High-temperature-resistant insulating material and preparation method thereof
By using high-temperature resistant insulating materials prepared by silicone resin and other materials, the problem of failure of existing insulating materials under high temperature conditions is solved, and the insulation protection performance in an environment of 400~600℃ is achieved, meeting the high-temperature resistant requirements of power batteries.
Patent Information
- Application Number
- CN202411268046.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-11
- Publication Date
- 2024-11-19
AI Technical Summary
The existing insulating materials fail under high temperature conditions, which cannot meet the insulation protection needs of power batteries in an environment of 400~600℃. Rapid thermal aging of conventional epoxy resins above 300℃ leads to attenuation of insulation performance.
Using silicone resin, bisphenol A type epoxy resin, phenolic modified epoxy resin, phenol curing agent, universal leveling agent, powdering additive, benzoin and amide wax, etc., it is prepared by melt extrusion and grinding. High temperature insulation material forms a protective coating that is baked and cured at 230°C.
The material still maintains insulation protection performance under high temperature environments of 400~600℃, meeting the normal operation needs of power batteries under extreme operating conditions.
Smart Images

Figure SMS_1 
Figure SMS_2
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of insulating protective materials, and in particular to a high temperature resistant insulating material and a preparation method thereof. Background Art
[0002] As the new energy vehicle market continues to expand, the safety of power batteries, as the core components of new energy vehicles, has attracted much attention.
[0003] The main components of power batteries, such as battery cells, cooling systems, cover plates, back plates, side plates and other supporting and fixing systems, busbar connection systems, motor systems, etc., all require surface protection materials to provide insulation protection and conventional protection. Epoxy powder coating is widely used due to its excellent insulation properties.
[0004] In recent years, with the increase in vehicle mileage and battery capacity, power batteries have increasingly higher requirements for the high temperature resistance of insulation materials. Many battery manufacturers have proposed that power battery insulation materials need to be able to provide protection and insulation at high temperatures of 400-600°C to ensure the normal operation of power batteries. In this case, conventional epoxy resin coatings tend to age rapidly at temperatures above 300°C, resulting in rapid attenuation of insulation performance, until they powder and detach from the protected electrical components, completely losing their corrosion protection and insulation protection functions. Therefore, it is difficult to meet the requirements of battery manufacturers.
[0005] Chinese invention patent CN103320013B discloses a method for preparing a high-temperature resistant powder coating, which uses silicone resin, epoxy resin, polyester resin as the main resin, and is prepared with glass powder, manganese iron black, mica powder, sand grain agent, hardener and leveling agent, but its insulation protection effect still needs to be further improved.
[0006] Based on this, the present invention designs a high temperature resistant insulating material and a preparation method thereof to solve the above problems. Summary of the invention
[0007] In view of the above-mentioned shortcomings of the prior art, the present invention provides a high temperature resistant insulating material and a preparation method thereof.
[0008] To achieve the above objectives, the present invention is implemented through the following technical solutions: A high temperature resistant insulating material comprises the following raw materials in percentage by weight: 20-40% silicone resin, 10-20% bisphenol A epoxy resin, 10-20% phenolic modified epoxy resin, 7.5-15% phenolic curing agent, 0.5-1% general leveling agent, 0.2-0.5% powdering agent, 0.3-0.5% benzoin, 0.3-0.5% amide wax, and the balance is pigment and filler.
[0009] Furthermore, the silicone resin is pure phenyl silicone resin.
[0010] Furthermore, the bisphenol A epoxy resin has an epoxy equivalent of 700-900 g / eq and a viscosity of 4500-8000 mPas / 150°C.
[0011] Furthermore, the epoxy equivalent of the phenolic modified epoxy resin is 500-600 g / eq, and the viscosity is 2000-4000 cps / 150°C.
[0012] Furthermore, the phenolic curing agent is a phenolic hydroxyl-terminated resin with a hydroxyl value of 230-260 mgKOH / g and a softening point of 80-100°C.
[0013] A method for preparing a high temperature resistant insulating material comprises the following steps: (1) Weigh the raw materials according to the following percentages: silicone resin 20-40%, bisphenol A epoxy resin 10-20%, phenolic modified epoxy resin 10-20%, phenolic curing agent 7.5-15%, general leveling agent 0.5-1%, powdering agent 0.2-0.5%, benzoin 0.3-0.5%, amide wax 0.3-0.5%, and the balance is pigment and filler; (2) Premix the raw materials for 2-10 minutes, and control the stirring speed at 100-300 r / min; (3) Melt extrusion: The mixed material is extruded through an extruder; (4) After cooling, the material is placed in a grinding device and ground into powder to obtain a high temperature resistant insulating material.
[0014] Furthermore, the aspect ratio of the extruder screw is selected to be 15:1~50:1.
