Packaging method of photosensitive sensor based on COB (Chip On Board) process

The photosensitive sensor is packaged through the COB process, which solves the problems of large size and large power consumption of traditional photosensitive sensors, achieving higher density, smaller volume and lower power consumption, and improving reliability in the aircraft.

CN118943207APending Publication Date: 2024-11-12XIAN OPTICAL VALLEY PHOTOELECTRIC TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411042328.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-31
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

Traditional photosensitive sensors are large in size and consume a lot of power, making it difficult to make breakthroughs in aircraft weight reduction and improve reliability.

Method used

The packaging method based on the COB process includes establishing a gold plating layer on the ceramic substrate, using a special suction nozzle to accurately position the silicon photocell on the solder, combining the white adhesive bonding protective cover and the PCB board, and bonding through the border equipment. And melt welding is carried out through the B4 fixture, and finally power-up testing and packaging are carried out.

Benefits of technology

It achieves higher chip density, reduced volume, reduced power consumption and better heat dissipation, and improves the reliability of the photosensitive sensor.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118943207A_ABST
    Figure CN118943207A_ABST
Patent Text Reader

Abstract

The invention relates to a packaging method of a photosensitive sensor based on a COB (chip on board) process, which comprises the following steps of: establishing a gold plating layer on a ceramic substrate (2), accurately positioning and placing a 2.72 * 2.72 silicon photocell (1) on a molten solder through a suction nozzle, and applying 5g of pressure to form a COC (3); then the protective cover (4) and the PCB (5) are bonded on the tube socket (6) through 930-4 (white glue), the bonded tube socket (6) is placed in a DB equipment special tool to be positioned, a glue dipping head is used for glue dipping, glue dispensing is carried out by accurately positioning in a coc placing area (13) of a bonding pad of the PCB (5), then a standby COC (3) is sucked through a special suction nozzle, and the COC (3) is accurately placed in the coc placing area (13) of the PCB (5), so that the COC (3) is accurately placed in the coc placing area (13) of the PCB (5). Putting into a nitrogen oven, baking at 150 DEG C for 1 hour, and curing; wB (wire bonding) is then carried out by using a wire bonding device, and finally the tube socket (6) and the tube cap (7) are assembled through a B4 clamp. According to the invention, higher chip density can be provided, the size is reduced, the power consumption is reduced, and better heat dissipation is realized.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a packaging technology of a photosensor, in particular to a packaging method of a photosensor based on a COB process. Background Art

[0002] Photosensitive sensors can be widely used in the light guide measurement and control systems of modern aircraft display screens. Whether the aircraft is in the day or at night, the intensity of ambient light can be detected in real time by photosensitive sensors, so that the "image" of the display screen can be clearly visible, allowing pilots to obtain "useful information" in a timely and accurate manner. However, most traditional photosensitive sensors are made of discrete components. The main problems of this traditional photosensitive sensor are large size and high power consumption. In the context of reducing the "weight" of the entire aircraft and improving reliability, new process methods must be used to design such devices. Summary of the invention

[0003] The purpose of the present invention is to provide a packaging method for a photosensitive sensor based on the COB process with small volume and energy consumption, so as to reduce the weight of the photosensitive sensor in an aircraft and improve the reliability.

[0004] The object of the present invention is achieved by a packaging method of a photosensitive sensor based on a COB process, which is characterized by comprising the following steps: Process 1: Use a special suction nozzle of DB (die bond) equipment to first suck up the ceramic substrate and place it on the heating table, build a gold-plated layer on the ceramic substrate, then use a special suction nozzle to suck up the gold-tin solder and accurately align it on the ceramic substrate. The heating table is heated to 360°C to melt the gold-tin solder. Use the suction nozzle to accurately position the 2.72*2.72 silicon photovoltaic cell on the molten solder and apply a pressure of 5g. After 5S, the heating table is cooled down, the solder between the silicon photovoltaic cell and the ceramic substrate cools down, and the grains formed in the liquid phase combine with each other to form a mechanical mixture to form a COC for standby use; Process 2: Use 930-4 (white glue) to bond the protective cover and PCB board to the tube holder, put them in the oven and bake at 150℃ for 1 hour. After the 930-4 (white glue) is cured, place the bonded tube holder in the special tooling of the DB equipment for positioning. Use the glue dipping head to dip the glue and accurately position it in the COC placement area 13 area of ​​the PCB pad. Then use the special suction nozzle to suck up the spare COC, and after accurately placing it in the COC placement area 13 area of ​​the PCB board, put it in the nitrogen oven and bake it at 150℃ for 1 hour for curing.

