Method for manufacturing battery laminate, device for manufacturing battery laminate, method for manufacturing battery member, and device for manufacturing battery member
By forming an insulating layer on the electrode and placing a second electrode thereon, a series of conveying processes are used to solve the problem of easy damage to the insulating layer during electrode manufacturing, thereby improving the safety and stability of the battery.
Patent Information
- Application Number
- CN202380026249.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-03-17
- Filing Date
- 2023-03-16
- Publication Date
- 2024-11-19
AI Technical Summary
Existing integrated electrode insulation layers are prone to cracking or damage during electrode manufacturing due to low strength, which affects battery safety.
The method of forming an insulating layer on an electrode and setting a second electrode thereon utilizes a series of transport steps to implement the forming of the insulating layer and the setting of the electrode, ensuring that the insulating layer is protected at an early stage.
It effectively suppresses the breakage of battery laminates during the manufacturing process, improving the safety and stability of the battery.
Smart Images

Figure CN118985070A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a method for producing a battery laminate, an apparatus for producing a battery laminate, a method for producing a battery component, and an apparatus for producing a battery component. Background Art
[0002] In recent years, the requirements for high output, high capacity and long life of power storage elements such as batteries and power generation elements such as fuel cells have increased rapidly. However, in order to achieve this goal, there are also various issues related to the safety of the elements. For example, short circuits between electrodes due to the displacement or damage of the insulating layer provided between the electrodes can easily cause battery rupture and fire accidents, so further improvements are required.
[0003] Under these circumstances, as shown in Patent Document 1, an insulating layer integrated with electrodes has been proposed.
[0004] Citation list
[0005] Patent Literature
[0006] [Patent Literature]
[0007] [Patent Document 1] Japanese Unexamined Patent Application Publication No. 2013-191550
[0008] [Patent Document 2] Japanese Unexamined Patent Application Publication No. 2012-33282 Summary of the invention
[0009] Technical issues
[0010] However, if the strength of the electrode as a substrate is low, the insulating layer integrated with the electrode may be deformed when subjected to impact such as bending, causing the insulating layer to easily crack and be damaged during the electrode manufacturing process. There is still room for improvement in this regard.
[0011] Solutions to the problem
[0012] An embodiment of the present invention provides a method for manufacturing a battery laminate, comprising: forming an insulating layer by applying a liquid composition to a first electrode; and arranging a second electrode on the first electrode having the insulating layer formed thereon, wherein the forming and arranging are performed by a series of conveying.
[0013] Effects of the Invention
[0014] According to the technology disclosed in the present invention, it is possible to suppress the occurrence of damage to the battery laminate during the electrode production process. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] A more complete understanding of the embodiments and many of the attendant advantages and features thereof can be readily obtained and understood from the following detailed description taken in conjunction with the accompanying drawings.
[0016] [ Figure 1 ]
[0017] Figure 1 This is a (first) diagram showing an apparatus for producing a battery laminate according to an embodiment.
[0018] [ Figure 2 ]
[0019] Figure 2 This is a (second) diagram showing an apparatus for producing a battery laminate according to an embodiment.
[0020] [ Figure 3 ]
[0021] Figure 3 FIG. 3 is a diagram showing a manufacturing apparatus for a battery laminate according to an embodiment.
[0022] [ Figure 4 ]
[0023] Figure 4 FIG. 4 is a fourth diagram showing a manufacturing apparatus for a battery stack according to an embodiment.
[0024] [ Figure 5 ]
[0025] Figure 5 FIG. 5 is a fifth diagram showing a manufacturing apparatus for a battery stack according to an embodiment.
[0026] [ Figure 6 ]
[0027] Figure 6 FIG. 6 is a diagram showing a manufacturing apparatus for a battery stack according to an embodiment.
[0028] [ Figure 7 ]
[0029] Figure 7 FIG. 7 is a seventh diagram showing a manufacturing apparatus for a battery stack according to an embodiment.
[0030] [ Figure 8 ]
[0031] Figure 8 is an example of a block diagram of the main hardware of the control unit.
[0032] [ Fig. 9 ]
[0033] Fig. 9 This is a diagram showing an example of main functional blocks of a control unit.
[0034] [ Fig.10 ]
[0035] Fig.10 Included are a plan view and a cross-sectional view showing a first electrode having an insulating layer formed thereon.
[0036] [ Fig.11 ]
[0037] Fig.11 It is a top view showing the first electrode on which the insulating layer is formed.
[0038] [ Fig.12 ]
[0039] Fig.12 It is a (first) plan view showing a state where a second electrode is provided on a first electrode on which an insulating layer is formed.
[0040] [ Fig.13 ]
[0041] Fig.13 It is a (second) plan view showing a state where a second electrode is provided on a first electrode on which an insulating layer is formed.
[0042] [ Fig.14 ]
[0043] Fig.14 It is a cross-sectional view of a battery stack.
[0044] [ Fig.15 ]
[0045] Fig.15 This is a table summarizing Examples and Comparative Examples.
[0046] [ Fig.16 ]
[0047] Fig.16 FIG. 1 is a (first) diagram showing a manufacturing apparatus for a battery component according to an embodiment.
[0048] [ Fig.17 ]
[0049] Fig.17 This is a (second) diagram showing a manufacturing apparatus for a battery component according to an embodiment.
[0050] [ Fig.18 ]
[0051] Fig.18 FIG. 3 is a diagram showing a manufacturing apparatus for a battery component according to an embodiment.
[0052] [ Fig.19 ]
[0053] Fig.19 FIG. 4 is a fourth diagram showing a manufacturing apparatus for a battery component according to an embodiment.
[0054] [ Fig. 20 ]
[0055] Fig. 20 FIG. 5 is a fifth diagram showing a manufacturing apparatus for a battery component according to an embodiment.
[0056] [ Fig.21 ]
[0057] Fig.21 FIG. 6 is a diagram showing a manufacturing apparatus for a battery component according to an embodiment.
[0058] [ Fig. 22 ]
[0059] Fig. 22 FIG. 7 is a seventh diagram showing a manufacturing apparatus for a battery component according to an embodiment.
[0060] [ Fig.23 ]
[0061] Fig.23 is an example of a block diagram of the main hardware of the control unit.
[0062] [ Fig.24 ]
[0063] Fig.24 This is a diagram showing an example of main functional blocks of a control unit.
[0064] [Figure 25]
[0065] Fig.25A and 25B Indicates the change in the conveying speed of the conveying unit.
[0066] [ Fig.26 ]
[0067] Fig.26 Included are a plan view and a cross-sectional view showing a first substrate having an insulating layer formed thereon.
[0068] [ Fig. 27 ]
[0069] Fig. 27 It is a top view showing the first substrate on which the insulating layer is formed.
[0070] [ Fig.28 ]
[0071] Fig.28 It is a (first) plan view showing a state where a second base material is provided on a first base material on which an insulating layer is formed.
[0072] [ Fig.29 ]
[0073] Fig.29 It is a (second) plan view showing a state where a second base material is provided on a first base material having an insulating layer formed thereon.
[0074] [ Fig.30 ]
[0075] Fig.30 It is a cross-sectional view of a battery component.
[0076] [ Fig.31 ]
[0077] Fig.31 This is a table summarizing Examples and Comparative Examples.
[0078] The accompanying drawings are intended to describe embodiments of the present disclosure and should not be interpreted as limiting the scope thereof. Unless explicitly noted, the accompanying drawings should not be considered to be drawn to scale. Moreover, throughout the several views, the same or similar reference numerals represent the same or similar components. DETAILED DESCRIPTION
[0079] In describing the embodiments shown in the drawings, specific terms are used for clarity. However, the disclosure of this specification is not intended to be limited to the specific terms selected, and it should be understood that each specific component includes all technical equivalents having similar functions, operating in a similar manner and achieving similar results.
[0080] Hereinafter, embodiments of the present invention will be described with reference to the accompanying drawings. As used herein, the singular forms "a", "an" and "the" are intended to include the plural forms as well, unless the context clearly indicates otherwise.
[0081] Hereinafter, the mode for implementing the present invention will be described with reference to the drawings. In addition, in each figure, the same reference numerals are sometimes attached to elements having the same function or shape, and repeated descriptions are omitted.
[0082] There is no particular limitation on the battery applicable to the present embodiment, and it can generally be applied to secondary batteries and capacitors as storage elements, and is particularly applicable to lithium-ion secondary batteries. In addition, the battery stack of the present embodiment includes a structure in which the negative electrode and the positive electrode are stacked in a form of sandwiching an insulating layer, and the negative electrode and the positive electrode are insulated from each other by the insulating layer. The battery is formed by a battery stack, an electrolyte injected into the battery stack, and a shell that seals the battery stack and the electrolyte.
[0083] <Electrodes (first electrode, second electrode)>
[0084] Electrode is a general term for the negative electrode and the positive electrode shown below, and one is sometimes referred to as the first electrode and the other as the second electrode. That is, when the first electrode is used as a component of the negative electrode, the second electrode refers to the positive electrode, and when the first electrode is used as a component of the positive electrode, the second electrode refers to the negative electrode. In addition, the electrode substrate for the negative electrode and the electrode substrate for the positive electrode are collectively referred to as the electrode substrate, and the negative electrode composite material layer and the positive electrode composite material layer are collectively referred to as the electrode composite material layer.
[0085] Electrode substrate
[0086] The negative electrode substrate and the positive electrode substrate are not particularly limited as long as they are conductive substrates. As the electrode substrate, aluminum foil, copper foil, stainless steel foil, titanium foil, and etched foils having fine holes can be used, but are not limited thereto. These electrode substrates are suitable for secondary batteries, capacitors, especially lithium ion secondary batteries, and porous electrode substrates for lithium ion capacitors as storage elements.
[0087] As the electrode substrate, carbon paper used in power generation elements such as fuel cells, fibrous electrodes made into flat electrodes in the form of nonwoven fabrics or weaving, open-hole electrode substrates formed with the above-mentioned micropores, etc. can be used, but are not limited to these. In addition, as the electrode substrate used in solar cell elements, in addition to the above, flat substrates such as glass or plastic formed with a transparent semiconductor film containing indium-titanium oxide or zinc oxide, flat substrates formed with an electrode film of a conductive thin film, etc. can also be listed, but are not limited to these.
[0088] Alternatively, the electrode substrate may be formed using the electrode substrate-forming liquid composition.
[0089] -Liquid composition for forming an electrode base layer-
[0090] The material constituting the electrode base material layer includes, but is not limited to, gold, silver, copper, silver-plated copper, aluminum, nickel, and cobalt.
[0091] From these metal oxide particles and metal particles, one kind may be selected or a plurality of kinds may be mixed in any ratio and used.
[0092] Among them, silver oxide, copper oxide, silver, copper, and silver-plated copper, which are sintered bodies of silver and / or copper formed by sintering, are preferred from the viewpoint of electrical conductivity.
[0093] The shape of the particles is not particularly limited, and spherical, flat (plate-like) or irregularly shaped particles may be used.
[0094] The particle size of the metal particles or metal oxide particles used depends on the desired printing accuracy. However, if the particle size is too small, ink formulation design becomes difficult and a large amount of protective colloid must be used to prevent aggregation.
[0095] On the other hand, when the particle size is too large, there are problems such as inability to print fine patterns, poor contact between particles, and difficulty in sintering.
[0096] Therefore, it is generally between 5 nm and 10 μm, preferably between 10 nm and 5 μm.
[0097] The particle size here refers to a number-based average particle size D50 (median particle size) that can be measured by a laser diffraction scattering method or a dynamic light scattering method.
[0098] Examples of reducing agents used in combination when using metal oxide particles include, but are not limited to, alcohol compounds such as methanol, ethanol, isopropanol, butanol, cyclohexanol, and terpineol, polyols such as ethylene glycol, propylene glycol, and glycerol, carboxylic acids such as formic acid, acetic acid, oxalic acid, and succinic acid, carbonyl compounds such as acetone, methyl ethyl ketone, cyclohexane, benzaldehyde, and octanal, ester compounds such as ethyl acetate, butyl acetate, and phenyl acetate, and hydrocarbon compounds such as hexane, octane, toluene, naphthalene, and decalin.
[0099] Among them, in consideration of the efficiency of the reducing agent, polyhydric alcohols such as ethylene glycol, propylene glycol, and glycerin, and carboxylic acids such as formic acid, acetic acid, and oxalic acid are preferred.
[0100] In order to print the conductor patterning composition containing metal oxide particles and a reducing agent and / or metal particles as ink, a binder resin may be added, or a binder resin which also serves as a reducing agent may be used.
[0101] As high molecular weight compounds that can also serve as reducing agents, poly-N-ethylene compounds such as polyvinyl pyrrolidone and polyvinyl caprolactone, polyalkylene glycol compounds such as polyethylene glycol, polypropylene glycol, and polyTHF, thermoplastic resins and thermosetting resins such as polyurethane, cellulose compounds and their derivatives, epoxy compounds, polyester compounds, chlorinated polyolefins, and polyacrylic acid compounds can be used, but are not limited to these.
[0102] Among them, polyvinyl pyrrolidone is preferred in view of the adhesive effect, and polyethylene glycol, polypropylene glycol, and polyurethane compounds are preferred in view of the reducing effect.
[0103] In addition, polyethylene glycol and polypropylene glycol belong to the category of polyols and have the property of being particularly suitable for use as reducing agents.
[0104] In the composition for forming an electrode base layer, the electrode base layer is formed by heating the reduced metal oxide particles or sintering the metal particles by internal heating.
[0105] In the internal heating method, the metal particles and / or metal oxide particles in the electrode base layer forming composition generate heat, but the base does not generate heat. Therefore, even when a plastic base having poor heat resistance is used, deformation of the base can be prevented.
[0106] Therefore, the composition for forming an electrode base layer can be heated until it sufficiently exhibits conductivity.
[0107] As the internal heating method, from the viewpoint of improving productivity, a heating method using pulse light irradiation or microwave irradiation can be used, and pulse light irradiation is more preferred.
[0108] <Functional layer>
[0109] The functional layer refers to a part of a component that is necessary to perform a function in the battery's storage or charging operation, such as an electrode composite material layer that has a function of exerting capacity in the positive electrode or negative electrode or a function of assisting ion conduction, or an insulating layer that has a function of assisting in maintaining insulation between the positive electrode or negative electrode or the positive and negative electrodes.
[0110] 《Electrode composite material layer》
[0111] The negative electrode composite material layer and the positive electrode composite material layer are not particularly limited and can be appropriately selected according to the purpose, for example, at least containing an active material (negative electrode active material or positive electrode active material), and can contain a binder (binder), a thickener, a conductive aid, a dispersant, a non-aqueous electrolyte, a solid electrolyte, a gel electrolyte, or one or more monomers that have been polymerized to become a gel electrolyte, etc. The negative electrode composite material layer contains the negative electrode active material, and the positive electrode composite material layer contains the positive electrode active material.
[0112] -Liquid composition for forming electrode composite material layer-
[0113] The liquid composition for forming an electrode composite material layer contains at least one of a positive electrode active material and a negative electrode active material.
[0114] The liquid composition for forming the electrode composite material layer applied by inkjet printing may also contain one or more of a dispersion medium, a dispersant, a conductive aid, a binder, a non-aqueous electrolyte, a solid electrolyte, a gel electrolyte, or a monomer that becomes a gel electrolyte through a polymerization process, as required.
[0115] The negative electrode composite material layer and the positive electrode composite material layer can be formed by dispersing a powdered active material or catalyst composition in a liquid, applying the liquid, fixing it on an electrode substrate and drying it. Usually, they can be formed by printing and coating using a spray, a dispenser, a die coater, etc., and then drying after coating.
[0116] The negative electrode active material is not particularly limited as long as it is a material that can reversibly absorb and release alkali metal ions, that is, a material that can absorb and release metals such as Li ions or Na ions that are alloyed with alkali metal ions. Typically, a carbon material containing graphite having a graphite-type crystal structure can be used as the negative electrode active material. Examples of such carbon materials include natural graphite, spherical or fibrous artificial graphite, difficult-to-graphitize carbon (hard carbon), and easily-graphitized carbon (soft carbon). Examples of materials other than carbon materials include lithium titanate. In addition, from the perspective of increasing the energy density of lithium-ion batteries, high-capacity materials such as silicon, tin, silicon alloys, tin alloys, silicon oxide, silicon nitride, and tin oxide are also particularly suitable for use as negative electrode active materials.
[0117] As the active material in the nickel-hydrogen battery, as a hydrogen storage alloy, Zr-Ti-Mn-Fe-Ag-V-Al-W or Ti 15 Zr 21 V 15 Ni 29 AB2 or A2B hydrogen storage alloys represented by Cr5Co5Fe1Mn8, etc.
[0118] Other examples of active materials include, but are not limited to, composite oxides of transition metals and Li, metal oxides, alloy materials, inorganic compounds such as transition metal sulfides, carbon materials, organic compounds, Li metal, and Na metal.
[0119] As composite oxides, LiMnO2, LiMn2O4, lithium titanate (Li4Ti5O 12 , Li2Ti3O7), lithium manganese titanate (LiMg 1 / 2 Ti 3 / 2 O4), lithium cobalt titanate (LiCo 1 / 2 Ti 3 / 2 O4), lithium zinc titanate (LiZn 1 / 2 Ti 3 / 2 O4), lithium iron titanate (LiFeTiO4), lithium chromium titanate (LiCrTiO4), lithium strontium titanate (Li2SrTi6O 14 ) or lithium barium titanate (Li2BaTi6O 14 )wait.
[0120] Examples of sodium composite oxides include, but are not limited to, sodium titanate, such as Na2Ti3O7 or Na4Ti5O 12 wait.
[0121] A part of Ti or Na in sodium titanate may be substituted with other elements.
[0122] Examples of such an element include at least one selected from the group consisting of Ni, Co, Mn, Fe, Al, and Cr.
[0123] Examples of metal oxides include, but are not limited to, TiO2, Nb2TiO7, WO3, MoO2, MnO2, V2O5, SiO2, SiO or SnO2, etc.
[0124] Examples of alloy materials include, but are not limited to, Al, Si, Sn, Ge, Pb, As, or Sb.
[0125] Examples of transition metal sulfides include, but are not limited to, FeS or TiS.
[0126] As the inorganic compound, a compound obtained by replacing the transition metal of the composite oxide with a different element may be used.
[0127] These negative electrode active materials may be used alone or in combination of two or more.
[0128] The positive electrode active material is not particularly limited as long as it is a material that can reversibly absorb and release alkali metal ions. Typically, a transition metal compound containing an alkali metal can be used as the positive electrode active material. For example, as a lithium-containing transition metal compound, a composite oxide containing at least one element selected from cobalt, manganese, nickel, chromium, iron and vanadium and lithium can be cited.
[0129] The composite oxide is not particularly limited, and examples thereof include lithium-containing transition metal oxides such as lithium cobalt oxide, lithium nickel oxide, and lithium manganese oxide, olivine-type lithium salts such as LiFePO 4 , chalcogenides such as titanium disulfide and molybdenum disulfide, and manganese dioxide.
