Method and device for inhibiting reservoir effect of coated alkali metal atom gas chamber

By controlling the temperature difference in the gas chamber and the sealing of the coating material, the problem of the reservoir effect of the coating alkali metal atomic gas chamber is solved, the polarization life and relaxation resistance are improved, and the stability and reversibility in the gas chamber are achieved .

CN118957499AActive Publication Date: 2024-11-15PEKING UNIV
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411028909.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-30
Publication Date
2024-11-15
Estimated Expiration
2044-07-30

AI Technical Summary

Technical Problem

The prior art is difficult to effectively suppress the reservoir effect of the coated alkali metal atomic gas chamber, resulting in a shortening of polarization life and a decrease in relaxation resistance. The commonly used glass locking method is complex and unreproducible, and the uncoated part will affect the polarization life. Measurement.

Method used

By controlling the maturation temperature difference between the bubble body and the bubble tail during the maturation process of the air chamber, and sealing the capillary with coating materials, the reservoir effect is suppressed and the ground polarization life and relaxation resistance are improved. Specific methods include isolation heating and water bath heating, ensuring uniform heating of the coating material, avoiding damage to the relaxation resistance, and stabilizing the atomic density through repeated heating and cooling operations.

Benefits of technology

Effectively suppress the reservoir effect, improve the ground-state polarization life and relaxation resistance of alkali metal atoms in the gas chamber, ensure the reversibility and repeatability of the coating gas chamber, and avoid measurement errors and performance degradation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118957499A_ABST
    Figure CN118957499A_ABST
Patent Text Reader

Abstract

The invention provides a method and device for inhibiting the reservoir effect of a coated alkali metal atom gas chamber, and the method comprises the steps: separately heating a bubble tail and a bubble body of a first coated gas chamber which is placed in a manner that the bubble tail faces upwards to a first preset temperature and a second preset temperature, the bubble tail and the bubble body are maintained at respective corresponding preset temperatures within a first preset time, and the first preset temperature is higher than a second preset temperature; heating the bubble tail of a first coating gas chamber which is naturally cooled to the room temperature and placed in a mode that the bubble tail faces downwards to a third preset temperature, and maintaining the bubble tail at the third preset temperature within a second preset time; and a bubble body of a first coating gas chamber which is naturally cooled to the room temperature and placed in a mode that the bubble tail faces upwards is heated to a fourth preset temperature in an isolated mode, the bubble body is maintained at the fourth preset temperature within third preset time, and the reservoir effect is effectively restrained. And the ground state polarization life and the anti-relaxation performance of alkali metal atoms in the air chamber are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of atomic gas chamber secondary processing and performance optimization, and in particular to a method and device for suppressing the reservoir effect of a film-coated alkali metal atomic gas chamber. Background Art

[0002] Atomic gas cells with long ground-state polarization lifetime have broad application prospects and great application value in the fields of quantum electromagnetic sensing, optical storage, and quantum frequency standards. In the implementation of long ground-state polarization lifetime, the coated atomic gas cell has advantages over the buffer gas cell, such as narrow magnetic resonance linewidth, low operating temperature, longer polarization lifetime, and smaller optical depth. It plays the role of a core device in high-sensitivity atomic magnetometers and other quantum precision measurement applications that use the interaction between light and atoms.

[0003] How to improve the ground state polarization lifetime of the coated atomic gas cell has always been a key issue that restricts the detection sensitivity of atomic magnetometers, atomic gyroscopes and other precision measuring instruments. For optical atomic magnetometers based on coated gas cells, the research goal is to approach the spin projection noise limit determined by spin destruction collisions when the sensitivity is close to the spin projection noise limit determined by spin destruction collisions when working at a higher temperature than the melting temperature of the coating. This requires extremely high coating anti-relaxation performance to ensure that the longitudinal relaxation time of the gas cell is almost not restricted by the coating relaxation rate. For ordinary coated atomic gas cells, the gas exchange between the alkali metal atomic vapor in the gas cell body (bubble body) and the alkali metal atomic reservoir at the end of the gas cell (bubble tail) can cause an average effect of anti-relaxation performance between the uncoated area of ​​the bubble tail and the coated area of ​​the bubble body, similar to a communicating vessel, which shortens the measured polarization lifetime. This is called the "reservoir effect". When the coating has serious defects, this effect is not obvious and is mainly limited by the intrinsic polarization lifetime in the bubble body, but it is crucial in a gas cell with uniform coating. This effect can be suppressed by reducing the capillary aperture at the connection between the bubble body and the bubble tail. The current internationally common method for suppressing the bubble tail reservoir effect is to add a movable "glass lock" with adjustable aperture at the capillary. This method has several significant defects in practical applications: first, the glass lock has a complex structure and requires fine parameter control based on the original design of the coated gas chamber, which increases the complexity of the application and has poor reproducibility. At present, there is no precedent reported internationally for successfully preparing multiple glass lock gas chambers from the same batch of gas chambers; second, the glass lock is not coated, and this part of the bare glass surface will be included in the measurement of the polarization life of the bubble after blocking the capillary, causing measurement errors and shortening of the polarization life. At present, there are international reports that the polarization life measured after the glass lock blocks the capillary is shorter than that without blocking, which loses the original purpose of designing the glass lock. Summary of the invention

[0004] In response to the above technical problems, the present application provides a method and device for suppressing the gas chamber reservoir effect of coated alkali metal atoms. By cleverly controlling the maturation temperature difference between the bubble body and the bubble tail during the gas chamber maturation process, the reservoir effect is effectively suppressed, thereby improving the ground state polarization life and anti-relaxation performance of the alkali metal atoms in the gas chamber.