[0015] Furthermore, the temperature of the extruder is controlled at 110-130°C, and the screw speed is controlled at 600-1000 rpm.
[0016] Furthermore, the D50 content in the particle size distribution is controlled at 30-40%.
[0017] Furthermore, in step 4, sieving is performed through 50-200 mesh.
[0018] Compared with the prior art, the present invention has the following beneficial effects: When the high temperature resistant insulating material of the present invention is used, the powder is coated on the surface of the workpiece to be protected, and a protective coating is formed after being baked and cured. The curing conditions are: 230° C., 15 min. The protective coating has both good insulation performance and good high temperature resistance performance. It can be seen from the coating testing experiment that the protective coating can withstand a high temperature environment of 400~600℃ for 1h and still has insulation protection performance, ensuring the normal operation of the power battery under extreme working conditions and meeting the battery manufacturers' requirements for the high temperature and insulation resistance of the insulation material. DETAILED DESCRIPTION
[0019] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described in combination with the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention. Embodiment 1
[0020] This embodiment provides a method for preparing a high temperature resistant insulating material, comprising the following steps: (1) Weigh the raw materials according to the following percentages: 150 kg silicone resin, 200 kg bisphenol A epoxy resin, 200 kg phenolic modified epoxy resin, 150 kg phenolic curing agent, 8 kg general leveling agent, 4 kg powdering agent, 5 kg benzoin, 5 kg amide wax, and 278 kg pigments and fillers; Among them, benzoin is the main degassing agent, which can reduce the viscosity and surface tension of the coating, allow small gas molecules to escape, and improve its fluidity and smoothness. Since the melting point of benzoin is not high enough, its degassing effect is limited, and it needs to be added with amide wax to solve the pinhole and dent problems of porous substrates. Powdering additives can increase the charging properties of powders, so that the powders are better charged during spraying, increase the powdering rate, reduce the electrostatic shielding effect, and improve the powdering of corners; The silicone resin is preferably pure phenyl silicone resin, which has good high temperature resistance; the epoxy equivalent of the bisphenol A epoxy resin is preferably 700~900g / eq, and the viscosity is preferably 4500~8000mPas / 150℃; the epoxy equivalent of the phenolic modified epoxy resin is preferably 500~600g / eq, and the viscosity is preferably 2000~4000cps / 150℃; the phenolic curing agent is a phenolic hydroxyl-terminated resin with a hydroxyl value of 230~260 mgKOH / g and a softening point of 80~100℃.
[0021] (2) Premix the raw materials for 2 minutes, and control the stirring speed at 300r / min; (3) Melt extrusion: The mixed material is extruded through an extruder; (4) After cooling, the material is placed in a grinding device and ground into powder, and sieved through 50 mesh to obtain a high temperature resistant insulating material. Embodiment 2
[0022] This embodiment provides a method for preparing a high temperature resistant insulating material, comprising the following steps: (1) Weigh the raw materials according to the following percentages: 200 kg silicone resin, 200 kg bisphenol A epoxy resin, 200 kg phenolic modified epoxy resin, 150 kg phenolic curing agent, 10 kg general leveling agent, 3 kg powdering agent, 5 kg benzoin, 5 kg amide wax, and 227 kg pigments and fillers; The silicone resin is preferably pure phenyl silicone resin, which has good high temperature resistance; the epoxy equivalent of the bisphenol A epoxy resin is preferably 700~900g / eq, and the viscosity is preferably 4500~8000mPas / 150℃; the epoxy equivalent of the phenolic modified epoxy resin is preferably 500~600g / eq, and the viscosity is preferably 2000~4000cps / 150℃; the phenolic curing agent is a phenolic hydroxyl-terminated resin with a hydroxyl value of 230~260 mgKOH / g and a softening point of 80~100℃.
[0023] (2) Premix the raw materials for 10 minutes, and control the stirring speed at 100 r / min; (3) Melt extrusion: The mixed material is extruded through an extruder; (4) After cooling, the material is placed in a grinding device and ground into powder, and sieved through 200 mesh to obtain a high temperature resistant insulating material. Embodiment 3
[0024] This embodiment provides a method for preparing a high temperature resistant insulating material, comprising the following steps: (1) Weigh the raw materials according to the following percentages: 300 kg silicone resin, 200 kg bisphenol A epoxy resin, 200 kg phenolic modified epoxy resin, 150 kg phenolic curing agent, 10 kg general leveling agent, 2 kg powdering agent, 5 kg benzoin, 5 kg amide wax, and 128 kg pigments and fillers; The silicone resin is preferably pure phenyl silicone resin, which has good high temperature resistance; the epoxy equivalent of the bisphenol A epoxy resin is preferably 700~900g / eq, and the viscosity is preferably 4500~8000mPas / 150℃; the epoxy equivalent of the phenolic modified epoxy resin is preferably 500~600g / eq, and the viscosity is preferably 2000~4000cps / 150℃; the phenolic curing agent is a phenolic hydroxyl-terminated resin with a hydroxyl value of 230~260 mgKOH / g and a softening point of 80~100℃.
