Semiconductor structure and forming method thereof
By optimizing the structure of the floating gate cantilever and the penetrating insulation layer, the reliability problem of traditional flash memory devices is solved, the performance and yield of separated gate flash memory devices are improved, and higher erasing tolerance and data retention time are achieved.
Patent Information
- Application Number
- CN202310519575.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-09
- Publication Date
- 2024-11-12
AI Technical Summary
Traditional stacked gate flash memory devices have reliability problems such as programming/erase interference, over-erase, charge retention characteristics, and erase durability. Separated gate flash memory devices require a more efficient and reliable floating gate cantilever structure to improve performance and yield. .
By forming a stacked structure of a floating gate dielectric layer, a floating gate layer, a control gate dielectric layer and a hard mask layer on the semiconductor substrate, the first and second trenches are formed, and the third dielectric layer thickness is increased to extend the floating gate. The cantilever, the floating gate layer etches part of the floating gate lowers the cantilever height, and changes the material and structure of the floating gate insulating layer, so that the angle between the cantilever and the insulating layer is less than 90 degrees.
The erase tolerance of the separated gate flash memory device is improved to more than 100,000 to more than 200,000 times, the erase voltage is reduced, the data retention time is extended, and the device performance and yield is improved.
Smart Images

Figure CN118946152A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of semiconductor technology, and in particular to a semiconductor structure and a method for forming the same. Background Art
[0002] Flash memory is a non-volatile memory device with electrical programmability and erasure, and is widely used in system-on-chip (SOC). From a structural point of view, flash memory devices can be mainly divided into stacked gate structure and split gate structure. Traditional stacked gate flash memory has reliability issues such as program / erase interference, over-erasure, charge retention characteristics and erase durability. Split gate flash memory uses a two-tube unit structure to effectively avoid the reliability issues of stacked gate flash memory.
[0003] The basic structure of a split-gate flash memory includes a semiconductor substrate with a source and a drain; a floating gate oxide layer, a floating gate, a control gate oxide layer and a control gate formed on the semiconductor substrate in sequence by a stack self-alignment process; an erase gate and a word line formed on the floating gate oxide layer, the erase gate is located in the middle of two floating gate control gate stacks, and the word line is located on both sides of the two floating gate control gate stacks; it also includes a sidewall layer formed on both sides of the control gate, the sidewall layer is used to self-align and etch the floating gate to form a floating gate cantilever. During the erase operation, the electric field is concentrated at the corner of the floating gate cantilever, which is conducive to the electrons in the floating gate tunneling into the erase gate through the floating gate cantilever corner, resulting in a higher erase efficiency. The excellence of the floating gate cantilever structure directly affects the performance of the device and the yield of the chip.
[0004] Therefore, it is necessary to provide a more effective and reliable floating gate cantilever structure to improve the performance and yield of split-gate flash memory devices. Summary of the invention
[0005] The present application provides a semiconductor structure and a method for forming the same, which can improve the performance and yield of a split-gate flash memory device.
[0006] One aspect of the present application provides a method for forming a semiconductor structure, comprising: providing a semiconductor substrate, on the surface of which a stacking structure of a floating gate dielectric layer, a floating gate layer, a control gate dielectric layer, a control gate layer and a hard mask layer is sequentially formed; etching the stacking structure to form a first trench and a second trench in the floating gate layer, wherein the first trench is located between two adjacent stacking structures, and the second trench is located on both sides of the first trench and the two adjacent stacking structures; forming a first sidewall of the stacking structure on both sides of the first trench, and forming a second sidewall of the stacking structure on both sides of the second trench, wherein the thickness of the first sidewall is greater than the thickness of the second sidewall; etching the remaining floating gate layer at the bottom of the first trench and the second trench to the surface of the floating gate dielectric layer; etching and removing part of the first sidewall; forming a dielectric material layer at the bottom and sidewall of the first trench and the bottom and sidewall of the second trench, wherein a part of the dielectric material layer located at the sidewall of the second trench constitutes a floating gate coupling dielectric layer, a part of the dielectric material layer located at the sidewall of the floating gate layer constitutes a floating gate tunneling insulating layer, and a part of the floating gate layer located at the lower surface of the first sidewall and the lower surface of the floating gate tunneling insulating layer constitutes a floating gate cantilever.
[0007] In some embodiments of the present application, the length of the floating gate cantilever is 250 angstroms to 350 angstroms; and the distance between the floating gate cantilever and the lower surface of the floating gate layer is 150 angstroms to 250 angstroms.
[0008] In some embodiments of the present application, the angle at which the floating gate tunneling insulating layer covers the floating gate cantilever is less than 90 degrees.
[0009] In some embodiments of the present application, the floating gate tunneling insulating layer has a thickness of 100 angstroms to 150 angstroms.
