Packaging body and forming method thereof

By performing plasma treatment or ion beam implantation on the top surface and sidewalls of semiconductor bare dies to reduce dopant concentration and increase hydrophobicity, and by using spin-coated dielectric material to fill gaps from bottom to top, the problems of void formation and increased cost during gap filling in the prior art are solved, achieving higher reliability and performance.

CN119008588APending Publication Date: 2024-11-22TAIWAN SEMICONDUCTOR MANUFACTURING CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410897941.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-07-17
Filing Date
2024-07-05
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

Existing semiconductor packaging technologies face manufacturing challenges in improving density and functionality, especially in filling the gaps between semiconductor dies, which can easily lead to voids and increase manufacturing costs.

Method used

The hydrophobicity of a semiconductor die is increased by performing plasma treatment or ion beam implantation on the top surface and sidewalls, using dopants such as fluorine to reduce the doping concentration. Subsequently, a spin-coated dielectric material is used to fill the gaps from bottom to top, reducing the roughness of the dielectric material and simplifying the cleaning process.

Benefits of technology

It improves the reliability and performance of the package, reduces manufacturing costs, avoids voids during filling, improves the interface with the overlay structure, and simplifies the cleaning process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119008588A_ABST
    Figure CN119008588A_ABST
Patent Text Reader

Abstract

A method includes bonding a first semiconductor die and a second semiconductor die to a substrate, wherein a gap is disposed between a first sidewall of the first semiconductor die and a second sidewall of the second semiconductor die; performing a plasma treatment to dope a top surface and sidewalls of each of the first semiconductor die and the second semiconductor die with a first dopant, wherein a concentration of the first dopant in the first sidewall decreases in a longitudinal direction from a top surface of the first semiconductor die toward a bottom surface of the first semiconductor die, a concentration of the first dopant in the second sidewall decreases in a longitudinal direction from a top surface of the second semiconductor die toward a bottom surface of the second semiconductor die; and filling the gap with a spin-on dielectric material.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a package and a method for forming the same, and more particularly to an integrated circuit package and a method for forming the same. Background Art

[0002] Semiconductor devices are used in a variety of electronic applications, such as personal computers, mobile phones, digital cameras, and other electronic devices. The manufacture of semiconductor devices involves sequentially depositing insulating or dielectric layers, conductive layers, and semiconductor layers on a semiconductor substrate, and patterning the various material layers using lithography and etching processes to form circuit components and elements on the semiconductor substrate.

[0003] New packaging technologies have been developed to increase the density and functionality of semiconductor devices. Packaging technologies for these relatively new semiconductor devices face manufacturing challenges. Summary of the invention

[0004] An embodiment of the present disclosure provides a method, comprising bonding a first semiconductor die and a second semiconductor die to a substrate, wherein a gap is disposed between a first sidewall of the first semiconductor die and a second sidewall of the second semiconductor die; performing plasma treatment to dope a top surface and a sidewall of each of the first semiconductor die and the second semiconductor die with a first dopant, wherein a concentration of the first dopant in the first sidewall decreases in a longitudinal direction from the top surface of the first semiconductor die toward a bottom surface of the first semiconductor die, and a concentration of the first dopant in the second sidewall decreases in a longitudinal direction from the top surface of the second semiconductor die toward a bottom surface of the second semiconductor die; and filling the gap with a spin-on dielectric material.

[0005] An embodiment of the present disclosure provides a method, comprising bonding a plurality of bare die to a first substrate, each of the bare die comprising a semiconductor substrate and an interconnect structure on the semiconductor substrate; after bonding the bare die to the first substrate, doping the top surface and side walls of each semiconductor substrate of the bare die with a first dopant so that the hydrophobicity of the side walls of each semiconductor substrate decreases in a longitudinal direction from the top surface of the semiconductor substrate toward the bottom surface of the semiconductor substrate; and forming a dielectric material between each of the bare die.

[0006] An embodiment of the present disclosure provides a package, including a redistribution structure, a first bare die, and a first dielectric material, wherein the first bare die is above the redistribution structure and electrically coupled to the redistribution structure, and the first dielectric material encapsulates the first bare die, wherein the sidewall of the first bare die includes a first dopant, wherein the concentration of the first dopant in the sidewall of the first bare die decreases in a longitudinal direction from the top surface of the first bare die toward the bottom surface of the first bare die. BRIEF DESCRIPTION OF THE DRAWINGS

[0007] The following detailed description and accompanying drawings provide a complete disclosure. It should be noted that, according to common practices in the industry, the drawings are not necessarily drawn to scale. In fact, the size of the components may be arbitrarily enlarged or reduced to provide a clear description.

[0008] Figures 1 to 4B Cross-sectional views are shown of intermediate steps during a process of forming an integrated circuit device stack 10 , in accordance with some embodiments.

[0009] Figures 5 to 15 Cross-sectional views are shown of intermediate steps during a process of forming an integrated circuit device stack 10 , in accordance with some embodiments.

[0010] Fig.16 A cross-sectional view of a package 20 is shown according to an alternative embodiment.

[0011] Fig.17 A cross-sectional view of a package 30 is shown according to an alternative embodiment.

[0012] Fig.18 A cross-sectional view of a package 40 is shown according to an alternative embodiment.

[0013] The reference numerals are described as follows:

[0014] 10: Integrated circuit device stacking

[0015] 20, 30, 40: Encapsulation

[0016] 60, 96, 412, 514: Substrate

[0017] 62: Active Surface

[0018] 64, 94: Interconnection structure

[0019] 65, 72, 104A, 104B: Bonding layer

[0020] 67, 91: Gap

[0021] 68, 89: Bare crystal

[0022] 70, 106: Carrier substrate

[0023] 74: Perforation

[0024] 80: Plasma treatment

[0025] 81: Implantation process

[0026] 82: Doping area

[0027] 82A: First doped region

[0028] 82B: Second doped region

[0029] 83: Gap filling process

[0030] 84, 102: Dielectric materials

[0031] 85: Axis

[0032] 86, 90: Dielectric layer

[0033] 88, 92, 108, 302, 314, 418, 424, 502: Conductive connectors

[0034] 98: Process

[0035] 99: Gap filling process

[0036] 100: Doping area

[0037] 100A: First doped region

[0038] 100B: Second doping region

[0039] 107: Under Bump Metal

[0040] 110: Draw a line

[0041] 170: Redistribution Structure

[0042] 171: Bare die connector

[0043] 174: Redistribution of metallization pattern

[0044] 176: Redistributed Dielectric Layer

[0045] 200: First packaging component

[0046] 202, 506: sealant

[0047] 218: Front-focused distribution structure

[0048] 222: Rear focus distribution structure

[0049] 224: Perforation

[0050] 300: Package substrate

[0051] 304: Under Bump Metal

[0052] 306, 312, 410, 416: Bonding pads

[0053] 308: Solder resist

[0054] 310: Baseboard core

[0055] 320, 518: Bottom filler

[0056] 400: Second packaging component

[0057] 402A, 402B: Stacked Dies

[0058] 406: Wire Bonding

[0059] 408: Molding material

[0060] 414: Conductive vias

[0061] 500: The third package component

[0062] 504: Bottom filling material

[0063] 508: Conductive bump

[0064] 512: Interconnection Structure

[0065] 516: Intermediary layer

[0066] 520: Electrical connector / metal pillar / microbump / pillar / bump electrical connector

[0067] 522: Electrical connector / metal cover / micro bump / cover / bump electrical connector

[0068] 524: Metal pillar / electrical connector

[0069] AA: Vertical direction / arrow

[0070] BB, XX, YY: Arrow

[0071] D1, D3: Depth

[0072] D2, D4: Doping depth / depth

[0073] H1, H2: Height

[0074] W1, W2: Width

[0075] θ1: Tilt angle DETAILED DESCRIPTION

[0076] The following disclosure provides many different embodiments or examples to implement the different features of the present invention. The following disclosure describes specific examples of various components and their arrangements to simplify the description. Of course, these specific examples are not intended to be limiting. For example, if the present disclosure describes a first feature formed on or above a second feature, it means that it may include an embodiment in which the first feature and the second feature are in direct contact, and may also include an embodiment in which an additional feature is formed between the first feature and the second feature, so that the first feature and the second feature may not be in direct contact. In addition, different examples in the following disclosure may reuse the same reference symbols and / or marks. These repetitions are for the purpose of simplification and clarity, and are not intended to limit the specific relationship between the different embodiments and / or structures discussed.

[0077] In addition, spatially related terms such as "below," "below," "lower," "above," "higher," and similar terms are used to facilitate description of the relationship between one element or feature and another element or features in the diagram. In addition to the orientation shown in the drawings, these spatially related terms are intended to include different orientations of the device in use or operation. The device may be turned to different orientations (rotated 90 degrees or other orientations), and the spatially related terms used herein may be interpreted in the same manner.

[0078] Various embodiments include methods of forming an integrated circuit package and the resulting structures. In some embodiments, semiconductor die may be bonded to a substrate, and a plasma treatment is performed to dope the top surface and sidewalls of each semiconductor die with a suitable dopant (e.g., fluorine). The doping concentration of the dopant in the corresponding sidewall of each semiconductor die may decrease in a longitudinal direction away from the top surface of the semiconductor die. A gap-filling process is then performed to fill the gaps between the semiconductor die with a dielectric material.

[0079] Due to the doping profiles of the semiconductor die, an increased hydrophobicity of the top surface and upper sidewalls of the semiconductor die can be achieved compared to the lower sidewalls of the semiconductor die. For example, the hydrophobicity of the sidewalls of the semiconductor die decreases in a longitudinal direction away from the top surface of the semiconductor die. As a result, during a gap fill process, the increased hydrophobicity of the top portion of the semiconductor die compared to the bottom portion of the semiconductor die can allow the dielectric material to fill and adhere to the bottom portion of the semiconductor die before filling and adhering to the top portion of the semiconductor die. This allows for bottom-up gap filling, thereby allowing gaps of greater depth to be filled without forming large voids. As a result, the reliability and performance of the device are improved. The bottom-up filling process can further reduce the roughness of the dielectric material, thereby allowing an improved interface with an overlying structure of the integrated circuit package and improved device reliability. Furthermore, after the gap-fill process, no residue is left on the top surface of the semiconductor die, thereby eliminating the need for a cleaning process after performing the gap-fill process and reducing manufacturing costs.

