is completed, whether the drilling depth is qualified or not is determined; 5, welding a new galvanic couple short tube; step 6, installing a new galvanic couple; and 7, checking and accepting the external wiring condition of the galvanic couple. The invention relates to the field of blast furnace hearth use, in particular to a blast furnace hearth thermocouple adding technology.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the application field of a blast furnace hearth, and in particular to a blast furnace hearth thermocouple installation technology. Background Art

[0002] The degree of erosion and the amount of residue on the blast furnace hearth and bottom are the two main factors affecting the life of the blast furnace. However, due to the continuous operation of the blast furnace, the erosion of the hearth and bottom can generally only be accurately assessed during overhaul. According to the erosion mechanism of the blast furnace, blast furnaces generally use monitoring methods such as thermocouples, water temperature difference and heat flux intensity to assess the degree of erosion of the hearth and bottom. Reasonable installation of thermocouples and accurate processing of their data can predict problems with the lining early. Generally, a pair of thermocouples are installed at different depths in the same part of the blast furnace to measure the temperature; if the gap and the thermal conductivity of the refractory are known, the heat flow can be calculated based on the temperature difference AT. Tracking changes in temperature and heat flow can provide a more accurate understanding of the condition of the lining.

[0003] Since the 6# blast furnace was put into operation, the furnace erosion has been serious. The water temperature difference of the 2# iron mouth is 0.7 degrees, the heat flux intensity is as high as 12000KCal / h.m2, the temperature of the center point at the elevation of 6.290 meters rises to 722℃; the temperature of the second point of the inner ring at the elevation of 7.092 meters rises to 574℃, and the temperature of the second point of the outer ring at the elevation of 7.895m rises to 604℃. In the past two years, two furnace protection measures have been taken for the 6# blast furnace: one is the use of vanadium-titanium iron mouth mud, and the other is the length of the tuyere is lengthened from 585mm to 613mm. A series of measures have been adopted, and the side wall temperature is basically stable at present.

[0004] The sharp rise and fall of the side wall temperature is a serious safety hazard of the furnace. When the side wall temperature is abnormally high or rises rapidly, the blast furnace is forced to limit production or temporarily stop the wind to ensure the safety of the furnace, resulting in production capacity loss and cost increase. At the same time, the area of ​​the 6# blast furnace furnace thermocouple monitoring is insufficient, and there are blind spots, which lacks effective means for the safe production of the blast furnace in the later stage.

[0005] Adding double couples to the side wall of the furnace can timely judge the erosion of carbon bricks and take effective measures in time, which is convenient for establishing a blast furnace longevity management system, strengthening longevity management, and avoiding excessively rapid burning of carbon bricks or sudden furnace burn-through accidents. Summary of the invention

[0006] The technical problem to be solved by the present invention is that the furnace erosion is serious, which affects the life of the blast furnace, the carbon bricks burn out too quickly, or the furnace burns through unexpectedly.

[0007] To solve the above problems, the technical solution adopted by the present invention is as follows: The present invention is a blast furnace hearth thermocouple installation technology, comprising the following steps: Step 1: Before the wind is shut down, the locations where thermocouples need to be added should be marked. The locations of the newly installed thermocouples and the positioning of the holes should be discussed by the production department, technical department, design institute, technical department, 6# blast furnace workshop, and piping workshop, and determined according to the actual situation in the production process; Step 2: Clear all obstacles around the furnace, and make sure there are as few obstacles as possible outside the furnace. The gap between the cooling walls can meet the requirements of the opening aperture. Step 3: Position and drill after ensuring safety; Step 4: After drilling is completed, confirm whether the drilling depth is qualified; Step 5, welding of new thermocouple short tube; Step 6: Install new thermocouple; Step 7: Check and accept the external wiring of the thermocouple; Step 8. After the new thermocouple is installed, the gap should be filled with carbonaceous material. Solidifiable carbonaceous material should be used. At the same time, the gas enclosed in the channel gap should be exhausted as much as possible to ensure the normal use of the newly installed thermocouple.