[0010] In some embodiments of the present application, the material of the floating gate tunneling insulating layer includes silicon oxynitride or nitrided silicon oxide.
[0011] In some embodiments of the present application, the material of the floating gate tunneling insulating layer is nitrided silicon oxide, and the method of forming the dielectric material layer includes: forming a silicon oxide layer at the bottom and side walls of the first trench and the bottom and side walls of the second trench; performing an annealing process on the silicon oxide layer, and introducing nitric oxide gas into the reaction chamber when performing the annealing process.
[0012] In some embodiments of the present application, the method for forming the first side wall and the second side wall includes: forming a first dielectric layer, a second dielectric layer and a third dielectric layer in sequence on the side wall of the stacked structure, the thickness of the third dielectric layer being greater than the thickness of the first dielectric layer and the second dielectric layer; removing the third dielectric layer located on one side of the second groove, the first dielectric layer and the second dielectric layer on both sides of the second groove constitute the first side wall, and the first dielectric layer, the second dielectric layer and the third dielectric layer on both sides of the first groove constitute the second side wall.
[0013] In some embodiments of the present application, the thickness of the first dielectric layer is 30-70 angstroms; the thickness of the second dielectric layer is 120-160 angstroms; and the thickness of the third dielectric layer is 300-500 angstroms.
[0014] In some embodiments of the present application, the method for forming the semiconductor structure further includes: forming an erase gate in the first trench; and forming a word line structure in the second trench.
[0015] Another aspect of the present application also provides a semiconductor structure, including: a semiconductor substrate, on the surface of which a stacking structure of a floating gate dielectric layer, a floating gate layer, a control gate dielectric layer, a control gate layer and a hard mask layer is sequentially formed; a first trench and a second trench, located in the stacking structure and stopping at the surface of the floating gate dielectric layer, the first trench is located between two adjacent stacking structures, and the second trench is located on both sides of the first trench and the two adjacent stacking structures; a first sidewall and a second sidewall, respectively located on the sidewall of the stacking structure close to the first trench and the sidewall of the stacking structure close to the second trench; a dielectric material layer, located at the bottom and sidewall of the first trench and the bottom and sidewall of the second trench, a portion of the dielectric material layer located at the sidewall of the second trench constitutes a floating gate coupling dielectric layer, a portion of the dielectric material layer located at the sidewall of the floating gate layer constitutes a floating gate tunneling insulating layer, and a portion of the floating gate layer located at the lower surface of the first sidewall and the lower surface of the floating gate tunneling insulating layer constitutes a floating gate cantilever.
[0016] In some embodiments of the present application, the length of the floating gate cantilever is 250 angstroms to 350 angstroms; and the distance between the floating gate cantilever and the lower surface of the floating gate layer is 150 angstroms to 250 angstroms.
[0017] In some embodiments of the present application, the angle at which the floating gate tunneling insulating layer covers the floating gate cantilever is less than 90 degrees.
[0018] In some embodiments of the present application, the floating gate tunneling insulating layer has a thickness of 100 angstroms to 150 angstroms.
[0019] In some embodiments of the present application, the material of the floating gate tunneling insulating layer includes silicon oxynitride or nitrided silicon oxide.
[0020] In some embodiments of the present application, the semiconductor structure further includes: an erase gate located in the first trench; and a word line structure located in the second trench.
[0021] The present application provides a semiconductor structure and a method for forming the same, which increases the thickness of a third dielectric layer so as to increase the length of a floating gate cantilever; etches a portion of the floating gate layer so as to reduce the height of the floating gate cantilever; changes the material of a floating gate tunneling insulating layer; when etching and removing a portion of the first sidewall, the top corner exposed by the floating gate layer is changed from a right-angle structure to an arc structure so that the angle between the floating gate cantilever and the floating gate tunneling insulating layer is less than 90 degrees; improves the structure of the floating gate cantilever and the floating gate tunneling insulating layer, and can improve the performance and yield of a split-gate flash memory device. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] The following figures describe in detail the exemplary embodiments disclosed in this application. The same reference numerals represent similar structures in several views of the drawings. Those skilled in the art will understand that these embodiments are non-limiting, exemplary embodiments, and the drawings are only for the purpose of illustration and description, and are not intended to limit the scope of this application. Other embodiments may also accomplish the inventive intent in this application. It should be understood that the drawings are not drawn to scale.
[0023] in:
[0024] Figures 1 to 8 It is a structural schematic diagram of each step in the method for forming a semiconductor structure described in an embodiment of the present application. DETAILED DESCRIPTION
[0025] The following description provides specific application scenarios and requirements of the present application, with the purpose of enabling those skilled in the art to make and use the content in the present application. It will be apparent to those skilled in the art that various local modifications to the disclosed embodiments are apparent, and the general principles defined herein may be applied to other embodiments and applications without departing from the spirit and scope of the present application. Therefore, the present application is not limited to the embodiments shown, but to the widest scope consistent with the claims.