[0130] Lithium-containing transition metal oxides are metal oxides containing lithium and transition metals or metal oxides in which a portion of the transition metal in the metal oxide is replaced by a heterogeneous element. Examples of heterogeneous elements include Na, Mg, Sc, Y, Mn, Fe, Co, Ni, Cu, Zn, Al, Cr, Pb, Sb, B, etc., among which Mn, Al, Co, Ni and Mg are preferred. As transition metal compounds containing alkali metals, polyanionic compounds having XO4 tetrahedrons (X=P, S, As, Mo, W or Si, etc.) in the crystal structure can also be used.
[0131] Among them, lithium-containing transition metal phosphate compounds such as lithium iron phosphate and lithium vanadium phosphate are preferred from the viewpoint of recyclability.
[0132] In particular, lithium vanadium phosphate has a high lithium diffusion coefficient and is excellent in output characteristics.
[0133] In addition, from the viewpoint of electron conductivity, the polyanion compound is preferably composited by coating the surface with a conductive auxiliary agent such as a carbon material.
[0134] Examples of sodium-containing transition metal compounds include, but are not limited to, NaMO2-type oxides, sodium chromite (NaCrO2), sodium ferrite (NaFeO2), sodium nickelate (NaNiO2), sodium cobaltate (NaCoO2), sodium manganate (NaMnO2) or sodium vanadate (NaVO2), etc.
[0135] A part of M may be substituted with a metal element other than M and Na, for example, at least one selected from Cr, Ni, Fe, Co, Mn, V, Ti and Al.
[0136] In addition, examples of sodium-containing metal oxides include, but are not limited to, Na2FePO4F, NaVPO4F, NaCoPO4, NaNiPO4, NaMnPO4, NaMn 1.5 Ni 0.5 O4 or Na2V2(PO4)3, etc.
[0137] The heterogeneous element may be one or more. These positive electrode active materials may be used alone or in combination of two or more. Examples of the active material in the nickel-hydrogen battery include nickel hydroxide and the like.
[0138] The binder for the negative electrode or the positive electrode is not particularly limited, and for example, PVDF, PTFE, polyethylene, polypropylene, aramid resin, polyamide, polyimide, polyamideimide, polyacrylonitrile, polyacrylic acid, polymethyl acrylate, polyethyl acrylate, polyhexyl acrylate, polymethacrylic acid, polymethyl methacrylate, polyethyl methacrylate, polyhexyl methacrylate, polyvinyl acetate, polyvinyl pyrrolidone, polyether, polyether sulfone, hexafluoropolypropylene, styrene-butadiene rubber, carboxymethyl cellulose, etc. can be used.
[0139] As other examples of binders, copolymers of two or more materials selected from tetrafluoroethylene, hexafluoroethylene, hexafluoropropylene, perfluoroalkyl vinyl ether, vinylidene fluoride, chlorotrifluoroethylene, ethylene, propylene, pentafluoropropylene, fluoromethyl vinyl ether, acrylic acid, and hexadiene may also be used. In addition, two or more materials may be selected and mixed for use.
[0140] The conductive aid contained in the electrode composite material layer may be, for example, graphite such as natural graphite or artificial graphite, carbon black such as acetylene black, ketjen black, channel black, furnace black, lamp black, thermal black, etc., conductive fibers such as carbon fibers or metal fibers, metal powders such as carbon fluoride and aluminum, conductive whiskers such as zinc oxide or potassium titanate, conductive metal oxides such as titanium oxide, organic conductive materials such as phenylene derivatives and graphene derivatives, etc.
[0141] The active material in the fuel cell generally uses a material in which metal particles such as platinum, ruthenium or platinum alloy are carried on a catalyst carrier such as carbon as a catalyst for the cathode electrode or the anode electrode. In order to carry catalyst particles on the surface of the catalyst carrier, for example, the catalyst carrier is suspended in water, and a precursor of the catalyst particles is added (examples of the precursor of the catalyst particles include but are not limited to materials containing alloy components such as chloroplatinic acid, dinitrodiaminoplatinum, platinum chloride, platinous chloride, diacetylacetonate platinum, dichlorodiamineplatinum, dichlorotetraamineplatinum, platinum sulfate, ruthenic acid chloride, iridic acid chloride, rhodic acid chloride, ferric chloride, cobalt chloride, chromium chloride, gold chloride, silver nitrate, rhodium nitrate, palladium chloride, nickel nitrate, ferric sulfate, copper chloride, etc.), and then dissolved in the suspension, an alkali is added to generate a metal hydroxide, and a catalyst carrier carried on the surface of the catalyst carrier is obtained at the same time. The catalyst carrier is coated on an electrode substrate and reduced under a hydrogen atmosphere, thereby obtaining an electrode composite material layer coated with catalyst particles (active material) on the surface.
[0142] In the case of solar cells, etc., the active material may include, in addition to tungsten oxide powder and titanium oxide powder, oxide semiconductor layers such as SnO2, ZnO, ZrO2, Nb2O5, CeO2, SiO2, and Al2O3. The semiconductor layer is supported with a pigment, for example, a ruthenium-III transition metal complex, a ruthenium-II transition metal complex, an osmium-III transition metal complex, an osmium-II transition metal complex, a ruthenium-cis-dihydrate bipyridine complex, phthalocyanine and porphyrin, an organic-inorganic perovskite crystal, and other compounds.
[0143] The positive electrode active material may be used alone or in combination of two or more.
[0144] The dispersion medium is not particularly limited as long as it can disperse the active substance, and examples thereof include aqueous dispersion media such as water, ethylene glycol or propylene glycol, and organic dispersion media such as N-methyl-2-pyrrolidone, 2-pyrrolidone, cyclohexanone, ethyl lactate, butyl acetate, mesitylene, ethylene glycol monoethyl ether, ethylene glycol monobutyl ether, ethylene glycol monoethyl ether acetate, diethylene glycol monoethyl ether, diethylene glycol monobutyl ether, propylene glycol monomethyl ether, propylene glycol monoethyl ether, propylene glycol monobutyl ether, dibutyl ether, diethyl ether, di-tert-butyl ether, 2-n-butoxymethanol, 2-dimethylethanol, N,N-dimethylacetamide, anisole, diethoxyethane, n-hexane, heptane, octane, nonane, decane or p-menthane, but the present invention is not limited thereto.
[0145] The dispersion medium may be used alone or in combination of two or more.
[0146] The conductive auxiliary agent may be preliminarily compounded with the active material, or may be added when preparing the dispersion.
[0147] As the conductive auxiliary agent, for example, in addition to conductive carbon black formed by a furnace method, an acetylene method, a gasification method, or the like, carbon materials such as carbon nanofibers, carbon nanotubes, graphene, and graphite particles can be used.
[0148] As the conductive additive other than the carbon material, for example, metal particles such as aluminum or metal fibers can be used.
[0149] The mass ratio of the conductive auxiliary agent to the active material is preferably 10% or less, more preferably 8% or less.
[0150] When the mass ratio of the conductive auxiliary agent to the active material is 10% or less, the stability of the dispersion is improved.
[0151] There are no particular restrictions on the dispersant as long as it can improve the dispersibility of the active material, polymer particles or conductive additive in the dispersion medium. Examples thereof include polymers such as polycarboxylic acid series, naphthalenesulfonic acid formaldehyde condensate series, polyethylene glycol, polycarboxylic acid partial alkyl ester series, polyether series, polyalkylene polyamine series, surfactants such as alkyl sulfonic acid series, quaternary ammonium series, higher alcohol alkylene oxide series, polyol ester series, alkyl polyamine series, and inorganics such as polyphosphate series.
[0152] In the case where the dispersant or the electrolyte material cannot sufficiently bind the positive electrode materials or the negative electrode materials to each other or bind the positive electrode material or the negative electrode material to the conductive layer, a binder may be added to ensure binding force.
[0153] The binder is not particularly limited as long as it can impart adhesive strength, but from the viewpoint of inkjet ejection properties, a compound that does not increase viscosity is preferred.
[0154] The binder may be obtained by polymerizing a monomer compound after inkjet printing, or polymer particles may also be used.
[0155] In addition, as a material that does not increase the viscosity of the liquid composition, a polymer compound that can be dispersed in a dispersion medium or the like can be used.
[0156] When a polymer compound soluble in the dispersion medium is used, the viscosity of the liquid composition having the polymer compound dissolved in the dispersion medium may be such that the liquid composition can be ejected from the liquid ejecting head.
[0157] Examples of the monomer used include, without particular limitation, a method comprising applying a dispersion containing a compound having a polymerizable site and a polymerization initiator or catalyst and then heating; or a method comprising irradiating with non-ionizing radiation, ionizing radiation or infrared radiation.
[0158] In a compound having a polymerizable site, the polymerizable site may be a monofunctional group or a polyfunctional group in the molecule.
[0159] In addition, the polyfunctional polymerizable compound refers to a compound having two or more polymerizable groups.
[0160] There is no particular limitation as the polyfunctional polymerizable compound as long as it can be polymerized by heating or by irradiation with non-ionizing radiation, ionizing radiation or infrared radiation.
[0161] Examples of the polyfunctional polymerizable compound include acrylate resins, methacrylate resins, urethane acrylate resins, vinyl ester resins, unsaturated polyesters, epoxy resins, oxetane resins, vinyl ethers, and resins utilizing ene-thiol reactions.
[0162] Among them, from the viewpoint of production efficiency, acrylate resins, methacrylate resins, urethane acrylate resins, or vinyl ester resins are preferred.
[0163] Examples of materials constituting the polymer particles include, but are not limited to, polyvinylidene fluoride, acrylic resin, polyamide compound, polyimide compound, polyamideimide, ethylene-propylene-butadiene rubber (EPBR), styrene-butadiene copolymer, nitrile rubber (HNBR), isoprene rubber, polyisobutylene, polyethylene glycol (PEO), polymethyl methacrylate (PMMA), polyethylene vinyl acetate (PEVA), polyethylene, polypropylene, polyurethane, nylon, polytetrafluoroethylene, polyphenylene sulfide, polyethylene terephthalate or polybutylene terephthalate, etc.
[0164] Examples of the polymer compound include, but are not limited to, polyamide compounds, polyimide compounds, polyamide-imide, ethylene-propylene-butadiene rubber (EPBR), styrene-butadiene rubber (SBR), nitrile rubber (NBR), isoprene rubber, polyisobutylene, polyethylene glycol (PEO), polymethyl methacrylate (PMMA), polyethylene-vinyl acetate (PEVA), and the like.
[0165] The mass ratio of the binder to the active material is preferably 10% or less, more preferably 5% or less.
[0166] When the mass ratio of the binder to the active material is 10% or less, the binding force during electrode formation can be increased without reducing the ejection property.
[0167] <Insulation layer>
[0168] The insulating layer is a component that physically isolates the positive electrode from the negative electrode and ensures the ionic conductivity between the positive electrode and the negative electrode, and is arranged on the collector or the electrode composite material layer or both. In addition, it can also be arranged on an insulating substrate such as glass, glass epoxy, polyimide (PI), polyethylene naphthalate (PEN), polyethylene terephthalate (PET), cellulose paper, or rubber. At this time, functions such as surface friction resistance and thermal adhesion can be given.
[0169] The insulating layer is not particularly limited, but preferably has a specific volume resistivity of 1×10 12 The volume resistivity of the layer with a volume resistivity of 1×10 12 (Ω·cm) or more, short circuit between the positive and negative electrodes will not occur. The film thickness of the insulating layer is not particularly limited as long as the insulation between the positive electrode and the negative electrode is maintained, and is preferably 1 μm to 50 μm, and more preferably 5 μm to 20 μm. When the film thickness is thinner than the above case, it is difficult to maintain good insulation between the positive electrode and the negative electrode. In addition, when the film thickness is thicker than the above case, it is difficult to ensure good ionic conductivity.
[0170] In addition, the insulating layer is a porous insulating layer having holes, and the size of the holes is not particularly limited as long as it has ion conductivity, but from the viewpoint of the permeability of the electrolyte, it is preferably 0.01 μm or more and 10 μm or less. In addition, the porosity of the insulating layer is preferably 30% or more, more preferably 50% or more.
[0171] In addition, as used in the subsequent description Fig.10 As shown, a thick film region can also be formed in the insulating layer around the electrode. Fig.10 In the figure, 9 represents the collector of the first electrode, 10 represents the active material of the first electrode, 11a represents the thin film region of the insulating layer, and 11b represents the thick film region of the insulating layer. Here, the periphery of the electrode is preferably the periphery of the surface of the first electrode provided with the electrode composite material layer, and more preferably, when the electrode laminate is formed by stacking a second electrode having a polarity different from that of the first electrode, in the surface of the electrode composite material layer of the first electrode, in the region where the second electrode does not face each other. By forming a thick film region, deformation of the end electrode can be prevented when the first electrode and the second electrode are stacked, and displacement during stacking can also be suppressed. The thick film region is formed by a material having a melting point or a glass transition temperature (Tg), and after stacking, the thick film region of the first electrode located above and below the stack can be heated and bonded.
[0172] The insulating layer according to the present embodiment may have a structure in which a plurality of resin structures are overlapped.
[0173] <Insulating layer forming liquid composition>
[0174] The liquid composition for forming an insulating layer is a liquid applied to form an insulating layer, and includes an organic and / or inorganic compound, a solvent or a dispersion, etc. The organic and / or inorganic compound, and the solvent or the dispersion can be appropriately selected as required as long as the organic layer and / or inorganic layer finally formed has insulating properties.
[0175] For example, as an inorganic material with insulating properties, metal oxides, metal nitrides, and other metal particles can be cited. As metal oxides, Al2O3 (aluminum oxide), TiO2, BaTiO3, ZrO2, etc. are preferred. As metal nitrides, aluminum nitride, silicon nitride, etc. are preferred. As other metal particles, preferably insoluble ionic crystal particles such as aluminum fluoride, calcium fluoride, barium fluoride, barium sulfate, or materials from mineral resources such as boehmite, zeolite, apatite, kaolin, mullite, spinel, olivine, sericite, bentonite, or their artificial products, etc. In addition, as an inorganic material with insulating properties, glass ceramic powder can be cited. Glass ceramic powder preferably uses crystallized glass ceramics of crystallized glass of ZnO-MgO-Al2O3-SiO2 system, uses BaO-Al2O3-SiO2 system ceramic powder or Al2O3-CaO-SiO2-MgO-B2O3 system ceramic powder, etc. Non-glass ceramics, but are not limited to this.
[0176] Among them, from the viewpoint of insulation and heat resistance, alumina and silica are preferred, and α-alumina is more preferred. α-Alumina can be used as a "junk" chemical species, that is, a scavenger for chemical species that can cause capacity decay in lithium-ion secondary batteries.
[0177] In addition, as a solid electrolyte, a ceramic solid electrolyte such as an oxide or sulfide can be used. As oxides, γ-Li3PO4, Li3BO4, 0.75Li4GeO4-0.25Li2ZnGeO4 solid solution, Li4SiO4-Zn2SiO4 solid solution, Li4GeO4-Li3VO4 solid solution as LISICON type oxides can be cited, and Li 1.3 Al 0.3 Ti 1.7 (PO4)3 or Li 1.6 Al 0.6 Ge 0.8 Ti 0.6 (PO4)3, (Li, La)TiO3 as a perovskite structure, La5Li3Nb2O as a garnet oxide 12 、Li5La3TaO 12 or Li7La3Zr2O 12 .
[0178] Examples of sulfides include, but are not limited to, Li4GeS4-Li3PS4 solid solution, Li4SiS4-Li3PS4 solid solution, Li3PS4-Li2S solid solution, Li2S-P2S5 solid solution, Li2S-SiS2, Li 10 GeP2S 12 , Argyro dite type Li6PS5X (X = Cl, Br, I) or L7P3S 11 Crystal.
[0179] (Ceramic solid electrolyte for sodium ion secondary batteries)
[0180] As oxides, NASICON type Na 1+x Zr2Si x P 3-x O 12 (0≤x≤1), or β-alumina type Na2O-11Al2O3. Examples of sulfides include Na2S-P2S5, Na3PS4, Na3SbS4, Na2S-SiS2, and Na2S-GeS2. As selenides, Na3PSe4 and the like can be cited. These can be used as composite electrolytes with polymers.
[0181] The particle size of these inorganic materials is preferably 10 μm or less, more preferably 3 μm or less. By forming the particle size, a dense porous structure can be formed, and a porous structure with good ion permeability without local unevenness inside the porous structure can be obtained. The inorganic material is dispersed in a liquid to prepare a liquid composition for forming an inorganic layer. The liquid is selected to be suitable for the dispersed inorganic material.
[0182] When the inorganic material is dispersed in a liquid, a binder is added. The binder has the function of fixing the inorganic material particles to each other in order to keep the inorganic material as an insulating layer. As the binder, acrylic resin, styrene butadiene resin, polyvinylidene fluoride resin, etc. can be used.
[0183] When preparing the ink for forming the inorganic layer, a homogenizer may be used to disperse the ink. The homogenizer may be a high-speed rotary shear stirring type, a high-pressure jet dispersion type, an ultrasonic dispersion type, a medium stirring and grinding type, or the like.
[0184] When preparing the ink for producing the inorganic layer, additives such as dispersants and surfactants may be used as needed. As dispersants and surfactants, MEGAFAC (DIC Corporation), MALIALIM (NOF Corporation), ESLEAM (NOF Corporation), SOLSPERSE (Lubri zol), POLYFLOW (Kyoeisha Chemical Co., Ltd.) and the like may be used. As other additives, propylene glycol, carboxymethyl cellulose and the like, which are thickening materials for adjusting the viscosity, may be used.
[0185] In addition, as an insulating organic and / or inorganic material, a resin can be used. In order to form the resin, a liquid composition for forming a resin layer is used in which at least one of the resin and the precursor of the resin (the resin and / or the precursor of the resin) is dissolved or dispersed in a liquid.
[0186] The liquid is selected to be suitable for dissolving or dispersing the resin, and specifically, water, hydrocarbon liquids, alcohol liquids, ketone liquids, ester liquids, and ether liquids can be used.
[0187] As the precursor of the resin and the resin, it is preferred that the resin or oligomer having a structure crosslinkable by ionizing radiation or infrared (heat) in the molecule is dissolved in a liquid. As the precursor of the resin and the resin, for example, a low molecular weight oligomer precursor in polyimide resin, polyester resin, polyamide resin, polyolefin resin, acrylic resin, or a part thereof is preferably modified with a hydrocarbon group having an aliphatic unsaturated bond, for example, a substance having an unsaturated bond such as allyl, allyloxy, acryloyl, butenyl, cinnamyl, cinnamoyl, crotonyl, cyclohexadienyl, isopropenyl, methacryloyl, pentenyl, propenyl, styryl, vinyl, butadienyl, etc., is preferably present on the side chain of a part of the acrylic copolymer.
