HEMT (High Electron Mobility Transistor) device structure for developing gallium nitride switch and power amplifier and preparation method

By adopting a multi-channel structure and groove design in gallium nitride HEMT devices, the problems of low current density and poor voltage withstand performance of the device are solved, the current density improvement and voltage withstand performance are achieved, and the RF switch and power amplifier are promoted. The output power is increased.

CN118969834APending Publication Date: 2024-11-15THE 13TH RES INST OF CHINA ELECTRONICS TECH GRP CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411089232.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-09
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

GaN HEMT devices have low current density, high on-resistance and poor withstand voltage performance, which limit the output power improvement space of RF switches and power amplifiers.

Method used

By adopting a multi-channel structure and groove design, by forming the first and second grooves in the combined layer and setting the gate in the first groove, one side of the gate is perpendicular to the same side of the second groove. , reduce the channel resistance between the gate source and gate drain, enhance the gate control capability of the device, and reduce the peak electric field.

Benefits of technology

It significantly improves the current density of the device, reduces the on-resistance, improves the voltage withstand performance, and improves the output power and withstand power of the GaN RF switch and power amplifier.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118969834A_ABST
    Figure CN118969834A_ABST
Patent Text Reader

Abstract

The invention provides an HEMT (High Electron Mobility Transistor) device for developing a gallium nitride switch and a power amplifier and a preparation method. The HEMT device comprises a substrate, a buffer layer, a plurality of combination layers, a source electrode, a drain electrode, a drain electrode and a passivation layer, a first groove and a second groove are formed in the multiple combined layers; the first groove is arranged from the bottom barrier layer to the top barrier layer in the plurality of combination layers; the second groove extends downwards into the barrier layer at the bottommost layer in the combined layer at the bottom of one side, close to the drain electrode, of the first groove; and the grid electrode is arranged in the first groove, the top surface of the grid electrode is higher than the upper part of the barrier layer at the topmost layer in the plurality of combination layers, one side of the grid electrode is attached to one side of the first groove close to the source electrode, and the other side of the grid electrode and one side of the second groove close to the source electrode are on the same vertical line. The current density of the HEMT device can be improved, the on resistance of the device can be reduced, and the voltage resistance of the HEMT device can be improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of semiconductor device manufacturing, and in particular to a HEMT device structure and a preparation method for developing a gallium nitride switch and a power amplifier. Background Art

[0002] Gallium nitride (GaN) RF power devices have advantages such as larger bandgap, higher breakdown field strength, higher electron saturation drift velocity and higher thermal conductivity. Compared with first-generation silicon and second-generation gallium arsenide, gallium nitride (GaN) RF power devices have greater output power, higher efficiency and smaller size. They have been widely used in many fields such as 5G communications and have demonstrated great advantages. RF switches and power amplifiers are typical representatives of gallium nitride RF power devices. The withstand power of gallium nitride RF switches and the output power of power amplifiers are still far from the theoretical predictions of materials, and there is still room for substantial improvement. It is of great significance to adopt new structures, new processes and new technologies to further improve the withstand power of gallium nitride RF switches and the output power of power amplifiers.

[0003] Increasing the concentration of two-dimensional electron gas in the channel of GaN heterojunction materials can increase the device current density and reduce the device channel on-resistance, which is beneficial to improving the withstand power of GaN RF switches and the output power of power amplifiers. However, after the concentration of two-dimensional electron gas increases, the gate control ability of the device becomes weaker, affecting the withstand voltage characteristics of the device. Therefore, the effect of two-dimensional electron gas concentration on the device current density and breakdown voltage is contradictory and needs to be considered comprehensively. In addition, there is an extremely strong spike electric field in the channel on the side of the gate-biased drain electrode of GaN-based HEMT devices, which is the main reason for the breakdown of the device. At present, gate field plates or source field plates are generally used to suppress the spike electric field.

[0004] In order to further improve the withstand power of GaN RF switches and the output power of power amplifiers, a device structure and preparation technology for developing GaN switches and power amplifiers is proposed, which can improve the device current density and reduce the device on-resistance. Summary of the invention

[0005] The present invention provides a HEMT device and a preparation method for developing a gallium nitride switch and a power amplifier, so as to solve the problems of low current density, high on-resistance and poor withstand voltage performance of HEMT devices in the prior art.

[0006] In a first aspect, the present invention provides a HEMT device for developing a gallium nitride switch and a power amplifier, comprising: a substrate;

[0007] A buffer layer is disposed above the substrate;

[0008] A plurality of combined layers are stacked on the buffer layer, each of the combined layers comprising a GaN channel layer and a barrier layer located above the GaN channel layer;

[0009] A source electrode is disposed above a topmost barrier layer among the plurality of combined layers;

[0010] A drain electrode is disposed above a top barrier layer among the plurality of combined layers;

[0011] A first groove and a second groove are provided inside the plurality of combined layers;

[0012] The first groove is disposed from above the bottom barrier layer among the plurality of combined layers to above the top barrier layer among the plurality of combined layers;

[0013] The second groove extends downward from the bottom of the first groove on the side close to the drain electrode to the bottommost barrier layer among the multiple combined layers;

[0014] A gate is disposed in the first groove, and its top surface is higher than the topmost barrier layer in the plurality of combined layers, one side of the gate is attached to one side of the first groove close to the source, and the other side of the gate is on the same vertical line as one side of the second groove close to the source;

[0015] The passivation layer covers the source electrode, the drain electrode, the gate electrode, the second groove, and the region not blocked by the topmost barrier layer in the plurality of combined layers.