[0005] Process 3: Place the semi-finished product of process 2 on the dedicated heating table of the wire bonding equipment, and use the wire bonding equipment to perform WB (wire bonding). Bond the gold fingers of the PCB board and the gold-plated fingers of the COC electrodes. The wire type is required to be SSB-2, the gold wire diameter is 25.4μm, the welding mode is friction, the pressure is 55g, the cycle is 5 times, and the heating table temperature is set to 35℃ (before welding), 120℃ (during welding), and 35℃ (after welding). At the same time, during bonding, ensure that the height and length of the wire bonding cannot contact other circuits.

[0006] Step 4: Check if there is any problem with the bonding wire connection. If there is any problem, wire it up. The wire-up process is the same as step 3. Process 5: Assemble the tube socket and the tube cap through the B4 fixture, and then place the assembled tube socket and tube cap of the B4 fixture in the vacuum transition box of the energy storage welding machine to draw vacuum, and then place the entire B4 fixture in the discharge table of the energy storage welding machine, release high-voltage current through the discharge table and apply 0.5Mpa pressure to melt and weld the tube socket and tube cap in the B4 fixture.

[0007] Process 6: Power on the semi-finished product of process 5 on the test fixture. The power supply voltage is DC ± 15V (DC power supply ± 15V). Use a black opaque rubber cap to completely cover the transparent glass sheet of the product. The product output is DC0V (DC 0V). Use a 100000Lx light source to illuminate the transparent glass sheet of the product. The product output is DC15V (DC 15V). The product is qualified. The qualified products are finally packaged.

[0008] The silicon photocell has a length of 2.72 mm, a width of 2.72 mm and a thickness of 2 mm.

[0009] The adhesive used for bonding is 930-4 white glue.

[0010] The assembly method of the present invention is as follows: the size of the PCB board is circular, which is the same as the outer diameter of the protective cover, and electrode connection columns are closely distributed around the outer periphery of the PCB board so that the transparent glass sheet is placed on the electrode connection columns without being easily damaged; finally, a pipe cap with an opening in the middle is sleeved on the protective cover so that the transparent glass sheet is concentric with the protective cover and the PCB board.

[0011] There is an external connection electrode at the bottom of the tube holder, which passes through the tube cap and the via hole of the PCB board, has a certain height with the top surface of the PCB board, and constitutes an electrode connection column.

[0012] There is an electrode bonding gold-plated finger on the PCB board on one side of the electrode connection column. The electrode bonding gold-plated finger is connected to the electrode bonding gold-plated finger through a metal wire, so that the external connection electrode is electrically connected to the silicon photovoltaic cell.

[0013] The silicon photocell has a silicon photocell gold finger, which is bonded to the gold-plated finger on the top surface of the PCB board through a metal wire.