[0026] The technical solution of the present invention is described in detail below in conjunction with the embodiments and drawings.
[0027] The applicant has found through experiments that the length and height of the floating gate cantilever are key factors affecting the erase efficiency, and the erase efficiency can be optimized by optimizing the structure there. In addition, the erase voltage can be reduced and the data retention time can be improved by changing the material of the floating gate tunneling insulating layer.
[0028] Based on this, the present application provides a semiconductor structure and a method for forming the same, which improves the structure of the floating gate cantilever and the floating gate tunneling insulating layer, and can improve the performance and yield of the split-gate flash memory device.
[0029] Figures 1 to 8 The following is a schematic diagram of the structure of each step in the method for forming a semiconductor structure according to an embodiment of the present application. The method for forming a semiconductor structure according to an embodiment of the present application is described in detail in conjunction with the accompanying drawings.
[0030] refer to Figure 1 As shown, a semiconductor substrate 100 is provided, and a stacking structure of a floating gate dielectric layer 110, a floating gate layer 120, a control gate dielectric layer 130, a control gate layer 140 and a hard mask layer 150 is sequentially formed on the surface of the semiconductor substrate 100.
[0031] In some embodiments of the present application, the semiconductor structure described in the present application is, for example, a split-gate flash memory device.
[0032] In some embodiments of the present application, the material of the semiconductor substrate 100 includes (i) an elemental semiconductor, such as silicon or germanium; (ii) a compound semiconductor, such as silicon carbide, gallium arsenide, gallium phosphide or indium phosphide; (iii) an alloy semiconductor, such as silicon germanium carbide, silicon germanium, gallium arsenide phosphide or gallium indium phosphide; or (iv) a combination of the above.
[0033] In some embodiments of the present application, the material of the floating gate dielectric layer 110 is, for example, silicon oxide. The thickness of the floating gate dielectric layer 110 is 80 to 100 angstroms, for example, 85 angstroms, 90 angstroms, or 95 angstroms. The method of forming the floating gate dielectric layer 110 includes a chemical vapor deposition process or a thermal oxidation process.
[0034] In some embodiments of the present application, the material of the floating gate layer 120 is, for example, polysilicon. The thickness of the floating gate layer 120 is 500 to 550 angstroms, for example, 510 angstroms, 520 angstroms, 525 angstroms, 530 angstroms, or 540 angstroms. The method of forming the floating gate layer 120 includes a chemical vapor deposition process or a physical vapor deposition process.
[0035] In some embodiments of the present application, the control gate dielectric layer 130 includes a three-layer stacked structure of silicon oxide-silicon nitride-silicon oxide. The method of forming the control gate dielectric layer 130 includes a chemical vapor deposition process or a physical vapor deposition process.
[0036] In some embodiments of the present application, the material of the control gate layer 140 is, for example, polysilicon. The thickness of the control gate layer 140 is 600 to 700 angstroms, for example, 620 angstroms, 640 angstroms, 650 angstroms, 660 angstroms, or 680 angstroms. The method of forming the control gate layer 140 includes a chemical vapor deposition process or a physical vapor deposition process.
[0037] In some embodiments of the present application, the material of the hard mask layer 150 is, for example, silicon nitride. The thickness of the hard mask layer 150 is 700 to 1400 angstroms, for example, 720 angstroms, 840 angstroms, 950 angstroms, 1060 angstroms, or 1180 angstroms. The method of forming the hard mask layer 150 includes a chemical vapor deposition process or a physical vapor deposition process.
[0038] refer to Figure 2 As shown, the stacked structure is etched into the floating gate layer 120 to form a first trench 101 and a second trench 102, wherein the first trench 101 is located between two adjacent stacked structures, and the second trench 102 is located on both sides of the first trench 101 and the two adjacent stacked structures. The first trench 101 is used to form an erase gate, and the second trench 102 is used to form a word line structure. The thickness of the floating gate layer 120 etched can determine the height of the floating gate cantilever, that is, the distance between the floating gate cantilever and the lower surface of the floating gate layer 120.
[0039] In some embodiments of the present application, a method for etching the stacked structure to form a first groove 101 and a second groove 102 in the floating gate layer 120 includes, for example: forming a patterned photoresist layer on the surface of the hard mask layer 150, the patterned photoresist layer defining the positions of the first groove 101 and the second groove 102; etching the hard mask layer 150, the control gate layer 140, and the control gate dielectric layer 130 to form the first groove 101 and the second groove 102 in the floating gate layer 120 using the patterned photoresist layer as a mask; and removing the patterned photoresist layer.