[0016] In a possible implementation, the thickness of the GaN channel layer of each combined layer in the plurality of combined layers is the same;

[0017] The thickness of the barrier layer of each combined layer in the plurality of combined layers is the same;

[0018] The GaN channel layer of each of the plurality of combined layers has the same material;

[0019] The material of the barrier layer of each of the plurality of combined layers is the same.

[0020] In a possible implementation manner, the material of the barrier layer includes AlGaN, InAlN, AlN or InAlN.

[0021] In a possible implementation, the gate is made of Ni / Au metal or Pt / Au metal.

[0022] In a possible implementation, the material of the substrate includes silicon carbide SiC or aluminum nitride AlN.

[0023] In a possible implementation, the material of the buffer layer includes gallium nitride or AlGaN.

[0024] In a second aspect, the present invention provides a HEMT device for developing a gallium nitride switch and a power amplifier, comprising:

[0025] substrate;

[0026] A buffer layer is disposed above the substrate;

[0027] A plurality of combined layers are stacked on the buffer layer, each of the combined layers comprising a GaN channel layer and a barrier layer located above the GaN channel layer;

[0028] A source electrode is disposed above a topmost barrier layer among the plurality of combined layers;

[0029] A drain electrode is disposed above a top barrier layer among the plurality of combined layers;

[0030] A third groove is provided from above the bottom barrier layer among the plurality of combined layers to above the top barrier layer among the plurality of combined layers;

[0031] A gate is disposed in the third groove, and a top surface thereof is higher than a topmost barrier layer in the plurality of combined layers, one side of the gate is attached to a side of the first groove close to the source, and a gap exists between the other side of the gate and the other side of the third groove;

[0032] Ion implantation is arranged in the barrier layer below the side of the third groove close to the drain electrode, and the width of the ion implantation area is the same as the width of the interval;

[0033] The passivation layer covers the source electrode, the drain electrode, the gate electrode, the third groove, and the area not blocked by the topmost barrier layer in the plurality of combined layers.

[0034] In a third aspect, the present invention provides a HEMT device for developing a gallium nitride switch and a power amplifier and a preparation method thereof, the method being used to prepare a HEMT device for developing a gallium nitride switch and a power amplifier provided in the first aspect, comprising:

[0035] Selecting a substrate;

[0036] growing a buffer layer on the substrate;

[0037] sequentially growing a plurality of combined layers on the buffer layer;

[0038] Prepare source and drain electrodes on both sides above the top barrier layer of the plurality of combined layers;

[0039] Etching a region from above the bottom barrier layer in the plurality of combined layers to above the top barrier layer in the plurality of combined layers to form a first groove;

[0040] Etching the barrier layer at the bottom of the first groove near the drain electrode to the inside of the barrier layer to form a second groove;

[0041] A gate is prepared, wherein the top surface of the gate is higher than the topmost barrier layer in the plurality of combined layers, one side of the gate is attached to one side of the first groove close to the source electrode, and the other side of the gate is in the same vertical line as one side of the second groove close to the source electrode;

[0042] A passivation layer is grown on the source, the drain, the gate, the second recess, and the region where the topmost barrier layer in the plurality of combined layers is not blocked.

[0043] In a fourth aspect, the present invention provides a HEMT device for manufacturing a gallium nitride switch and a power amplifier and a preparation method thereof, wherein the method is used to prepare a HEMT device for manufacturing a gallium nitride switch and a power amplifier provided in the second aspect, comprising:

[0044] Selecting a substrate;

[0045] growing a buffer layer on the substrate;

[0046] sequentially growing a plurality of combined layers on the buffer layer;

[0047] Prepare source and drain electrodes on both sides above the top barrier layer of the plurality of combined layers;

[0048] Etching a region from above the bottom barrier layer in the plurality of combined layers to above the top barrier layer in the plurality of combined layers to form a third groove;

[0049] Performing ion implantation on the barrier layer below the side of the third groove close to the drain electrode, wherein the width of the ion implantation area is the same as the width of the spacer;

[0050] A gate is prepared in the third groove, wherein the top surface of the gate is higher than the topmost barrier layer in the plurality of combined layers, one side of the gate is attached to one side of the third groove close to the source, and there is a gap between the other side of the gate and the other side of the third groove;

[0051] A passivation layer is grown on the source, the drain, the gate, the second recess, and the region where the topmost barrier layer in the plurality of combined layers is not blocked.

[0052] In a possible implementation, the ions implanted are fluorine ions or magnesium ions.