[0005] In a first aspect, the present application provides a method for suppressing the gas chamber reservoir effect of a film-coated alkali metal atom, comprising:

[0006] The bubble tail and the bubble body of the first coating air chamber placed with the bubble tail facing upward are isolated and heated to a first preset temperature and a second preset temperature respectively, and the bubble tail and the bubble body are maintained at their respective corresponding preset temperatures within a first preset time, wherein the first preset temperature is greater than the second preset temperature;

[0007] Heat the bubble tail of the first coating air chamber that is naturally cooled to room temperature and placed with the bubble tail facing downward to a third preset temperature, and maintain the bubble tail at the third preset temperature for a second preset time;

[0008] Insulating and heating the bubble of the first coating air chamber that is naturally cooled to room temperature and placed with the bubble tail facing upward to a fourth preset temperature, and maintaining the bubble at the fourth preset temperature for a third preset time;

[0009] When the bubble is naturally cooled to room temperature, a second coating air chamber in which the reservoir effect has been suppressed is obtained.

[0010] An embodiment of the present application provides a method for suppressing the reservoir effect of the gas chamber of coated alkali metal atoms. During the maturation process of the coated gas chamber, different parts of the gas chamber are temperature-controlled and heated, and the placement of the gas chamber is continuously changed. The excess molten coating material in the bubble tail and the bubble body is deposited in the capillary at the connection between the bubble tail and the bubble body through the action of gravity, and the bubble tail reservoir is blocked by the coating material, thereby suppressing the reservoir effect or even completely eliminating the reservoir effect, thereby improving the ground state polarization lifetime and anti-relaxation performance of the alkali metal atoms in the gas chamber.

[0011] In a possible implementation, the heating of the bubble isolation to the second preset temperature, the heating of the bubble tail to the third preset temperature, and the heating of the bubble isolation to the fourth preset temperature are all performed by water bath heating;

[0012] During the water bath heating process, the capillary at the connection between the bubble body and the bubble tail of the first coating air chamber is always immersed in the distilled water used for water bath heating.

[0013] In the embodiments of the present application, a water bath heating scheme is used multiple times, which can make the coated part of the coating chamber heated evenly, avoid destroying the original anti-relaxation performance of the coating chamber during the heating process, and is beneficial to maintaining and improving the anti-relaxation performance of the coating chamber.

[0014] Furthermore, the first coating air chamber is a coating air chamber in which the coating material is over-evaporated.

[0015] In the embodiment of the present application, the coating air chamber with excessive evaporation of the coating material is limited as the treatment object, ensuring that there is sufficient coating material in the air chamber to seal and cover the capillaries at the connection between the bubble body and the bubble tail, and at the same time, it is beneficial for the coating to fully cover the inner surface of the air chamber body, eliminating the negative impact of the bare glass surface on the anti-relaxation performance.

[0016] In a possible implementation, the method further includes stabilizing the atomic number density of the second coating gas chamber, including:

[0017] The second coating air chamber is subjected to several heating and cooling operations to obtain a corresponding stable coating air chamber, wherein the interval between each heating and cooling operation is a fourth preset time, and each heating and cooling operation is specifically:

[0018] The bubble body of the second coating air chamber is placed with the bubble tail facing upward and is isolated and heated to a fifth preset temperature, and the bubble body is maintained at the fifth preset temperature for a fifth preset time.

[0019] An embodiment of the present application provides a method for stabilizing the atomic number density in an air chamber. After obtaining a second coated air chamber in which the reservoir effect has been suppressed, the relative stability of the atomic number density in the air chamber within a wide temperature range can be further achieved through repeated heating. At the same time, benefiting from the unique reservoir effect suppression method of the present application, during the repeated heating process, the capillary of the second coated air chamber is always in a blocked state. Therefore, during the heating process, the bubble tail and the bubble body will not produce gas interaction and thus affect the relative stability of the atomic number density. During the temperature maintenance process, the temperature inside the bubble body will not be affected by the bubble tail temperature, thereby further improving the stability of the atomic number density in the air chamber and enriching the application scenarios of the present application.

[0020] Furthermore, the fourth preset time and the fifth preset time are determined according to the atomic number density and the ground state polarization lifetime of the second coating gas chamber.

[0021] In a possible implementation, the method further includes restoring the second film-depositing air chamber to the first film-depositing air chamber, including:

[0022] heating the capillary at the connection between the bubble body and the bubble tail of the second coating air chamber placed in a manner that the bubble tail faces upward to a sixth preset temperature;

[0023] When the capillary tube reaches the sixth preset temperature, continue to heat the capillary tube within a sixth preset time;

[0024] When the foam body is naturally cooled to room temperature, the first coating air chamber reduced by the second coating air chamber is obtained.

[0025] The embodiment of the present application provides a method for restoring a coating gas chamber that suppresses the reservoir effect. By continuously heating the capillary, the capillary blocked by the coating material is cleared again, ensuring the reversibility and repeatability of the method for suppressing the reservoir effect of the coating alkali metal atom gas chamber provided by the present application, making the application of the present application more flexible and the suppression of the reservoir effect of the coating alkali metal atom gas chamber safer. For example, after a second coating gas chamber with poor performance is obtained due to improper operation, it can also be restored to the first coating gas chamber without causing irreversible damage to the coating gas chamber.