[0014] The advantages of the present invention are as follows: compared with the traditional chip packaging process, the present invention forms a COC (3) by establishing a gold-plated layer on a ceramic substrate (2), accurately positioning a 2.72*2.72 silicon photovoltaic cell (1) on a molten solder through a suction nozzle and applying a pressure of 5g; then the protective cover (4) and the PCB board (5) are bonded to the tube seat (6) by using 930-4 (white glue), the bonded tube seat (6) is placed in a special tooling of a DB device for positioning, the glue dipping head is dipped in glue and accurately positioned in the coc placement area 13 area of ​​the pad of the PCB board (5) for dispensing glue, and then the spare COC (3) is sucked by a special suction nozzle, and after being accurately placed in the coc placement area 13 area of ​​the PCB board (5), it is placed in a nitrogen oven at 150°C and baked for 1 hour for curing; then a wire bonding device is used for WB (wire bonding), and finally the tube seat (6) and the tube cap (7) are assembled by a B4 fixture. The present invention can provide higher chip density, smaller volume, lower power consumption and better heat dissipation.

[0015] The present invention will be further described below in conjunction with the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 It is a process flow chart of the present invention; Figure 2 This is an exploded view of the COC process; Figure 3 It is a combination diagram of the COC process; Figure 4 is the photosensitive sensor bonding diagram; Figure 5 This is the photosensitive sensor packaging diagram.

[0017] In the figure: 1. Silicon photocell; 2. Ceramic substrate; 3. COC; 4. Protective cover; 5. PCB board; 6. Tube socket; 7. Tube cap; 8. Support column; 9. Transparent glass sheet; 10. Electrode bonding gold-plated fingers; 11. Support platform; 12. External connection electrode; 13. COC placement area; 14. Silicon photocell gold fingers. DETAILED DESCRIPTION

[0018] In order to further explain the technical means and methods adopted by the present invention to achieve the predetermined purpose, the specific implementation methods, structural features and methods of the present invention are described in detail below in conjunction with the accompanying drawings and embodiments.

[0019] like Figure 1 The present invention relates to a packaging method of a photosensitive sensor based on a COB process, which is characterized by comprising the following steps: Process 1: Use the special suction nozzle of the DB equipment to first suck up the ceramic substrate 2 and place it on the heating table, build a gold-plated layer on the ceramic substrate 2, then use the special suction nozzle to suck up the gold-tin solder and accurately align it on the ceramic substrate 2. The heating table is heated to 360°C to melt the gold-tin solder. Use the suction nozzle to accurately position the 2.72*2.72 silicon photovoltaic cell 1 on the molten solder and apply a pressure of 5g. After 5S, the heating table is cooled down, the solder between the silicon photovoltaic cell 1 and the ceramic substrate is cooled, and the grains formed in the liquid phase are combined with each other into a mechanical mixture to form COC3 for standby use; Process 2: Use 930-4 (white glue) to bond the protective cover 4 and PCB board 5 to the tube holder 6, put them in the oven and bake at 150℃ for 1 hour. The 930-4 (white glue) is solidified. The bonded tube holder 6 is placed in the special tooling of the DB equipment for positioning. Use the glue dipping head to dip the glue and accurately locate it in the COC placement area 13 area of ​​the PCB board 5 pad. Then use the special suction nozzle to suck the spare COC3 and accurately place it in the COC placement area 13 area of ​​the PCB board 5. Figure 3 As shown, the film was placed in a nitrogen oven and baked at 150° C. for 1 hour for curing.

[0020] Process 3: Place the semi-finished product of process 2 on the dedicated heating table of the wire bonding equipment, and use the wire bonding equipment to perform WB (wire bonding). Bond the gold finger of PCB board 5 and the electrode bonding gold-plated finger 10 of COC 3. The wire type is SSB-2 wire type, the gold wire diameter is 25.4μm, the welding mode is friction, the pressure is 55g, the cycle is 5 times, and the heating table temperature is set to 35℃ (before welding), 120℃ (during welding), and 35℃ (after welding). At the same time, during bonding, ensure that the height and length of the wire bonding cannot contact other circuits, such as Figure 4 shown.