[0053] The present invention provides a HEMT device and a preparation method for developing a gallium nitride switch and a power amplifier, wherein the HEMT device comprises a substrate, a buffer layer, a plurality of combined layers, a source electrode, a drain electrode, a drain electrode and a passivation layer; a first groove and a second groove are provided inside the plurality of combined layers; the first groove is provided above the bottommost barrier layer in the plurality of combined layers to above the topmost barrier layer in the plurality of combined layers; the second groove extends downward from the bottom of the first groove near the drain electrode to the inside of the bottommost barrier layer in the combined layers; a gate electrode is provided in the first groove, and the top surface is higher than the topmost barrier layer in the plurality of combined layers, one side of the gate electrode is attached to one side of the first groove near the source electrode, and the other side of the gate electrode is on the same vertical line as one side of the second groove near the source electrode. The present invention can significantly reduce the channel resistance between the gate source electrode and the gate drain electrode, and improve the current density of the device by preparing a multi-channel structure, and enhance the gate control capability of the device by providing the groove, so the present invention can improve the current density of the HEMT device, reduce the on-resistance of the device, and improve the withstand voltage performance of the HEMT device. BRIEF DESCRIPTION OF THE DRAWINGS

[0054] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings in the following description are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.

[0055] Figure 1A It is a schematic diagram of the structure of a traditional single-channel HEMT device;

[0056] Figure 1B It is a schematic diagram of the structure of a conventional multi-channel HEMT device;

[0057] Figure 1C It is a schematic diagram of the structure of a conventional multi-channel combined recessed gate structure HEMT device;

[0058] Figure 2 It is a structural schematic diagram of a HEMT device for developing a gallium nitride switch and a power amplifier provided by an embodiment of the present invention;

[0059] Figure 3 It is a schematic structural diagram of a HEMT device for developing a gallium nitride switch and a power amplifier provided by another embodiment of the present invention;

[0060] Figure 4A-4G The preparation provided by the embodiment of the present invention Figure 2 A schematic flow chart of a method for preparing a HEMT device;

[0061] Figure 5A-5G The preparation provided by the embodiment of the present invention Figure 3 Schematic diagram of the process for preparing a HEMT device. DETAILED DESCRIPTION

[0062] In order to enable people in the technical field to better understand the present solution, the technical solution in the embodiment of the present solution will be clearly described below in conjunction with the drawings in the embodiment of the present solution. Obviously, the described embodiment is an embodiment of a part of the present solution, not all of the embodiments. Based on the embodiments in the present solution, all other embodiments obtained by ordinary technicians in the field without creative work should fall within the scope of protection of the present solution.

[0063] The term "including" and any other variations in the specification and claims of this solution and the above drawings mean "including but not limited to", and is intended to cover non-exclusive inclusions and is not limited to the examples listed in the text. In addition, the terms "first" and "second" are used to distinguish different objects, not to describe a specific order.

[0064] The following is a detailed description of the implementation of the present invention in conjunction with the specific drawings:

[0065] In order to facilitate understanding of the technical solutions in the embodiments of the present application, some of the terms involved in the embodiments of the present application are first explained below:

[0066] High electron mobility transistor (HEMT), also known as modulation-doped FET (MODFET), is a type of field effect transistor that uses two materials with different energy gaps to form a heterojunction to provide a channel for carriers, unlike metal oxide semiconductor field effect transistors, which directly use doped semiconductors instead of junctions to form a conductive channel. Gallium arsenide and gallium arsenide aluminum ternary compound semiconductors are optional materials for this device. Of course, there can be many other combinations depending on the specific application. For example, indium-containing devices generally show better high-frequency performance, while gallium nitride (GaN) high electron mobility transistors developed in recent years have attracted a lot of attention due to their good high-frequency characteristics. High electron mobility transistors can operate at extremely high frequencies, so they are widely used in mobile phones, satellite TV and radars. RF switches and power amplifiers are typical representatives of gallium nitride RF power devices.

[0067] The heterojunction of a semiconductor is a special PN junction, which is formed by depositing two or more thin films of different semiconductor materials on the same substrate in sequence. These materials have different energy band gaps and can be compounds such as gallium arsenide or semiconductor alloys such as silicon-germanium.

[0068] The diode characteristics of semiconductor heterostructures are very close to ideal diodes. In addition, by adjusting the thickness and band gap of each semiconductor material layer, the response parameters of the diode current and voltage can be changed. Semiconductor heterostructures have a significant impact on semiconductor technology and are key components of high-frequency transistors and optoelectronic devices.

[0069] In the drawings of the present invention, S represents a source, G represents a gate, and D represents a drain.

[0070] Figure 1A A schematic diagram of the structure of a conventional single-channel HEMT device provided by an embodiment of the present invention. Figure 1A The structure includes: a substrate, a buffer layer, a GaN channel layer, a barrier layer, a source electrode, a gate electrode, a drain electrode and a passivation layer.

[0071] exist Figure 1A In the present invention, the HEMT device adopts a traditional single-channel structure, in which the channel resistance between the gate source and the gate drain is high, which is not conducive to improving the power characteristics of the GaN RF switch and the power amplifier.