[0026] In a second aspect, accordingly, the present application provides a device for suppressing the gas chamber reservoir effect of a film-coated alkali metal atom, the device being used to implement any method for suppressing the gas chamber reservoir effect of a film-coated alkali metal atom described in the present application, the device comprising a heating furnace, a heating module and a temperature control module;

[0027] The heating furnace comprises a container and a heat-insulating cover plate, wherein the container is used to load the first coating air chamber for heating, and the heat-insulating cover plate is used to isolate the bubble tail and bubble body of the first coating air chamber during the heating process;

[0028] The outside of the heating furnace is connected to the heating module, and the heating module includes a high-temperature resistant heating belt, two annular heating plates, three programmable AC power supplies and two normally-off relays, wherein the high-temperature resistant heating belt is wrapped around the surface of the container, and is connected to the first programmable AC power supply through the first normally-off relay, and is used to heat the container, the first annular heating plate is located above the thermal insulation cover plate, and is connected to the second programmable AC power supply through the second normally-off relay, and is used to heat the bubble tail passing through the thermal insulation cover plate, the second annular heating plate is wrapped around the capillary at the connection between the bubble body and the bubble tail of the first coating air chamber, and is connected to the third programmable AC power supply, and is used to continuously heat the capillary;

[0029] The temperature control module includes two thermistor probes, a temperature data acquisition system and a multi-channel PID automatic control system, wherein the two thermistor probes are connected to the input end of the temperature data acquisition system for acquiring temperature data of a preset position, and the multi-channel PID automatic control system is respectively connected to the output end of the temperature data acquisition system and two normally-off relays for controlling the on and off of the two normally-off relays through temperature data, thereby controlling the heating temperature of the high-temperature resistant heating belt and the first annular heating plate.

[0030] The embodiment of the present application provides a device for suppressing the gas chamber reservoir effect of the alkali metal atom of the film coating, which is used to implement any method of suppressing the gas chamber reservoir effect of the alkali metal atom of the film coating described in the present application. Among them, the container and the heat-insulating cover plate in the heating furnace can realize the isolation of different parts of the film coating gas chamber, and the heating module can realize the heating of the fixed position through a programmable AC power supply and a correspondingly connected heating belt or heating plate, wherein the high-temperature resistant heating belt is wrapped around the surface of the container, and distilled water can be added to the container to realize water bath heating, and the annular heating plate can be directly heated to the contacted position. At the same time, the device is also equipped with a temperature control module, which can automatically control the heating module to heat to a preset temperature. During the heating process of the heating module, the temperature control module obtains the real-time temperature of the corresponding position through the thermistor probe, and transmits the real-time temperature to the multi-channel PID automatic control system, so that the multi-channel PID automatic control system compares the real-time temperature with the preset temperature, and controls the on and off of the normally-off relay according to the comparison result to realize the control of the heating temperature. While realizing the method of suppressing the gas chamber reservoir effect of the alkali metal atom of the film coating, the embodiment of the present application can also automatically heat the specified position to the preset temperature, thereby improving the implementation efficiency of the method.

[0031] Furthermore, a through hole of a preset diameter is provided on the thermal insulation cover plate and a matching cross rubber plug is embedded therein. When the first coated air chamber is placed with the bubble tail facing upward, the bubble tail can pass through the cross rubber plug and be fixed at any preset height.

[0032] In the embodiment of the present application, a through hole of a preset diameter is provided on the thermal insulation cover plate and a matching cross rubber plug is embedded therein, so that the coating air chamber can pass the bubble tail through the cross rubber plug to achieve isolated heating. At the same time, the cross rubber plug can also fix the coating air chamber so that the bubble body of the coating air chamber is suspended inside the heating furnace, so that the coating part of the coating air chamber is heated evenly, which is beneficial to maintain and improve the anti-relaxation performance of the coating air chamber.

[0033] In one possible implementation, the multi-channel PID automatic control system includes an input differential module and a dual-channel temperature feedback module, wherein the input differential module is used to differentiate the temperature data of two inputs to obtain the temperature difference between the two temperature data, and the dual-channel temperature feedback module is used to compare the temperature data of the two inputs with the corresponding preset temperatures respectively, thereby controlling the on and off of the two normally-off relays.

[0034] In an embodiment of the present application, the multi-channel PID automatic control system is constructed by a differential module and a dual-channel temperature feedback module, so that the multi-channel PID automatic control system can adjust the on and off of two normally-off relays in real time according to the two-channel temperature data obtained, thereby accurately controlling the temperature difference between the bubble body and the bubble tail of the coating gas chamber during the heating and insulation process, thereby realizing differential temperature heating.

[0035] Furthermore, the length of the second annular heating plate is smaller than the length of the capillary tube, and asbestos insulation material is provided between the second annular heating plate and the foam body.

[0036] In the embodiment of the present application, since the second annular heating plate is mainly used to heat the capillary and thus realize the reduction of the coated air chamber, the length of the second annular heating plate is set to be smaller than the length of the capillary in order to avoid accidentally heating the bubble tail or the bubble body during the heating of the capillary; similarly, asbestos insulation material is arranged under the second annular heating plate to prevent the heating plate at high temperature from directly contacting the coated bubble body and destroying the anti-relaxation performance of the coating, thereby improving the safety of the reduction process of the coated air chamber. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] Figure 1 : A schematic flow chart of a method for suppressing the gas chamber reservoir effect of coated alkali metal atoms provided in an embodiment of the present application.

[0038] Figure 2 : A schematic diagram of the structure of a device for suppressing the gas chamber reservoir effect of coated alkali metal atoms provided in an embodiment of the present application during use.

[0039] Figure 3 : A flow chart of a method for suppressing the reservoir effect using a device for suppressing the reservoir effect of a film-coated alkali metal atom gas chamber provided in an embodiment of the present application.

[0040] Figure 4 : Another structural schematic diagram of a device for suppressing the gas chamber reservoir effect of coated alkali metal atoms provided in an embodiment of the present application during use. DETAILED DESCRIPTION

[0041] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.

[0042] It should be noted that the step numbers in the text are only for the convenience of explanation of the specific embodiments and do not serve to limit the order in which the steps are executed. In the description of this application, the terms "first" and "second" are only used for descriptive purposes and cannot be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features.

[0043] Throughout the entire specification, the coated gas chamber described in this specification is a coated alkali metal atom gas chamber, and the coated alkali metal atom gas chamber is produced by coating the inner wall of the alkali metal atom gas chamber based on anti-relaxation coating materials and anti-relaxation coating technology.