[0080] Figures 1 to 15 A cross-sectional view is shown of an intermediate stage in the fabrication of an integrated circuit device stack 10 in accordance with some embodiments. Figure 1 A wafer including one or more bare die 68 is shown. The substrate 60 of the wafer may include a bulk semiconductor substrate, a semiconductor-on-insulator (SOI) substrate, a multilayer semiconductor substrate, etc. The semiconductor material of the substrate 60 may be silicon; germanium; a compound semiconductor including silicon germanium, silicon carbide, gallium arsenide, gallium phosphide, indium phosphide, indium arsenide, and / or indium antimonide; an alloy semiconductor including SiGe, GaAsP, AlInAs, AlGaAs, GaInAs, GaInP, and / or GaInAsP; or a combination thereof. Other substrates may also be used, such as multilayer or gradient substrates. The substrate 60 may be doped or undoped. Devices such as transistors, capacitors, resistors, diodes, etc. may be formed in and / or on the active surface 62 of the substrate 60.

[0081] Through-vias (TVs) 74 are formed to extend from active surface 62 of substrate 60 into substrate 60. When substrate 60 is a silicon substrate, through-vias 74 are sometimes also referred to as through-substrate vias or through-silicon vias. Through-vias 74 may be formed by forming recesses in substrate 60, for example, by etching, milling, laser technology, combinations thereof, etc. A thin barrier layer may be conformally deposited on substrate 605 and in the recesses, for example, by chemical vapor deposition (CVD), atomic layer deposition (ALD), physical vapor deposition (PVD), thermal oxidation, combinations thereof, etc. The barrier layer may include a nitride or an oxynitride, such as titanium nitride, titanium oxynitride, tantalum nitride, tantalum oxynitride, tungsten nitride, combinations thereof, etc. A conductive material may be deposited on the thin barrier layer and in the recesses. The conductive material may be formed by electrochemical plating, chemical vapor deposition, atomic layer deposition, physical vapor deposition, combinations thereof, etc. Examples of the conductive material are copper, tungsten, aluminum, silver, gold, combinations thereof, etc. Excess conductive material and barrier layer on the substrate 605 are removed by, for example, chemical-mechanical polishing (CMP). Thus, the through-hole 74 may include a conductive material and a thin barrier layer between the conductive material and the substrate 60.

[0082] An interconnect structure 64 including one or more dielectric layers and corresponding metallization patterns is formed on the active surface 62. The metallization patterns in the dielectric layers can route electrical signals between devices and / or vias 74, for example by using vias and / or traces, and can include vias 74, and can also include various electrical devices, such as capacitors, resistors, inductors, etc. The various devices and metallization patterns can be interconnected to form an integrated circuit that performs one or more functions. The integrated circuit can include memory, processors, sensors, amplifiers, power distribution devices, input / output circuits, etc. In addition, the topmost dielectric layer of the interconnect structure 64 can be used as a substrate for subsequent bonding to a carrier substrate 70 (described in Figure 3 The bonding layer 65 is used in the middle.

[0083] As an example of a layer forming the interconnect structure 64, an inter-metallization dielectric (IMD) layer may be formed. The inter-metallization dielectric layer may be formed, for example, by any suitable method (e.g., spin coating, chemical vapor deposition (CVD), plasma-enhanced chemical vapor deposition (PECVD), high-density plasma chemical vapor deposition (HDP-CVD), etc.) from a low-K dielectric material, such as phosphosilicate glass (PSG), borophosphosilicate glass (BPSG), fluorosilicate glass (FSG), SiO x C y , Spin-On-Glass, Spin-On-Polymer, Silicon Carbon Materials, Compounds thereof, Composites thereof, Combinations thereof, etc. The metallization pattern may be formed in the intermetallic dielectric layer, for example, by depositing and patterning a photoresist material on the intermetallic dielectric layer using a photolithography technique to expose the portion of the intermetallic dielectric layer that will become the metallization pattern. An etching process such as an anisotropic dry etching process may be used to create a recess and / or opening in the intermetallic dielectric layer corresponding to the exposed portion of the intermetallic dielectric layer. The recess and / or opening may be lined with a diffusion barrier layer and filled with a conductive material. The diffusion barrier layer may include one or more layers of tantalum nitride, tantalum, titanium nitride, titanium, cobalt tungsten, etc., or combinations thereof, deposited by atomic layer deposition (ALD) or the like. The conductive material of the metallization pattern may include copper, aluminum, tungsten, silver, and combinations thereof, etc., deposited by chemical vapor deposition, physical vapor deposition (PVD), or the like. Any excess diffusion barrier and / or conductive material on the intermetallic dielectric layer may be removed, for example, by using chemical mechanical polishing (CMP). Additional layers of interconnect structure 64 may be formed by repeating these steps. Bonding layer 65 may be deposited over the additional layers of interconnect structure 64. In some embodiments, bonding layer 65 may be an oxide, such as silicon oxide, silicon oxynitride, or the like, or a combination thereof, and may be formed by high density plasma chemical vapor deposition, flowable chemical vapor deposition (FCVD), chemical vapor deposition, atomic layer deposition, physical vapor deposition, or the like, or a combination thereof.

[0084] exist Figure 2In the embodiment of the present invention, substrate 60 including interconnect structure 64 is singulated into individual dies 68. Generally, each of dies 68 includes the same circuitry, such as the same devices and metallization patterns, although some or all of dies 68 may have different circuitry. Singulation may include sawing, dicing, etc.

[0085] The die 68 may include a logic die (e.g., a central processing unit, a graphics processing unit, a system-on-a-chip (SoC), a field-programmable gate array (FPGA), a microcontroller, etc.), a memory die (e.g., a dynamic random access memory (DRAM) die, a static random access memory (SRAM) die, etc.), a power management die (e.g., a power management integrated circuit (PMIC) die), a radio frequency (RF) die, a sensor die, a micro-electro-mechanical-system (MEMS) die, a signal processing die (e.g., a digital signal processing (DSP) die), a front-end die (e.g., an analog front-end (AFE) die), etc. or a combination thereof. Moreover, in some embodiments, the die 68 may have different surface areas, and in other embodiments, each die 68 may have the same surface area.

[0086] Figure 3 The bare die 68 is shown bonded to a carrier substrate 70. A bonding layer 72 may be formed on the carrier substrate 70, and the bonding layer 65 of each bare die 68 is bonded to the bonding layer 72 on the carrier substrate 70. The bonding layer 72 may include an oxide, such as silicon oxide, silicon oxynitride, etc., or a combination thereof, and may be formed by high density plasma chemical vapor deposition (HDP-CVD), flow chemical vapor deposition (FCVD) (e.g., deposition of chemical vapor deposition-based materials in a remote plasma system and post curing to convert them to oxides), atomic layer deposition (ALD), physical vapor deposition (PVD), etc., or a combination thereof. Other oxide materials formed by any acceptable process may be used to form the bonding layer 72 on the carrier substrate 70.

[0087] In one embodiment, each bare die 68 can be bonded to the carrier substrate 70 by a dielectric-to-dielectric bonding process (e.g., oxide-to-oxide bonding) to form a dielectric-to-dielectric bond (e.g., oxide-to-oxide bonding). The dielectric-to-dielectric bonding can be initiated by activating the bonding layer 65 and / or the bonding layer 72, followed by applying pressure, heat, and / or other bonding process steps to bond the bonding layer 65 to the surface of the bonding layer 72. The activation of the bonding layer 65 and the bonding layer 72 can be performed using, for example, dry processing, wet processing, plasma processing, exposure to H2, exposure to N2, exposure to O2, combinations thereof, etc. In embodiments using wet processing, for example, an RCA cleaning process can be used. Activation assists the dielectric-to-dielectric bonding of the bonding layer 65 and the bonding layer 72, for example, by allowing lower pressure and temperature to be used in a subsequent dielectric-to-dielectric bonding process. Through this treatment, the number of OH groups at the surface of the bonding layer 65 and / or the bonding layer 72 is increased. After the surfaces of the bonding layer 65 and / or the bonding layer 72 are activated, the bonding layer 65 and the bonding layer 72 can be contacted together at a relatively low temperature (e.g., room temperature) to form weak bonds. Subsequently, annealing is performed to strengthen the weak bonds and form a dielectric-to-dielectric bond. During the annealing, H of the OH bond is outgassed, thereby forming Si-O-Si bonds between the bonding layer 65 and the bonding layer 72, thereby strengthening the bond.

[0088] After the die 68 are bonded to the carrier substrate 70, gaps 67 may be provided between adjacent die 68. For example, the width W1 of the gap 67 between the first sidewall of the first die 68 and the second sidewall of the adjacent die 68 is in the range of 10 μm to 200 μm. In one embodiment, the height H1 of each die 68 is in the range of 100 μm to 500 μm, and each gap 67 may have a depth in the range of 100 μm to 500 μm.

[0089] exist Figure 4A in Figure 360 is performed on the structure shown in the figure to dope the top surface and sidewalls of each bare die 68 with fluorine. In detail, the top surface and sidewalls of the substrate 60 of each bare die 68 are doped with fluorine. The plasma treatment 80 is performed using a power source such as radio frequency (RF) or direct current (DC) to excite a gas mixture including fluorine and generate a fluorine plasma. When the gas molecules of the gas mixture are ionized and dissociated into charged particles (e.g., ions and electrons), a fluorine plasma is formed. The gas mixture may include CF4, C2F6, C4F8, etc. The top surface and sidewalls of the substrate 60 of each bare die 68 are exposed to the fluorine plasma for a specific duration, which allows fluorine atoms to penetrate the material of the substrate 60 and replace some atoms in the lattice structure of the substrate 60. The fluorine doping amount can be controlled by adjusting the duration of exposure and the concentration of fluorine in the gas mixture. After performing the plasma treatment 80, the doping concentration of fluorine in the top surface of each bare die 68 decreases in the longitudinal direction (as shown by arrow XX) from the top surface of the bare die 68 toward the bottom surface. In addition, the fluorine doping concentration and doping depth D2 of each sidewall of the bare wafer 68 (later Figure 5 68) decreases in the same longitudinal direction as arrow XX from the top surface of die 68 toward the bottom surface of die 68. In other embodiments, the top surface and sidewalls of each die 68 may be doped with boron or phosphorus instead of fluorine. This may also be achieved using plasma-based techniques.