[0072] Figure 1B A schematic diagram of the structure of a conventional multi-channel HEMT device provided by an embodiment of the present invention. Figure 1B The structure includes: a substrate, a buffer layer, a stacked layer of three GaN channel layers and a barrier layer, a source electrode, a gate electrode, a drain electrode, and a passivation layer.

[0073] exist Figure 1B In this device, a multi-channel structure is used. Figure 1A Compared with the traditional single-channel structure, the channel resistance between the gate source and the gate drain is reduced, but this method cannot further enhance the gate control capability of the device, that is, the control ability of the gate metal over the channel electrons.

[0074] Figure 1C A schematic diagram of a conventional multi-channel recessed gate HEMT device provided by an embodiment of the present invention. Figure 1C The structure includes: a substrate, a buffer layer, a combination layer of three GaN channel layers and barrier layers, a source electrode, a groove, a drain electrode and a passivation layer, and a gate electrode is combined with the groove.

[0075] exist Figure 1B The HEMT device adopts a multi-channel combined with a recessed gate structure. Figure 1B Compared with the traditional multi-channel structure, the gate control capability of the device is improved, but it cannot reduce the electron concentration in the channel on the side of the drain electrode. The high electron concentration will form an extremely strong peak electric field, causing the device to break down.

[0076] However, this method cannot further enhance the gate control capability of the device, that is, the ability of the gate metal to control channel electrons.

[0077] Based on the above, the present invention provides a HEMT device for developing a GaN switch and a power amplifier, which can reduce the channel resistance between the gate source and the gate drain, improve the power characteristics of the GaN RF switch and the power amplifier, enhance the gate control capability of the device, and improve the withstand voltage characteristics of the device. For details, see Figure 2 .

[0078] like Figure 2 As shown, a HEMT device for developing a gallium nitride switch and a power amplifier provided by an embodiment of the present invention includes:

[0079] Substrate 21;

[0080] A buffer layer 22 is disposed above the substrate 21;

[0081] A plurality of combined layers 24 are stacked on the buffer layer 22, each of the combined layers comprising a GaN channel layer and a barrier layer located above the GaN channel layer;

[0082] A source electrode 25 is disposed above the topmost barrier layer among the plurality of combined layers 24;

[0083] A drain electrode 26 is disposed above the top barrier layer among the plurality of combined layers 24;

[0084] The plurality of combined layers 24 are provided with a first groove 27 and a second groove 28 inside;

[0085] The first groove 27 is disposed above the bottom barrier layer among the plurality of combined layers 24 to above the top barrier layer among the plurality of combined layers 24;

[0086] The second groove 28 extends downward from the bottom of the first groove 27 on the side close to the drain 26 to the bottommost barrier layer among the plurality of combined layers 24 ;

[0087] The gate 29 is disposed in the first groove 27, and the top surface thereof is higher than the topmost barrier layer in the plurality of combined layers 24, one side of the gate 29 is attached to one side of the first groove 27 close to the source 25, and the other side of the gate 29 is on the same vertical line as one side of the second groove 28 close to the source 25;

[0088] The passivation layer 20 covers the source 25 , the drain 26 , the gate 27 , the second groove 28 , and the region of the topmost barrier layer in the plurality of combined layers 24 that is not blocked.

[0089] Exemplarily, the number of layers of the combined layer in this embodiment is selected to be three layers, that is, a combined layer of three GaN channel layers and a barrier layer located above the GaN channel layer is stacked above the buffer layer in this embodiment, such as Figure 2 As shown, the combined layer 241 is one of the multiple combined layers 24 .

[0090] In a possible implementation, the material of the substrate 21 may be silicon carbide SiC, silicon Si, aluminum nitride AlN, sapphire, etc., which is not limited here.

[0091] In a possible implementation, the material of the buffer layer 22 may be gallium nitride or AlGaN, etc., which is not limited here.

[0092] In a possible implementation, the thickness of the GaN channel layer of each combination layer in the plurality of combination layers 24 is the same. Exemplarily, the thickness of the GaN channel layer can be selected to be 10 nm ≤ the thickness of the GaN channel layer ≤ 150 nm, which is not limited here.

[0093] In a possible implementation, the barrier layer of each combination layer in the plurality of combination layers 24 has the same thickness. Exemplarily, the thickness of the barrier layer can be selected to be 2 nm ≤ the thickness of the barrier layer ≤ 30 nm, which is not limited here.

[0094] In a possible implementation, the material of the GaN channel layer of each combination layer in the plurality of combination layers 24 is the same.

[0095] In a possible implementation, the barrier layer of each combination layer in the plurality of combination layers 24 is made of the same material. For example, AlGaN, InAlN, AlN, InAlGaN and the like can be selected, which is not limited here.

[0096] In one possible implementation, Figure 2 The HEMT device shown further includes an active region 23 disposed between the buffer layer 22 and the bottommost GaN channel layer of the plurality of combined layers 24 .