[0188] In addition, for polybutylene terephthalate, polyethylene terephthalate, polyacrylonitrile, polyvinylidene fluoride, polyether ketone, polyethylene naphthalate, polysulfone, polyimide, polyester, polypropylene, polyformaldehyde, polyamide, polyvinylpyrrolidone and cellulose, a dispersed precursor or cellulose nanofiber with a molecular weight of less than 10,000 can also be used, and they can be heated by ionizing radiation or infrared rays, thereby improving the insolubility and cross-linking properties after formation.
[0189] Furthermore, in order to improve the crosslinking property, these precursors may contain up to about 30 parts by weight of an azide compound. For example, 3,3′-dichloro-4,4′-diazidodiphenylmethane, 4,4′-diazidodiphenyl ether, 4,4′-diazidodiphenyl disulfide, 4,4′-diazidodiphenyl sulfide, 4,4′-diazidodiphenyl sulfide, 4-azidodiphenyl sulfone, 4-azidochalcone, 4-azido-4′-hydroxychalcone, 4-azido-4′-methoxychalcone, 4-azido-4′-morpholinochalcone, 4-dimethylamino-4′-azidochalcone, 2,6-bis(4′-azido)- ... 4-Azido-cinnamyl)-4-methylcyclohexanone, 2,6-bis(4′-azido-cinnamyl)-cyclohexanone, cinnamyl-4-azidoacetophenone, 4-azido-cinnamylacetophenone, 4-azido-4′-dimethylaminocinnamylacetophenone, cinnamyl-4-azido-cinnamylacetone, 2,6-bis(4′-azido-cinnamyl)-4-methylcyclohexanone, 2,6-bis(4′-azido-cinnamyl)-cyclohexanone, 1,4′-azido-benzylideneindene, 1,4′-azido-benzylideneindene, 1 , 4′-azidobenzylidene-3-α-hydroxy-4″-azidobenzylindene, 9,4′-azidobenzylidenefluorene, 9,4′-azidocinnamylfluorene, 4,4′-diazide stilbene-2,2′-disulfonyl-N-(p-methoxyphenyl)amide, 4,4′-diazide stilbene-2,2′-disulfonyl-N-(p-hydroxyethylphenyl)amide, 4,4′-diazide stilbene-2,2′-disulfonyl-N-(p-hydroxyphenyl)amide, 4,4′-diazide stilbene-2,2′-disulfonyl-N-(p-hydroxyethylphenyl)amide Sulfonylamide, 4,4′-diazide benzophenone, 4,4′-diazide stilbene, 4,4′-diazide chalcone, 4,4′-diazide benzylideneacetone, 6-azido-2-(4′-azidophenylvinyl)benzimidazole, 3-azidobenzylideneaniline-N-oxy-p-(4-azidophenylvinylamide)benzoic acid, 1,4-bis(3′-azidophenylvinyl)benzene, 3,3′-diazide diphenyl sulfone, 4,4′-diazide diphenylmethane, etc., but are not limited thereto.
[0190] Among them, 2,6-bis-(4'-azidobenzylidene)-4-methylcyclohexanone and the like are particularly preferred. The solvents for dissolving these materials are not particularly limited, and solvents that can dissolve the compounds and whose boiling points and surface tensions are suitable for the subsequent coating and drying processes can be used alone or in a mixed manner with an adjusted ratio. In the case where the resin layer formed by the resin has voids inside, ions of the electrolyte and the like can actually pass through, which is preferred in terms of being able to function as a separator or preventing thermal runaway.
[0191] From the viewpoint of the permeability and retention of the electrolyte, it is preferred that the material not only has ion permeability but also has fine openings. It is more preferred that the resin contains a material such as a foaming agent, and is heated after coating, or contains a soluble salt such as an electrolyte, and after coating, it is immersed in the electrolyte to form openings or pores due to the dissolution of the salt, thereby being able to show ion permeability. Alternatively, a block-shaped molecular skeleton is formed after coating to form a specific phase separation or microphase separation to form fine openings, thereby similarly showing ion permeability, or by containing a volatile solvent in the ink composition, solid-liquid phase separation is caused in polymerization after printing, and then, by removing (drying) the solvent, a fine mesh-like opening can be obtained. In particular, a liquid composition that causes solid-liquid phase separation (hereinafter also referred to as "polymerization-induced phase separation") by polymerization is preferred because it can obtain a porous resin structure with high ion permeability in a short time.
[0192] As for the shape of the porous insulating layer, from the viewpoint of ensuring good permeability of liquid or gas, it is preferred to have a three-dimensional branched mesh structure of a resin solid or an inorganic solid as a skeleton, and a structure in which a plurality of holes of the porous insulating layer are continuously connected. That is, the porous insulating layer has a plurality of holes, and preferably one hole has connectivity linked to other holes around it and is three-dimensionally developed. The holes are connected to each other, so that liquid and gas can easily penetrate.
[0193] As a method for confirming that the holes are connected, for example, a method for confirming the continuous connection between the holes by image observation of the cross section of the porous structure by a scanning electron microscope (SEM) etc. can be cited. In addition, as one of the physical properties obtained by connecting the holes, air permeability can be cited. The air permeability of the porous structure is, for example, measured according to JIS P8117, preferably less than 1000 seconds / 100mL, more preferably less than 500 seconds / 100mL, and most preferably less than 300 seconds / 100mL. At this time, the air permeability is measured, for example, using a Gurley air permeability meter (manufactured by Toyo Seiki Seisakusho) etc. Thus, it can be cited, such as judging that the holes are connected according to the air permeability of less than 1000 seconds / 100mL.
[0194] There is no particular restriction on the cross-sectional shape of the hole, and various shapes such as approximately circular, approximately elliptical, and approximately polygonal can be cited. In addition, the size of the hole is not particularly limited. Here, the so-called size of the hole refers to the length of the longest straight line that can be drawn in the cross-sectional shape. The size of the hole can be determined by a cross-sectional photograph taken by a scanning electron microscope (SEM) or the like. The size of the hole in the porous structure is preferably greater than 0.1 μm and less than 10 μm, and more preferably greater than 0.1 μm and less than 1 μm. By making the size of the hole greater than 0.1 μm and less than 10 μm, the penetration of liquid and gas occurs sufficiently in the porous structure, and functions such as material separation and reaction field can be effectively demonstrated.
[0195] In addition, as described later, when the porous structure is used as an insulating layer of a storage element, by making the pore size less than 10 μm, it is possible to prevent a short circuit between the positive electrode and the negative electrode caused by lithium dendrites generated inside the storage element, thereby improving safety. The porosity of the porous structure is preferably 30% or more, and more preferably 50% or more.
[0196] In addition, the porosity of the porous structure is preferably 90% or less, more preferably 85% or less. By making the porosity 30% or more, liquid and gas permeation occurs sufficiently in the porous structure, and functions such as material separation and reaction field can be effectively exhibited. In addition, when the porous structure is used as an insulating layer in a storage element, the permeability of the electrolyte and the permeability of the ions are improved, and the reaction inside the storage element is effectively carried out.
[0197] In addition, by making the porosity less than 90%, the strength of the porous structure is improved. In addition, as a method for measuring the porosity of the porous structure, there is no particular limitation, and for example, the following method can be cited: unsaturated fatty acids (commercially available butter) are filled in the porous structure, after osmium staining, the internal cross-sectional structure is cut out with FIB, and the porosity is measured using SEM.
[0198] The porous insulating layer formed of resin is a porous resin structure having a skeleton formed of resin and a portion where the skeleton is not formed as pores. In addition, the resin structure is preferably a co-continuous structure or a monolithic structure in which the resin portion and the pore portion are continuous.
[0199] The continuity of the resin portion refers to a structure in which no interface exists in the resin portion. That is, it is different from a structure in which a plurality of resin particles are bonded and connected by a binder or the like which is a resin different from the resin particles. Such a structure can be formed by, for example, the polymerization-induced phase separation method described above and below.
[0200] The resin may contain a resin as a gel electrolyte and a nonaqueous electrolyte, an ionic liquid, glyme, or an electrolyte salt.
[0201] --Polymerizable compounds--
[0202] The polymerizable compound forms a resin by polymerization, and forms a porous resin when polymerized in a liquid composition causing polymerization to induce phase separation. The resin formed by the polymerizable compound preferably has a resin of a network structure formed by the application of active energy rays, such as (for example, irradiation of light, heating, etc.), such as preferably acrylate resin, methacrylate resin, carbamate acrylate resin, vinyl ester resin, unsaturated polyester resin, epoxy resin, oxetane resin, vinyl ether resin, and resin formed by ene-thiol reaction. In addition, from the viewpoint of easily forming a structure using highly reactive free radical polymerization, from the perspective of production efficiency, more preferably acrylate resin, methacrylate resin, carbamate acrylate resin, vinyl ester resin as a resin formed by a polymerizable compound with (meth) acryloyl, as a resin formed by a polymerizable compound with vinyl. These can be used alone, or more than two kinds can be used in combination. In the case of using more than two kinds in combination, as a combination of polymerizable compounds, there is no particular limitation, and it can be appropriately selected according to the purpose, for example, in order to impart flexibility, it is preferred to mix other resins with polyurethane acrylate resin as the main component. In the present invention, polymerizable compounds having an acryloyl group or a methacryloyl group are collectively referred to as polymerizable compounds having a (meth)acryloyl group.
[0203] The polymerizable compound preferably has at least one free radical polymerizable functional group. Examples thereof include monofunctional, difunctional, trifunctional or higher free radical polymerizable compounds, functional monomers, and free radical polymerizable oligomers. Among them, free radical polymerizable compounds having two or more functional groups are preferred.
[0204] Examples of the monofunctional radical polymerizable compound include 2-(2-ethoxyethoxy)ethyl acrylate, methoxypolyethylene glycol monoacrylate, methoxypolyethylene glycol monomethacrylate, phenoxypolyethylene glycol acrylate, 2-acryloyloxyethyl succinate, 2-ethylhexyl acrylate, 2-hydroxyethyl acrylate, 2-hydroxypropyl acrylate, tetrahydrofurfuryl acrylate, 2-ethylhexyl carbitol acrylate, 3-methoxybutyl acrylate, benzyl acrylate, cyclohexyl acrylate, isoamyl acrylate, isobutyl acrylate, methoxytriethylene glycol acrylate, phenoxytetraethylene glycol acrylate, hexadecyl acrylate, isostearyl acrylate, octadecyl acrylate, styrene monomer, etc. These may be used alone or in combination of two or more.
[0205] Examples of the bifunctional radical polymerizable compound include 1,3-butanediol diacrylate, 1,4-butanediol diacrylate, 1,4-butanediol dimethacrylate, 1,6-hexanediol diacrylate, 1,6-hexanediol dimethacrylate, diethylene glycol diacrylate, polyethylene glycol diacrylate, neopentyl glycol diacrylate, EO-modified bisphenol A diacrylate, EO-modified bisphenol F diacrylate, neopentyl glycol diacrylate, tricyclodecane dimethanol diacrylate, etc. These may be used alone or in combination of two or more.
[0206] Examples of the radical polymerizable compound having three or more functions include trimethylolpropane triacrylate (TMPTA), trimethylolpropane trimethacrylate, EO-modified trimethylolpropane triacrylate, PO-modified trimethylolpropane triacrylate, caprolactone-modified trimethylolpropane triacrylate, HPA-modified trimethylolpropane trimethacrylate, pentaerythritol triacrylate, pentaerythritol tetraacrylate (PETTA), glycerol triacrylate, ECH-modified glycerol triacrylate, EO-modified glycerol triacrylate, PO-modified glycerol triacrylate, tri(acryloyloxyethyl)isocyanurate, dipentaerythritol hexaacrylate (DPHA), caprolactone-modified dipentaerythritol hexaacrylate, dipentaerythritol hydroxypentaacrylate, alkyl-modified dipentaerythritol pentaacrylate, alkyl-modified dipentaerythritol tetraacrylate, alkyl-modified dipentaerythritol triacrylate, dimethylolpropane tetraacrylate (DTMPTA), pentaerythritol ethoxy tetraacrylate, EO-modified phosphoric acid triacrylate, 2,2,5,5-tetramethylolcyclopentanone tetraacrylate, etc. These may be used alone or in combination of two or more.
[0207] The content of the polymerizable compound in the liquid composition causing polymerization-induced phase separation is preferably 5.0% by mass or more and 70.0% by mass or less, more preferably 10.0% by mass or more and 50.0% by mass or less, and most preferably 20.0% by mass or more and 40.0% by mass or less relative to the total amount of the liquid composition. When the content of the polymerizable compound is 70.0% by mass or less, the pores of the porous resin obtained are several nanometers or less, the size is not too small, and the porous resin has a suitable porosity, which can suppress the tendency of liquid or gas to be difficult to penetrate, and is therefore preferred. In addition, when the content of the polymerizable compound is 5.0% by mass or more, the three-dimensional network structure of the resin is fully formed, the porous structure can be fully obtained, and the strength of the obtained porous structure also shows a tendency to increase, and is therefore preferred.
[0208] --Porogen--
[0209] The solvent used to cause polymerization-induced phase separation (hereinafter referred to as "porogen") is a liquid that is miscible with the polymerizable compound. In addition, the porogen is a liquid that is incompatible with (phase-separated) the polymer (resin) produced during the polymerization of the polymerizable compound in the liquid composition. By including a solvent in the liquid composition, when the polymerizable compound is polymerized in the liquid composition, in other words, when the first active energy ray and the second active energy ray are sequentially irradiated in the liquid composition, a porous resin is formed. In addition, it is preferred that a compound (hereinafter referred to as a polymerization initiator) that can dissolve free radicals or acids generated by light or heat is dissolved. One type of solvent may be used alone, or two or more types may be used in combination. In addition, the porogen is not polymerizable.
[0210] At normal pressure, the boiling point of a single porogen or the boiling point of two or more porogens in combination is preferably 50°C to 250°C, more preferably 70°C to 200°C. By setting the boiling point to 50°C or more, the vaporization of the porogen near room temperature is suppressed, the liquid composition is easily handled, and the content of the porogen in the liquid composition is easily controlled. In addition, by setting the boiling point to 250°C or less, the time in the process of drying the porogen after polymerization can be shortened, thereby improving the productivity of the porous resin. In addition, since the amount of porogen remaining in the porous resin can be suppressed, the quality can be improved when the porous resin is used as a functional layer such as a substance separation layer for separating substances or a reaction layer as a reaction field.
[0211] Furthermore, the boiling point of a single porogen or a combination of two or more porogens is preferably 120° C. or higher at normal pressure.
[0212] As the porogen, for example, glycols such as diethylene glycol monomethyl ether, ethylene glycol monobutyl ether, ethylene glycol monoisopropyl ether, and dipropylene glycol monomethyl ether, esters such as γ-butyrolactone and propylene carbonate, and amides such as N,N-dimethylacetamide can be cited. In addition, liquids with relatively large molecular weights such as methyl myristate, methyl decanoate, methyl myristate, and tetradecane can also be cited. In addition, liquids such as acetone, 2-ethylhexanol, and 1-bromonaphthalene can also be cited.
[0213] Furthermore, it is not necessarily the case that the liquids exemplified above are porogens. As described above, a porogen is a liquid that is miscible with a polymerizable compound and is immiscible (phase-separated) with a polymer (resin) produced during the polymerization of the polymerizable compound in a liquid composition. In other words, whether a certain liquid is a porogen is determined by the relationship between the polymerizable compound and the polymer (resin formed by the polymerization of the polymerizable compound).
[0214] In addition, the liquid composition only needs to contain at least one porogen having the above-mentioned specific relationship with the polymerizable compound, so the range of material selection when preparing the liquid composition is wide, and the design of the liquid composition becomes easy. By expanding the range of material selection when preparing the liquid composition, the corresponding range is expanded when considering the characteristics required for the liquid composition from the viewpoint other than the formation of a porous structure.
[0215] For example, when a liquid composition is ejected by an inkjet method, a liquid composition having ejection stability and the like is required from a viewpoint other than forming pores, and since the range of material selection is wide, the design of the liquid composition becomes easy.
[0216] As described above, the liquid composition may contain at least one porogen having the specific relationship with the polymerizable compound, and therefore, the liquid composition may further contain a liquid that does not have the specific relationship with the polymerizable compound (a liquid that is not a porogen). However, the content of the liquid that does not have the specific relationship with the polymerizable compound (a liquid that is not a porogen) is preferably 10.0% by mass or less, more preferably 5.0% by mass or less, further preferably 1.0% by mass or less, and most preferably does not contain the liquid, relative to the total amount of the liquid composition.
[0217] Relative to the total amount of the liquid composition, the content of the porogen in the liquid composition is preferably 30.0 mass % or more and 95.0 mass % or less, more preferably 50.0 mass % or more and 90.0 mass % or less, and most preferably 60.0 mass % or more and 80.0 mass % or less. When the content of the porogen is 30.0 mass % or more, the size of the pores of the obtained porous body is less than a few nm, the size is not too small, and the porous resin has a suitable porosity, which can suppress the tendency of liquid or gas to be difficult to penetrate, so it is preferred. In addition, when the content of the porogen is 95.0 mass % or less, the three-dimensional network structure of the resin is fully formed, the porous structure can be fully obtained, and the strength of the obtained porous structure also shows a tendency to increase, so it is preferred.
[0218] The mass ratio of the content of the polymerizable compound to the content of the porogen in the liquid composition (polymerizable compound:porogen) is preferably 1.0:0.4 to 1.0:19.0, more preferably 1.0:1.0 to 1.0:9.0, and most preferably 1.0:1.5 to 1.0:4.0.
[0219] ---Polymerization-induced phase separation---
[0220] Polymerization-induced phase separation makes it possible to form a porous resin. Polymerization-induced phase separation refers to a state in which a polymerizable compound and a porogen are miscible, but a polymer (resin) produced during the polymerization of the polymerizable compound and the porogen are incompatible (phase separation occurs). Although there are other methods for obtaining a porous resin by phase separation, since a porous body having a network structure can be formed by using the polymerization-induced phase separation method, it can be expected that a porous body with high tolerance to chemicals or heat can be formed. In addition, compared with other methods, the advantages of short process time and easy surface modification can also be cited.
[0221] Next, the process of forming a porous resin using polymerization-induced phase separation is described. The polymerizable compound undergoes a polymerization reaction by light irradiation or the like to form a resin. During this process, the solubility of the porogen in the growing resin decreases, resulting in phase separation between the resin and the porogen. Finally, the resin forms a porous structure in which the pores are filled with the porogen.
[0222] During drying, the porogen and the like are removed, leaving a porous resin. Therefore, in order to form a porous resin having an appropriate porosity, the compatibility between the porogen and the polymerizable compound, and the compatibility between the porogen and the resin formed by polymerizing the polymerizable compound, are studied.
[0223] The compatibility between the porogen and the polymerizable compound is determined as follows.