[0090] Figure 4A Shown in Figure 3 The implantation process 81 is performed on the structure shown, as previously described in Figure 4A An alternative to performing the plasma treatment 80 described in . An implantation process 81 may be performed instead of the previously described plasma treatment 80 described in . Figure 4A The plasma treatment 80 described in the above. The implantation process 81 may be performed in Figure 3 An ion beam implantation process is performed on the structure shown to dope the top surface and sidewalls of each die 68 with fluorine. In detail, the top surface and sidewalls of the substrate 60 of each die 68 are doped with fluorine. In the implantation process 81, an implantation substance (e.g., a fluorine dopant) is introduced using an ion substance, which is ionized and accelerated using multiple ion beams to impact the substrate 60 of each die 68. This will cause thousands of atoms of the substrate 60 of each die 68 to be displaced from each ion implantation, and the fluorine dopant is subsequently distributed within the substrate 60. The amount of fluorine doping can be controlled by changing the energy and dosage of the multiple ion beams. As shown in FIG. Figure 4AAs shown, the implantation process 81 may direct the implanted substance (e.g., fluorine dopant) at an inclination angle θ1 relative to an axis 85 perpendicular to the main surface of the carrier substrate 70. In some embodiments, the inclination angle θ1 may be in a range of 0° to 15°. Performing the implantation process 81 by directing the implanted substance (e.g., fluorine dopant) at the inclination angle θ1 enables the sidewalls of each bare die 68 to be doped with fluorine. After performing the implantation process 81, the doping concentration of fluorine in the top surface of each bare die 68 decreases in the longitudinal direction moving from the top surface of the bare die 68 to the bottom surface (as shown by arrow XX). In addition, the doping concentration of fluorine in each sidewall of the bare die 68 and the doping depth D2 (subsequently in Figure 5 ) decreases in the longitudinal direction of arrow XX from the top surface of die 68 toward the bottom surface of die 68.

[0091] Figure 5 Shown in Figure 3 Executed on the structure shown Figure 4A Plasma treatment 80 or Figure 4A After the plasma treatment 80 or the implantation process 81 is performed, the top surface and the sidewalls of the substrate 60 of each bare die 68 are doped with fluorine to form a doped region 82. The doped region 82 may include a first doped region 82A on the top surface of the substrate 60 and a second doped region 82B in the sidewalls of the substrate 60. The first doped region 82A may be disposed between the second doped regions 82B. The substrate 60 of each bare die 68 may be doped so that the first doped region 82A extends longitudinally from the top surface of the substrate 60 to a depth D1 below the top surface of the substrate 60. The first doped region 82A may overlap with the through-hole 74, wherein the first doped region 82A is disposed above the top surface of the through-hole 74. In one embodiment, the doping concentration of fluorine in the first doped region 82A decreases in the longitudinal direction of the arrow XX above (e.g., from the top surface of the substrate 60 toward the bottom surface of the substrate 60).

[0092] The substrate 60 of each bare die 68 may be doped so that each second doped region 82B extends laterally from the corresponding sidewall of the substrate 60 to a depth D2 in the substrate 60. Each second doped region 82B is disposed between the sidewall of the substrate 60 and the corresponding through-hole 74, and each second doped region 82B may also extend below the first doped region 82A. In some embodiments, each second doped region 82B may extend along the entire sidewall of the substrate 60. In some embodiments, each second doped region 82B may extend only along a portion of the sidewall of the substrate 60. For example, each second doped region 82B may extend along the top portion of the sidewall of the substrate 60, while the bottom portion of the sidewall of the substrate 60 is not doped. In addition, the doping concentration of fluorine in each second doped region 82B decreases in the longitudinal direction of arrow XX (e.g., moving from the top surface of the substrate 60 to the bottom surface of the substrate 60). In addition, the doping concentration of fluorine in each second doped region 82B decreases in the lateral direction of arrow YY moving from the corresponding sidewall of the substrate 60 to the substrate 60. Each sidewall of the substrate 60 may include a first portion of the sidewall of the substrate 60 below the first doped region 82A. The doping depth D2 of each second doped region 82B decreases in the longitudinal direction of arrow XX from the highest point of the corresponding first portion of the sidewall to the lowest point of the second doped region 82B.

[0093] The top surface and sidewalls of the substrate 60 of each bare die 68 are doped by performing a plasma treatment 80 or an implantation process 81 to form a doped region 82, resulting in an increase in the hydrophobicity of the top surface and sidewalls of the substrate 60 (for example, the area of ​​the substrate 60 having the doped region 82). Hydrophobicity refers to the ability of a material to resist wetting, and the hydrophobicity of a specific location of the substrate 60 may correspond to the degree to which this location is doped with fluorine. Since the fluorine doping concentration in each second doped region 82B decreases in the longitudinal direction from the top surface of the substrate 60 toward the bottom surface of the substrate 60, the hydrophobicity of each sidewall of the substrate 60 also decreases in the longitudinal direction from the top surface of the substrate 60 toward the bottom surface of the substrate 60. In this way, in the subsequent gap filling process (in Figure 6During the process of filling the gaps 67 between the die 68 (described in the drawings), the top portion of the sidewalls of the substrate 60 of each adjacent die 68 has a greater hydrophobicity than the bottom portion of the sidewalls of the substrate 60 of each die 68. Therefore, the top portion of the sidewalls of the substrate 60 of each die 68 is more resistant to adhesion of the gap filling material to the top portion of the sidewalls than the bottom portion of the sidewalls. This results in the gap filling material being more likely to adhere to the bottom portion of the sidewalls in the gap 67 than to the top portion of the sidewalls in the gap 67. This allows each gap 67 to be filled from the bottom up, so that the bottom portion of the gap 67 is filled before the top portion of the gap 67 is filled. In addition, because the top surface of the substrate 60 of each die 68 has an increased hydrophobicity, the gap filling process does not accumulate residues on the top surface of the substrate 60 of each die 68, thereby eliminating the need for a residue cleaning process. In this way, the process can be simplified and the manufacturing cost can be reduced.

[0094] exist Figure 6 In the embodiment of the present invention, a gap filling process 83 is performed to fill the gaps 67 between the sidewalls of adjacent die 68 with dielectric material 84, and to surround each die 68 with dielectric material 84. The gap filling process includes a coating process, a curing process, and a thermal annealing process, which are performed to form a spin-on dielectric material (e.g., dielectric material 84) on the carrier substrate 70, such as Figure 6 . The coating process may include a spin coating process, etc. In one embodiment, the spin coating process is used to introduce a silicon-containing liquid precursor into the exposed surface of the bare die 68 (for example, in the gap 67), the bonding layer 65, and the bonding layer 72. The spin coating process is performed to globally deposit the silicon-containing liquid precursor on the carrier substrate 70, which may include filling the gap 67 between adjacent bare die 68. Due to the difference in hydrophobicity of the exposed surface of the above-mentioned substrate 60, the spin coating process may be a bottom-up process, so that the bottom of the gap 67 is filled before the top of the gap 67. In one embodiment, the silicon-containing liquid precursor includes perhydro-polysilazane (PHPS). The chemical formula of the perhydro-polysilazane compound is (SiH2NH) n, wherein n is a positive integer. The perhydropolysilazane compound includes a Si-N bond as a repeating unit and is a silicon-containing polymer composed of Si, N and H. The perhydropolysilazane compound has a linear structure, a chain structure, a cross-linked structure or a cyclic structure in the molecule. After the coating process, the silicon-containing liquid precursor may partially fill the gap 67 (for example, the highest point of the silicon-containing liquid precursor is below the highest surface of the bare wafer 68). Due to the hydrophobicity of the top portion of the sidewall of the bare wafer 68, the top surface of the silicon-containing liquid precursor in the gap 67 may have a curved (for example, convex) surface.

[0095] Advantages can be achieved by performing a plasma treatment 80 or an implantation process 81 to dope the top surface and sidewalls of the substrate 60 of each die 68 with a fluorine dopant to form doped regions 82. This results in an increase in the hydrophobicity of the top surface and sidewalls of the substrate 60 of each die 68. Because the doping concentration of fluorine in each second doped region 82B decreases in the longitudinal direction from the top surface of the substrate 60 toward the bottom surface of the substrate 60, the hydrophobicity of each sidewall of the substrate 60 also decreases in the longitudinal direction from the top surface of the substrate 60 toward the bottom surface of the substrate 60. A coating process of a gap filling process 83 is then performed to fill the gaps 67 between the sidewalls of adjacent die 68 with a silicon-containing liquid precursor of a dielectric material 84. These advantages include that the top portion of the sidewall of the substrate 60 of each adjacent die 68 is more resistant to adhesion of the silicon-containing liquid precursor than the bottom portion of the sidewall. This is because the top portion of the sidewall of the substrate 60 of each bare die 68 is more hydrophobic than the bottom portion of the sidewall of the substrate 60 of each bare die 68. This results in the silicon-containing liquid precursor being more likely to adhere to the bottom portion of the sidewall in the gap 67 than the top portion of the sidewall in the gap 67. This allows each gap 67 to be filled from the bottom up, where the bottom portion of the gap 67 is filled before the top portion of the gap 67 is filled. In this way, gaps 67 having a larger depth (e.g., having a depth in the range of 100 μm to 500 μm) can be filled with the silicon-containing liquid precursor of the dielectric material 84 without forming large voids in the silicon-containing liquid precursor or the subsequently formed dielectric material 84. This results in improved device reliability and device performance.

[0096] In addition, filling the gap 67 from the bottom up with a silicon-containing liquid precursor also results in a reduction in the surface roughness of the subsequently formed dielectric material 84, thereby allowing the surface roughness of the dielectric material 84 to be measured by a 10 Angstrom stylus (e.g., the arithmetic average roughness (Ra) of the dielectric material 84 is less than or equal to 10 Angstroms). The reduced surface roughness allows the dielectric material 84 to form a better bonding interface to bond with other subsequently formed layers, components or structures. In this way, the reliability of the device is improved. In addition, due to the hydrophobicity of the top surface of each substrate 60 of the bare die 68, no residue accumulates on the top surface of the bare die 68 after the coating process of the gap filling process 83 is performed, thereby eliminating the need for a cleaning process after performing the gap filling process 83.

[0097] Since the perhydropolysilazane compound includes a silicon-containing polymer composed of Si, N, and H, the silicon-containing liquid precursor of the dielectric material 84 formed on the carrier substrate 70 and in the gap 67 is a material containing silicon and nitrogen, and is converted into a material containing silicon and oxygen by oxidation during a subsequent thermal treatment process described below.

[0098] After performing the coating process of the gap filling process 83, a curing process may then be performed. The curing process is performed to remove moisture or solvent from the silicon-containing liquid precursor of the dielectric material 84 to form a solid phase of the dielectric material 84. In some embodiments, the curing process may be performed using a hot plate, an oven, a heating chamber, or the like. An ultraviolet (UV) light source may provide radiation to generate heat energy required to remove moisture or solvent from the silicon-containing liquid precursor of the dielectric material 84. In some embodiments, the curing process is an ultraviolet thermal curing process and is performed by exposing the substrate to ultraviolet heat energy with or without a curing gas. The curing process may be performed at a temperature in the range of 20°C to 400°C. During the curing process, the Si-N and Si-H bonds of the perhydropolysilazane compound are decomposed to form silicon nitride.