[0097] Based on the above, the HEMT device for developing a gallium nitride switch and a power amplifier provided in this embodiment adopts a gallium nitride heterojunction multi-channel structure, which can greatly reduce the channel resistance between the gate 29 source 26 and the gate 29 drain 26, and improve the device current density, which is beneficial to improve the power characteristics of the gallium nitride radio frequency switch and the power amplifier. Compared with the traditional multi-channel combined with a recessed gate structure, the present application etches a second groove 28 in the channel on the side of the gate 29 biased towards the drain 26, reduces the electron concentration in this area, reduces the peak electric field strength in this area, and improves the device withstand voltage characteristics.

[0098] like Figure 3 FIG. 1 is a schematic diagram of a HEMT device for developing a gallium nitride switch and a power amplifier according to another embodiment of the present invention, comprising:

[0099] Substrate 31;

[0100] A buffer layer 32 is disposed above the substrate 31;

[0101] A plurality of combined layers 34 are stacked on the buffer layer 32, each of the combined layers comprising a GaN channel layer and a barrier layer located above the GaN channel layer;

[0102] A source electrode 35 is disposed above the topmost barrier layer among the plurality of combined layers 34;

[0103] A drain electrode 36 is disposed above the top barrier layer among the plurality of combined layers 34;

[0104] The third groove 37 is provided from above the bottom barrier layer among the plurality of combined layers 34 to above the top barrier layer among the plurality of combined layers 34;

[0105] A gate 38 is disposed in the third groove 37, and the top surface of the gate is higher than the topmost barrier layer in the plurality of combined layers 34, one side of the gate is attached to the side of the third groove 37 close to the source, and there is a gap between the other side of the gate 38 and the other side of the third groove 37;

[0106] An ion implantation is performed on the barrier layer below one side of the third groove 37 close to the drain 36, and the width of the ion implantation area is the same as the width of the interval;

[0107] The passivation layer 39 covers the source 35 , the drain 36 , the gate 38 , the third groove 37 , and the region where the topmost barrier layer in the plurality of combined layers 34 is not blocked.

[0108] In a possible implementation, the ions implanted are fluorine ions or magnesium ions.

[0109] Exemplarily, the number of layers of the combined layer in this embodiment is selected to be three layers, that is, a combined layer of three GaN channel layers and a barrier layer located above the GaN channel layer is stacked above the buffer layer in this embodiment, such as Figure 3 As shown, the combined layer 341 is one of the multiple combined layers 34 .

[0110] In a possible implementation, the material of the substrate 31 may be silicon carbide SiC, silicon Si, aluminum nitride AlN, sapphire, etc., which is not limited here.

[0111] In a possible implementation, the material of the buffer layer 32 may be gallium nitride or AlGaN, etc., which is not limited here.

[0112] In a possible implementation, the thickness of the GaN channel layer of each combination layer in the plurality of combination layers 34 is the same. Exemplarily, the thickness of the GaN channel layer can be selected to be 10 nm ≤ the thickness of the GaN channel layer ≤ 150 nm, which is not limited here.

[0113] In a possible implementation, the barrier layer of each combination layer in the plurality of combination layers 34 has the same thickness. Exemplarily, the thickness of the barrier layer can be selected to be 2 nm ≤ the thickness of the barrier layer ≤ 30 nm, which is not limited here.

[0114] In a possible implementation, the material of the GaN channel layer of each combination layer in the plurality of combination layers 34 is the same.

[0115] In a possible implementation, the barrier layer of each combination layer in the plurality of combination layers 34 is made of the same material. For example, materials such as AlGaN or InAlN or AlN or InAlGaN may be selected, which are not limited here.

[0116] In one possible implementation, Figure 3 The HEMT device shown further includes an active region 33 disposed between the buffer layer 32 and the bottommost GaN channel layer among the plurality of combined layers 34 .

[0117] Compared with the traditional multi-channel combined recessed gate structure, the present application performs ion implantation in the channel on the side of the gate 38 biased towards the drain 36 to reduce the electron concentration in this area, reduce the peak electric field strength in this area, and improve the device's withstand voltage characteristics.

[0118] The present application also provides a method for preparing a HEMT device for manufacturing a gallium nitride switch and a power amplifier. Before introducing the above method, some of the terms involved in the method of the present application are first explained:

[0119] Etching is the process of selectively removing unwanted materials from the surface of silicon wafers by chemical or physical methods. Its basic goal is to correctly replicate the mask pattern on the silicon wafer coated with glue. With the development of micro-manufacturing technology, etching has become a general term for stripping and removing materials by solution, reactive ions or other mechanical methods, and has become a universal term for micro-manufacturing.

[0120] Ion implantation refers to the phenomenon that when a beam of ions in a vacuum is shot at a solid material, the ion beam knocks the atoms or molecules of the solid material out of the surface of the solid material. This phenomenon is called sputtering. When the ion beam hits the solid material, it bounces back from the surface of the solid material or passes through the solid material. These phenomena are called scattering. Another phenomenon is that after the ion beam hits the solid material, it is resisted by the solid material and its speed slowly decreases, and finally it stays in the solid material. This phenomenon is called ion implantation.