[0021] Step 4: Check if there is any problem with the bonding wire connection. If there is any problem, wire it up. The wire-up process is the same as step 3. Process 5: Assemble the tube seat 6 and the tube cap 7 through the B4 fixture, and then place the B4 fixture connected to the assembled tube seat 6 and tube cap 7 in the vacuum transition box of the energy storage welding machine to draw vacuum, and then place the entire B4 fixture in the discharge table of the energy storage welding machine, release high voltage current through the discharge table and apply 0.5Mpa pressure to melt and weld the tube seat 6 and tube cap 7 in the B4 fixture. The package shape is as follows Figure 5 shown.

[0022] Process 6: Power on the semi-finished product of process 5 on the test fixture. The power supply voltage is DC ± 15V. Use a black opaque rubber cap to completely cover it. Figure 5The transparent glass sheet 9 of the product shown, the product output is DC0V, and the light source used is 100000Lx Figure 5 The transparent glass sheet 9 of the product shown has a DC15V output, and the product is qualified. The qualified products are finally packaged and put into storage.

[0023] The silicon photocell 1 has a length of 2.72 mm, a width of 2.72 mm and a thickness of 2 mm.

[0024] The substrate is either a copper substrate or an aluminum substrate.

[0025] The adhesive used for bonding is 930-4 (white glue).

[0026] The size of the PCB board 5 is circular, and it has the same outer diameter as the protective cover 4. Electrode connecting posts 8 are closely distributed around the outer periphery of the PCB board 5 so that the transparent glass sheet 9 is placed on the electrode connecting posts 8 without being easily damaged; finally, a pipe cap 7 with an opening in the middle is sleeved on the protective cover 4 so that the transparent glass sheet 9 is concentric with the protective cover 4 and the PCB board 5.

[0027] The protective cover 4 is placed on the support platform 11 of the tube base 6 so that the protective cover 4, the tube base 6 and the support platform 11 are concentric.

[0028] There is an external connection electrode 12 at the bottom of the tube holder 6. The external connection electrode 12 passes through the via holes of the tube cap 7 and the PCB board 5, and has a height with the top surface of the PCB board 5, and at the same time constitutes an electrode connection column 8. There is an electrode bonding gold-plated finger 10 on the PCB board 5 on one side of the electrode connection column 8. The electrode bonding gold-plated finger 10 is connected to the electrode bonding gold-plated finger 10 through a metal wire, so that the external connection electrode 12 is electrically connected to the silicon photovoltaic cell 1.

[0029] In the present invention, the silicon photocell 1 has a silicon photocell gold finger 14, which is bonded to the gold-plated finger on the top surface of the PCB board 5 through a metal wire.

[0030] Compared with the traditional chip packaging process, the present invention can provide higher chip density, smaller volume, lower power consumption and better heat dissipation.

[0031] The bonding process has high control requirements for temperature. Too high a temperature will not only produce too much oxide and affect the bonding quality, but also reduce the image monitoring accuracy and device reliability due to the influence of thermal stress and strain.

[0032] Therefore, it also includes at least: a temperature control unit, which is used to control the temperature of the bonding device and improve the influence of the change of the temperature of the bonding device on the bonding quality.

[0033] For ordinary technicians to whom the present invention belongs, some simple deductions or substitutions can be made without departing from the concept of the present invention, which should be regarded as belonging to the protection scope of the invention.