[0099] After performing the curing process of the gap filling process 83, a thermal annealing process is performed to anneal the dielectric material 84 and convert it from silicon nitride to silicon oxide. The thermal energy provided by the thermal annealing process can also increase the density (densify) and strengthen the bonding structure of the dielectric material 84. During the thermal annealing process, an annealing gas including at least one oxygen-containing gas is supplied. The oxygen from the oxygen-containing gas reacts with the silicon atoms and converts the silicon nitride into silicon oxide. The thermal energy provided by the thermal annealing process breaks the Si-N bonds, allowing the oxygen atoms to bond and attach to the silicon atoms to form the annealed dielectric material 84 including silicon oxide. Therefore, the temperature during the thermal annealing process is generally predetermined to provide sufficient thermal energy to convert the Si-N bonds into Si-O bonds, thereby forming the desired silicon oxide material. During the thermal annealing process, the supplied oxygen-containing gas may include O2, O3, steam (H2O), H2O2, air, CO2, CO, etc. or a combination thereof. During the thermal annealing process, the process temperature may be greater than 350°C, such as in the range of 400°C to 1200°C.

[0100] exist Figure 7 In the process, a planarization step (e.g., a grinding process, a chemical mechanical polishing process, etc.) may be performed to thin down the die 68 and level the top surface of the dielectric material 84. After the planarization process, the top surface of the die 68 (e.g., the substrate 60 of each die 68) and the top surface of the dielectric material 84 are substantially coplanar. The planarization process may remove the entire first doped region 82A of each die 68. In addition, the top portion of the second doped region 82B of each die 68 may also be removed during the planarization step. As a result, after the planarization step is performed, the top surface of the central region of each die 68 overlapping the corresponding through-hole 74 is not doped. However, the bottom portion of the second doped region 82B remains on the sidewall of the substrate 60 of each die 68.

[0101] Figure 8 Shows that previously Figure 7 The planarization steps described in can continue to further thin the die 68 and the dielectric material 84 until the top surface of the through-hole 74 is exposed and the top surface of the die 68 (e.g., the substrate 60 of each die 68), the top surface of the dielectric material 84, and the top surface of the through-hole 74 are substantially coplanar.

[0102] Further references Figure 8 , conductive connectors 88 are formed on the top surface of the die 68 and the top surface of the through-hole 74. The conductive connectors 88 may be formed of metal (e.g., copper, aluminum, etc.) and may be formed by, for example, plating. The conductive connectors 88 may be conductive posts, pads, etc. for external connection. The conductive connectors 88 may be electrically connected to the through-hole 74 and the interconnect structure 64.

[0103] Then, a dielectric layer 86 is formed to laterally encapsulate the conductive connector 88. The dielectric layer 86 may be an oxide, a nitride, a carbide, a polymer, or the like, or a combination thereof. The dielectric layer 86 may be formed, for example, by spin coating, lamination, chemical vapor deposition (CVD), or the like. Initially, the dielectric layer 86 may bury the conductive connector 88 so that the top surface of the dielectric layer 86 is above the top surface of the conductive connector 88. The conductive connector 88 may be exposed through the dielectric layer 86 by a removal process, which may be applied to each layer to remove excess material above the conductive connector 88. The removal process may be a planarization process, such as chemical mechanical polishing (CMP), etch-back, or a combination thereof. After the planarization process, the top surfaces of the conductive connector 88 and the dielectric layer 86 are coplanar (within the variation of the process).

[0104] exist Fig. 9 In the embodiment of the present invention, die 89 is bonded to its corresponding die 68. Die 89 may then be referred to as the top die, and die 68 may then be referred to as the bottom die. Die 89 may be similar to die 68, and may be bonded to the corresponding die 68 using the same techniques as previously described. Figure 1 to Figure 2 89. For example, each die 89 may include a substrate 96 and an interconnect structure 94, which may include similar materials as substrate 60 and interconnect structure 64, respectively, and may be formed using similar processes. In addition, the die 89 may include or not include through-holes (TVs) similar to through-holes 74 of the die 68. Devices such as transistors, capacitors, resistors, diodes, etc. may be formed in the active surface of the substrate 96 of each die 89 and / or on the active surface of the substrate 96 of each die 89. In addition, each die 89 may include a conductive connector 92 and a dielectric layer 90 that may be in the interconnect structure 94 of the die 89 and / or on the interconnect structure 94 of the die 89. The conductive connector 92 may be formed using similar processes and materials as the conductive connector 88. The dielectric layer 90 may be formed using similar processes and materials as the dielectric layer 86.

[0105] In some embodiments, each die 68 and the corresponding die 89 are bonded such that the active surface of the die 89 and the back side of the die 68 face each other (e.g., "face-to-back" bonding). For example, each die 68 is bonded to the corresponding die 89 using a hybrid bonding process such that the dielectric layer 90 of the interconnect structure 94 is bonded to the dielectric layer 86 by dielectric-to-dielectric bonding without using any adhesive material (e.g., die attach film), and the conductive connector 92 is bonded to the conductive connector 88 by metal-to-metal bonding without using any eutectic material (e.g., solder). The bonding may include pre-bonding and annealing. During pre-bonding, a small pressing force may be applied to press the die 89 against the die 68. The pre-bonding is performed at a low temperature (e.g., room temperature), such as a temperature in the range of 15° C. to 30° C., and after the pre-bonding, the dielectric layer 90 is bonded to the dielectric layer 86. The bond strength is then improved in a subsequent annealing step, wherein the dielectric layer 90 and the dielectric layer 86 are annealed at a high temperature (e.g., a temperature in the range of 140° C. to 500° C.). After annealing, bonds, such as fusion bonds, are formed that join the dielectric layer 90 and the dielectric layer 86. For example, the bonds may be covalent bonds between the material of the dielectric layer 90 and the material of the dielectric layer 86. In addition, due to the annealing process, the materials of the conductive connector 92 and the conductive connector 88 may inter-diffuse and bond together. The conductive connector 92 and the conductive connector 88 are connected to each other in a one-to-one correspondence. The conductive connector 92 and the conductive connector 88 may be in physical contact after pre-bonding, or may expand during annealing to form physical contact. In addition, during annealing, the materials (e.g., copper) of the conductive connector 92 and the conductive connector 88 intermingle, so that a metal-to-metal bond is also formed. As such, the resulting bond between die 68 and die 89 is a hybrid bond that includes both dielectric-to-dielectric bonding and metal-to-metal bonding.

[0106] In this way, each die 68 is electrically connected to the corresponding die 89 . For example, the interconnect structure 94 of each die 89 can be electrically connected to the interconnect structure 64 of the corresponding die 68 through the through-hole 74 .

[0107] After bonding the die 89 to the die 68 corresponding thereto, a gap 91 may be provided between adjacent die 89. For example, a width W2 of the gap 91 between a first sidewall of a first die 89 and a second sidewall of an adjacent die 89 is in a range of 10 μm to 200 μm. In one embodiment, the width W2 may be different from the width W1. In one embodiment, the width W2 may be less than or greater than the width W1. In one embodiment, a height H2 of each die 89 is in a range of 100 μm to 500 μm. In one embodiment, each gap 91 may have a depth in a range of 100 μm to 500 μm.

[0108] exist Fig.10 in Fig. 9 Process 98 is performed on the structure shown. Process 98 may be similar to that previously described in Figure 4A The plasma treatment 80 described in the plasma treatment, or process 98, may be similar to that previously described in Figure 4A The implantation process 81 described in the implantation process.

[0109] Fig.11 Shown in Fig.10 89. The structure after performing process 98 (e.g., plasma treatment or implantation process) on the structure shown. After performing process 98, the top surface and sidewalls of the substrate 96 of each bare die 89 are doped with fluorine to form doped regions 100. The doped regions 100 may include a first doped region 100A in the top surface of the substrate 96 and a second doped region 100B in the sidewalls of the substrate 96. The first doped region 100A may be disposed between the second doped regions 100B. The substrate 96 of each bare die 89 may be doped so that the first doped region 100A extends longitudinally from the top surface of the substrate 96 to a depth D3 below the top surface of the substrate 96. In one embodiment, the doping concentration of fluorine in the first doped region 100A decreases in the longitudinal direction AA from the top surface of the substrate 96 toward the bottom surface of the substrate 96.

[0110] The substrate 96 of each bare die 89 may be doped so that each second doped region 100B extends laterally from a corresponding sidewall of the substrate 96 to a depth D4 in the substrate 96. Each second doped region 100B is disposed between the sidewall of the substrate 96 and the corresponding through-hole (if present), and each second doped region 100B may also extend below the first doped region 100A. Each second doped region 100B may extend along the entire sidewall of the substrate 96. In one embodiment, each second doped region 100B may extend only along a portion of the sidewall of the substrate 96. For example, each second doped region 100B may extend along the top portion of the sidewall of the substrate 96, while the bottom portion of the sidewall of the substrate 96 is not doped. In addition, the doping concentration of fluorine in each second doped region 100B decreases in the longitudinal direction of arrow AA (e.g., moving from the top surface of the substrate 96 to the bottom surface of the substrate 96). In addition, the doping concentration of fluorine in each second doped region 100B decreases in the lateral direction of arrow BB moving from the corresponding sidewall of the substrate 96 to the substrate 96. Each sidewall of substrate 96 may include a first portion of the sidewall of substrate 96 below first doped region 100A. Doping depth D4 of each second doped region 100B decreases in the longitudinal direction of arrow BB from the highest point of the corresponding first portion of the sidewall to the lowest point of second doped region 100B.

[0111] Doping the top surface and sidewalls of the substrate 96 of each die 89 by performing the process 98 to form the doped regions 100 results in an increase in the hydrophobicity at the top surface and sidewalls of the substrate 96. Because the fluorine doping concentration in each second doped region 100B decreases in the longitudinal direction from the top surface of the substrate 96 toward the bottom surface of the substrate 96, the hydrophobicity of each sidewall of the substrate 96 decreases in the longitudinal direction from the top surface of the substrate 96 toward the bottom surface of the substrate 96. As a result, in the subsequent gap filling process ( Fig.12During the process of filling the gaps 91 between the die 89 (described in ), the top portion of the sidewalls of the substrate 96 of each adjacent die 89 has a greater hydrophobicity than the bottom portion of the sidewalls of the substrate 96 of each die 89. Therefore, the top portion of the sidewalls of the substrate 96 of each die 89 is more resistant to the gap filling material adhering to the top portion of the sidewalls than the bottom portion of the sidewalls. This results in the gap filling material being more likely to adhere to the bottom portion of the sidewalls in the gap 91 than to the top portion of the sidewalls in the gap 91. This allows each gap 91 to be filled from the bottom up, where the bottom portion of the gap 91 is filled before the top portion of the gap 91 is filled. In addition, because the top surface of the substrate 96 of each die 89 has an increased hydrophobicity, the gap filling process does not accumulate residues on the top surface of the substrate 96 of each die 89, thereby eliminating the need for a cleaning process for the residues. In this way, processing can be simplified and manufacturing costs can be reduced.