[0224] First, the liquid composition is injected into a quartz microcell, and the transmittance of light (visible light) of the liquid composition at a wavelength of 550 nm is measured while stirring at 300 rpm using a stirrer. In the present invention, a light transmittance of 30% or more is considered to be a state in which the polymerizable compound and the porogen are compatible, and a light transmittance of less than 30% is considered to be a state in which the polymerizable compound and the porogen are incompatible. In addition, the following are the conditions related to the measurement of light transmittance.
[0225] -Quartz microcell: special microcell with screw cap (trade name: M25-UV-2)
[0226] - Transmittance measurement equipment: USB4000 manufactured by Ocean Optics
[0227] -Stirring speed: 300rpm
[0228] -Measurement wavelength: 550nm
[0229] - Reference: In a state where air is contained in a quartz microcell, the transmittance of light at a wavelength of 550 nm is measured and obtained (transmittance: 100%).
[0230] The compatibility of the porogen with the resin formed by polymerizing the polymerizable compound is determined as follows.
[0231] First, on an alkali-free glass substrate, resin particles are evenly dispersed on the substrate by spin coating to form a gap agent. Then, the substrate coated with the gap agent and the alkali-free glass substrate not coated with the gap agent are bonded to each other in a manner of clamping the surface coated with the gap agent. Then, the liquid composition is filled between the bonded substrates using capillary phenomenon to make a "component for measuring haze before UV irradiation". Then, the component for measuring haze before UV irradiation is irradiated with UV to cure the liquid composition. Finally, the "component for measuring haze" is made by sealing the surrounding of the substrate with a sealant. The various conditions during production are as follows:
[0232] -Alkali-free glass substrate: Made by Nippon Electric Glass Co., Ltd., 40mm, t=0.7mm, OA-10G
[0233] - Gap agent: Made by Sekisui Chemical, resin micro beads GS-L100, average particle size 100μm
[0234] - Spin coating conditions: dispersion drop volume 150 μL, rotation speed 1000 rpm, rotation time 30 s
[0235] -Filled liquid composition volume: 160 μL
[0236] -UV irradiation conditions: UV-LED is used as the light source, the wavelength of the light source is 365nm, and the irradiation intensity is 30mW / cm 2 , irradiation time 20s
[0237] - Sealant: TB3035B (manufactured by Three Bond)
[0238] Next, the haze value (haze) is measured using the prepared haze measuring element before UV irradiation and the haze measuring element. The measured value in the haze measuring element before UV irradiation is used as a reference (haze value 0), and the increase rate of the measured value (haze value) in the haze measuring element relative to the measured value in the haze measuring element before UV irradiation is calculated. For the haze value in the haze measuring element, the lower the miscibility between the resin formed by polymerizing the polymerizable compound and the porogen, the higher the value, and the higher the miscibility, the lower the value. In addition, the higher the haze value, the easier it is for the resin formed by polymerizing the polymerizable compound to form a porous structure. In the present invention, the case where the rate of increase of the haze value is 1.0% or more is judged as a state in which the resin and the porogen are incompatible, and the case where it is less than 1.0% is judged as a state in which the resin and the porogen are compatible. In addition, the equipment used in the measurement is as follows:
[0239] -Haze measuring equipment: Haze meter NDH5000, manufactured by Nippon Denshoku Industries
[0240] --Polymerization Initiator--
[0241] A polymerization initiator is a material that can generate active species such as free radicals or cations by light energy or heat energy, and initiate polymerization of a polymerizable compound. As the polymerization initiator, one or more known free radical polymerization initiators, cationic polymerization initiators, base generators, etc. can be used alone or in combination, and preferably a photo-free radical polymerization initiator is used.
[0242] As the photoradical polymerization initiator, a photoradical generator can be used. For example, a photoradical polymerization initiator such as Michler's ketone or benzophenone, which has a trade name such as Irgacure or Darocur, can be suitably used. More specifically, compounds include benzophenone and acetophenone derivatives, such as α-hydroxy- or α-aminoacetophenone, 4-aroyl-1,3-dioxolane, benzyl ketal, 2,2-diethoxyacetophenone, p-dimethylaminoacetophenone, p-dimethylaminopropiophenone, benzophenone, 2-dichlorobenzophenone, pp'-dichlorobenzophenone, pp'-bisdiethylaminobenzophenone, Michler's ketone, biphenyl, benzoin, benzyl dimethyl ketal, tetramethylthiuram monosulfide, thioxanthone, 2-chlorothioxanthone, 2-methyl Thioxanthone, azobisisobutyronitrile, benzoyl peroxide, di-tert-butyl peroxide, 1-hydroxycyclohexyl phenyl ketone, 2-hydroxy-2-methyl-1-phenyl-1-one, 1-(4-isopropylphenyl)-2-hydroxy-2-methylpropane-1-one, methyl benzoylformate, benzoin isopropyl ether, benzoin methyl ether, benzoin ethyl ether, benzoin ether, benzoin isobutyl ether, benzoin n-butyl ether, benzoin n-propyl, 1-hydroxy-cyclohexyl-phenyl-ketone, 2-benzyl-2-dimethylamino-1-(4-morpholinophenyl)-butanone-1, 1-hydroxy-cyclohexyl-phenyl-ketone, 2,2-dimethoxy-1,2-diphenylethane-1-one, bis(η 5 -2,4-cyclopentadien-1-yl)-bis(2,6-difluoro-3-(1H-pyrrol-1-yl)-phenyl)titanium (bis(1-(2,4-difluorophenyl)-3-pyrrolyl) titanocene, bis(2,4,6-trimethylbenzoyl)-phenylphosphine oxide, 2-methyl-1[4-(methylthio)phenyl]-2-morpholinopropane-1-one, 2-hydroxy-2-methyl-1-phenyl-propane-1-one (Dar ocur1173), bis(2,6-dimethoxybenzoyl)-2,4,4-trimethyl-pentylphosphine oxide, 1-[4-(2-hydroxyethoxy)-phenyl]-2-hydroxy-2-methyl-1-propane-1-one monoacylphosphine oxide, bisacylphosphine oxide or titanocene, fluorescein, anthraquinone, thioxanthone or xanthone, rofenine dimer, trihalomethyl compound or dihalomethyl compound, active ester compound, organic boron compound, etc.
[0243] Furthermore, a photo-crosslinking radical initiator such as a diazide may be simultaneously contained. When the polymerization is performed only by heat, a thermal polymerization initiator such as azobisisobutyronitrile (AIBN), which is a common radical initiator, may be used.
[0244] In order to obtain a sufficient curing speed, the content of the polymerization initiator when the total mass of the polymerizable compound is 100.0 mass% is preferably 0.05 mass% to 10.0 mass%, more preferably 0.5 mass% to 5.0 mass%.
[0245] -Physical properties of liquid composition-
[0246] From the viewpoint of operability when adding the liquid composition, the viscosity of the liquid composition at 25°C is preferably 1.0 MPa·s or more and 150.0 MPa·s or less, more preferably 1.0 MPa·s or more and 30.0 MPa·s or less, and most preferably 1.0 MPa·s or more and 25.0 MPa·s or less. When the viscosity of the liquid composition is made to be 1.0 MPa·s or more and 30.0 MPa·s or less, even when the liquid composition is applied to an inkjet method, good ejection properties can be obtained. Here, the viscosity can be measured, for example, using a viscometer (equipment name: RE-550L, manufactured by Toki Industry Co., Ltd.) or the like.
[0247] 《Method for producing a laminate for a battery》
[0248] The manufacturing method of the battery stack of this embodiment includes: an insulating layer forming step of imparting a liquid composition to a first electrode to form an insulating layer; and an electrode setting step of setting a second electrode on the first electrode formed with the insulating layer, and the insulating layer forming step and the electrode setting step are implemented by a series of conveyances.
[0249] Here, "on the first electrode" means "on the current collector" or "on the electrode composite material layer", or both.
[0250] For example, when the first electrode is formed only of a current collector, an insulating layer is formed on the current collector. In addition, when the first electrode is formed of a current collector and an electrode composite material layer formed on the current collector, the insulating layer may be formed only on the electrode composite material layer, or the insulating layer may be formed on the current collector exposed from the electrode composite material layer and on the electrode composite material layer.
[0251] In this way, by using a series of conveyances to implement the insulating layer forming process and the electrode setting process, the occurrence of damage to the battery stack during the electrode manufacturing process can be suppressed. That is, since the insulating layer is a component that is easily damaged by cracks, it is preferred to set the second electrode on the insulating layer at an early stage after the insulating layer is formed. By using a series of conveyances to implement the insulating layer forming process and the electrode setting process, the second electrode can be set on the insulating layer at an early stage after the insulating layer is formed, so the second electrode functions as a protective component for protecting the insulating layer, and the occurrence of damage to the battery stack can be suppressed.
[0252] In addition, in the present specification and claims, the so-called "series of conveyances" ("conveyance series") refers to a process implemented by one conveyance, for example, in the case where the first electrode is conveyed by winding, it means that the insulating layer forming process and the setting process are implemented in one conveying process. In addition, from the viewpoint of suppressing the occurrence of damage to the battery stack, the case where the setting process is immediately implemented after the conveyance including the insulating layer forming process that can show its effect can also be taken as its object. In addition, the "roller conveyance" mentioned here is a method of conveying while applying tension between the conveyance start point and the conveyance end point, and the conveying object component can also be supported by supporting components such as guide wheels as needed. Roller conveying includes but is not limited to roller-to-roller conveying. Roller conveying also includes, for example, a case where the conveying object component is wound into a roll at the conveyance start point and the conveyance object component is not wound into a roll at the conveyance end point.
[0253] In addition, when the first electrode is transported using a conveyor belt, whether the conveyor belt is one or multiple is not used as a basis for determining whether it is a series of transport. For example, even if there are multiple conveyor belts, the case where the first electrode moves continuously from one conveyor belt to another conveyor belt also belongs to a series of transport.
[0254] The manufacturing method of the battery stack of this embodiment may include, as required, an electrode composite material layer forming step of forming an electrode composite material layer on a current collector, an irradiation step of irradiating a liquid composition with active energy rays, a removal step of removing a solvent contained in the liquid composition, an electrode processing step of processing the electrode into a battery cell after setting a second electrode, etc. In this case, for example, as long as the irradiation step is a series of steps with the insulating layer forming step and the setting step, the irradiation step may also be performed between the insulating layer forming step and the electrode setting step.
[0255] In addition, it is preferred that the first electrode is a negative electrode and the second electrode is a positive electrode. When the positive electrode is provided on the negative electrode, no useless area is generated in each electrode, productivity can be improved, and thus it is preferred. In addition, it is also preferred from the viewpoint of being able to improve the safety of the battery.
[0256] <Insulating layer forming step>
[0257] The insulating layer forming step is a step of forming an insulating layer composed of an organic layer and / or an inorganic layer on the object to be applied as the first electrode. The insulating layer forming step includes a step of adding a liquid composition to the object to be applied as the first electrode to form a liquid composition layer for forming an insulating layer, and may also include an irradiation step of irradiating the liquid composition with active energy rays, a removal step of removing the solvent contained in the liquid composition, etc. As the insulating layer, from the viewpoint of lightness and imparting functions by temperature changes, an organic layer is preferred, and from the viewpoint of firmness and heat resistance, an inorganic layer is preferred.
[0258] In the insulating layer forming step, the insulating layer may also be formed to have Fig.10 The shape having a concave-convex pattern including concave portions and convex portions as shown. In this case, the convex portion is preferably formed outside the region where the second electrode is provided. Fig.10 In the example of FIG. 1 , the thick film region 11 b of the insulating layer is a convex portion, and the thin film region 11 a of the insulating layer exposed inside the thick film region 11 b is a concave portion.
[0259] <Step of providing liquid for forming insulating layer>
[0260] The insulating layer forming liquid application step is a step of applying an insulating layer forming liquid composition containing an organic and / or inorganic compound and a solvent or a dispersion liquid to a target object serving as the first electrode.
[0261] The liquid composition imparted preferably forms a liquid composition layer as a liquid film of the liquid composition on the imparted object. As a method for imparting the liquid composition, there is no particular limitation, for example, spin coating, casting, micro-gravure coating, gravure coating, rod coating, roller coating, wire rod coating, dip coating, slit coating, capillary coating, spray coating, nozzle coating, gravure printing, screen printing, flexographic printing, offset printing, reverse printing, inkjet printing and other various printing methods can be cited. Wherein, from the viewpoint of being able to control the position of imparting the liquid composition, preferably the liquid ejection method such as inkjet printing.
[0262] <Irradiation process>
[0263] The irradiation step is a step of irradiating the liquid composition provided in the liquid providing step with active energy rays. In particular, in the case of a liquid composition that causes polymerization-induced phase separation, the irradiation step increases the porosity of the porous resin, i.e., the insulating layer, which is finally produced, thereby, for example, improving the absorbency of fluids such as liquids or gases in the porous resin. Specifically, by irradiating the liquid composition with active energy rays, a porous precursor having a porous structure is formed, and the porous structure is the basis for forming a porous resin having a high porosity.
[0264] The active energy ray is not particularly limited as long as it is a ray that can impart the energy required to promote the polymerization reaction of the polymerizable compound, and examples thereof include ultraviolet rays, electron beams, α rays, β rays, γ rays, and X-rays. Among them, ultraviolet rays are preferred. In addition, when a high-energy light source is used, a polymerization reaction can be initiated even without using a polymerization initiator.
[0265] The reason why the porous precursor is formed by the irradiation step will be described below, limited to the case where the liquid composition undergoes polymerization-induced phase separation.
[0266] As described above, when a porous resin is formed by polymerization-induced phase separation, the structure, properties, etc. of the porous resin vary depending on the polymerization conditions. For example, when a porous resin is formed under conditions in which polymerization of a polymerizable compound is promoted by irradiating a liquid composition with active energy rays having a strong irradiation intensity, polymerization continues until phase separation occurs sufficiently, and thus there is a tendency that it is difficult to produce a porous resin having a high porosity.
[0267] Therefore, in order to form a porous resin with a high porosity, the irradiation intensity of the active energy ray should not be set too high. Specifically, the irradiation intensity of the active energy ray is preferably 1 W / cm 2 Below, more preferably 300mW / cm 2 Below, most preferably 100mW / cm 2 However, if the irradiation intensity of the active energy ray is too low, phase separation will proceed excessively, which will easily lead to uneven and coarse porous structures. Furthermore, the irradiation time will also be prolonged, and the production efficiency will be reduced. Therefore, it is preferably 10 mW / cm 2 More preferably, 30 mW / cm 2 above.
[0268] <Removal process>
[0269] The removal step is a step of removing the solvent or dispersion from the liquid composition. The method for removing the solvent or dispersion is not particularly limited, and an example thereof is a method of removing the solvent or dispersion from the porous resin by heating. In this case, heating under reduced pressure can further promote the removal of the solvent or dispersion, and can suppress the solvent or dispersion from remaining in the formed insulating layer, which is preferred.
[0270] <Electrode installation process>
[0271] The electrode setting process is to form an insulating layer on the first electrode, such as Fig.12 The process of setting the second electrode is shown in FIG. Fig.12In the figure, 9 represents the collector of the first electrode, 11b represents the thick film region of the insulating layer, 12 represents the collector of the second electrode, and 13 represents the active material of the second electrode. There is no particular limitation on the method for setting the second electrode, but if the setting region is not in an appropriate position, a short circuit will occur between the first electrode and the second electrode. Therefore, the electrode setting process preferably includes an alignment process for adjusting the setting position of the second electrode after forming the insulating layer on the first electrode. In addition, in order to prevent offset after the second electrode is set, an adhesive or a viscous material may be applied to the first electrode and / or the second electrode before the second electrode is set.
[0272] <Electrode composite material layer forming step>
[0273] The electrode composite material layer forming step is a step of forming an electrode composite material layer on a target object as a first electrode. The electrode composite material layer forming step includes a step of imparting a liquid composition layer for forming an electrode composite material layer to the target object as a first electrode, and a step of removing a solvent contained in the liquid composition.
[0274] <Step of providing liquid for forming electrode composite material layer>
[0275] The electrode composite material layer formation liquid process is to give the electrode composite material layer formation liquid composition containing powdered active material, catalyst composition, dispersion liquid, etc. to the object to be given as the first electrode. The liquid composition given preferably forms a liquid composition layer as a liquid film of the liquid composition on the object to be given. As a method for giving the liquid composition, there is no particular limitation, for example, spin coating, casting, micro-gravure coating, gravure coating, rod coating, roller coating, wire rod coating, dip coating, slit coating, capillary coating, spray coating, nozzle coating, gravure printing, screen printing, flexographic printing, offset printing, reverse printing, inkjet printing and other various printing methods can be cited. Wherein, from the viewpoint of being able to control the position of the liquid composition, liquid ejection methods such as inkjet printing are preferred.
[0276] <Transportation process>
[0277] The conveying process is a process of conveying the first electrode. As the conveying process, from the viewpoint that damage to the first electrode or the insulating layer caused by friction between the first electrode or the insulating layer and the conveying device can be suppressed by reducing the contact area between the first electrode or the insulating layer and the conveying device in the conveying process, winding and conveying without using a conveyor belt for conveying is preferred.
[0278] <Electrode processing>
[0279] The electrode processing step is a step of processing the first electrode after the insulating layer forming step. In the electrode processing step, for example, in the first electrode provided with the second electrode, the first electrode can be cut to produce an electrode stack in which the second electrode is provided on the first electrode formed with the insulating layer. In the electrode processing step, it is preferred to cut the first electrode in such a way that the area of the first electrode is larger than the area of the second electrode. Thus, it is possible to prevent the end of the cut first electrode from short-circuiting with the end of the second electrode.
[0280] When the insulating layer includes a material having a melting point or a glass transition point, in the electrode processing step, for example, a plurality of electrode stacks are prepared in which a second electrode is provided on a first electrode having an insulating layer, and one electrode stack and another electrode stack are bonded together by heating at least a portion. Fig.10 In the case of the thick film region 11 b of the insulating layer shown in the figure, the electrode stacks located above and below may be arranged to face each other, and the thick film regions of the facing electrode stacks may be heat-bonded to each other.
[0281] In the electrode processing step, for example, the first electrode provided with the second electrode may be stacked or rolled up to produce a stacked body or a rolled up body. When the first electrode provided with the second electrode is stacked or rolled up, the first electrode may be cut at an appropriate timing.
[0282] As a lamination method, there can be mentioned a method of cutting a first electrode provided with a second electrode into a plurality of sheets to produce a plurality of electrode laminates, and laminating the plurality of electrode laminates. Fig.13 As shown, a method of stacking the first electrode and the second electrode at a certain distance in a folded manner to form a pleated structure (accordion structure) can be cited. Fig.13 In the figure, 9 denotes a current collector of the first electrode, 11b denotes a thick film region of the insulating layer, 12 denotes a current collector of the second electrode, and 13 denotes an active material of the second electrode.
[0283] For example, the coiling can be done using Figure 2 That is, the second electrode 6 can be fed with a rolled second electrode by the second electrode conveying device 4b on the first electrode 6 being conveyed, and the second electrode can be continuously laminated on the first electrode 6, and then wound up by the electrode processing unit 500 located in the rear half of the electrode setting part 400.