[0008] Furthermore, the location requirements of the newly added thermocouples can effectively monitor the residual thickness of the carbon bricks.

[0009] Furthermore, the scope of ensuring safety includes the safety of cooling walls, carbon bricks and personnel.

[0010] Furthermore, controlling the entry speed and depth of the drill bit during drilling is the key to avoiding damaging or piercing the carbon bricks. Therefore, when drilling, first determine the residual thickness of the carbon bricks based on the temperature of the surrounding thermocouples, then preset the target depth of the drilling, and simultaneously monitor the temperature in real time during the drilling process. Start measuring the temperature when entering the carbon bricks, and do it in batches. The temperature should not exceed 500°C.

[0011] Furthermore, the drilling depth needs to meet the thickness of the furnace shell plus the thickness of the refractory material between the furnace shell and the cooling wall plus the thickness of the cooling wall plus the thickness of the refractory material between the carbon brick and the cooling wall plus the depth of the galvanic couple buried in the carbon brick, 158-162mm.

[0012] Furthermore, different drill bits are used for materials of different materials during the drilling process, and the drill bits are replaced appropriately during the drilling process.

[0013] Furthermore, the flange cap of the thermocouple is welded and sealed, and the grouting valve is closed.

[0014] Furthermore, the key parts are divided into 2 There is 1 thermocouple arranged.

[0015] Preferably, ensure that the furnace is in a monitored state without blind spots, focus on monitoring key parts of the blast furnace furnace, and if the existing thermocouples are restored, if the site conditions permit, thermocouples can be appropriately added in key parts such as the elephant foot area, the iron mouth area and the iron mouth angle position. Main contents include: thermocouple opening and installation (including thermocouple spare parts), laying of thermocouple wires (including compensation wires), etc.

[0016] The beneficial effects achieved by the present invention using the above structure are as follows: 1. It can timely judge the erosion of carbon bricks and take effective measures in time to facilitate the establishment of a blast furnace longevity management system, strengthen longevity management, and avoid excessive burning of carbon bricks or sudden furnace burn-through accidents.

[0017] 2. After implementation, the blast furnace worked continuously for a period of time, achieving safe, long-lasting and efficient production, bringing huge economic benefits to the company. DETAILED DESCRIPTION

[0018] The present invention relates to a blast furnace hearth thermocouple installation technology. Example 1

[0019] The technology of adding thermocouples to the blast furnace hearth includes the following steps: Step 1: Before the wind is shut down, the locations where thermocouples need to be added should be marked. The locations of the newly installed thermocouples and the positioning of the holes should be discussed by the production department, technical department, design institute, technical department, 6# blast furnace workshop, and piping workshop, and determined according to the actual situation in the production process; Step 2: Clear all obstacles around the furnace, and make sure there are as few obstacles as possible outside the furnace. The gap between the cooling walls can meet the requirements of the opening aperture. Step 3: Position and drill after ensuring safety; Step 4: After drilling is completed, confirm whether the drilling depth is qualified; Step 5, welding of new thermocouple short tube; Step 6: Install new thermocouple; Step 7: Check and accept the external wiring of the thermocouple; Step 8. After the new thermocouple is installed, the gap should be filled with carbonaceous material. Solidifiable carbonaceous material should be used. At the same time, the gas enclosed in the channel gap should be exhausted as much as possible to ensure the normal use of the newly installed thermocouple.

[0020] The newly added thermocouple location requirements can effectively monitor the residual thickness of carbon bricks.

[0021] The scope of ensuring safety includes the safety of cooling walls, carbon bricks and personnel.

[0022] Mastering the entry speed and depth of the drill bit when drilling is the key to avoid damaging or piercing the carbon bricks. Therefore, when drilling, first determine the residual thickness of the carbon bricks based on the temperature of the surrounding thermocouples, then preset the target depth of the drill hole, and monitor the temperature in real time during the drilling process. Start measuring the temperature when entering the carbon brick, and do it in batches. The temperature should not exceed 500°C.