[0112] exist Fig.12 In the embodiment of the present invention, a gap filling process 99 is performed to fill the gaps 91 between the sidewalls of adjacent die 89 with dielectric material 102 and surround each die 89 with dielectric material 102. The gap filling process 99 may be similar to that previously described in Figure 6 The gap filling process 83 described in the foregoing and similar processes and similar materials may be used to fill the gap 91 between the sidewalls of adjacent die 89 with dielectric material 102. For example, the gap filling process 99 includes a coating process, a curing process, and a thermal annealing process, which are performed to form a spin-on dielectric material (e.g., dielectric material 102) over the dielectric material 84 and the carrier substrate 70. In embodiments where the width W2 is greater than the width W1, the dielectric material 102 is also formed to overlap a portion of the die 68. The coating process, the curing process, and the thermal annealing process are similar to those previously described. Figure 6 The coating process, curing process, and thermal annealing process described in the gap filling process 83 are similar.

[0113] Advantages can be achieved by performing process 98 to dope the top surface and sidewalls of substrate 96 of each die 89 with a fluorine dopant to form doped regions 100. This results in an increase in the hydrophobicity of the top surface and sidewalls of substrate 96 of each die 89. Because the doping concentration of fluorine in each second doped region 100B decreases in the longitudinal direction from the top surface of substrate 96 toward the bottom surface of substrate 96, the hydrophobicity of each sidewall of substrate 96 also decreases in the longitudinal direction from the top surface of substrate 96 toward the bottom surface of substrate 96. A coating process of gap filling process 99 is then performed to fill gaps 91 between the sidewalls of adjacent die 89 with a silicon-containing liquid precursor of dielectric material 102. Advantages include that the top portion of the sidewall of substrate 96 of each adjacent die 89 is more resistant to adhesion of the silicon-containing liquid precursor than the bottom portion of the sidewall. This is because the top portion of the sidewall of the substrate 96 of each bare die 89 is more hydrophobic than the bottom portion of the sidewall of the substrate 96 of each bare die 89. This results in the silicon-containing liquid precursor being more likely to adhere to the bottom portion of the sidewall in the gap 91 than the top portion of the sidewall in the gap 91. This allows each gap 91 to be filled from the bottom up, where the bottom portion of the gap 91 is filled before the top portion of the gap 91 is filled. In this way, the gap 91 having a larger depth (e.g., having a depth in the range of 100 μm to 500 μm) can be filled with the silicon-containing liquid precursor of the dielectric material 102 without forming large voids in the silicon-containing liquid precursor or the subsequently formed dielectric material 102. This results in improved device reliability and device performance.

[0114] In addition, filling the gap 91 from the bottom up with a silicon-containing liquid precursor also results in a reduction in the surface roughness of the subsequently formed dielectric material 102, thereby allowing the surface roughness of the dielectric material 102 to be measured by a 10 angstrom stylus (e.g., the arithmetic average roughness (Ra) of the dielectric material 102 is less than or equal to 10 angstroms). The reduced surface roughness allows the dielectric material 102 to form a better bonding interface to bond with other subsequently formed layers, components or structures. In this way, the reliability of the device is improved. In addition, due to the hydrophobicity of the top surface of each substrate 96 of the bare die 89, no residue accumulates on the top surface of the bare die 89 after the coating process of the gap filling process 99 is performed, thereby eliminating the need to perform a cleaning process after the gap filling process 99.

[0115] After performing the coating process, the curing process, and the thermal annealing process of the gap filling process 99 , a dielectric material 102 including silicon oxide is disposed between sidewalls of adjacent dies 89 (eg, within the gap 91 ). In addition, the dielectric material 102 surrounds each die 89 .

[0116] exist Fig.13During the process, a planarization step (e.g., a grinding process, a chemical mechanical polishing process, etc.) may be performed to thin the die 89 and level the top surface of the dielectric material 102. After the planarization process, the top surface of the die 89 (e.g., the substrate 96 of each die 89) and the top surface of the dielectric material 102 are substantially coplanar. The planarization process may remove the entire first doped region 100A of each die 89. In addition, the top portion of the second doped region 100B of each die 89 may also be removed during the planarization step. As a result, after the planarization step is performed, the top surface of the central region of each die 89 is undoped. However, the bottom portion of the second doped region 100B remains on the sidewalls of the substrate 96 of each die 89.

[0117] Fig.13 Also shown is a carrier substrate 106 bonded to the top surface of the die 89 and the dielectric material 102 after the planarization step. The carrier substrate 106 may be a semiconductor substrate (e.g., a silicon substrate or wafer), a glass carrier substrate, a ceramic carrier substrate, etc. The carrier substrate 106 is bonded to the top surface of the die 89 and the dielectric material 102 using a suitable technique such as dielectric-to-dielectric bonding. For example, in various embodiments, the top surface of the die 89 and the dielectric material 102 may be bonded to the surface of the carrier substrate 106 using dielectric-to-dielectric bonding using a bonding layer 104A on the top surface of the die 89 and the dielectric material 102 and a bonding layer 104B on the surface of the carrier substrate 106. In some embodiments, the bonding layer 104A and the bonding layer 104B may each include silicon oxide formed on the top surface of the die 89 and the dielectric material 102 and the surface of the carrier substrate 106 by a deposition process such as chemical vapor deposition (CVD), physical vapor deposition (PVD), etc. In other embodiments, the bonding layer 104B may be formed by thermal oxidation of the silicon surface on the carrier substrate 106.

[0118] Prior to bonding, at least one of the bonding layer 104A or the bonding layer 104B may be subjected to surface treatment. The surface treatment may include plasma treatment. The plasma treatment may be performed in a vacuum environment. After the plasma treatment, the surface treatment may further include a cleaning process (e.g., cleaning with deionized water, etc.) that may be applied to the bonding layer 104A and / or the bonding layer 104B. The carrier substrate 106 is then aligned and pressed against the top surface of the bare die 89 and the dielectric material 102 to perform pre-bonding of the bare die 89 and the dielectric material 102 to the carrier substrate 106. The pre-bonding may be performed at room temperature (between about 20 degrees and about 25 degrees). After the pre-bonding, the bare die 89 and the dielectric material 102 and the carrier substrate 106 are bonded to each other. The bonding process may be enhanced by a subsequent annealing step. For example, this may be accomplished by heating the bare die 89, the dielectric material 102, and the carrier substrate 106 to a temperature of about 170 degrees for about 1 hour.

[0119] exist Fig.14 In the embodiment of the present invention, after attaching the carrier substrate 106 to the top surface of the bare die 89 and the dielectric material 102, a planarization process may be performed to remove the carrier substrate 70. In some embodiments, the planarization process may be a chemical mechanical polishing planarization process, an etch-back process, a combination thereof, etc. However, any suitable planarization process may be utilized. In addition, according to some embodiments, the planarization process further removes the first bonding layer 72. In addition, the planarization process may remove portions of the bonding layer 65 and the dielectric material 84. In one embodiment, after the planarization process, the bottom surfaces of the bonding layer 65 and the dielectric material 84 are flush.

[0120] Fig.14 Further shown is a redistribution structure 170 formed over the bonding layer 65 and the bottom surface of the dielectric material 84 . Fig.14 Also shown are die connectors 171 formed through bonding layer 65 that allow redistribution structure 170 to be physically and electrically coupled to die 89 and die 68 .

[0121] In one embodiment, an opening (not separately shown) is formed through the bonding layer 65 to expose the metallization pattern within the interconnect structure 64. A bare die connector 171, such as a conductive post (e.g., formed of a metal such as copper), extends through the opening in the bonding layer 65 and is physically and electrically coupled to the metallization pattern within the interconnect structure 64. The bare die connector 171 may be formed, for example, by plating.

[0122] In addition, in one embodiment, the redistribution structure 170 includes a redistribution dielectric layer 176 and a redistribution metallization pattern 174. The redistribution metallization pattern 174 may also be referred to as a redistribution layer or a redistribution line. The redistribution structure 170 is shown as an example having one layer of metallization pattern. More dielectric layers and metallization patterns may be formed in the redistribution structure 170. If more dielectric layers and metallization patterns are to be formed, the steps and processes discussed below may be repeated.

[0123] In one embodiment, the redistribution metallization pattern 174 includes conductive elements that are physically coupled and electrically coupled to the bare die connector 171. As an example of forming the redistribution metallization pattern 174, a seed layer is formed on the bonding layer 65 and the bottom surface of the dielectric material 84 (e.g., on the bare die connector 171). In some embodiments, the seed layer is a metal layer, which may be a single layer or a composite layer including multiple sub-layers formed of different materials. In some embodiments, the seed layer includes a titanium layer and a copper layer on the titanium layer. The seed layer may be formed using, for example, physical vapor deposition. A photoresist is then formed on the seed layer and patterned. The photoresist may be formed by spin coating, etc., and may be exposed to patterning. The pattern of the photoresist corresponds to the redistribution metallization pattern 174. The aforementioned patterning forms an opening through the photoresist to expose the seed layer. Then, a conductive material is formed in the opening of the photoresist and on the exposed portion of the seed layer. The conductive material may be formed by plating, such as electroplating or chemical plating. The conductive material may include a metal such as copper, titanium, tungsten, aluminum, etc. The combination of the conductive material and the portion of the seed layer below it forms the redistribution metallization pattern 174. The photoresist and the portion of the seed layer on which the conductive material is not formed are removed. The photoresist may be removed by an acceptable ashing or stripping process, such as using an oxygen plasma, etc. Once the photoresist is removed, the exposed portion of the seed layer is removed, such as by using an acceptable etching process, such as by wet etching or dry etching.

[0124] In one embodiment, the redistribution dielectric layer 176 is deposited on the redistribution metallization pattern 174 and on the bottom surface of the bonding layer 65 and the dielectric material 84. In some embodiments, the redistribution dielectric layer 176 is formed of a photosensitive material such as polybenzoxazole (PBO), polyimide, benzocyclobutene (BCB), etc., which can be patterned using a lithography mask. The redistribution dielectric layer 176 can be formed by spin coating, lamination, chemical vapor deposition, etc. or a combination thereof. The redistribution dielectric layer 176 is then patterned. The aforementioned patterning forms an opening that exposes a portion of the redistribution metallization pattern 176. The aforementioned patterning can be performed by an acceptable process, such as by exposing and developing the redistribution dielectric layer 176 when the redistribution dielectric layer 176 is a photosensitive material, or by using an etch such as an anisotropic etch.