[0121] Ohmic contact, that is, when metal contacts semiconductor, non-rectifying contact can be formed. When semiconductor contacts metal, a barrier layer is often formed. However, when the semiconductor doping concentration is very high, electrons can pass through the barrier by tunneling, thus forming a low-resistance ohmic contact. Ohmic contact is very important for semiconductor devices. The formation of a good ohmic contact is conducive to the input and output of current. Different alloys with different formulations are often selected as ohmic contact materials for different semiconductor materials. Ohmic contact is widely used in metal processing. The main measures to achieve it are high doping in the semiconductor surface layer or the introduction of a large number of recombination centers.

[0122] Metal-Organic Chemical Vapour Deposition (MOCVD) is a technology for growing semiconductor thin films on substrates. Using MOCVD technology, many nanolayers can be deposited with extremely high precision, each with a controllable thickness, to form materials with specific optical and electrical properties. MOCVD is a key process technology used in the manufacture of LED chips and power devices.

[0123] Molecular beam epitaxy (MBE) is a newly developed epitaxial film-making method and also a special vacuum coating process. Epitaxy is a new technology for preparing single crystal thin films. It is a method of growing thin films layer by layer along the crystal axis of the substrate material under appropriate substrate and suitable conditions. The advantages of this technology are: the substrate temperature used is low, the film growth rate is slow, the beam intensity is easy to accurately control, and the film composition and doping concentration can be quickly adjusted with the change of the source. This technology has been used to prepare single crystal films as thin as dozens of atomic layers, as well as ultra-thin layer quantum microstructure materials formed by alternating the growth of films with different components and different doping.

[0124] The following is an introduction to the preparation method of HEMT devices used to develop gallium nitride switches and power amplifiers.

[0125] FIG. 4A to FIG. 4G The preparation provided by the embodiment of the present invention Figure 2 The schematic diagram of the process flow of the HEMT device shown in FIG. 1 includes:

[0126] S401, first select a substrate 21.

[0127] For example, the material of the substrate 21 may be silicon carbide SiC, silicon Si, aluminum nitride AlN, sapphire, or the like.

[0128] S402 , growing a buffer layer 22 on the substrate 21 by using MOCVD or MBE equipment.

[0129] For example, the material of the buffer layer 22 may be gallium nitride or AlGaN.

[0130] S403 , a plurality of composite layers 24 are sequentially grown on the buffer layer 22 using MOCVD or MBE equipment.

[0131] Exemplarily, the thickness of the GaN channel layer can be selected to be between 10nm≤GaN channel layer thickness≤150nm, and the thickness of the barrier layer can be selected to be between 2nm≤barrier layer thickness≤30nm, and the material of the GaN channel layer of each combination layer in the multiple combination layers 24 is the same.

[0132] After completing step S401 to step S403, the current structure of the HEMT is as follows: Figure 4A As shown, Figure 4A The preparation provided by the embodiment of the present invention Figure 2 A schematic diagram of a process of manufacturing a substrate 21, a buffer layer 22 and a plurality of combination layers 24 of a HEMT device.

[0133] S404, using dry etching or ion implantation to isolate the active region 23 of the HEMT device, such as Figure 4B As shown, Figure 4B The preparation provided by the embodiment of the present invention Figure 2 A schematic flow chart of a method for preparing an active region 23 of a HEMT device.

[0134] S405, preparing a source electrode 25 and a drain electrode 26 on both sides above the topmost barrier layer of the plurality of combined layers 24, such as Figure 4C As shown, Figure 4C The preparation provided by the embodiment of the present invention Figure 2 A schematic flow chart of a method for preparing a source 25 and a drain 26 of a HEMT device.

[0135] Exemplarily, this step may adopt a high temperature alloy process or a regrowth process.

[0136] S406, etching the area above the bottom barrier layer in the plurality of combined layers 24 to the area above the top barrier layer in the plurality of combined layers 24 to form a first groove 27, such as Figure 4D As shown, Figure 4D The preparation provided by the embodiment of the present invention Figure 2 A schematic flow chart of a method for preparing the first groove 27 of a HEMT device.

[0137] S407, etching the barrier layer at the bottom of the first groove 27 near the drain 26 to the inside of the barrier layer to form a second groove 28, such as Figure 4E As shown, Figure 4E The preparation provided by the embodiment of the present invention Figure 2A schematic flow chart of a method for preparing the second groove 28 of a HEMT device.

[0138] S408, prepare a gate 29, the top surface of the gate 29 is higher than the topmost barrier layer in the plurality of combined layers 24, one side of the gate 29 is attached to one side of the first groove 27 close to the source 25, and the other side of the gate 29 is on the same vertical line as one side of the second groove 28 close to the source 26, such as Figure 4F As shown, Figure 4F The preparation provided by the embodiment of the present invention Figure 2 A schematic flow chart of a method for preparing a gate 29 of a HEMT device.

[0139] For example, the gate metal may be Ni / Au metal or Pt / Au metal.