[0040] refer to Figure 3 and Figure 4 As shown, a first sidewall 161 of the stacked structure is formed on both sides of the first trench 101 , and a second sidewall 162 of the stacked structure is formed on both sides of the second trench 102 . The thickness of the first sidewall 161 is greater than that of the second sidewall 162 .
[0041] refer to Figure 3As shown, a first dielectric layer 141, a second dielectric layer 142 and a third dielectric layer 143 are sequentially formed on the sidewalls of the stacked structure (specifically, the hard mask layer 150, the control gate layer 140, the control gate dielectric layer 130 and a portion of the floating gate layer 120), and the thickness of the third dielectric layer 143 is greater than the thickness of the first dielectric layer 141 and the second dielectric layer 142. Increasing the thickness of the third dielectric layer 143 can increase the length of the floating gate cantilever. Parts of the first dielectric layer 141 and the third dielectric layer 143 are also located on the surface of the floating gate layer 120.
[0042] In some embodiments of the present application, the method for forming the first dielectric layer 141, the second dielectric layer 142 and the third dielectric layer 142 includes: forming the first dielectric layer 141 and the second dielectric layer 142 on the sidewalls of the hard mask layer 150, the control gate layer 140, the control gate dielectric layer 130 and a portion of the floating gate layer 120 and on the surface of the hard mask layer 150 and the floating gate layer 120; etching and removing a portion of the first dielectric layer 141 and the second dielectric layer 142 on the surface of the hard mask layer 150 and the floating gate layer 120, leaving only the first dielectric layer 141 and the second dielectric layer 142 located on the hard mask layer 150 and the floating gate layer 120. The first dielectric layer 141 and the second dielectric layer 142 on the side walls of the hard mask layer 150, the control gate layer 140, the control gate dielectric layer 130 and part of the floating gate layer 120 are formed; a third dielectric layer 143 is formed on the side walls of the second dielectric layer 142 and on the surfaces of the first dielectric layer 141, the hard mask layer 150 and the floating gate layer 120; and a part of the third dielectric layer 143 on the surfaces of the first dielectric layer 141, the hard mask layer 150 and the floating gate layer 120 is etched and removed, and only the third dielectric layer 143 located on the side walls of the second dielectric layer 142 is retained.
[0043] In some embodiments of the present application, the material of the first dielectric layer 141 is, for example, silicon oxide, and the thickness of the first dielectric layer 141 is 30-70 angstroms; the material of the second dielectric layer 142 is, for example, silicon nitride, and the thickness of the second dielectric layer 142 is 120-160 angstroms; the material of the third dielectric layer 143 is, for example, silicon oxide, and the thickness of the third dielectric layer 143 is 300-500 angstroms. The total thickness of the first dielectric layer 141, the second dielectric layer 142, and the third dielectric layer 143 determines the length of the floating gate cantilever. In order to ensure process compatibility, reduce the variables in the present application and the conventional process, keep the thickness of the first dielectric layer 141 and the second dielectric layer 142 unchanged, and increase the thickness of the third dielectric layer 143 to increase the length of the floating gate cantilever.
[0044] refer to Figure 4As shown, the third dielectric layer 143 located on one side of the second groove 102 is removed, the first dielectric layer 141 and the second dielectric layer 142 on both sides of the second groove 102 constitute the second side wall 162, and the first dielectric layer 141, the second dielectric layer 142 and the third dielectric layer 143 on both sides of the first groove 101 constitute the first side wall 161.
[0045] refer to Figure 5 As shown, the floating gate layer 120 remaining at the bottom of the first trench 101 and the second trench 102 is etched to the surface of the floating gate dielectric layer 110 .
[0046] refer to Figure 6 As shown, a portion of the first sidewall 161 is etched away. Specifically, for example, the third dielectric layer 143 in the first sidewall 161 can be etched away. It should be understood that the present application only uses etching to remove the third dielectric layer 143 as an example, and in fact, a portion of the first sidewall 161 with any thickness can be etched away along the sidewall of the first sidewall 161.
[0047] refer to Figure 7 As shown, a dielectric material layer 170 is formed on the bottom and sidewalls of the first trench 101, the bottom and sidewalls of the second trench 102, the hard mask layer 150, the first sidewall 161, and the upper surface of the second sidewall 162. It should be noted that during the formation of the dielectric material layer 170, the top corner of the floating gate layer 120 needs to be kept as a sharp corner structure.