[0125] After patterning the redistribution dielectric layer 176, under bump metallizations (UBMs) 107 are formed for external connection to the redistribution structure 170 and the overlying die 68 and die 89. The under bump metallization 107 has a bump portion extending along the major surface of the redistribution dielectric layer 176, and has a via portion extending through the redistribution dielectric layer 176 to physically and electrically couple to the redistribution metallization pattern 174. In this way, the under bump metallization 107 is electrically coupled to the overlying die 68 and die 89. The under bump metallization 107 can be formed of the same material as the redistribution metallization pattern 174. In some embodiments, the under bump metallization 107 has a different size than the redistribution metallization pattern 174.

[0126] In addition, in one embodiment, the conductive connector 108 is formed on the under bump metal 107. The conductive connector 108 may be a ball grid array (BGA) connector, a solder ball, a metal column, a controlled collapse chip connection (C4) bump, a microbump, a bump formed by electroless nickel-electroless palladium-immersion gold technique (ENEPIG), etc. The conductive connector 108 may include a conductive material, such as solder, copper, aluminum, gold, nickel, silver, palladium, tin, etc. or a combination thereof. In some embodiments, the conductive connector 108 is formed by initially forming a solder layer by evaporation, electroplating, printing, solder transfer, ball placement, etc. Once the solder layer is formed on the structure, reflow may be performed to shape the material into a desired bump shape. In another embodiment, the conductive connector 108 includes a metal column (e.g., a copper column) formed by sputtering, printing, electroplating, chemical plating, chemical vapor deposition, etc. The metal pillars may be solder-free and have substantially longitudinal sidewalls. In some embodiments, a metal capping layer is formed on top of the metal pillars. The metal capping layer may include nickel, tin, tin-lead, gold, silver, palladium, indium, nickel-palladium-gold, nickel-gold, etc. or a combination thereof, and may be formed by a plating process.

[0127] exist Fig.15 In the Fig.14 The singulation process may include a mechanical process, such as a segmentation process, a cutting process, etc. In some embodiments, the singulation process may include an etching process, a laser process, a mechanical process, and / or a combination thereof. The singulation process will Fig.14 The structure shown in FIG. 1 is singulated into a plurality of integrated circuit device stacks 10 . Fig.15 The resulting one singulated integrated circuit device stack 10 is shown. The singulated integrated circuit device stack 10 may be further processed and integrated as a component of a semiconductor package as described in further detail below.

[0128] Fig.16 A cross-sectional view of a package body 20 incorporating an integrated circuit device stack 10 as a package component according to some embodiments is shown. Unless otherwise specified, the same reference symbols in this embodiment (and the embodiments discussed later) represent components formed by the same process. Figures 1 to 15 The same components as in the illustrated embodiments, therefore, the process steps and applicable materials are not repeated here. Figures 1 to 15The integrated circuit device stack 10 described in the embodiment is further packaged to form a package 20. The package 20 may also be referred to as an integrated fan-out (InFO) package. Fig.16 Only one integrated circuit device stack 10 is shown, but the package 20 may include more than one integrated circuit device stack 10 .

[0129] The package body 20 includes a first package component 200, the first package component 200 including an integrated circuit device stack 10, the integrated circuit device stack 10 is disposed on and electrically connected to the front side redistribution structure 218. The integrated circuit device stack 10 is connected by connecting the conductive connector 108 (previously Fig.14 Described in but Fig.16 The first package component 200 may further include a rear side redistribution structure 222 and a through-hole 224 extending through the encapsulant 202, which electrically connects the rear side redistribution structure 222 to the front side redistribution structure 218. In the illustrated embodiment, the rear side redistribution structure 222 may include one or more dielectric layers and at least one metallization pattern (sometimes referred to as a redistribution layer or a redistribution line).

[0130] The under bump metal 304 may be disposed on the front side redistribution structure 218 and electrically connected to the front side redistribution structure 218. The under bump metal 304 may be made of the same material as the metallization pattern of the front side redistribution structure 218. The conductive connector 302 is disposed on the under bump metal 304 and electrically connected to the under bump metal 304. The conductive connector 302 may be a ball grid array (BGA) connector, a solder ball, a metal pillar, a controlled collapse wafer connection (C4) bump, a micro bump, a bump formed by chemical nickel palladium gold (ENEPIG), etc. The conductive connector 302 may include a conductive material, such as solder, copper, aluminum, gold, nickel, silver, palladium, tin, etc. or a combination thereof.

[0131] The package substrate 300 may be coupled to the first package component 200 using a conductive connector 302. The package substrate 300 may include a printed circuit board (PCB). In one embodiment, the package substrate 300 includes a substrate core 310 and a bonding pad 306 on the substrate core 310. The substrate core 310 may be made of a semiconductor material such as silicon, germanium, diamond, etc. Alternatively, compound materials such as silicon germanium, silicon carbide, gallium arsenide, indium arsenide, indium phosphide, silicon germanium carbide, gallium arsenide phosphide, gallium indium phosphide, combinations of these, etc. may also be used. In addition, the substrate core 310 may be a semiconductor-on-insulator substrate. Generally, a semiconductor-on-insulator substrate includes a semiconductor material layer such as epitaxial silicon, germanium, silicon germanium, semiconductor on insulator, silicon germanium on insulator (SGOI), or a combination thereof. In an alternative embodiment, the substrate core 310 is based on an insulating core, such as a fiberglass reinforced resin core. An exemplary core material is a fiberglass resin, such as FR (flameretardant) 4. Alternative core materials include bismaleimide-triazine resin (BTresin), or other printed circuit board materials or films. Build-up films such as Ajinomoto build-up film (ABF) or other laminated materials can be used for substrate core 310.

[0132] The substrate core 310 may include active devices as well as passive devices (not shown). Various devices such as transistors, capacitors, resistors, combinations thereof, etc. may be used to generate the structural and functional requirements of the design of the device stack. Such devices may be formed using any suitable method.

[0133] The substrate core 310 may also include metallization layers and vias (not shown), wherein the bonding pads 306 are physically and / or electrically coupled to the metallization layers and vias. The metallization layers may be formed over active devices and passive devices and are designed to connect various devices to form functional circuits. The metallization layers may be formed of alternating layers of dielectric materials (e.g., low-k dielectric materials) and conductive materials (e.g., copper), with vias interconnecting the conductive material layers, and may be formed by any suitable process (e.g., deposition, damascene, dual damascene, etc.). In some embodiments, the substrate core 310 is substantially free of active devices and passive devices.

[0134] In some embodiments, the conductive connector 302 is reflowed to attach the first package component 200 to the bonding pad 306. The conductive connector 302 electrically and / or physically couples the package substrate 300 including the metallization layer in the substrate core 310 to the first package component 200. In some embodiments, a solder resist 308 is formed on the substrate core 310. The conductive connector 302 can be disposed in an opening in the solder resist 308 to electrically and mechanically couple to the bonding pad 306. The solder resist 308 can be used to protect areas of the substrate core 310 from external damage.

[0135] The conductive connector 302 may have an epoxy flux (not shown) formed thereon before reflow, wherein at least some epoxy portion of the epoxy flux remains after the first package component 200 is attached to the package substrate 300. The remaining epoxy portion may function as an underfill to reduce stress and protect joints created by reflowing the conductive connector 302. In some embodiments, an underfill 320 may be formed between the first package component 200 and the package substrate 300 and around the conductive connector 302. The underfill 320 may be formed by a capillary flow process after the first package component 200 is attached, or may be formed by a suitable deposition method before the first package component 200 is attached.

[0136] In one embodiment, the package substrate 300 may include a bonding pad 312 on the substrate core 310. A conductive connector 314 may be coupled to the bonding pad 312 to allow the package substrate 300 to be electrically coupled to an external circuit or device. The conductive connector 314 may be a ball grid array (BGA) connector, a solder ball, a metal column, a controlled collapse wafer connection (C4) bump, a microbump, a bump formed by chemical nickel palladium gold (ENEPIG), etc. The conductive connector 314 may include a conductive material, such as solder, copper, aluminum, gold, nickel, silver, palladium, tin, etc. or a combination thereof. In some embodiments, a solder resist 308 is formed on the substrate core 310, and the conductive connector 314 may be disposed in an opening in the solder resist 308 to electrically couple and mechanically couple to the bonding pad 312. The solder resist 308 may be used to protect an area of ​​the substrate core 310 from external damage.

[0137] In some embodiments, passive devices (e.g., surface mount devices (SMDs), not shown) may also be attached to the first package component 200 (e.g., under bump metallurgy 304) or the package substrate 300 (e.g., bonding pads 306). For example, the passive device may be bonded to the same surface of the first package component 200 or the package substrate 300 as the conductive connector 302. The passive device may be attached to the first package component 200 before mounting the first package component 200, or may be attached to the package substrate 300 before or after mounting the first package component 200 on the package substrate 300.

[0138] The second package component 400 is coupled to the first package component 200 using a conductive connector 418. The conductive connector 418 can be disposed on the metallization pattern of the rear side redistribution structure 222 of the first package component 200 and electrically connected to the metallization pattern of the rear side redistribution structure 222 of the first package component 200. The second package component 400 includes, for example, a substrate 412 and one or more stacked dies (e.g., stacked die 402A and stacked die 402B) coupled to the substrate 412. Although a group of stacked dies (stacked die 402A and stacked die 402B) is shown, in other embodiments, a plurality of stacked dies (each having one or more stacked dies) can be disposed side by side and coupled to the same surface of the substrate 412. The substrate 412 can be made of a semiconductor material, such as silicon, germanium, diamond, etc. In some embodiments, compound materials such as silicon germanium, silicon carbide, gallium arsenide, indium arsenide, indium phosphide, silicon germanium carbide, gallium arsenic phosphide, gallium indium phosphide, combinations of these, etc. can also be used. In addition, substrate 412 may be a semiconductor on insulator (SOI) substrate. Generally, a semiconductor on insulator substrate includes a semiconductor material layer, such as epitaxial silicon, germanium, silicon germanium, semiconductor on insulator, silicon germanium on insulator (SGOI), or a combination thereof. In an alternative embodiment, substrate 412 is based on an insulating core, such as a fiberglass reinforced resin core. An exemplary core material is a fiberglass resin, such as FR4. Alternatives to the core material include triazine (BT) resin, or other printed circuit board (PCB) materials or films. A laminated film such as Ajinomoto laminated film (ABF) or other laminated materials may be used for substrate 412.

[0139] Substrate 412 may include active devices as well as passive devices (not shown). Various devices such as transistors, capacitors, resistors, combinations thereof, etc. may be used to generate the structural and functional requirements of the design of second package component 400. Any suitable method may be used to form the devices.

[0140] The substrate 412 may also include metallization layers (not shown) and conductive vias 414. The metallization layers may be formed over active devices and passive devices and are designed to connect various devices to form functional circuits. The metallization layers may be formed of alternating layers of dielectric materials (e.g., low-k dielectric materials) and conductive materials (e.g., copper), with vias interconnecting the conductive material layers, and may be formed by any suitable process (e.g., deposition, damascene, dual damascene, etc.). In some embodiments, the substrate 412 is substantially free of active devices and passive devices.