[0044] Embodiment 1:

[0045] like Figure 1 As shown, embodiment 1 provides a method for suppressing the gas chamber reservoir effect of the plated alkali metal atoms, including steps S1-S4:

[0046] Step S1, isolating and heating the bubble tail and the bubble body of the first coating air chamber placed in a bubble tail-upward manner to a first preset temperature and a second preset temperature respectively, and maintaining the bubble tail and the bubble body at their respective corresponding preset temperatures within a first preset time, wherein the first preset temperature is greater than the second preset temperature;

[0047] Step S2, heating the bubble tail of the first coating air chamber that is naturally cooled to room temperature and placed with the bubble tail facing downward to a third preset temperature, and maintaining the bubble tail at the third preset temperature for a second preset time;

[0048] Step S3, isolating and heating the bubble of the first coating air chamber that has been naturally cooled to room temperature and placed with its bubble tail facing upward to a fourth preset temperature, and maintaining the bubble at the fourth preset temperature for a third preset time;

[0049] Step S4: After the foam body is naturally cooled to room temperature, a second coating air chamber in which the reservoir effect has been suppressed is obtained.

[0050] An embodiment of the present application provides a method for suppressing the reservoir effect of the gas chamber of coated alkali metal atoms. During the maturation process of the coated gas chamber, different parts of the gas chamber are temperature-controlled and heated, and the placement of the gas chamber is continuously changed. The excess molten coating material in the bubble tail and the bubble body is deposited in the capillary at the connection between the bubble tail and the bubble body through the action of gravity, and the bubble tail reservoir is blocked by the coating material, thereby suppressing the reservoir effect or even completely eliminating the reservoir effect, thereby improving the ground state polarization lifetime and anti-relaxation performance of the alkali metal atoms in the gas chamber.

[0051] In a preferred embodiment, the first preset temperature is set to 70 degrees Celsius, the second preset temperature is set to 61 degrees Celsius, the third preset temperature is set to 63 degrees Celsius, the fourth preset temperature is set to 61 degrees Celsius, the room temperature is between 20-35 degrees Celsius, the first preset time is 2 hours, the second preset time is 9 hours, and the third preset time is 12 hours.

[0052] In a possible implementation, the heating of the bubble isolation to the second preset temperature, the heating of the bubble tail to the third preset temperature, and the heating of the bubble isolation to the fourth preset temperature are all performed by water bath heating;

[0053] During the water bath heating process, the capillary at the connection between the bubble body and the bubble tail of the first coating air chamber is always immersed in the distilled water used for water bath heating.

[0054] In the embodiments of the present application, a water bath heating scheme is used multiple times, which can make the coated part of the coating chamber heated evenly, avoid destroying the original anti-relaxation performance of the coating chamber during the heating process, and is beneficial to maintaining and improving the anti-relaxation performance of the coating chamber.

[0055] Furthermore, the first coating air chamber is a coating air chamber in which the coating material is over-evaporated.

[0056] In the embodiment of the present application, the coating air chamber with excessive evaporation of the coating material is limited as the treatment object, ensuring that there is sufficient coating material in the air chamber to seal and cover the capillaries at the connection between the bubble body and the bubble tail, and at the same time, it is beneficial for the coating to fully cover the inner surface of the air chamber body, eliminating the negative impact of the bare glass surface on the anti-relaxation performance.

[0057] In a possible implementation, after completing step S4, the method further includes stabilizing the atomic number density of the second coating gas chamber, including:

[0058] The second coating air chamber is subjected to several heating and cooling operations to obtain a corresponding stable coating air chamber, wherein the interval between each heating and cooling operation is a fourth preset time, and each heating and cooling operation is specifically:

[0059] The bubble body of the second coating air chamber is placed with the bubble tail facing upward and is isolated and heated to a fifth preset temperature, and the bubble body is maintained at the fifth preset temperature for a fifth preset time.

[0060] In a preferred embodiment, the fifth preset temperature is 47 degrees Celsius, and since the heating of the bubble body is isolated heating, the temperature of the bubble tail is always at room temperature during this process. The fourth preset time is 30 days, and the fifth preset time is 30 minutes.

[0061] An embodiment of the present application provides a method for stabilizing the atomic number density in an air chamber. After obtaining a second coated air chamber in which the reservoir effect has been suppressed, the relative stability of the atomic number density in the air chamber within a wide temperature range can be further achieved through repeated heating. At the same time, benefiting from the unique reservoir effect suppression method of the present application, during the repeated heating process, the capillary of the second coated air chamber is always in a blocked state. Therefore, during the heating process, the bubble tail and the bubble body will not produce gas interaction and thus affect the relative stability of the atomic number density. During the temperature maintenance process, the temperature inside the bubble body will not be affected by the bubble tail temperature, thereby further improving the stability of the atomic number density in the air chamber and enriching the application scenarios of the present application.

[0062] Furthermore, the fourth preset time and the fifth preset time are determined according to the atomic number density and the ground state polarization lifetime of the second coating chamber. In a preferred embodiment, the changes in the atomic number density and the ground state polarization lifetime in the coating chamber can be monitored daily during the interval between each operation, and the fourth preset time and the fifth preset time can be dynamically adjusted. Furthermore, the number of operations of the heating and cooling operations can also be flexibly adjusted according to the changes in the atomic number density and the ground state polarization lifetime of the second coating chamber. Generally, for the paraffin coating chamber, the number of operations of the heating and cooling operations needs to be performed more than 3 times.