[0284] In addition, when the number of layers stacked as a zigzag structure or the number of turns wound as a roll structure reaches a target number, a target stacked body or roll can be obtained by cutting.
[0285] In addition, the electrode processing step may be implemented between the insulating layer forming step and the electrode setting step. That is, the electrode setting step may be implemented immediately after the electrode processing step. For example, in the electrode processing step, the first electrode before the second electrode is set may be cut, and the electrode setting step may be implemented immediately after cutting. Here, the so-called immediately means that the electrode processing step and the electrode setting step are in a series of steps, and between the electrode processing step and the electrode setting step, the cut first electrode will not be temporarily moved to another place, etc. That is, the electrode processing step is provided between the insulating layer forming step and the electrode setting step, and the electrode setting step is implemented immediately after the electrode processing step, which is included in the series of conveyances of the present invention. The flow of the steps described here can be, for example, as follows Figure 3 The battery shown is realized by a manufacturing apparatus for a laminate (described later).
[0286] In addition, the electrode processing step may be performed between the insulating layer forming step and the electrode setting step, and the second electrode processing step may be performed after the electrode setting step. For example, an electrode stack having a second electrode provided on the insulating layer of the cut first electrode may be stacked in the second electrode processing step. Alternatively, an electrode stack having a plurality of second electrodes provided on the insulating layer of the cut first electrode may be wound up in the second electrode processing step.
[0287] By performing the electrode setting step immediately after the electrode processing step, the second electrode can be provided on the insulating layer at an early stage after the insulating layer is formed. Therefore, the second electrode functions as a protective member for protecting the insulating layer, and the occurrence of damage to the battery stack can be suppressed.
[0288] 《Equipment for producing laminated body for battery》
[0289] The manufacturing apparatus of the battery laminate of this embodiment includes an insulating layer forming unit for applying a liquid composition to a first electrode to form an insulating layer, and an electrode setting unit for setting a second electrode on the first electrode formed with the insulating layer, and the insulating layer forming unit and the electrode setting unit are arranged in a series of conveying areas for conveying the first electrode. In addition, the manufacturing apparatus of the battery laminate of this embodiment may include an irradiation unit for irradiating the liquid composition with active energy rays, a removal unit for removing the solvent contained in the liquid composition, an electrode processing unit for processing the electrode into a battery cell after setting the second electrode, etc. as needed.
[0290] Reference Figures 1 to 9 The details of the manufacturing apparatus of the battery laminate are described. Figure 1 It is a schematic diagram showing an example of an apparatus for producing a laminated body for a battery.
[0291] The battery stack manufacturing device 1, which is an example of a manufacturing device for a battery stack, is a device for manufacturing an electrode using the liquid composition. The battery stack manufacturing device 1 includes: an insulating layer forming unit 600 composed of a liquid imparting unit 100 that imparts a liquid composition 7 to form an insulating layer on a first electrode 6; an electrode setting unit 400 that sets a second electrode on the formed insulating layer through a series of conveying implementations; and a control unit 800 that controls the insulating layer forming unit 600 and the electrode setting unit 400. The battery stack manufacturing device 1 also has a winding unit 8. In the case where the battery stack manufacturing device 1 has a plurality of winding units 8, a part or all of the winding units 8 can also be controlled to rotate by the control unit 800, and the first electrode 6 can be conveyed at a predetermined speed to function as a conveying unit. In addition, a part of the winding unit 8 can also function as a guide wheel of a supporting member.
[0292] In addition, a schematic diagram of an example of a manufacturing apparatus for a battery laminate is shown below. Figure 2 to Figure 7 As shown, in addition to the structure shown in the battery stack manufacturing device 1, it can also have: an irradiation unit 200, which implements the process of activating the polymerization initiator in the liquid composition and obtaining the insulating layer by polymerization of the polymerizable compound; a removal unit 300, which implements the process of heating the liquid composition to remove the solvent; an electrode processing unit 500, which processes the electrode into a battery cell after setting the second electrode, etc. The irradiation unit 200, the removal unit 300 and the electrode processing unit 500 are controlled by the control unit 800. In addition, as Figure 6 and Figure 7 The battery laminate production apparatus shown can apply the liquid composition to both surfaces of the first electrode 6 .
[0293] <Insulating layer forming unit>
[0294] The insulating layer forming unit 600 includes at least a liquid applying unit 100, and may include an irradiation unit 200 and / or a removal unit 300 as required. The insulating layer forming unit 600 may also form the insulating layer to have a Fig.10 The shape of the concavo-convex pattern including concave portions and convex portions is shown. At this time, it is preferred that the convex portion is formed outside the region where the second electrode is provided.
[0295] <Liquid application unit>
[0296] The liquid imparting unit 100 comprises: a printing device 1a for implementing an imparting process of imparting a liquid composition to the first electrode 6; a storage container 1b for storing the liquid composition; and a supply pipe 1c for supplying the liquid composition stored in the storage container 1b to the printing device 1a.
[0297] The storage container 1b stores the liquid composition 7, and the liquid applying unit 100 ejects the liquid composition 7 from the printing device 1a, and applies the liquid composition 7 to the first electrode 6 to form a thin film of the liquid composition layer. In addition, the storage container 1b may be a structure integrated with the battery laminate manufacturing device 1, or a structure detachable from the battery laminate manufacturing device 1. In addition, it may be a container for applying to a storage container integrated with the battery laminate manufacturing device 1 or a storage container detachable from the battery laminate manufacturing device 1.
[0298] The printing device 1a is not particularly limited as long as it can impart the liquid composition 7. For example, any printing device corresponding to various printing methods such as spin coating, cast film, micro-gravure coating, gravure coating, rod coating, roller coating, wire rod coating, dip coating, slit coating, capillary coating, spray coating, nozzle coating, gravure printing, screen printing, flexographic printing, offset printing, reverse printing, and inkjet printing can be used.
[0299] The storage container 1b and the supply pipe 1c may be arbitrarily selected as long as they can stably store and supply the liquid composition 7. The material constituting the storage container 1b and the supply pipe 1c preferably has light-shielding properties in the shorter wavelength region of ultraviolet light and visible light. Thus, when the liquid composition 7 contains a polymerizable compound, polymerization can be prevented from being initiated by external light.
[0300] <Irradiation unit>
[0301] The irradiation unit 200 is, for example, Figure 5 As shown, there are light irradiation devices 2a for polymerizing polymerizable compounds by irradiating active energy rays such as heat and light to the liquid composition, and polymerization inert gas circulation devices 2b for circulating polymerization inert gas. When the liquid composition formed by the liquid applying unit 100 contains a polymerizable compound, the light irradiation device 2a irradiates light in the presence of polymerization inert gas to form an insulating layer.
[0302] Light irradiation device 2a is suitably selected according to the absorption wavelength of the photopolymerization initiator contained in the liquid composition layer, as long as it is a device that can initiate and make the compound in the liquid composition layer continue to polymerize, it is not particularly limited, for example, ultraviolet light sources such as high pressure mercury lamp, metal halide lamp, hot cathode tube, cold cathode tube, LED, etc. can be cited. However, since the shorter the wavelength of light is, the more it tends to easily reach the deep part, it is preferred to select the light source according to the thickness of the porous film formed.
[0303] Next, the polymerization inert gas circulation device 2b plays the role of reducing the concentration of polymerization-active oxygen contained in the atmosphere, so that the polymerization reaction of the polymerizable compound near the surface of the liquid composition layer proceeds unhindered. Therefore, the polymerization inert gas used is not particularly limited as long as it satisfies the above functions, and examples thereof include nitrogen, carbon dioxide, argon, etc.
[0304] In addition, as the flow rate of the polymerization inert gas, in consideration of effectively obtaining the inhibitory reduction effect, the O2 concentration is preferably less than 20% (an environment with an oxygen concentration lower than that of the atmosphere), more preferably 0% to 15%, and most preferably 0% to 5%.
[0305] In order to realize stable polymerization progress conditions, the polymerization inert gas circulation device 2b is preferably provided with a temperature regulating device capable of regulating the temperature.
[0306] <Exclude unit>
[0307] Remove unit 300, e.g. Figure 4 As shown, a heating device 3a is provided, and the residual solvent in the formed insulating layer is heated, dried and removed by the heating device 3a. The removal unit 300 may also perform the solvent removal process under reduced pressure.
[0308] In addition, the removal unit 300 may remove the photopolymerization initiator remaining in the insulating layer by heating and drying it with the heating device 3 a .
[0309] The heating device 3a is not particularly limited as long as it satisfies the above-mentioned functions, and examples thereof include an IR heater and a hot air heater.
[0310] Furthermore, the heating temperature and the heating time may be appropriately selected according to the boiling point of the solvent contained in the insulating layer and the thickness of the film to be formed.
[0311] <Electrode installation unit>
[0312] The electrode setting unit 400 is as follows Figure 1 to Figure 7 As shown, there is a second electrode container 4a, and the second electrode is set on the insulating layer formed on the first electrode by the second electrode conveying device 4b. The second electrode container 4a can be a wound electrode or a sheet electrode. In addition, the second electrode conveying device 4b is not particularly limited as long as it can convey the electrode, and for example, a device that uses an adsorption mechanism to implement the conveyance can be cited. The electrode setting unit 400 can also have an alignment mechanism that is equipped with a camera or the like to adjust the setting position of the second electrode as needed.
[0313] <Electrode processing unit>
[0314] The electrode processing unit 500 processes the first electrode having the insulating layer formed thereon. Figure 2 As shown, there is an electrode processing device 5. The electrode processing unit 500, for example, winds up or stacks a first electrode provided with a second electrode. In addition, the electrode processing unit 500 cuts the first electrode in the first electrode provided with the second electrode. At this time, the electrode processing unit 500 preferably cuts in a manner that the area of the first electrode is larger than the area of the second electrode. Thereby, it is possible to prevent the end of the cut first electrode from short-circuiting with the end of the second electrode. In the case of winding or stacking the first electrode provided with the second electrode, the electrode processing unit 500 can cut the first electrode at an appropriate time.
[0315] In the case where the insulating layer includes a material having a melting point or a glass transition point, the electrode processing unit 500, for example, produces a plurality of electrode stacks in which a second electrode is provided on a first electrode having an insulating layer, and heats one electrode stack and another electrode stack to bond at least a portion thereof. The electrode processing unit 500 may also cut the first electrode before providing the second electrode. In this case, the second electrode processing unit may be provided after providing the second electrode for lamination or winding.
[0316] In this way, the electrode processing unit 500 can perform electrode cutting, wrinkling, lamination or winding of the first electrode, thermal bonding between the first electrodes after lamination or winding, etc. according to the target battery form.
[0317] <Control unit>
[0318] Figure 8 This is an example of the main hardware block diagram of the control unit. Figure 8 As shown, the control unit 800 includes, for example, a CPU 801 , a ROM 802 , a RAM 803 , an NVRAM 804 , an ASIC 805 , an I / O 806 , and an operation panel 807 .
[0319] The CPU 801 controls the battery stack manufacturing device as a whole. The ROM 802 stores the program executed by the CPU 801 and other fixed data. The RAM 803 temporarily stores data related to the manufacture of the battery stack, etc. The NV RAM 804 is a non-volatile memory for maintaining data even when the power supply of the device is cut off. The ASIC 805 processes input and output signals for controlling image processing and other devices as a whole. The I / O 806 is an interface for inputting and outputting signals with the insulating layer forming unit 600, the electrode setting unit 400, etc. The operation panel 807 inputs and displays information required by the control unit 800.
[0320] Fig. 9 This is an example of a main functional block diagram of a control unit. Fig. 9As shown, the control unit 800 has an insulating layer forming control unit 851, an electrode setting control unit 852, and an electrode processing control unit 853 as functional blocks.
[0321] The insulating layer forming control unit 851 controls the insulating layer forming unit 600. For example, the insulating layer forming control unit 851 issues a command for controlling the time and amount of the liquid composition to be applied to the liquid applying unit 100. For example, in the case of forming the insulating layer by inkjet printing, the insulating layer forming control unit 851 issues a command to the liquid applying unit 100 to apply the liquid composition in a manner of predetermined waveform information, ejection times and other ejection conditions, and predetermined time and number of liquid droplets.
[0322] In addition, for example, the insulating layer formation control unit 851 issues a command to the irradiation unit 200 for controlling the time, irradiation amount, etc. when the active energy line is irradiated to the liquid composition. In addition, for example, the insulating layer formation control unit 851 issues a command to the removal unit 300 for controlling the time, heating amount, etc. when the solvent remaining in the insulating layer is heated to dry and remove it.
[0323] The electrode setting control unit 852 issues instructions to the electrode setting unit 400 for controlling the time of adsorbing the electrode, the speed of conveying the adsorbed electrode, etc. In the case where the electrode setting unit 400 has an alignment mechanism, the electrode setting control unit 852 controls the alignment mechanism to adjust the setting position of the second electrode based on the position information from an image sensor such as a camera.
[0324] For example, when cutting the first electrode using a laser, the electrode processing control unit 853 issues a command to the electrode processing unit 500 to control the amount of light emitted by the laser or to scan the laser based on position information from an image sensor such as a camera. In addition, for example, the electrode processing control unit 853 issues a command to the electrode processing unit 500 to control the start time and end time of zigzag folding, lamination, winding, etc. of the first electrode. In addition, for example, the electrode processing control unit 853 issues a command to the electrode processing unit 500 to control the heating temperature or heating time when thermal bonding, etc. between the first electrodes after lamination or winding is performed.
[0325] Hereinafter, the battery and the like will be described in more detail by way of Examples and Comparative Examples, but the present invention includes but is not limited to the following Examples.
[0326] [Example]
[0327] First, the negative electrode and the positive electrode used in each example and each comparative example were produced.
[0328] <Production of negative electrode>
[0329] For the formation of the negative electrode composite material layer, 97.0 mass% of graphite, 1.0 mass% of thickener (carboxymethyl cellulose), 2.0 mass% of polymer (styrene butadiene rubber), and 100.0 mass% of water as a solvent were added to prepare the negative electrode coating. The negative electrode coating was applied to both sides of the copper foil substrate and dried to obtain a negative electrode composite material layer with a unit area weight of 9.0 mg / cm on one side. 2 Then, the negative electrode was pressed using a roller press to obtain a volume density of 1.6 g / cm 3 At this time, the total film thickness of the negative electrode was 112.0 μm.
[0330] <Production of positive electrode>
[0331] As the positive electrode active material, 92.0% by mass of lithium nickel oxide (NCA), 3.0% by mass of acetylene black as a conductive material, and 5.0% by mass of polyvinylidene fluoride (PVDF) as a binder were prepared and dispersed in N-methylpyrrolidone (NMP) to make a positive electrode coating. The positive electrode coating was applied to both sides of the aluminum foil substrate and dried to obtain a positive electrode composite material layer with a unit area weight of 15.0 mg / cm on one side. 2 Next, the electrode was pressed using a roller press to a volume density of 2.8 g / cm 3 , and the positive electrode to be used was obtained. At this time, the total film thickness of the positive electrode was 132.0 μm. Finally, the positive electrode was punched out using a die punching machine (punching area: 47.0 mm×27.0 mm).
[0332] [Example 1]
[0333] - Adjustment of the insulating layer forming liquid composition -
[0334] The materials were mixed in the following proportions to prepare a liquid composition for forming an insulating layer: 29.0% by mass of tricyclodecane dimethanol diacrylate (manufactured by Daicel-Allnex Co., Ltd.) as a polymerizable compound A, 70.0% by mass of dipropylene glycol monomethyl ether (manufactured by Kanto Chemical Industry Co., Ltd.) as a solvent (porogen), and 1.0% by mass of Irgacure 184 (manufactured by BASF Corporation) as a polymerization initiator were mixed to obtain a liquid composition for forming an insulating layer.
[0335] <Formation of insulating layer and provision of second electrode>
[0336] use Figure 6 The battery laminate production apparatus shown here forms an insulating layer and provides a second electrode.
[0337] -Formation of insulating layer-
[0338] First, the liquid composition for forming the functional layer is filled into the die coating printing device. As the negative electrode of the first electrode, a coiled material with a collector width of 60 mm and a composite material layer width of 50 mm is prepared. For the negative electrode transported at 50 mm / sec, the ejection amount of the liquid composition is controlled to form an insulating layer with a film thickness of 20.0 μm on both sides of the negative electrode composite material layer. Then, the coating area is immediately UV irradiated in a N2 atmosphere (light source: UV-LED (manufactured by Phoseon, trade name: FJ800), wavelength: 365 nm, irradiation intensity: 30 mW / cm 2 , irradiation time: 20s) to solidify it.
[0339] Next, the cured product was heated at 120° C. for 1 minute using a hot air drying oven to remove the solvent, thereby obtaining a first electrode with an insulating layer.
[0340] - Arrangement of the second electrode -
[0341] After forming the insulating layer, the positive electrode was placed as the second electrode on the insulating layer (thin film region) of the first electrode with the insulating layer. Then, the first electrode with the insulating layer provided with the second electrode was cut into a size of 60.0 mm×30.0 mm to obtain a first electrode group.
[0342] [Evaluation 1: Film impact resistance test]
[0343] The obtained first electrode group was subjected to strength test according to the following evaluation steps 1-1 to 1-3. The results are as follows Fig.15 shown.
[0344] Step 1-1: Apply load
[0345] A pin was pressed from above onto the obtained first electrode group to apply a load.
[0346] In Comparative Examples 1 to 8, since the second electrode was not provided, the strength test was performed on the first electrode with an insulating layer without the second electrode, instead of the first electrode group.
[0347] Step 1-2: Preparation of the battery before electrolyte injection
[0348] In Comparative Examples 1 to 8, the positive electrodes were first stacked facing each other. The laminate was used as a sealing material to seal the laminate. Fig.14 The battery before filling with electrolyte is shown.
[0349] Step 1-3: Short circuit evaluation between positive and negative electrodes
[0350] For the obtained battery, a digital multimeter was used to check whether there was a short circuit between the positive and negative electrodes.
[0351] The short circuit determination criteria are based on the resistance value displayed by the digital multimeter, as shown below.
[0352] a: No short circuit (30MΩ or above)
[0353] b: There is a short circuit (less than 30MΩ)
[0354] [Evaluation 2: Battery drive confirmed]
[0355] The battery before the electrolyte injection obtained in Evaluation 1 was subjected to a battery driving test according to the following evaluation steps 2-1 to 2-2. However, if a short circuit was determined in Evaluation 1, Evaluation 2 was not carried out. The results are as follows: Fig.15 shown.
[0356] Step 2-1: Making the battery
[0357] The battery before the electrolyte injection obtained in Evaluation 1 was vacuum dried at 120°C for 12 hours, and the electrolyte was injected. At this time, the thick film region of the first electrode located above and below the stack was heated and bonded at the electrode end of Example 4 and Comparative Example 4. In addition, as the electrolyte, a solution obtained by adding LiPF6 as an electrolyte to a mixture of ethylene carbonate (EC) and dimethyl carbonate (DMC) (a mixture with a mass ratio of "EC: DMC = 1: 1") to a concentration of 1.5 mol / L was used.