[0023] The drilling depth needs to meet the thickness of the furnace shell plus the thickness of the refractory material between the furnace shell and the cooling wall plus the thickness of the cooling wall plus the thickness of the refractory material between the carbon brick and the cooling wall plus the depth of the electric couple buried in the carbon brick, which is 160mm.

[0024] During the drilling process, different drill bits should be used for materials of different materials, and the drill bits should be replaced reasonably during the drilling process.

[0025] Weld and seal the flange cap of the thermocouple and close the grouting valve.

[0026] Key areas are divided into 0.5m 2 There is 1 thermocouple arranged. Example 2

[0027] The technology of adding thermocouples to the blast furnace hearth includes the following steps: Step 1: Before the wind is shut down, the locations where thermocouples need to be added should be marked. The locations of the newly installed thermocouples and the positioning of the openings need to be discussed by the production department, technical department, design institute, technical department, 6# blast furnace workshop, and piping workshop, and determined based on the actual situation in the production process; Step 2: Clear all obstacles around the furnace, and make sure there are as few obstacles as possible outside the furnace. The gap between the cooling walls can meet the requirements of the opening aperture. Step 3: Position and drill after ensuring safety; Step 4: After drilling is completed, confirm whether the drilling depth is qualified; Step 5, welding of new thermocouple short tube; Step 6: Install new thermocouple; Step 7: Check and accept the external wiring of the thermocouple; Step 8. After the new thermocouple is installed, the gap should be filled with carbonaceous material. Solidifiable carbonaceous material should be used. At the same time, the gas enclosed in the channel gap should be exhausted as much as possible to ensure the normal use of the newly installed thermocouple.

[0028] The newly added thermocouple location requirements can effectively monitor the residual thickness of carbon bricks.

[0029] The scope of ensuring safety includes the safety of cooling walls, carbon bricks and personnel.

[0030] Mastering the entry speed and depth of the drill bit when drilling is the key to avoid damaging or piercing the carbon bricks. Therefore, when drilling, first determine the residual thickness of the carbon bricks based on the temperature of the surrounding thermocouples, then preset the target depth of the drill hole, and monitor the temperature in real time during the drilling process. Start measuring the temperature when entering the carbon brick, and do it in batches. The temperature should not exceed 500°C.

[0031] The drilling depth needs to meet the thickness of the furnace shell plus the thickness of the refractory material between the furnace shell and the cooling wall plus the thickness of the cooling wall plus the thickness of the refractory material between the carbon brick and the cooling wall plus the depth of the electric couple buried in the carbon brick, which is 158mm.

[0032] During the drilling process, different drill bits should be used for materials of different materials, and the drill bits should be replaced reasonably during the drilling process.

[0033] Weld and seal the flange cap of the thermocouple and close the grouting valve.

[0034] Key areas are divided into 0.5m 2 There is 1 thermocouple arranged. Example 3

[0035] The technology of adding thermocouples to the blast furnace hearth includes the following steps: Step 1: Before the wind is shut down, the locations where thermocouples need to be added should be marked. The locations of the newly installed thermocouples and the positioning of the openings need to be discussed by the production department, technical department, design institute, technical department, 6# blast furnace workshop, and piping workshop, and determined based on the actual situation in the production process; Step 2: Clear all obstacles around the furnace, and make sure there are as few obstacles as possible outside the furnace. The gap between the cooling walls can meet the requirements of the opening aperture. Step 3: Position and drill after ensuring safety; Step 4: After drilling is completed, confirm whether the drilling depth is qualified; Step 5, welding of new thermocouple short tube; Step 6: Install new thermocouple; Step 7: Check and accept the external wiring of the thermocouple; Step 8. After the new thermocouple is installed, the gap should be filled with carbonaceous material. Solidifiable carbonaceous material should be used. At the same time, the gas enclosed in the channel gap should be exhausted as much as possible to ensure the normal use of the newly installed thermocouple.

[0036] The newly added thermocouple location requirements can effectively monitor the residual thickness of carbon bricks.