[0140] S409, growing a passivation layer 20 on the source 25, the drain 26, the gate 29, the second groove 28 and the region where the topmost barrier layer in the plurality of combined layers 24 is not blocked, such as Figure 4G As shown, Figure 4G The preparation provided by the embodiment of the present invention Figure 2 A schematic flow chart of a method for preparing a passivation layer 20 of a HEMT device.

[0141] For example, the material of the passivation layer 20 may be SiN or SiO 2 .

[0142] Based on the above, this embodiment adopts dry etching to form the second groove 28, which reduces the electron concentration in this area, reduces the peak electric field intensity in this area, and improves the withstand voltage characteristics of the device.

[0143] Figure 5A-5G The preparation provided by the embodiment of the present invention Figure 3 A schematic flow chart of a method for preparing a HEMT device is provided, wherein the method comprises:

[0144] S501, first select a substrate 31.

[0145] For example, the material of the substrate 31 may be silicon carbide SiC, silicon Si, aluminum nitride AlN, sapphire, or the like.

[0146] S502 , growing a buffer layer 32 on the substrate 31 by using MOCVD or MBE equipment.

[0147] For example, the material of the buffer layer 32 may be gallium nitride or AlGaN.

[0148] S503 , a plurality of composite layers 34 are sequentially grown on the buffer layer 32 using MOCVD or MBE equipment.

[0149] Exemplarily, the thickness of the GaN channel layer can be selected to be between 10nm≤GaN channel layer thickness≤150nm, and the thickness of the barrier layer can be selected to be between 2nm≤barrier layer thickness≤30nm, and the material of the GaN channel layer of each combination layer in the multiple combination layers 34 is the same.

[0150] After completing step S501 to step S503, the current structure of the HEMT is as follows: Figure 5A As shown, Figure 5A The preparation provided by the embodiment of the present invention Figure 3 A schematic flow chart of a method for preparing a substrate 31, a buffer layer 32 and a plurality of combined layers 34 of a HEMT device.

[0151] S504, using dry etching or ion implantation to isolate the active region 33 of the HEMT device, such as Figure 5B As shown, Figure 5B The preparation provided by the embodiment of the present invention Figure 3 A schematic flow chart of a method for preparing an active region 33 of a HEMT device.

[0152] S505, preparing a source electrode 35 and a drain electrode 36 on both sides above the topmost barrier layer of the plurality of combined layers 34, such as Figure 5C As shown, Figure 5C The preparation provided by the embodiment of the present invention Figure 3 A schematic flow chart of a method for preparing a source 35 and a drain 36 of a HEMT device.

[0153] Exemplarily, this step may adopt a high temperature alloy process or a regrowth process.

[0154] S506, etching the area above the bottom barrier layer in the plurality of combined layers 34 to the area above the top barrier layer in the plurality of combined layers 34 to form a third groove 37, such as Figure 5D As shown, Figure 5D The preparation provided by the embodiment of the present invention Figure 3 A schematic flow chart of a method for preparing the third groove 37 of the HEMT device.

[0155] S507, ion implantation is performed on the barrier layer below the side of the third groove 37 close to the drain 36, and the width of the ion implantation area is the same as the width of the interval, such as Figure 5E As shown, Figure 5E The preparation provided by the embodiment of the present invention Figure 3 Schematic diagram of the process flow of the ion implantation preparation method of the HEMT device, where the interval refers to the interval of "there is a interval between the other side of the gate and the other side of the third groove" in step S508.

[0156] S508, a gate 38 is formed in the third groove 37, the top surface of the gate 38 is higher than the topmost barrier layer in the plurality of combined layers, one side of the gate 38 is attached to the side of the third groove 37 close to the source 35, and there is a gap between the other side of the gate 38 and the other side of the third groove 37. Fig. 5F As shown, Fig. 5F The preparation provided by the embodiment of the present invention Figure 3 A schematic flow chart of a method for preparing a gate 38 of a HEMT device.

[0157] For example, the gate metal may be Ni / Au metal or Pt / Au metal.

[0158] S509, growing a passivation layer 39 on the source 35, the drain 36, the gate 37, the third groove 37 and the region where the topmost barrier layer in the plurality of combined layers is not blocked. Figure 5G As shown, Figure 5G The preparation provided by the embodiment of the present invention Figure 3 A schematic flow chart of a method for preparing a passivation layer 39 of a HEMT device.

[0159] Based on the above, this embodiment performs ion implantation in the channel on the side of the gate 38 that is biased toward the drain 36 , thereby reducing the electron concentration in this area, reducing the peak electric field intensity in this area, and improving the withstand voltage characteristics of the device.