[0358] Step 2-2: Determination of initial battery capacity
[0359] The positive and negative leads of the prepared battery were connected to the charge and discharge test device, and constant current and constant voltage charging was performed at a maximum voltage of 4.2V, a charge and discharge rate of 0.2C, and 5 hours. After charging, it was left to stand in a constant temperature chamber at 40°C for 5 days. Then, constant current discharge was performed to 2.5V at a charge and discharge rate of 0.2C. Then, constant current and constant voltage charging was performed at a maximum voltage of 4.2V, a charge and discharge rate of 0.2C, and 5 hours. After standing for 10 minutes, constant current discharge was performed to 2.5V at a charge and discharge rate of 0.2C. The discharge capacity at this time was taken as the initial capacity.
[0360] a: Confirm that the initial capacity is less than the theoretical capacity ±10%
[0361] b: Confirm that the initial capacity is ±10% or more of the theoretical capacity
[0362] [Comparative Example 1]
[0363] The first electrode having an insulating layer was obtained in the same manner as in Example 1 except that the arrangement of the second electrode in Example 1 was changed to the following steps. Then, evaluations 1 and 2 were carried out in the same manner as in Example 1. The results are shown in FIG. Fig.15 shown.
[0364] - Arrangement of the second electrode -
[0365] After the insulating layer is formed, the positive electrode is not provided as the second electrode, and the first electrode is cut into a size of 60.0 mm×30.0 mm to obtain the first electrode.
[0366] [Example 2]
[0367] The same operation as in Example 1 was performed except that the formation of the insulating layer in Example 1 was changed to the following steps to obtain a first electrode group with an insulating layer provided with a second electrode. Then, evaluations 1 and 2 were performed in the same manner as in Example 1. The results are as follows: Fig.15 shown.
[0368] -Formation of insulating layer-
[0369] use Figure 7 The insulating layer was formed and the second electrode was arranged using the manufacturing device shown in FIG. First, the liquid composition for forming the functional layer was filled into an inkjet ejection device equipped with a GEN5 head (manufactured by Ricoh Print Systems Co., Ltd.). Then, for the negative electrode, the ejection amount of the liquid composition was controlled to form the following on both sides of the negative electrode: Fig.11 The coating area of the insulating layer (thin film area) and the insulating layer (thick film area) in the shape of the image shown. The area of the insulating layer (thin film area) is 47.0 mm × 27.0 mm, and the film thickness is 20.0 μm. In addition, the film thickness of the insulating layer (thick film area) is 26.0 μm. Then, the coating area is immediately irradiated with UV (light source: UV-LED (manufactured by Phoseon, trade name: FJ800), wavelength: 365 nm, irradiation intensity: 30 mW / cm 2 The cured product was then heated at 120° C. for 1 minute using a hot air drying furnace to remove the porogen and obtain an insulating layer.
[0370] [Comparative Example 2]
[0371] The first electrode having an insulating layer was obtained in the same manner as in Example 2 except that the arrangement of the second electrode in Example 2 was changed to the following steps. Then, evaluations 1 and 2 were carried out in the same manner as in Example 1. The results are shown in FIG. Fig.15 shown.
[0372] - Arrangement of the second electrode -
[0373] After the insulating layer is formed, the positive electrode is not provided as the second electrode, and the first electrode is cut into a size of 60.0 mm×30.0 mm to obtain the first electrode.
[0374] [Example 3]
[0375] The same operation as in Example 1 was performed except that the formation of the insulating layer forming liquid composition in Example 1 was changed to the following steps to obtain a first electrode group with an insulating layer provided with a second electrode. Then, evaluations 1 and 2 were performed in the same manner as in Example 1. The results are as follows: Fig.15 shown.
[0376] -Formation of Liquid Composition for Forming Insulating Layer-
[0377] 39.0 mass % of EBECRYL 8402 (manufactured by Daicel-Allnex Co., Ltd.) as a polymerizable compound B, 60.0 mass % of diisobutyl ketone (manufactured by Kanto Chemical Industry Co., Ltd.) as a porogen, and 1.0 mass % of Irgacure 819 (manufactured by BASF Corporation) as a polymerization initiator were mixed to obtain a liquid composition for forming an insulating layer.
[0378] [Comparative Example 3]
[0379] The first electrode having an insulating layer was obtained in the same manner as in Example 3 except that the arrangement of the second electrode in Example 3 was changed to the following steps. Then, evaluations 1 and 2 were carried out in the same manner as in Example 1. The results are shown in FIG. Fig.15 shown.
[0380] - Arrangement of the second electrode -
[0381] After the insulating layer is formed, the positive electrode is not provided as the second electrode, and the first electrode is cut into a size of 60.0 mm×30.0 mm to obtain the first electrode.
[0382] [Example 4]
[0383] The same operation as in Example 3 was performed except that the formation of the insulating layer in Example 3 was changed to the following steps to obtain a first electrode group with an insulating layer provided with a second electrode. Then, evaluations 1 and 2 were performed in the same manner as in Example 1. The results are as follows: Fig.15 shown.
[0384] -Formation of insulating layer-
[0385] use Figure 7 The manufacturing apparatus shown implements the formation of the insulating layer and the provision of the second electrode.
[0386] The liquid composition for forming the functional layer was filled into an inkjet ejection device equipped with a GEN5 head (manufactured by Ricoh Print Systems Co., Ltd.). For the negative electrode, the ejection amount of the liquid composition was controlled to form the following on both sides of the negative electrode: Fig.11The coating area of the insulating layer (thin film area) and the insulating layer (thick film area) in the shape of the image shown. The area of the insulating layer (thin film area) is 47.0 mm × 27.0 mm, the film thickness is 20.0 μm, and the film thickness of the insulating layer (thick film area) is 26.0 μm. Then, the coating area is immediately irradiated with UV (light source: UV-LED (manufactured by Phoseon, trade name: FJ800), wavelength: 365 nm, irradiation intensity: 30 mW / cm 2 The cured product was then heated at 120° C. for 1 minute using a hot air drying furnace to remove the porogen and obtain an insulating layer.
[0387] [Comparative Example 4]
[0388] The first electrode having an insulating layer was obtained in the same manner as in Example 4 except that the arrangement of the second electrode in Example 4 was changed to the following steps. Then, evaluations 1 and 2 were carried out in the same manner as in Example 1. The results are shown in FIG. Fig.15 shown.
[0389] - Arrangement of the second electrode -
[0390] After the insulating layer is formed, the positive electrode is not provided as the second electrode, and the first electrode is cut into a size of 60.0 mm×30.0 mm to obtain the first electrode.
[0391] [Example 5]
[0392] The same operation as in Example 1 was performed except that the formation of the insulating layer forming liquid composition in Example 1 was changed to the following steps to obtain a first electrode group with an insulating layer provided with a second electrode. Then, evaluations 1 and 2 were performed in the same manner as in Example 1. The results are as follows: Fig.15 shown.
[0393] -Formation of Liquid Composition for Forming Insulating Layer-
[0394] Preparation of α-alumina (primary particle size (D50) of 0.5 μm, specific surface area of 7.8 g / m 2) 40.0 mass %, a mixed solution of dimethyl sulfoxide and ethylene glycol (DMSO-EG) 58.0 mass %, and MALIALIM HKM-150A (manufactured by NOF Corporation) as a dispersant 2.0 mass % were mixed to prepare a pre-dispersion liquid. The pre-dispersion liquid was placed in a container together with zirconium oxide beads (Φ2 mm), and a freezing nano-pulverizer NP-100 (manufactured by Thinky Co., Ltd.) was used to perform a dispersion treatment at 1500 rpm for 3 minutes to obtain a dispersion liquid. The zirconium oxide beads were removed from the obtained dispersion liquid using a 25 μm mesh filter to prepare an insulating layer forming liquid composition.
[0395] [Comparative Example 5]
[0396] The first electrode having an insulating layer was obtained in the same manner as in Example 5 except that the arrangement of the second electrode in Example 5 was changed to the following steps. Then, evaluations 1 and 2 were carried out in the same manner as in Example 1. The results are shown in FIG. Fig.15 shown.
[0397] - Arrangement of the second electrode -
[0398] After the insulating layer is formed, the positive electrode is not provided as the second electrode, and the first electrode is cut into a size of 60.0 mm×30.0 mm to obtain the first electrode.
[0399] [Example 6]
[0400] The same operation as in Example 1 was performed except that the formation of the insulating layer in Example 1 was changed to the following steps to obtain a first electrode group with an insulating layer provided with a second electrode. Then, evaluations 1 and 2 were performed in the same manner as in Example 1. The results are as follows: Fig.15 shown.
[0401] -Formation of insulating layer-
[0402] use Figure 7 The insulating layer was formed and the second electrode was arranged using the manufacturing apparatus shown in the figure. The liquid composition for forming the functional layer was filled into an inkjet ejection device equipped with a GEN5 head (manufactured by Ricoh Print Systems Co., Ltd.). For the negative electrode, the ejection amount of the liquid composition was controlled to form the following on both sides of the negative electrode: Fig.11 The coating area of the insulating layer (thin film area) and the insulating layer (thick film area) in the shape of the image shown. The area of the insulating layer (thin film area) is 47.0 mm × 27.0 mm, and the film thickness is 20.0 μm. In addition, the film thickness of the insulating layer (thick film area) is 26.0 μm. Then, the coating area is immediately irradiated with UV (light source: UV-LED (manufactured by Phoseon, trade name: FJ800), wavelength: 365 nm, irradiation intensity: 30 mW / cm2 The cured product was then heated at 120° C. for 1 minute using a hot air drying furnace to remove the porogen and obtain an insulating layer.
[0403] [Comparative Example 6]
[0404] The first electrode having an insulating layer was obtained in the same manner as in Example 6 except that the arrangement of the second electrode in Example 6 was changed to the following steps. Then, evaluations 1 and 2 were carried out in the same manner as in Example 1. The results are shown in FIG. Fig.15 shown.
[0405] - Arrangement of the second electrode -
[0406] After the insulating layer is formed, the positive electrode is not provided as the second electrode, and the first electrode is cut into a size of 60.0 mm×30.0 mm to obtain the first electrode.
[0407] like Fig.15 As shown, any embodiment received an evaluation of a in both evaluation 1 and evaluation 2. That is, Fig.15 The results show that by setting the second electrode, the impact resistance of the film is improved, and good battery characteristics are obtained. In addition, this result does not depend on the type of material forming the insulating layer, but only depends on whether the second electrode is set. That is, as long as it is a material that can form an insulating layer, whether the insulating layer is an organic material or an inorganic material, the impact resistance of the film can be improved by setting the second electrode, and good battery characteristics can be obtained.
[0408] In addition, it was also shown that when a polymerizable compound B with a low glass transition temperature (Tg) is used as the material of the insulating layer, by setting a second electrode and heating after stacking, it was confirmed that the thick film area of the first electrode located above and below the stack at the electrode ends was heated and bonded, resulting in a stacked body in which electrode deviation is unlikely to occur after stacking.
[0409] Furthermore, in recent years, demands for higher output, higher capacity, and longer life of power storage devices such as batteries and power generation devices such as fuel cells have been rapidly increasing.
[0410] To realize such a battery, high-quality battery components are required to improve the stable characteristics and safety of the element.
[0411] For example, in order to prevent uneven battery reaction, it is important that functional layers such as active materials and insulating layers present inside the battery have a film with uniform thickness.
[0412] Furthermore, in order to prevent the separator from being punctured inside the battery, it is important that burrs, which may cause puncture, are not generated at the edge of the electrode where various functional layers are formed.
[0413] Furthermore, in addition to achieving such high-quality battery components, having high production efficiency is also important.
[0414] In order to achieve high productivity, as in Patent Document 2, by adding a cutting or folding process for conveying a substrate or a setting process for opposing electrodes to a roll coating device for battery manufacturing, the efficiency of the battery production process is improved and the quality is improved.
[0415] However, when the cutting process is performed during roller conveyance, the contact between the conveyed component and the cutting blade easily causes distortion, wrinkles, and burrs to occur at the electrode end.
[0416] On the other hand, the quality of the electrode end can be improved by reducing the roller conveying speed during cutting, but there is a problem that the thickness of the functional film is uneven when applying due to the speed change during cutting, and there is room for improvement in terms of quality.
[0417] In this case, the manufacturing method of the battery component includes: a conveying step of conveying the first substrate while changing the speed of the first substrate; a functional film forming step of forming a functional film by ejecting a liquid composition onto the first substrate being conveyed by a liquid ejection method. If necessary, there may be an irradiation step of irradiating the liquid composition with active energy rays, a removal step of removing the solvent contained in the liquid composition, a substrate processing step of processing the substrate into a battery cell after setting a second substrate, etc.
[0418] <Functional film forming process>
[0419] The functional film forming step is a step of forming a functional film composed of a conductive layer or an insulating layer on a target object as a first base material.
[0420] The functional film forming step includes a liquid applying step of applying a liquid composition to a target object, which is a conductive layer substrate or an insulating layer substrate as a first substrate, to form a liquid composition layer.
[0421] Furthermore, the functional film forming step may include, as necessary, an irradiation step of irradiating the liquid composition with active energy rays, a removal step of removing a solvent contained in the liquid composition, and the like.
[0422] <Liquid application process>
[0423] The liquid application step is a step of applying a liquid composition containing an organic and / or inorganic compound, a solvent, a dispersion liquid, etc. to an object to be applied, which is the first substrate.
[0424] The applied liquid composition preferably forms a liquid composition layer as a liquid film of the liquid composition on the object to be applied.
[0425] As a method for applying the liquid composition, a liquid ejection method such as an inkjet printing method is preferred.
[0426] Thus, even when the first substrate is conveyed at a variable speed, the ejection cycle, ejection amount, etc. of the inkjet can be instantly changed, and a functional film with less uneven film thickness can be formed on the first substrate.
[0427] Therefore, it is preferable to change the signal for discharging the liquid composition in synchronization with the speed change of the conveying step, or the signals may be synchronized with each other.
[0428] <Irradiation process>
[0429] The irradiation step is a step of irradiating the liquid composition provided in the liquid providing step with active energy rays.
[0430] In particular, in the case of a liquid composition that causes polymerization-induced phase separation, the irradiation step increases the porosity of the porous resin, ie, the insulating layer, which is finally produced, thereby improving the absorption of fluids such as liquids and gases into the porous resin.
[0431] Specifically, by irradiating the liquid composition with active energy rays, a porous precursor having a porous structure which is a basis for forming a porous resin having a high porosity is formed.
[0432] The active energy ray is not particularly limited as long as it can impart energy required to promote the polymerization reaction of the polymerizable compound, and examples thereof include ultraviolet rays, electron beams, α rays, β rays, γ rays, and X rays, among which ultraviolet rays are preferred.
[0433] Furthermore, especially when a high-energy light source is used, a polymerization reaction can be initiated even without using a polymerization initiator.
[0434] The reason why the porous precursor is formed by the irradiation step will be described below, limited to the case where the liquid composition undergoes polymerization-induced phase separation.
[0435] As described above, when a porous resin is formed by polymerization-induced phase separation, the structure, properties, etc. of the porous resin vary depending on the polymerization conditions. For example, when a porous resin is formed under conditions in which polymerization of a polymerizable compound is promoted by irradiating a liquid composition with active energy rays having a strong irradiation intensity, polymerization continues until phase separation occurs sufficiently, and thus there is a tendency that it is difficult to produce a porous resin having a high porosity.
[0436] Therefore, in order to form a porous resin with a high porosity, the irradiation intensity of the active energy ray should not be set too high. Specifically, the irradiation intensity of the active energy ray is preferably 1 W / cm 2Below, more preferably 300mW / cm 2 Below, most preferably 100mW / cm 2 However, if the irradiation intensity of the active energy ray is too low, phase separation will proceed excessively, which will easily lead to uneven and coarse porous structures. Furthermore, the irradiation time will also be prolonged, and the production efficiency will be reduced. Therefore, it is preferably 10 mW / cm 2 More preferably, 30 mW / cm 2 above.
[0437] <Removal process>
[0438] The removal step is a step of removing the solvent or dispersion from the liquid composition. The method for removing the solvent or dispersion is not particularly limited, and an example thereof is a method of removing the solvent or dispersion from the porous resin by heating. In this case, heating under reduced pressure can further promote the removal of the solvent or dispersion, and can suppress the solvent or dispersion from remaining in the formed insulating layer, which is preferred.
[0439] <Substrate Setting Process>
[0440] The substrate setting step is performed in, for example, Fig. 27 On the first substrate having the functional film formed thereon, for example Fig.28 The process of setting the second substrate is shown.
[0441] Note that Fig. 27 and Fig.28 , mark 9 represents a current collector of a negative electrode as an example of a first substrate, mark 11a represents a thin film region of an insulating layer as an example of a functional film, mark 11b represents a thick film region of an insulating layer as an example of a functional film, mark 12 represents a current collector of a positive electrode as an example of a second substrate, and mark 13 represents an active material of a positive electrode as an example of a second substrate.
[0442] The method of providing the second substrate is not particularly limited, but if the area provided is not an appropriate area, a short circuit may occur between the first substrate and the second substrate.
[0443] Therefore, it is preferable that the substrate setting step includes an alignment step of adjusting the setting position of the second substrate after forming the insulating layer on the first substrate.
[0444] Here, in order to prevent displacement after the second substrate is provided, an adhesive or viscous material may be applied on the first substrate and / or the second substrate before the second substrate is provided.
[0445] <Base material processing step>
[0446] The substrate processing step is a step of processing the first substrate on which the functional film is formed, downstream of the functional film forming step.
[0447] The substrate processing step may include at least one of a cutting step, a folding step, and a bonding step.
[0448] In the substrate processing step, for example, after providing the second substrate, the first substrate may be cut to produce a substrate laminate in which the second substrate is provided on the first substrate on which the functional film is formed.
[0449] In the substrate processing step, the first substrate is preferably cut so that the area of the first substrate is larger than the area of the second substrate.
[0450] This can prevent a short circuit between the end portion of the cut first base material and the end portion of the second base material.
[0451] When the insulating layer contains a material having a melting point or a glass transition point, in the substrate processing step, for example, a plurality of substrate stacks are prepared in which a second substrate is arranged on a first substrate having an insulating layer formed thereon, and one substrate stack is at least partially bonded to another substrate stack by heating.
[0452] For example, in the functional film forming step, when the insulating layer is formed to have a concave-convex pattern including concave portions and convex portions, that is, when the base laminate has Fig.26 In the case of the thick film region 11 b of the insulating layer shown in the figure, the thick film regions of the upper and lower base laminates may be heat-bonded to each other.
[0453] In the substrate processing step, for example, the first substrate provided with the second substrate may be stacked or rolled up to produce a stacked body or a rolled body.
[0454] When the first substrate and the second substrate are wound or stacked, the first substrate may be cut at an appropriate timing.