[0063] In a possible implementation, the method further includes restoring the second film-depositing air chamber to the first film-depositing air chamber, including:

[0064] heating the capillary at the connection between the bubble body and the bubble tail of the second coating air chamber placed in a manner that the bubble tail faces upward to a sixth preset temperature;

[0065] When the capillary tube reaches the sixth preset temperature, continue to heat the capillary tube within a sixth preset time;

[0066] When the foam body is naturally cooled to room temperature, the first coating air chamber reduced by the second coating air chamber is obtained.

[0067] In a preferred embodiment, the sixth preset temperature is set to 95 degrees Celsius, and the sixth preset time is set to 1 hour. In order to avoid the influence of the water bath heating scheme on other parts of the coating chamber, a heating plate is generally used to contact the capillary for heating.

[0068] The embodiment of the present application provides a method for restoring a coating gas chamber that suppresses the reservoir effect. By continuously heating the capillary, the capillary blocked by the coating material is cleared again, ensuring the reversibility and repeatability of the method for suppressing the reservoir effect of the coating alkali metal atom gas chamber provided by the present application, making the application of the present application more flexible and the suppression of the reservoir effect of the coating alkali metal atom gas chamber safer. For example, after a second coating gas chamber with poor performance is obtained due to improper operation, it can also be restored to the first coating gas chamber without causing irreversible damage to the coating gas chamber.

[0069] Embodiment 2:

[0070] Accordingly, embodiment 2 provides a device for suppressing the gas chamber reservoir effect of alkali metal atoms in film coating, the device is used to implement any method for suppressing the gas chamber reservoir effect of alkali metal atoms in film coating described in the present application, the device includes a heating furnace, a heating module and a temperature control module;

[0071] The heating furnace comprises a container and a heat-insulating cover plate, wherein the container is used to load the first coating air chamber for heating, and the heat-insulating cover plate is used to isolate the bubble tail and bubble body of the first coating air chamber during the heating process;

[0072] The outside of the heating furnace is connected to the heating module, and the heating module includes a high-temperature resistant heating belt, two annular heating plates, three programmable AC power supplies and two normally-off relays, wherein the high-temperature resistant heating belt is wrapped around the surface of the container, and is connected to the first programmable AC power supply through the first normally-off relay, and is used to heat the container, the first annular heating plate is located above the thermal insulation cover plate, and is connected to the second programmable AC power supply through the second normally-off relay, and is used to heat the bubble tail passing through the thermal insulation cover plate, the second annular heating plate is wrapped around the capillary at the connection between the bubble body and the bubble tail of the first coating air chamber, and is connected to the third programmable AC power supply, and is used to continuously heat the capillary;

[0073] The temperature control module includes two thermistor probes, a temperature data acquisition system and a multi-channel PID automatic control system, wherein the two thermistor probes are connected to the input end of the temperature data acquisition system for acquiring temperature data of a preset position, and the multi-channel PID automatic control system is respectively connected to the output end of the temperature data acquisition system and two normally-off relays for controlling the on and off of the two normally-off relays through temperature data, thereby controlling the heating temperature of the high-temperature resistant heating belt and the first annular heating plate.

[0074] The embodiment of the present application provides a device for suppressing the gas chamber reservoir effect of the alkali metal atom of the film coating, which is used to implement any method of suppressing the gas chamber reservoir effect of the alkali metal atom of the film coating described in the present application. Among them, the container and the heat-insulating cover plate in the heating furnace can realize the isolation of different parts of the film coating gas chamber, and the heating module can realize the heating of the fixed position through a programmable AC power supply and a correspondingly connected heating belt or heating plate, wherein the high-temperature resistant heating belt is wrapped around the surface of the container, and distilled water can be added to the container to realize water bath heating, and the annular heating plate can be directly heated to the contacted position. At the same time, the device is also equipped with a temperature control module, which can automatically control the heating module to heat to a preset temperature. During the heating process of the heating module, the temperature control module obtains the real-time temperature of the corresponding position through the thermistor probe, and transmits the real-time temperature to the multi-channel PID automatic control system, so that the multi-channel PID automatic control system compares the real-time temperature with the preset temperature, and controls the on and off of the normally-off relay according to the comparison result to realize the control of the heating temperature. While realizing the method of suppressing the gas chamber reservoir effect of the alkali metal atom of the film coating, the embodiment of the present application can also automatically heat the specified position to the preset temperature, thereby improving the implementation efficiency of the method.

[0075] Furthermore, a through hole of a preset diameter is provided on the thermal insulation cover plate and a matching cross rubber plug is embedded therein. When the first coated air chamber is placed with the bubble tail facing upward, the bubble tail can pass through the cross rubber plug and be fixed at any preset height.

[0076] In the embodiment of the present application, a through hole of a preset diameter is provided on the thermal insulation cover plate and a matching cross rubber plug is embedded therein, so that the coating air chamber can pass the bubble tail through the cross rubber plug to achieve isolated heating. At the same time, the cross rubber plug can also fix the coating air chamber so that the bubble body of the coating air chamber is suspended inside the heating furnace, so that the coating part of the coating air chamber is heated evenly, which is beneficial to maintain and improve the anti-relaxation performance of the coating air chamber.

[0077] In one possible implementation, the multi-channel PID automatic control system includes an input differential module and a dual-channel temperature feedback module, wherein the input differential module is used to differentiate the temperature data of two inputs to obtain the temperature difference between the two temperature data, and the dual-channel temperature feedback module is used to compare the temperature data of the two inputs with the corresponding preset temperatures respectively, thereby controlling the on and off of the two normally-off relays.

[0078] In an embodiment of the present application, the multi-channel PID automatic control system is constructed by a differential module and a dual-channel temperature feedback module, so that the multi-channel PID automatic control system can adjust the on and off of two normally-off relays in real time according to the two-channel temperature data obtained, thereby accurately controlling the temperature difference between the bubble body and the bubble tail of the coating gas chamber during the heating and insulation process, thereby realizing differential temperature heating.