[0048] Among them, part of the dielectric material layer 170 located on the side wall of the second trench 102 constitutes a floating gate coupling dielectric layer; part of the dielectric material layer 170 located on the side wall of the floating gate layer 120 close to the first trench 101 constitutes a floating gate tunneling insulating layer 180; part of the floating gate layer 120 located on the lower surface of the first sidewall 161 and the lower surface of the floating gate tunneling insulating layer 180 constitutes a floating gate cantilever 190. That is to say, the part of the floating gate layer 120 protruding from the control gate layer 140 and close to the first trench 101 is the floating gate cantilever 190. The floating gate tunneling insulating layer 180 covers the corner of the floating gate cantilever 190.
[0049] In some embodiments of the present application, the length a of the floating gate cantilever 190 is 250 angstroms to 350 angstroms, for example, 280 angstroms, 300 angstroms or 330 angstroms, etc.; the distance b between the floating gate cantilever 190 and the lower surface of the floating gate layer 120 is 150 angstroms to 300 angstroms, for example, 180 angstroms, 200 angstroms or 220 angstroms, etc.
[0050] In some embodiments of the present application, the angle at which the floating gate tunneling insulating layer 180 covers the floating gate cantilever 190 is less than 90 degrees, for example, 88 degrees, 85 degrees, 82 degrees or 80 degrees.
[0051] In some embodiments of the present application, the thickness of the floating gate tunneling insulating layer 180 is 100 angstroms to 150 angstroms, for example, 110 angstroms, 120 angstroms, 130 angstroms or 140 angstroms. The length of the floating gate tunneling insulating layer 180 is 280 angstroms to 360 angstroms. The height of the floating gate tunneling insulating layer 180 is 150 angstroms to 300 angstroms. The length of the floating gate tunneling insulating layer 180 is 280 angstroms to 360 angstroms.
[0052] In some embodiments of the present application, the material of the floating gate tunneling insulating layer 180 includes silicon oxynitride or nitrided silicon oxide.
[0053] In some embodiments of the present application, the material of the floating gate tunneling insulating layer 180 is nitrided silicon oxide, and the method of forming the dielectric material layer 170 includes: forming a silicon oxide layer at the bottom and side walls of the first trench and the bottom and side walls of the second trench; performing an annealing process on the silicon oxide layer, and introducing nitric oxide gas into the reaction chamber when performing the annealing process.
[0054] In the technical solution of the present application, the structure of the floating gate cantilever and the floating gate tunneling insulating layer is improved by improving the manufacturing process, thereby increasing the erase and write tolerance of the split-gate flash memory device to more than 100,000 to 200,000 times, and at the same time, the erase voltage can be reduced to improve the data retention time in reliability. Specifically, the thickness of the third dielectric layer is increased to increase the length of the floating gate cantilever; a portion of the floating gate layer is etched to reduce the height of the floating gate cantilever; the material of the floating gate tunneling insulating layer is changed; when etching and removing a portion of the first sidewall, the top corner exposed by the floating gate layer is changed from a right-angle structure to an arc structure, so that the angle between the floating gate cantilever and the floating gate tunneling insulating layer is less than 90 degrees.
[0055] refer to Figure 8 As shown, an erase gate 191 is formed in the first trench 101, and a word line structure 192 is formed in the second trench 102. The erase gate 191 and the word line structure 192 are made of, for example, polysilicon.
[0056] The present application provides a semiconductor structure and a method for forming the same, which improves the structure of a floating gate cantilever and a floating gate tunneling insulating layer, and can improve the performance and yield of a split-gate flash memory device.
[0057] The embodiment of the present application also provides a semiconductor structure, referring to Figure 8As shown, it includes: a semiconductor substrate 100, on the surface of which a stacking structure of a floating gate dielectric layer 110, a floating gate layer 120, a control gate dielectric layer 130, a control gate layer 140 and a hard mask layer 150 is sequentially formed; a first trench 101 and a second trench 102 are located in the stacking structure and stop at the surface of the floating gate dielectric layer 110, the first trench 101 is located between two adjacent stacking structures, and the second trench 102 is located on both sides of the first trench 101 and the two adjacent stacking structures; a first sidewall 161 and a second sidewall 162 are respectively located The stacked structure sidewalls close to the first trench 101 and the stacked structure sidewalls close to the second trench 102; the dielectric material layer 170, located at the bottom and sidewalls of the first trench 101 and the bottom and sidewalls of the second trench 102, the portion of the dielectric material layer 170 located at the sidewalls of the second trench 102 constitutes a floating gate coupling dielectric layer, the portion of the dielectric material layer 170 located at the sidewalls of the floating gate layer 120 constitutes a floating gate tunneling insulating layer 180, and the portion of the floating gate layer 120 located at the lower surface of the first sidewall 161 and the lower surface of the floating gate tunneling insulating layer 180 constitutes a floating gate cantilever 190.