[0141] The substrate 412 may have a bonding pad 410 and a bonding pad 416, the bonding pad 410 being on a first side of the substrate 412 to couple to the stacked die 402, and the bonding pad 416 being on a second side of the substrate 412 to couple to the conductive connector 418, the second side of the substrate 412 being opposite to the first side. In some embodiments, the bonding pad 410 and the bonding pad 416 are formed by forming a recess (not shown) in a dielectric layer (not shown) on the first side and the second side of the substrate 412. The recess may be formed to allow the bonding pad 410 and the bonding pad 416 to be embedded in the dielectric layer. In other embodiments, since the bonding pad 410 and the bonding pad 416 may be formed on the dielectric layer, the recess is omitted. In some embodiments, the bonding pad 410 and the bonding pad 416 include a thin seed layer (not shown) made of copper, titanium, nickel, gold, palladium, etc. or a combination thereof. The conductive material of the bonding pad 410 and the bonding pad 416 may be deposited on the thin seed layer. The conductive material may be formed by electrochemical plating, chemical plating, chemical vapor deposition, atomic layer deposition (ALD), physical vapor deposition, etc. or a combination thereof. In one embodiment, the conductive material of the bonding pad 410 and the bonding pad 416 is copper, tungsten, aluminum, silver, gold, etc. or a combination thereof.

[0142] In some embodiments, the bonding pads 410 and the bonding pads 416 are under bump metals including three layers of conductive materials, such as a titanium layer, a copper layer, and a nickel layer. Other arrangements of materials and layers (e.g., an arrangement of chromium / chrome copper alloy / copper / gold, an arrangement of titanium / titanium tungsten / copper, or an arrangement of copper / nickel / gold) may be used to form the bonding pads 410 and the bonding pads 416. Any suitable material or material layer that may be used for the bonding pads 410 and the bonding pads 416 is fully intended to be included within the scope of the present invention. In some embodiments, the conductive vias 414 extend through the substrate 412 and couple at least one bonding pad 410 to at least one bonding pad 416.

[0143] In the illustrated embodiment, the stacked die 402 is coupled to the substrate 412 by wire bonds 406, but other connections, such as conductive bumps, may also be used. In one embodiment, the stacked die 402 is a stacked memory die. For example, the stacked die 402 may be a memory die, such as a dynamic random access memory (DRAM) die, a static random access memory (SRAM) die, a low-power (LP) double data rate (DDR) memory module, such as LPDDR (lowpower double data rate) 1, LPDDR2, LPDDR3, LPDDR4, and the like.

[0144] The stacked die 402 and the wire bonds 406 may be encapsulated by a molding material 408. For example, the molding material 408 may be molded onto the stacked die 402 and the wire bonds 406 using compression molding. In some embodiments, the molding material 408 is a molding compound, a polymer, an epoxy resin, a silicon oxide filler material, or the like, or a combination thereof. A curing process may be performed to cure the molding material 408, and the curing process may be thermal curing, UV curing, or the like, or a combination thereof.

[0145] Fig.17 FIG. 2 shows a cross-sectional view of a package body 30 according to some embodiments. Unless otherwise specified, the same reference symbols in this embodiment (and the embodiments discussed later) represent components formed by the same process. Figures 1 to 16 Therefore, the process steps and applicable materials are not repeated here. Figures 1 to 15 The one or more integrated circuit device stacks 10 described in the embodiment of the present invention are further packaged to form a package 30. The package 30 may also be referred to as a chip-on-wafer-on-substrate (CoWoS) package.

[0146] Fig.16 A specific packaging configuration is shown. Other packaging configurations may also be used in other embodiments. Fig.17 , a third package component 500 is shown, which may include one or more integrated circuit device stacks 10. In an embodiment, the third package component 500 may also include additional integrated circuit devices, such as transistors, capacitors, inductors, resistors, metallization layers, conductive connectors, etc., therein as required for specific functions. In some embodiments, the third package component 500 may include more than one device of the same type, or may include different devices. Fig.17 The invention shows a stack of three integrated circuit devices 10 (previously shown in Figures 1 to 15The third package component 500 (described in ), the three integrated circuit device stacks 10 are packaged and connected with the redistribution structure and the contact pads. In other embodiments, the third package component 500 may include any number of integrated circuit device stacks 10.

[0147] The third package component 500 may also include an interposer 516, which includes a substrate 514 and an interconnect structure 512. Each integrated circuit device stack 10 is attached to the interconnect structure 512 by means of an electrical connector 520 / 522 and a metal pillar 524, for example, by flip-chip bonding. The metal pillar 524 is formed on the redistribution structure 170 of each integrated circuit device stack 10, and the electrical connector 520 / 522 is formed at the top surface of the interconnect structure 512 on the conductive pad, which is formed in the dielectric layer of the interconnect structure 512. In some embodiments, the electrical connector 520 / 522 includes a metal pillar 520 with a metal capping layer 522 on the metal pillar 520, which may be a solder cap. The electrical connector 520 / 522 (including the pillar 520 and the capping layer 522) is sometimes referred to as a microbump 520 / 522. In some embodiments, the metal pillars 520 include conductive materials such as copper, aluminum, gold, nickel, palladium, etc. or combinations thereof, and may be formed by sputtering, printing, electroplating, chemical plating, chemical vapor deposition, or combinations thereof. The metal pillars 520 may be solder-free and have substantially longitudinal sidewalls. In some embodiments, each metal capping layer 522 is formed on each top surface of the metal pillars 520. The metal capping layer 522 may include nickel, tin, tin-lead, gold, copper, silver, palladium, indium, nickel-palladium-gold, nickel-gold, etc. or combinations thereof, and may be formed by a plating process. The metal pillars 524 may be similar to the metal pillars 520, and their description is not repeated here.

[0148] In another embodiment, the electrical connector 520 / 522 does not include a metal column, and is a solder ball and / or bump, such as a controlled collapse wafer connection (C4), electroless nickel immersion gold (ENIG), chemical nickel palladium gold (ENEPIG) to form a bump, etc. In such an embodiment, the bump electrical connector 520 / 522 may include a conductive material, such as solder, copper, aluminum, gold, nickel, silver, palladium, tin, etc. or a combination thereof. The electrical connector 520 / 522 may be formed by initially forming a solder layer by methods such as evaporation, electroplating, printing, solder transfer, ball placement, etc. Once the solder layer is formed on the structure, reflow may be performed to shape the material into the desired bump shape.

[0149] In one embodiment, the integrated circuit device stack 10 is bonded to the interconnect structure 512 by a reflow process. During the reflow process, the electrical connectors 520 / 522 / 524 come into contact to physically and electrically couple the integrated circuit device stack 10 to the interconnect structure 512.

[0150] The third package component 500 may further include an underfill material 504 dispensed between the integrated circuit device stacks 10 and the interconnect structure 512 . In some embodiments, the third package component 500 may include an encapsulant 506 surrounding each integrated circuit device stack 10 .

[0151] Still refer to Fig.17 , the packaging substrate 300 (previously Fig.16 306. The conductive connector 502 may be coupled to the bonding pad 306. The conductive connector 502 may be a ball grid array (BGA) connector, a solder ball, a metal column, a controlled collapse wafer connection (C4) bump, a microbump, a bump formed by chemical nickel palladium gold (ENEPIG), etc. The conductive connector 502 may include a conductive material, such as solder, copper, aluminum, gold, nickel, silver, palladium, tin, etc. or a combination thereof. In some embodiments, a solder resist 308 is formed on the substrate core 310, and the conductive connector 502 may be disposed in an opening in the solder resist 308 to electrically couple and mechanically couple to the bonding pad 306. The solder resist 308 may be used to protect an area of ​​the substrate core 310 from external damage.

[0152] The third package component 500 is placed on the conductive connector 502 of the package substrate 300, thereby forming an electrical connection between the third package component 500 and the package substrate 300. The third package component 500 can be placed so that the conductive bump 508 is aligned with the conductive connector 502 of the package substrate 300. Once there is physical contact, the conductive connector 502 of the package substrate 300 can be bonded to the third package component 500 using a reflow process. An underfill 518 can then be formed around the conductive connector 502 between the third package component 500 and the package substrate 300.

[0153] Fig.18 FIG. 4 is a cross-sectional view of a package body 40 according to some embodiments. Unless otherwise specified, the same reference symbols in this embodiment (and the embodiments discussed later) represent components formed by the same process. Figures 1 to 17 The same components as in the illustrated embodiments, therefore, the process steps and applicable materials are not repeated here. Figures 1 to 15 One or more integrated circuit device stacks 10 described in the accompanying drawings are further packaged to form a package body 40 .

[0154] exist Fig.18 In the embodiment, for example, the conductive connector 108 (previously described in Fig.14 Attaching the integrated circuit device stack 10 to the package substrate 300 (previously described in Fig.16 as well as Fig.17). In some embodiments, the conductive connector 108 is reflowed to attach the integrated circuit device stack 10 to the bonding pad 306 of the package substrate 300. The conductive connector 108 electrically and / or physically couples the package substrate 300 including the metallization layer in the substrate core 310 to the integrated circuit device stack 10. In some embodiments, a solder resist 308 is formed on the substrate core 310. The conductive connector 108 can be disposed in an opening in the solder resist 308 to electrically and mechanically couple to the bonding pad 306. The solder resist 308 can be used to protect an area of ​​the substrate core 310 from external damage.

[0155] The conductive connector 108 may have an epoxy flux (not shown) formed thereon before reflow, wherein at least some epoxy portion of the epoxy flux remains after the integrated circuit device stack 10 is attached to the package substrate 300. This remaining epoxy portion may function as an underfill to reduce stress and protect the joint created by the reflow of the conductive connector 108. In some embodiments, an underfill 320 may be formed between the integrated circuit device stack 10 and the package substrate 300 and around the conductive connector 108. The underfill 320 may be formed by a capillary flow process after the first package component 200 is attached, or may be formed by a suitable deposition method before the integrated circuit device stack 10 is attached.

[0156] The second packaged component 400 (previously in Fig.16 4 (described in the drawings) is coupled to the package substrate 300. The conductive connector 424 can be coupled to the bonding pad 306 of the package substrate 300 and the bonding pad 416 of the second package component to allow the package substrate 300 to be electrically coupled to the second package component 400. The conductive connector 424 can be a ball grid array (BGA) connector, a solder ball, a metal pillar, a controlled collapse wafer connection (C4) bump, etc. The conductive connector 424 may include a conductive material, such as solder, copper, aluminum, gold, nickel, silver, palladium, tin, etc. or a combination thereof.