[0037] The scope of ensuring safety includes the safety of cooling walls, carbon bricks and personnel.

[0038] Mastering the entry speed and depth of the drill bit when drilling is the key to avoid damaging or piercing the carbon bricks. Therefore, when drilling, first determine the residual thickness of the carbon bricks based on the temperature of the surrounding thermocouples, then preset the target depth of the drill hole, and monitor the temperature in real time during the drilling process. Start measuring the temperature when entering the carbon brick, and do it in batches. The temperature should not exceed 500°C.

[0039] The drilling depth needs to meet the thickness of the furnace shell plus the thickness of the refractory material between the furnace shell and the cooling wall plus the thickness of the cooling wall plus the thickness of the refractory material between the carbon brick and the cooling wall plus the depth of the electric couple buried in the carbon brick, which is 162mm.

[0040] During the drilling process, different drill bits should be used for materials of different materials, and the drill bits should be replaced reasonably during the drilling process.

[0041] Weld and seal the flange cap of the thermocouple and close the grouting valve.

[0042] Key areas are divided into 0.5m 2 There is 1 thermocouple arranged.

[0043] It should be understood that although this specification is described according to implementation methods, not every implementation method contains only one independent technical solution. This narrative method of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment can also be appropriately combined to form other implementation methods that can be understood by those skilled in the art.

Claims

1. Blast furnace hearth thermocouple installation technology, It is characterized in that The steps include: Step 1: Before the wind is shut down, the locations where thermocouples need to be added should be marked. The locations of the newly installed thermocouples and the positioning of the openings need to be discussed by the production department, technical department, design institute, technical department, 6# blast furnace workshop, and piping workshop, and determined based on the actual situation in the production process; Step 2: Clear all obstacles around the furnace, and make sure there are as few obstacles as possible outside the furnace. The gap between the cooling walls can meet the requirements of the opening aperture. Step 3: Position and drill after ensuring safety; Step 4: After drilling is completed, confirm whether the drilling depth is qualified; Step 5, welding of new thermocouple short tube; Step 6: Install new thermocouple; Step 7: Check and accept the external wiring of the thermocouple; Step 8. After the new thermocouple is installed, the gap should be filled with carbonaceous material. Solidifiable carbonaceous material should be used. At the same time, the gas enclosed in the channel gap should be exhausted as much as possible to ensure the normal use of the newly installed thermocouple.

2. The blast furnace hearth thermocouple installation technology according to claim 1, Features: The position of the newly added thermocouple in step 1 is required to effectively monitor the residual thickness of the carbon bricks.

3. The blast furnace hearth thermocouple installation technology according to claim 1, Features: The scope of ensuring safety in the step 3 includes the safety of cooling walls, carbon bricks and personnel.

4. The blast furnace hearth thermocouple installation technology according to claim 1, Features: Controlling the entry speed and depth of the drill bit during drilling in step three is the key to avoid damaging or piercing the carbon bricks. Therefore, when drilling, first determine the residual thickness of the carbon bricks based on the temperature of the surrounding thermocouples, then preset the target depth of the drilling, and simultaneously monitor the temperature in real time during the drilling process. Start measuring the temperature when entering the carbon bricks, and do it in batches. The temperature should not exceed 500°C.

5. The blast furnace hearth thermocouple installation technology according to claim 4, Features: The drilling depth in step three needs to meet the thickness of the furnace shell plus the thickness of the refractory material between the furnace shell and the cooling wall plus the thickness of the cooling wall plus the thickness of the refractory material between the carbon brick and the cooling wall plus the depth of the galvanic couple buried in the carbon brick, which is 158-162mm.

6. The blast furnace hearth thermocouple installation technology according to claim 5, Features: In the step three, different drill bits are used for materials of different materials during the drilling process, and the drill bits are replaced appropriately during the drilling process.

7. The blast furnace hearth thermocouple installation technology according to claim 2, Features: In step 1, the key parts are divided into 0.5m 2 There is 1 thermocouple arranged.