[0058] In some embodiments of the present application, the semiconductor structure described in the present application is, for example, a split-gate flash memory device.
[0059] In some embodiments of the present application, the material of the semiconductor substrate 100 includes (i) an elemental semiconductor, such as silicon or germanium; (ii) a compound semiconductor, such as silicon carbide, gallium arsenide, gallium phosphide or indium phosphide; (iii) an alloy semiconductor, such as silicon germanium carbide, silicon germanium, gallium arsenide phosphide or gallium indium phosphide; or (iv) a combination of the above.
[0060] In some embodiments of the present application, the floating gate dielectric layer 110 is made of, for example, silicon oxide. The thickness of the floating gate dielectric layer 110 is 80 to 100 angstroms, for example, 85 angstroms, 90 angstroms, or 95 angstroms.
[0061] In some embodiments of the present application, the floating gate layer 120 is made of polysilicon, for example, and has a thickness of 500 to 550 angstroms, for example, 510 angstroms, 520 angstroms, 525 angstroms, 530 angstroms, or 540 angstroms.
[0062] In some embodiments of the present application, the control gate dielectric layer 130 includes a three-layer stacked structure of silicon oxide-silicon nitride-silicon oxide.
[0063] In some embodiments of the present application, the material of the control gate layer 140 is, for example, polysilicon. The thickness of the control gate layer 140 is 600 to 700 angstroms, for example, 620 angstroms, 640 angstroms, 650 angstroms, 660 angstroms, or 680 angstroms.
[0064] In some embodiments of the present application, the material of the hard mask layer 150 is, for example, silicon nitride. The thickness of the hard mask layer 150 is 100 to 1200 angstroms, for example, 120 angstroms, 340 angstroms, 550 angstroms, 760 angstroms, or 980 angstroms.
[0065] refer to Figure 8 As shown, a first sidewall 161 of the stacked structure (specifically, the hard mask layer 150, the control gate layer 140, the control gate dielectric layer 130 and a portion of the floating gate layer 120) is formed on both sides of the first trench 101, and a second sidewall 162 of the stacked structure (specifically, the hard mask layer 150, the control gate layer 140, the control gate dielectric layer 130 and a portion of the floating gate layer 120) is formed on both sides of the second trench 102.
[0066] Continue to refer Figure 8 As shown, the first spacer 161 and the second spacer 162 include a double-layer structure of a first dielectric layer 141 and a second dielectric layer 142. Part of the first dielectric layer 141 is also located on the surface of the floating gate layer 120.
[0067] In some embodiments of the present application, the material of the first dielectric layer 141 is, for example, silicon oxide, and the thickness of the first dielectric layer 141 is 30-70 angstroms; the material of the second dielectric layer 142 is, for example, silicon nitride, and the thickness of the second dielectric layer 142 is 120-160 angstroms.
[0068] Continue to refer Figure 8 As shown, a dielectric material layer 170 is formed on the bottom and sidewalls of the first trench 101 , the bottom and sidewalls of the second trench 102 , the hard mask layer 150 , the first spacer 161 , and the upper surfaces of the second spacer 162 .
[0069] Among them, part of the dielectric material layer 170 located on the side wall of the second trench 102 constitutes a floating gate coupling dielectric layer; part of the dielectric material layer 170 located on the side wall of the floating gate layer 120 close to the first trench 101 constitutes a floating gate tunneling insulating layer 180; part of the floating gate layer 120 located on the lower surface of the first sidewall 161 and the lower surface of the floating gate tunneling insulating layer 180 constitutes a floating gate cantilever 190. That is to say, the part of the floating gate layer 120 protruding from the control gate layer 140 and close to the first trench 101 is the floating gate cantilever 190. The floating gate tunneling insulating layer 180 covers the corner of the floating gate cantilever 190.
[0070] In some embodiments of the present application, the length a of the floating gate cantilever 190 is 250 angstroms to 350 angstroms, for example, 280 angstroms, 300 angstroms or 330 angstroms, etc.; the distance b between the floating gate cantilever 190 and the lower surface of the floating gate layer 120 is 150 angstroms to 300 angstroms, for example, 180 angstroms, 200 angstroms or 220 angstroms, etc.
[0071] In some embodiments of the present application, the angle at which the floating gate tunneling insulating layer 180 covers the floating gate cantilever 190 is less than 90 degrees, for example, 88 degrees, 85 degrees, 82 degrees or 80 degrees.
[0072] In some embodiments of the present application, the thickness of the floating gate tunneling insulating layer 180 is 100 angstroms to 150 angstroms, for example, 110 angstroms, 120 angstroms, 130 angstroms or 140 angstroms. The length of the floating gate tunneling insulating layer 180 is 280 angstroms to 360 angstroms. The height of the floating gate tunneling insulating layer 180 is 150 angstroms to 300 angstroms. The length of the floating gate tunneling insulating layer 180 is 280 angstroms to 360 angstroms.