[0455] Examples of the lamination method include a method of cutting the first substrate provided with the second substrate into a plurality of sheets to produce a plurality of substrate laminates, and laminating the plurality of substrate laminates, but the method is not limited thereto.
[0456] like Fig.29 As shown, another example of the lamination method includes, but is not limited to, a method of laminating the first substrate with the second substrate spaced therefrom so that the first electrode is folded in a zigzag structure.
[0457] exist Fig.29 , mark 9 represents a current collector of a negative electrode as an example of a first substrate, mark 11b represents a thick film region of an insulating layer as an example of a functional film, mark 12 represents a current collector of a positive electrode as an example of a second substrate, and mark 13 represents an active material of a positive electrode as an example of a second substrate.
[0458] For example, you can use Fig.18 The battery component manufacturing apparatus shown (described later) is used for this purpose.
[0459] That is, the second substrate conveying device 4 b can supply the rolled second substrate to the first substrate 6 being conveyed, and the second substrate can be continuously stacked on the first substrate 6 , and then wound up by the substrate processing unit 500 located in the latter half of the substrate setting unit 400 .
[0460] When the number of layers stacked in a zigzag structure or the number of turns wound as a roll structure reaches a predetermined number, a target stacked body or wound body can be obtained by cutting.
[0461] <Transportation process>
[0462] The conveying step is a step of conveying the first base material so as to perform various steps on the first base material.
[0463] In the conveying step, the first substrate can be conveyed at a variable speed.
[0464] Thus, even when a series of steps for manufacturing a battery component include a step of placing a second substrate on a first substrate and a substrate processing step such as cutting and creasing the first substrate, the accuracy of placement or processing can be improved.
[0465] Therefore, it is preferable that the conveying speed in the conveying step is changed according to the processing time of the base material processing step.
[0466] That is, it is preferable to change the speed according to the operations of the substrate processing step such as setting of the second substrate, cutting and wrinkling of the first substrate, etc.
[0467] The method for conveying the first substrate is not particularly limited, and examples thereof include conveying by a conveyor belt method, in addition to a take-up conveying method.
[0468] The roller conveyance referred to here is a method of conveying while applying tension between the conveyance start point and the conveyance end point, and the conveyance target member may be supported by a supporting member such as a guide wheel as necessary.
[0469] Roller conveying includes, but is not limited to, roller-to-roller conveying.
[0470] Roller conveyance also includes, for example, a case where the conveyance target member is wound into a roll at the conveyance start point and the conveyance target member is not wound into a roll at the conveyance end point.
[0471] As the speed change operation, for example, when the first substrate needs to be subjected to a process that interferes with conveyance of the first substrate, such as a cutting or bending process, it is preferable to decelerate from a predetermined speed and convey the first substrate at a speed slower than the predetermined speed.
[0472] By performing such a speed change operation, it is possible to suppress damage to the end portion of the base material even during the cutting or bending process.
[0473] Furthermore, after deceleration, it is preferred to accelerate to the original conveying speed after necessary processing steps such as cutting or bending steps that may interfere with conveying of the first substrate are performed.
[0474] By performing such an operation, productivity can be improved.
[0475] 《Equipment for manufacturing battery parts》
[0476] The manufacturing device of the battery component of this embodiment comprises: a conveying unit for conveying a first substrate; a functional film forming unit for forming a functional film by spraying a liquid composition onto the conveyed first substrate using a liquid spraying method; and a control unit for controlling the conveying unit, wherein the control unit controls the conveying speed of the conveying unit so that the first substrate is conveyed while changing speed.
[0477] In addition, the manufacturing method of the battery component of this embodiment may have an irradiation unit for irradiating the liquid composition with active energy rays, a removal unit for removing the solvent contained in the liquid composition, a substrate processing unit for processing the substrate into a battery cell after the second substrate is set, etc. as needed.
[0478] Reference Figure 16 to Figure 2 5 The details of the manufacturing apparatus for battery components will be described.
[0479] Fig.16 It is a schematic diagram showing an example of a battery component manufacturing apparatus.
[0480] The battery component manufacturing apparatus 1 as an example of a battery component manufacturing apparatus is an apparatus for manufacturing a battery component using the above-mentioned liquid composition.
[0481] The battery component manufacturing apparatus 1 includes a functional film forming unit 600 composed of a liquid applying unit 100 for applying a liquid composition on a first substrate to form a functional film.
[0482] The battery component manufacturing apparatus 1 may include a substrate processing unit 500 and the like.
[0483] As a schematic diagram of an example of an apparatus for manufacturing a battery component Figures 17 to 22 As shown, in addition to the processes described for the battery component manufacturing apparatus 1, a processing unit group may be provided, such as an irradiation unit 200 that performs a process of activating a polymerization initiator in a liquid composition to obtain an insulating layer by polymerization of a polymerizable compound, and a removal unit 300 that performs a process of heating the liquid composition to remove a solvent.
[0484] <Functional film forming unit>
[0485] The functional film forming unit 600 includes at least a liquid applying unit 100 , and may include an irradiation unit 200 and a removal unit 300 as necessary.
[0486] <Liquid application unit>
[0487] The liquid imparting unit 100 includes: an inkjet device 1a for implementing an imparting process of imparting a liquid composition onto a first substrate, a storage container 1b for storing the liquid composition, and a supply pipe 1c for supplying the liquid composition stored in the storage container 1b to the inkjet device 1a.
[0488] The storage container 1 b stores the liquid composition 7 , and the liquid applying unit 100 ejects the liquid composition 7 from the inkjet device 1 a to apply the liquid composition 7 onto the first substrate to form a thin film-like liquid composition layer.
[0489] In addition, the storage container 1 b may be a structure that is integrated with the battery component manufacturing apparatus 1 , or may be a structure that is detachable from the battery component manufacturing apparatus 1 .
[0490] Alternatively, the container may be a container for providing the battery to a storage container integrated with the battery laminate production apparatus 1 or a storage container detachable from the battery laminate production apparatus 1 .
[0491] The storage container 1 b and the supply pipe 1 c may be arbitrarily selected as long as they can stably store and supply the liquid composition 7 .
[0492] The material constituting the storage container 1 b and the supply pipe 1 c preferably has light-shielding properties in the shorter wavelength region of ultraviolet light and visible light.
[0493] Thus, when the liquid composition 7 contains a polymerizable compound, it is possible to prevent polymerization from being initiated by external light.
[0494] When the liquid applying step is performed in the liquid applying section 100 , it is preferred that the conveyance speed of the first substrate is high from the viewpoint of high productivity.
[0495] <Processing unit group>
[0496] The processing unit group is a group composed of processing units that process the first substrate transported by the transport unit, and includes, for example, an irradiation unit, a removal unit, a substrate setting unit, and a substrate processing unit.
[0497] <Irradiation unit>
[0498] The irradiation unit 200 is, for example, Fig.19As shown, there are a light irradiation device 2a for polymerizing a polymerizable compound by irradiating a liquid composition with active energy rays such as heat and light, and a polymerization inert gas circulation device 2b for circulating a polymerization inert gas.
[0499] When a polymerizable compound is contained in the liquid composition formed by the liquid applying unit 100, the light irradiation device 2a irradiates light in the presence of a polymerization inert gas to form an insulating layer.
[0500] The light irradiation device 2a is appropriately selected according to the absorption wavelength of the photopolymerization initiator contained in the liquid composition layer. As long as it is a device that can initiate and continuously polymerize the compounds in the liquid composition layer, there is no particular limitation. Examples include ultraviolet light sources such as high-pressure mercury lamps, metal halide lamps, hot cathode tubes, cold cathode tubes, and LEDs.
[0501] However, since light with a shorter wavelength generally tends to reach a deeper portion more easily, it is preferred to select a light source according to the thickness of the porous membrane to be formed.
[0502] Next, the polymerization inert gas circulation device 2b plays the role of reducing the concentration of polymerization-active oxygen contained in the atmosphere, so that the polymerization reaction of the polymerizable compound near the surface of the liquid composition layer proceeds without hindrance.
[0503] Therefore, the polymerization inert gas used is not particularly limited as long as it satisfies the above-mentioned function, and examples thereof include nitrogen, carbon dioxide, argon, and the like.
[0504] In addition, as the flow rate of the polymerization inert gas, in consideration of effectively obtaining the inhibitory reduction effect, the O2 concentration is preferably less than 20% (an environment with an oxygen concentration lower than that of the atmosphere), more preferably 0% to 15%, and most preferably 0% to 5%.
[0505] In order to realize stable polymerization progress conditions, the polymerization inert gas circulation device 2b is preferably provided with a temperature regulating device capable of regulating the temperature.
[0506] When the irradiation step is performed in the irradiation unit 200 , it is preferable that the conveyance speed of the first substrate is relatively slow in order to allow a sufficient polymerization reaction to proceed.
[0507] <Removal>
[0508] Remove unit 300, e.g. Fig.17 As shown, a heating device 3a is provided, and the residual solvent in the formed insulating layer is heated, dried and removed by the heating device 3a.
[0509] The removal unit 300 may perform the solvent removal step under reduced pressure.
[0510] In addition, the removal unit 300 may remove the photopolymerization initiator remaining in the insulating layer by heating and drying it with the heating device 3 a .
[0511] The heating device 3a is not particularly limited as long as it satisfies the above-mentioned functions, and examples thereof include an IR heater and a hot air heater.
[0512] Furthermore, the heating temperature and the heating time may be appropriately selected according to the boiling point of the solvent contained in the insulating layer and the thickness of the film to be formed.
[0513] When the removal step is performed in the removal unit 300 , the conveyance speed of the first substrate is preferably relatively slow because a sufficient amount of the solvent can be removed.
[0514] <Substrate installation unit>
[0515] After forming a functional film on the first substrate, the substrate disposing unit 400 disposes a second substrate on the functional film.
[0516] For example, Fig.18 As shown, the substrate placement unit 400 has a second substrate container 4a, and the second substrate is placed on the functional film formed on the first substrate through the second substrate conveying device 4b.
[0517] The second substrate container 4 a may be a roll-shaped substrate or a sheet-shaped substrate.
[0518] The second substrate transport device 4 b is not particularly limited as long as it can transport the substrate, and examples thereof include a device that transports the substrate using a suction mechanism.
[0519] The substrate installation unit 400 may also include an alignment mechanism equipped with a camera or the like to adjust the installation position of the second electrode as necessary.
[0520] When the substrate setting step is performed in the substrate setting unit 400 , the conveyance speed of the first substrate is preferably slow for the reasons of positional accuracy of setting and reducing damage to the first substrate caused by friction during setting.
[0521] <Substrate processing unit>
[0522] The substrate processing unit 500 processes the first substrate on which the functional film is formed downstream of the functional film forming unit 600 .
[0523] The substrate processing unit 500 may perform at least one of cutting, bending and laminating.
[0524] The substrate processing unit 500 can, for example, cut the first substrate after providing the second substrate to produce a substrate stack.
[0525] The substrate processing unit 500 may roll up or stack the first substrate provided with the second substrate.
[0526] When the insulating layer includes a material having a melting point or a glass transition point, in the base material processing unit 500 , for example, one base material stack and another base material stack are at least partially bonded together by heating.
[0527] The substrate processing unit 500 may be, for example, Figure 16 to Figure 22 As shown, there is a substrate processing device 5, which implements substrate cutting, zigzag folding, stacking or winding of the first substrate according to the target battery shape, and thermal bonding between the first substrates after stacking or winding.
[0528] When processing the substrate in the substrate processing unit 500 , it is preferred that the conveyance speed of the first substrate is relatively slow because damage such as wrinkles on the processed substrate can be reduced.
[0529] <Conveying unit>
[0530] The transport unit transports the first substrate in order to perform various steps on the first substrate.
[0531] For example, if the first substrate is transported by a roll-to-roll method or a conveyor belt method, the transport unit is, for example, Fig.16 The roller unit 8 shown in the figure.
[0532] When the battery component manufacturing apparatus includes a plurality of roller units 8 , a part or all of the roller units 8 may be controlled to rotate by the control unit 800 to convey the first substrate 6 at a predetermined speed, thereby functioning as conveying units.
[0533] In addition, a part of the roller unit 8 may also function as a guide wheel of the supporting member.
[0534] <Control unit>
[0535] Fig.23 This is an example of the main hardware block diagram of the control unit.
[0536] like Fig.23 As shown, the control unit 800 has, for example, a CPU 801 , a ROM 802 , a RAM 803 , an NVRAM 804 , an ASIC 805 , an I / O 806 , and an operation panel 807 .
[0537] The CPU 801 controls the entire battery stack manufacturing apparatus.
[0538] The ROM 802 stores programs executed by the CPU 801 and other fixed data.
[0539] RAM 803 temporarily stores data related to the battery component and the like.
[0540] The NVRAM 804 is a nonvolatile memory for retaining data even when the power of the device is turned off.
[0541] The ASIC 805 processes input and output signals for controlling image processing and other overall devices.
[0542] The I / O 806 is an interface for performing signal input and output with the functional film forming unit 600 , the substrate setting unit 400 , and the like.
[0543] The operation panel 807 performs input and display of information required by the control unit 800 .
[0544] Fig.24 This is an example of a main functional block diagram of a control unit.
[0545] like Fig.24 As shown, the control unit 800 has an insulating layer forming control unit 851, a substrate setting control unit 852, a substrate processing control unit 853, and a conveying control unit 854 as functional blocks.
[0546] The functional film formation control unit 851 controls the functional film formation unit 600 .
[0547] For example, the functional film formation control unit 851 issues a command to the liquid applying unit 100 for controlling the time or amount of applying the liquid composition.
[0548] For example, when forming a functional film by inkjet printing, the functional film formation control unit 851 issues a command to the liquid applying unit 100 to apply the liquid composition in a manner with predetermined waveform information, ejection conditions such as the number of ejections, and a predetermined time and number of droplets.
[0549] In addition, for example, the functional film formation control unit 851 issues a command to the irradiation unit 200 for controlling the time, irradiation amount, and the like when the active energy ray is irradiated to the liquid composition.
[0550] In addition, for example, the functional film formation control unit 851 issues a command to the removal unit 300 for controlling the time, heating amount, and the like when heating the solvent remaining in the insulating layer to dry and remove it.
[0551] The substrate setting control unit 852 issues a command to the substrate setting unit 400 for controlling the time of adsorption of the electrode, the speed of conveying the adsorbed electrode, and the like, for example.
[0552] When the substrate setting unit 400 has an alignment mechanism, the substrate setting control unit 852 controls the alignment mechanism to adjust the setting position of the second substrate based on position information from an image sensor such as a camera.
[0553] For example, when cutting the first substrate using laser, the substrate processing control unit 853 issues a command to the substrate processing unit 500 to control the amount of laser light emitted or to scan the laser based on position information from an image sensor such as a camera.
[0554] In addition, for example, the substrate processing control unit 853 issues a command to the substrate processing unit 500 to control the start time, end time, etc. of zigzag folding, lamination, winding, etc. of the first substrate.
[0555] In addition, for example, the base material processing control unit 853 issues a command to the base material processing unit 500 to control the heating temperature or heating time when performing thermal bonding between the first base materials after stacking or winding.
[0556] The conveyance control unit 854 controls the conveyance speed of the conveyance unit.
[0557] The conveyance control unit 854 can control the conveyance speed of the conveyance unit by, for example, making the rotation speed of one or more roller units 8 variable.
[0558] The transport control unit 854 preferably changes the transport speed of the transport unit according to the processing time of the substrate processing unit 500 .
[0559] For example, as a speed change action of the conveying unit controlled by the conveying control unit 854, when performing a process that hinders the conveyance of the first substrate, such as necessary cutting or folding processes, it is preferred to control it to be decelerating and / or has been decelerated to convey the first substrate at a speed slower than the predetermined conveying speed.
[0560] By performing such a speed change operation, it is possible to suppress damage to the end portion of the base material even during the cutting or zigzag folding process.
[0561] Furthermore, after the conveyance control unit 854 decelerates, it is preferred that the conveyance speed be accelerated to the original conveyance speed after performing a necessary process such as a cutting process or a zigzag folding process that interferes with the conveyance of the first substrate.
[0562] By performing such an operation, productivity can be improved.
[0563] The transport control unit 854 controls so that when the transport speed is high, the liquid applying unit applies the liquid to the first substrate at high speed, and when the transport speed is low, the liquid applying unit applies the liquid to the first substrate at low speed.
[0564] In addition, during acceleration and deceleration, the liquid is supplied under the control of the discharge conditions corresponding to the change in the conveying speed.
[0565] By performing such control, a substrate having a high-quality functional film of a certain thickness can be produced with good productivity.
[0566] In addition, for example Fig.25A As shown, the conveying control unit 854 can set a period during which the conveying unit conveys at a high speed, a period during which the conveying unit conveys at a low speed, and a transition period from a low speed to a high speed or from a high speed to a low speed.
[0567] The conveying speed of the conveying unit can also be controlled to be more than 3 time periods.
[0568] In addition, there may be a period of time when the conveyance is performed at a constant speed of high or low speed.
[0569] In addition, if Fig.25B As shown, the conveying speed of the conveying unit may be controlled to have a curve, such as a sine curve, without a constant speed region.
[0570] In addition, low speed also includes the case where the speed is zero.
[0571] In addition, the control unit 800 may control a processing unit group including one or more processing units.
[0572] At this time, the control unit 800 preferably links the conveying speed control of the conveying unit and the control of the plurality of processing units.
[0573] For example, when the conveying speed is low, substrate processing such as cutting and zigzag folding of the first substrate requiring a relatively slow conveying speed is performed on the substrate processing unit 500 .
[0574] By performing such control, a high-quality base material can be produced with good productivity.
[0575] In addition, the control unit 800 preferably controls the application conditions of the liquid application unit 100, the transport speed of the transport unit, and the plurality of processing units in a linked manner.
[0576] For example, the control unit 800 preferably changes the signal for ejecting the liquid composition in synchronization with the change in speed of the delivery unit.
[0577] Hereinafter, the battery and the like will be described in more detail with reference to Examples and Comparative Examples, but the present invention is not limited to these Examples.
[0578] [Example]
[0579] First, the negative electrode and the positive electrode used in each example and each comparative example were produced.
[0580] <Production of negative electrode>
[0581] For forming a negative electrode composite material layer, 97.0 mass % of graphite, 1.0 mass % of a thickener (carboxymethyl cellulose), 2.0 mass % of a polymer (styrene butadiene rubber), and 100.0 mass % of water as a solvent were added to prepare a negative electrode coating.
[0582] The negative electrode coating was applied to both sides of the copper foil substrate and dried to obtain a negative electrode composite material layer with a unit area weight of 9.0 mg / cm on one side. 2 of the negative electrode.
[0583] Then, the electrode was pressed using a roller press to obtain a volume density of 1.6 g / cm 3 , and obtain the negative electrode used.
[0584] At this time, the total film thickness of the negative electrode was 112.0 μm.