[0079] Furthermore, the length of the second annular heating plate is smaller than the length of the capillary tube, and asbestos insulation material is provided between the second annular heating plate and the foam body.

[0080] In the embodiment of the present application, since the second annular heating plate is mainly used to heat the capillary and thus realize the reduction of the coated air chamber, the length of the second annular heating plate is set to be smaller than the length of the capillary in order to avoid accidentally heating the bubble tail or the bubble body during the heating of the capillary; similarly, asbestos insulation material is arranged under the second annular heating plate to prevent the heating plate at high temperature from directly contacting the coated bubble body and destroying the anti-relaxation performance of the coating, thereby improving the safety of the reduction process of the coated air chamber.

[0081] In a preferred embodiment, the structural schematic diagram of the device for suppressing the gas chamber reservoir effect of the film-coated alkali metal atoms is as follows: Figure 2 As shown, it includes a high temperature resistant heating belt 1, a boron nitride heating furnace 2, distilled water 3, an air chamber bubble 4, a capillary tube 5 at the connection, a first detachable annular heating plate 6, a first waterproof thermistor probe 7, a temperature data acquisition system 8, a multi-channel PID automatic control system 9, a first normally-off relay 10, a first programmable AC power supply 11, a first control output port 12, a second control output port 13, a second programmable AC power supply 14, a second normally-off relay 15, an air chamber bubble tail 16, a second detachable annular heating plate 17, a third programmable AC power supply 18, a heat preservation cover 19, and a second waterproof thermistor probe 20;

[0082] The air chamber bubble 4 and the capillary tube 5 at the connection are immersed in the distilled water 3 contained in the boron nitride heating furnace 2. The heating furnace 2 is covered with a heat preservation cover 19, and the heat preservation cover 19 is perforated to facilitate the first waterproof thermistor probe 7 and other heating devices to enter the interior of the heating furnace 2. The second detachable annular heating plate 17 is wound and fixed on the outside of the air chamber bubble tail 16, and its heating is controlled by the second programmable AC power supply 14 and the normally-off relay 15; the first detachable annular heating plate 6 is wound on the outside of the capillary tube 5 at the connection, and its heating is controlled by the third programmable AC power supply 18. The waterproof thermistor probes 7 and 20 are respectively fixed on the outer surfaces of the air chamber bubble 4 and the air chamber bubble tail 16, and the other ends are connected to the input port of the temperature data acquisition system 8. The high-temperature resistant heating belt 1 is evenly wound on the outside of the boron nitride heating furnace 2, and its heating is controlled by the first programmable AC power supply 11 and the normally-off relay 10.

[0083] The output port of the temperature data acquisition system 8 is connected to the input end of the multi-channel PID automatic control system 9, and the control output ports 12 and 13 are respectively connected to the two normally-off relays 10 and 15 that control the programmable AC power supplies 11 and 14. The temperature information feedback provided by the temperature data acquisition system 8 controls the on and off of the normally-off relays 10 and 15, thereby controlling the heating power of the corresponding boron nitride heating furnace and bubble tail, thereby achieving the purpose of separate temperature regulation.

[0084] Further, such as Figure 3 As shown, the specific steps of using the above device to implement the method of suppressing the gas chamber reservoir effect of the plated alkali metal atoms described in this application are as follows:

[0085] 1) Preparing a coating chamber for evaporating excess coating material.

[0086] 2) In stage one, while keeping the programmable AC power supplies 11, 14, and 18 disconnected, inject a sufficient amount of distilled water 3 into the boron nitride heating furnace 2, and put the air chamber bubble tail 16 into the heating furnace with the air chamber bubble tail facing upwards. The tail passes through the cross rubber plug on the insulation cover 19 and is fixed at a height until the air chamber bubble body 4 and the capillary 5 at the connection are completely immersed in the distilled water 3; two waterproof thermistor probes 7 and 20 are respectively fixed on the side walls of the air chamber bubble body 4 and the air chamber bubble tail 16.

[0087] 3) Set the first preset temperature and the second preset temperature of the stage one of the multi-channel PID automatic control system 9: the bubble tail is 70°C, the bubble body (water temperature) is 61°C, turn on the programmable AC power supply 11, 14, and when the measured temperature fed back by the waterproof thermistor probes 7, 20 is lower than the set initial working temperature, the normally-off relays 10, 15 are closed, and the high-temperature resistant heating belt 1 and the detachable annular heating plate 17 perform AC heating on the bubble body 4 (inside the heating furnace 2) and the bubble tail 16 respectively.

[0088] 4) When the measured temperatures of the two waterproof thermistor probes 7 and 20 reach the first preset temperature and the second preset temperature for the first time, the temperature control maintenance stage of stage one is entered, and the multi-channel PID automatic control system 9 receives the data input by the temperature data acquisition system 8, and controls the on and off of the normally-off relays 10 and 15 through the output ports 12 and 13 respectively, so as to maintain the temperature difference between the air chamber bubble 4 and the air chamber bubble tail 16 for 2 hours, and then turns off the programmable AC power supplies 11 and 14 to allow the air chamber bubble tail 16 and the air chamber bubble 4 to cool naturally to room temperature.

[0089] 5) Stage 2: Remove the second detachable annular heating plate 17 and open the heat preservation cover 19, take out the coated air chamber that has cooled to room temperature and put it back into the boron nitride heating furnace 2 with the air chamber tail 16 facing downward, and re-fix the two waterproof thermistor probes 7 and 20 on the distilled water 3 and the bubble body 4 respectively. During the treatment process of stage 2, ensure that the capillary 5 at the connection is always immersed in the distilled water 3. The schematic diagram of the device of stage 2 is shown in the figure. Figure 4 shown.

[0090] 6) The third preset temperature of the second stage is set for the multi-channel PID automatic control system 9: the air chamber bulb 4 (water temperature) is set to 63° C. During the second stage processing, the second waterproof thermistor probe 20 attached to the bulb 4 always monitors the air temperature above the boron nitride heating furnace 2.