[0025] (2) Premix the raw materials for 5 minutes, and control the stirring speed at 200r / min; (3) Melt extrusion: The mixed material is extruded through an extruder; (4) After cooling, the material is placed in a grinding device and ground into powder, and sieved through 100 mesh to obtain a high temperature resistant insulating material. Embodiment 4
[0026] This embodiment provides a method for preparing a high temperature resistant insulating material, comprising the following steps: (1) Weigh the raw materials according to the following percentages: 400 kg silicone resin, 100 kg bisphenol A epoxy resin, 100 kg phenolic modified epoxy resin, 75 kg phenolic curing agent, 10 kg general leveling agent, 2 kg powdering agent, 5 kg benzoin, 5 kg amide wax, and 303 kg pigments and fillers; The silicone resin is preferably pure phenyl silicone resin, which has good high temperature resistance; the epoxy equivalent of the bisphenol A epoxy resin is preferably 700~900g / eq, and the viscosity is preferably 4500~8000mPas / 150℃; the epoxy equivalent of the phenolic modified epoxy resin is preferably 500~600g / eq, and the viscosity is preferably 2000~4000cps / 150℃; the phenolic curing agent is a phenolic hydroxyl-terminated resin with a hydroxyl value of 230~260 mgKOH / g and a softening point of 80~100℃.
[0027] (2) Premix the raw materials for 8 minutes, and control the stirring speed at 150r / min; (3) Melt extrusion: The mixed material is extruded through an extruder; (4) After cooling, the material is placed in a grinding device and ground into powder, and sieved through 80 mesh to obtain a high temperature resistant insulating material. Embodiment 5
[0028] The silicone resin is preferably pure phenyl silicone resin, which has good high temperature resistance; the epoxy equivalent of the bisphenol A epoxy resin is preferably 700~900g / eq, and the viscosity is preferably 4500~8000mPas / 150℃; the epoxy equivalent of the phenolic modified epoxy resin is preferably 500~600g / eq, and the viscosity is preferably 2000~4000cps / 150℃; the phenolic curing agent is a phenolic hydroxyl-terminated resin with a hydroxyl value of 230~260 mgKOH / g and a softening point of 80~100℃.
[0029] The silicone resin is preferably pure phenyl silicone resin, which has good high temperature resistance; the epoxy equivalent of the bisphenol A epoxy resin is preferably 700~900g / eq, and the viscosity is preferably 4500~8000mPas / 150℃; the epoxy equivalent of the phenolic modified epoxy resin is preferably 500~600g / eq, and the viscosity is preferably 2000~4000cps / 150℃; the phenolic curing agent is a phenolic hydroxyl-terminated resin with a hydroxyl value of 230~260 mgKOH / g and a softening point of 80~100℃. Embodiment 6
[0030] The aspect ratio of the extruder screw is preferably 15:1-50:1, the temperature of the extruder is preferably controlled at 110-130°C, the screw speed is preferably controlled at 600-1000 rpm, and the D50 (median particle size) content in the particle size distribution is preferably controlled at 30-40%. Embodiment 7
[0031] The main components of the powder coating auxiliary agent are surfactant, nitrogen-containing compound and fatty acid.
[0032] Alternatively, the powder coating aid may also be an inorganic substance (such as metal oxides, etc.). Embodiment 8
[0033] The filler may be one or a combination of two or more of wollastonite, silica powder, barium sulfate, mica powder, and glass powder.
[0034] Comparative Example 1 This embodiment provides a method for preparing a high temperature resistant insulating material, comprising the following steps: (1) Silicone resin 0kg, bisphenol A epoxy resin 200kg, phenolic modified epoxy resin 200kg, phenolic curing agent 150kg, general leveling agent 5kg, powdering agent 5kg, benzoin 3kg, amide wax 3kg, pigments and fillers 434kg; (2) Premix the raw materials for 10 minutes, and control the stirring speed at 100 r / min; (3) Melt extrusion: The mixed material is extruded through an extruder; (4) After cooling, the material is placed in a grinding device and ground into powder, and sieved through 200 mesh to obtain a high temperature resistant insulating material.
[0035] Comparative Example 2 This embodiment provides a method for preparing a high temperature resistant insulating material, comprising the following steps: (1) Weigh the raw materials according to the following percentages: 500 kg silicone resin, 50 kg bisphenol A epoxy resin, 50 kg phenolic modified epoxy resin, 37.5 kg phenolic curing agent, 10 kg general leveling agent, 2 kg powdering agent, 5 kg benzoin, 5 kg amide wax, and 340.5 kg pigments and fillers; (2) Premix the raw materials for 5 minutes, and control the stirring speed at 200r / min; (3) Melt extrusion: The mixed material is extruded through an extruder; (4) After cooling, the material is placed in a grinding device and ground into powder, and sieved through 100 mesh to obtain a high temperature resistant insulating material.