[0585] <Production of positive electrode>
[0586] 92.0 mass % of lithium nickel oxide (NCA) as a positive electrode active material, 3.0 mass % of acetylene black as a conductive material, and 5.0 mass % of polyvinylidene fluoride (PVDF) as a binder were prepared and dispersed in N-methylpyrrolidone (NMP) to prepare a positive electrode coating.
[0587] The positive electrode coating was applied to both sides of the aluminum foil substrate and dried to obtain a positive electrode composite material layer with a unit area weight of 15.0 mg / cm on one side. 2 The positive electrode.
[0588] Next, the electrode was pressed using a roller press to a volume density of 2.8 g / cm 3 , and obtain the positive electrode to be used.
[0589] At this time, the total film thickness of the positive electrode was 132.0 μm.
[0590] Finally, the positive electrode was punched out using a die punching machine (punching area: 47.0 mm×27.0 mm).
[0591] [Example 1]
[0592] - Adjustment of the insulating layer forming liquid composition -
[0593] The materials were mixed in the following proportions to prepare an insulating layer forming liquid composition.
[0594] A liquid composition for forming an insulating layer was obtained by mixing 29.0 mass % of tricyclodecane dimethanol diacrylate (produced by Daicel-Allnex Co., Ltd.) as a polymerizable compound (resin A), 70.0 mass % of dipropylene glycol monomethyl ether (produced by Kanto Chemical Industry Co., Ltd.) as a solvent (porogen), and 1.0 mass % of Irgacure 184 (produced by BASF) as a polymerization initiator.
[0595] <Formation of Insulating Layer and Cutting of First Base Material>
[0596] use Fig.19 The manufacturing apparatus shown implements the formation of the insulating layer and the cutting of the first substrate.
[0597] The negative electrode was prepared in the form of a roll having a current collector width of 60 mm and a composite material layer width of 50 mm, and conveyed while continuously changing between two speeds in conjunction with a cutting mechanism as described below.
[0598] Non-cutting: 50mm / sec
[0599] Cutting: 0mm / sec
[0600] While being transported, the insulating layer forming liquid composition is filled into the inkjet printing device. For the variably transported negative electrode, the discharge amount is controlled so that the amount of the attached liquid composition is constant, and an insulating layer with a thickness of 20.0 μm is formed on both sides of the negative electrode composite material layer.
[0601] Then, the coated area was immediately irradiated with UV light (light source: UV-LED (manufactured by Phoseon, trade name: FJ800), wavelength: 365 nm, irradiation intensity: 30 mW / cm 2 , irradiation time: 20s) to solidify it.
[0602] Next, the cured product was heated at 120° C. for 1 minute using a hot air drying oven to remove the solvent.
[0603] Finally, in a substrate processing step provided after the removal step, the negative electrode was cut into a size of 60.0 mm in length×30.0 mm in width, thereby obtaining a negative electrode having an insulating layer formed thereon.
[0604] [Evaluation 1: Evaluation of film thickness uniformity]
[0605] The film thickness uniformity of the obtained negative electrode was evaluated according to the following procedure.
[0606] The area 10.0 mm relative to the center in the width direction in the area where the negative electrode composite material layer is formed is taken as the center of the composite material layer, and the areas at both ends are taken as the ends of the composite material layer. The film thickness is measured with a micrometer at three randomly selected locations in the center of the composite material layer and the ends of the composite material layer, and the uniformity of the film thickness of the functional membrane is judged based on the size of each average value.
[0607] In addition, as in Example 2, when the insulating layer has a thin film region and a thick film region, the film thickness is measured at 3 randomly selected locations in the thin film region with a micrometer, and the thickness uniformity of the functional film is determined based on the size of each average value.
[0608] The results are as follows Fig.31 shown.
[0609] and, Fig.31 The solid image in the "Printed Image" column in shows that the insulating layer is formed only by the thin film region without forming the thick film region.
[0610] In addition, the pattern image means that a thin film region and a thick film region are formed on the insulating layer.
[0611] a: The average thickness of the composite material layer at the end is 10% smaller than the average thickness of the composite material layer at the center.
[0612] b: The average thickness of the composite material layer at the end is greater than the average thickness of the composite material layer at the center by 10% or more.
[0613] [Evaluation 2: Evaluation of the electrode cut end portion]
[0614] As evaluation of the cut end of the electrode, the shape of the negative electrode cut into a size of 60.0 mm in length×30.0 mm in width was measured.
[0615] Although the negative electrode was cut into a shape with a width of 30.0 mm, it is considered that the width was shorter than 30.0 mm when wrinkles or twists were generated at the electrode end due to the contact of the cutter blade with the negative electrode moving in the conveying direction during cutting.
[0616] Therefore, the accurate width of the cut negative electrode was measured, and the cut end portion of the electrode was evaluated according to the following criteria.
[0617] The results are as follows Fig.31 shown.
[0618] a: The difference between the measured width after cutting and the specified value is less than ±5%
[0619] b: The difference between the measured width after cutting and the specified value is more than ±5%.
[0620] [Comparative Example 1]
[0621] A first substrate having an insulating layer was obtained in the same manner as in Example 1 except that the transport method of the negative electrode in Example 1 was changed to transport at a constant speed of 50.0 mm / sec.
[0622] Then, in the same manner as in Example 1, Evaluations 1 and 2 were carried out.
[0623] The results are as follows Fig.31 shown.
[0624] [Comparative Example 2]
[0625] A first base material having an insulating layer was obtained in the same manner as in Example 1 except that the method for forming the insulating layer in Example 1 was changed to a die coating method.
[0626] Then, in the same manner as in Example 1, Evaluations 1 and 2 were carried out.
[0627] The results are as follows Fig.31 shown.
[0628] [Example 2]
[0629] A first base material having an insulating layer was obtained in the same manner as in Example 1 except that the formation region of the insulating layer in Example 1 was changed to the following region.
[0630] Then, in the same manner as in Example 1, Evaluations 1 and 2 were carried out.
[0631] The results are as follows Fig.31 shown.
[0632] -Formation Area of Insulating Layer of Example 2-
[0633] For the negative electrode, the ejection amount of the liquid composition is controlled to form an insulating layer (thin film region) and an insulating layer (thick film region) on both sides of the negative electrode composite material layer to form Fig.26 The pattern image shape shown.
[0634] The area of the insulating layer (thin film region) was 47.0 mm×27.0 mm, and the film thickness was 20.0 μm. The film thickness of the insulating layer (thick film region) was 26.0 μm.
[0635] [Comparative Example 3]
[0636] A first substrate having an insulating layer was obtained in the same manner as in Example 2 except that the transport method of the negative electrode in Example 2 was changed to transport at a constant speed of 50.0 mm / sec.
[0637] Then, in the same manner as in Example 1, Evaluations 1 and 2 were carried out.
[0638] The results are as follows Fig.31 shown.
[0639] [Comparative Example 4]
[0640] A first base material having an insulating layer was obtained in the same manner as in Example 2 except that the method for forming the insulating layer in Example 2 was changed to a die coating method.
[0641] Then, in the same manner as in Example 1, Evaluations 1 and 2 were carried out.
[0642] The results are as follows Fig.31 shown.
[0643] [Example 3]
[0644] A first substrate having an insulating layer was obtained in the same manner as in Example 1, except that the formation of the insulating layer-forming liquid composition in Example 1 was changed to the following steps.
[0645] Then, in the same manner as in Example 1, Evaluations 1 and 2 were carried out.
[0646] The results are as follows Fig.31 shown.
[0647] -Formation of Liquid Composition for Forming Insulating Layer in Example 3-
[0648] 39.0 mass % of EBECRYL 8402 (manufactured by Daicel-Allnex Co., Ltd.) as a polymerizable compound (resin B), 60.0 mass % of diisobutyl ketone (manufactured by Kanto Chemical Industry Co., Ltd.) as a porogen, and 1.0 mass % of Irgacure 819 (manufactured by BASF Corporation) as a polymerization initiator were mixed to obtain a liquid composition for forming an insulating layer.
[0649] [Comparative Example 5]
[0650] A first substrate having an insulating layer was obtained in the same manner as in Example 3 except that the transport method of the negative electrode in Example 3 was changed to transport at a constant speed of 50.0 mm / sec.
[0651] Then, in the same manner as in Example 1, Evaluations 1 and 2 were carried out.
[0652] The results are as follows Fig.31 shown.
[0653] [Comparative Example 6]
[0654] A first base material having an insulating layer was obtained in the same manner as in Example 3 except that the method for forming the insulating layer in Example 3 was changed to a die coating method.
[0655] Then, in the same manner as in Example 1, Evaluations 1 and 2 were carried out.
[0656] The results are as follows Fig.31 shown.
[0657] [Example 4]
[0658] A first substrate having an insulating layer was obtained in the same manner as in Example 3 except that the formation region of the insulating layer in Example 3 was changed to the following region.
[0659] Then, in the same manner as in Example 1, Evaluations 1 and 2 were carried out.
[0660] The results are as follows Fig.31 shown.
[0661] -Formation Region of Insulating Layer of Example 4-
[0662] For the negative electrode, the ejection amount of the liquid composition is controlled to form an insulating layer (thin film region) and an insulating layer (thick film region) on both sides of the negative electrode composite material layer to form Fig.26 The pattern image shape shown.
[0663] The area of the insulating layer (thin film region) was 47.0 mm×27.0 mm, and the film thickness was 20.0 μm. The film thickness of the insulating layer (thick film region) was 26.0 μm.
[0664] [Comparative Example 7]
[0665] A first substrate having an insulating layer was obtained in the same manner as in Example 4 except that the transport method of the negative electrode in Example 4 was changed to transport at a constant speed of 50.0 mm / sec.
[0666] Then, in the same manner as in Example 1, Evaluations 1 and 2 were carried out.
[0667] The results are as follows Fig.31 shown.
[0668] [Comparative Example 8]
[0669] A first base material having an insulating layer was obtained in the same manner as in Example 4 except that the method for forming the insulating layer in Example 4 was changed to a die coating method.
[0670] Then, in the same manner as in Example 1, Evaluations 1 and 2 were carried out.
[0671] The results are as follows Fig.31 shown.
[0672] [Example 5]
[0673] A first substrate having an insulating layer was obtained in the same manner as in Example 1, except that the formation of the insulating layer-forming liquid composition in Example 1 was changed to the following steps.
[0674] Then, in the same manner as in Example 1, Evaluations 1 and 2 were carried out.
[0675] The results are as follows Fig.31 shown.
[0676] -Formation of Liquid Composition for Forming Insulating Layer in Example 5-
[0677] As an inorganic solid material, α-alumina (primary particle size (D50): 0.5 μm, specific surface area: 7.8 g / m 2 ) 40.0 mass %, a mixed solution of dimethyl sulfoxide and ethylene glycol (DMSO-EG) 58.0 mass %, and MALIALIM HKM-150A (manufactured by NOF Corporation) as a dispersant 2.0 mass % were mixed to prepare a preliminary dispersion.
[0678] The preliminary dispersion was placed in a container together with zirconium oxide beads (φ2 mm), and a dispersion treatment was performed at 1500 rpm for 3 minutes using a freezing nano-pulverizer NP-100 (manufactured by Thinky Co., Ltd.) to obtain a dispersion.
[0679] The zirconium oxide beads were removed from the obtained dispersion using a 25 μm mesh filter to prepare an insulating layer forming liquid composition.
[0680] [Comparative Example 9]
[0681] A first substrate having an insulating layer was obtained in the same manner as in Example 5 except that the transport method of the negative electrode in Example 5 was changed to transport at a constant speed of 50.0 mm / sec.
[0682] Then, in the same manner as in Example 1, Evaluations 1 and 2 were carried out.
[0683] The results are as follows Fig.31 shown.
[0684] [Comparative Example 10]
[0685] A first base material having an insulating layer was obtained in the same manner as in Example 5 except that the method for forming the insulating layer in Example 5 was changed to a die coating method.
[0686] Then, in the same manner as in Example 1, Evaluations 1 and 2 were carried out.
[0687] The results are as follows Fig.31 shown.
[0688] -Battery production-
[0689] The positive electrode and the negative electrode obtained in the present example and the comparative example were stacked so as to face each other.
[0690] Use laminated outer packaging material as outer packaging for sealing, making Fig.30 The energy storage element is shown before being filled with electrolyte.
[0691] The obtained element was vacuum dried at 120° C. for 12 hours, and then injected with an electrolyte solution.
[0692] At this time, it was confirmed that Examples 3 and 4 and Comparative Examples 5, 6, 7 and 8 were heat-bonded at the electrode end and the thick film region of the first electrode located above and below the stack.
[0693] In addition, as the electrolyte solution, a solution obtained by adding LiPF6 as an electrolyte to a mixture of ethylene carbonate (EC) and dimethyl carbonate (DMC) (a mixture with a mass ratio of "EC:DMC=1:1") so that the concentration thereof becomes 1.5 mol / L was used.
[0694] according to Fig.31 By changing the conveying speed synchronously with the electrode cutting process, the quality of the electrode end becomes good, and by adopting an inkjet method as a printing method, the unevenness of the film thickness of the formed functional film can be suppressed, and the uniformity of the film thickness also becomes good.
[0695] In addition, this means that the effect can be obtained regardless of the material, whether it is an organic material or an inorganic material.
[0696] Furthermore, it was shown that when a resin B with a low glass transition temperature (Tg) is used as the material of the insulating layer, by setting a second electrode and heating after stacking, it was confirmed that the thick film area of the first electrode located above and below the stack at the electrode end was heated and bonded, resulting in a stacked body that is not prone to electrode deviation after stacking.
[0697] As mentioned above, although the preferred embodiments and the like have been described in detail, the present invention is not limited to the embodiments and the like described above, and various modifications and substitutions can be made to the embodiments and the like described above without departing from the scope described in the claims.
[0698] The above embodiments are illustrative and do not limit the present invention. Therefore, according to the above teachings, many additional modifications and variations are possible. For example, within the scope of the present invention, the elements and / or features of different illustrative embodiments can be combined and / or replaced with each other.
[0699] Any of the operations described above may be performed in various other ways, such as in an order different from that described above.
[0700] This patent application is based on and claims the benefit of priority of Japanese Patent Applications No. 2022-043144 and No. 2022-043142 filed with the Japan Patent Office on March 17, 2022, and the entire contents of the above patent applications are incorporated herein by reference.
[0701] Reference numerals list
[0702] 1a Printing device (inkjet device)
[0703] 1b Storage container
[0704] 1c Supply pipe
[0705] 2a Light irradiation device
[0706] 2b Inert polymerization gas circulation device
[0707] 3a Heating device
[0708] 4a Second electrode container (second substrate container)
[0709] 4b Second electrode conveying device (second substrate conveying device)
[0710] 5 Electrode processing device (substrate processing device)
[0711] 6. First electrode (first substrate)
[0712] 7 Liquid Composition
[0713] 8-roller unit
[0714] 9 Current collector of the first electrode (current collector of the negative electrode)
[0715] 10. Active material of the first electrode (active material of the negative electrode)
[0716] 11a Thin film area of the insulating layer
[0717] 11b Thick film area of the insulating layer
[0718] 12. Current collector of the second electrode (current collector of the positive electrode)
[0719] 13. Active material of the second electrode (active material of the positive electrode)
[0720] 100 Liquid Imparting Unit
[0721] 200 Irradiation Units
[0722] 300 Remove unit
[0723] 400 Electrode setting unit (substrate setting unit)
[0724] 500 Electrode processing unit (substrate processing unit)
[0725] 600 Insulation layer forming unit (functional film forming unit)
[0726] 800 Control Unit
[0727] 801 CPU
[0728] 802 ROM
[0729] 803 RAM
[0730] 804 NVRAM
[0731] 805 ASIC
[0732] 806 I / O
[0733] 807 Operation Panel
[0734] 851 Insulation layer forming control unit (functional film forming control unit)
[0735] 852 Electrode setting control unit (substrate setting control unit)
[0736] 853 Electrode processing control unit (substrate processing control unit)
[0737] 854 Conveyor Control Unit
Claims
1. A method for producing a battery laminate, comprising: forming an insulating layer by applying a liquid composition onto the first electrode; and A second electrode is provided on the first electrode having the insulating layer formed thereon, in, The forming and setting are performed through a series of conveying. 2 . The method for producing a battery laminate according to claim 1 , further comprising processing the first electrode after forming the first electrode.
3. The method for producing a battery laminate according to claim 2, in, The insulating layer includes a material having a melting point or a glass transition temperature, and The process includes manufacturing a plurality of electrode stacks in which a second electrode is provided on a first electrode formed with an insulating layer, and at least partially bonding one electrode stack of the plurality of electrode stacks and another electrode stack of the plurality of electrode stacks by heating.
4. The method for producing a battery laminate according to claim 2, in, The processing includes cutting the first electrode before disposing the second electrode, and the disposing is performed immediately after the processing.
5. The method for producing a battery laminate according to any one of claims 1 to 4, in, The first electrode includes a cathode, and the second electrode includes an anode.
6. The method for producing a battery laminate according to any one of claims 1 to 5, in, The forming includes forming the insulating layer into a shape having a concavo-convex pattern including concave portions and convex portions.
7. A manufacturing device for a battery stack, the device comprising: an insulating layer forming unit configured to form an insulating layer by applying a liquid composition onto the first electrode; and an electrode setting unit configured to set a second electrode on the first electrode formed with the insulating layer, in, The insulating layer forming unit and the electrode setting unit are arranged in a transport series region for transporting the first electrode. 8 . The manufacturing apparatus of the battery laminate according to claim 7 , further comprising an electrode processing unit configured to process the first electrode on which the insulating layer is formed.
9. The manufacturing device of the battery laminate according to claim 8, in, The insulating layer includes a material having a melting point or a glass transition temperature, and The electrode processing unit is configured as follows: manufacturing a plurality of electrode stacks in which a second electrode is provided on a first electrode formed with an insulating layer, and The one electrode stack and the other electrode stack are heated to at least partially bond the one electrode stack and the other electrode stack.
10. The manufacturing device of the battery laminate according to claim 8, in, The electrode processing unit is configured to cut the first electrode before providing the second electrode, and The electrode setting unit is configured to set the second electrode on the cut first electrode.
11. The device for producing a battery laminate according to any one of claims 7 to 10, in, The first electrode includes a cathode, and the second electrode includes an anode.
12. The device for producing a battery laminate according to any one of claims 7 to 11, in, The insulating layer forming unit forms the insulating layer into a shape having a concavo-convex pattern including concave portions and convex portions.
13. A method for manufacturing a battery component, comprising: conveying a first substrate at a variable speed; and The liquid composition is discharged onto the conveyed first substrate by a liquid discharging method to form a functional film.
14. A manufacturing device for a battery component, the device comprising: A conveying unit configured to convey a first substrate; a functional film forming unit configured to discharge a liquid composition onto the first substrate being transported by a liquid discharge method to form a functional film; as well as a control unit configured to control the conveying unit, The control unit controls the conveying speed of the conveying unit to convey the first substrate at a variable speed.