[0157] Embodiments of the present disclosure have some advantageous features. Embodiments include bonding semiconductor die to a substrate, and performing a plasma treatment to dope the top surface and sidewalls of each semiconductor die with a suitable dopant (e.g., fluorine). The doping concentration of the dopant in the corresponding sidewall of each semiconductor die may decrease in a longitudinal direction away from the top surface of the semiconductor die. A gap filling process is then performed to fill the gaps between the semiconductor die with a dielectric material.

[0158] One or more embodiments disclosed herein may allow for increased hydrophobicity of the top surface and upper sidewalls of a semiconductor die compared to the lower sidewalls of the semiconductor die. For example, the hydrophobicity of the sidewalls of the semiconductor die decreases in a longitudinal direction away from the top surface of the semiconductor die. As a result, during a gap fill process, the increased hydrophobicity of the top portion of the semiconductor die compared to the bottom portion of the semiconductor die may allow the dielectric material to fill and adhere to the bottom portion of the semiconductor die before filling and adhering to the top portion of the semiconductor die. This allows the gap to be filled from the bottom up, thereby allowing a greater depth of gap to be filled without forming large voids. As a result, the reliability and performance of the device are improved. The bottom-up filling process may further reduce the roughness of the dielectric material, thereby allowing an improved interface with an overlying structure of an integrated circuit package and improved device reliability. In addition, after the gap fill process, no residue will accumulate on the top surface of the semiconductor die, eliminating the need for a cleaning process after performing the gap fill process and reducing manufacturing costs.

[0159] According to some embodiments, a method is provided, comprising bonding a first semiconductor die and a second semiconductor die to a substrate, wherein a gap is disposed between a first sidewall of the first semiconductor die and a second sidewall of the second semiconductor die; performing plasma treatment to dope a top surface and a sidewall of each of the first semiconductor die and the second semiconductor die with a first dopant, wherein a concentration of the first dopant in the first sidewall decreases in a longitudinal direction from a top surface of the first semiconductor die toward a bottom surface of the first semiconductor die, and a concentration of the first dopant in the second sidewall decreases in a longitudinal direction from a top surface of the second semiconductor die toward a bottom surface of the second semiconductor die; and filling the gap with a spin-on dielectric material.

[0160] According to some embodiments, performing the plasma treatment includes exposing the top surface and sidewalls of each of the first semiconductor die and the second semiconductor die to a fluorine plasma. According to some embodiments, the fluorine plasma is generated by a gas mixture including CF4, C2F6, or C4F8. According to some embodiments, the dopant depth of the first sidewall decreases in a longitudinal direction from the top surface of the first semiconductor die toward the bottom surface of the first semiconductor die, and the dopant depth of the second sidewall decreases in a longitudinal direction moving from the top surface of the second semiconductor die to the bottom surface of the second semiconductor die. According to some embodiments, filling the gap with a spin-on dielectric material includes spin-coating a silicon-containing liquid precursor on the substrate to fill the gap with the silicon-containing liquid precursor. According to some embodiments, the method further includes planarizing the top surfaces of the first semiconductor die, the second semiconductor die, and the spin-on dielectric material after filling the gap with the spin-on dielectric material, wherein after planarizing the top surfaces of the first semiconductor die, the second semiconductor die, and the spin-on dielectric material, the spin-on dielectric material has an arithmetic average roughness (Ra) of less than or equal to 10 angstroms. According to some embodiments, after planarizing the top surfaces of the first semiconductor die, the second semiconductor die, and the spin-on dielectric material, a top surface of a central region of each of the first semiconductor die and the second semiconductor die is undoped. According to some embodiments, after planarizing the top surfaces of the first semiconductor die, the second semiconductor die, and the spin-on dielectric material, a third semiconductor die is bonded to the first semiconductor die, and a fourth semiconductor die is bonded to the second semiconductor die.

[0161] According to some embodiments, a method is provided, comprising bonding a plurality of bare die to a first substrate, each of the bare die comprising a semiconductor substrate and an interconnect structure on the semiconductor substrate; after bonding the bare die to the first substrate, doping a top surface and a side wall of each semiconductor substrate of the bare die with a first dopant so that the hydrophobicity of the side wall of each semiconductor substrate decreases in a longitudinal direction from the top surface of the semiconductor substrate toward the bottom surface of the semiconductor substrate; and forming a dielectric material between each of the bare die.

[0162] According to some embodiments, the concentration of the first dopant in the sidewall of each semiconductor substrate decreases in a longitudinal direction from the top surface of the semiconductor substrate toward the bottom surface of the semiconductor substrate. According to some embodiments, doping the top surface and the sidewall of each semiconductor substrate of the bare crystal includes exposing the top surface and the sidewall of each semiconductor substrate to a fluorine plasma. According to some embodiments, the fluorine plasma is generated by a gas mixture including CF4, C2F6 or C4F8. According to some embodiments, doping the top surface and the sidewall of each semiconductor substrate includes performing an ion beam implantation process to introduce the first dopant into the top surface and the sidewall of each semiconductor substrate. According to some embodiments, the ion beam implantation process includes directing the implanted substance at an inclined angle, and the inclined angle is in the range of 0° to 15° relative to an axis perpendicular to the main surface of the first substrate. According to some embodiments, forming a dielectric material between each of the bare wafers includes: spin-coating a silicon-containing liquid precursor on a first substrate to fill the gap between each of the bare wafers with the silicon-containing liquid precursor, wherein after the silicon-containing liquid precursor is spin-coated on the first substrate, the highest point of the silicon-containing liquid precursor is below the top surface of the bare wafer; and performing a curing process to form a solid phase of the dielectric material in the gap.

[0163] According to some embodiments, a package is provided, including a redistribution structure, a first die, and a first dielectric material, wherein the first die is above the redistribution structure and electrically coupled to the redistribution structure, the first dielectric material encapsulates the first die, wherein the sidewall of the first die includes a first dopant, wherein the concentration of the first dopant in the sidewall of the first die decreases in a longitudinal direction from a top surface of the first die toward a bottom surface of the first die.

[0164] According to some embodiments, the first dopant is fluorine. According to some embodiments, the hydrophobicity of the sidewalls of the first die decreases in a longitudinal direction from a top surface of the first die toward a bottom surface of the first die. According to some embodiments, the package further includes a second die and a second dielectric material, the second die being above and bonded to the first die, the second dielectric material encapsulating the second die, wherein the sidewalls of the second die include the first dopant, wherein a concentration of the first dopant in the sidewalls of the second die decreases in a longitudinal direction from a top surface of the second die toward a bottom surface of the second die. According to some embodiments, the second dielectric material is silicon oxide, and the second dielectric material overlaps a portion of the top surface of the first die.

[0165] The foregoing text summarizes the features of many embodiments so that those with ordinary knowledge in the art can better understand the present disclosure from various aspects. Those with ordinary knowledge in the art should understand and can easily design or modify other processes and structures based on the present disclosure to achieve the same purpose and / or achieve the same advantages as the embodiments introduced herein. Those with ordinary knowledge in the art should also understand that these equivalent structures do not deviate from the spirit and scope of the invention of the present disclosure. Various changes, substitutions or modifications may be made to the present disclosure without departing from the spirit and scope of the invention of the present disclosure.

Claims

1. A method for forming a package, characterized in that: include: Bonding a first semiconductor die and a second semiconductor die to a substrate, wherein a gap is disposed between a first sidewall of the first semiconductor die and a second sidewall of the second semiconductor die; performing a plasma treatment to dope top surfaces and sidewalls of each of the first semiconductor die and the second semiconductor die with a first dopant, wherein a concentration of the first dopant in the first sidewall decreases in a longitudinal direction from a top surface of the first semiconductor die toward a bottom surface of the first semiconductor die, and a concentration of the first dopant in the second sidewall decreases in a longitudinal direction from a top surface of the second semiconductor die toward a bottom surface of the second semiconductor die; as well as The gap is filled with a spin-on dielectric material.

2. The method for forming a package according to claim 1, wherein: Performing the plasma treatment includes exposing the top surface and the sidewalls of each of the first semiconductor die and the second semiconductor die to a fluorine plasma.

3. The method for forming a package according to claim 1, wherein: A dopant depth of the first sidewall decreases in the longitudinal direction from the top surface of the first semiconductor die toward the bottom surface of the first semiconductor die, and a dopant depth of the second sidewall decreases in the longitudinal direction moving from the top surface of the second semiconductor die toward the bottom surface of the second semiconductor die.

4. The method for forming a package according to claim 1, wherein: Filling the gap with the spin-on dielectric material includes spin-coating a silicon-containing liquid precursor on the substrate to fill the gap with the silicon-containing liquid precursor.

5. The method for forming a package according to claim 4, wherein: Also includes: After filling the gap with the spin-on dielectric material, the top surfaces of the first semiconductor bare crystal, the second semiconductor bare crystal, and the spin-on dielectric material are planarized, wherein after planarizing the top surfaces of the first semiconductor bare crystal, the second semiconductor bare crystal, and the spin-on dielectric material, an arithmetic mean roughness of the spin-on dielectric material is less than or equal to 10 angstroms.

6. The method for forming a package according to claim 5, wherein: After planarizing the top surfaces of the first semiconductor die, the second semiconductor die, and the spin-on dielectric material, a top surface of a central region of each of the first semiconductor die and the second semiconductor die is undoped.

7. A method for forming a package, characterized in that: include: A plurality of bare dies are bonded to a first substrate, each of the plurality of bare dies comprising: a semiconductor substrate; and an interconnect structure on the semiconductor substrate; After bonding the plurality of bare die to the first substrate, doping the top surfaces and the side walls of each of the semiconductor substrate of the plurality of bare die with a first dopant so that a hydrophobicity of the side walls of each of the semiconductor substrates decreases in a longitudinal direction from the top surface of the semiconductor substrate toward a bottom surface of the semiconductor substrate; and A dielectric material is formed between each of the plurality of dies.

8. A package, characterized in that: include: A distributed structure; a first bare die on the redistribution structure and electrically coupled to the redistribution structure; as well as A first dielectric material encapsulates the first die, wherein several sidewalls of the first die include a first dopant, wherein a concentration of the first dopant in the several sidewalls of the first die decreases in a longitudinal direction from a top surface of the first die toward a bottom surface of the first die.

9. The package according to claim 8, characterized in that It further includes a second die and a second dielectric material, the second die is above the first die and bonded to the first die, the second dielectric material encapsulates the second die, wherein several sidewalls of the second die include the first dopant, wherein a concentration of the first dopant in the several sidewalls of the second die decreases in a longitudinal direction from a top surface of the second die toward a bottom surface of the second die.

10. The package according to claim 9, wherein: The second dielectric material is silicon oxide, and the second dielectric material overlaps a portion of the top surface of the first die.