[0036] Experimental Example 1 The materials of Example 1 to Example 4 and Comparative Example 1 to Comparative Example 2 were cured, and the properties of the coatings were tested. The results are shown in Table 1.
[0037] Table 1 Coating performance test results
[0038] Note: The film thickness test refers to GB / T 13452.2, and the adhesion test refers to GB / T 9286.
[0039] Experimental Example 2 On the basis of Example 3, single factor experiments were conducted for the epoxy equivalent and viscosity of bisphenol A epoxy resin, the epoxy equivalent and viscosity of phenolic modified epoxy resin, and the hydroxyl value of phenolic curing agent. The obtained materials were cured and the properties of the coating were tested. The results are shown in Table 2.
[0040] Table 2 Coating performance test results
[0041] Note: The film thickness test refers to GB / T 13452.2, and the adhesion test refers to GB / T 9286.
[0042] When the high temperature resistant insulating material of the present invention is used, the powder is coated on the surface of the workpiece to be protected, and a protective coating is formed after being baked and cured. The curing conditions are: 230° C., 15 min. The protective coating has both good insulation performance and good high temperature resistance performance. It can be seen from the coating testing experiment that the protective coating can withstand a high temperature environment of 400~600℃ for 1h and still has insulation protection performance, ensuring the normal operation of the power battery under extreme working conditions and meeting the battery manufacturers' requirements for the high temperature and insulation resistance of the insulation material.
[0043] The above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit the same. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that the technical solutions described in the aforementioned embodiments may still be modified, or some of the technical features may be replaced by equivalents. Such modifications or replacements will not cause the essence of the corresponding technical solutions to deviate from the spirit and scope of the technical solutions of the embodiments of the present invention.
Claims
1. A high temperature resistant insulating material, characterized in that: The invention comprises the following raw materials in percentage by weight: 20-40% silicone resin, 10-20% bisphenol A epoxy resin, 10-20% phenolic modified epoxy resin, 7.5-15% phenolic curing agent, 0.5-1% general leveling agent, 0.2-0.5% powdering agent, 0.3-0.5% benzoin, 0.3-0.5% amide wax, and the balance is pigment and filler.
2. The high temperature resistant insulating material and the preparation method thereof according to claim 1, characterized in that: The silicone resin is pure phenyl silicone resin.
3. The high temperature resistant insulating material and the preparation method thereof according to claim 2, characterized in that: The bisphenol A epoxy resin has an epoxy equivalent of 700-900 g / eq and a viscosity of 4500-8000 mPas / 150°C.
4. The high temperature resistant insulating material and the preparation method thereof according to claim 3, characterized in that: The epoxy equivalent of the phenolic modified epoxy resin is 500-600 g / eq, and the viscosity is 2000-4000 cps / 150°C.
5. The high temperature resistant insulating material and the preparation method thereof according to claim 4, characterized in that: The phenolic curing agent is a phenolic hydroxyl-terminated resin with a hydroxyl value of 230-260 mgKOH / g and a softening point of 80-100°C.
6. A method for preparing a high temperature resistant insulating material according to any one of claims 1 to 5, characterized in that: The following steps are involved: (1) Weigh the raw materials according to the following percentages: silicone resin 20-40%, bisphenol A epoxy resin 10-20%, phenolic modified epoxy resin 10-20%, phenolic curing agent 7.5-15%, general leveling agent 0.5-1%, powdering agent 0.2-0.5%, benzoin 0.3-0.5%, amide wax 0.3-0.5%, and the balance is pigment and filler; (2) Premix the raw materials for 2-10 minutes, and control the stirring speed at 100-300 r / min; (3) Melt extrusion: The mixed material is extruded through an extruder; (4) After cooling, the material is placed in a grinding device and ground into powder to obtain a high temperature resistant insulating material.
7. The high temperature resistant insulating material and the preparation method thereof according to claim 6, characterized in that: The length-to-diameter ratio of the extruder screw is selected to be 15:1~50:
1.
8. The high temperature resistant insulating material and the preparation method thereof according to claim 7, characterized in that: The temperature of the extruder is controlled at 110~130℃, and the screw speed is controlled at 600~1000rmp.
9. The high temperature resistant insulating material and the preparation method thereof according to claim 8, characterized in that: The D50 content in the particle size distribution is controlled at 30~40%.
10. The high temperature resistant insulating material and the preparation method thereof according to claim 9, characterized in that: In step 4, sieve through 50-200 mesh.
Citation Information
Patent Citations
High-temperature-resistant powder coating and preparation method thereof
CN115418163A
Powder coating composition
CN116463030A