[0073] In some embodiments of the present application, the material of the floating gate tunneling insulating layer 180 includes silicon oxynitride or nitrided silicon oxide.
[0074] In the technical solution of the present application, the structure of the floating gate cantilever and the floating gate tunneling insulating layer is improved, and the erase and write tolerance of the split gate flash memory device is increased to 100,000 to 200,000 times or more, and the erase voltage can also be reduced to improve the data retention time in reliability. Specifically, the thickness of the third dielectric layer is increased to increase the length of the floating gate cantilever; a portion of the floating gate layer is etched to reduce the height of the floating gate cantilever; the material of the floating gate tunneling insulating layer is changed; when etching and removing a portion of the first sidewall, the top corner exposed by the floating gate layer is changed from a right-angle structure to an arc structure, so that the angle between the floating gate cantilever and the floating gate tunneling insulating layer is less than 90 degrees.
[0075] Continue to refer Figure 8 As shown, an erase gate 191 is formed in the first trench 101, and a word line structure 192 is formed in the second trench 102. The erase gate 191 and the word line structure 192 are made of, for example, polysilicon.
[0076] The present application provides a semiconductor structure and a method for forming the same, which improves the structure of a floating gate cantilever and a floating gate tunneling insulating layer, and can improve the performance and yield of a split-gate flash memory device.
[0077] In summary, after reading the contents of this application, those skilled in the art will appreciate that the aforementioned application contents may be presented only in an exemplary manner and may not be restrictive. Although not explicitly stated herein, those skilled in the art will appreciate that this application is intended to encompass various reasonable changes, improvements and modifications to the embodiments. These changes, improvements and modifications are within the spirit and scope of the exemplary embodiments of this application.
[0078] It should be understood that the term "and / or" used in this embodiment includes any or all combinations of one or more of the associated listed items. It should be understood that when an element is referred to as being "connected" or "coupled" to another element, it can be directly connected or coupled to another element, or there can also be intermediate elements.
[0079] Similarly, it should be understood that when an element such as a layer, region, or substrate is referred to as being "on" another element, it can be directly on the other element or there can be intervening elements. In contrast, the term "directly" means that there are no intervening elements. It should also be understood that the terms "comprising," "containing," "including," or "comprising," when used in this application document, indicate the presence of the recited features, wholes, steps, operations, elements, and / or components, but do not exclude the presence or addition of one or more other features, wholes, steps, operations, elements, components, and / or groups thereof.
[0080] It should also be understood that although the terms first, second, third, etc. can be used to describe various elements, these elements should not be limited by these terms. These terms are only used to distinguish one element from another element. Therefore, without departing from the teachings of the present application, the first element in some embodiments can be referred to as the second element in other embodiments. The same reference numerals or the same reference signs represent the same elements throughout the specification.
[0081] In addition, the present specification describes exemplary embodiments by reference to idealized exemplary cross-sectional views and / or plan views and / or stereograms. Therefore, differences from the illustrated shapes due to, for example, manufacturing techniques and / or tolerances are foreseeable. Therefore, the exemplary embodiments should not be interpreted as being limited to the shapes of the regions shown herein, but should include deviations in shapes caused by, for example, manufacturing. For example, an etched region shown as a rectangle will typically have circular or curved features. Therefore, the region shown in the figure is schematic in nature, and its shape is not intended to illustrate the actual shape of the region of the device nor to limit the scope of the exemplary embodiments.
Claims
1. A method for forming a semiconductor structure, characterized in that: include: Providing a semiconductor substrate, on the surface of which a stacking structure of a floating gate dielectric layer, a floating gate layer, a control gate dielectric layer, a control gate layer and a hard mask layer is sequentially formed; Etching the stacked structure to form a first trench and a second trench in the floating gate layer, wherein the first trench is located between two adjacent stacked structures, and the second trench is located on both sides of the first trench and the two adjacent stacked structures; A first sidewall of the stack structure is formed on both sides of the first trench, and a second sidewall of the stack structure is formed on both sides of the second trench, wherein the thickness of the first sidewall is greater than the thickness of the second sidewall; Etching the floating gate layer remaining at the bottom of the first trench and the second trench to the surface of the floating gate dielectric layer; Etching and removing a portion of the first sidewall; A dielectric material layer is formed at the bottom and sidewalls of the first trench and the bottom and sidewalls of the second trench, a portion of the dielectric material layer located on the sidewalls of the second trench constitutes a floating gate coupling dielectric layer, a portion of the dielectric material layer located on the sidewalls of the floating gate layer constitutes a floating gate tunneling insulating layer, and a portion of the floating gate layer located on the lower surface of the first sidewall and the lower surface of the floating gate tunneling insulating layer constitutes a floating gate cantilever.