[0091] 7) When the measured temperature of the first waterproof thermistor probe 7 fixed in the distilled water 3 reaches the third preset temperature for the first time, the second stage of temperature control maintenance is entered, and the current working temperature is maintained for 9 hours. After that, the first programmable AC power supply 11 is turned off to cool the inside of the boron nitride heating furnace 2 to room temperature.

[0092] 8) Stage 3: Repeat the coating air chamber placement and heating methods of stage 1. The difference from stage 1 is that the air chamber bubble tail 16 is not heated, so that the air chamber bubble tail 16 is always maintained at room temperature. The fourth preset temperature of stage 3 is set for the multi-channel PID automatic control system 9: the air chamber bubble body 4 (water temperature) is 61°C.

[0093] 9) When the temperature measured by the first waterproof thermistor probe 7 fixed on the bulb 4 reaches the fourth preset temperature for the first time, the stage three temperature control holding stage is entered, and the current temperature of the distilled water 3 is maintained for 12 hours. After that, the first programmable AC power supply 11 is turned off to allow the inside of the boron nitride heating furnace 2 to naturally cool to room temperature, thereby obtaining a second coating gas chamber in which the reservoir effect has been suppressed.

[0094] 10) According to the different requirements for the working performance of the coating gas chamber in the future: if the atomic number density in the gas chamber needs to be stabilized, steps 11 and 12 are performed; if the gas exchange between the reservoir and the bubble 4 needs to be restored, steps 13 and 14 are performed.

[0095] 11) Repeat the coating air chamber placement and heating method of stage 1. The difference from stage 1 is that the air chamber tail 16 is not heated, so that the air chamber tail 16 is always maintained at room temperature. The fifth preset temperature is set for the multi-channel PID automatic control system 9: the air chamber body 4 (water temperature) is 47°C. During the heating process, since the capillary 5 at the connection has been blocked, the fluctuation of the temperature of the air chamber tail 16 will not affect the maintenance of the temperature of the air chamber body 4.

[0096] 12) When the temperature measured by the first waterproof thermistor probe 7 attached to the air chamber bubble 4 reaches the fifth preset temperature in step 11 for the first time, the temperature control maintenance stage is entered to maintain the current temperature of the distilled water 3 for 30 minutes, and then the first programmable AC power supply 11 is turned off to allow the inside of the boron nitride heating furnace 2 to naturally cool to room temperature. Steps 11 and 12 form a cycle, and a single cycle interval is 30 days.

[0097] 13) With the programmable AC power supplies 11, 14, and 18 disconnected, the distilled water 3 is emptied from the boron nitride heating furnace 2, and the bubble tail 16 of the film-coated air chamber to be treated is placed in the heating furnace 2 with the bubble tail 16 facing upward, and the bubble tail 16 of the air chamber is passed through and fixed through the cross rubber plug on the heat-insulating cover plate 19, and the second waterproof thermistor probe 20 is fitted and fixed on the capillary 5 at the connection of the film-coated air chamber, and the other end is connected to the temperature data acquisition system 8; and the sixth preset temperature is set for the multi-channel PID automatic control system 9: the temperature of the capillary 5 at the connection is 95°C, and the programmable AC power supply 18 locally heats the capillary 5 at the connection through the first detachable annular heating plate. In this step, the negative impact of the water bath heating scheme on other parts of the air chamber except the capillary 5 at the connection is eliminated.

[0098] 14) When the temperature measured by the second waterproof thermistor probe 20 attached to the capillary 5 at the connection reaches the sixth preset temperature in step 13 for the first time, the same current is maintained to continue heating for 1 hour, and then the programmable AC power supply 18 is turned off to allow the inside of the boron nitride heating furnace 2 to cool naturally to room temperature.

[0099] Among them, the second detachable annular heating plate 17 is a single-layer flexible PCB circuit board, which is close to the air chamber tail 16 during the heating process of stage one, the second waterproof thermistor probe 20 is fixed to the outside of the second detachable annular heating plate 17 by thermal conductive tape, and the first waterproof thermistor probe 7 enters the interior of the boron nitride heating furnace 2 through the cross rubber plug on the insulation cover 19 and is fixed to the inner wall of the bubble body 4 by thermal conductive tape. In stage two, when the air chamber tail 16 is inverted downward, the coated air chamber does not need additional physical support, and relying on its own gravity, the entire air chamber tail 16 and the capillary 5 at the connection can be immersed in the distilled water 3, and part of the air chamber bubble body 4 is also immersed in the distilled water.

[0100] In a preferred embodiment, the inhibitory effect of the reservoir effect of the coating gas chamber using the method and device provided by the present application is shown in Table 1. From the change in polarization life before and after capillary plugging in Table 1, it can be concluded that the present application can achieve effective inhibition of the reservoir effect and improve the ground state polarization life and anti-relaxation performance of the alkali metal atoms in the gas chamber.

[0101] Table 1

[0102]

[0103] The specific embodiments described above further describe the purpose, technical solutions and beneficial effects of the present application in detail. It should be understood that the above description is only a specific embodiment of the present application and is not intended to limit the scope of protection of the present application. It is particularly pointed out that for those skilled in the art, any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present application should be included in the scope of protection of the present application.