[0160] The above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit the same. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that the technical solutions described in the aforementioned embodiments may still be modified, or some of the technical features may be replaced by equivalents. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A HEMT device for developing gallium nitride switches and power amplifiers, characterized in that: include: substrate; A buffer layer, disposed above the substrate; A plurality of combined layers are stacked on the buffer layer, each of the combined layers comprising a GaN channel layer and a barrier layer located above the GaN channel layer; A source electrode disposed above the topmost barrier layer among the plurality of combined layers; A drain electrode disposed above the topmost barrier layer among the plurality of combined layers; The plurality of combined layers are provided with a first groove and a second groove inside; The first groove is arranged from above the bottommost barrier layer among the plurality of combined layers to above the topmost barrier layer among the plurality of combined layers; The second groove extends downward from the bottom of the first groove on the side close to the drain electrode to the bottommost barrier layer of the plurality of combined layers; A gate is disposed in the first groove, and the top surface of the gate is higher than the topmost barrier layer in the plurality of combined layers, one side of the gate is attached to the side of the first groove close to the source, and the other side of the gate is on the same vertical line as the side of the second groove close to the source; A passivation layer covers the source electrode, the drain electrode, the gate electrode, the second groove, and an area of ​​the topmost barrier layer in the plurality of combined layers that is not blocked.

2. A HEMT device for developing gallium nitride switches and power amplifiers as claimed in claim 1, characterized in that: The thickness of the GaN channel layer of each of the plurality of combined layers is the same; The barrier layer of each of the plurality of combined layers has the same thickness; The GaN channel layer of each of the plurality of combined layers has the same material; The material of the barrier layer of each of the plurality of combined layers is the same.

3. A device structure for developing a gallium nitride switch and a power amplifier as claimed in claim 1, characterized in that: The material of the barrier layer includes AlGaN, InAlN, AlN or InAlN.

4. A HEMT device for developing a gallium nitride switch and a power amplifier as claimed in claim 1, characterized in that: The gate is made of Ni / Au metal or Pt / Au metal.

5. A HEMT device for developing gallium nitride switches and power amplifiers as claimed in claim 1, characterized in that: The material of the substrate includes silicon carbide SiC or aluminum nitride AlN.

6. A HEMT device for developing gallium nitride switches and power amplifiers as claimed in claim 1, characterized in that: The material of the buffer layer includes gallium nitride or AlGaN.

7. A HEMT device for developing gallium nitride switches and power amplifiers, characterized in that: include: substrate; A buffer layer, disposed above the substrate; A plurality of combined layers are stacked on the buffer layer, each of the combined layers comprising a GaN channel layer and a barrier layer located above the GaN channel layer; A source electrode disposed above the topmost barrier layer among the plurality of combined layers; A drain electrode disposed above the topmost barrier layer among the plurality of combined layers; A first groove is provided from above the bottom barrier layer of the plurality of combined layers to above the top barrier layer of the plurality of combined layers; A gate is disposed in the third groove, and a top surface thereof is higher than a topmost barrier layer in the plurality of combined layers, one side of the gate is attached to a side of the third groove close to the source, and a gap exists between the other side of the gate and the other side of the third groove; Ion implantation is arranged on the barrier layer below the side of the third groove close to the drain electrode, and the width of the ion implantation area is the same as the width of the interval; A passivation layer covers the source electrode, the drain electrode, the gate electrode, the third groove, and an area of ​​the topmost barrier layer in the plurality of combined layers that is not blocked.

8. A method for preparing a HEMT device for developing a gallium nitride switch and a power amplifier, the method being used to prepare a HEMT device for developing a gallium nitride switch and a power amplifier as claimed in any one of claims 1 to 6, characterized in that: selecting the substrate; growing the buffer layer on the substrate; sequentially growing the plurality of combined layers above the buffer layer; Prepare the source electrode and the drain electrode on both sides above the barrier layer at the top of the plurality of combined layers; Etching a region from above the bottommost barrier layer in the plurality of combined layers to above the topmost barrier layer in the plurality of combined layers to form the first groove; Etching the barrier layer at the bottom of the first groove on the side close to the drain electrode to the inside of the barrier layer to form the second groove; Prepare the gate, wherein the top surface of the gate is higher than the topmost barrier layer in the plurality of combined layers, one side of the gate is attached to one side of the first groove close to the source, and the other side of the gate is on the same vertical line as one side of the second groove close to the source; The passivation layer is grown on the source, the drain, the gate, the second groove, and the region where the topmost barrier layer in the plurality of combined layers is not blocked.

9. A method for preparing a HEMT device for developing a gallium nitride switch and a power amplifier, the method being used to prepare the HEMT device for developing a gallium nitride switch and a power amplifier as claimed in claim 7, characterized in that: selecting the substrate; growing the buffer layer on the substrate; sequentially growing the plurality of combined layers above the buffer layer; The source electrode and the drain electrode are prepared on both sides above the barrier layer at the top layer of the plurality of combined layers; Etching a region from above the bottommost barrier layer in the plurality of combined layers to above the topmost barrier layer in the plurality of combined layers to form the third groove; Performing ion implantation on the barrier layer below the side of the third groove close to the drain electrode, wherein the width of the ion implantation area is the same as the width of the interval; The gate is prepared in the third groove, the top surface of the gate is higher than the topmost barrier layer in the plurality of combined layers, one side of the gate is attached to the side of the third groove close to the source, and there is the gap between the other side of the gate and the other side of the third groove; The passivation layer is grown on the source electrode, the drain electrode, the gate electrode, the third recess, and an area where the topmost barrier layer in the plurality of combined layers is not blocked.