2. The method for forming a semiconductor structure according to claim 1, wherein: The length of the floating gate cantilever is 250 angstroms to 350 angstroms; the distance between the floating gate cantilever and the lower surface of the floating gate layer is 150 angstroms to 250 angstroms.
3. The method for forming a semiconductor structure according to claim 1, wherein: The angle at which the floating gate tunneling insulating layer covers the floating gate cantilever is less than 90 degrees.
4. The method for forming a semiconductor structure according to claim 1, wherein: The floating gate tunneling insulating layer has a thickness of 100 angstroms to 150 angstroms.
5. The method for forming a semiconductor structure according to claim 1, wherein: The material of the floating gate tunneling insulating layer includes silicon oxynitride or nitrided silicon oxide.
6. The method for forming a semiconductor structure according to claim 5, wherein: The material of the floating gate tunneling insulating layer is nitrided silicon oxide, and the method for forming the dielectric material layer includes: forming a silicon oxide layer at the bottom and sidewalls of the first trench and the bottom and sidewalls of the second trench; An annealing process is performed on the silicon oxide layer, and nitrogen oxide gas is introduced into the reaction chamber during the annealing process.
7. The method for forming a semiconductor structure according to claim 1, wherein: The method of forming the first sidewall spacer and the second sidewall spacer comprises: Forming a first dielectric layer, a second dielectric layer and a third dielectric layer in sequence on the sidewall of the stacked structure, wherein the thickness of the third dielectric layer is greater than that of the first dielectric layer and the second dielectric layer; The third dielectric layer on one side of the second trench is removed, the first dielectric layer and the second dielectric layer on both sides of the second trench constitute the second sidewall, and the first dielectric layer, the second dielectric layer and the third dielectric layer on both sides of the first trench constitute the first sidewall.
8. The method for forming a semiconductor structure according to claim 7, wherein: The thickness of the first dielectric layer is 30-70 angstroms; the thickness of the second dielectric layer is 120-160 angstroms; and the thickness of the third dielectric layer is 300-500 angstroms.
9. The method for forming a semiconductor structure according to claim 1, wherein: Also includes: forming an erase gate in the first trench; A word line structure is formed in the second trench.
10. A semiconductor structure, characterized in that: include: A semiconductor substrate, wherein a stacked structure of a floating gate dielectric layer, a floating gate layer, a control gate dielectric layer, a control gate layer and a hard mask layer is sequentially formed on the surface of the semiconductor substrate; A first trench and a second trench are located in the stacked structure and stop at the surface of the floating gate dielectric layer, the first trench is located between two adjacent stacked structures, and the second trench is located on both sides of the first trench and the two adjacent stacked structures; A first sidewall and a second sidewall are respectively located on a sidewall of the stack structure close to the first groove and a sidewall of the stack structure close to the second groove; A dielectric material layer is located at the bottom and side walls of the first trench and the bottom and side walls of the second trench. Part of the dielectric material layer located at the side walls of the second trench constitutes a floating gate coupling dielectric layer, part of the dielectric material layer located at the side walls of the floating gate layer constitutes a floating gate tunneling insulating layer, and part of the floating gate layer located at the lower surface of the first sidewall and the lower surface of the floating gate tunneling insulating layer constitutes a floating gate cantilever.
11. The semiconductor structure according to claim 10, characterized in that The length of the floating gate cantilever is 250 angstroms to 350 angstroms; the distance between the floating gate cantilever and the lower surface of the floating gate layer is 150 angstroms to 250 angstroms.
12. The semiconductor structure according to claim 10, wherein: The angle at which the floating gate tunneling insulating layer covers the floating gate cantilever is less than 90 degrees.
13. The semiconductor structure according to claim 10, wherein: The floating gate tunneling insulating layer has a thickness of 100 angstroms to 150 angstroms.
14. The semiconductor structure according to claim 10, wherein: The material of the floating gate tunneling insulating layer includes silicon oxynitride or nitrided silicon oxide.
15. The semiconductor structure according to claim 10, wherein: Also includes: an erase gate located in the first trench; and a word line structure located in the second trench.
Citation Information
Patent Citations
Method for improving erasing efficiency of floating gate type flash memory and floating gate type flash memory
CN108122920A
Method for manufacturing flash memory device
CN109378314A
Method for manufacturing flash memory device
CN110137085A
Memory cell structure and forming method thereof
CN115715086A
Cited By
Semiconductor structure, semiconductor memory and preparation method of semiconductor structure
CN120035142A
A semiconductor structure, a semiconductor memory and a method for manufacturing a semiconductor structure
CN120035142B