Claims

1. A method for inhibiting the gas chamber reservoir effect of alkali metal atoms in a film, characterized in that: include: The bubble tail and the bubble body of the first coating air chamber placed with the bubble tail facing upward are isolated and heated to a first preset temperature and a second preset temperature respectively, and the bubble tail and the bubble body are maintained at their respective corresponding preset temperatures within a first preset time, wherein the first preset temperature is greater than the second preset temperature; Heat the bubble tail of the first coating air chamber that is naturally cooled to room temperature and placed with the bubble tail facing downward to a third preset temperature, and maintain the bubble tail at the third preset temperature for a second preset time; Insulating and heating the bubble of the first coating air chamber that is naturally cooled to room temperature and placed with the bubble tail facing upward to a fourth preset temperature, and maintaining the bubble at the fourth preset temperature for a third preset time; When the bubble is naturally cooled to room temperature, a second coating air chamber in which the reservoir effect has been suppressed is obtained.

2. A method for suppressing the gas chamber reservoir effect of alkali metal atoms in film coating as claimed in claim 1, characterized in that: The steps of heating the bubble isolation to the second preset temperature, heating the bubble tail to the third preset temperature, and heating the bubble isolation to the fourth preset temperature are all performed by water bath heating; During the water bath heating process, the capillary at the connection between the bubble body and the bubble tail of the first coating air chamber is always immersed in the distilled water used for water bath heating.

3. A method for suppressing the gas chamber reservoir effect of alkali metal atoms in film coating as claimed in claim 1, characterized in that: The first coating air chamber is a coating air chamber in which the coating material is over-evaporated.

4. A method for suppressing the gas chamber reservoir effect of alkali metal atoms in a film coating as claimed in claim 1, characterized in that: The method further includes stabilizing the atomic number density of the second coating gas chamber, including: The second coating air chamber is subjected to several heating and cooling operations to obtain a corresponding stable coating air chamber, wherein the interval between each heating and cooling operation is a fourth preset time, and each heating and cooling operation is specifically: The bubble body of the second coating air chamber is placed with the bubble tail facing upward and is isolated and heated to a fifth preset temperature, and the bubble body is maintained at the fifth preset temperature for a fifth preset time.

5. A method for suppressing the gas chamber reservoir effect of alkali metal atoms in film coating as claimed in claim 4, characterized in that: The fourth preset time and the fifth preset time are determined according to the atomic number density and the ground state polarization lifetime of the second coating gas chamber.

6. A method for suppressing the gas chamber reservoir effect of alkali metal atoms in film coating as claimed in claim 1, characterized in that: The method further includes restoring the second film-depositing air chamber to the first film-depositing air chamber, including: heating the capillary at the connection between the bubble body and the bubble tail of the second coating air chamber placed in a manner that the bubble tail faces upward to a sixth preset temperature; When the capillary tube reaches the sixth preset temperature, continue to heat the capillary tube within a sixth preset time; When the foam body is naturally cooled to room temperature, the first coating air chamber reduced by the second coating air chamber is obtained.

7. A device for suppressing the gas chamber reservoir effect of alkali metal atoms in film coating, characterized in that: The device is used to implement any one of the methods for suppressing the gas chamber reservoir effect of the coated alkali metal atoms as described in claims 1-6, and the device comprises a heating furnace, a heating module and a temperature control module; The heating furnace comprises a container and a heat-insulating cover plate, wherein the container is used to load the first coating air chamber for heating, and the heat-insulating cover plate is used to isolate the bubble tail and bubble body of the first coating air chamber during the heating process; The outside of the heating furnace is connected to the heating module, and the heating module includes a high-temperature resistant heating belt, two annular heating plates, three programmable AC power supplies and two normally-off relays, wherein the high-temperature resistant heating belt is wrapped around the surface of the container, and is connected to the first programmable AC power supply through the first normally-off relay, and is used to heat the container, the first annular heating plate is located above the thermal insulation cover plate, and is connected to the second programmable AC power supply through the second normally-off relay, and is used to heat the bubble tail passing through the thermal insulation cover plate, the second annular heating plate is wrapped around the capillary at the connection between the bubble body and the bubble tail of the first coating air chamber, and is connected to the third programmable AC power supply, and is used to continuously heat the capillary; The temperature control module includes two thermistor probes, a temperature data acquisition system and a multi-channel PID automatic control system, wherein the two thermistor probes are connected to the input end of the temperature data acquisition system for acquiring temperature data of a preset position, and the multi-channel PID automatic control system is respectively connected to the output end of the temperature data acquisition system and two normally-off relays for controlling the on and off of the two normally-off relays through temperature data, thereby controlling the heating temperature of the high-temperature resistant heating belt and the first annular heating plate.

8. A device for suppressing the gas chamber reservoir effect of alkali metal atoms in film coating as claimed in claim 7, characterized in that: The thermal insulation cover plate is provided with a through hole of a preset diameter and is embedded with a matching cross rubber plug. When the first coated air chamber is placed with the bubble tail facing upward, the bubble tail can pass through the cross rubber plug and be fixed at any preset height.

9. The device for suppressing the gas chamber reservoir effect of the alkali metal atoms in the film coating as claimed in claim 7, characterized in that: The multi-channel PID automatic control system includes an input differential module and a dual-channel temperature feedback module, wherein the input differential module is used to differentiate the temperature data of two inputs to obtain the temperature difference between the two temperature data, and the dual-channel temperature feedback module is used to compare the temperature data of the two inputs with the corresponding preset temperatures respectively, thereby controlling the on and off of the two normally-off relays.

10. The device for suppressing the gas chamber reservoir effect of the alkali metal atoms in the film coating as claimed in claim 7, characterized in that: The length of the second annular heating plate is smaller than the length of the capillary tube, and asbestos heat insulation material is provided between the second annular heating plate and the foam body.

Citation Information

Patent Citations

  • Manufacturing method for mini quartz glass atomic gas chamber

    CN107311103A

  • Preparation method of all-glass alkali metal atom air chamber

    CN110015636A

  • Coating alkali metal atom gas chamber curing system and using method for prolonging atom spin relaxation life

    CN110274472A

  • Apparatus and method for increasing spin relaxation times for alkali atoms in alkali vapor cells

    US20120112749A1