Claims

1. A packaging method for a photosensitive sensor based on COB technology, characterized by: The steps include: Step 1: Use the nozzle of the DB device to suck up the ceramic substrate (2) and place it on the heating table, build a gold-plated layer on the ceramic substrate (2), then use the nozzle to suck up the gold-tin solder and align it on the ceramic substrate, heat the heating table to 360°C to melt the gold-tin solder, and use the nozzle to position the 2.72*2.72 silicon photovoltaic cell (1) on the molten solder and apply a pressure of 5g. After 5S, the heating table is cooled down, the solder between the silicon photovoltaic cell (1) and the ceramic substrate (2) cools down, and the crystal grains formed in the liquid phase are combined with each other to form a mechanical mixture to form COC (3) for standby use; Step 2: Use 930-4 (white glue) to bond the protective cover (4) and the PCB board (5) to the tube holder (6), and bake them in an oven at 150°C for 1 hour. The 930-4 (white glue) is cured. The bonded tube holder (6) is placed in the DB equipment tooling for positioning. Use a glue dipping head to apply glue by accurately positioning it in the coc placement area (13) of the pad of the PCB board (5). Then use a suction nozzle to suck up the spare COC (3), and after accurately placing it in the coc placement area (13) of the PCB board (5), put it in a nitrogen oven and bake it at 150°C for 1 hour to cure it. Step 3: Place the semi-finished product of step 2 on the dedicated heating table of the wire bonding equipment, and use the wire bonding equipment to perform WB (wire bonding) to bond the gold finger of the PCB board (5) and the electrode bonding gold-plated finger (10) of the COC (3). The wire type is required to be SSB-2 wire type, the gold wire diameter is 25.4μm, the welding mode is selected as friction, the pressure is 55g, the cycle is 5 times, and the heating table temperature is set to 35℃ (before welding), 120℃ (during welding), and 35℃ (after welding). At the same time, during bonding, ensure that the height and length of the wire bonding cannot contact other circuits; Step 4: Check if there is any problem with the bonding wire connection. If there is any problem, wire it up. The wire-up process is the same as step 3. Step 5: Assemble the tube seat (6) and the tube cap (7) through a B4 fixture, then place the B4 fixture connected to the assembled tube seat (6) and tube cap (7) in a vacuum transition box of an energy storage welding machine to draw a vacuum, then place the entire B4 fixture in a discharge table of the energy storage welding machine, release a high voltage current through the discharge table and apply a pressure of 0.5 MPa to melt and weld the tube seat (6) and tube cap (7) in the B4 fixture; Process 6: The semi-finished product of process 5 is tested on the test fixture with a power supply voltage of DC ± 15V. A black opaque rubber cap is used to completely cover the transparent glass sheet (9) of the product. The product output is DC0V. A 100000Lx light source is used to illuminate the transparent glass sheet (9) of the product. The product output is DC15V, and the product is qualified. The qualified products are finally packaged and put into storage.

2. The packaging method of a photosensor based on COB technology according to claim 1 is characterized in that: The silicon photocell (1) has a length of 2.72 mm, a width of 2.72 mm and a thickness of 2 mm.

3. The packaging method of a photosensor based on COB technology according to claim 1 is characterized in that: The adhesive used for bonding is 930-4 white glue.

4. The packaging method of a photosensor based on COB technology according to claim 1 is characterized in that: The PCB board (5) is circular in size and has the same outer diameter as the protective cover (4). Electrode connection posts (8) are closely spaced around the outer periphery of the PCB board (5) so that the transparent glass sheet (9) can be placed on the electrode connection posts (8) without being easily damaged. Finally, a tube cap (7) with an opening in the middle is sleeved on the protective cover (4) so ​​that the transparent glass sheet (9) is concentric with the protective cover (4) and the PCB board (5).

5. The packaging method of a photosensor based on COB technology according to claim 1 is characterized in that: An external connection electrode (12) is provided at the bottom of the tube seat (6). The external connection electrode (12) passes through the via hole of the tube cap (7) and the PCB board (5) and is at a height with the top surface of the PCB board (5), and at the same time forms an electrode connection column (8).

6. The packaging method of a photosensor based on COB technology according to claim 4 is characterized in that: An electrode bonding gold-plated finger (10) is provided on the PCB board (5) on one side of the electrode connection column (8); the electrode bonding gold-plated finger (10) is connected to the electrode bonding gold-plated finger (10) via a metal wire, so that the external connection electrode (12) is electrically connected to the silicon photocell (1).

7. The packaging method of a photosensor based on COB technology according to claim 1 is characterized in that: The silicon photocell (1) has a silicon photocell gold finger (14), which is bonded to the gold-plated finger on the top surface of the PCB board (5) through a metal wire.